Wiring board

A dual-density wiring board design with fine conductor layers and smooth insulating surfaces addresses the challenge of forming continuous seed layers on recessed surfaces, achieving high insulation and reduced short circuits for efficient signal transmission.

JP2024157988AInactive Publication Date: 2024-11-08IBIDEN CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023072725
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-26
Publication Date
2024-11-08
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The formation of recesses on the surface of interlayer insulating layers and via surfaces in printed wiring boards makes it difficult to create a continuous and uninterrupted seed layer, necessitating thick seed layers which in turn complicates the formation of fine wiring patterns with high insulation properties.

Method used

A wiring board design with two buildup sections, each having different wiring densities, where the first buildup section includes conductor layers with finer wiring and insulating layers containing inorganic particles partially and fully embedded in resin, ensuring a smooth surface for a thin seed layer formation, thereby preventing short circuits and enabling fine wiring.

Benefits of technology

The design allows for fine wiring without short circuits, providing high insulation properties and ease of manufacturing with reduced etching residue, resulting in a high-quality wiring board with low conductor resistance and minimal transmission loss.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024157988000001_ABST
    Figure 2024157988000001_ABST
Patent Text Reader

Abstract

To improve a quality of a wiring board containing a plurality of conductive layers having different wiring densities.SOLUTION: A wiring board 1 of an embodiment contains a first built-up part 10 and a second built-up part 20 that are laminated. A minimum width W1 of a wiring 12w contained in a conductive layer 12 of the first built-up part 10 is smaller than a minimum width W2 of a wiring 22w contained in a conductive layer 22a of the second built-up part 20, and a minimum interval G1 of both of the wirings 12w is smaller than a minimum interval G2 of both of the wirings 22w. An insulation layer 11 contains a resin 110 and an inorganic particle 5. The inorganic particle 5 contains: a first inorganic particle 51 partially embedded into the resin 110; and a second inorganic particle 52 wholly embedded into the resin 110. The first inorganic particle 51 is formed of a first part projected from the resin 110 and a second part embedded to the resin 110. A front surface 11a of the insulation layer 11 converted by the conductive layer 12 is formed of: a front surface 110a of the resin 110; and an exposure surface 51aa of the first part, exposed from the resin 110.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wiring board. [Background technology]

[0002] Patent Document 1 discloses a printed wiring board including an interlayer insulating layer using a mixture of a thermosetting resin and an inorganic filler, and a seed layer and a plating layer formed on the interlayer insulating layer. The surface of the interlayer insulating layer and the side and bottom surfaces of a via provided in the interlayer insulating layer have recesses formed by preferentially etching the inorganic filler. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent Publication No. 2021-19061 Summary of the Invention [Problem to be solved by the invention]

[0004] In the printed wiring board disclosed in Patent Document 1, a recess is formed on the surface of the interlayer insulating layer and the exposed surface in the via, so it is considered that it is difficult to form a continuous seed layer that is not interrupted in the recess. In order to form a continuous seed layer that completely covers the surface of the insulating layer including the recess and the exposed surface in the via, it is necessary to form a thick seed layer. However, if the seed layer is thick, it is difficult to provide a wiring pattern that is fine and has high insulation between adjacent patterns. [Means for solving the problem]

[0005] The wiring board of the present invention has a first surface and a second surface opposite to the first surface, and includes a first buildup section including laminated insulating layers and conductor layers, and a second buildup section including laminated insulating layers and conductor layers, the first buildup section is laminated on the first surface side of the second buildup section, the minimum width of the wiring included in the conductor layer of the first buildup section is smaller than the minimum width of the wiring included in the conductor layer of the second buildup section, the minimum interval between the wiring included in the conductor layer of the first buildup section is smaller than the minimum interval between the wiring included in the conductor layer of the second buildup section, the insulating layer of the first buildup section includes resin and inorganic particles, the inorganic particles include first inorganic particles partially embedded in the resin and second inorganic particles entirely embedded in the resin, the first inorganic particles are formed of a first portion protruding from the resin and a second portion embedded in the resin, and a surface of the insulating layer of the first buildup section covered with the conductor layer of the first buildup section is formed of a surface of the resin and an exposed surface of the first portion exposed from the resin.

[0006] According to an embodiment of the present invention, a wiring board including a plurality of conductor layers having different wiring densities can be provided with fine wiring that is less likely to cause short circuits between adjacent wirings. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a cross-sectional view showing an example of a wiring board according to an embodiment of the present invention. [Diagram 2] An enlarged view of part II in Figure 1. [Diagram 3] An enlarged view of part III in FIG. [Figure 4A] 1 is a cross-sectional view showing an example of a wiring substrate according to an embodiment in a manufacturing process; [Figure 4B] 1 is a cross-sectional view showing an example of a wiring substrate according to an embodiment in a manufacturing process; [Figure 4C] FIG. 4 is an enlarged view showing a partial cross section of an example of a wiring substrate according to an embodiment during a manufacturing process. [Figure 4D] FIG. 4 is an enlarged view showing a partial cross section of an example of a wiring substrate according to an embodiment during a manufacturing process. [Figure 4E] FIG. 4 is an enlarged view showing a partial cross section of an example of a wiring substrate according to an embodiment during a manufacturing process. [Figure 4F] FIG. 4 is an enlarged view showing a partial cross section of an example of a wiring substrate according to an embodiment during a manufacturing process. [Figure 4G] FIG. 4 is an enlarged view showing a partial cross section of an example of a wiring substrate according to an embodiment during a manufacturing process. [Figure 4H] FIG. 4 is an enlarged view showing a partial cross section of an example of a wiring substrate according to an embodiment during a manufacturing process. [Figure 4I] FIG. 4 is an enlarged view showing a partial cross section of an example of a wiring substrate according to an embodiment during a manufacturing process. [Figure 4J] 1 is a cross-sectional view showing an example of a wiring substrate according to an embodiment in a manufacturing process; [Figure 4K] 1 is a cross-sectional view showing an example of a wiring substrate according to an embodiment in a manufacturing process; [Figure 4L] 1 is a cross-sectional view showing an example of a wiring substrate according to an embodiment in a manufacturing process; [Figure 4M] 1 is a cross-sectional view showing an example of a wiring substrate according to an embodiment in a manufacturing process; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] <Structure of wiring board according to embodiment> A wiring board according to an embodiment will be described with reference to the drawings. FIG. 1 shows a cross-sectional view of a wiring board 1, which is an example of a wiring board according to an embodiment. FIG. 2 shows an enlarged view of part II in FIG. 1. The wiring board 1 is merely an example of the wiring board according to this embodiment. The number and thickness of each of the conductor layers and insulating layers in the wiring board according to this embodiment, and the conductor patterns included in each conductor layer are not limited to the number and thickness of each of the conductor layers and insulating layers included in the wiring board 1 of FIG. 1, and the conductor patterns. In addition, in each drawing referred to in the following description, a specific portion may be drawn enlarged so that the disclosed embodiment can be easily understood, and the components may not be drawn in exact proportion to each other in terms of size and length.

[0009] As shown in FIG. 1 and FIG. 2, the wiring board 1 has two surfaces (a first surface 1F and a second surface 1B opposite to the first surface 1F) perpendicular to the thickness direction of the wiring board 1. The wiring board 1 includes a first buildup section 10 and a second buildup section 20. The first buildup section 10 is laminated on the first surface 1F side of the second buildup section 20. The lamination direction of the first buildup section 10 and the second buildup section 20 is the thickness direction of the wiring board 1. The first buildup section 10 and the second buildup section 20 overlap each other entirely. The wiring board 1 of FIG. 1 further includes a third buildup section 30 laminated on the second surface 1B side of the wiring board 1 in the second buildup section 20, and a solder resist 40 covering the surface of the third buildup section 30. The wiring board of this embodiment may be a coreless wiring board that does not include a core layer, like the wiring board 1 of FIG. 1.

[0010] In the description of the wiring board 1 of this embodiment, the first surface 1F side of the wiring board 1 is also referred to as the "top" or "upper side", and the second surface 1B side of the wiring board 1 is also referred to as the "bottom" or "lower side". In addition, the surface of each component facing the first surface 1F side of the wiring board 1 is also referred to as the "top surface", and the surface facing the second surface 1B side of the wiring board 1 is also referred to as the "bottom surface".

[0011] The first buildup section 10 has a first surface 10F which is a surface common to the first surface 1F of the wiring board 1, and a second surface 10B which is a surface opposite to the first surface 10F. The first buildup section 10 includes conductor layers 12 (first conductor layers) and insulating layers 11 (first insulating layers) which are alternately laminated. Each conductor layer 12 is formed on the lower surface of the insulating layer 11 adjacent thereto above. The first buildup section 10 further includes a conductor layer 12a which is the conductor layer in the first buildup section 10 closest to the first surface 1F of the wiring board 1.

[0012] Conductive layer 12a is embedded in insulating layer 11 at the portion of first buildup section 10 closest to first surface 1F of wiring board 1, and has an upper surface exposed to first surface 1F. The exposed upper surface of conductor layer 12a and the upper surface of insulating layer 11 in which conductor layer 12a is embedded form the first surface 1F of wiring board 1.

[0013] The first surface 1F of the wiring board 1 includes one or more component regions (component region Ea1 and component region Ea2 in the example of FIG. 1) on which mounted components (component E1 and component E2 in the example of FIG. 1) are mounted when the wiring board 1 is used. The first surface 1F of the wiring board 1 can be a component mounting surface that is at least partially covered by mounted components such as component E1 and component E2 when the wiring board 1 is used.

[0014] Each of the conductor layers 12 and 12a includes an arbitrary conductor pattern. The conductor layer 12a constituting the component mounting surface in the first build-up section 10 includes a component mounting pad 12p made of a conductor pad. The component mounting pad 12p is embedded in the insulating layer 11 constituting the first surface 1F of the wiring board 1, and one surface of the component mounting pad 12p is exposed to the first surface 1F. The exposed surface of the component mounting pad 12p can be connected to an electrode of a mounted component by, for example, a conductive bonding material (not shown) such as solder. A surface treatment layer (not shown) made of a plating layer containing, for example, nickel, palladium, and gold may be formed on the exposed surface of the component mounting pad 12p.

[0015] Examples of the components E1 and E2 that can be mounted on the wiring board 1 include electronic components such as active components such as semiconductor integrated circuit devices and transistors. As some examples, the components E1 and E2 can be integrated circuit devices such as logic chips, processing devices such as MPUs (Micro Processor Units), and memory devices such as HBMs (High Bandwidth Memory).

[0016] The first buildup section 10 further includes via conductors 13 (first via conductors) that penetrate each insulating layer 11. The via conductors 13 are formed in openings 13a that penetrate each insulating layer 11. Each via conductor 13 connects the lower conductor layer 12 of each insulating layer 11 including the via conductor 13 to the upper conductor layer 12 or conductor layer 12a. Each via conductor 13 is formed integrally with the conductor layer 12 that is in contact with it at an end portion on the second surface 1B side of the wiring board 1.

[0017] The second buildup section 20 has a first surface 20F which is the surface on the first surface 1F side of the wiring board 1, and a second surface 20B which is the surface opposite to the first surface 20F. The first surface 20F of the second buildup section 20 faces the second surface 10B of the first buildup section 10. The second buildup section 20 includes conductive layers 22 and insulating layers 21 (second insulating layers) which are alternately stacked, and via conductors 23 (second via conductors) which penetrate each insulating layer 21. The second buildup section 20 further includes a conductive layer 22a (second conductor layer) which is the conductive layer closest to the first surface 20F of the second buildup section 20, and a via conductor 23a. The via conductor 23a is formed integrally with the conductive layer 22a, and penetrates the insulating layer 11 in the first buildup section 10 which is closest to the second buildup section 20. A first surface 20F of the second buildup section 20 is formed by the top surface of the insulating layer 21 that is located closest to the first buildup section 10 among the multiple insulating layers 21, and the top surface of the conductor layer 22a.

[0018] On the other hand, the second surface 20B of the second buildup section 20 is constituted by the lower surfaces of the insulating layer 21 and the conductor layer 22 which are closest to the second surface 1B of the wiring board 1 in the second buildup section 20. In the wiring board 1 of FIG. 1, the second surface 20B of the second buildup section 20 faces the surface (upper surface) of the third buildup section 30 facing the first surface 1F of the wiring board 1.

[0019] Each of the conductor layers 22 and 22a includes an arbitrary conductor pattern. Each of the conductor layers 22 and 22a is formed on the lower surface of the insulating layer 21 or insulating layer 11 adjacent thereto above. Each of the via conductors 23 connects the lower conductor layer 22 of the insulating layer 21 through which the via conductor 23 penetrates, to the upper conductor layer 22 or conductor layer 22a. The via conductor 23a connects the conductor layer 22a to the conductor layer 12 of the first buildup section 10.

[0020] The third buildup section 30 includes an insulating layer 31 (third insulating layer), a conductor layer 32 (third conductor layer), and a via conductor 33 (third via conductor), which are stacked together. The conductor layer 32 includes an arbitrary conductor pattern, such as a conductor pad 32p. The via conductor 33 connects the conductor layer 32 and the conductor layer 22 included in the second buildup section 20.

[0021] The solder resist 40 is formed on the surface of each of the insulating layer 31 and the conductor layer 32 on the second surface 1B side of the wiring board 1. An opening 41 is formed in the solder resist 40, and the conductor pad 32p is exposed in the opening 41. The solder resist 40 is formed using, for example, a photosensitive polyimide resin or an epoxy resin.

[0022] 1, second side 1B of wiring board 1 consists of the surface of solder resist 40 on the second side 1B side of wiring board 1 and the exposed surface of conductor layer 32 exposed from solder resist 40. However, the wiring board of this embodiment does not necessarily include third buildup portion 30 and / or solder resist 40. The second side of a wiring board in an embodiment that does not include third buildup portion 30 consists of second side 20B of second buildup portion 20, or solder resist formed on second side 20B of second buildup portion 20 and an exposed portion of second side 20B from the solder resist.

[0023] The second surface 1B of the wiring board 1 can be a connection surface to be connected to an external element when the wiring board 1 itself is mounted on an external element such as an external wiring board (for example, a motherboard of an electric device). In the example of Fig. 1, the conductor pad 32p of the third buildup section 30 can be connected to an arbitrary board, electric component, mechanical component, or the like.

[0024] The insulating layers 11, 21, and 31 may be formed using a thermosetting insulating resin such as an epoxy resin, a bismaleimide triazine resin (BT resin), and a phenol resin. The insulating layers 11, 21, and 31 may be formed using a thermoplastic insulating resin such as a fluororesin, a liquid crystal polymer (LCP), a fluoroethylene resin (PTFE), a polyester resin (PE), or a modified polyimide resin (MPI). The insulating layers 11, 21, and 31 may contain the same insulating resin or different insulating resins.

[0025] The insulating layers 11, 21, and 31 may contain a core material (reinforcing material) made of glass fiber or the like. In the example of FIG. 1, the insulating layer 31 contains a core material 31a. The core material 31a may impart appropriate rigidity to the wiring board 1. The core material 31a may be, for example, glass fiber or aramid fiber. On the other hand, each insulating layer that does not contain a core material such as glass fiber may facilitate the formation of fine wiring on its surface or increase adhesion with the conductor layer. In the example of FIG. 1, neither the insulating layer 11 nor the insulating layer 21 contains a core material.

[0026] Although omitted in FIG. 1, the insulating layers 11, 21, and 31 may further include inorganic particles added as a filler to the insulating resin constituting each of the insulating layers 11, 21, and 31. Each insulating layer containing inorganic particles is given, for example, a low thermal expansion coefficient and high thermal conductivity. In the wiring board 1 of this embodiment, as shown in FIG. 2, the insulating layer 11 of the first buildup section 10 contains a plurality of inorganic particles 5 and the insulating resin 110 such as the epoxy resin described above. The content of the inorganic particles 5 in the insulating layer 11 is, for example, 75 wt % or more. In the example of FIG. 2, the insulating layer 21 included in the second buildup section 20 contains inorganic particles 6. The inorganic particles 5 and the inorganic particles 6 are fine particles made of, for example, silica (SiO2), alumina, or mullite.

[0027] In the example of FIG. 2, the maximum particle size of the inorganic particles 5 is smaller than the maximum particle size of the inorganic particles 6. The "particle size" of each of the inorganic particles 5 and 6 is the longest distance between two points on the surface of each inorganic particle. For example, the maximum particle size of the inorganic particles 5 is 1 μm or less, and the average particle size of the inorganic particles 5 is 0.5 μm or less. On the other hand, the maximum particle size of the inorganic particles 6 is, for example, 4 μm or less. When the particle size of the inorganic particles 5 and 6 is small, short circuit defects due to leak paths along the inorganic particles are unlikely to occur even between wirings arranged at fine intervals in the conductor layer in contact with each insulating layer. In addition, it may be easy to form a fine via conductor. The first build-up section 10 including the inorganic particles 5 having a smaller particle size has good reliability regarding insulation between wirings and may include wirings arranged at a fine pitch.

[0028] The conductor layers 12, 12a and the via conductors 13, the conductor layers 22, 22a and the via conductors 23, 23a, and the conductor layer 32 and the via conductors 33 may be formed using any metal having suitable electrical conductivity, such as copper or nickel. Although each of these conductor layers and each of the via conductors is depicted as a single layer in Fig. 1, each of the conductor layers and each of the via conductors may have a multi-layer structure, such as the conductor layers 12, 22a and the via conductor 13 shown in Fig. 2.

[0029] In the example of FIG. 2, the conductor layer 12 (and the conductor layer 12a not shown in FIG. 2) and the via conductor 13 are formed of a first layer 12α located on the first surface 1F side (see FIG. 1) of the wiring board 1, and a second layer 12β formed on the surface (lower surface) of the first layer 12α on the second surface 1B side (see FIG. 1) of the wiring board 1. The second layer 12β may be, for example, an electrolytic plating film layer made of a metal film formed by electrolytic plating. The first layer 12α may be a seed layer that can be used as a power supply layer when the second layer 12β is formed by electrolytic plating. The thickness of the first layer 12α may be, for example, 0.2 μm or more and less than 0.5 μm. If the thickness of the first layer 12α is less than 0.5 μm, conductor residue is unlikely to occur during etching, and therefore short-circuit defects are unlikely to occur in the conductor layer 12.

[0030] Conductive layer 22a (and conductive layer 22 and via conductors 23, 23a not shown in FIG. 2) includes first layer 22α and second layer 22β formed on the lower surface of first layer 22α, which may be an electrolytic plating film layer. First layer 22α is used as a power supply layer when second layer 22β is formed. First layers 12α, 22α are made of, for example, a sputtering film or an electroless plating film. When first layers 12α, 22α are made of a sputtering film, good adhesion is obtained between each conductive layer and insulating layer 11 or insulating layer 21. When first layers 12α, 22α are made of a sputtering film, first layers 12α, 22α may each include, for example, a first film made of a copper alloy on the first surface 1F side of wiring board 1 and a second film made of approximately copper on the second surface 1B side, although not shown in the figure.

[0031] As an example, the first layer 12α of the conductor layer 12 included in the first buildup section 10 may be a sputtered film, and the first layers 22α of the conductor layers 22, 22a included in the second buildup section 20 may be electroless plated films. The adhesion strength between the insulating layer 11 and the conductor layer 12 in the first buildup section 10 may be sufficiently high. Also, the conductor layers 22, 22a may be easily formed in the formation of the second buildup section 20.

[0032] 2, the conductor layer 32 and the via conductor 33 may each have a layer made of a material similar to the first layer 22α and a layer made of a material similar to the second layer 22β of the conductor layer 22. The conductor layer 32 may further include a layer made of a metal foil located closer to the insulating layer 31 than these two layers.

[0033] As shown in FIG. 1, the via conductors 13, 23, 23a, and 33 all have a tapered shape that narrows from the second surface 1B to the first surface 1F of the wiring board 1. Because the via conductors 13, 23, 23a, and 33 have such a tapered shape, the conductor layer on the first surface 1F side, which may be a component mounting surface, may include wiring arranged at a finer pitch. The shape of the horizontal cross section (cross section perpendicular to the thickness direction of the wiring board 1) of each of the via conductors 13, 23, 23a, and 33 is not necessarily limited to a circle. "Diameter narrowing" simply means that the distance between the longest two points on the circumference of each via conductor in the horizontal cross section (hereinafter, this distance is also referred to as the "width" of each via conductor) becomes smaller.

[0034] The via conductors 13 included in the first buildup section 10 have an aspect ratio (distance between the upper surface of the lower conductor layer 12 to which the via conductor 13 is connected and the lower surface of the upper conductor layer 12 or conductor layer 12a / width of the via conductor 13 on the upper surface of the lower conductor layer 12) of, for example, 0.5 or more and 1.0 or less. The first buildup section 10 may include via conductors 13 that include wiring arranged at a fine pitch and have low conductor resistance that is unlikely to break. The width of each of the via conductors 13 on the upper surface of the lower conductor layer 12 is, for example, about 10 μm. On the other hand, the width of each of the via conductors 23 in the second buildup section 20 on the upper surface of the lower conductor layer 22 is about 50 μm.

[0035] As described above, the conductor layer included in each buildup section may include any conductor pattern. As shown in FIG. 2, the conductor layer 12 includes a wiring 12w as a conductor pattern, and the conductor layer 22a includes a wiring 22w. The wiring 12w has a wiring width W1 as its width. The wiring 12w has a wiring interval G1 as the interval between adjacent wirings 12w. The wiring width W1 is the minimum wiring width of the wiring included in the conductor layer 12a or the conductor layer 12 of the first buildup section 10. The wiring interval G1 is the minimum interval of the interval between the wirings included in the conductor layer 12a or the conductor layer 12 of the first buildup section 10.

[0036] On the other hand, the wiring 22w has a wiring width W2 as its width. The wiring 22w has a wiring interval G2 as the interval between adjacent wirings 22w. The wiring width W2 is the minimum width among the wiring widths of the wirings included in the conductor layer 22a or the conductor layer 22 of the second buildup section 20. Furthermore, the wiring interval G2 is the minimum interval among the intervals between the wirings included in the conductor layer 22a or the conductor layer 22 of the second buildup section 20. As shown in FIG. 2, the wiring width W1 and the wiring width W2 are different. Furthermore, the wiring interval G1 and the wiring interval G2 are different.

[0037] In this way, in the wiring board of the embodiment, the conductor layer 12 that constitutes the first buildup section 10 together with the insulating layer 11 can be a conductor layer that includes wiring arranged according to a wiring rule different from the wiring of the conductor layer included in the second buildup section 20.

[0038] In the wiring board 1 of the embodiment, the first buildup section 10 may be a laminate of such a conductor layer 12 and an insulating layer 11. The wiring board 1 of the embodiment, which includes the second buildup section 20 and the first buildup section 10 including a conductor layer different from the conductor layer of the second buildup section 20 in terms of the minimum wiring width and minimum wiring spacing, may include fine wiring only in the necessary conductor layer. Furthermore, the wiring board 1 of the embodiment may include, as another conductor layer, a conductor layer including easily formable wiring having a wider width and spacing.

[0039] In the wiring board 1 of the present embodiment, the minimum width of the wiring included in the conductor layer 12 or conductor layer 12a of the first buildup section 10 (wiring width W1 in the example of FIG. 2) is smaller than the minimum width of the wiring included in the conductor layer 22a or conductor layer 22 of the second buildup section 20 (wiring width W2 in the example of FIG. 2). Furthermore, in the wiring board 1 of the embodiment, the minimum interval between the wiring included in the conductor layer 12a or conductor layer 12 of the first buildup section 10 (wiring interval G1 in the example of FIG. 2) is smaller than the minimum interval between the wiring included in the conductor layer 22 or conductor layer 22a of the second buildup section 20 (wiring interval G2 in the example of FIG. 2). As an example, the minimum width of the wiring included in the conductor layer 12 can be 1 μm or more and 3 μm or less, and the minimum interval between the wiring included in the conductor layer 12 can be 1 μm or more and 3 μm or less. Because first buildup section 10 is configured with conductor layer 12 including wiring arranged at such a fine pitch, wiring having more suitable characteristics may be provided in response to the electrical signals carried by the wiring in first buildup section 10. Also, the density of the wiring in first buildup section 10 may be high, and therefore a small wiring board 1 may be obtained.

[0040] The minimum width of wiring included in conductor layers such as conductor layer 22a and conductor layer 22 constituting second buildup section 20 may be, for example, about 4 μm, and the minimum spacing may be, for example, about 6 μm. The conductor layers of second buildup section 20 may be easily formed.

[0041] In the wiring board 1 of this embodiment, the aspect ratio of each wiring such as the wiring 12w included in the conductor layer 12 of the first buildup section 10 can be, for example, 2.0 or more and 4.0 or less. Wires with such an aspect ratio can have low conductor resistance for a small wiring width, and can therefore serve as a signal transmission path with low insertion loss. For example, signals can be transmitted between components mounted on the wiring board 1 with little transmission loss. In addition, a desired characteristic impedance can be easily obtained, and therefore the insertion loss can be further reduced.

[0042] In the example of FIG. 1 and FIG. 2, the thickness of the conductor layer 12 is different from the thickness of the conductor layer 22 and the conductor layer 22a. The thickness of the insulating layer 11 is different from the thickness of the insulating layer 21. Thus, in this embodiment, the first buildup section 10 may be a laminate of an insulating layer and a conductor layer having a thickness different from that of the conductor layer of the second buildup section 20. Also, in this embodiment, the first buildup section 10 may be a laminate of an insulating layer and a conductor layer having a thickness different from that of the insulating layer of the second buildup section 20. Furthermore, as described above, the particle size of the inorganic particles 5 contained in the insulating layer 11 is different from the particle size of the inorganic particles 6 contained in the insulating layer 21. Therefore, in this embodiment, the first buildup section 10 may be a laminate of an insulating layer made of a material different from that of the insulating layer of the second buildup section 20 and a conductor layer.

[0043] In the wiring board 1, the thickness of a conductor layer included in the first buildup section 10, such as the conductor layer 12, may be, for example, 4 μm or more and 7 μm or less. This is less likely to leave etching residue during manufacturing, and may be advantageous for arranging wiring 12w and the like arranged at fine intervals. The thickness of the insulating layer 11 included in the first buildup section 10 may be, for example, about 7.5 to 10 μm. On the other hand, the thickness of a conductor layer included in the second buildup section 20, such as the conductor layers 22 and 22a, may be 10 μm or more and less than 20 μm. Furthermore, the thickness of an insulating layer included in the second buildup section 20, such as the insulating layer 21, may be 20 μm or more and less than 100 μm.

[0044] The surface of the conductor layer 12 of the first buildup section 10 on the second buildup section 20 side (the second surface 1B side of the wiring board 1) may be a polished surface having a polished finish. In the example of FIG. 1, the surface on the second surface 1B side of all four conductor layers 12 is a polished surface. The polished surface may have a surface roughness lower than that of a plating film formed as is by metal deposition, for example. Therefore, it is considered that the wiring included in each conductor layer 12 having a polished surface is less likely to experience a decrease in signal transmission characteristics or an increase in voltage drop. For example, the polished surface that each conductor layer 12 has as the surface on the second surface 1B side may have an arithmetic mean roughness of 0.3 μm or less. When such a surface roughness is obtained, the above-mentioned effects on transmission characteristics may be obtained.

[0045] Although not shown, in the wiring board 1 of FIG. 1, the wiring width of the wiring of the conductor layer 32 included in the third buildup section 30 is larger than the wiring width of the wiring included in the second buildup section 20, such as the wiring 22w. The wiring interval of the wiring of the conductor layer 32 is larger than the wiring interval of the wiring included in the second buildup section 20. The insulating layer 31 and the conductor layer 32 in the third buildup section 30 are both formed thicker than the insulating layer 21 and the conductor layers 22, 22a in the second buildup section 20. For example, the thickness of the insulating layer 31 is about 100 μm or more and 200 μm or less. The thickness of the conductor layer 32 is about 20 μm. The width of the via conductor 33 formed in the insulating layer 31 (the width at the top surface of the conductor layer 32) is about 100 μm.

[0046] FIG. 3 shows an enlarged view of part III in FIG. 2. Referring to FIG. 3 in addition to FIG. 2, the resin 110 and the inorganic particles 5 constituting each insulating layer 11 of the first build-up section 10 are further described. As shown in FIG. 2 and FIG. 3, the inorganic particles 5 in the wiring board 1 of this embodiment include first inorganic particles 51 and second inorganic particles 52. The first inorganic particles 51 and the second inorganic particles 52 are each spherical in shape. The first inorganic particles 51 are inorganic particles that are partially embedded in the resin 110 corresponding to each inorganic particle 5 among the inorganic particles 5. On the other hand, the second inorganic particles 52 are inorganic particles that are entirely embedded in the resin 110 corresponding to each inorganic particle 5 among the inorganic particles 5. Note that the "corresponding resin 110" refers to the resin 110 constituting the insulating layer 11 that contains most of the inorganic particles 5 of interest.

[0047] 3, the first inorganic particles 51 are formed of first portions 51a protruding from the corresponding resin 110 and second portions 51b embedded in the corresponding resin 110. A surface 11a (for example, a lower surface that is a surface of the insulating layer 11 on the second buildup section 20 side) of the insulating layer 11 covered with the conductor layer 12 is formed of a surface 110a of the resin 110 (for example, a lower surface of the resin 110 facing the second buildup section 20 side) and an exposed surface 51aa of the first portions 51a of the first inorganic particles 51 exposed from the surface 110a of the resin 110.

[0048] When the first portion 51a protrudes from the resin 110, the surface 11a of the insulating layer 11 has slight irregularities. However, the surface 110a of the resin 110 is not intentionally roughened in the manufacturing process of the wiring board 1, as described below. Therefore, the surface 11a of the insulating layer 11 has almost no recesses. The arithmetic mean roughness (Ra) of the surface 11a of the insulating layer 11 (the surface on the second buildup section 20 side) is, for example, less than 0.08 μm. The arithmetic mean roughness (Ra) of the surface 11a is preferably 0.05 μm or less, and more preferably 0.03 μm or less.

[0049] In the example of Fig. 3, the first inorganic particles 51 overlapping the conductive pattern of the conductive layer 12 are covered by the first layer 12α of the conductive layer 12 and are not exposed from the first layer 12α. Therefore, the second layer 12β without pinholes, bubbles, etc. can be formed by electrolytic plating. Similarly, in the example of Fig. 2, the first inorganic particles 51 overlapping the conductive pattern of the conductive layer 22a are covered by the first layer 22α of the conductive layer 22a and are not exposed from the first layer 22α. Therefore, the second layer 22β without pinholes, bubbles, etc. can be formed by electrolytic plating.

[0050] The ratio R of the volume of the first portion 51a of the first inorganic particle 51 to the volume of the first inorganic particle 51 (volume of the first portion 51a / volume of the entire first inorganic particle 51) may be, for example, greater than 0 and equal to or less than 0.4. The ratio R is preferably equal to or less than 0.2. The ratio R is more preferably equal to or less than 0.1. The ratio R is most preferably equal to or less than 0.05. The ratio R can be calculated, for example, using a cross-sectional view such as that shown in FIG. 3 obtained by cutting the wiring board 1 on a plane perpendicular to the surface 11a of the insulating layer 11. That is, the cross-sectional area 51aS of the first portion 51a and the cross-sectional area 51S of the entire first inorganic particle 51 are obtained using the cross-sectional view such as that shown in FIG. 3. The ratio R may be represented by the ratio of the cross-sectional area 51aS to the cross-sectional area 51S (cross-sectional area 51aS / cross-sectional area 51S). If the first portion 51a is at least half or less of the first inorganic particles 51, the area ratio of the first portion 51a to the entire first inorganic particles 51 cannot be smaller than the volume ratio. In other words, if the area ratio is 0.4 or less, the volume ratio is also 0.4 or less. Therefore, in the evaluation of the volume ratio R, the ratio R may be represented by the area ratio.

[0051] As an example, when the ratio R is evaluated, 50 first inorganic particles 51 are observed, and if the ratio R for all of the first inorganic particles 51 is greater than 0 and less than or equal to 0.4, the ratio R in the wiring board being evaluated is determined to be greater than 0 and less than or equal to 0.4.

[0052] As shown in FIG. 3, the inorganic particles 5 further include third inorganic particles 53 that form the inner wall surface 13b of the opening 13a penetrating the insulating layer 11. The shape of the third inorganic particles 53 is a spherical decapitated shape. The shape of the third inorganic particles 53 is obtained by cutting a sphere with a plane. The shape of the third inorganic particles 53 is obtained by cutting the second inorganic particles 52 with a plane. The shape of the third inorganic particles 53 and the shape of the second inorganic particles 52 are different. The third inorganic particles 53 have a flat portion 53a. The flat portion 53a forms the inner wall surface 13b of the opening 13a. The inner wall surface 13b is formed by the third inorganic particles 53 and the resin 110. More specifically, the inner wall surface 13b is formed by the surface 110b of the resin 110 exposed to the opening 13a and the flat portion 53a of the third inorganic particles 53. The flat portion 53a and the surface 110b of the resin 110 are approximately flush with each other. The surface 110b of the resin 110 that forms the inner wall surface 13b has no irregularities. The surface 110b of the resin 110 is generally smooth. The exposed surface of the flat portion 53a (the surface that forms the inner wall surface 13b) also has no irregularities. The exposed surface of the flat portion 53a is also generally smooth. Therefore, the inner wall surface 13b is generally smooth. The arithmetic mean roughness (Ra) of the inner wall surface 13b may be 1.0 μm or less.

[0053] In the wiring board 1 of this embodiment, the surface 11a of the insulating layer 11 of the first build-up section 10 is formed by the surface 110a of the resin 110 and the exposed surface 51aa of the first portion 51a of the first inorganic particle 51 exposed from the surface 110a of the resin 110. The surface 11a of the insulating layer 11 does not have a recess. Therefore, when the first layer (seed layer) 12α of the conductor layer 12 is formed on the surface 11a by sputtering, the continuous first layer 12α is formed even if the thickness of the sputtering film is thin. Therefore, the first layer 12α can be formed thin. If the first layer 12α is thin, for example, in the formation of the conductor layer 12 by a semi-additive method, after the formation of the second layer 12β by pattern plating, the unnecessary portion of the first layer 12α is reliably removed by, for example, etching. Therefore, even between fine conductor patterns such as the wiring 12w, short-circuit defects are unlikely to occur. In addition, the amount of etching when the first layer 12α is removed is small, and therefore the etching time is short, so that the amount of the second layer 12β exposed to the etching solution during the etching is small. The conductor layer 12 can have fine wiring such as the wiring 12w having a width according to the design value. Therefore, the wiring board 1 can have high quality.

[0054] Furthermore, in the example of FIG. 3, the inner wall surface 13b of the opening 13a penetrating the insulating layer 11 is formed by the flat portion 53a of the third inorganic particles 53 and the resin 110. As described above, the inner wall surface 13b is formed smoothly. Therefore, it is possible to form the first layer 12α of uniform thickness in the opening 13a, and therefore the first layer 12α can be formed thinly even on the inner wall surface 13b of the opening 13a. Therefore, short circuit defects are less likely to occur between fine conductor patterns such as the wiring 12w. The conductor layer 12 is more likely to have wiring such as the wiring 12w with a width according to the design value. Therefore, the wiring board 1 can have higher quality.

[0055] Next, with reference to Figures 4A to 4M, an example of a method for manufacturing the wiring board of this embodiment will be described, taking as an example the case of manufacturing the wiring board 1 illustrated in Figure 1. Unless otherwise stated, each component may be formed using any of the materials previously described for each component of the wiring board 1.

[0056] As shown in FIG. 4A, a support substrate S, which is, for example, a glass substrate, is prepared. An adhesive layer AL containing, for example, a photoplastic azobenzene-based polymer adhesive is formed on the surface of the support substrate S by coating, lamination, or the like. Then, a metal film layer 120 made of, for example, copper or nickel is formed on the adhesive layer AL by electroless plating or sputtering, or by attaching a metal foil using the adhesive layer AL. The support substrate S has a first surface Sa and a second surface Sb. In FIGS. 4B to 4M to be referred to below, the second surface Sb side is omitted from illustration, and only the first surface Sa side is shown. However, the wiring substrate 1 may also be formed on the second surface Sb side by performing the same process as that on the first surface Sa side.

[0057] As shown in FIG. 4B, a conductor layer 12a including conductor pads (component mounting pads 12p) is formed on the adhesive layer AL. In forming the conductor layer 12a, a plating resist (not shown) having openings corresponding to the formation regions of the conductor patterns to be included in the conductor layer 12a is formed on the metal film layer 120 shown in FIG. 4A by laminating a dry film, exposing to light, and developing. Then, the conductor layer 12a is formed by electrolytic plating using the metal film layer 120 as a power supply layer. Thereafter, the plating resist is removed, and further, the portion of the metal film layer 120 exposed by removing the plating resist is removed by etching or the like. The conductor layer 12a in the state shown in FIG. 4B is obtained.

[0058] Furthermore, an insulating layer 11 is formed to cover the conductor layer 12a. The insulating layer 11 is formed, for example, by laminating a film-like epoxy resin on the conductor layer 12a and thermocompressing it. As described above, the insulating layer 11 (as well as the insulating layer 21 and the insulating layer 31 (see FIG. 4L to FIG. 4M) formed in a later process) can be formed using a thermosetting resin such as BT resin or phenol resin, or a thermoplastic resin such as fluororesin or LCP, in addition to the epoxy resin. For example, a film-like resin containing inorganic particles 5 (see FIG. 4C) made of silica (SiO2), alumina, mullite, or the like, and the insulating resin 110 (see FIG. 4C) made of the epoxy resin, phenol resin, or the like described above is used. In the state shown in FIG. 4B, all of the inorganic particles 5 contained in the insulating layer 11 can be second inorganic particles 52 (see FIG. 4C).

[0059] A protective film PF made of a polyethylene terephthalate (PET) film or the like is provided on the surface (lower surface) 11a of the insulating layer 11. For example, a film-like resin having the protective film PF is laminated in forming the insulating layer 11. The protective film PF may be attached to the insulating layer 11 or the film-like resin constituting the insulating layer 11 via a release agent (not shown) or the like for easy peeling off of the protective film PF.

[0060] As shown in FIG. 4C, an opening 13a is formed by irradiation with a carbon dioxide laser beam or the like at a position in the insulating layer 11 where the via conductor 13 (see FIG. 1) will be formed. FIG. 4C and FIGS. 4D to 4I, which will be referred to below, show enlarged views of a portion corresponding to the IVC portion in FIG. 4B after the steps described in each figure are performed. The formation of the opening 13a by irradiation with a carbon dioxide laser beam or the like is performed while the surface 11a of the insulating layer 11 is protected by a protective film PF. Even if the resin 110 is scattered during the irradiation with the laser beam, the scattered resin 110 is prevented from adhering to the surface 11a of the insulating layer 11. Then, the opening 13a penetrating the protective film PF and the insulating layer 11 is formed.

[0061] The inner wall surface 13b of the opening 13a is formed of the resin 110 and inorganic particles 54 of the inorganic particles 5 that protrude from the resin 110. By irradiating the insulating layer 11 with laser light, a part of the second inorganic particles 52 embedded in the resin 110 protrudes from the resin 110 to become the inorganic particles 54. The inorganic particles 54 forming the inner wall surface 13b include a part protruding from the resin 110 and a part buried in the resin 110. In order to control the shape of the inner wall surface 13b, a predetermined treatment is applied to the inner wall surface 13b. The size of the unevenness of the inner wall surface 13b is controlled by controlling the conditions for treating the inner wall surface 13b. Preferably, the part of the inorganic particles 54 that protrudes from the resin 110 is selectively removed by the treatment.

[0062] As a result, as shown in Fig. 4D, third inorganic particles 53 having flat portions 53a are formed. As an example, the inner wall surface 13b of the opening 13a is treated with a chemical after irradiation with the laser light, thereby forming the third inorganic particles 53. For example, the inner wall surface 13b is treated with an etching solution having a faster etching rate for the inorganic particles 5 than for the resin 110. As an example, a permanganate solution is used.

[0063] Alternatively, the third inorganic particles 53 may be formed by treating the inner wall surface 13b with a plasma gas. The shape of the inner wall surface 13b can be controlled by controlling the conditions of the plasma treatment. As some examples, the etching rate of the inorganic particles 5 and the etching rate of the resin 110 are controlled by adjusting conditions such as temperature, concentration, time, type and pressure of the plasma gas. For example, plasma gas such as argon, tetrafluoromethane, a mixture of tetrafluoromethane and oxygen, or sulfur hexafluoride is used.

[0064] That is, a part of the spherical second inorganic particles 52 protrudes into the opening 13a by forming the opening 13a by irradiation with a laser beam to become an inorganic particle 54 (see FIG. 4C), and the protruding part is cut off on a flat surface by the above-mentioned appropriate processing. As described later, when a metal film 121 (see FIG. 4F) is formed as a seed layer on the inner wall surface 13b of the opening 13a by, for example, sputtering in a later process, the protruding part of the inorganic particle 54 may hinder the growth of the sputtering film. A seed layer that is continuous on the inner wall surface 13b may not be formed. Or, a thick seed layer may be required to be formed, making it impossible to form fine wiring.

[0065] In contrast, in the manufacture of the wiring board 1 of the embodiment, the protruding portions of the inorganic particles 54 are removed to form the third inorganic particles 53 having flat portions 53a. The flat portions 53a are planar. The inner wall surface 13b of the opening 13a is formed by the flat portions 53a of the third inorganic particles 53 and the surface 110b of the resin 110 exposed in the opening 13a. The flat portions 53a forming the inner wall surface 13b and the surface 110b of the resin 110 are substantially flush with each other. No irregularities are formed on the inner wall surface 13b. A smooth inner wall surface 13b is obtained.

[0066] The treatment of the inner wall surface 13b is performed in a state where the surface 11a of the insulating layer 11 is protected by the protective film PF. Therefore, the surface 11a of the insulating layer 11 is not easily eroded by, for example, chemicals or plasma gas during the treatment of the inner wall surface 13b.

[0067] After the processing of the inner wall surface 13b of the opening 13a, the inside of the opening 13a is cleaned as necessary. By cleaning the inside of the opening 13a, resin residues generated when the opening 13a is formed are removed. That is, the cleaning may include a desmearing process. The cleaning of the inside of the opening 13a is performed by a plasma treatment, for example. That is, the cleaning may be performed by a dry process. The surface 11a of the insulating layer 11 is not affected by the plasma treatment because it is covered with the protective film PF. Therefore, at this point, no irregularities are formed on the surface 11a of the insulating layer 11. The surface 11a is not roughened. Note that, if the inside of the opening 13a is sufficiently cleaned by the processing of the inner wall surface 13b in the preceding process, the cleaning of the inside of the opening 13a after the processing of the inner wall surface 13b may be omitted.

[0068] After the inside of the opening 13a is cleaned (after the inner wall surface 13b is treated if cleaning of the inside of the opening 13a is omitted), the protective film PF is removed from the insulating layer 11.

[0069] As shown in FIG. 4E, the surface 11a of the insulating layer 11 is exposed. As described above, the surface 11a of the insulating layer 11 is not affected by the chemicals or plasma gas used to clean the inside of the opening 13a or to treat the inner wall surface 13b. Therefore, the surface 11a after the protective film PF is removed is flat as shown by the two-dot chain line in FIG. 4E. The flat surface 11a is cleaned. As an example, the surface 11a is dry etched. The dry etching is performed by sputtering (argon sputtering) using argon gas, for example. By cleaning by dry etching or the like, the resin 110 forming the insulating layer 11 is removed by about 20 nm near the surface 11a. The release agent and / or adhesive (not shown) interposed between the protective film PF (see FIG. 4D) and the insulating layer 11 may be removed together with the resin 110 near the surface 11a. In dry etching such as argon sputtering, the resin 110 near the surface 11a is selectively removed, that is, more quickly than the inorganic particles 5 (second inorganic particles 52) near the surface 11a.

[0070] The thickness of the resin 110 is reduced by cleaning. As a result, a part of the inorganic particles 5 (second inorganic particles 52) present near the surface 11a is partially exposed from the surface (lower surface) 110a of the resin 110. A part of the second inorganic particles 52 buried in the resin 110 is exposed from the surface 110a of the resin 110 to become the first inorganic particles 51. That is, the first inorganic particles 51 are formed from the second inorganic particles 52. The shape of the first inorganic particles 51 and the shape of the second inorganic particles 52 are substantially the same and may be spherical. The first inorganic particles 51 are composed of a part protruding from the resin 110 and a part buried in the resin 110. The surface 11a of the insulating layer 11 is formed by the surface 110a of the resin 110 and an exposed surface 51aa of the first inorganic particles 51 from the surface 110a of the resin 110. The exposed surface 51aa is exposed from the resin 110 by cleaning by dry etching or the like. The surface 11a of the insulating layer 11 is not roughened. Therefore, almost no recesses are formed on the surface 11a.

[0071] As shown in FIG. 4F, a metal film 121 made of, for example, copper or nickel is formed on the inner wall surface 13b of the opening 13a, the exposed surface of the component mounting pad 12p, and the surface 11a of the insulating layer 11 by sputtering or electroless plating. The metal film 121 functions as a seed layer when a metal film 122 (see FIG. 4H) is formed by electrolytic plating in a later process. When the metal film 121 is formed by sputtering, the metal film 121 may have high adhesion with the insulating layer 11. A part of the metal film 121 may become the first layer 12α (see FIG. 2) constituting the conductor layer 12 formed on the insulating layer 11. The protruding portion of the first inorganic particle 51 from the surface 11a of the insulating layer 11 is covered with the metal film 121. The exposed surface of the third inorganic particle 53 on the inner wall surface 13b of the opening 13a is also covered with the metal film 121.

[0072] As described above, the surface 11a of the insulating layer 11 has substantially no recesses. In addition, the inner wall surface 13b of the opening 13a has no recesses and is substantially smooth. Therefore, a thin but continuous metal film 121 can be formed by sputtering. For example, the metal film 121 has a thickness of 0.05 μm or more and less than 0.5 μm. If the thickness of the metal film 121 is less than 0.5 μm, fine wiring may be formed on the insulating layer 11.

[0073] As shown in FIG. 4G, a plating resist R having an opening R1 is provided on the metal film 121. The plating resist R is formed, for example, by laminating a dry film on the metal film 121, and the opening R1 is formed, for example, by a photolithography technique. The opening R1 is formed in a pattern corresponding to a conductor pattern to be included in the conductor layer 12 (see FIG. 4J) formed on the insulating layer 11. As described above, the wiring such as the wiring 12w (see FIG. 2) included in the conductor layer 12 may have a wiring width of 3 μm or less. Each opening R1 is formed with an opening width according to the wiring width to be included in each conductor pattern such as the wiring 12w formed in each opening R1. Also, as described above, the wiring of the conductor layer 12 may have an aspect ratio of 2.0 or more and 4.0 or less. Therefore, preferably, the plating resist R is formed having a thickness (height) greater than or equal to the thickness (height) of the wiring that satisfies the aspect ratio to be included in the wiring to be formed.

[0074] If the surface 11a of the insulating layer 11 has a recess when the plating resist R is formed, air due to the recess is likely to be trapped between the plating resist R and the metal film 121. However, the surface 11a of the insulating layer 11 in the wiring board 1 of the embodiment has almost no recess. Therefore, the surface of the metal film 121 also has almost no recess. Therefore, air is unlikely to remain between the plating resist R and the metal film 121. In addition, the contact area between the plating resist R and the metal film 121 is large. Even if the width W3 of the plating resist R between the openings R1 is, for example, about 1 μm to 3 μm, which may be the minimum wiring interval of the conductor layer 12, a plating resist R that is unlikely to peel off from the metal film 121 can be formed.

[0075] As shown in FIG. 4H, a metal film 122 made of, for example, copper or nickel is formed in an opening R1 of a plating resist R by electrolytic plating using a metal film 121 as a power supply layer. A part of the metal film 122 can become a second layer 12β (see FIG. 2) constituting a conductor layer 12 formed on an insulating layer 11. A via conductor 13 is formed in an opening 13a of the insulating layer 11. As in the example of FIG. 4H, the metal film 122 may be formed so as to fill the entire opening R1 and further have a curved surface protruding from the surface (lower surface) of the plating resist R. This may allow wiring having a desired thickness and aspect ratio to be formed more reliably.

[0076] As shown in FIG. 4I, a part of the lower surface (surface opposite to the conductor layer 12a) of the metal film 122 is removed by polishing. At least the protruding part of the metal film 122 from the lower surface of the plating resist R is removed. The metal film 122 is polished until the total thickness with the metal film 121 reaches the thickness required for the conductor layer 12 (see FIG. 4J) formed on the insulating layer 11, for example, to 7 μm or less. As in the example of FIG. 4I, a part of the lower surface of the plating resist R may also be removed together with a part of the metal film 122. The metal film 122 is polished by any method, such as chemical mechanical polishing (CMP). As a result of polishing, the lower surface of the metal film 122 may have an arithmetic mean roughness of 0.3 μm or less.

[0077] After polishing the metal film 122, the plating resist R is removed. Furthermore, the portion of the metal film 121 that is not covered with the metal film 122 is removed by, for example, quick etching.

[0078] As shown in Fig. 4J, a conductor layer 12 including predetermined conductor patterns separated from each other, such as wiring 12w, is obtained. In Fig. 4J, like Fig. 1, the conductor layer 12 is shown to have only one layer, but the conductor layer 12 is composed of the metal film 122 shown in Fig. 4I and the metal film 121 after a part of the metal film 122 is removed from the state of Fig. 4I as described above.

[0079] As shown in Fig. 4K, three sets of insulating layers 11 and conductor layers 12, and via conductors 13 are further formed on the insulating layer 11 and conductor layer 12 formed in the steps up to Fig. 4J in the same manner as described with reference to Fig. 4B to Fig. 4I. Then, on the laminate of the conductor layer 12 and insulating layer 11 thus formed, an insulating layer 11 is further laminated in the same manner as the other insulating layers 11, and an opening 13a penetrating the insulating layer 11 is formed by irradiation with laser light or the like. The first build-up section 10 is completed.

[0080] 4L, a conductor layer 22a and a via conductor 23a are formed on the underside of the first buildup section 10. The second buildup section 20 is formed by repeating the formation of the insulating layer 21, the conductor layer 22, and the via conductor 23. The conductor layer 22a, the conductor layer 22, the via conductor 23a, and the via conductor 23 are formed by any method for forming a conductor layer and a via conductor, such as a semi-additive method. The insulating layer 21 can be formed by laminating and thermocompression bonding a film-like resin, similar to the method for forming the insulating layer 11.

[0081] As shown in FIG. 4M, the insulating layer 31, the conductor layer 32, and the via conductors 33 penetrating the insulating layer 31 of the third buildup section 30 are formed on the surface (second surface 20B) of the second buildup section 20 opposite to the support substrate S side. The insulating layer 31 in FIG. 4M is formed by laminating and thermocompression bonding prepregs containing an insulating resin such as epoxy resin impregnated in a core material 31a made of glass fiber or the like. The insulating layer 31 may be formed by thermocompression bonding of a film-like resin, similar to the insulating layer 21. The conductor layer 32 and the via conductors 33 may be formed, for example, by a semi-additive method, similar to the method for forming the conductor layer 22 and the via conductors 23, or may be formed by any other method for forming a conductor layer, such as a subtractive method. The formation of the third buildup section 30 is completed.

[0082] Furthermore, a solder resist 40 is formed by depositing a photosensitive epoxy resin film or a polyimide resin film on the surfaces of the insulating layer 31 and the conductor layer 32. Then, openings 41 that define the conductor pads 32p are formed by photolithography.

[0083] Thereafter, the support substrate S is removed. For example, the adhesive layer AL is irradiated with a laser beam, and after the adhesive layer AL is softened, the support substrate S is peeled off from the conductor layer 12a and the insulating layer 11. The upper surface of the conductor layer 12a and the upper surface of the insulating layer 11 are exposed. If the adhesive layer AL remains, it is removed using an appropriate solvent. The wiring board 1 shown in FIG. 1 is completed.

[0084] The wiring board of the embodiment is not limited to those having the structure illustrated in each drawing, and the structure, shape, and material illustrated in this specification. Each build-up portion included in the wiring board of the embodiment may have any number of insulating layers and conductor layers as described above. In addition, the wiring board of the embodiment does not necessarily include the third build-up portion. The outermost insulating layer and conductor layer on the opposite side to the component mounting surface of the wiring board of the embodiment may not be formed thicker than the insulating layer and conductor layer in the second build-up portion, and the outermost insulating layer on the opposite side to the component mounting surface of the wiring board may not include a core material. The inorganic particles included in the insulating layer of the first build-up portion may not include inorganic particles that constitute the inner wall surface of the opening for forming a via conductor, such as the third inorganic particles. [Explanation of symbols]

[0085] 1. Wiring board 1F, 1st floor 1B 2nd side 10 First build-up section 11 Insulating layer (first insulating layer) 11a: Surface (lower surface) of insulating layer 11 on the second buildup portion side 110 Resin of insulating layer 11 110a Surface (lower surface) of resin 110 12, 12a Conductive layer (first conductive layer) 12w, 22w wiring 12α 1st layer (seed layer) 12β 2nd layer (electrolytic plating layer) 13, 23, 33 Via conductor 13a aperture 13b Inner wall surface of opening 20 Second Build-up Section 21 Insulating layer (second insulating layer) 22, 22a Conductive layer (second conductive layer) 30 Third Build-up Section 31 Insulating layer (third insulating layer) 31a Core material 32 Conductor layer (third conductor layer) 5, 6 Inorganic particles 51 First inorganic particle 51a Part 1 51aa exposed surface 51b Part 2 52 Second inorganic particle 53 Third inorganic particle 53a Flat area E1, E2 parts Ea1, Ea2 parts area G1: The minimum distance between the traces in the conductor layer of the first build-up G2: Minimum spacing between traces in the conductor layer of the second build-up W1 Width of the wiring included in the conductor layer of the first build-up section (minimum width) W2 Width of the wiring included in the conductor layer of the second build-up section (minimum width)

Claims

1. a first surface and a second surface opposite the first surface; a first buildup section including insulating layers and conductor layers stacked one on the other; a second buildup section including an insulating layer and a conductor layer stacked one on the other; A wiring board comprising: the first buildup section is laminated on the first surface side of the second buildup section, and a minimum width of a wiring included in a conductor layer of the first buildup section is smaller than a minimum width of a wiring included in a conductor layer of the second buildup section; a minimum interval between wirings included in the conductor layer of the first buildup portion is smaller than a minimum interval between wirings included in the conductor layer of the second buildup portion; the insulating layer of the first buildup section contains a resin and inorganic particles, the inorganic particles include first inorganic particles partially embedded in the resin and second inorganic particles entirely embedded in the resin; the first inorganic particles are formed of a first portion protruding from the resin and a second portion embedded in the resin, The surface of the insulating layer of the first buildup portion that is covered with the conductor layer of the first buildup portion is formed by the surface of the resin and an exposed surface of the first portion that is exposed from the resin.

2. 2. The wiring board according to claim 1, the minimum width of the wiring included in the conductor layer of the first buildup portion is 3 μm or less; The minimum distance between the wirings included in the conductor layer of the first buildup portion is 3 μm or less.

3. 2. The wiring board according to claim 1, wherein the aspect ratio of the wiring included in the conductor layer of the first buildup portion is not less than 2.0 and not more than 4.

0.

4. 2. The wiring board according to claim 1, wherein a surface of the conductor layer of the first build-up portion is a polished surface.

5. 2. The wiring board according to claim 1, further comprising a third buildup section laminated on the second surface side of the second buildup section, the third buildup section including an insulating layer, a conductive layer, and a via conductor.

6. 6. The wiring board according to claim 5, wherein the insulating layer included in the third buildup section includes a core material.

7. 7. The wiring board according to claim 6, wherein the core material is glass fiber.

8. 2. The wiring board according to claim 1, wherein the first surface is a component mounting surface.

9. 2. The wiring board according to claim 1, wherein a ratio of a volume of the first portion to a volume of the first inorganic particles is greater than 0 and is equal to or smaller than 0.

4.

10. 2. The wiring board according to claim 1, wherein the arithmetic mean roughness (Ra) of the surface of the insulating layer of the first buildup portion is less than 0.08 [mu]m.

11. 2. The wiring board according to claim 1, the first buildup portion further includes a via conductor formed in an opening penetrating the insulating layer of the first buildup portion, The inorganic particles further include third inorganic particles forming an inner wall surface of the opening, the inner wall surface is formed by the third inorganic particles and the resin, The third inorganic particles have a flat portion that forms the inner wall surface.

12. 12. The wiring board according to claim 11, wherein the arithmetic mean roughness (Ra) of the inner wall surface is 1.0 [mu]m or less.

13. 12. The wiring board according to claim 11, wherein the third inorganic particles have a spherical decapitated shape.

14. 2. The wiring board according to claim 1, the first buildup portion further includes a via conductor penetrating the insulating layer of the first buildup portion, the conductor layer and the via conductor of the first buildup portion are formed of a seed layer and an electrolytic plating film layer formed on a surface of the seed layer, The seed layer has a thickness of less than 0.5 μm.

15. 2. The wiring board according to claim 1, the first buildup portion further includes a via conductor penetrating the insulating layer of the first buildup portion, The via conductor has a shape whose diameter decreases from the second surface to the first surface.

16. 2. The wiring board according to claim 1, the conductor layer of the first buildup portion is formed of a seed layer and an electrolytic plating film layer formed on a surface of the seed layer, The seed layer is a sputtered film.

Citation Information

Patent Citations

  • Printed wiring board and manufacturing method thereof

    JP2021019061A