Workpiece inspection method and device

The workpiece inspection method employs oblique illumination and FFT to detect and exclude laser-induced defects, ensuring precise processing conditions and preventing damage in workpieces like silicon wafers.

JP2024160046AActive Publication Date: 2024-11-11TOKYO SEIMITSU CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2024113254
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-07-16
Publication Date
2024-11-11
Estimated Expiration
2040-07-06

AI Technical Summary

Technical Problem

Laser processing in workpieces, such as silicon wafers, results in scattered light that causes defects like splash damage, which can harm the workpiece and devices formed on its surface, necessitating a method to accurately detect and suppress these defects.

Method used

A workpiece inspection method using oblique illumination and image processing techniques, including fast Fourier transform (FFT) and binarization, to detect and exclude laser-induced defects, allowing for precise setting of processing conditions.

Benefits of technology

Accurately detects minute defects caused by laser light scattering, enabling robust processing conditions to prevent damage and improve device quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024160046000001_ABST
    Figure 2024160046000001_ABST
Patent Text Reader

Abstract

To provide a workpiece inspection method and device capable of detecting a defect, generated by scattering etc., of laser light, precisely at low cost.SOLUTION: A workpiece inspection method comprises: an imaging process of using an imaging device (306) to capture an image of a workpiece (CW) within an inspection range after laser processing while obliquely lighting the workpiece; an image processing process of subjecting the image of the workpiece within the inspection range after the laser processing to fast Fourier transformation to extract high-frequency components, and then performing binarization processing; and a detecting process of detecting a processing-time defect, formed with scattered light or leakage light in the laser processing, from the image of the workpiece within the inspection range after the laser processing which has been processed through the image processing process.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a workpiece inspection method and apparatus and a workpiece machining method, and more particularly to a technique for cleaving a workpiece having a laser machining area therein. [Background technology]

[0002] Conventionally, there is known a laser dicing device that irradiates a laser beam along a processing line by focusing the beam inside a workpiece such as a silicon wafer, and forms a laser processing area that is a starting point for cutting inside the workpiece along the processing line. The workpiece with the laser processing area formed therein is then cut along the cutting line by a cutting process such as expanding or breaking, and divided into individual chips. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2018-064049 A Summary of the Invention [Problem to be solved by the invention]

[0004] When forming a laser processing area inside a workpiece, some of the laser light may be scattered in a sputter-like manner due to structures inside the workpiece (e.g., defects (e.g., scratches, voids, etc.), particles such as impurities, processing marks, cracks inside the workpiece caused by laser processing, etc.), or may leak out to the side opposite the incident surface of the laser light. Such scattered light can cause defects (e.g., point-like defects, hereinafter referred to as splash damage) inside the workpiece (see, for example, Patent Document 1). Splash damage can damage the workpiece and devices formed on the surface of the workpiece, reducing the quality of the devices, so there is a demand for suppressing its occurrence.

[0005] The present invention has been made in consideration of the above circumstances, and aims to provide a work inspection method and apparatus, and a work processing method, capable of accurately detecting defects caused by scattering of laser light, etc. [Means for solving the problem]

[0006] In order to solve the above problems, a work inspection method according to a first aspect of the present invention includes an imaging step of capturing an image of an inspection area of ​​a work after laser processing using an imaging device while obliquely illuminating the work; an image processing step of performing a fast Fourier transform on the image of the inspection area of ​​the work after laser processing and performing a binarization process; a detection step of detecting machining defects formed by scattered light or leakage light caused during laser processing from the image of the inspection area of ​​the work after laser processing that has been image-processed in the image processing step; and a setting step of setting machining conditions in accordance with the detection results of the machining defects.

[0007] A workpiece inspection method according to a second aspect of the present invention is the same as the first aspect, but uses a workpiece consisting of only a workpiece layer.

[0008] A work inspection method according to a third aspect of the present invention, in the first or second aspect, comprises the steps of: capturing an image of the inspection range of the work before laser processing using an imaging device while providing oblique illumination to the work; and performing a fast Fourier transform on the image of the inspection range of the work before laser processing and performing a binarization process. The detection step comprises the steps of detecting a defective portion in the inspection range of the work from the image of the inspection range of the work before laser processing; detecting defect candidates from the defects detected in the image of the inspection range of the work after laser processing; and identifying processing defects by excluding the defective portion, the laser processed area formed in the work by laser processing, and the shadow of the laser processed area from the defect candidates.

[0009] A workpiece processing method according to a fourth aspect of the present invention performs laser processing of a workpiece to be processed based on processing conditions set by the workpiece inspection method according to any of the first to third aspects.

[0010] A work inspection device according to a fifth aspect of the present invention includes an imaging device that captures an image of an inspection area of ​​a work after laser processing while illuminating the work from an oblique angle, an image processing unit that applies a fast Fourier transform to the image of the inspection area of ​​the work after laser processing and performs binarization processing, a detection unit that detects machining defects formed by scattered light or leakage light caused during laser processing from the image of the inspection area of ​​the work after laser processing that has been image-processed by the image processing unit, and a setting unit that sets machining conditions according to the detection results of the machining defects. Effect of the Invention

[0011] According to the present invention, by performing fast Fourier transform on images of the inspection area of ​​the workpiece before and after laser processing and performing binarization processing, it is possible to accurately detect minute defects caused by scattering of laser light, etc. [Brief description of the drawings]

[0012] [Figure 1] FIG. 1 is a diagram showing an outline of the configuration of a laser dicing device. [Diagram 2] FIG. 2 is a plan view and a cross-sectional view of a workpiece to be inspected when oblique illumination (dark-field illumination system) is used. [Diagram 3] FIG. 3 is a plan view and a cross-sectional view of a workpiece to be inspected when using coaxial epi-illumination (bright-field illumination system). [Figure 4] Figure 4 shows an image of the inspection workpiece captured using oblique illumination (dark-field illumination system). [Diagram 5] Figure 5 shows an image of the inspection workpiece captured using coaxial epi-illumination (bright-field illumination system). [Figure 6] FIG. 6 is an image obtained by capturing an image of the inspection workpiece CW. [Figure 7] FIG. 7 is an image showing the result of performing binarization processing on the original image of FIG. [Figure 8] FIG. 8 is an image showing the result of dynamic thresholding on the original image of FIG. [Figure 9]FIG. 9 is an image showing the result of dynamic thresholding on the original image of FIG. [Figure 10] FIG. 10 shows a captured image of the workpiece under inspection after FFT processing. [Figure 11] FIG. 11 is an image showing the extraction result of splash damage. [Figure 12] FIG. 12 is a flowchart showing a method for setting processing conditions for laser dicing. [Figure 13] FIG. 13 is a flowchart showing the process of detecting defects during machining. [Figure 14] FIG. 14 is a flowchart showing the process of evaluating defects during processing. [Figure 15] FIG. 15 is a flowchart showing the process of setting the processing conditions. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, preferred embodiments of a workpiece inspection method and apparatus and a workpiece machining method according to the present invention will be described with reference to the accompanying drawings.

[0014] In this embodiment, laser processing is performed on an inspection workpiece CW using a laser dicing device 10. Then, images of the inspection range of the inspection workpiece CW before and after processing (for example, the inside, surface (upper and lower surfaces) of the inspection workpiece CW, etc.) are used to distinguish and detect missing parts that exist before the laser processing from processing defects including splash damage caused by the laser processing.

[0015] Next, the processing conditions are evaluated based on the detection results of the defects during processing to determine whether or not the processing conditions need to be changed. If it is determined that the processing conditions need to be changed, the processing conditions are reset. This makes it possible to appropriately set the processing conditions for the workpiece W to be produced.

[0016] (Laser dicing equipment) First, the laser dicing apparatus 10 will be described with reference to Fig. 1. Fig. 1 is a diagram showing an outline of the configuration of the laser dicing apparatus 10.

[0017] As shown in the figure, the laser dicing apparatus 10 of this embodiment includes a work moving section 100, an optical system unit (laser engine) 400, a control section 12, etc. The optical system unit 400 includes a laser optical section 200 and an observation optical section 300.

[0018] The control unit 12 includes a CPU (Central Processing Unit), a memory, an input / output circuit unit, and the like, and controls the operation of each unit of the laser dicing apparatus 10.

[0019] The workpiece moving unit 100 includes a suction stage 102 that suction-holds the inspection workpiece CW and the workpiece W to be produced (hereinafter, these may be collectively referred to as the workpiece W), and an XYZθ table 104 that is provided on a main body base 106 of the laser dicing device 10 and that precisely moves the suction stage 102 in the XYZθ directions. The workpiece W is precisely moved in the XYZθ directions in the figure by this workpiece moving unit 100.

[0020] The workpiece W has a backgrind (BG) tape B having an adhesive attached to one surface of the front surface, and is placed on the suction stage 102 with the back surface facing upward.

[0021] The work W may be mounted on the suction stage 102 with a dicing sheet having an adhesive attached to one surface thereof and integrated with the frame via the dicing sheet. In this case, the work W is mounted on the suction stage 102 with the front surface facing upward. In the following description, the surface of the work W exposed to the optical system unit 400 side is referred to as the upper surface, and the surface to which the BG tape B is attached is referred to as the lower surface. The work W may be directly suctioned to the suction stage 102.

[0022] The laser optical unit 200 includes a laser oscillator 202, a collimator lens 204, a half mirror 206, a condenser lens (light-collecting lens) 208, and a driving means 210 for slightly moving the laser light in the Z direction relative to the workpiece W. As a light source for the laser oscillator 202, for example, a semiconductor laser excited Nd:YAG (Yttrium Aluminum Garnet) laser is used. The laser light oscillated from the laser oscillator 202 passes through an optical system including the collimator lens 204, the half mirror 206, and the condenser lens 208, and is then focused on an inspection range of the workpiece W. The Z-direction position of the focal point is adjusted by slightly moving the condenser lens 208 in the Z direction.

[0023] The observation optical unit 300 includes an observation light source 302, a condenser lens 304, an imaging device (camera, such as an IR (infrared) sensor or a CCD (Charge Coupled Device) camera) 306, an image processing unit 308, and a monitor 310. The control unit 12 and the observation optical unit 300 are an example of a work inspection device.

[0024] The observation light source 302 irradiates the workpiece W with approximately circular (ring-shaped) oblique illumination light (oblique illumination light) L1 from a position offset from the optical axis AX of the condensing lens 208. The observation light source 302 is a ring illumination unit having a plurality of lighting units arranged in a circular ring shape around the condensing lens 208. Here, as the plurality of lighting units, for example, LEDs (Light Emitting Diodes) or directional bullet-shaped LEDs or the like can be used.

[0025] In this embodiment, a ring illumination unit is used as the observation light source 302 for oblique illumination, but the present invention is not limited to this. For example, a ring illumination unit may be arranged around the workpiece W to irradiate the workpiece W with illumination light that is obliquely incident thereon, or the workpiece W may be obliquely illuminated with light converted into a ring shape using a conical lens or a light shielding plate having an annular opening.

[0026] When the workpiece W is obliquely illuminated using the observation light source 302, the light scattered by the workpiece W passes through the condenser lenses 208 and 304 and enters the camera 306 serving as observation means, which captures an image of the workpiece W. This captured image data is input to an image processing unit 308 and used for alignment of the workpiece W. In addition, this captured image data is displayed on a monitor 310 via the control unit 12.

[0027] The observation optical unit 300 is capable of capturing images of defects, including splash damage, in the inspection range of the workpiece W. In this case, the oblique illumination light L1 has a longer wavelength than visible light. When the workpiece W is a silicon wafer, for example, infrared light is used. The oblique illumination light L1 irradiated to the workpiece W passes through the inspection range of the workpiece W and is scattered by splash damage (see FIG. 2) on the lower surface of the workpiece W. This scattered light passes through condenser lenses 208 and 304 and enters a camera 306, which captures an image including defects in the inspection range of the workpiece W. In this captured image, areas other than the area where the defects, including splash damage, are formed (hereinafter referred to as background areas) are dark, and the defects, including splash damage, are white (dark-field illumination system). The dark-field illumination system will be described later with reference to FIGS. 2 to 5.

[0028] This captured image data is input to an image processing unit 308 and used to detect defects in the inspection range of the workpiece W. In addition, the image of the inspection range of the workpiece W is displayed on a monitor 310 together with the defect detection results. This allows the operator to check and correct the defect detection results while looking at the monitor 310.

[0029] In this embodiment, images including defects in the inspection range of the workpiece W are captured before and after processing to form a laser processing area using laser light. This makes it possible to distinguish and detect missing parts that exist before laser processing and processing defects including splash damage caused by laser processing.

[0030] In this embodiment, the image of the workpiece W is captured using the laser optical unit 200 and the observation optical unit 300, but the present invention is not limited to this. For example, an image of the inspection range of the workpiece W may be captured using the optical system and camera of a microscope installed for aligning the workpiece W.

[0031] When forming a laser processing area on the workpiece W, a laser beam L is emitted from a laser oscillator 202, and the laser beam L passes through an optical system including a collimator lens 204, a half mirror 206, and a condenser lens 208, and is then irradiated onto an inspection area of ​​the workpiece W. The Z-direction position of the focal point of the irradiated laser beam L is accurately set to a predetermined position within the inspection area of ​​the workpiece W by adjusting the Z-direction position of the workpiece W using the XYZθ table 104 and controlling the position of the condenser lens 208.

[0032] In this state, the XYZθ table 104 is fed for processing in the X direction, which is the dicing direction. As a result, one line of laser processing area R1 is formed in the inspection range of the workpiece W along the processing line CL1 of the workpiece W (see FIG. 2). Then, when one line of laser processing area R1 is formed along the processing line CL1, the XYZθ table 104 is indexed and fed one pitch in the Y direction, and a laser processing area R1 is also formed on the next processing line. Next, when the laser processing area R1 is formed along all of the processing lines CL1 in the X direction, the XYZθ table 104 is rotated 90° around the Z axis, and a laser processing area R1 is similarly formed on the processing line CL1 in the X direction after the rotation.

[0033] Here, the laser processing area R1 refers to an area where the physical properties such as density, refractive index, and mechanical strength inside the workpiece W are different from those of the surrounding area due to irradiation with laser light, and the strength is lower than that of the surrounding area. The laser processing area R1 includes, for example, a crack area. The workpiece W in which the laser processing area is formed is transported to a grinding device (not shown), and the back surface of the workpiece W is ground to remove the laser processing area R1. Then, when an expandable tape is attached to the back surface side of the workpiece W and expanded, the workpiece W is fractured by the cracks that extend from the laser processing area R1 to the front surface side of the workpiece W. As a result, the workpiece W is separated into individual chips.

[0034] (Oblique illumination (dark field illumination system)) Next, the workpiece CW for inspection will be described with reference to Fig. 2. Fig. 2 shows a plan view and a cross-sectional view of the workpiece for inspection when oblique illumination (dark-field illumination system) is used. Fig. 2(A) is a plan view (top view) of the workpiece for inspection, and Fig. 2(B) is a cross-sectional view taken along line BB of Fig. 2(A).

[0035] As shown in FIG. 2B, the inspection workpiece CW according to this embodiment includes a workpiece layer WL made of the same material (for example, silicon, etc.) as the workpiece W to be produced.

[0036] The inspection workpiece CW is adsorbed and held with its front surface facing down in the laser dicing device 10. The inspection workpiece CW shown in FIG. 2 includes a missing portion P1 containing impurities (particles). Note that in FIG. 2, for the sake of simplicity, only one missing portion P1 is shown. In this embodiment, an observation light source 302 is used to obliquely illuminate the inspection workpiece CW with oblique illumination light L1 that transmits through the inspection workpiece CW, while an image of the inspection workpiece CW before machining is captured by a camera 306. Then, the control unit 12 detects the missing portion P1 from this image.

[0037] When laser processing is performed on the inspection workpiece CW, a laser processed region R1 (see FIG. 2B) is formed along the processing line CL1 (see FIG. 2A) in the inspection range of the work layer WL.

[0038] During laser processing, part of the laser light is scattered in the inspection range of the work layer WL and leaks out to the underside of the work layer WL. When this scattered light and leaked light reach the underside of the work layer WL, the detection layer DL is partially melted. This causes a change in the reflectance of the interface between the work layer WL and the detection layer DL when illumination light (oblique illumination light (polarized illumination light), for example, infrared light) is irradiated onto the inspection workpiece CW. Based on this change in reflectance, defects can be detected from an image of the inspection workpiece CW after processing.

[0039] In the example shown in Fig. 2, splash damages SD1 to SD3 formed by scattered light and damage BD (hereinafter referred to as direct damage) formed by leaked light leaking to the underside of the laser processing area R1 are shown. The splash damages SD1 to SD3 are point-like defects formed by a part of the laser light being scattered in a sputter-like manner by structures in the inspection range of the work layer WL. The direct damage BD is a defect formed by a part of the laser light leaking to the underside of the laser processing area R1, and is formed along the processing line CL1.

[0040] In this embodiment, while the workpiece CW for inspection is obliquely illuminated with the oblique illumination light L1, the interface between the workpiece layer WL and the detection layer DL is set as the focus plane FP (in-focus plane) using the camera 306 to capture the image of the workpiece CW for inspection after processing. As shown in Fig. 2, the image of the workpiece CW for inspection after processing includes the missing part P1 and the direct damage BD in addition to the splash damages SD1 to SD3.

[0041] In these captured images, most of the illumination light L1 that passes through the background region does not return to the camera 306, and the illumination light L1 that is irradiated to the defect including splash damage is scattered, and part of the scattered light L2 reaches the camera 306. For this reason, the background region is darker than the defect including splash damage, and the defect including splash damage appears as a white region.

[0042] As described later, when oblique illumination is performed, a part of the illumination light L1 that passes through the lower surface side of the inspection workpiece CW is reflected by the surface of the porous (e.g., particulate ceramic dense body) of the suction stage (chuck) 102 and returns to the camera 306 side. This causes uneven brightness in the background area of ​​the captured image (see FIG. 6, etc.). In this embodiment, while the reflected light from the porous surface of the suction stage 102 is blurred, minute defects such as splash damage SD1 to SD3, missing part P1, and direct damage BD have high frequency components, and this is utilized to extract the defects. Specifically, the defects are extracted by extracting only high frequency components from the captured image of the inspection workpiece CW using fast Fourier transform (FFT).

[0043] That is, the control unit 12 uses the image processing unit 308 to apply FFT to the image of the inspection workpiece CW before processing to detect the defective part P1, and stores information about its position and shape (for example, coordinates, etc.). Next, the control unit 12 uses the image processing unit 308 to apply FFT to the image of the inspection workpiece CW after processing to detect all defects as candidates for processing defects (hereinafter referred to as defect candidates), including splash damages SD1 to SD3. These defect candidates may include the defective part P1 and direct damage BD in addition to the splash damages SD1 to SD3. Then, the control unit 12 excludes the defective part P1 detected in advance from the defect candidates. Furthermore, the control unit 12 extracts the direct damage BD along the processing line CL1 from the image of the inspection workpiece CW after processing, and excludes it from the defect candidates. As a result, the splash damages SD1 to SD3 are extracted as processing defects.

[0044] According to this embodiment, by applying FFT to images of the inspection range of the workpiece before and after laser processing, minute defects caused by scattering of laser light or the like can be detected with high accuracy.

[0045] Incidentally, for the defective portion P1, the area including the previously detected defective portion P1 may be masked to exclude it from the detection target of the defect candidate. Here, the mask area is an area defined by the contour of the defective portion P1, to which a margin is added for the repeatability accuracy of the transport error of the inspection workpiece CW and the like. By defining the mask area in this way, the mask area can be minimized, and therefore the area subject to detection of machining defects can be maximized, and it is possible to prevent oversight of detection of machining defects.

[0046] Furthermore, it is also possible to generate a pattern in the detection layer DL of the workpiece CW for inspection, and align the workpiece CW for inspection by detecting this pattern using an alignment camera or the like, thereby correcting the transport error. In this case, it is possible to further reduce the transport error of the workpiece CW for inspection, and therefore the mask area can be further reduced. This allows the area subject to detection of machining defects to be enlarged, and it is possible to more reliably prevent undetected machining defects.

[0047] In this embodiment, the workpiece CW for inspection is made up of the workpiece layer WL, but the present invention is not limited to this. It is also possible to use the workpiece CW1 for inspection in which the detection layer DL shown in FIG. 3 is formed.

[0048] (Coaxial epi-illumination (bright-field illumination system)) In this embodiment, oblique illumination (dark-field illumination system) is used, but the present invention can also be applied when coaxial epi-illumination (bright-field illumination system) is used. When coaxial epi-illumination is used, an inspection workpiece CW1 having a detection layer DL shown in FIG. 3 is used.

[0049] FIG. 3 is a plan view and a cross-sectional view of a workpiece to be inspected when using coaxial epi-illumination (bright-field illumination system).

[0050] As shown in FIG. 3, the inspection work CW1 includes a work layer WL and a detection layer DL formed on the lower surface of the work layer WL in the figure (the surface (front surface) side to be inspected). The work layer WL is formed of, for example, silicon or the like. The detection layer DL is formed by evaporating a low melting point metal (for example, tin, etc.), a low melting point alloy, etc. onto the work layer WL. The detection layer DL may be formed of a coating of resin or the like. Furthermore, the inspection work CW1 is not limited to one having a detection layer DL formed thereon, and for example, one having a lower surface of the work layer WL mirror-finished to increase reflectivity (for example, a mirror work) may be used.

[0051] The workpiece CW1 for inspection is adsorbed and held with the detection layer DL facing down in a laser dicing device (not shown). Then, laser processing is performed on the workpiece CW1 for inspection, and a laser processing region R1 is formed inside the workpiece layer WL. Note that the reference character R2 in FIG. 3 is a shadow that is generated when a part of the illumination light L10 is blocked by the laser processing region R1. This shadow R2 is imaged along the processing line CL1.

[0052] In the region where the splash damages SD1 to SD3 are formed, the reflectance of the interface FP between the work layer WL and the detection layer DL changes when the inspection work CW1 is irradiated with illumination light L1 with high transmittance (infrared light if the inspection work CW1 is a silicon wafer). Therefore, by performing coaxial epi-illumination using illumination light L10 and capturing an image of reflected light L12 from the interface FP using a camera 306, the splash damages SD1 to SD3 can be detected.

[0053] In the example shown in Fig. 3, a process for forming a metal vapor deposition film with a low melting point is required, but the sensitivity to scattered light and leaked light during laser processing can be increased, and splash damages SD1 to SD3 can be easily detected. Then, based on the detection result of splash damage in the inspection workpiece CW1, processing conditions for laser processing that can suppress the occurrence of splash damage can be obtained. As a result, when performing laser processing on the workpiece to be produced, processing conditions can be set so that the device formed on the surface of the workpiece is not affected by splash damage.

[0054] (Images captured with dark-field and bright-field illumination systems) Next, we will explain the images of the workpiece for inspection captured by the dark-field illumination system and the bright-field illumination system. Figure 4 shows an image of the workpiece for inspection captured by the oblique illumination (dark-field illumination system), and Figure 5 shows an image of the workpiece for inspection captured by the coaxial epi-illumination (bright-field illumination system).

[0055] The example shown in FIG. 5 is an image obtained by performing coaxial epi-illumination on an inspection workpiece CW1 (see FIG. 3) having a detection layer DL. In this case, in the background region other than the region where the defect including splash damage (circled region) is formed, the illumination light L1 is reflected by the detection layer DL made of a metal vapor deposition film. On the other hand, in the region where the defect including splash damage (circled region) is formed, the illumination light L10 is diffused by the splash damage SD1 to SD3, so the reflected light L12 does not return to the incident side of the illumination light L10. For this reason, in FIG. 5, the background region emits white light, and the defect including splash damage (circled region) is a dark region (bright-field illumination system). Since splash damage is a minute defect, if the reflected light amount around the defect is strong, the contrast between the background region and the defect is reduced due to charge leakage from the pixels surrounding the pixel corresponding to the defect on the sensor, lens aberration, etc. For this reason, in the case of a bright-field illumination system, splash damage is likely to go undetected.

[0056] On the other hand, in the example shown in Figure 4, the background area is dark, and the defect (circled area) including splash damage is a white area. Since the defect emits white light, it can be seen that the area where the defect formed has a locally uneven shape on the underside of the inspection workpiece CW. When dark-field illumination is used, reflected light is generated by the uneven shape, and the area where the defect formed actively lights up. As a result, the area where the defect formed is captured large without being affected by leakage charge or lens aberration. Therefore, when a dark-field illumination system is used, the effect of emphasizing the defect is obtained, and the effect of improving robustness can be obtained.

[0057] (Splash Damage Extraction) Next, a procedure for extracting splash damage from an image obtained by imaging the inspection workpiece CW will be specifically described.

[0058] Fig. 6 is an image (hereinafter also referred to as the original image) obtained by imaging the workpiece CW for inspection, and Fig. 7 is an image showing the result of performing binarization processing on the original image of Fig. 6. The original image of Fig. 6 includes splash damages SD1 to SD4.

[0059] When oblique illumination is performed, a part of the illumination light L1 that passes through the lower surface side of the inspection workpiece CW is reflected by the porous surface of the suction stage (chuck) 102 and returns to the camera 306. For this reason, as shown in FIG 6, uneven brightness occurs in the background area of ​​the captured image.

[0060] When the original image in Fig. 6 is subjected to binarization processing with a constant threshold value, the image shown in Fig. 7 is obtained. As shown in Fig. 7, the splash damages SD2 and SD3 cannot be extracted because they are included in the high-luminance area N1 in the background area.

[0061] Furthermore, noise occurs in the peripheral area N2 of the high-luminance area N1 due to variations in the gray levels of the pixels. The influence of this noise makes it difficult to separate the splash damage SD4 in the peripheral area N2 of the high-luminance area N1 from the background area.

[0062] Therefore, it is conceivable to extract defects by performing dynamic threshold processing for each local region of the captured image. In dynamic threshold processing, for example, first, a mean value image (= threshold image) is generated using a local averaging filter or a local median filter. Next, binarization processing (dynamic threshold processing) that takes brightness unevenness into consideration is performed by using this mean value image as a threshold. This adjusts the threshold for noise caused by minute brightness fluctuations of pixels.

[0063] 8 and 9 are images showing the results of dynamic thresholding of the original image of FIG. FIG. 8 shows an example where an appropriate threshold can be set by dynamic threshold processing (Comparative Example 1), and FIG. 9 shows an example where an appropriate threshold cannot be set by dynamic threshold processing (Comparative Example 2). As shown in FIG. 8, when an appropriate threshold can be set, it is possible to extract splash damage SD1 to SD4 from the background. On the other hand, as shown in FIG. 9, when an appropriate threshold cannot be set, a large number of noises caused by uneven brightness are extracted as defect candidates. These noises are only slightly different from the splash damages SD1 to SD4 in terms of characteristics such as shape and size, and it is difficult to separate the noises from the splash damages SD1 to SD4.

[0064] As shown in Figures 8 and 9, dynamic threshold processing is not robust against changes in visibility, and the stability of processing results in production equipment is low. For this reason, depending on the results of dynamic threshold processing, errors may occur frequently, and the production process may be temporarily stopped repeatedly (so-called "choco stop"). In addition, when noise is removed by applying a general spatial filter, splash damage SD1 to SD4 may also be removed at the same time.

[0065] Therefore, in this embodiment, the following method is used to improve robustness against changes in visibility. That is, while the reflected light from the porous surface of the suction stage 102, which causes noise, is blurred, the defects to be extracted (including the missing part P1 and splash damages SD1 to SD4) have the characteristics of high frequency components, and this is utilized to extract the defects. Specifically, the defects are extracted by using FFT to extract only high frequency components from the captured image of the inspection workpiece CW.

[0066] FIG. 10 is a captured image of the inspection workpiece after FFT processing, and FIG. 11 is an image showing the extraction result of splash damage.

[0067] Applying FFT to the original image in Figure 6 results in a two-dimensional spatial frequency characteristic map of the original image. Here, spatial frequency is the degree of change in brightness per unit length expressed as a frequency. The minute defects to be extracted have a short period of change in brightness per unit length and a high spatial frequency. As a result, as shown in Figure 10, only the high-frequency region containing the defect to be extracted is extracted, and noise in the background region caused by uneven brightness is removed. This has the effect of highlighting only the defect to be extracted in the original image.

[0068] Next, the position, shape, and size of the defect to be extracted are identified by performing binarization processing on the image after FFT processing in Figure 10. The position, shape, and size of this defect are superimposed on the original image to obtain the image shown in Figure 11. This makes it possible to extract only the splash damages SD1 to SD4.

[0069] (How to set processing conditions) Next, a method for setting processing conditions according to this embodiment will be described with reference to Figures 12 to 15. Figure 12 is a flow chart showing a method for setting processing conditions for laser dicing.

[0070] First, the inspection workpiece CW is carried into the laser dicing device 10 (processing section) and adsorbed and held on the suction stage 102 (step S10). Then, the observation optical section 300 irradiates the inspection workpiece CW with oblique illumination light L1, and the camera 306 captures an image of the inspection workpiece CW before processing (step S12: imaging process). The inspection workpiece CW may be adsorbed and held on the suction stage 102 via the BG tape B, or may be directly adsorbed on the suction stage 102.

[0071] Next, the inspection workpiece CW is processed by the laser dicing device 10, and a laser processing region R1 is formed in the inspection range of the inspection workpiece CW (step S14). Then, the observation optical unit 300 irradiates the inspection workpiece CW with oblique illumination light L1, and the processed inspection workpiece CW is imaged by the camera 306 (step S16: imaging step).

[0072] Next, the control unit 12 compares images of the inspection workpiece CW before and after processing to detect machining defects including splash damage formed by laser processing (step S18). Here, the control unit 12 and the image processing unit 308 function as a detection unit of the present invention. Then, the control unit 12 evaluates the detected machining defects according to the detection results of the machining defects (step S20). The control unit 12 determines whether or not to change the machining conditions based on the evaluation results of the machining defects.

[0073] If the machining conditions are to be reset (Yes in step S22), the control unit 12 resets the machining conditions (step S24). On the other hand, if the machining conditions are not to be reset (No in step S22), the control unit 12 saves machining defect information including the machining defect evaluation results and images of the inspection workpiece CW before and after machining (step S26). Here, the control unit 12 functions as the setting unit of the present invention. The machining defect information saved in step S26 becomes viewable by the operator as a quality record.

[0074] Next, the process of detecting defects during machining will be described with reference to a flowchart shown in FIG.

[0075] First, the control unit 12 applies FFT to the images of the inspection workpiece CW before and after processing, which are respectively captured in steps S12 and S16, to extract high-frequency components, and then performs binarization processing (step S180: image processing step). Then, the control unit 12 detects a missing part (P1) from the image of the inspection workpiece CW before processing, which has been image-processed in step S180 (step S182). Next, the control unit 12 detects defect candidates (BD, R2, P1, and SD1 to SD3) and the processing line CL1 from the image of the inspection workpiece CW after processing, which has been image-processed in step S180 (step S184). Then, the control unit 12 excludes the missing part (P1), the direct damage BD along the processing line CL1, and the shadow R2 of the laser processing region R1 from the defect candidates in the image of the inspection workpiece CW after processing, and identifies the processing defects SD1 to SD3 (step S186).

[0076] In this embodiment, the images of the inspection range of the inspection workpiece CW before and after the laser processing are compared to identify the machining defects, but the present invention is not limited to this. For example, map data including information on the position and size of the defective part in the inspection workpiece CW may be acquired in advance and stored in the control unit 12 (map data acquisition unit). Then, the defective part in the map data may be excluded from the image of the inspection workpiece CW after processing to identify the machining defects. In this case, the imaging of the inspection workpiece CW before the laser processing (step S12) and the detection of the defective part (step S182) are omitted.

[0077] Here, the map data may be created by imaging one inspection workpiece CW (e.g., a silicon wafer) in the same manner as above to detect missing parts. Then, this map data may be used in common for inspecting silicon wafers cut from the same silicon ingot as the inspection workpiece CW used to create the map data.

[0078] In the above embodiment, the images or map data before and after the laser processing are used to distinguish between the missing portion and the processing defect, but the present invention is not limited to this. For example, the missing portion and the processing defect may be distinguished from the characteristics such as the shape, size, or position of the defect candidate detected from the image after the laser processing. In other words, the processing defect may be detected only from at least the image after the laser processing.

[0079] Next, the evaluation process for the machining defects will be described with reference to a flowchart shown in FIG.

[0080] First, the control unit 12 calculates an evaluation value of the machining defects (step S200). The evaluation value of the machining defects is the number of machining defects, their size, and their distance from the machining line CL1. The number of machining defects may be calculated, for example, by calculating the number of machining defects per unit area in an area surrounded by the machining line CL1 (an area for one chip). The evaluation value of the machining defects may also be calculated, for example, as a numerical value normalized by the average value in the inspection workpiece CW.

[0081] Next, the control unit 12 compares the evaluation value of the processing defect with the error limit value (step S202). In steps S202 to S204, a representative value (e.g., a maximum value, an average value, a median value, etc.) of the evaluation value of various processing defects is compared with the error limit value to determine whether or not to reset the processing conditions.

[0082] If any of the evaluation values ​​of the machining defects is equal to or greater than the error limit value (Yes in step S204), the control unit 12 outputs an instruction to reset the machining conditions (step S206). On the other hand, if any of the evaluation values ​​of the machining defects is less than the error limit value (No in step S204), the control unit 12 outputs an instruction not to reset the machining conditions (step S208).

[0083] Next, the process of setting the processing conditions will be described with reference to a flowchart shown in FIG.

[0084] First, the control unit 12 identifies the type of evaluation value of the processing defect that is equal to or greater than the error limit value (step S240). Next, the control unit 12 displays candidates for changing the processing conditions on the monitor 310 according to the type of evaluation value that is equal to or greater than the error limit value (step S242).

[0085] Next, the control unit 12 receives an instruction input for selecting a candidate for the processing condition from the operator (step S244), and resets the processing condition (step S246). Note that the processing condition may be reset arbitrarily by the operator.

[0086] Here, the processing conditions include, for example, the wavelength, spot diameter, output, repetition frequency, pulse width, numerical aperture (NA) of the condenser lens 208, position of the focal point, polarization characteristics, processing feed speed, etc. of the laser beam. The spot diameter and the position of the focal point of the laser beam can be adjusted, for example, by moving the condenser lens 208 in the Z direction. The numerical aperture of the condenser lens 208 can be adjusted, for example, by an aperture. The polarization characteristics can be adjusted, for example, by using a wavelength plate. By adjusting the processing conditions exemplified above, the evaluation values ​​of the processing defects, such as the number, size, and distance of the processing defects from the processing line CL1, are adjusted so as to be less than the error limit value.

[0087] In the workpiece machining method according to the present embodiment, laser machining is performed on the workpiece W to be machined, based on the machining conditions reset by the above steps, and the workpiece W is ground and broken. As a result, the workpiece W is divided into individual chips.

[0088] According to this embodiment, by extracting high-frequency components from an image of the inspection workpiece CW captured using a dark-field illumination system, it becomes possible to detect machining defects caused by scattering of laser light, etc., with high accuracy and at low cost. Furthermore, according to this embodiment, it becomes possible to accurately evaluate the effect of laser processing on the quality of the device according to the detection result of the machining defect, and to appropriately set the processing conditions for the laser processing.

[0089] Furthermore, in this embodiment, the control unit 12 may determine whether or not the laser processing area is formed at the target position based on the detection result of the position of the shadow R2 of the laser processing area R1 and the direct damage BD along the processing line CL1 (laser processing area). If the control unit 12 determines that the laser processing area is not formed at the target position, it may calculate the correction amount of the laser processing position and reset the laser processing conditions. [Explanation of symbols]

[0090] 10...laser dicing device, 12...control unit, 100...work moving unit, 102...suction stage, 104...XYZθ table, 106...main body base, 200...laser optical unit, 202...laser oscillator, 204...collimating lens, 206...half mirror, 208...condenser lens (light collecting lens), 210...driving means, 300...observation optical unit, 302...observation light source, 304...condenser lens, 306...camera, 308...image processing unit, 310...monitor, 400...optical system unit (laser engine)

Claims

1. an imaging step of capturing an image of an inspection range of the workpiece after the laser processing of the workpiece by using an imaging device while obliquely illuminating the workpiece; an image processing step of performing a fast Fourier transform on an image of the inspection range of the workpiece after the laser processing to extract high-frequency components and perform a binarization process; A detection process for detecting defects during processing formed by scattered light or leaked light generated during the laser processing from an image of the inspection range of the workpiece after the laser processing, which has been image-processed in the image processing process; A workpiece inspection method comprising:

2. The method of claim 1 , wherein the workpiece comprises only a workpiece layer.

3. A step of capturing an image of an inspection range of the workpiece before the laser processing using the imaging device while obliquely illuminating the workpiece; A step of applying a fast Fourier transform to an image of the inspection range of the work before the laser processing to extract high-frequency components and performing a binarization process; The detection step includes: detecting a missing portion in an inspection range of the work from an image of the inspection range of the work before the laser processing; detecting defect candidates from defects detected in an image of an inspection range of the workpiece after the laser processing; A step of identifying the processing defect by excluding the missing portion, the laser processing area formed in the workpiece by the laser processing, and a shadow of the laser processing area from the defect candidate; The workpiece inspection method according to claim 1 or 2, further comprising:

4. an imaging device that captures an image of an inspection range of a workpiece after laser processing of the workpiece while performing oblique illumination on the workpiece; an image processing unit that performs a fast Fourier transform on an image of the inspection range of the workpiece after the laser processing to extract high-frequency components and perform a binarization process; A detection unit that detects defects during processing formed by scattered light or leaked light generated during the laser processing from an image of the inspection range of the workpiece after the laser processing that has been image-processed by the image processing unit; A workpiece inspection device comprising:

Citation Information

Patent Citations

  • Inspecting wafer, and method for using inspecting wafer

    JP2017037912A

  • Inspection wafer, and method for using inspection wafer

    JP2018064049A

  • Inspection apparatus

    JP2018112408A

  • Evaluation method for evaluating fuzz generation on fiber

    JP2020071193A

  • Laser processing method and device

    JP2020077767A