Bonding method
The described bonding method uses jig members to apply adhesives around narrow frame display devices, ensuring reliable and defect-free adhesive layers by curing and removing jig members, addressing space constraints and adhesive reliability issues.
Patent Information
- Application Number
- JP2023075232
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-28
- Publication Date
- 2024-11-08
AI Technical Summary
Conventional dam-and-fill bonding methods are unsuitable for display modules with narrow frames due to lack of space for applying dam material, leading to potential air bubble entry, peeling, and reliability issues in the adhesive layer.
A bonding method using first and second jig members to apply adhesives around the display device, ensuring space for adhesive application, followed by curing and removing the jig members, allowing for stable adhesive layer formation even in narrow frames.
Ensures high-quality and reliable adhesive layer formation in narrow frame display modules, preventing defects like peeling and air bubble entry, and maintaining consistent adhesive thickness despite warping or design constraints.
Smart Images

Figure 2024159317000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for bonding a liquid crystal module or an organic EL display module used in a display such as a television device or a monitor to a cover panel. [Background technology]
[0002] Patent Document 1 discloses a method for manufacturing an organic EL display device comprising an array substrate having an organic EL film and electrode pattern, as well as signal lines, scanning lines and switching elements within an image display area in which pixels are arranged in a matrix, a counter substrate bonded to the array substrate, a dam material arranged to surround the image display area, and a fill material filling the gap surrounded by the array substrate, the counter substrate and the dam material. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2015-79580 A Summary of the Invention [Problem to be solved by the invention]
[0004] The present disclosure has been devised in consideration of the conventional circumstances, and provides a bonding method that enables dam and fill bonding even in narrow-frame display modules where there is almost no space for applying dam material, and ensures the quality and high reliability of the adhesive layer after bonding. [Means for solving the problem]
[0005] The present disclosure provides a bonding method for bonding a front panel and a display device, which are rectangular in plan view, together with an adhesive, the method including: placing a first jig member arranged in contact with the four peripheral sides of the display device on top of a second jig member arranged on the rear side of the display device and having an area larger than that of the display device; applying a first adhesive to the top of the first jig member and surrounding the periphery of the display device; filling the space inside the first adhesive and between the display device and the front panel with a second adhesive; hardening the first adhesive and the second adhesive; and removing the first jig member and the second jig member after the hardening. Effect of the Invention
[0006] According to the present disclosure, dam & fill bonding can be performed even in narrow-frame display modules where there is almost no space to apply dam material, making it possible to ensure the quality and high reliability of the adhesive layer after bonding. [Brief description of the drawings]
[0007] [Figure 1] Cross-section of a display module bonded together using a typical dam-and-fill method [Diagram 2] Cross-section of a narrow-bezel display module bonded using a typical dam-and-fill method [Diagram 3] An illustration of the issues involved in applying dam-and-fill lamination to narrow-bezel display modules [Figure 4] FIG. 1 is a schematic cross-sectional view showing an example of a basic structure of a narrow-frame display module according to a first embodiment; [Diagram 5] Schematic cross-sectional view of an adhesive curing process according to the first embodiment. [Figure 6] Schematic cross-sectional view of a jig member removal process according to the first embodiment. [Figure 7] FIG. 1 is a schematic cross-sectional view showing an example of penetration of a filler material into a narrow-frame display module according to a first embodiment; [Figure 8] FIG. 11 is a schematic cross-sectional view showing an example of a basic structure of a narrow-frame display module according to a second embodiment. [Figure 9] FIG. 11 is a schematic cross-sectional view showing an example of a basic structure of a narrow-frame display module according to a modified example of the second embodiment. [Figure 10] 1 is a schematic cross-sectional view of a display device having a warped shape at one end side in a narrow frame display module according to the first embodiment, when the display device is bonded by a dam-and-fill method; [Figure 11] Schematic cross-sectional view showing an example of measuring the height difference value [Figure 12] FIG. 11 is a schematic cross-sectional view showing an example of a basic structure of a narrow-frame display module according to a third embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] (Background to this disclosure) Recent mobile terminals, such as mobile phones such as smartphones and tablet terminals, often have both a touch panel and a display device. The display device here is typically a liquid crystal module or an organic electroluminescence (EL) module. Conventionally, the touch panel and the display device were separate components, and the display device was attached inside the housing of the mobile terminal. The touch panel was mounted on the front side of the display device as part of the exterior, and an air layer was generally placed between these two components.
[0009] Recently, however, a technology for bonding these touch panels and display devices with optical adhesives (hereinafter sometimes referred to as "direct bonding") has been established, mainly for small displays, and many products are already beginning to spread on the market. Direct bonding is expected to have various advantages, such as suppressing reflection, improving brightness, improving strength, preventing condensation, and preventing dust from entering.
[0010] However, on the other hand, the shapes and specifications of the touch panels and display devices to be bonded have become more diverse, and various bonding methods have been proposed in response to this diversification. In terms of materials, there are also many types of materials used for bonding. For example, there are highly transparent double-sided adhesives called Optical Clear Adhesive (OCA), highly transparent liquid resins called Optical Clear Resins (OCR), and liquid resins called hybrid OCR that are semi-cured and bonded together. On the other hand, there are also bonding methods such as the roller bonding method, which uses OCA in an atmospheric environment to bond by applying roller pressure, and the dam and fill method, which uses two types of OCR, a dam material and a fill material, to bond while removing air in a vacuum environment (see, for example, Patent Document 1). In particular, the latter bonding method in a vacuum environment is known to have the advantage that air bubbles are less likely to be trapped, and even if they are trapped, they tend to disappear in the subsequent process. This makes it possible to freely control the thickness of the adhesive layer by freely adjusting the height of the dam material, enabling highly reliable bonding. In fact, this method is now being adopted by many manufacturers in industries where product reliability is important, such as the automotive industry.
[0011] In general, the dam & fill method is said to be suitable for bonding large-sized objects. The reason is that the thickness of the adhesive layer can be freely adjusted with the dam material (hereinafter sometimes abbreviated as "dam material"). The larger the size, the more the reliability of the adhesive layer becomes an issue when bonding a touch panel and a display device. The adhesive material (e.g. OCR) used in the dam & fill method is usually a very soft material with a low storage modulus. However, if the adhesive layer is set thin, the adhesive layer between the touch panel and the display device is loaded when heated or cooled due to the difference in thermal expansion and thermal contraction between the touch panel and the display device, and problems such as peeling of the adhesive layer occur. Therefore, the larger the size, the more often the method of setting the adhesive layer thick and bonding them together is usually used. Therefore, the dam & fill method is often used mainly for large-sized objects because the thickness of the adhesive layer can be controlled by applying a thick dam material. However, this method also has disadvantages.
[0012] For example, in recent years, narrow-frame displays have become more common in end products such as smartphones and tablets from the viewpoint of design. Usually, the dam material is applied to the outer area of the image display area (generally called the "active area") of the display device. However, in the case of a narrow-frame display, this outer area becomes narrower than the outer area of the image display area of a conventional display device, and the space for applying the dam material becomes zero or infinitesimally narrow. The dam material is often selected to have a refractive index close to that of the fill material (hereinafter sometimes abbreviated as "fill material"). Since the boundary area between the dam material and the fill material is often invisible to the naked eye, in some cases, the dam material is applied as close as possible to the outer edge of the screen display area. However, in the surface where two different materials (dam material, fill material) meet, air bubbles may be introduced during manufacturing, or appearance defects such as peeling may occur around the boundary during product reliability testing. This increases the possibility of defects occurring on the product side. In other words, the previous dam and fill method was unsuitable for manufacturing narrow-bezel displays, and because it was difficult to secure space to apply the dam material, it was difficult to apply it to bonding touch panels and display devices.
[0013] Therefore, in the following embodiment, an example of a bonding method will be described that enables dam and fill bonding even in narrow-frame display modules that have no space for applying dam material, and ensures the quality and high reliability of the adhesive layer after bonding.
[0014] Hereinafter, with reference to the drawings as appropriate, an embodiment specifically disclosing the bonding method according to the present disclosure will be described in detail. However, more detailed explanation than necessary may be omitted. For example, detailed explanation of already well-known matters or duplicate explanation of substantially the same configuration may be omitted. This is to avoid the following explanation becoming unnecessarily redundant and to facilitate understanding by those skilled in the art. Note that the attached drawings and the following explanation are provided to enable those skilled in the art to fully understand the present disclosure, and are not intended to limit the subject matter described in the claims.
[0015] First, before specifically describing an embodiment (present embodiment) of the bonding method according to the present disclosure, examples of a display module bonded by a general dam & fill method and a narrow-frame display module bonded by the dam & fill method will be described with reference to Figs. 1 to 3. Fig. 1 is a cross-sectional view of a display module 100 bonded by the general dam & fill method. Fig. 2 is a cross-sectional view of a narrow-frame display module 200 bonded by general dam & fill bonding. Fig. 3 is an explanatory diagram of a problem when applying dam & fill bonding to a narrow-frame display module 300.
[0016] In the following description, the up, down, left and right directions of the display are the directions shown in the attached drawings. In other words, the up and down direction indicates the thickness direction of the display, and the left and right direction indicates the surface direction of the display. In addition, in the description of Figures 2 and 3, elements that overlap with the description of Figures 1 and 2 are given the same reference numerals, and the description is simplified or omitted, and different contents are described.
[0017] 2. Display module bonded using a typical dam-and-fill construction method The display module 100 shown in FIG. 1 is composed of a front panel 101, a display device 103, a polarizing plate 105, a filler material 106, and a dam material 107.
[0018] The front panel 101 is, for example, a touch panel, a cover glass, a resin cover lens, or the like.
[0019] The display device 103 is a liquid crystal panel, an organic EL display, a microLED display, or the like, and a part of the front side and all the periphery of the sides are covered by a bezel member 108. The front panel 101 and the display device 103 shown in Fig. 1 are bonded together by a dam material 107 and a fill material 106 using a dam and fill method. In general, a type of highly transparent adhesive called an optical adhesive is often used for both the dam material 107 and the fill material 106, and acrylic resins and silicone resins are the mainstream materials.
[0020] In the dam and fill method, first, dam material 107 is applied onto the image display area (i.e., active area 104) of display device 103, which is rectangular in plan view, then fill material 106 is applied within the area surrounded by dam material 107, and front panel 101 is lowered from above and bonded together. Note that since the dam and fill method itself is a known technology, a detailed explanation of the manufacturing process will be omitted.
[0021] A characteristic feature of the cross-sectional structure example in Fig. 1 is the position of dam material 107. Front panel 101 has a silkscreened section 102 (non-transparent section) that has been silkscreened on its back surface (in other words, the underside), and a transparent section 109 for viewing images on display device 103. Most common monitor products have this configuration. Display device 103 also has an active area 104 that displays images, and a polarizing plate 105 thereon that has an area larger than that of active area 104. Polarizing plate 105 is disposed on top of active area 104.
[0022] The dam material 107 is applied on this polarizing plate 105, further on the outer periphery side than the active area 104, and on the back side (in other words, the lower side) of the silk-screened portion 102. In other words, the dam material 107 is applied at a position that cannot be seen with the naked eye from the outside. This is because the dam material 107 and the fill material 106 are different materials with different refractive indices (however, materials with relatively similar refractive indices are selected), and therefore the contact interface between the dam material 107 and the fill material 106 can sometimes be seen with the naked eye. Therefore, if the contact interface between the dam material 107 and the fill material 106 falls within the active area 104, the image quality will be degraded.
[0023] 3. Narrow-frame display module bonded using a typical dam-and-fill method Recently, from a design perspective, monitor components have become narrower in frame, and it has become very difficult to apply the dam and fill method to such components, resulting in structures that differ from those shown in Figure 1. An example of a display module with a narrower frame that has been bonded together using the dam and fill method is described below with reference to Figures 2 and 3.
[0024] The narrow-frame display module 200 shown in Fig. 2 is configured with a front panel 101, a display device 103, a polarizing plate 105, a filler material 106, and a dam material 107, similar to the display module 100 shown in Fig. 1. Similarly, the narrow-frame display module 300 shown in Fig. 3 is configured with a front panel 101, a display device 103, a polarizing plate 105, a filler material 106, and a dam material 107, similar to the display module 100 shown in Fig. 1 or the narrow-frame display module 200 shown in Fig. 2.
[0025] For example, in the narrow frame display module 200, both the frame width 201 of the silk screen printing section 102 of the front panel 101 (in other words, the frame width of the front panel) and the frame portion 202 of the display device 103 are narrower than those of the display module 100 in Fig. 1. Note that the frame portion 202 of the display device 103 refers to the outer side of the active area 104.
[0026] Unlike the display module 100 in FIG. 1, the narrow frame display module 200 in FIG. 2 does not have enough space to apply the dam material 107 on the polarizing plate 105. Therefore, in the narrow frame display module 200 in FIG. 2, the position of the dam material 107 when the front panel 101 and the display device 103 are bonded together is a position that covers both a part of the outer peripheral edge of the polarizing plate 105 and a part of the polarizing plate 105 side of the bezel member 108 of the display device 103. Here, the bezel member 108 is usually tape or metal, and tape is mainly used especially for small inch displays. In this case, if the bezel member 108 is tape, the height of the dam material 107 is not stable due to wrinkles in the tape, etc., and the thickness of the adhesive layer cannot be made uniform, which may cause display defects such as display unevenness. In addition, since the dam material 107 is applied across the bezel member 108 and the polarizing plate 105, there are areas where three different materials are mixed, and the difference in the amount of thermal expansion of each member causes defects in product quality such as peeling or bright spots of cracks during reliability tests under heat, etc. On the other hand, in the bonding method, the height of the dam material 107 is high only in a part, so that the fill material 106 breaks out of the dam material 107, causing manufacturing problems such as contamination or damage to the members.
[0027] A state in which the frame is narrower than that shown in FIG. 2 will be described with reference to the schematic diagram of FIG.
[0028] In the narrow frame display module 300 of FIG. 3, the frame width 201 of the silk screen printing section 102 and the frame width of the frame section 202 of the display device 103 are narrower than those of the narrow frame display module 200 of FIG. 2. It is known that the structural example shown in FIG. 3 is often adopted in organic EL displays and the like. Although FIG. 3 shows an example in which a bezel member 108 is provided, in some cases, the bezel member 108 may be omitted. In the structural example of FIG. 3, there is no physical space to apply the dam material 107 in the first place, and the dam material 107 almost overflows from the display device 103. For this reason, there is a problem that the dam and fill method cannot be applied to the manufacture of the narrow frame display module 300.
[0029] (Embodiment 1) Next, based on the explanation of Figs. 1 to 3, a first embodiment of a bonding method according to the present disclosure will be explained with reference to Figs. 4 to 6. Fig. 4 is a schematic cross-sectional view showing an example of a basic structure of a narrow-bezel display module 400 according to the first embodiment. Fig. 5 is a schematic cross-sectional view of an adhesive curing process according to the first embodiment. Fig. 6 is a schematic cross-sectional view of a jig member removal process according to the first embodiment. In the explanation of Figs. 4 to 6, elements that overlap with the explanation of Figs. 1 to 3 are given the same reference numerals, and explanations are simplified or omitted, and differences will be explained.
[0030] The narrow frame display module 400 shown in Fig. 4 is composed of a front panel 101, a display device 103, a polarizing plate 105, a filter material 106, and a dam material 107. The dam material 107 may be omitted. Also in the narrow frame display module 400, similar to the structural example of Fig. 3, the frame width 201 of the silk screen printing unit 102 and the frame width of the frame portion 202 of the display device 103 are narrower than those of the narrow frame display module 200 of Fig. 2.
[0031] 4. Detailed procedure of the dam and fill construction method according to the first embodiment In the narrow-frame display module 400 shown in FIG. 4, a dam-and-fill method (more specifically, a dam-and-fill bonding method) for bonding the narrow-frame front panel 101 and the narrow-frame display device 103 together will be described.
[0032] In the first embodiment, a first jig member 401 is disposed around the outer periphery of the display device 103, and a second jig member 402 is disposed on the back side (in other words, the lower side) of the display device 103. The first jig member 401 is fitted into the second jig member 402. An upper surface 403 of the first jig member 401 is at the same height as an upper surface 404 of a polarizing plate 105 disposed on the upper side of the active area 104 of the display device 103, or is lower than that height. It is preferable that the first jig member 401 and the outer periphery side surface of the display device 103 are in contact with each other without any gaps. In order to eliminate such gaps, for example, pressing with a spring or the like, or contact with an elastic body or adhesive can be considered.
[0033] The bonding method using the dam-and-fill method according to the first embodiment is carried out in the following procedure. (Step 1) A process of attaching the display device 103 with two jig members (Step 2) Process of bonding the front panel 101 and the display device 103 (Step 3) Adhesive curing process for two adhesives (Step 4) Removal process of the two jig components
[0034] Each process will be described in turn below.
[0035] (Step 1) A process of attaching the display device 103 with two jig members Display device 103 is attached to first jig member 401 and second jig member 402. Specifically, the outer peripheral side surface of display device 103 is held by first jig member 401, and in this state, first jig member 401 and display device 103 are placed on second jig member 402. Display device 103 has active area 104, and polarizing plate 105 having an area larger than active area 104 is placed above display device 103, which is the same as the structural examples in FIGS. 1 to 3.
[0036] (Step 2) Process of bonding the front panel 101 and the display device 103 After (Step 1), front panel 101 and display device 103 are bonded together by the dam and fill method. At this time, dam material 107 is applied to the back side (in other words, the lower side) of silk-screened portion 102, which is the same as the structural example of FIGS. 1 to 3. However, dam material 107 is characterized in that it is applied not on polarizing plate 105 or on bezel member 108, but on first jig member 401. More specifically, in the bonding process using the dam and fill method in (Step 2), dam material 107 is applied first. Then, fill material 106 is applied within the area surrounded by dam material 107. In this way, front panel 101 and display device 103 are bonded together.
[0037] (Step 3) Adhesive curing process for two adhesives After front panel 101 and display device 103 are bonded together by the dam and fill method in (Step 2), the process proceeds to a hardening process for the two adhesives (i.e., dam material 107 and fill material 106). Even in this case, first jig member 401 and second jig member 402 are handled in the attached state shown in FIG. 4, and the adhesive hardening process is carried out (see FIG. 5).
[0038] The adhesive curing process is achieved by a front UV curing device 501 and a side UV curing device 502. The front UV curing device 501 is disposed at a position facing the transmissive portion 109 of the front panel 101, and each of the pair of side UV curing devices 502 is disposed at a position facing the outer peripheral side surface of the front panel 101 with the silk-screened portion 102 of the front panel 101 as the main subject.
[0039] The front UV curing device 501 is a device intended to harden the components to which the filler material 106 is bonded by hardening the filler material 106 with irradiated UV (i.e., ultraviolet light) through the transparent portion 109 of the front panel 101. The side UV curing device 502 is a device intended to harden the portion of the silkscreen printing unit 102 not irradiated with UV from the front UV curing device 501 and the filler material 106 by hardening the back portion of the silkscreen printing unit 102 of the front panel 101 (i.e., the portion not irradiated with UV from the front UV curing device 501) with irradiated UV (i.e., ultraviolet light).
[0040] Here, since the upper surface 403 of the first jig member 401 is located below the upper surface 404 of the polarizing plate 105, the UV irradiated from the side UV curing device 502 reaches deep inside (in other words, penetrates), which provides the effect of stabilizing the curing of the adhesive across the rear side of the silk-screened section 102. The first jig member 401 is preferably made of a material that transmits UV, such as a transparent body. Since UV from the side must be irradiated into a narrow gap, the first jig member 401 transmits UV, which makes it possible to irradiate more UV light into the gap on the rear side of the silk-screened section 102, thereby providing the effect of suppressing poor curing of the adhesive (dam material 107, fill material 106).
[0041] When a UV-curable resin is used for the adhesive (dam material 107, fill material 106), it is preferable to harden the adhesive layer using these two types of devices (front UV curing device 501, side UV curing device 502). However, when a room temperature curing adhesive is used, these devices (front UV curing device 501, side UV curing device 502) may not be used. In either case, the bonding method according to the first embodiment is characterized in that the display device 103 is fixed in position to the first jig member 401 and the second jig member 402, and the adhesive (i.e., the dam material 107, the fill material 106) is cured in the state in which the front panel 101 and the display device 103 are bonded together by the dam & fill method.
[0042] (Step 4) Removal process of the two jig components After (Step 3), a process for removing the two jig members is performed. This process is a step for removing the bonded narrow-frame display module 400 from the first jig member 401 and the second jig member 402 after the adhesive has hardened.
[0043] In this process, the first jig member 401 is separated by an operator from the narrow frame display module 400 with the dam material 107 applied thereto, or is removed with the dam material 107 remaining on the narrow frame display module 400. When the adhesive strength between the dam material 107 and the filler material 106 is stronger than the adhesive strength between the dam material 107 and the first jig member 401, the dam material 107 often remains on the narrow frame display module 400 side. Conversely, when a gel-like material is selected for the filler material 106, the adhesive strength between the dam material 107 and the first jig member 401 becomes stronger, and the dam material 107 is separated from the narrow frame display module 400 while adhering to the first jig member 401.
[0044] In the case where the dam material 107 is allowed to remain in the housing of the final product as a design of the final product, the dam material 107 and the first jig member 401 can be separated by selecting a material with high releasability (for example, silicon or Teflon (registered trademark)) for the first jig member 401 or applying a release agent onto the first jig member 401, and the dam material 107 can be left in the housing of the final product. The dam material 107 is usually a material necessary for manufacturing to perform the dam & fill process, and does not affect the performance of the final product of the narrow frame display module 400. For this reason, the dam material 107 may or may not remain in the housing of the final product, and this is a matter that can be appropriately decided by the designer and is not limited in the first embodiment. In addition, the first jig member 401 and the second jig member 402 are separated at the same time. By making the first jig member 401 and the second jig member 402 separable, it is possible to obtain the effects that separation from the narrow-bezel display module 400 is significantly easier and cleaning of the adhesive is also easier.
[0045] As described above, according to the bonding method of the first embodiment, the dam-and-fill method can be implemented even for display components with narrow frames, and there is an effect that a highly reliable product can be obtained.
[0046] (Embodiment 2) Next, a second embodiment of the bonding method according to the present disclosure will be described with reference to Figs. 7 to 9. Fig. 7 is a schematic cross-sectional view showing an example of the penetration of a filler into a narrow frame display module 400 according to the first embodiment. Fig. 8 is a schematic cross-sectional view showing an example of a basic structure of a narrow frame display module according to the second embodiment. Fig. 9 is a schematic cross-sectional view showing an example of a basic structure of a narrow frame display module according to a modified example of the second embodiment. In the description of Figs. 7 to 9, elements that overlap with the description of Figs. 1 to 6 are given the same reference numerals, and the description is simplified or omitted, and only different contents will be described.
[0047] First, with reference to FIG. 7, a phenomenon that may occur when further improvements to the bonding method according to the first embodiment are considered will be described.
[0048] The bonding method according to the first embodiment includes a step of applying filler material 106 after applying dam material 107 (see step 2). When filler material 106 is applied around dam material 107, there is a possibility that filler material 106 will drip into gap 701 between display device 103 and first jig member 401 due to capillary action, and will also permeate into gap 702 between display device 103 and second jig member 402.
[0049] This often depends on the viscosity of the filler 106. For example, the lower the viscosity of the filler 106, the higher the possibility of the above-mentioned phenomenon of penetration occurring. When this phenomenon of penetration occurs, in the final process of separating the first jig member 401 and the second jig member 402 from the narrow frame display module 400, the surface tension of the filler 106 makes it difficult to separate the first jig member 401 and the second jig member 402 from the narrow frame display module 400, and there is a possibility that an external load is applied to the narrow frame display module 400 during separation. In particular, many of the components that make up today's narrow frame displays are thin, and have a structure that is easily damaged by external loads.
[0050] In the following second embodiment, therefore, a structural example will be described that makes it difficult for the above-mentioned decrease in permeation to occur in a narrow-frame display module manufactured based on the bonding method according to the first embodiment.
[0051] 5. Detailed procedure of the dam and fill construction method according to the second embodiment The detailed steps of the dam-and-fill construction method according to the embodiment 2 are almost the same as those of the dam-and-fill construction method according to the embodiment 1. The following will describe in detail the differences from the embodiment 1.
[0052] The narrow frame display module 500 shown in Fig. 8 is composed of a front panel 101, a display device 103, a polarizing plate 105, a filter material 106, and a dam material 107. The dam material 107 may be omitted. Also in the narrow frame display module 500, similar to the structural example of Fig. 3 or Fig. 4, the frame width 201 of the silk screen printing unit 102 and the frame width of the frame portion 202 of the display device 103 are narrower than those of the narrow frame display module 200 of Fig. 2.
[0053] In the second embodiment, unlike the first embodiment, a liquid pool 801 is provided in the second jig member 402. The liquid pool 801 can be provided as a recess formed by cutting out a part of the second jig member 402 in a quadrangular prism shape in a plan view.
[0054] In the example of FIG. 8, the liquid pool 801 is provided by carving into the second jig member 402. The liquid pool 801 is preferably provided in an area close to the outer peripheral end side of the display device 103, for example. With this configuration, the fill material 106 that has flowed down the gap 701 between the display device 103 and the first jig member 401 can be accumulated in the liquid pool 801. Therefore, the liquid pool 801 functions as a structure that blocks the fill material 106, and can prevent the fill material 106 from flowing into the gap 702 between the display device 103 and the second jig member 402. This makes it possible to remove the display device 103 without applying an external load to the first jig member 401 and the second jig member 402 in the removal process (see step 4) of the first jig member 401 and the second jig member 402.
[0055] 8, the narrow frame display module 600 shown in Fig. 9 is configured with a front panel 101, a display device 103, a polarizing plate 105, a filter material 106, and a dam material 107. The dam material 107 may be omitted. Also in the narrow frame display module 600, similar to the structural example of Fig. 3 or Fig. 4, the frame width 201 of the silk screen printing unit 102 and the frame width of the frame portion 202 of the display device 103 are narrower than those of the narrow frame display module 200 of Fig. 2.
[0056] Furthermore, the liquid pool according to the second embodiment is not limited to the example shown in FIG. 8, and may be provided in a manner similar to liquid pool 901 shown in FIG.
[0057] 9, a plurality of steps (for example, two steps on each of the left and right sides) are formed in the second jig member 402, and the first jig member 401 is placed on the surface of the outermost step (i.e., the lowest step), with the inner step portion serving as the liquid pool 901. The structural example of FIG. 9 also has the effect of preventing the filler material 106 that has flowed down the gap 701 between the display device 103 and the first jig member 401 from flowing into the gap 702 between the display device 103 and the second jig member 402, and it becomes possible to remove the display device 103 without applying an external load to the first jig member 401 and the second jig member 402 in the removal process (see step 4).
[0058] As described above, the bonding process according to the second embodiment has the effect of suppressing defects caused by external loads in the manufacturing process.
[0059] (Embodiment 3) Next, a bonding method according to a third embodiment of the present disclosure will be described with reference to Figs. 10 to 12. Fig. 10 is a schematic cross-sectional view of a display device having a warped shape at one end side in the narrow frame display module 400 according to the first embodiment when the display device is bonded by a dam-and-fill method. Fig. 11 is a schematic cross-sectional view showing a measurement example of a difference in height. Fig. 12 is a schematic cross-sectional view showing an example of a basic structure of a narrow frame display module 700 according to the third embodiment. In the description of Figs. 10 to 12, elements that overlap with the description of Figs. 1 to 9 are given the same reference numerals, and the description is simplified or omitted, and only different contents will be described.
[0060] First, referring to Fig. 10, a phenomenon that may occur when further improvements to the bonding method according to the embodiment 1 are considered will be described. For example, when using the bonding method according to the embodiment 1, there is a possibility that a display device 103 with one end warped may be used. This is due to, for example, manufacturing variations in the display device 103, and can be said to be an unavoidable problem.
[0061] 10, when one end of the display device 103 is warped, the height of the dam material 107 is set to a predetermined height depending only on the heights of the second jig member 402 and the first jig member 401. For this reason, a phenomenon occurs in which the thickness h1 of the adhesive layer (dam material 107, filler material 106) at the warped end (right side) is thinner than the thickness h2 of the adhesive layer (dam material 107, filler material 106) at the other end (left side) that is not warped.
[0062] The direct bonding technique, particularly the dam and fill method, has the advantage that it is possible to control the thickness of the adhesive layer, form a thick adhesive layer, and achieve highly reliable adhesion. However, if the adhesive layer is partially thin, this leads to reduced reliability. Therefore, when bonding a warped display device 103, using the bonding method according to the first embodiment has disadvantages.
[0063] Therefore, in the following third embodiment, an example will be described in which this disadvantage is solved and an adhesive layer having a predetermined thickness is formed over the entire outer side surface of the display device 103 even when a warped display device 103 is used.
[0064] 6. Detailed procedure of the dam and fill construction method according to the third embodiment The detailed steps of the dam-and-fill construction method according to the embodiment 3 are almost the same as those of the dam-and-fill construction method according to the embodiment 1. The following will describe in detail the differences from the embodiment 1.
[0065] 11, display device 103 has a portion that is partially warped and deformed at one end side. In this state, display device 103 is attached to first jig member 401 and second jig member 402, as in embodiment 1. In embodiment 3, a displacement meter 1101 is disposed to measure the height of both top surface 1105 of the end of display device 103 and top surface 1106 of first jig member 401 in this state. Note that the height referred to here indicates, for example, the height from the bottom surface of second jig member 402.
[0066] The displacement meter 1101 is preferably a non-contact type such as a laser displacement meter. For example, in the case of a laser displacement meter, the height of the upper surface 1105 of the end of the display device 103 is measured based on the time sum of the forward and backward passes of the laser light 1103 irradiated from the displacement meter 1101 and the speed of the laser light 1103. Similarly, the height of the upper surface 1106 of the first jig member 401 is measured based on the time sum of the forward and backward passes of the laser light 1104 irradiated from the displacement meter 1101 and the speed of the laser light 1104. This makes it possible to derive information on the difference in height (thickness h3) between one end of the partially warped display device 103 and the first jig member 401.
[0067] In addition, in place of the laser displacement meter, a contact type displacement meter or the like may also be used, but the displacement measuring means is not limited in the third embodiment.
[0068] Moreover, the third embodiment is characterized in that the difference in height (thickness h1) between the display device 103 and the first jig member 401 is reflected in the setting of the height of the dam material 107 to be applied subsequently. In other words, if the difference in height is large, feedback is applied such that the dam material 107 on one end side of the partially warped part of the display device 103 is applied higher by the difference in height (thickness h3) than the height (predetermined set value) of the dam material 107 on the warped side.
[0069] In the dam and fill method, the dam material 107 is usually applied from a dispenser, but by increasing the amount of material dispensed by the dispenser or slowing down the moving speed of the dispenser, it is possible to construct a higher dam. The applied and laminated structure is shown in Figure 12.
[0070] 12, the dam material 107a on the right side is applied higher than the dam material 107 on the left side by the difference in height (thickness h3) between the display device 103 and the first jig member 401. This makes it possible to form a thick adhesive layer even in the right end area 1201, thereby achieving the effect of improving the reliability of the product.
[0071] As described above, the bonding method according to the third embodiment makes it possible to adjust the heights of the dam materials used in the dam-and-fill method to be the same or different, taking into account the warpage of the display device 103. This solves the problem of the adhesive layer becoming thinner due to the warpage of the display device 103, and ultimately makes it possible to provide a highly reliable bonding structure, which is a feature of the dam-and-fill method.
[0072] As described above, the present disclosure discloses the following technical ideas.
[0073] <Technology 1> A bonding method for bonding a front panel (101) and a display device (103) that are rectangular in plan view with adhesive (107, 106), a first jig member (401) arranged in contact with the four peripheral sides of the display device is placed on a second jig member (402) arranged on the rear surface of the display device and having an area larger than that of the display device; Applying a first adhesive (107) to an upper portion of the first jig member and surrounding a periphery of the display device; a second adhesive (106) is filled inside the first adhesive and between the display device and the front panel; hardening the first adhesive and the second adhesive, and removing the first jig member and the second jig member after the hardening; Bonding method.
[0074] As a result, the bonding method makes it possible to perform dam and fill bonding even in display modules with narrow frames where there is no space to apply dam material, making it possible to ensure the quality and high reliability of the adhesive layer after bonding.
[0075] <Technology 2> the front panel has a transmissive portion (109) that allows an image from the display device to be viewed, and a non-transmissive portion (102) that is provided around the transmissive portion and has a width smaller than that of the transmissive portion; The first adhesive bonds an upper portion of the first jig member and a lower portion of the non-transparent portion. The bonding method described in Technology 1.
[0076] As a result, the lamination method makes it possible to stably form a high-quality adhesive layer between the front panel and the display device even as the frame of the front panel becomes narrower.
[0077] <Technology 3> The first jig member is in contact with the display device without any gap. The bonding method according to Technology 1 or 2.
[0078] As a result, the lamination method can prevent the filler material from dripping into spaces between the display device and the first and second jig members.
[0079] <Technology 4> a polarizing plate having an area larger than an area of the image display area of the display device is placed on an upper surface of the image display area of the display device; an upper surface of the first jig member is lower than an upper surface of the image display area of the display device on which the polarizing plate is placed; The lamination method according to any one of Techniques 1 to 3.
[0080] This allows the lamination method to provide stable hardening of the filler material when exposed to UV light from the side.
[0081] <Technology 5> a liquid pool portion (801, 901) that blocks the second adhesive from flowing onto a bottom surface of the display device is provided on the end side of the display device and on the second jig member; 5. The bonding method according to claim 1.
[0082] This makes it possible to prevent the second adhesive (that is, the filler material 106) from flowing onto the bottom surface of the display device 103 when using the bonding method.
[0083] <Technology 6> measuring a first height indicating a height of an upper surface of an end portion of the display device and a second height indicating a height of an upper surface of the first jig member; deriving a difference between the first height and the second height, and setting the derived difference value as at least one height of the first adhesive; 6. The bonding method according to claim 1 .
[0084] As a result, with the bonding method, even if the display device 103 is partially warped and deformed, the thickness of the adhesive layer can be kept approximately constant over the entire display device 103, and deterioration of product reliability can be suppressed.
[0085] <Technology 7> The first adhesive is a dam material and the second adhesive is a fill material. 7. The bonding method according to claim 1.
[0086] As a result, the lamination method can utilize the well-known dam-and-fill method and achieve a high-quality adhesive layer.
[0087] Although various embodiments have been described above with reference to the accompanying drawings, the present disclosure is not limited to such examples. It is clear that a person skilled in the art can conceive of various modifications, corrections, substitutions, additions, deletions, and equivalents within the scope of the claims, and it is understood that these also belong to the technical scope of the present disclosure. In addition, the components in the various embodiments described above may be arbitrarily combined within the scope of the invention. [Industrial Applicability]
[0088] The present disclosure is applicable to bonding a narrow-frame type front panel (for example, a cover glass or a touch panel) and a display device (for example, a liquid crystal module) that has almost no space for applying a dam material. [Explanation of symbols]
[0089] 100 Display Module 101 Front Panel 102 Silk Printing Department 103 Display Devices 104 Active Area 105 Polarizing Plate 106 Filling material 107 Dam material 108 Bezel material 109 Transparent part 200 Narrow Bezel Display Module 201 Frame width 202 Frame section 300 Narrow Bezel Display Module 400 Narrow Bezel Display Module 401 First jig member 402 Second jig member 403 Upper surface of first jig member 404 Top surface 500 Narrow Bezel Display Module 501 Front UV curing equipment 502 Side UV curing equipment 701 Gap 702 Gap 801 Liquid pool 901 Liquid pool 1001 Adhesive layer thickness 1101 Displacement meter 1102 Height difference between the edge of the display device and the first jig member 1103 Laser light 1104 Laser light 1105 Top surface of display device edge 1106 Upper surface of first jig member 1201 Display module right end area
Claims
1. A bonding method for bonding a front panel and a display device, which are rectangular in plan view, with an adhesive, comprising the steps of: a first jig member arranged in contact with the four peripheral sides of the display device is arranged on a second jig member arranged on the rear surface of the display device and having an area larger than an area of the display device; Applying a first adhesive to an upper portion of the first jig member and surrounding a periphery of the display device; a second adhesive is filled inside the first adhesive and between the display device and the front panel; hardening the first adhesive and the second adhesive, and removing the first jig member and the second jig member after the hardening; Bonding method.
2. the front panel has a transmissive portion that allows an image from the display device to be viewed, and a non-transmissive portion that is provided around the transmissive portion and has a width smaller than a width of the transmissive portion; The first adhesive bonds an upper portion of the first jig member and a lower portion of the non-transparent portion. The bonding method according to claim 1 .
3. The first jig member is in contact with the display device without any gap. The bonding method according to claim 1 .
4. a polarizing plate having an area larger than an area of the image display area of the display device is placed on an upper surface of the image display area of the display device; an upper surface of the first jig member is lower than an upper surface of the image display area of the display device on which the polarizing plate is placed; The bonding method according to claim 1.
5. a liquid pool portion is provided on the end portion of the display device and on the second jig member to prevent the second adhesive from flowing onto a bottom surface of the display device; The bonding method according to claim 1 .
6. measuring a first height indicating a height of an upper surface of an end portion of the display device and a second height indicating a height of an upper surface of the first jig member; deriving a difference between the first height and the second height, and setting the derived difference value as at least one height of the first adhesive; The bonding method according to any one of claims 1 to 5.
7. The first adhesive is a dam material and the second adhesive is a fill material. The bonding method according to claim 1 .
Citation Information
Patent Citations
Manufacturing method for organic el display device
JP2015079580A