Manufacturing method of multilayer film for recording / reproducing and manufacturing device for multilayer film for recording / reproducing

The described method efficiently manufactures multilayer films for recording and reproduction by using UV curable resin, a polygonal roller, and laminating techniques, addressing material limitations and equipment challenges of previous methods.

JP2024159982AActive Publication Date: 2024-11-08PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2024150746
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2020-01-27
Filing Date
2024-09-02
Publication Date
2024-11-08
Estimated Expiration
2040-11-17

AI Technical Summary

Technical Problem

Existing methods for manufacturing multilayer films for recording and reproduction, such as co-extrusion and repeated coating and curing, are limited by narrow material selection and require large equipment, making them costly and difficult to scale efficiently.

Method used

A method involving a coating step with ultraviolet curable resin, a drying step, a winding step using a polygonal roller, and UV irradiation to laminate layers efficiently, along with a laminating roller to apply pressure and a separator arrangement to manage layer separation.

Benefits of technology

This approach allows for the efficient production of multilayer films with improved material selection and reduced equipment requirements, enabling cost-effective manufacturing of high-capacity optical disks.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024159982000001_ABST
    Figure 2024159982000001_ABST
Patent Text Reader

Abstract

To provide a manufacturing method of multilayer films for recording / reproducing and a manufacturing device for multilayer films for recording / reproducing for efficiently manufacturing multilayer films for recording / reproducing.SOLUTION: A manufacturing method of multilayer films for recording / reproducing includes: a coating process in which a liquid containing an ultraviolet-curing resin whose optical properties change when irradiated with light is applied to one surface of a film through which light passes; a drying process in which the liquid applied to the film by the coating process is dried; a winding process in which a coated film which is a film in which the liquid is coated after the drying process, is wound by rotating a polygonal roller whose cross-sectional shape perpendicular to the rotation axis is polygonal; an ultraviolet irradiation process in which the coated film wound around the polygonal roller is irradiated with ultraviolet light; and a laminating process in which a laminating roller is provided at the position where the coated film starts to be wound around the polygonal roller and a pressing force is applied in the direction toward the rotation axis against one side of the polygonal roller.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method and an apparatus for manufacturing a recording and reproducing multilayer film. [Background technology]

[0002] As a method for increasing the recording capacity of optical discs, a method has been proposed in which a laminated film is used in which multiple light-transmitting films (intermediate layers) and recording layers whose optical properties change when irradiated with light are alternately stacked.

[0003] Known methods for producing laminated films using a roll-to-roll (R2R) system include a co-extrusion method and a method of repeating coating and curing (Patent Documents 1 and 2). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Special Publication No. 2016-506589 [Patent Document 2] U.S. Patent No. 7,936,802 DISCLOSURE OF THEINVENTION [Problem to be solved by the invention]

[0005] However, the co-extrusion method can only use thermoplastic materials, and in addition, the solubility of the dye and the solubility of the two laminated materials must be taken into consideration. Therefore, the co-extrusion method has the problem that the range of material choices is very narrow.

[0006] In addition, although the method of repeating coating and drying allows for a wider range of material choices, it requires repeating coating and curing to create multiple layers, or preparing a large number of original rolls and bonding them together by roll lamination, etc. Therefore, the method of repeating coating and drying requires large equipment, and has the problem that it is very difficult to balance cost and yield.

[0007] An object of the present disclosure is to provide a technique for efficiently manufacturing a multilayer film for recording and reproducing. [Means for solving the problem]

[0008] A method for manufacturing a multilayer film for recording and playback according to one embodiment of the present disclosure includes a coating step of coating one side of a film through which light passes with a liquid that contains an ultraviolet curing resin and whose optical properties change when irradiated with light; a drying step of drying the liquid coated on the film by the coating step; a winding step of rotating a polygonal roller having a polygonal cross-sectional shape perpendicular to the rotation axis to wind up a coated film on which the liquid has been coated after the drying step; an ultraviolet irradiation step of irradiating ultraviolet light onto the coated film wound around the polygonal roller; and a lamination step of providing a laminating roller at a position where the coated film begins to be wound around the polygonal roller, and applying a pressing force in a direction toward the rotation axis to one side of the polygonal roller.

[0009] An apparatus for manufacturing a multilayer film for recording and playback according to one embodiment of the present disclosure includes a coating device that coats one side of a film through which light passes with a liquid that contains an ultraviolet-curing resin and whose optical properties change when irradiated with light; a drying device that dries the liquid applied to the film by the coating device; a polygonal roller that has a polygonal cross-sectional shape perpendicular to its axis of rotation and rotates to wind up a coated film that is a film coated with the liquid after drying by the drying device; an ultraviolet irradiation device that irradiates ultraviolet light onto the coated film wound around the polygonal roller; and a lamination roller that is provided at a position where the coated film begins to be wound around the polygonal roller and applies a pressing force in a direction toward the axis of rotation to one side of the polygonal roller. Effect of the Invention

[0010] According to the present disclosure, a multilayer film for recording and reproduction can be efficiently manufactured. [Brief description of the drawings]

[0011] [Figure 1]FIG. 1 is a diagram showing an example of the configuration of a manufacturing apparatus for a recording and reproducing multilayer film according to the first embodiment. [Diagram 2] FIG. 2 is a diagram showing an example of a method for manufacturing an optical disc. [Diagram 3] FIG. 3 is a diagram for explaining the cutting step. [Figure 4] FIG. 4 is a diagram for explaining the cutting step. [Diagram 5] FIG. 5 is a diagram for explaining the bonding step. [Figure 6] FIG. 6 is a diagram for explaining the recording process. [Figure 7] FIG. 7 is a diagram showing an example of the configuration of a manufacturing apparatus for a recording and reproducing multilayer film according to the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Hereinafter, the embodiments of the present disclosure will be described in detail with reference to the drawings as appropriate. However, more detailed description than necessary may be omitted. For example, detailed description of already well-known matters and duplicated description of substantially the same configuration may be omitted. This is to avoid the following description becoming unnecessarily redundant and to facilitate understanding by those skilled in the art. Note that the accompanying drawings and the following description are provided to enable those skilled in the art to fully understand the present disclosure, and are not intended to limit the subject matter described in the claims.

[0013] (Embodiment 1) <Production equipment configuration> 1 is a diagram showing a configuration example of a manufacturing apparatus for a recording and reproducing multilayer film (hereinafter simply referred to as a "manufacturing apparatus") according to embodiment 1. In the explanation of FIG. 1, for convenience, the direction from left to right in the drawing is expressed as the X-axis, the direction from bottom to top in the paper as the Y-axis, and the direction from the back to the front in the paper as the Z-axis.

[0014] The manufacturing apparatus 10 includes a film roller 20, a pretreatment apparatus 25, a coating apparatus 30, a drying apparatus 40, a laminating roller 50, a polygonal roller 60, an ultraviolet (UV) irradiation apparatus 70, and a separator placement apparatus 80.

[0015] Film roller 20 is a device on which an original roll of film 101 is set. Film 101 is a transparent thin film that transmits light, such as a PET (polyethylene terephthalate) film. Film 101 forms intermediate layer 121 in multilayer film 120 (see FIG. 5) for recording and reproducing optical discs. Film 101 has a thickness (thickness in the Y-axis direction) of, for example, 10 μm or less.

[0016] The film roller 20 constitutes a roll-to-roll (R2R) system together with the polygonal roller 60. That is, the film roller 20 rotates in accordance with the rotation of the polygonal roller 60, and the film 101 is pulled out from the original roll set on the film roller 20, and the pulled out film 101 is wound up by the polygonal roller 60 while maintaining a tensioned state.

[0017] Pretreatment device 25 is a device that performs a step of performing a UV ozone treatment and / or a plasma treatment on both sides of film 101 (hereinafter referred to as a "pretreatment step").

[0018] The coating device 30 is a device that performs a process of coating one side of the film 101 with the liquid adhesive 102 (hereinafter referred to as the "coating process"). For example, the coating device 30 applies the liquid adhesive 102 in a uniform film thickness by a die coating method to the upper surface (the surface in the positive direction of the Y axis) of the film 101 pulled out from the film roller 20. The coating device 30 applies the adhesive 102 in a film thickness of, for example, 10 μm or less. Hereinafter, the surface of the film 101 to which the adhesive 102 is applied may be referred to as the upper surface, inner surface, or coated surface, and the surface of the film 101 to which the adhesive 102 is not applied may be referred to as the lower surface, outer surface, or non-coated surface.

[0019] The adhesive 102 contains at least an ultraviolet (UV) curable resin and a material whose optical properties (e.g., reflectance or refractive index) change when irradiated with light. The material whose optical properties change when irradiated with light may be an organic colorant (dye) that is easily soluble in a solvent. The organic colorant may cause two-photon absorption. The adhesive 102 may contain a crosslinking agent and a photopolymerization initiator in addition to the above materials. The adhesive 102 forms a recording layer 122 in a multilayer film 120 for recording and reproducing optical discs (see FIG. 5).

[0020] The drying device 40 is a device that performs a process of drying the adhesive 102 applied to the film 101 (hereinafter referred to as the "drying process"). For example, the drying device 40 heats and dries the adhesive 102 on the film 101 after the application process. The heating temperature is, for example, 150 degrees or less. As a result, the solvent contained in the liquid adhesive 102 applied to the upper surface of the film 101 evaporates, the viscosity of the adhesive 102 increases, and the thickness of the adhesive 102 decreases. The thickness of the adhesive 102 after the drying process is, for example, 1 μm or less. In other words, the drying device 40 dries the adhesive 102 on the upper surface of the film 101 so that the thickness of the adhesive 102 after the drying process is 1 μm or less. Hereinafter, the film 101 and the adhesive 102 applied to the upper surface of the film 101 after the drying process are collectively referred to as the applied film 103.

[0021] The polygonal roller 60 is a device that performs a step of winding up the coating film 103 (hereinafter referred to as the "winding step"). The polygonal roller 60 is a roller that has a rotation axis 61 parallel to the Z axis and has a polygonal cross section perpendicular to the rotation axis 61. That is, the three-dimensional shape of the polygonal roller 60 is a shape of a prism that has been turned on its side. Hereinafter, when the polygonal roller 60 is considered as a prism, each side surface (surfaces parallel to the Z axis) is referred to as a plate 62, and the boundary line (side parallel to the Z axis) between adjacent side surfaces is referred to as an edge 63. In other words, the side connecting the vertices of the opposing bottom surfaces of the prism is referred to as an edge 63. In this embodiment, as shown in FIG. 1, an example of the polygonal roller 60 having a hexagonal cross section (i.e., a hexagonal prism) will be described, but the cross section of the polygonal roller 60 may be any polygonal shape. It is preferable that the cross section of the polygonal roller 60 is a regular polygon.

[0022] The polygonal roller 60 rotates around a rotation axis 61, and winds up the coating film 103 after the drying process. As the polygonal roller 60 winds up the coating film 103, the coating film 103 is laminated on each plate 62 of the polygonal roller 60. For example, when the polygonal roller 60 rotates 20 times, 20 layers of the coating film 103 are laminated on each plate 62. In other words, 20 pairs of the intermediate layer 121 and the recording layer 122 are laminated. Hereinafter, the coating film 103 laminated is referred to as a laminated film 104.

[0023] The length of one side of the polygon of polygonal roller 60 is equal to or greater than the diameter 2r of the optical disc (see FIG. 4). In addition, the length of edge 63 of polygonal roller 60 is equal to or greater than the diameter 2r of the optical disc. This is because, as will be described later, in the cutting process, laminated film 104 formed on each plate 62 of polygonal roller 60 is cut into a circle with the same diameter 2r as the optical disc to obtain circular laminated film 106 (see FIG. 4).

[0024] 1 and 3, the polygonal roller 60 may have gaps 64 of a predetermined width formed along the edge 63 from the vertices of the polygon toward the rotation axis 61. As a result, in a cutting process, as described below, by inserting a blade into the gap 64 and moving the blade along the edge 63, the laminate film 104 can be removed from the polygonal roller 60 and the roll of laminate film 104 wound around the polygonal roller 60 can be divided into laminate films 104 for each plate 62 (see FIG. 4).

[0025] The laminating roller 50 is a device that performs a process of applying pressure to the coating film 103 newly wound around the polygonal roller 60 (hereinafter referred to as the "laminating process"). For example, the laminating roller 50 is provided at a position where the new coating film 103 starts to be wound around the polygonal roller 60, and applies a pressing force to one side (plate 62) of the polygonal roller 60 in a direction toward the rotation axis 61 of the polygonal roller 60 (upward in FIG. 1 (positive direction of the Y axis)). The rotation axis of the laminating roller 50 can move in a direction (upward and downward in FIG. 1 (Y axis direction)) toward or away from the rotation axis 61 of the polygonal roller 60 according to the rotation of the polygonal roller 60. This makes it possible to prevent gaps and air bubbles from occurring between the outer surface of the coating film 103 previously wound around the polygonal roller 60 and the inner surface of the coating film 103 newly wound around the polygonal roller 60 (i.e., wound on the outermost side). That is, the coating films 103 are stacked closely together with no gaps.

[0026] The UV irradiation device 70 is a device that performs a step of irradiating ultraviolet (UV) rays onto the coated film 103 wound around the polygonal roller 60 (hereinafter referred to as the "UV irradiation step"). For example, the UV irradiation device 70 irradiates UV onto the coated film 103 wound around the polygonal roller 60 after it has been pressed by the laminating roller 50. This causes the UV curable resin contained in the adhesive 102 on the inner surface of the coated film 103 that has been newly wound around the polygonal roller 60 (i.e., the outermost one) to harden and adhere to the outer surface of the coated film 103 previously wound around the polygonal roller 60. That is, the stacked coated films 103 are fixed together.

[0027] The separator placement device 80 is a device that performs a step of placing a separator 105 on the upper surface of the coating film 103 every time the polygonal roller 60 rotates a predetermined number of times (hereinafter referred to as the "separator placement step"). The separator 105 is a sheet of a material that does not adhere to either the adhesive 102 or the film 101, such as a paper sheet. The length of the separator 105 in the X-axis direction is, for example, equal to or greater than the perimeter of the polygon of the polygonal roller 60.

[0028] For example, when the polygonal roller 60 has rotated a predetermined number of times, the separator arrangement device 80 arranges the separator 105 on the upper surface of the coated film 103 after the drying process and before it is taken up by the polygonal roller 60. The separator 105 arranged on the upper surface of the coated film 103 is taken up by the polygonal roller 60 together with the coated film 103 by the rotation of the polygonal roller 60. As a result, even if the UV irradiation process 205 is performed on the newly taken up coated film 103 together with the separator 105 and the adhesive 102 on the upper surface of the coated film 103 is cured, the inner surface of the coated film 103 does not adhere to the outer surface of the separator 105 taken up together with it. Therefore, the separator placement device 80 places a separator 105 every time the polygonal roller 60 rotates the number of times equal to the desired number of layers in the laminated film 104, so that the roll of the laminated film 104 can be separated into a predetermined number of layers without cutting the film 101 midway through R2R. That is, a plurality of laminated films 104 with the desired number of layers can be obtained from each plate 62.

[0029] <Optical disc manufacturing method> FIG. 2 is a diagram showing an example of a method for manufacturing an optical disc.

[0030] The manufacturing method of the recording and reproducing multilayer film 120 includes a pretreatment step 200, a coating step 201, a drying step 202, a winding step 203, a laminating step 204, a UV irradiation step 205, a separator arrangement step 206, and a cutting step 207. However, this manufacturing method is only an example, and at least one of these steps may be omitted when manufacturing the recording and reproducing multilayer film 120.

[0031] In the method for manufacturing an optical disc, the recording and reproducing multilayer film 120 manufactured by the above-mentioned manufacturing method is further subjected to a cutting step 208 and a bonding step 209. These steps will be described in detail below.

[0032] <<Pretreatment process>> In the pretreatment process 200, the film 101 is subjected to a double-sided UV ozone treatment and / or a plasma treatment, etc. This modifies the surface of the film 101, and can improve the coatability in the coating process 201 and the adhesion in the UV irradiation process 205.

[0033] <<Coating process>> In the coating process 201, the coating device 30 applies liquid adhesive 102 to the upper surface of the film 101, which has been pulled out from the film roller 20 and maintained in a taut state, by a die coating method so as to have a uniform film thickness of, for example, 10 μm or less. As a result, the adhesive 102 is applied to the upper surface of the film 101 in a uniform film thickness.

[0034] <<Drying process>> In the drying step 202, the drying device 40 heats and dries the adhesive 102 applied to the upper surface of the film 101 in the application step 201 so as to have a uniform film thickness of, for example, 1 μm or less, to obtain a coated film 103. The temperature for heating and drying is, for example, 150° C. or less. This causes the solvent contained in the adhesive 102 applied to the upper surface of the film 101 to evaporate, increasing the viscosity of the adhesive 102 and reducing the film thickness of the adhesive 102.

[0035] <<Winding process>> In the winding step 203, the polygonal roller 60 rotates to wind up the coated film 103 after the drying step 202 while maintaining the tension state of the film 101 by R2R. As a result, one layer of the coated film 103 is laminated on each plate 62 of the polygonal roller 60 every time the polygonal roller 60 rotates once. That is, the number of layers of the coated film 103 corresponding to the number of rotations of the polygonal roller 60 are laminated on each plate 62 of the polygonal roller 60. Therefore, the laminated film 104 with the number of layers corresponding to the number of rotations of the polygonal roller 60 can be easily produced.

[0036] In FIG. 1, the film roller 20 and the polygonal roller 60 both rotate counterclockwise. However, the rotation directions of the film roller 20 and the polygonal roller 60 can be in any direction as long as R2R can be achieved.

[0037] <<Lamination Process>> In the lamination process 204, the lamination roller 50 applies a pressing force to the outermost coated film 103 wound around the polygonal roller 60 by the winding process 203. This prevents the generation of gaps and air bubbles between the outer surface of the coated film 103 previously wound around the polygonal roller 60 and the inner surface of the coated film 103 newly wound around the polygonal roller 60 (i.e., the outermost wound). That is, the coated films 103 are laminated precisely without gaps.

[0038] <<UV Irradiation Process>> In the UV irradiation process 205, the UV irradiation device 70 irradiates UV on the coated film 103 after the lamination process 204 wound around the polygonal roller 60. As a result, the UV curable resin contained in the adhesive 102 on the inner surface of the coated film 103 newly wound around the polygonal roller 60 (i.e., the outermost wound) cures and adheres to the outer surface of the coated film 103 previously wound around the polygonal roller 60. That is, the laminated coated films 103 are fixed. Note that the UV irradiation process 205 may be performed at any position while the coated film 103 newly wound around the polygonal roller 60 makes one full rotation.

[0039] <<Separator Placement Process>> In the separator arrangement step 206, the separator arrangement device 80 arranges a separator 105 on the upper surface of the coated film 103 after the drying step 202 and before it is taken up by the polygonal roller 60 every time the polygonal roller 60 rotates a predetermined number of times (when the determination 221 in FIG. 2 is YES). As a result, the separator 105 arranged on the upper surface of the coated film 103 is taken up by the polygonal roller 60 together with the coated film 103 by further rotation of the polygonal roller 60. Therefore, even if the UV irradiation step 205 is performed on the coated film 103 newly taken up together with the separator 105 and the adhesive 102 on the inner surface of the coated film 103 is cured, the inner surface of the coated film 103 does not adhere to the outer surface of the separator 105 taken up together with it. Therefore, the separator placement device 80 places a separator 105 each time the polygonal roller 60 rotates a number of times equal to the desired number of layers in the laminated film 104, thereby making it possible to obtain the desired number of layers of the laminated film 104 from each plate 62 without cutting the film 101 midway through R2R.

[0040] For example, if a 20-layer recording / reproducing multilayer film 120 is desired, the separator arrangement step 206 is performed every 20 rotations of the polygonal roller 60. As a result, a separator 105 is sandwiched between every 20 layers of the roll of laminated film 104 wound around the polygonal roller 60 after completion of R2R. Therefore, in a cutting step 207 described later, when the roll of laminated film 104 wound around the polygonal roller 60 is cut in the Z-axis direction along the edge 63, the laminated film 104 formed on each plate 62 is separated into 20 layers by the separator 105. In other words, a plurality of 20-layer laminated films 104 can be obtained from one plate 62.

[0041] <<Cutting process>> FIG. 3 is a diagram for explaining the cutting step 207. As shown in FIG.

[0042] The cutting step 207 is performed after the winding by the polygonal roller 60 is completed (when the determination 222 in FIG. 2 is YES). In the cutting step 207, a blade is passed through a gap 64 formed along the edge 63 from the apex of the polygon toward the rotation axis 61, as shown by the dotted line 66 in FIG. 3, and the roll of laminated film 104 wound around the polygonal roller 60 is cut in the Z-axis direction along the edge 63 of the polygonal roller 60. This allows the laminated film 104 to be removed from the polygonal roller 60, and also allows flat laminated film 104 to be obtained from each plate 62 of the polygonal roller 60.

[0043] Furthermore, when the separator 105 is sandwiched, the laminated film 104 on each plate 62 after the cutting process 207 is separated by the separator 105. For example, when the separator 105 is sandwiched every 20 layers, a plurality of 20-layer laminated films 104 can be obtained on each plate 62 of the polygonal roller 60.

[0044] <<Cutting process>> FIG. 4 is a diagram for explaining the cut-out step 208. As shown in FIG.

[0045] 4, in the cut-out process 208, the laminate film 104 obtained from each plate 62 of the polygonal roller 60 after being cut in the cutting process 207 is cut into a circle having a diameter 2r, the same as that of an optical disc. The circular laminate film 104 obtained in the cut-out process 208 is called a circular laminate film 106. In the cut-out process 208, a plurality of circular laminate films 106 may be cut out from one laminate film 104.

[0046] <<Attachment process>> FIG. 5 is a diagram for explaining the pasting step 209. As shown in FIG.

[0047] In the lamination step 209, as shown in Fig. 5, the circular laminated film 106 (i.e., the recording and reproducing multilayer film 120) is laminated to the substrate 110 with guide tracks. The guide tracks are projections and recesses for guiding the recording and reproducing light irradiated onto the optical disc. The substrate 110 with guide tracks may be made of, for example, a plastic material or glass, and from the viewpoint of cost, it is preferable to use a plastic material. The plastic material may be, for example, a polycarbonate resin, a polyolefin resin, an acrylic resin, or the like.

[0048] Additionally, in the bonding step 209, a transparent protective layer 130 that transmits light may be formed on the circular laminated film 106. The material of the protective layer 130 may be a resin such as a photocurable resin (particularly an ultraviolet-curable resin) or a slow-acting thermosetting resin. The cover layer 133 may have low optical absorption for the laser light used. The cover layer 133 may be formed using a resin such as polycarbonate, amorphous polyolefin, or polymethyl methacrylate (PMMA), or glass.

[0049] By this bonding step 209, an optical disk is manufactured in which the circular laminated film 106 (that is, the recording / reproducing multilayer film 120) is bonded to the substrate 110 with guide tracks.

[0050] <Recording process> Fig. 6 is a diagram for explaining the recording process. By carrying out the recording process on the optical disc (see Fig. 5) manufactured by the process of Fig. 2, data can be recorded on each recording layer 122 of the optical disc. The recording process is carried out by, for example, a drive device for recording and reproducing.

[0051] In the recording process, as shown in Fig. 6, a desired recording layer 122 and a desired position among the multiple recording layers 122 of the optical disc are irradiated with light (e.g., blue light). This changes the optical characteristics (e.g., reflectance or refractive index) of the position irradiated with the light. The position where the optical characteristics change is called a recording mark 123.

[0052] As shown in FIG. 6, an optical disc manufactured by the manufacturing method of the present disclosure has a large number of recording layers 122, and therefore can record a large amount of data compared to a conventional optical disc having a small number of recording layers.

[0053] When reproducing data recorded on an optical disc, light (e.g., blue light) is irradiated onto a desired recording layer 122 and a desired position among the multiple recording layers 122 of the optical disc. Since optical characteristics (e.g., reflectance or refractive index) differ depending on whether or not a recording mark 123 is present at that position, it is possible to detect whether or not a recording mark 123 is present at that position by detecting the difference in optical characteristics for the irradiated light. This allows the data recorded on the recording layer 122 of the optical disc to be reproduced.

[0054] As described above, the manufacturing apparatus and method according to the first embodiment can efficiently manufacture the recording and reading multilayer film 120 having a desired number of layers. Also, the material selectivity for the recording layer 122 can be improved.

[0055] (Embodiment 2) In the first embodiment, a method for manufacturing laminated film 104 with a desired number of layers without cutting film 101 in the middle of R2R by arranging separator 105 is described. In the second embodiment, a manufacturing apparatus and a manufacturing method for manufacturing laminated film 104 with a desired number of layers by cutting coated film 103 in the middle of R2R without arranging separator 105 are described. In the second embodiment, the same reference symbols are used for components already described in the first embodiment, and descriptions thereof may be omitted.

[0056] <Production equipment configuration> FIG. 7 is a diagram showing an example of the configuration of a manufacturing apparatus according to the second embodiment. In FIG.

[0057] The manufacturing apparatus 10 includes a film roller 20, a pretreatment device 25, a coating device 30, a drying device 40, a guide roller 90, a laminating roller 50, a polygonal roller 60, and a UV irradiation device 70.

[0058] The film roller 20, the pretreatment device 25, the coating device 30, the drying device 40, the laminating roller 50, the polygonal roller 60, and the UV irradiation device 70 have been described in the first embodiment.

[0059] The guide roller 90 is a device that guides the conveyance of the coated film 103 to the polygonal roller 60 after the drying step 202. For example, the guide roller 90 holds the coated film 103 from above and below, and maintains the tension of the film 101. As a result, even if the coated film 103 is cut at the cutting position 91 between the guide roller 90 and the polygonal roller 60, the tension of the film 101 is maintained between the guide roller 90 and the film roller 20.

[0060] Therefore, when the desired number of layers of laminated film 104 has been wound around polygonal roller 60, coating film 103 is cut at cutting position 91, and the steps from cutting step 207 described in embodiment 1 onwards are carried out on laminated film 104 wound around polygonal roller 60, thereby manufacturing an optical disc having recording / reproducing multilayer film 120 with the desired number of layers. In addition, since the tension on film 101 is maintained between guide roller 90 and film roller 20, polygonal roller 60 can start to newly wind up coating film 103 cut at cutting position 91.

[0061] As described above, according to the manufacturing apparatus and manufacturing method of the second embodiment, a recording and reading multilayer film having a desired number of layers can be manufactured without arranging the separator 105.

[0062] (Manufacturing equipment control) The operation of each component of the manufacturing apparatus 10 described above may be controlled by a predetermined control device (not shown). For example, the control device includes a processor and a memory. The processor cooperates with the memory to control the operation of each component of the manufacturing apparatus 10 described above. For example, the processor reads out from the memory and executes a computer program that controls the operation of each component of the manufacturing apparatus 10 described above. The control device may be built into the manufacturing apparatus 10. Alternatively, the control device may be a device separate from the manufacturing apparatus 10, and control the manufacturing apparatus 10 through a predetermined communication network.

[0063] Summary of the Disclosure A method for manufacturing a recording / reproducing multilayer film (120) according to one embodiment of the present disclosure includes a coating step (201) of coating one side of a film (101) through which light passes with a liquid (102) containing an ultraviolet curing resin and changing its optical properties when irradiated with light, a drying step (202) of drying the liquid coated on the film (101) in the coating step (201), a winding step (203) of rotating a polygonal roller (60) having a polygonal cross section perpendicular to a rotation axis (61) to wind up a coated film (103) that is the film (101) coated with the liquid (102) after the drying step (202), and an ultraviolet irradiation step (205) of irradiating the coated film (103) wound around the polygonal roller (60) with ultraviolet light. The liquid (102) may contain an organic dye whose optical properties change when irradiated with light.

[0064] According to this manufacturing method, the coating film (103) newly wound (i.e., wound outermost) around the polygonal roller (60) is irradiated with ultraviolet light. As a result, the ultraviolet curing resin contained in the liquid (102) applied to one side of the coating film (103) is cured, and one side of the newly wound coating film (103) is bonded to the other side of the coating film (103) previously wound around the polygonal roller (60). Therefore, as the polygonal roller (60) rotates, multiple coating films (103) are stacked on the polygonal roller (60), forming a recording / reproducing multilayer film (120). That is, according to this manufacturing method, the recording / reproducing multilayer film (120) can be efficiently manufactured.

[0065] The above-mentioned method for producing the recording and reproducing multilayer film (120) may further include a separator arrangement step (206) of arranging a sheet-like separator (105) on the upper surface of the coated film (103) after the drying step (202) and before the winding step (203) every time the polygonal roller (60) rotates a predetermined number of times.

[0066] According to this manufacturing method, the separator (105) is wound up on the polygonal roller (60) together with the coating film (103) every time the polygonal roller (60) rotates a predetermined number of times. In this case, the ultraviolet curing resin contained in the liquid (102) applied to one side of the coating film (103) newly wound on the polygonal roller (60) is cured by irradiation with ultraviolet light, but does not adhere to the surface of the separator (105) wound together. Therefore, by setting the predetermined number of rotations of the polygonal roller (60) to the desired number of layers in the recording and reproducing multilayer film (120), the recording and reproducing multilayer film (120) with the desired number of layers can be efficiently manufactured without cutting the film (101) in the middle of R2R.

[0067] The polygonal roller (60) may have gaps (64) formed from the vertices of the polygon toward the rotation axis (61). The method for producing the recording / reproducing multilayer film (120) may further include a cutting step (207) of cutting the roll of the laminated film (104) on which the coating film (103) after the ultraviolet ray irradiation step (205) is laminated, wound around the polygonal roller (60), with a blade inserted into the gaps (64).

[0068] According to this manufacturing method, the laminated film (104) formed on each plate (62) of the polygonal roller (60) can be easily removed from the polygonal roller (60), and a flat laminated film 104 can be obtained from each plate (62).

[0069] A manufacturing apparatus (10) for a multilayer film (120) for recording and playback according to one embodiment of the present disclosure includes an application device (30) that applies a liquid (102) containing an ultraviolet-curable resin and having optical properties that change when irradiated with light to one side of a film (101) through which light passes, a drying device (40) that dries the liquid (102) applied to the film (101) by the application device, a polygonal roller (60) having a polygonal cross-sectional shape perpendicular to the rotation axis (61) and that rotates to wind up a coated film (103) that is the film (101) coated with the liquid (102) after drying by the drying device (40), and an ultraviolet irradiation device (70) that irradiates ultraviolet rays to the coated film (103) wound around the polygonal roller (60).

[0070] According to this configuration, the coating film (103) newly wound (i.e., wound outermost) around the polygonal roller (60) is irradiated with ultraviolet light. As a result, the ultraviolet curable resin contained in the liquid (102) applied to one side of the coating film (103) is cured, and one side of the newly wound coating film (103) is bonded to the other side of the coating film (103) previously wound around the polygonal roller (60). Therefore, as the polygonal roller (60) rotates, multiple coating films (103) are stacked on the polygonal roller (60), forming a recording / reproducing multilayer film (120). That is, according to this configuration, the recording / reproducing multilayer film (120) can be efficiently manufactured.

[0071] The manufacturing apparatus (10) for the recording / reproducing multilayer film (120) described above may further include a film roller (20) on which the original roll of the film (101) is set. The film roller (20) and the polygonal roller (60) may form a roll-to-roll (R2R) configuration.

[0072] According to this configuration, the recording / reproducing multilayer film (120) can be efficiently manufactured by R2R.

[0073] Although the embodiments have been described above with reference to the accompanying drawings, the present disclosure is not limited to such examples. It is clear that a person skilled in the art can conceive of various modifications, corrections, substitutions, additions, deletions, and equivalents within the scope of the claims, and it is understood that these also belong to the technical scope of the present disclosure. In addition, the components in the above-mentioned embodiments may be arbitrarily combined within the scope of the invention. [Industrial Applicability]

[0074] The technique of the present disclosure is useful for producing a multilayer film for recording and reproduction. [Explanation of symbols]

[0075] 10. Manufacturing equipment for multi-layer films for recording and playback 20 Film Roller 25 Pretreatment Equipment 30 Coating equipment 40 Drying equipment 50 Laminating Roller 60 Polygonal Roller 61 Rotational axis 62 Plate 63 Edge 64 Gap 70 Ultraviolet (UV) irradiation device 80 Separator placement device 90 Guide roller 101 Film 102 Adhesive 103 Coated film 104 Laminated Film 105 Separator 106 Circular laminated film 110 Board with guide track 120 Multilayer film for recording and playback 121 Middle Class 122 Recording Layer 123 Record Mark 130 Protective layer 200 Pre-treatment process 201 Coating process 202 Drying process 203 Winding process 204 Lamination process 205 Ultraviolet (UV) irradiation process 206 Separator placement process 207 Cutting process 208 Cutting process 209 Attachment process

Claims

1. A coating process of coating one surface of a film through which light passes with a liquid that contains an ultraviolet curing resin and whose optical properties change when irradiated with light; a drying step of drying the liquid applied to the film in the application step; a winding step in which a polygonal roller having a polygonal cross section perpendicular to a rotation axis is rotated to wind up the coated film, which is the film coated with the liquid after the drying step; an ultraviolet ray irradiation step of irradiating the coated film wound around the polygonal roller with ultraviolet rays; and a lamination process of providing a lamination roller at a position where the coating film starts to be wound around the polygonal roller and applying a pressing force in a direction toward the rotation axis to one side of the polygonal roller. A method for manufacturing a multi-layer film for recording and reproducing.

2. The lamination roller is movable in a direction toward and away from the rotation axis. A method for producing the multi-layer film for recording and reproducing according to claim 1.

3. and a separator placement step of placing a sheet-like separator on the upper surface of the coated film after the drying step and before the winding step, every time the polygonal roller rotates a predetermined number of times.

3. A method for producing the multilayer film for recording and reproducing according to claim 1 or 2.

4. The polygonal roller has gaps formed from the vertices of the polygon toward the rotation shaft, A cutting step of cutting the roll of the laminated film on which the coating film is laminated after the ultraviolet ray irradiation step, wound around the polygonal roller, by inserting a blade through the gap, A method for producing the multilayer film for recording and reproducing according to any one of claims 1 to 3.

5. A coating device that coats a liquid, which includes an ultraviolet curing resin and whose optical properties change when irradiated with light, on one side of a film through which light passes; a drying device that dries the liquid applied to the film by the application device; a polygonal roller having a polygonal cross section perpendicular to a rotation axis, which rotates to wind up the coating film on which the liquid has been coated after drying by the drying device; an ultraviolet irradiation device that irradiates ultraviolet light onto the coating film wound around the polygonal roller; a lamination roller that is provided at a position where the coating film starts to be wound around the polygonal roller and applies a pressing force to one side of the polygonal roller in a direction toward the rotation axis, Manufacturing equipment for multi-layer films for recording and playback.

6. The lamination roller is movable in a direction toward and away from the rotation axis.

6. An apparatus for manufacturing a multi-layer film for recording and reproducing according to claim 5.

Citation Information

Patent Citations

  • Manufacture of recording medium and device thereof

    JP1996324849A

  • Method and apparatus for sticking of sheet to plate

    JP1997019904A

  • Method and apparatus for straightening perforated band like material

    JP2001286931A

  • Apparatus for producing transparent layer for optical information recording medium

    JP2006082050A

  • Elastic roller, method of manufacturing the same, fixing apparatus, and image forming apparatus

    JP2011021660A