Method for etching etching layer
The method of generating an etching plasma and using plasma-free atomic layer deposition with tungsten hexafluoride at controlled temperatures addresses the challenge of maintaining vertical profiles in semiconductor etching, reducing sidewall curvature and preventing device damage.
Patent Information
- Application Number
- JP2024131827
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2018-11-05
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-06
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing etching methods for semiconductor devices face challenges in maintaining a vertical profile with minimal lateral CD growth while avoiding profile trade-offs such as reduced mask selectivity, etch rate, and feature clogging, particularly when high temperatures are required for sidewall passivation.
A method involving the generation of an etching plasma followed by a plasma-free atomic layer deposition process to deposit a protective film on sidewalls, using tungsten hexafluoride (WF6) at controlled temperatures below 100°C, with multiple cycles of reactant gas exposure and purging to form a non-conformal protective film.
This approach maintains a vertical etching profile with reduced sidewall curvature and prevents damage to semiconductor devices, ensuring high aspect ratio etching without compromising etch rate or mask selectivity.
Smart Images

Figure 2024156947000001_ABST
Abstract
Description
[Background technology]
[0001] [CROSS REFERENCE TO RELATED APPLICATIONS] This application claims the benefit of priority to U.S. Application No. 62 / 755,707, filed November 5, 2018, which is incorporated by reference herein for all purposes.
[0002] The present disclosure relates to methods of forming semiconductor devices on a semiconductor wafer, and more particularly to etching recessed features in an etching layer of a stack.
[0003] In forming a semiconductor device, an etching layer may be etched to form a contact hole or a trench. Some semiconductor devices may be formed by etching a silicon oxide (SiO2) based layer. Summary of the Invention
[0004] To achieve the above and in accordance with the objectives of the present disclosure, a method for etching a feature in a stack comprising a dielectric material on a substrate is provided. In step (a), an etching plasma is generated from an etching gas, and the stack is exposed to the etching plasma to partially etch a feature in the stack. In step (b), an atomic layer deposition process is provided after step (a) to deposit a protective film on the sidewall. The atomic layer deposition process includes a number of cycles, each cycle including: exposing the stack to a first reactive gas comprising WF6, where the first reactive gas is adsorbed on the stack; and exposing the stack to a plasma formed from a second reactive gas, where the plasma formed from the second reactive gas reacts with the adsorbed first reactive gas to form a protective film on the stack. In step (c), steps (a)-(b) are repeated at least once.
[0005] In another embodiment, an apparatus for etching features in a stack is provided. A process chamber is provided. A substrate support is inside the process chamber. A gas inlet provides gas to the process chamber. A gas source provides gas to the gas inlet and includes an etching gas source, a WF6 gas source, and a reactive gas source. An exhaust pump is provided to exhaust gas from the process chamber. An electrode provides RF power to the process chamber. At least one power source provides power to the electrode. A controller is controllably connected to the gas source and the at least one power source and comprises at least one processor and a computer readable medium. The computer readable medium comprises computer code for effecting etching of the stack by a first plurality of cycles, each of the first plurality of cycles including partially etching the stack and depositing a layer on the stack by atomic layer deposition by providing a second plurality of cycles. Each cycle of the second plurality of cycles includes flowing a WF6-containing gas from a WF6 gas source, adsorbing the WF6-containing gas into the stack, stopping the flow of the WF6-containing gas, and exposing the stack to a plasma of a reactive gas from a reactive gas source, where the plasma converts the adsorbed WF6-containing gas into an atomic layer deposition layer.
[0006] These and other features of the present disclosure will be described in more detail below in the detailed description of the present disclosure taken in conjunction with the following figures. [Brief description of the drawings]
[0007] The present disclosure is illustrated by way of example and not limitation in the figures of the accompanying drawings, in which like reference numerals refer to like elements and in which:
[0008] [Figure 1] 1 is a high level flow chart of one embodiment.
[0009] [Figure 2A] 1 is a schematic diagram of a laminate processed according to one embodiment. [Figure 2B] 1 is a schematic diagram of a laminate processed according to one embodiment. [Figure 2C] 1 is a schematic diagram of a laminate processed according to one embodiment. [Figure 2D] 1 is a schematic diagram of a laminate processed according to one embodiment. [Figure 2E] 1 is a schematic diagram of a laminate processed according to one embodiment. [Figure 2F] 1 is a schematic diagram of a laminate processed according to one embodiment. [Figure 2G] 1 is a schematic diagram of a laminate processed according to one embodiment.
[0010] [Diagram 3] 1 is a schematic diagram of an etching chamber that may be used in one embodiment.
[0011] [Figure 4] FIG. 1 is a schematic diagram of a computer system that may be used to implement one embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] The present disclosure will now be described in detail with reference to several exemplary embodiments as illustrated in the accompanying drawings. In the following description, numerous specific details are set forth in order to provide a thorough understanding of the present disclosure. However, it will be apparent to one skilled in the art that the present disclosure may be practiced without some or all of these specific details. In other instances, well-known process steps and / or structures have not been described in detail in order not to unnecessarily obscure the present disclosure.
[0013] High aspect ratio etches require maintaining a vertical profile with minimum lateral CD (critical dimension) growth (CD curvature). Also, profile tradeoffs such as reduced mask selectivity, reduced etch rate, or capping / clogging of features must be avoided. CD curvature is caused by etching the sidewalls of the features. To reduce the CD curvature, a passivation layer may be placed on the sidewalls. Some methods deposit the sidewall passivation at temperatures higher than 250°C to provide uniform passivation. Such high temperatures can damage semiconductor devices.
[0014] In an example embodiment, FIG. 1 is a high level flow chart of an embodiment. This embodiment may be used to process a stack 200 as shown in FIG. 2A. FIG. 2A is a cross-sectional view of stack 200 with substrate 204 disposed beneath etch layer 208 disposed beneath mask 212. In this example, mask 212 is a hard mask such as a plasma enhanced chemical vapor deposition (PECVD) amorphous carbon mask. In this example, etch layer 208 is a dielectric layer made of a dielectric material such as silicon oxide (SiO2). One or more layers (not shown) may be disposed between substrate 204 and etch layer 208. One or more layers (not shown) may also be disposed between etch layer 208 and mask 212.
[0015] The features are partially etched into the etch layer 208 (step 104). An example recipe for partially etching the features into the etch layer 208 (step 104) provides a pressure of 5 to 50 mTorr. Radio frequency (RF) power is provided at a frequency of 60 megahertz (MHz) with a power of 500 watts (W) to 10 kilowatts (kW) and at a frequency of 400 kilohertz (kHz) with a power of 1 kW to 30 kW. The RF power is pulsed between these power levels. An etch gas is provided. The etch gas includes oxygen (O2), fluorocarbons, and / or hydrofluorocarbons. The etch gas is turned into a plasma by the RF power. The plasma provides the radical ions responsible for the high aspect ratio etch. Such a plasma is referred to herein and in the claims as an etch plasma. Once the partial etch is complete, the flow of the etch gas is stopped. The RF power is stopped or reduced so that no plasma is generated. FIG. 2B is a cross-sectional view of stack 200 after feature 216 has been partially etched.
[0016] After the partial etch (step 104), an atomic layer deposition process is provided to deposit a protective film on the sidewalls of the feature 216 (step 108). The atomic layer deposition process (step 108) includes a cyclic process with multiple cycles. In a first stage of one cycle of the atomic layer deposition process (step 108), the stack 200 is exposed to a first reactant gas including tungsten hexafluoride (WF6) (step 112). A gas flow including 0.5-200 sccm of WF6 is provided. In this embodiment, the first reactant gas is not plasmatized. As a result, this process is plasma-free. The stack temperature is maintained at a temperature between 40° C. and 80° C. The first reactant gas adsorbs on the surface of the stack 200. The flow of the first reactant gas is stopped after 3 seconds.
[0017] Without being bound by theory, it is believed that WF6 chemically reacts with SiO2 to form a layer of tungsten oxide silicide (SiOW). Figure 2C is a cross-sectional view of stack 200 after SiOW layer 220 has been formed on the surface (including sidewalls) of feature 216. SiOW layer 220 is not drawn to scale, but is shown thicker to better illustrate SiOW layer 220.
[0018] After the first reactant gas is adsorbed (step 112), a first purge is provided to purge the first reactant gas (step 116). In this example, the first purge is provided by flowing O2 into the plasma processing chamber. Other embodiments may have a purge gas of pure nitrogen (N2), or a mixture of N2 and argon (Ar), or pure Ar. The O2 purge gas can generate a plasma immediately after the first purge. The purge gas flow is stopped after 5 seconds. The first purge completely removes any unadsorbed tungsten (W) before the plasma is formed in the next step.
[0019] After the first purge is completed (step 116), the stack 200 is exposed to a plasma formed from a second reactant gas (step 120). The stack 200 and the chamber are maintained at a temperature less than 150° C. A second reactant gas is provided. In this example, the second reactant gas is O2. The second reactant gas is turned into a plasma by providing excitation energy at a power of 200 W to 20 kW and a frequency of 60 MHz. A bias RF signal is provided at a power of 200 W to 50 kW and a frequency of 100 kHz to 27 MHz. The plasma is extinguished after 3 seconds.
[0020] After the stack 200 is exposed to the plasma formed from the second reactant gas (step 120), a second purge is provided to purge residual plasma ion radicals (step 124). In this example, the second purge is provided by flowing the second reactant gas into the plasma processing chamber without sufficient RF power to form a plasma. The second reactant gas is used to purge residual plasma. Other embodiments may have other purge gases. Some embodiments may turn off the RF power. The purge gas flow is stopped after 5 seconds. The second purge completely removes plasma ion radicals from the plasma processing chamber. The atomic layer deposition cycle is then repeated. In this example, the atomic layer deposition process (step 108) is performed for 3 to 100 cycles.
[0021] FIG. 2D is a cross-sectional view of stack 200 after multiple cycles of atomic layer deposition process (step 108) are applied to form protective film 224 on the sidewalls of feature 216. In this example, protective film 224 comprises tungsten oxide. Protective film 224 is not drawn to scale. Because atomic layer deposition process (step 108) uses a plasma rather than a plasma-free thermal process, protective film 224 is not as conformal as a film deposited using a plasma-free thermal process. Protective film 224 may also not be of as high quality as a film deposited using a plasma-free thermal process. Because protective film 224 is not conformal, in this embodiment protective film 224 does not extend to the bottom of feature 216.
[0022] After the atomic layer deposition process (step 108) is completed, the feature 216 is further etched (step 128). An example recipe for further etching the feature into the etch layer 208 provides a pressure of 5-50 mTorr. RF power is provided at a frequency of 60 MHz with a power of 2 kW-8 kW and at a frequency of 400 kHz with a power of 4 kW-25 kW. The RF power is pulsed between these power levels. An etching gas is provided. The etching gas includes O2, fluorocarbons, and / or hydrofluorocarbons. The etching gas is turned into an etching plasma by the RF power. FIG. 2E is a cross-sectional view of the stack 200 after the feature 216 has been further etched.
[0023] If the etching of the feature is not complete (step 132) (i.e., the feature is not etched to its final depth), the process returns to the atomic layer deposition process (step 108). The atomic layer deposition process (step 108) is repeated. Figure 2F is a cross-sectional view of stack 200 after the atomic layer deposition process (step 108) has been repeated and a new protective film 228 has been formed. The new protective film 228 is not conformal because it was formed using a plasma.
[0024] Feature 216 is further etched (step 128). The cycle of atomic layer deposition process (step 108) and further etching (step 128) is repeated until etching of feature 216 is complete (step 132). Figure 2G is a cross-sectional view of stack 200 after feature 216 has been etched to its final depth.
[0025] The above embodiment provides sidewall passivation to prevent or reduce feature bowing by using plasma during the atomic layer deposition process (step 108). If a thermal atomic layer deposition process is used to deposit tungsten, a deposition temperature or chamber temperature higher than 250° C. would be used. Temperatures higher than 250° C. may damage the semiconductor device being formed. The atomic layer deposition process using plasma to deposit the tungsten-containing protective film (step 108) provides a poor quality protective film with poor conformality. However, it has been found that a tungsten-containing non-conformal protective film is sufficient to prevent or reduce sidewall bowing.
[0026] In various embodiments, the atomic layer deposition process (step 108) is performed at a deposition temperature or chamber temperature of less than 100° C. In various embodiments, the plasma formed by the second reactant gas provides either oxidation or nitridation. If the plasma from the second reactant gas provides oxidation, in various embodiments, the second reactant gas includes an oxygen-containing component (e.g., at least one of oxygen (O2), ozone (O3), carbonyl sulfide (COS), carbon dioxide (CO2), sulfur dioxide (SO2), and carbon monoxide (CO)). Argon (Ar) or krypton (Kr) may also be used as a carrier gas. If the plasma from the second reactant gas provides nitridation, the second reactant gas includes a nitrogen-containing component (e.g., at least one of nitrogen (N2) and ammonia (NH3)). Ar or Kr may also be used as a carrier gas. If the second reactant gas includes N2, the second reactant gas may further include H2.
[0027] In various embodiments, the hard mask may be formed from amorphous carbon, boron-doped carbon, boron-doped silicon, metal-doped carbon, or polysilicon. In various embodiments, the etch layer 208 is a silicon oxide-based dielectric layer. In various embodiments, the etch layer 208 is a stack of different material layers. In various embodiments, at least one of the etch layers 208 is a layer of a dielectric material. In various embodiments, the atomic layer deposition process (step 108) provides a protective film 228 that is non-conformal and does not reach the bottom of the feature 216. In various embodiments, the RF power may be continuous wave. In other embodiments, the RF power may be pulsed power. In various embodiments, the pulsed RF power may have a pulse repetition rate between 100 Hz and 5 kHz. In various embodiments, the pulsed RF power may have a duty cycle between 5% and 95%.
[0028] Additionally, because the atomic layer deposition process (step 108) uses plasma rather than thermal processing, it may be performed in-situ in the same plasma processing chamber as the etching process (step 128). Since all steps are performed in the same plasma processing chamber, an in-situ atomic layer deposition process (step 108) provides higher throughput.
[0029] In an exemplary embodiment, FIG. 3 is a schematic diagram of an etching reactor that may be used in an embodiment. In one or more embodiments, the plasma processing chamber 300 includes a gas distribution plate 306 providing a gas inlet and an electrostatic chuck (ESC) 308 inside an etching chamber 349 surrounded by a chamber wall 352. Inside the etching chamber 349, the stack 200 is placed on the ESC 308. The ESC 308 is also a substrate support. An edge ring 309 surrounds the ESC 308. A gas source 310 is connected to the etching chamber 349 through the gas distribution plate 306. In this example, the gas source 310 includes an etching gas source 312, a WF6 gas source 316, and a reactant gas source 318. The ESC temperature controller 350 is connected to a chiller 314. In this embodiment, the chiller 314 provides a coolant to a flow passage 315 in or near the ESC 308 to cool the ESC 308. A radio frequency (RF) source 330 provides RF power to the lower electrode. In this embodiment, the ESC 308 is the bottom electrode. In an exemplary embodiment, 400 kHz and 60 MHz power sources constitute the RF source 330. In this embodiment, the top electrode and the gas distribution plate 306 are grounded. In this embodiment, one generator is provided for each frequency. In other embodiments, other arrangements of RF sources and electrodes may be used. A controller 335 is controllably connected to the RF source 330, the exhaust pump 320, and the gas source 310. An example of such an etching chamber is the Flex™ Etch System manufactured by Lam Research Corporation of Fremont, California. The processing chamber is a CCP (capacitively coupled plasma) reactor or an ICP (inductively coupled plasma) reactor.
[0030] 4 is a high-level block diagram illustrating a computer system 400 suitable for implementing the controller 335 used in the embodiments. The computer system may have many physical forms ranging from integrated circuits, printed circuit boards, and small handheld devices to large supercomputers. The computer system 400 includes one or more processors 402 and may further include an electronic display device 404 (for displaying images, text, and other data), a main memory 406 (e.g., random access memory (RAM)), a storage device 408 (e.g., a hard disk drive), a removable storage device 410 (e.g., an optical disk drive), a user interface device 412 (e.g., a keyboard, touch screen, keypad, mouse, or other pointing device, etc.), and a communication interface 414 (e.g., a wireless network interface). The communication interface 414 allows software and data to be transferred between the computer system 400 and external devices through a link. The system may also include a communication infrastructure 416 (e.g., a communication bus, crossover bar, or network) to which the devices / modules are connected.
[0031] Information transferred through communications interface 414 may be in the form of signals, such as electronic, electromagnetic, optical, or other signals that can be received by communications interface 414 over a communications link that transmits the signals, and may be implemented using wires or cables, fiber optics, telephone lines, cellular phone links, radio frequency links, and / or other communications paths. Through such communications interfaces, one or more processors 402 may receive information from a network or output information to a network in the course of performing steps of the methods described above. Additionally, method embodiments may be performed solely on a processor or may be performed over a network, such as the Internet, in cooperation with a remote processor that shares some of the processing.
[0032] The term "non-transitory computer-readable medium" generally refers to main memory, secondary memory, removable storage, and storage devices (hard disks, flash memory, disk drive memory, CD-ROMs, and other forms of persistent memory), and should not be construed to include transitory objects such as carrier waves or signals. Examples of computer code include machine code produced by a compiler and files containing higher level code that are executed by a computer using an interpreter. The computer-readable medium may also be computer code embodied in a carrier wave and transmitted by a computer data signal representing a sequence of instructions executable by a processor.
[0033] Although the present disclosure has been described in terms of several exemplary embodiments, there are changes, modifications, permutations, and various substitute equivalents that fall within the scope of the present disclosure. It should also be noted that there are many alternative ways of implementing the methods and apparatuses of the present disclosure. It is therefore intended that the following appended claims be interpreted to include all such changes, modifications, permutations, and various substitute equivalents that fall within the true spirit and scope of the present disclosure.
Claims
1. 1. A method of etching features in a layered structure including a dielectric material on a substrate, comprising: (a) generating an etching plasma from an etching gas and exposing the stack to the etching plasma to partially etch a feature into the stack; (b) after (a), providing an atomic layer deposition process to deposit a protective film on the sidewall, the atomic layer deposition process comprising a plurality of cycles, each cycle comprising: (i) WF 6 exposing the stack to a first reactant gas comprising: (ii) exposing the stack to a plasma formed from a second reactive gas, the plasma formed from the second reactive gas reacting with the adsorbed first reactive gas to form the protective film on the stack; (c) repeating (a)-(b) at least once; A method comprising:
2. 2. The method of claim 1 , The method, wherein the step of providing the atomic layer deposition process further comprises maintaining a deposition temperature below 150°C.
3. 2. The method of claim 1 , The method of claim 1, wherein the second reactant gas comprises at least one of an oxygen-containing component and a nitrogen-containing component.
4. 2. The method of claim 1 , The second reaction gas is COS, CO 2 , CO, SO 2 , O 2 , N 2 , N.H. 3 , and O 3 The method includes at least one of the following:
5. 2. The method of claim 1 , The laminate is made of SiO 2 A method comprising:
6. 6. The method of claim 5, The method, wherein the stack further comprises a hard mask.
7. 7. The method of claim 6, The method, wherein the hard mask comprises one or more of amorphous carbon, boron doped carbon, boron doped silicon, metal doped carbon, and polysilicon.
8. 2. The method of claim 1 , The method, wherein the step of providing the atomic layer deposition process is performed for 2 to 100 cycles.
9. 2. The method of claim 1 , Each cycle further comprises: purging the first reactant gas after exposing the stack to the first reactant gas and before exposing the stack to the plasma formed by the second reactant gas; purging the plasma formed from the second reactive gas after exposing the stack to the plasma formed from the second reactive gas; A method comprising:
10. 2. The method of claim 1 , The method, wherein the step of exposing the stack to the first reactive gas is a plasma-free step.
11. 2. The method of claim 1 , A method wherein steps (a)-(c) are performed in situ.
12. 1. An apparatus for etching features in a layered film, comprising: a processing chamber; a substrate support within the processing chamber; a gas inlet for providing gas to the processing chamber; a gas source for providing the gas to the gas inlet, a source of etching gas; W.F. 6 A gas source; a gas source, including a reactive gas source; an exhaust pump for exhausting gases from the processing chamber; an electrode for providing RF current to the processing chamber; at least one power source for providing power to the electrodes; a controller controllably connected to the gas source and the at least one power source, the controller comprising: At least one processor; 16. A computer readable medium comprising computer code for effecting etching of a stack through a first plurality of cycles, each of the first plurality of cycles comprising: partially etching the stack; and depositing a layer on the stack by atomic layer deposition by providing a second plurality of cycles, each cycle of the second plurality of cycles comprising: The WF 6 Gas source to WF 6 flowing a contained gas; The WF 6 Adsorbing the contained gas; The WF 6 stopping said flow of contained gas; exposing the layer to a plasma of a reactive gas from the reactive gas source, the plasma dissolving the adsorbed WF 6 and converting the containing gas into an atomic layer deposition layer. An apparatus comprising:
13. 13. The apparatus of claim 12, further comprising: The apparatus further comprises a chiller for cooling the substrate support.
14. 13. The apparatus of claim 12, The computer readable medium further comprises computer code for cooling the substrate support to a temperature of 150° C. or less.
15. 13. The apparatus of claim 12, W.F. 6 The apparatus, wherein the step of flowing a containing gas is a plasma-free step.
16. 13. The apparatus of claim 12, The reactive gas source is COS, CO 2 , CO, SO 2 , O 2 , N 2 , N.H. 3 , and O 3 The apparatus is at least one source of.
17. 13. The apparatus of claim 12, The apparatus, wherein the step of providing the atomic layer deposition process is performed for 2 to 100 cycles.
18. 13. The apparatus of claim 12, Each cycle of the second plurality of cycles further comprises: The WF 6 purging the first reactant gas after stopping the flow of the containing gas and before exposing the stack to the plasma formed by the second reactant gas; purging the plasma formed from the second reactive gas after exposing the stack to the plasma formed from the second reactive gas; 13. An apparatus comprising:
Citation Information
Patent Citations
Method of manufacturing semiconductor device
JP2017163032A
Substrate support having area between mesas of different depth and corresponding temperature dependent processing method
JP2018098497A
Ultrathin atomic layer deposition film accuracy thickness control
US20160276148A1
Mask shrink layer for high aspect ratio dielectric etch
US20170076945A1
Method of Forming a Feature of a Target Material on a Substrate
US20170178905A1
Cited By
Print zone driver for a printer conveyor belt
US12304194B2
Print zone encoder
US12420570B2