Wiring board

The wiring board design addresses low adhesion issues by using a copper alloy sputtered film for via conductors, enhancing connection reliability and signal transmission in high-density circuits.

JP2024157951AInactive Publication Date: 2024-11-08IBIDEN CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023072650
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-26
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The adhesion between the alloy layer and the electroless copper plating film layer in existing printed wiring boards is relatively low, leading to undesirable connection reliability of via holes and conductor circuits.

Method used

A wiring board design with alternating layers of insulating and conductor layers, featuring a first build-up portion with fine wiring and a second build-up portion with wider wiring, utilizing a sputtered film layer of copper alloy for the via conductor, which enhances adhesion and connection reliability.

Benefits of technology

The design provides improved adhesion and connection reliability between via conductors and conductor layers, allowing for high-density circuit wiring with enhanced signal transmission and mechanical stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024157951000001_ABST
    Figure 2024157951000001_ABST
Patent Text Reader

Abstract

To provide a wiring board with sufficient connection reliability.SOLUTION: A wiring board of an embodiment includes: a first build-up part including a first insulation layer 11, a first conductor layer 12, and a first veer conductor 13 filling a first veer opening 11a; and a second build-up part including a second insulation layer and a second conductor layer. A wiring width and an inter-wiring distance of wiring included in the first conductor layer 12 are smaller than a wiring width and an inter-wiring distance of wiring included in the second conductor layer. The first conductive layer 12 and the first veer conductor 13 each comprise a first layer 12a and a second layer 12b. The first layer 12 has: a lower layer 12aa contacting with a surface of the first insulation layer 11 and an internal surface and a bottom surface of the first veer opening 11a; and an upper layer 12ab covering the lower layer 12aa. The lower layer 12aa is a sputtering film made of an alloy containing copper, aluminum, and specific elements. The upper layer 12ab is a sputtering film made of copper.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wiring board. [Background technology]

[0002] Patent Document 1 discloses a printed wiring board including a conductor layer, a resin insulating layer covering the conductor layer, a conductor circuit formed on the resin insulating layer, and a via hole penetrating the resin insulating layer to connect the conductor circuit and the conductor layer. The conductor circuit and the via hole include a layer including an alloy layer and an electroless copper plating film in contact with the resin insulating layer, and a layer made of an electrolytic copper plating film formed on the electroless copper plating film. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2000-124602 A Summary of the Invention [Problem to be solved by the invention]

[0004] In the printed wiring board disclosed in Patent Document 1, it is believed that the adhesion between the alloy layer and the electroless copper plating film layer may be relatively low, and the connection reliability of the via holes and conductor circuits may be undesirable. [Means for solving the problem]

[0005] The wiring board of the present invention has a first surface and a second surface opposite to the first surface, and includes a first build-up portion including a first insulating layer and a first conductor layer that are alternately stacked, a first via opening that penetrates the first insulating layer and a first via conductor that fills the first via opening, and a second build-up portion including a second insulating layer and a second conductor layer that are alternately stacked. the first build-up section is stacked on top of the second build-up section and is located closer to the first surface than the second build-up section; a minimum wiring width of the wiring included in the first conductor layer is smaller than a minimum wiring width of the wiring included in the second conductor layer; a minimum inter-wiring distance of the wiring included in the first conductor layer is smaller than a minimum inter-wiring distance of the wiring included in the second conductor layer; the first conductor layer and the first via conductor include a first layer covering a surface of the first insulating layer and an inner wall surface and a bottom surface of the first via opening, and a second layer on the first layer; the first layer has a lower layer in contact with the surface of the first insulating layer and the inner wall surface and a bottom surface of the first via opening, and an upper layer covering the lower layer; the lower layer is a sputtered film formed of an alloy containing copper, aluminum, and a specific element, the specific element being at least one of nickel, zinc, gallium, silicon, and magnesium; and the upper layer is a sputtered film formed of copper.

[0006] According to an embodiment of the present invention, the upper and lower layers are sputtered films, and a wiring board can be provided in which the upper and lower layers are relatively strongly adhered to each other and the connection reliability between the first via conductors and the first conductor layer is relatively good. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a cross-sectional view showing an example of a wiring board according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a partially enlarged view of FIG. 1 showing an example of a wiring board according to an embodiment of the present invention. [Figure 3A] 1A to 1C are diagrams showing an example of a method for manufacturing a wiring board according to an embodiment of the present invention; [Figure 3B] 1A to 1C are diagrams showing an example of a method for manufacturing a wiring board according to an embodiment of the present invention; [Figure 3C]1A to 1C are diagrams showing an example of a method for manufacturing a wiring board according to an embodiment of the present invention; [Figure 3D] 1A to 1C are diagrams showing an example of a method for manufacturing a wiring board according to an embodiment of the present invention; [Figure 3E] 1A to 1C are diagrams showing an example of a method for manufacturing a wiring board according to an embodiment of the present invention; [Figure 3F] 1A to 1C are diagrams showing an example of a method for manufacturing a wiring board according to an embodiment of the present invention; [Figure 3G] 1A to 1C are diagrams showing an example of a method for manufacturing a wiring board according to an embodiment of the present invention; [Figure 3H] 1A to 1C are diagrams showing an example of a method for manufacturing a wiring board according to an embodiment of the present invention; [Figure 3I] 1A to 1C are diagrams showing an example of a method for manufacturing a wiring board according to an embodiment of the present invention; [Figure 3J] 1A to 1C are diagrams showing an example of a method for manufacturing a wiring board according to an embodiment of the present invention; [Figure 3K] 1A to 1C are diagrams showing an example of a method for manufacturing a wiring board according to an embodiment of the present invention; [Figure 3L] 1A to 1C are diagrams showing an example of a method for manufacturing a wiring board according to an embodiment of the present invention; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] A wiring board according to an embodiment will be described with reference to the drawings. FIG. 1 is a cross-sectional view showing a wiring board 1, which is an example of a wiring board according to an embodiment. Note that the wiring board 1 is merely an example of the wiring board according to this embodiment. The laminated structure of the wiring board according to this embodiment and the number of conductor layers and insulating layers are not limited to the laminated structure of the wiring board 1 shown in FIG. 1 and the number of conductor layers and insulating layers included in the wiring board 1. In addition, the drawings referred to are not intended to show the exact ratio of each component, but are drawn to make the features of the present invention easy to understand.

[0009] The wiring board 1 of the embodiment has a laminated structure including a first buildup section 10 and a second buildup section 20, each of which is composed of a conductor layer and an insulating layer that are alternately laminated. The first buildup section 10 has two surfaces that are perpendicular to its thickness direction (lamination direction), namely, one surface 10F and the other surface 10B opposite to the one surface 10F. The second buildup section 20 has two surfaces that are perpendicular to its thickness direction (lamination direction), namely, one surface 20F and the other surface 20B opposite to the one surface 20F. The wiring board 1 has two surfaces that are perpendicular to its thickness direction (first surface 1F and second surface 1B opposite to the first surface 1F). The wiring board 1 of the embodiment is preferably a coreless wiring board that does not include a core layer.

[0010] In the example shown in FIG. 1, the wiring board 1 further includes a third buildup section 30 composed of an insulating layer and a conductor layer on the side of the second buildup section 20 opposite to the first buildup section 10 side. The third buildup section 30 has two surfaces perpendicular to its thickness direction (stacking direction), namely, one side 30F and the other side 30B opposite to the one side 30F. In the example shown, the one side 10F of the first buildup section 10 constitutes the first side 1F, and the other side 30B of the third buildup section 30 constitutes the second side 1B. If the wiring board 1 does not have the third buildup section 30, the second side 1B may be constituted by the other side 20B of the second buildup section 20.

[0011] The first buildup section 10 includes relatively fine wiring and may have relatively dense circuit wiring. In the example of Fig. 1, the first buildup section 10 has insulating layers 11 (first insulating layers 11) and conductor layers 12 (first conductor layers 12) that are alternately laminated. The conductor layers 12 that face each other across the first insulating layer 11 are connected by via conductors 13 (first via conductors 13).

[0012] As shown in the figure, the via conductor 13 is formed in a tapered shape that reduces in diameter from the other surface 10B of the first buildup section 10 toward one surface 10F. Note that, although the term "reduced diameter" is used here for convenience, the shape of the via conductor 13 is not necessarily limited to a circular shape. "Reduced diameter" simply means that the diameter of the via conductor 13 (the distance between the longest two points on the periphery in a horizontal cross section) becomes smaller. Note that the via diameter of the via conductor 13 (the diameter of the contact surface of the via conductor 13 with the conductor layer 12 on the other surface 10B side) is about 10 μm.

[0013] One side 10F of the first buildup section 10 is composed of the surface of the first conductor layer 12 and the surface of the first insulating layer 11 exposed from the pattern of the first conductor layer 12. The first conductor layer 12 is patterned to have a predetermined conductor pattern. In the illustrated example, the first conductor layer 12 constituting the one side 10F is formed into a pattern having a plurality of conductor pads 12p. As illustrated, the conductor layer 12 constituting the other side 10B of the first buildup section 10 and in contact with the second buildup section 20 may have a thickness different from the other conductor layers 12 in the first buildup section 10.

[0014] The conductor pad 12p constitutes the outermost surface (first surface 1F) of the wiring board 1, and constitutes a component mounting surface to which external electronic components in the wiring board 1 can be connected. The component mounting surface of the wiring board 1 can have a plurality of component mounting regions. For example, as shown in the example of FIG. 1, two component mounting regions (EA1, EA2) can be formed corresponding to the regions to which electronic components E1, E2 are to be mounted. In mounting an external electronic component on the wiring board 1 of the illustrated example, the exposed conductor pad 12p can be electrically and mechanically connected to the external electronic component, for example, via a conductive bonding material (not shown) such as solder between the exposed conductor pad 12p and the connection pad of the external electronic component. At this time, a plating layer (not shown) including, for example, a nickel layer and a tin layer may be formed in advance on the surface of the conductor pad 12p. When a plurality of component mounting regions are formed, a conductor pattern may be formed in the conductor layer 12 in the first build-up section 10 such that the conductor pads 12p located in adjacent component mounting regions can be electrically connected to each other. When the wiring board 1 is used, the multiple electronic components mounted thereon can be electrically connected to each other through a short path via the first buildup portion 10. This may improve the degree of freedom in circuit design via the multiple electronic components that can be mounted on the wiring board 1 when it is used.

[0015] Examples of electronic components E1 and E2 that can be mounted on the wiring board 1 include active components such as semiconductor integrated circuit devices and transistors. Specifically, the electronic components E1 and E2 can be integrated circuits such as logic chips incorporating logic circuits, processing devices such as MPUs (Micro Processor Units), and memory elements such as HBMs (High Bandwidth Memory).

[0016] The first insulating layer 11 of the first buildup section 10 may be formed using an insulating resin such as an epoxy resin, a phenolic resin, etc. The first insulating layer 11 may include any of a fluororesin, a liquid crystal polymer (LCP), a polytetrafluoroethylene resin (PTFE), a polyester resin (PE), and a modified polyimide resin (MPI).

[0017] Examples of conductors constituting the first conductor layer 12 and the first via conductor 13 include copper and nickel, and preferably copper is used. In the example shown in Fig. 1, the first conductor layer 12 and the first via conductor 13 are shown as single layers, but the first conductor layer 12 and the via conductor 13 may be configured as a multilayer structure. For example, as will be described in detail later with reference to Fig. 2, the first conductor layer 12 and the first via conductor 13 may have a multilayer structure including a metal film layer (sputtered film layer) and a plating film layer (preferably an electrolytic plating film layer).

[0018] The first conductor layer 12 may have fine wiring FW, which is high-density wiring with a relatively small wiring width and inter-wiring distance (shortest distance between adjacent wirings). The fine wiring FW may have the smallest pattern width and inter-pattern distance among the wiring that constitutes the wiring board 1. In the illustrated example, of the multiple first conductor layers 12 included in the first buildup section 10, four conductor layers 12 have fine wiring FW, which is high-density wiring. However, the number of first conductor layers 12 with fine wiring FW that the first buildup section 10 has is not limited.

[0019] The fine wiring FW included in the first buildup section 10 has a wiring width and a wiring distance smaller than the wiring width and the wiring distance of the wiring included in the conductor layer 22 (second conductor layer 22) in the second buildup section 20 described later. Specifically, for example, the minimum wiring width of the fine wiring FW may be 3 μm or less, and the minimum wiring distance between adjacent wirings may be 3 μm or less. When the first buildup section 10 has the fine wiring FW, wiring having more appropriate characteristics corresponding to the electric signal that can be carried by the wiring in the first buildup section 10 may be provided. It is also considered that the density of the wiring in the first buildup section 10 may be improved, and the degree of freedom of wiring design may be improved. From the same viewpoint, the aspect ratio of the fine wiring FW is, for example, 2.0 or more and 4.0 or less.

[0020] The first conductor layer 12 including the micro wiring FW in the first buildup section 10 may have a thickness of, for example, 7 μm or less. The first insulating layer 11 in the first buildup section 10 has a thickness of, for example, about 7.5 to 10 μm. In this case, the first insulating layer 11 preferably does not include a core material (reinforcing material) made of glass fiber, aramid fiber, or the like.

[0021] As shown in FIG. 1, the first buildup section 10 is in contact with one surface 20F of the second buildup section 20. That is, the other surface 10B of the first buildup section 10, which is composed of the surfaces of the insulating layer 11 and the conductor layer 12 of the first buildup section 10, faces one surface 20F of the second buildup section 20. The second buildup section 20 has an insulating layer 21 (second insulating layer 21) and a conductor layer 22 (second conductor layer 22) that are alternately laminated, similar to the first buildup section 10. The second insulating layer 21 has a via conductor 23 that penetrates the second insulating layer 21. Each conductor layer 22 is patterned to have a predetermined conductor pattern. As shown in FIG. 1, the second buildup section 20 does not include a core layer.

[0022] 1, in the wiring board 1, a third buildup section 30 may be further laminated on the other surface 20B side of the second buildup section 20. The other surface 20B configured by the surface of the second conductor layer 22 of the second buildup section 20 and the surface of the second insulating layer 21 exposed from the pattern of the second conductor layer 22 faces one surface 30F of the third buildup section 30. The third buildup section 30 includes an insulating layer 211 (third insulating layer 211) and a conductor layer 212 (third conductor layer 212). A via conductor 33 is formed in the insulating layer 211 to penetrate the insulating layer 211 and connect the conductor layer 212 to the conductor layer 22 configuring the other surface 20B of the second buildup section 20.

[0023] 1, the third buildup section 30 further includes a solder resist layer 31 that covers the surfaces of the insulating layer 211 and the conductor layer 212. The solder resist layer 31 is formed using, for example, a photosensitive polyimide resin or an epoxy resin. An opening 31a is formed in the solder resist layer 31, and a conductor pad 32p of the conductor layer 212 is exposed from the opening 31a.

[0024] The insulating layer 21 constituting the second buildup section 20 may be formed using an insulating resin, similar to the insulating layer 11. The insulating layers 11, 21 may each contain the same insulating resin within each buildup section, or may contain different insulating resins. Each insulating layer 21 may contain a core material (reinforcing material) made of glass fiber or aramid fiber. In the illustrated example, the insulating layer 211 of the third buildup section 30 contains a core material 21b made of glass fiber. Each insulating layer 11, 21, 211 may further contain silica (SiO 2 The filler may contain inorganic particles such as fine particles of carbide, alumina, or mullite.

[0025] The conductor layer 22 of the second buildup section 20 and the conductor layer 212 of the third buildup section 30 and the via conductors 23, 33 may be formed using any metal such as copper or nickel, similar to the conductor layer 12 and the via conductor 13. As shown in Fig. 1, each of the via conductors 23 included in the second buildup section 20 and each of the via conductors 33 included in the third buildup section 30 are formed in a tapered shape that decreases in diameter from the second surface 1B side of the wiring board 1 toward the first surface 1F side, similar to the via conductors 13 of the first buildup section 10.

[0026] The wiring width and the distance between the wirings included in the second conductor layer 22 of the second buildup section 20 and the third conductor layer 212 of the third buildup section 30 are larger than the wiring width and the distance between the wirings included in the first conductor layer 12 of the first buildup section 10. The thickness of the second conductor layer 22 is formed to be thicker than the thickness of the first conductor layer 12, for example, about 10 μm or more. The second conductor layer 22 of the second buildup section 20 does not include a fine wiring pattern similar to the fine wiring FW of the first buildup section 10. For example, the minimum wiring width of the wiring included in the second conductor layer 22 is about 4 μm, and the minimum spacing between the wirings is about 6 μm. The aspect ratio of the wiring included in the second conductor layer 22 may be approximately equal to the aspect ratio of the fine wiring FW of the conductor layer 12, for example, about 2.0 or more and 4.0 or less. The via diameter of the via conductor 23 (the diameter of the contact surface of the via conductor 23 with the conductor layer 22 on the other surface 20B side) is about 50 μm.

[0027] In the illustrated wiring board 1, for example, both the insulating layer 211 and the conductor layer 212 in the third buildup section 30 are formed thicker than the insulating layer 21 and the conductor layer 22 in the second buildup section 20. For example, the thickness of the insulating layer 211 is about 100 μm or more and about 200 μm or less. The thickness of the conductor layer 212 is about 20 μm. The via diameter of the via conductor 33 formed in the insulating layer 211 (the diameter of the via conductor 33 at the contact surface with the conductor layer 212 on the other surface 30B side) is about 100 μm.

[0028] Like the first conductor layer 12 and the first via conductor 13, the conductor layers 22, 212 and the via conductors 23, 33 may be configured with a multilayer structure, for example, a multilayer structure including a metal film layer (preferably a sputtered film layer or an electroless plating film layer) and a plating film layer (preferably an electrolytic plating film layer). The second buildup section 20 and the third buildup section 30 do not include a fine wiring pattern such as the fine wiring FW of the first buildup section 10. In such a case, the metal film layer of the multilayer structure constituting the conductor layer 22 and the via conductors 23 and the conductor layer 212 and the via conductors 33 may be an electroless plating film layer formed by an electroless plating film, particularly an electroless copper plating film layer, and the plating film layer may be an electrolytic plating film layer formed by an electrolytic plating film, particularly an electrolytic copper plating film layer.

[0029] In addition, the second surface 1B of the wiring board 1 opposite to the component mounting surface of the wiring board 1 can be a connection surface to be connected to an external element when the wiring board 1 itself is mounted on an external element such as an external wiring board (for example, a motherboard of an electric device). The conductor pad 32p can be connected to an arbitrary board, electric component, or mechanical component.

[0030] Next, the first conductor layer 12 in the first buildup section 10 and the first via conductor 13 formed integrally with the first conductor layer 12 will be described in detail with reference to Fig. 2, which is an enlarged view of the region II surrounded by a dashed line in Fig. 1. Note that Fig. 2 is depicted with the top-bottom direction (thickness direction of the wiring board 1) inverted from Fig. 1A, with one surface 10F located on the lower side of the paper and the other surface 10B located on the upper side of the paper. Note that hereinafter, in the description of the wiring board 1 with reference to Fig. 2, the one surface 10F side will be referred to as the "bottom" or "lower side", and the other surface 10B side will be referred to as the "top" or "upper side".

[0031] As shown in FIG. 2, the first insulating layer 11 has a via opening 11a penetrating the first insulating layer 11. The first via conductor 13, which connects the first conductor layers 12 facing each other across the first insulating layer 11, is formed by filling the via opening 11a with a conductor. Specifically, as shown in the figure, the first layer 12a, which is a metal film layer formed by sputtering and which constitutes the first conductor layer 12, and the second layer 12b, which may be an electrolytic plating film layer, fill the via opening 11a to constitute the first via conductor 13. The first conductor layer 12 and the first via conductor 13 are integrally formed. The via opening 11a formed in the first insulating layer 11 is also referred to as the first via opening 11a.

[0032] The via opening 11a can be formed by, for example, irradiating a laser beam from the upper surface of the insulating layer 11 at a position where the first via conductor 13 of the first insulating layer 11 is to be formed. The diameter of the formed via opening 11a can be large on the side irradiated with the laser beam and small on the opposite side (the back side) of the side irradiated with the laser beam. Therefore, the via opening 11a can be formed so that the diameter is large on the upper side and small on the lower side. As shown in FIG. 2, the inner wall surface of the via opening 11a is inclined from the upper side to the lower side of the insulating layer 11. For example, the via opening 11a can be formed so that the aspect ratio of the via conductor 13 (height from the upper surface of the lower conductor layer 12 to which the via conductor 13 is connected to the lower surface of the upper conductor layer / diameter of the via conductor 13 on the upper surface of the lower conductor layer 12) is about 0.5 or more and about 1.0 or less.

[0033] As described later in the description of the manufacturing method of the wiring board, after the via opening 11a is perforated by irradiating the first insulating layer 11 with a laser beam, the inner wall of the via opening 11a is desmeared. The desmearing can be performed by a dry process. When the first insulating layer 11 contains inorganic particles, the inorganic particles exposed from the inner wall of the via opening 11a can be formed to have a flat portion along the inner wall surface due to the desmearing. That is, the entire inner wall surface of the via opening 11a can be formed relatively smoothly as a surface having a predetermined angle with respect to the bottom surface of the via opening 11a (the upper surface of the conductor layer 12). In other words, the inner wall surface of the first via opening 11a can be a surface in which the surface of the insulating resin and the flat portion of the inorganic particles are configured to be approximately flush with each other. Even when the first insulating layer 11 contains inorganic filler (inorganic particles), the inner wall surface of the via opening 11a can be formed to be relatively smooth with a small degree of roughness. Since the inner wall surface of the via opening 11a is formed relatively smoothly, the surface of the first via conductor 13 that contacts the inner wall surface of the via opening 11a can also be formed relatively smoothly. Therefore, the transmission loss of the signal transmitted through the first via conductor 13 can be suppressed to be relatively small.

[0034] The first layer 12a covers a part of the upper surface of the first insulating layer 11 and the entire inner wall surface and bottom surface of the via opening 11a. The first layer 12a can function as a power supply layer when the second layer 12b is formed by electrolytic plating. The first layer 12a has a two-layer structure including a lower layer 12aa and an upper layer 12ab. The lower layer 12aa is a sputtered film layer of a copper alloy formed by sputtering using an alloy containing copper as a target. The upper layer 12ab is a sputtered film layer of copper formed by sputtering using copper as a target.

[0035] Specifically, the lower layer 12aa is a sputtered film layer formed of an alloy containing copper, aluminum, and a specific element, and the upper layer 12ab is a sputtered film layer formed of copper. Here, the "specific element" means any one of nickel, zinc, gallium, silicon, and magnesium. The first layer 12a covering the inner wall surface of the via opening 11a and the upper surface of the first insulating layer 11 has a structure including the lower layer 12aa and the upper layer 12ab, so that the adhesion between the inner wall surface of the via opening 11a and the upper surface of the first insulating layer 11 and the first layer 12a can be improved. In particular, when the lower layer 12aa is a sputtered film layer of a copper alloy as described above, the inner wall surface of the via opening 11a and the upper surface of the first insulating layer 11 can have relatively good adhesion to the lower layer 12aa.

[0036] More specifically, the copper content in the sputtered film layer constituting the lower layer 12aa is greater than 90 at%. The copper content in the sputtered film layer constituting the lower layer 12aa may be less than 99 at%. The aluminum content in the sputtered film layer constituting the lower layer 12aa is, for example, 1.0 at% or more and 15.0 at% or less. For example, the lower layer 12aa may be a sputtered film layer formed of an alloy containing copper, aluminum, and silicon. In this case, the silicon content in the alloy may be 0.5 at% or more and 10.0 at% or less. For example, the lower layer 12aa may further contain carbon in addition to copper, aluminum, and the specific element, and in this case, the carbon content may be 50 ppm or less. For example, the lower layer 12aa may further contain oxygen in addition to copper, aluminum, and the specific element, and in this case, the oxygen content may be 100 ppm or less. The copper content in the sputtered film layer constituting upper layer 12ab is greater than 99.9 at %. The copper content in the sputtered film layer constituting upper layer 12ab is preferably 99.95 at % or greater.

[0037] In the first layer 12a, the lower layer 12aa and the upper layer 12ab are configured as sputtered film layers formed in a vacuum. With this configuration, the lower layer 12aa and the upper layer 12ab can have relatively good adhesion. Specifically, since the lower layer 12aa and the upper layer 12ab are sputtered films formed in a vacuum, an oxide film is unlikely to be formed in the lower layer 12aa and the upper layer 12ab. Therefore, compared to the case of an electroless plating film formed in an oxygen-containing atmosphere, for example, the adhesion between the lower layer 12aa and the upper layer 12ab can be realized well. A wiring board having a first conductor layer 12 and a first via conductor 13 with high connection reliability can be provided.

[0038] The upper surface of the first conductor layer 12 may be a polished surface with relatively small roughness and high flatness. When the surface of the conductor layer 12 is a polished surface with relatively small roughness, good high-frequency transmission characteristics may be obtained in the first buildup section 10.

[0039] Next, with reference to FIGS. 3A to 3L, a method for manufacturing a wiring board according to an embodiment will be described, taking as an example the case where the wiring board 1 shown in FIG. 1 is manufactured. Each component formed in the manufacturing method described below may be formed using the material exemplified as the material of the corresponding component in the description of the wiring board 1 in FIG. 1, unless otherwise specified. Hereinafter, in the description of the manufacturing method of the wiring board 1, the side closer to the support substrate GS is referred to as the "bottom" or "lower side", and the side farther from the support substrate GS is referred to as the "upper" or "upper side". Therefore, the surface facing the support substrate GS side of each element constituting the wiring board 1 is referred to as the "lower surface", and the surface facing the opposite side to the support substrate GS is also referred to as the "upper surface". The wiring board 1 may be formed by manufacturing a first buildup section 10 on the support substrate GS, a second buildup section 20 on the first buildup section 10, and a third buildup section 30 on the second buildup section 20 (see FIG. 1).

[0040] First, as shown in Fig. 3A, a support substrate GS having a good surface flatness, such as a glass substrate, is prepared. Metal film layers 121 are formed on both surfaces of the support substrate GS via adhesive layers AL containing an azobenzene-based polymer adhesive that can be attached and detached by, for example, light irradiation. The metal film layer 121 is a metal film (preferably a copper film) layer formed by, for example, electroless plating or sputtering. The metal film layer 121 may be made of a relatively thin metal foil.

[0041] 3B, a conductor layer 12 having a plurality of conductor pads 12p including a metal film layer 121 and a plating film layer 122 is formed on the support substrate GS via an adhesive layer AL. In forming the conductor layer 12, for example, a plating resist is formed on the metal film layer 121, and openings corresponding to the formation areas of the pattern of the conductor pads 12p are formed in the plating resist by, for example, a photolithography technique. Next, a plating film layer 122 is formed in the openings by electrolytic plating using the metal film layer 121 as a seed layer. After forming the plating film layer 122, the plating resist is removed, and the metal film layer 121 exposed by removing the plating resist is etched to form the state shown in FIG. 3B.

[0042] Next, as shown in FIG. 3C, an insulating layer 11 is laminated to cover the conductor layer 12. For example, an insulating resin such as an epoxy resin or a phenol resin may be used as the insulating layer 11. Fluorine resin, liquid crystal polymer (LCP), fluoroethylene resin (PTFE), polyester resin (PE), or modified polyimide resin (MPI) may also be used. The insulating layer 11 may be formed by thermocompressing these resins formed into a film on the conductor layer 12. A protective film PF is formed on the insulating layer 11 to completely cover the upper surface of the insulating layer 11. The protective film PF is, for example, a film made of polyethylene terephthalate (PET). A release agent may be interposed between the protective film PF and the upper surface of the insulating layer 11.

[0043] Next, a via opening 11a is formed at a position in the insulating layer 11 where a via conductor 13 (see FIG. 1) is to be formed, for example, by irradiation with a carbon dioxide laser beam or an excimer laser beam. The via opening 11a is formed penetrating the protective film PF and the insulating layer 11. The via opening 11a may be formed in a shape that reduces in diameter from the upper surface of the insulating layer 11 toward the bottom surface (the upper surface of the conductor layer 12). After the via opening 11a is formed by the laser beam, the inner surface (bottom surface and inner wall surface) of the via opening 11a may be desmeared. The desmearing may be preferably performed by a dry desmearing using a plasma gas (including, for example, tetrafluoromethane). The desmearing may also be performed while protecting the surface of the insulating layer 11 with the protective film PF formed on the surface of the insulating layer 11. After the desmearing in the via opening 11a, the protective film PF is removed from the upper surface of the insulating layer 11.

[0044] When the first insulating layer 11 contains an inorganic filler, the filler particles exposed from the inner wall of the via opening 11a are formed to have a flat portion along the inner wall surface by the desmearing process. That is, the entire inner wall surface of the via opening 11a can be formed relatively smoothly as a surface having a predetermined angle with respect to the bottom surface of the via opening 11a (the upper surface of the conductor layer 12). Even when the first insulating layer 11 contains an inorganic filler, the inner wall surface of the via opening 11a can be formed relatively smoothly with less roughness.

[0045] 3C to 3L show a laminate formed on one surface of the support substrate GS, and laminates that may be formed on the opposite surface are omitted. However, the opposite surface may also have laminates in the same manner and number, or conductive layers and insulating layers in a manner and number different from those on the one surface, or such conductive layers and insulating layers may not be formed.

[0046] Next, as shown in FIG. 3D corresponding to the region D surrounded by the dashed line in FIG. 3C, the first layer 12a constituting the conductor layer 12 (see FIG. 3F) is formed by sputtering on the inner wall surface of the via opening 11a and on the upper surface of the insulating layer 11. Specifically, first, the lower layer 12aa is formed by sputtering on the upper surface of the insulating layer 11, on the inner wall surface of the via opening 11a, and on the upper surface of the conductor layer 12 constituting the bottom surface of the via opening 11a. The lower layer 12aa is formed by sputtering using an alloy containing copper, aluminum, and any one of the specific elements (nickel, zinc, gallium, silicon, magnesium) as a target. Then, the upper layer 12ab is formed by sputtering so as to cover the lower layer 12aa. The upper layer 12ab is formed by sputtering using copper as a target. The sputtering is performed in a vacuum.

[0047] Next, as shown in Fig. 3E, a plating resist R1 having an opening R11 corresponding to a conductor pattern to be formed is provided on the metal film (first layer) 12a. Note that in Figs. 3E to 3I, the first layer 12a of the two-layer structure shown in Fig. 3D is shown as a single layer for ease of viewing.

[0048] Next, the second layer 12b, which is an electrolytic plating film layer, is formed in the opening R11 of the plating resist R1 by electrolytic plating using the first layer 12a as a power supply layer. Next, the plating resist R1 is removed, and then the portion of the first layer 12a that is not covered by the second layer 12b is removed by etching or the like. As a result, as shown in FIG. 3F, a conductor layer 12 consisting of the first layer 12a and the second layer 12b and having a fine wiring FW is formed. In addition, the inside of the via opening 11a is completely filled with the second layer 12b, which is an electrolytic plating film, to form a via conductor 13.

[0049] Next, as shown in Figure 3G, a desired number of insulating layers 11 and conductor layers 12, as well as via conductors 13 penetrating each insulating layer, are formed on the conductor layer 12 and insulating layer 11 in a manner similar to the method for forming the insulating layer 11, conductor layer 12, and via conductors 13 described above.

[0050] 3H, an outermost insulating layer 11 among the insulating layers 11 of the first buildup section 10 (see FIG. 1) is formed on the upper side of the conductor layer 12. After that, a via opening 11a for forming the via conductor 13 (see FIG. 1) is formed by laser processing in the insulating layer 11 at a position corresponding to the location where the via conductor 13 (see FIG. 1) is to be formed.

[0051] 3I, the conductor layer 12 constituting the other surface 10B is formed simultaneously with the via conductor 13 filling the via opening 11a by using any conductor pattern forming method such as a semi-additive method. The formation of the first buildup portion 10 on the supporting substrate GS is then completed.

[0052] Next, as shown in Fig. 3J, a second buildup section 20 is formed on the conductor layers 12 and insulating layers 11 constituting the other surface 10B of the first buildup section 10. The insulating layers 21 can be formed by thermocompression bonding of a film-like resin. The conductor layers 22 can be formed by any method for forming a conductor pattern, such as a semi-additive method. A desired number of insulating layers 21 and conductor layers 22, as well as via conductors 23 penetrating each insulating layer 21, are formed. Note that in Figs. 3J to 3L, each conductor layer is shown as a single layer, similar to Fig. 1.

[0053] As shown in FIG. 3K, the third buildup section 30 is formed on the insulating layer 21 and the conductor layer 22 constituting the other surface 20B of the second buildup section 20. The insulating layer 211, the conductor layer 212, and the via conductor 33 penetrating the insulating layer 211 are formed by a method similar to the method for forming the insulating layer 21, the conductor layer 22, and the via conductor 23. As the insulating resin for forming the insulating layer 211, a prepreg containing an insulating resin such as an epoxy resin or a BT resin impregnated in a reinforcing material (core material) made of glass fiber may be used. Next, the solder resist layer 31 is formed by forming a photosensitive epoxy resin or polyimide resin layer on the surfaces of the insulating layer 211 and the conductor layer 212. Then, the openings 31a defining the conductor pads 32p are formed by photolithography.

[0054] Next, as shown in Fig. 3L, the support substrate GS is removed. The lower surface of the conductor pad 12p and the lower surface of the insulating layer 11 are exposed. In removing the support substrate GS, the adhesive layer AL is softened by, for example, irradiating it with laser light, and then the support substrate GS is peeled off from the conductor pad 12p and the insulating layer 11. Note that the adhesive layer AL that may remain on the surfaces of the conductor pad 12p and the insulating layer 11 can be removed by cleaning. The wiring substrate 1 shown in Fig. 1 is completed.

[0055] The wiring board of the embodiment is not limited to those having the structure illustrated in each drawing, and the structure, shape, and material illustrated in this specification. Each build-up portion included in the wiring board of the embodiment may have any number of insulating layers and conductor layers as described above. In addition, the manufacturing method of the wiring board of the embodiment is not limited to the method described with reference to Figures 3A to 3L, and the conditions and order thereof may be changed arbitrarily. A specific process may be omitted, or another process may be added. For example, a plating layer including a nickel layer and a tin layer may be formed on the surface of the conductor pad 12p exposed after removing the support substrate GS. [Explanation of symbols]

[0056] 1. Wiring board 10 First build-up section 20 Second Build-up Section 30 Third Build-up Section 11 Insulating layer (first insulating layer) 21 Insulating layer (second insulating layer) 211 Insulating layer (third insulating layer) 12 Conductive layer (first conductive layer) 22 Conductive layer (second conductive layer) 212 Conductor layer (third conductor layer) 13 Via conductor (first via conductor) 23 Via conductor 33 Via conductor 12a 1st layer 12b 2nd layer 12aa lower layer 12ab upper layer 12p contact pad 32p contact pad FW Fine wiring E1, E2 electronic components EA1, EA2 component mounting area 10F, 20F, 30F One side 10B, 20B, 30B other side 1F, 1st floor 1B 2nd side

Claims

1. a first surface and a second surface opposite the first surface; a first build-up section including a first insulating layer and a first conductor layer alternately stacked, a first via opening penetrating the first insulating layer, and a first via conductor filling the first via opening; a second buildup section including second insulating layers and second conductor layers alternately stacked; A wiring board comprising: the first buildup portion is laminated on the second buildup portion and is located closer to the first surface than the second buildup portion, a minimum value of the wiring width of the wiring included in the first conductor layer is smaller than a minimum value of the wiring width of the wiring included in the second conductor layer; a minimum value of the distance between the wirings included in the first conductor layer is smaller than a minimum value of the distance between the wirings included in the second conductor layer; the first conductor layer and the first via conductor include a first layer covering a surface of the first insulating layer and an inner wall surface and a bottom surface of the first via opening, and a second layer on the first layer; the first layer has a lower layer in contact with a surface of the first insulating layer and an inner wall surface and a bottom surface of the first via opening, and an upper layer covering the lower layer; the lower layer is a sputtered film formed of an alloy containing copper, aluminum, and a specific element, the specific element being at least one of nickel, zinc, gallium, silicon, and magnesium; The upper layer is a sputtered film formed of copper.

2. 2. The wiring board according to claim 1, wherein the specific element is silicon.

3. 3. The wiring board according to claim 2, wherein the silicon content in the alloy is 0.5 at % or more and 10.0 at % or less.

4. 2. The wiring board according to claim 1, wherein the aluminum content in the alloy is 1.0 at % or more and 15.0 at % or less.

5. 2. The wiring board according to claim 1, wherein the alloy further contains carbon.

6. 6. The wiring board according to claim 5, wherein the carbon content in the alloy is 50 ppm or less.

7. 2. The wiring board according to claim 1, wherein the alloy further contains oxygen.

8. 8. The wiring board according to claim 7, wherein the oxygen content in the alloy is 100 ppm or less.

9. 2. The wiring board according to claim 1, wherein the copper content of the lower layer is 90 at % or more.

10. 2. The wiring board according to claim 1, wherein the upper layer has a copper content of 99.9 at % or more.

11. 2. A wiring board according to claim 1, wherein the first insulating layer contains insulating resin and inorganic particles, and the inner wall surface of the first via opening is a surface in which the surface of the insulating resin and the flat portion of the inorganic particles are approximately flush with each other.

12. 2. The wiring board according to claim 1, wherein the minimum value of the wiring width of the wiring included in the first conductor layer is 3 [mu]m or less, and the minimum value of the distance between the wirings included in the first conductor layer is 3 [mu]m or less.

13. 2. The wiring board according to claim 1, wherein the aspect ratio of the wiring included in the first conductor layer is not less than 2.0 and not more than 4.

0.

14. 2. The wiring board according to claim 1, wherein the surface of the first conductor layer on the second surface side is a polished surface.

15. 2. The wiring board according to claim 1, further comprising a third buildup section on the second surface side of the second buildup section, the third buildup section including a third insulating layer and a third conductor layer.

16. 16. The wiring board according to claim 15, wherein the third insulating layer includes a core material.

17. 17. The wiring board according to claim 16, wherein the core material includes glass fiber.

18. 2. The wiring board according to claim 1, wherein the first via conductor has a shape whose diameter decreases from the second surface to the first surface.

Citation Information

Patent Citations

  • Printed wiring board

    JP2000124602A