Method of preparing cement plastic mixture
A cement-plastic mixture using plastic waste and specific additives addresses the ecological use challenge, producing high-strength construction materials with improved thermal insulation and water resistance.
Patent Information
- Application Number
- JP2024137028
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-06-07
- Filing Date
- 2024-08-16
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2042-06-07
AI Technical Summary
Existing cement mixtures lack a method for ecological use and consumption of plastic waste, which is a challenge in the construction and masonry field.
A cement-plastic mixture is prepared by combining crushed plastic waste with cement, silica sand, and other additives like a plasticizer, setting accelerator, and synthetic fibers, following a specific mixing process to create a high-strength, self-leveling composition.
The method results in a high-strength cementitious plastic mixture that can be used to produce various construction products, effectively utilizing plastic waste and enhancing thermal insulation and water impermeability.
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for the preparation of a cement-plastic mixture which can be used for the production of building and stone products. The present invention is in the field of construction and masonry. [Background technology]
[0002] Currently, products based on cement, silica sand and stone, granite or marble chips, such as terrazzo, are commonly known in the construction and masonry fields. Terrazzo is a poured or precast in place composite material that is used for floor and wall treatments. It contains chips of marble, quartz, granite, glass or other suitable material poured together with a cementitious binder (for chemical bonding), a polymeric binder (for physical bonding), or a combination of both.
[0003] Russian Patent No. 2739910 C1 is known in the prior art, which describes a polymer-cement dry construction mix containing Portland cement, a polymeric binder, sand, glass fibers and a modifier, the polymeric binder being a redispersible polyvinyl acetate polymer powder or polyvinyl acetate copolymer.
[0004] A two-component fast-setting plastic cement is also known from CN112063160A, in which the first component is a polyether polyol, a hardener, a surface hydroxylated modified paraffin, a thickener and a solid filler. The second component is a polyether polyol, a catalyst, a crosslinker, a paraffin modified with surface hydroxyl groups, a thickener and a solid. Paraffin with a certain hydroxyl content is introduced into these two components.
[0005] In order to reduce the bulk density, increase the thermal insulation and ensure water impermeability, there has also been a tendency to mix acrylate rubber asphalt into the cement, as is the case in patent document 3 (Slovak Utility Model No. 1692 U).
[0006] Building mixes containing cement and paper pulp are also known, as described in Slovak Utility Model No. 4239 U, which reduces production costs and reduces the weight of the product.
[0007] All of the above mentioned building mixtures, also based on cement, have their own specific preparation methods. Summary of the Invention [Problem to be solved by the invention]
[0008] The problem of cementitious mixtures, which has not yet been fully explored, is now calling for the design of such compositions and methods for their preparation that would also allow the ecological use and consumption of plastic waste. The result of this effort is the method for the preparation of cement-plastic mixtures described in the present invention. [Means for solving the problem]
[0009] The above-mentioned problems of cement mixtures are solved by the proposed cement-plastic mixture, which can be prepared in a specific manner according to the invention. For the purposes of the present invention, the term "cement-plastic mixture" can be understood as meaning a composition of the following composition: It can be a mixture preferably containing crushed plastics, which cannot be recycled further. It is possible to use all kinds of plastics, preferably in pieces of 1 mm to 20 mm, or even higher pieces, or chopped plastic strips, except for plastic pellets. It can also be cement, for example Portland grey or white, with a strength of 32.5 MPa to 52.5 MPa.
[0010] Portland grey and Portland white represent historical names for cements that may be used synonymously with hydraulic binders.
[0011] Finally, a superplasticizer, such as Melment, a superplasticizer based on melamine formaldehyde resin with a density of 20 / 40, and water may be used. According to the invention, the superplasticizer may be based on, or may contain, or may be produced from, melamine formaldehyde, and / or may meet the EN 934-2 2019+A1:2012 standard. The mixture further contains silica sand with a fragmentation of 0.3 mm to 2.0 mm and / or a set accelerator, such as Betodur A5, thus chloride-free concrete and / or synthetic fibers, such as ARC 42 / 30 mm, i.e. alkali-resistant (AR) glass fibers, which may be specifically designed for use in concrete and / or powder coatings and / or silica fume (microsilica) SiO2. These components of the mixture are represented by the following percentages for the individual components: 29% to 43% by weight of plastic waste; 56% to 69% by weight of cement, 1.0% to 2.0% by weight of superplasticizer and these components add up to 100% and represent the base mixture. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] 6.0% to 12% by weight of silica sand, and / or 0.4% to 0.9% by weight of a setting promoter, and / or 0.04% to 0.07% by weight of ARC synthetic fibers, and / or 0.02% to 0.08% by weight of paint, and / or 4.0% to 14.0% by weight of water, and / or 4.0% to 15.0% by weight of silica fume (microsilica) SiO2 At least one additional additive component comprising or consisting of is added to the base mixture.
[0013] The weight percentage of the additional component according to the present invention means the percentage which is the addition to the weight of the base mixture such that the final product has an additional weight of, for example, 6%, of Y weight units (e.g., kilograms) of the base mixture plus the additional component, resulting in a total mass Y*1.06 of the mass of the base mixture according to this example.
[0014] Thus, the weight percentage of the additional components is added to the mass of the base mix and calculated as if the base mix without the additional components was 100%, resulting in a total final product (cement-plastic mix) mass of 106% relative to the mass of the base mix in the above example.
[0015] The essence of the method for preparing a cement-plastic mixture according to the invention is In a first step, plastic waste, cement, water and optionally quartz sand are mixed in a mixing device, preferably at a temperature between 8°C and 25°C, preferably for 3 to 4 minutes; In the second step, at least one of the components, a flow agent, and / or a solidification promoter, and / or a synthetic fiber, and / or a paint, and / or optionally a microsilicate SiO2, is added and mixed, preferably for 6 to 10 minutes. The problem lies in the fact that...
[0016] The result of the mix is a high strength cement-plastic mixture with a self-leveling density.
[0017] The advantages of the method for preparing a cement-plastic mixture according to the invention are evident from its external effects. The effect and novelty lies in the unique composition of the mixture being mixed in a unique way with a precisely defined order of addition of the components of the mixture and / or time intervals of mixing.
[0018] From this cement-plastic mixture according to the invention it is possible to produce garden furniture, for example benches, flower pots, waste baskets, tables, large-format paving, facade elements, as well as cast pre-manufactured parts, which can be cut, sanded, sandblasted, impregnated and also machined with chipping or non-chipping techniques.
[0019] It is understood that the particular embodiments of the method for preparing a cement-plastic mixture according to the present invention are presented for the purpose of illustrating the solution, and not as a limitation of the solution. Those skilled in the art will find or be able to ascertain using no more than routine experimentation many equivalents to the specific embodiments of the method for preparing a cement-plastic mixture according to the present invention. Such equivalents will also fall within the scope of the present claims.
[0020] Optimal mixing of the individual components of a cement-plastic mixture is not a problem for a person skilled in the art, so these features have not been treated in detail. EXAMPLES
[0021] In this example of a specific embodiment of the present invention, a method for preparing a cement-plastic mixture according to the present invention is described. 29% to 43% by weight of plastic waste; 56% to 69% by weight of cement, 1.0% to 2.0% by weight of superplasticizer A cement-plastic mixture is prepared.
[0022] In addition, the weight of the base mixture is 4.0% to 14.0% by weight of water, and / or 6.0% to 12% by weight of silica sand, and / or 0.4% to 0.9% by weight of a setting promoter, and / or 0.04% to 0.07% by weight of ARC synthetic fibers, and / or 0.02% to 0.08% by weight of paint, and / or 4.0% to 15% by weight of silica fume (microsilica) SiO2 At least one additional component may be added, comprising or consisting of:
[0023] The cement-plastic mixture of this composition is In a first step, plastic waste, cement, water and optionally quartz sand are mixed in a mixing device, preferably at a temperature between 8°C and 25°C, preferably for 3 minutes; In the second step, at least one of the components, a flow agent, and / or a solidification promoter, and / or a synthetic fiber, and / or a paint, and / or a silica fume (microsilica) SiO2, is added and mixed for preferably 9 minutes. It is prepared by
[0024] The result of the mix is a high strength cement-plastic mixture with a self-leveling density. [Industrial Applicability]
[0025] The process for preparing a cement-plastic mixture according to the invention is intended for the construction and masonry sector. [Prior art documents] [Patent documents]
[0026] [Patent Document 1] Russian Patent No. 2739910 C1 [Patent Document 2] Chinese Patent No. 112063160 A Specification [Patent Document 3] Slovak Utility Model No. 1692 U Specification [Patent Document 4] Slovak Utility Model No. 4239 U Specification
Claims
1. A method for preparing a cement-plastic mixture, the cement-plastic mixture comprising the base mixture of plastic scrap, cement and a superplasticizer in the following percentage ranges, totaling 100% by weight of the base mixture: In a first step, 29% to 43% by weight of plastic scrap; 56% to 69% by weight of cement; 4.0% to 14.0% by weight of water; is mixed in a mixing device, preferably at a temperature between 8° C. and 25° C., preferably for 3 to 4 minutes, In a second step, 1.0% to 2.0% by weight of a flow agent; At least one additional component; is added, said additional component being 0.4% to 0.9% by weight of a setting promoter; 0.04% to 0.07% by weight of ARC synthetic fibers; 0.02% to 0.08% by weight of paint; all components are mixed preferably for 6 to 10 minutes; 11. A method of making a cement-plastic mixture, characterized in that said water and said additional components are provided in the aforementioned percentages in addition to the weight of said base mixture.
2. The method for preparing a cement-plastic mixture according to claim 1, characterized in that in the first step, an additional component of 6.0% to 12% by weight of silica sand with a fragmentation of 0.3 to 2.0 mm is included in the mixing process.
3. In the second step, 4.0% to 15% by weight of an additional component, silica fume (microsilica) SiO 2 2. The method for preparing a cement-plastic mixture according to claim 1, characterized in that the mixing process includes:
Citation Information
Patent Citations
Method of manufacturing molded boards
JP1977114618A
Plastic-mixed lightweight cement product
JP1994321601A
Plastic-containing cement hardened body and its production
JP2000203919A
Extruded plastic aggregate for concrete
JP2018504345A
Structural lightweight concrete comprising waste plastics