Semiconductor device and method of manufacturing semiconductor device
A semiconductor device with a recessed two-layer source electrode structure and insulating film filling addresses the issue of increased surface resistance, enhancing reliability and reducing resistance through even current distribution.
Patent Information
- Application Number
- JP2023076310
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-02
- Publication Date
- 2024-11-15
AI Technical Summary
Conventional semiconductor devices face increased surface electrode resistance due to miniaturization, limiting the reduction of on-resistance, and existing methods to reduce this resistance, such as increasing wire diameter or forming plating electrodes, face limitations in reliability and cost.
The semiconductor device incorporates a two-layer source electrode structure with a recessed upper electrode extending perpendicular to the contact hole, and an insulating film filling the recess, to distribute current evenly and reduce surface resistance.
This design effectively reduces surface electrode resistance by providing a thick region for current flow, improving reliability and reducing wire bonding damage while maintaining manufacturing efficiency.
Smart Images

Figure 2024160850000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a semiconductor device and a method for manufacturing the semiconductor device. [Background technology]
[0002] Conventionally, semiconductor devices are known in which a plurality of recesses are formed in an electrode layer in order to prevent stress from concentrating in a specific portion of the electrode layer and causing cracks (see, for example, Patent Document 1 below). Also known is a semiconductor device in which an SOG film is embedded in the recesses of the source electrode to flatten the electrode surface in order to increase the adhesive strength with the lead (see, for example, Patent Document 2 below). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2009-266935 A [Patent Document 2] JP 2003-101024 A Summary of the Invention [Problem to be solved by the invention]
[0004] In conventional semiconductor devices, the on-resistance of the semiconductor element itself has been reduced by miniaturization, but there has been a problem that the surface electrode resistance of the semiconductor element is no longer negligible. The object of the present invention is to provide a semiconductor device and a method for manufacturing the semiconductor device that can reduce the surface electrode resistance of the semiconductor element. [Means for solving the problem]
[0005] In order to solve the above-mentioned problems and achieve the object of the present invention, the semiconductor device according to the present invention has the following features. The semiconductor device includes a semiconductor substrate of a first conductivity type, a drift layer of the first conductivity type provided on a first main surface of the semiconductor substrate, a base layer of a second conductivity type provided in a surface layer of the drift layer, a source region of the first conductivity type selectively provided in a surface layer of the base layer, a gate electrode provided on a surface of the base layer and the source region via a gate insulating film, an interlayer insulating film covering the source region and the gate electrode, a contact hole having a longitudinal direction in a first direction provided in the interlayer insulating film on the surface of the source region, and a front surface electrode provided on the interlayer insulating film. The front surface electrode is composed of a lower electrode on the interlayer insulating film and an upper electrode on the lower electrode, and the upper electrode has a recess extending in a second direction perpendicular to the first direction.
[0006] In addition, in the semiconductor device according to the present invention, the upper electrode is in a stripe shape having a longitudinal direction in the second direction.
[0007] In addition, in the semiconductor device according to the present invention, the contact holes are in a stripe shape having a longitudinal direction in the first direction.
[0008] In addition, the semiconductor device according to the present invention, in the above-mentioned invention, further comprises a conductive wire connected to the front surface electrode, and the connection direction of the wire is the first direction.
[0009] In the semiconductor device according to the present invention, in the above-mentioned invention, a width of the recess in a short side direction is smaller than a diameter of the wire.
[0010] In the semiconductor device according to the present invention, in the above-mentioned invention, a surface of the lower electrode in contact with the upper electrode is flatter than a surface of the interlayer insulating film.
[0011] In addition, in the semiconductor device according to the present invention, the lower electrode is made of Al-Si, Al-Si-Cu, or Al-Cu.
[0012] In addition, in the semiconductor device according to the present invention, the upper electrode is formed of Al, Al--Si, Al--Si--Cu, Al--Cu, Al, or Cu.
[0013] In addition, the semiconductor device according to the present invention is characterized in that, in the above-mentioned invention, the recess is provided in a surface of the upper electrode that contacts the lower electrode, and the recess is filled with an insulating film.
[0014] In addition, in the semiconductor device according to the present invention, in the above-mentioned invention, the thickness of the upper electrode on the insulating film is 0.5 to 5 times the distance between adjacent insulating films.
[0015] In addition, in the semiconductor device according to the present invention, the insulating film is formed of inorganic SiO2, SiN or organic polyimide resin.
[0016] In addition, the manufacturing method of the semiconductor device according to the present invention, in the above-mentioned invention, first, a first step is performed to form a drift layer of a first conductivity type on a first main surface of a semiconductor substrate of a first conductivity type. Next, a second step is performed to form a base layer of a second conductivity type on a surface layer of the drift layer. Next, a third step is performed to selectively form a source region of a first conductivity type on a surface layer of the base layer. Next, a fourth step is performed to form a gate electrode on the surface of the base layer and the source region via a gate insulating film. Next, a fifth step is performed to form an interlayer insulating film covering the source region and the gate electrode. Next, a sixth step is performed to form a contact hole having a longitudinal direction in a first direction in the interlayer insulating film on the surface of the source region. Next, a seventh step is performed to form a front surface electrode on the interlayer insulating film. The seventh step includes a step of forming a lower electrode on the interlayer insulating film, and a step of forming an upper electrode on the lower electrode having a recess extending in a second direction perpendicular to the first direction.
[0017] In addition, the manufacturing method of a semiconductor device according to the present invention is characterized in that, in the above-mentioned invention, the seventh step includes the steps of forming the lower electrode on the interlayer insulating film, forming a resist on the lower electrode, forming an opening in the resist reaching the lower electrode, forming a metal film in the resist and in the opening, and forming the upper electrode on the lower electrode by removing the metal film and the resist on the resist.
[0018] In addition, the manufacturing method of a semiconductor device according to the present invention is characterized in that, in the above-mentioned invention, the seventh step includes a step of forming the lower electrode on the interlayer insulating film, a step of forming an insulating film on the lower electrode, a step of forming an opening in the insulating film reaching the lower electrode, and a step of forming the upper electrode on the lower electrode by forming a metal film in the insulating film and the opening. Effect of the Invention
[0019] The semiconductor device and the method for manufacturing the semiconductor device according to the present invention have the effect of reducing the surface electrode resistance of the semiconductor element. [Brief description of the drawings]
[0020] [Figure 1] 1 is an enlarged plan view showing a structure of a semiconductor device according to a first embodiment. [Diagram 2] 2 is a cross-sectional view taken along the line X1-X1 of FIG. 1, showing the structure of the semiconductor device according to the first embodiment. [Diagram 3] 2 is a cross-sectional view taken along the line X2-X2 of FIG. 1, showing the structure of the semiconductor device according to the first embodiment. [Figure 3a] 2 is a cross-sectional view showing a current flow in a source electrode of the semiconductor device according to the first embodiment. FIG. [Figure 3b] 11 is a cross-sectional view showing a current flow in a source electrode when the extending direction of a recess is parallel to the longitudinal direction of a contact hole. FIG. [Figure 4] 2 is a cross-sectional view taken along the line Y1-Y1 of FIG. 1, showing the structure of the semiconductor device according to the first embodiment. [Diagram 5] FIG. 1 is a plan view (part 1) illustrating a structure of a semiconductor device according to a first embodiment. [Figure 6] FIG. 2 is a plan view (part 2) illustrating the structure of the semiconductor device according to the first embodiment. [Figure 7] 1 is a cross-sectional view (part 1) showing a state during the manufacture of the semiconductor device according to the first embodiment; [Figure 8] 4 is a cross-sectional view (part 2) showing a state during the manufacture of the semiconductor device according to the first embodiment. FIG. [Figure 9] 4 is a cross-sectional view (part 3) showing a state during the manufacture of the semiconductor device according to the first embodiment. FIG. [Figure 10] 4 is a cross-sectional view showing a state during the manufacture of the semiconductor device according to the first embodiment (part 4). FIG. [Figure 11] 5 is a cross-sectional view showing a state during the manufacture of the semiconductor device according to the first embodiment (part 5). FIG. [Figure 12]1 showing a structure of a semiconductor device according to a second embodiment. FIG. [Figure 13] 1 showing a cross-sectional view of a semiconductor device according to a second embodiment taken along the line X2-X2 of FIG. [Figure 14] 1 showing a structure of a semiconductor device according to a second embodiment. FIG. [Figure 15] 11 is a cross-sectional view (part 1) showing a state during the manufacture of a semiconductor device according to a second embodiment. FIG. [Figure 16] FIG. 2 is a cross-sectional view (part 2) showing a state during the manufacture of the semiconductor device according to the second embodiment. [Figure 17] 11 is a cross-sectional view (part 3) showing a state during the manufacture of the semiconductor device according to the second embodiment. FIG. [Figure 18] FIG. 4 is a cross-sectional view showing a state during the manufacture of the semiconductor device according to the second embodiment (part 4). [Figure 19] 5 is a cross-sectional view showing a state during the manufacture of the semiconductor device according to the second embodiment (part 5). FIG. [Figure 20] FIG. 6 is a cross-sectional view showing a state during the manufacture of the semiconductor device according to the second embodiment (part 6). [Figure 21] FIG. 7 is a cross-sectional view showing a state during the manufacture of the semiconductor device according to the second embodiment; [Figure 22] FIG. 8 is a cross-sectional view showing a state during the manufacture of the semiconductor device according to the second embodiment; [Diagram 23] FIG. 9 is a cross-sectional view showing a state during the manufacture of the semiconductor device according to the second embodiment; [Figure 24] FIG. 10 is a cross-sectional view showing a state during the manufacture of a semiconductor device according to the second embodiment; [Diagram 25] FIG. 11 is a cross-sectional view showing a state during the manufacture of a semiconductor device according to the second embodiment; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0021] A preferred embodiment of the semiconductor device and the method for manufacturing the semiconductor device according to the present invention will be described in detail below with reference to the accompanying drawings. In this specification and the accompanying drawings, in a layer or region marked with n or p, electrons or holes are the majority carriers, respectively. In addition, + and - marked with n or p mean that the impurity concentration is higher and lower than that of a layer or region not marked with them, respectively. When the notations of n and p including + and - are the same, it indicates that the concentrations are close, but the concentrations are not necessarily the same. In the following description of the embodiment and the accompanying drawings, the same symbols are marked for similar configurations, and duplicated explanations are omitted. In addition, the description of the same or equivalent should preferably include within ±5% in consideration of variations in manufacturing.
[0022] (Embodiment 1) First, a conventional semiconductor device will be described. As described above, in conventional semiconductor devices, the on-resistance (on-voltage) of the semiconductor element (semiconductor chip) itself is decreasing due to improved design and processing accuracy through miniaturization and the like. As a result, the resistance of the surface electrode of the semiconductor element that connects the substrate of the semiconductor element to the external electrode is becoming non-negligible. In particular, the resistance of the surface electrode in the lateral direction (in-plane direction) is increasing. By increasing the thickness of the metal film of the surface electrode, the resistance of the surface electrode is reduced, current concentration is alleviated, and the tolerance can be improved. However, since thickening the metal film reduces the equipment capacity, reduces processing accuracy, and requires design changes, the thickness of the metal film can only be increased to a certain extent. For this reason, the wire diameter and number of wires connected to the surface electrode are increased, and a plated electrode is formed on the surface of the metal film.
[0023] Increasing the wire diameter or number of wires not only reduces the wire resistance component, but also reduces the thin area of the metal film by bonding a wire that is much thicker than the metal film of the semiconductor element, which is equivalent to thickening the metal film at the bonded portion, reducing the resistance of the metal film and suppressing current concentration, improving the durability. In addition, the thicker metal film reduces damage caused by wire bonding, improving the reliability of the semiconductor element.
[0024] In addition, when a plating electrode is formed on the metal film of a semiconductor element, the surface electrode becomes thicker by stacking a plating electrode that is thicker than the metal film, making it possible to reduce the resistance of the surface electrode. In reality, a solder layer is also formed on the plating electrode, so the reduction in surface electrode resistance is small, but the wire resistance and L (inductance) component decrease. In addition, the cross-sectional area of the current path increases, acting as a ballast resistor, suppressing current concentration and improving the withstand voltage.
[0025] However, due to the constraints of the wire bonding equipment and the package, there are limitations on the wire diameter and number of wires, and the reduction of the surface electrode resistance is also limited. In addition, for the reasons mentioned above, there is a limit to the thickness of the metal film of the semiconductor element, and the reduction of bonding damage with a wire diameter that is overwhelmingly thicker than that of the metal film is insufficient. For this reason, there are stitch bonding and ribbon wire as an improvement method within the limitations, but there is a problem that the increase in the number of bonds and the bonding area not only increases costs but also increases the wire bonding damage, thereby reducing the reliability of the semiconductor element.
[0026] Furthermore, in the case of a configuration of a plating electrode and a solder layer, although both the plating electrode and the solder layer are thick, they have a higher resistivity than the metal film of the semiconductor element, and the effect of reducing resistance by the plating electrode and the solder layer is low. In addition, the plating solution contains a large number of metal ions, which may penetrate into the semiconductor element, thereby reducing the reliability of the semiconductor element.
[0027] A semiconductor device and a method for manufacturing the semiconductor device according to a first embodiment that solves the above problems will be described below. FIG. 1 is an enlarged plan view showing the structure of the semiconductor device according to the first embodiment. FIG. 2 is an X1-X1 cross-sectional view of FIG. 1 showing the structure of the semiconductor device according to the first embodiment. FIG. 3 is an X2-X2 cross-sectional view of FIG. 1 showing the structure of the semiconductor device according to the first embodiment. FIG. 4 is a Y1-Y1 cross-sectional view of FIG. 1 showing the structure of the semiconductor device according to the first embodiment. The structure of the semiconductor device according to the first embodiment will be described using a trench MOSFET 70 as an example.
[0028] The trench MOSFET 70 is a MOSFET having a MOS (Metal Oxide Semiconductor) gate on the front surface (the surface on the p-type base layer 5 side described later) of a semiconductor substrate (silicon substrate: semiconductor chip) made of silicon (Si). As shown in FIGS. 1 to 4, the trench MOSFET 70 has an active region 50, an active region outer periphery 55, and an edge termination region 60 surrounding the active region 50 and the active region outer periphery 55. The active region 50 and the active region outer periphery 55 are regions through which a current flows in an on-state. The edge termination region 60 includes a breakdown voltage holding region that relaxes the electric field on the front surface side of the semiconductor substrate in the drift region and holds a breakdown voltage. A MOS structure is provided in the active region 50, and a MOS structure is not provided in the active region outer periphery 55.
[0029] The boundary between the active region 50 and the peripheral portion 55 of the active region is formed by a trench having a n + The boundary between the active region outer periphery 55 and the edge termination region 60 is the edge of the source electrode 10, which will be described later. In the active region 50 of Figures 2 and 3, two unit cells (functional units of an element) are shown, and other unit cells adjacent to these are not shown. Here, a unit cell extends from the center of a trench 18 to the center of an adjacent trench 18.
[0030] n + The n-type semiconductor substrate (first conductivity type semiconductor substrate) 1 is a silicon single crystal substrate doped with, for example, arsenic (As) or phosphorus (P). + An n-type drift layer (drift layer of a first conductivity type) 2 is provided on a semiconductor substrate 1. The n-type drift layer 2 is + The low-concentration n-type layer has a lower impurity concentration than the n-type semiconductor substrate 1 and is doped with, for example, phosphorus. + The n-type drift layer 2 is used as a semiconductor substrate, and a n-type + A mold region may be provided. + The n-type semiconductor substrate 1 and the n-type drift layer 2 together form a semiconductor base. +An n-type buffer layer (not shown) is formed on the n-type semiconductor substrate 1. + The n-type buffer layer may be disposed at a lower impurity concentration than the n-type semiconductor substrate 1. The n-type buffer layer is, for example, a low-concentration n-type layer doped with phosphorus. A MOS gate structure (element structure) is formed on the front surface side of the semiconductor substrate. In addition, a back surface electrode 11 that serves as a drain electrode is provided on the back surface of the semiconductor substrate.
[0031] In addition, a p-type base layer (a base layer of a second conductivity type) 5 is provided in the surface layer of the n-type drift layer 2. + A p-type source region (first conductivity type source region) 6 is selectively provided in the surface layer of the p-type base layer 5. + The p-type source region 6 ++ A mold contact region 33 may optionally be provided.
[0032] A trench structure having a longitudinal direction in the y direction is formed on the first main surface side (p-type base layer 5 side) of the semiconductor substrate. The trench structure is composed of a trench 18, a gate insulating film 7, and a gate electrode 8. Specifically, the trench 18 is formed in the n-type region of the p-type base layer 5. + The p-type base layer 5 and the n-type base layer 6 are formed on the surface opposite to the semiconductor substrate 1 (the first main surface of the semiconductor body). + The gate electrode 8 penetrates the p-type source region 6 to reach the n-type drift layer 2. A gate insulating film 7 is formed along the inner wall of the trench 18 on the bottom and side walls of the trench 18, and a gate electrode 8 is provided inside the gate insulating film 7 in the trench 18. The gate electrode 8 is insulated from the p-type base layer 5 by the gate insulating film 7. A part of the gate electrode 8 may protrude from above the trench 18 (the side where a source electrode 10 described later is provided) toward the source electrode 10.
[0033] The interlayer insulating film 9 is provided over the entire first main surface side of the semiconductor substrate so as to cover the gate electrode 8 embedded in the trench 18. The interlayer insulating film 9 is provided with a contact hole 16 having a longitudinal direction in the y direction. The contact hole 16 has, for example, a stripe shape extending in the y direction. The source electrode (front surface electrode) 10 is connected to the n + The contact hole 16 is in contact with the source electrode 10, and the p-type base layer 5 is in contact with the source region 6. ++ A type contact region 33 may be provided. The source electrode 10 is electrically insulated from the gate electrode 8 by an interlayer insulating film 9. A barrier metal 15 may be provided between the source electrode 10 and the interlayer insulating film 9 to prevent diffusion of metal atoms from the source electrode 10 to the gate electrode 8 side, for example.
[0034] In addition, contact plugs 14 may be embedded in contact holes 16 formed in the interlayer insulating film 9. The contact plugs 14 are, for example, metal films made of tungsten (W) which has high embedding properties. In this case, a trench contact structure is used to prevent n + By drawing out holes in the p-type base layer 5 at a position deeper than the n-type source region 6, parasitic bipolar action can be suppressed and the breakdown voltage can be improved. + through the p-type source region 6 ++ A trench is provided in contact with the n-type contact region 33, and the contact hole 16 is formed through the interlayer insulating film 9 and the n-type contact region 33. + through the p-type source region 6 ++ This is a contact structure provided so as to be in contact with the mold contact region 33. On the source electrode 10, a protective film (not shown) such as a passivation film made of polyimide is selectively provided.
[0035] In the edge termination region 60 that maintains the breakdown voltage, a gate insulating film 7 and a field oxide film 20 are provided on the front surface side of the semiconductor substrate, and a conductive film 22 made of a polycrystalline silicon film that is connected to the gate electrode 8 is provided on the field oxide film 20. An interlayer insulating film 9 is provided on the semiconductor substrate and the conductive film 22. A gate metal electrode 13 that is electrically connected to a gate electrode pad (not shown) is provided on the conductive film 22. The gate metal electrode 13 contacts the conductive film 22 through a contact hole 16 formed in the interlayer insulating film 9, and is insulated from the semiconductor substrate by the field oxide film 20. A barrier metal 15 that prevents diffusion of metal atoms from the gate metal electrode 13 to the gate electrode 8 side may be provided between the gate metal electrode 13 and the interlayer insulating film 9. A contact plug 14 may be embedded in the contact hole 16 formed in the interlayer insulating film 9. The contact plug 14 is, for example, a metal film made of tungsten (W) that has high embedding properties.
[0036] In addition, the edge termination region 60 includes p - A breakdown voltage structure such as a p-type RESURF region 24 and a p-type guard ring may be provided. A channel stopper 23 may be provided outside the breakdown voltage structure, and a field plate (not shown) may be provided on the n-type channel stopper 23. - The RESURF region 24 and the channel stopper 23 may be provided in an annular shape on the outer periphery of the chip.
[0037] In the first embodiment, the source electrode 10 has a two-layer structure in which a first source electrode (lower electrode) 10a provided on the interlayer insulating film 9 and a second source electrode (upper electrode) 10b provided on the first source electrode 10a are laminated. The first source electrode 10a and the second source electrode 10b may be formed of the same material, for example, Al-Si, Al-Si-Cu, or Al-Cu. Since Al has high interdiffusibility with the semiconductor substrate and forms an alloyed spike, which deteriorates the characteristics, it is not preferable to form the first source electrode 10a from Al, but the second source electrode 10b, which is not in direct contact with the semiconductor substrate, may be formed from Al. A Cu-based metal such as Cu may be used as the second source electrode 10b. The first source electrode 10a and the second source electrode 10b have the same thickness, which is about 3 μm to 7 μm, which is the same as the thickness of a normal source electrode. Moreover, it is preferable that the surface of the first source electrode 10a in contact with the second source electrode 10b is flatter than the interlayer insulating film 9 and has small surface unevenness. Having small surface unevenness means that the difference between the highest and lowest points from the surface of the n-type drift layer 2 is small.
[0038] 5 and 6 are plan views showing the structure of the semiconductor device according to the first embodiment. As shown in FIG. 5, the second source electrode 10b preferably has a recess 19 extending in a direction (x direction, second direction) perpendicular to the longitudinal direction (y direction, first direction) of the contact hole 16. The recess 19 is, for example, a stripe shape having a longitudinal direction in the x direction. The recess 19 is, for example, a portion where the second source electrode 10b is not present on the first source electrode 10a as shown in FIG. 4. The recess 19 may also be, for example, a portion where the second source electrode 10b is thin on the first source electrode 10a.
[0039] The wire connected to the source electrode 10 has a thickness of 100 μm or more and 500 μm or less. However, since the thickness of the source electrode 10 becomes thinner when the wire enters the recess 19, it is preferable that the width W1 (see FIG. 4) of the recess 19 is larger than the width of the unit cell and smaller than the thickness of the wire. Furthermore, it is preferable that the width of the recess in the long side direction is larger than the diameter of the wire and smaller than the active region dimension. It is also preferable that the pitch in the short side direction represented by the sum of the width of the second source electrode 10b and the recess is larger than twice the cell size and smaller than half the diameter of the wire. Since the thickness of the wire connected to the source electrode 10 is overwhelmingly larger than the thickness of the first source electrode 10a and the second source electrode 10b and the width W1 of the recess 19, the source electrode under the wire does not become thinner during wire bonding because the width W1 of the recess 19 is filled.
[0040] Thus, in embodiment 1, there is a thick region that is about twice as thick as a normal source electrode, and the current flowing through the thick region increases, so that the resistance of the surface electrode composed of first source electrode 10a and second source electrode 10b can be reduced.
[0041] Here, Fig. 3a is a cross-sectional view showing a current flow in the source electrode of the semiconductor device according to the first embodiment. Fig. 3a is an enlarged view of the dotted line portion in Fig. 3. As shown in Fig. 3a, in the first embodiment, the extending direction of the recess 19 and the longitudinal direction of the contact hole 16 are perpendicular to each other, so that the second source electrode 10b can uniformly extract the current I flowing through the first source electrode 10a.
[0042] In contrast, FIG. 3b is a cross-sectional view showing the flow in the source electrode when the extending direction of the recess is parallel to the longitudinal direction of the contact hole. As shown in FIG. 3b, in this case, since there is a recess in the direction of flow of the current I, even if the second source electrode 10b extracts the current I flowing in the first source electrode 10a, it must return it to the first source electrode 10a, and the current I flowing in the first source electrode 10a cannot be extracted uniformly. In this way, by making the extending direction of the recess 19 perpendicular to the longitudinal direction of the contact hole 16, it becomes difficult to be affected by the thin area of the front electrode having a high sheet resistance, and the resistance of the front electrode can be reduced more than when the extending direction of the recess 19 is parallel to the longitudinal direction of the contact hole 16.
[0043] As shown in FIG. 6, the connection direction (wire bonding direction) of the wire 25, which is the direction in which the wire 25 extends, is preferably perpendicular to the extension direction (x direction) of the recess 19. In this case, the long side T of the region L where the wire 25 contacts the source electrode 10 is the wire bonding direction, and when a current flows from the side S on the y direction side of the semiconductor device 70 to the region L, the surface electrode is thin, and the number of times the current passes through the recess 19 with high resistance is reduced, thereby reducing the sheet resistance. In addition, when a plurality of regions L where the wire 25 contacts the source electrode 10 are provided, it is preferable that the number of low-resistance recesses 19 in the wire bonding direction (y direction) between adjacent regions L is small. In the example of FIG. 6, two regions L are provided, and one recess 19 is provided in the y direction between them.
[0044] In addition, the second source electrode 10b thickens the source electrode 10, thereby reducing wire bonding damage, and reducing the yield rate and deterioration of characteristics. Furthermore, the thick source electrode 10 can reduce the intrusion of mobile ions in the plating solution even in elements that form plating electrodes on their surfaces, improving the reliability of the semiconductor elements. Furthermore, by providing the recess 19 in the second source electrode 10b, the surface area of the source electrode 10 is increased, improving heat dissipation.
[0045] (Method of Manufacturing a Semiconductor Device According to the First Embodiment) Next, a method for manufacturing the semiconductor device according to the first embodiment will be described. Figs. 7 to 11 are cross-sectional views showing the semiconductor device according to the first embodiment in the process of being manufactured. The method for forming a MOS gate structure on the front surface side of the semiconductor substrate is the same as in the existing manufacturing method, and therefore is not shown in the figures. First, n + The n-type drain layer + A type semiconductor substrate 1 is prepared. Next, + On the front surface of the n-type semiconductor substrate 1, + An n-type drift layer 2 having a low impurity concentration is epitaxially grown on a n-type semiconductor substrate 1.
[0046] Next, an oxide film mask is formed at a predetermined position on the surface of the n-type drift layer 2 by photolithography and etching. Next, using the formed oxide film mask as a mask, ion implantation of p-type impurities, such as boron (B), is performed to form a p-type base layer 5 in the surface layer of the n-type drift layer 2. At the same time, a channel stopper 23 may be formed on the surface side of the n-type drift layer 2 and on the end side of the edge termination region 60 (opposite the active region 50). The channel stopper 23 may be either n-type or p-type. The channel stopper 23 may be formed by ion implantation of n-type impurities, such as phosphorus (P) or p-type impurities, such as boron (B). Next, ion implantation of p-type impurities, such as boron (B), is performed on the surface side of the n-type drift layer 2 and on the active region 50 side of the edge termination region 60 to form a p-type base layer 5. - A type RESURF region 24 may be formed.
[0047] Next, a trench oxide film mask (not shown) having a predetermined opening width is formed by photolithography on the surface of the p-type base layer 5. Next, a trench 18 reaching the n-type drift layer 2 is formed by dry etching.
[0048] Next, isotropic etching is performed to remove damage to the trench 18, and sacrificial oxidation is performed to round the corners of the bottom of the trench 18 and the opening of the trench 18. Only one of the isotropic etching and the sacrificial oxidation may be performed. Also, the sacrificial oxidation may be performed after the isotropic etching.
[0049] Next, the gate insulating film 7 is formed along the surface of the p-type base layer 5 and the bottom and sidewalls of the trench 18. This gate insulating film 7 may be formed by thermal oxidation at a temperature of about 1000° C. in an oxygen atmosphere. Alternatively, this gate insulating film 7 may be formed by a method of deposition by a chemical reaction such as high temperature oxidation (High Temperature Oxide: HTO).
[0050] Next, polysilicon made of, for example, a polycrystalline silicon layer (Poly-Si) doped with phosphorus atoms is formed on the gate insulating film 7. Next, the active region 50 is etched to leave polysilicon that will become the gate electrode 8 inside the trench 18, and polysilicon that will become the conductive film 22 in the edge termination region 60. At this time, the polysilicon embedded in the trench 18 may be etched by performing etch-back so as to be left inside the surface of the n-type drift layer 2, or may be patterned and etched so as to protrude outside the surface of the n-type drift layer 2. As a result, in the edge termination region 60, at least the polysilicon is electrically connected to the gate electrode 8 in the trench 18, and the conductive film 22 is left so as to form a field plate that covers the field oxide film 20.
[0051] Next, a mask having desired openings is formed on the surface of the p-type base layer 5 by photolithography, for example, using a resist. Then, using this resist mask as a mask, n-type impurities are ion-implanted by ion implantation. As a result, n-type impurities are implanted into a part of the surface region of the p-type base layer 5. + A type source region 6 is then formed. + The mask used in the ion implantation for forming the n-type source region 6 is removed. +A heat treatment is then performed to activate the source region 6 .
[0052] In the above manufacturing method, the gate structure consisting of the trench 18, the gate insulating film 7, and the gate electrode 8 is formed after the formation of the p-type base layer 5, but the p-type base layer 5 may be formed after the formation of the gate structure. By forming the p-type base layer 5 after the formation of the gate structure, it is possible to easily adjust the concentration of the p-type base layer 5. + After the source region 6 is formed, a gate structure composed of a trench 18, a gate insulating film 7 and a gate electrode 8 may be formed.
[0053] Next, an interlayer insulating film 9 made of, for example, phosphorus glass and having a thickness of about 1 μm is formed so as to cover the gate electrode 8. Next, the interlayer insulating film 9 is patterned by photolithography. + The contact hole 16 is formed to expose the p-type source region 6 and the p-type base layer 5. In the active region 50 and the peripheral portion 55 of the active region, the contact hole 16 is + The doped ...
[0054] Next, p-type impurities are ion-implanted into the surface side of the p-type base layer 5 exposed by the contact hole 16, thereby forming a p ++ A contact region 33 may be formed. ++ The contact region 33 is an n + The contact hole 16 is formed immediately after the formation of the n-type source region 6, and the contact hole 16 is formed through the interlayer insulating film 9 and the n-type source region 6. + The p-type source region 6 is penetrated ++ It may be formed so as to be in contact with the mold contact region 33 .
[0055] A method for manufacturing the source electrode 10 of the first embodiment will be described below. First, a metal film such as aluminum or an alloy mainly composed of aluminum is formed on the interlayer insulating film 9 by sputtering or the like. Next, the metal film is separated into electrodes in the active region 50 and the edge termination region 60 to form the first source electrode 10a and the gate metal electrode 13. The state up to this point is shown in FIG. 7. In FIGS. 7 to 11, the semiconductor substrate 30 is used, and detailed descriptions of the internal MOS structure are omitted.
[0056] Before forming the metal film, a barrier metal 15 made of a titanium film (Ti), a titanium nitride film (TiN), or a laminated film of these (for example, Ti / TiN, etc.) may be formed by sputtering. A contact plug 14 may be embedded in the contact hole 16 via the barrier metal 15. The material of the contact plug 14 may be tungsten (W). The contact plug 14 may be formed by forming a tungsten film by a CVD method and then etching back the tungsten film. During the etch-back, the barrier metal 15 may also be etched, or the barrier metal 15 may be left unetched. In this case, it is preferable to use a trench contact structure because parasitic bipolar action can be suppressed. Here, the trench contact structure is formed by forming an interlayer insulating film 9 and an n + The p-type source region 6 is ++ This is a contact structure in which a contact hole 16 in contact with a mold contact region 33 is filled with a contact plug 14 .
[0057] Next, a lift-off resist 35 is applied onto the first source electrode 10a, the gate metal electrode 13, and the interlayer insulating film 9, a mask 36 having an opening in the region where the second source electrode 10b is to be formed is formed, and exposure 37 is performed. This opening is formed so that its longitudinal direction is perpendicular to the longitudinal direction of the contact hole 16. The state up to this point is shown in FIG. 8. Next, the lift-off resist 35 is patterned, and the resist 35 is removed from the region where the second source electrode 10b is to be formed. The state up to this point is shown in FIG. 9.
[0058] Next, a metal film 34 of aluminum or an alloy mainly composed of aluminum is formed by sputtering or the like on the lift-off resist 35. In the opening of the lift-off resist 35, the metal film 34 is formed on the first source electrode 10a. The state up to this point is shown in FIG.
[0059] Next, the lift-off resist 35 and the metal film 34 formed on the lift-off resist 35 are removed (lift-off) to form the second source electrode 10b. The state up to this point is shown in FIG. 11. As a result, in the active region 50, the source electrode 10 is connected to the n-type source electrode 10 via the barrier metal 15 and the contact plug 14. + Type source region 6 and p ++ In the active region outer periphery 55, the source electrode 10 is connected to the p-type contact region 33. In the active region outer periphery 55, the source electrode 10 is connected to the p-type base layer 5 via the barrier metal 15 and the contact plug 14. In the edge termination region 60, the gate metal electrode 13 is connected to the conductive film 22 via the barrier metal 15 and the contact plug 14. Thus, in the first embodiment, by lifting off the metal film 34, the second source electrode 10b having a recess extending in a direction perpendicular to the longitudinal direction of the contact hole 16 is formed on the first source electrode 10a, forming a region that is about twice as thick as a normal source electrode.
[0060] Next, n + On the surface of the n-type semiconductor substrate 1 (the back surface of the semiconductor base), a metal film such as nickel (Ni), titanium (Ti), gold (Au), silver (Ag), aluminum (Al), an alloy mainly composed of aluminum, or a laminated film of these (for example, Ti / Ni / Au, Al / Ti / Ni / Au, etc.) is formed as a back electrode 11. Then, the n-type semiconductor substrate 1 is heat-treated to form a back electrode 11. + An ohmic junction is formed between the back surface electrode 11 and the semiconductor substrate 1. This completes the trench MOSFET 70 shown in FIGS.
[0061] As described above, according to the first embodiment, the source electrode has a two-layer structure in which a first source electrode provided on an interlayer insulating film and a second source electrode provided on the first source electrode are laminated, and the second source electrode has a recess extending in a direction perpendicular to the longitudinal direction of the contact hole. As a result, compared to a normal source electrode, there is a thick region that is about twice as thick, and the current flowing in the thick region increases, so that the resistance of the surface electrode including the first source electrode and the second source electrode can be reduced.
[0062] (Embodiment 2) Next, a second embodiment will be described. An enlarged plan view showing the structure of the semiconductor device according to the second embodiment is the same as FIG. 1 of the first embodiment, and therefore will not be described. FIG. 12 is a cross-sectional view taken along X1-X1 in FIG. 1 showing the structure of the semiconductor device according to the second embodiment. FIG. 13 is a cross-sectional view taken along X2-X2 in FIG. 1 showing the structure of the semiconductor device according to the second embodiment. FIG. 14 is a cross-sectional view taken along Y1-Y1 in FIG. 1 showing the structure of the semiconductor device according to the second embodiment.
[0063] As shown in FIG. 14, in the second embodiment, the second source electrode 10b has a recess 19 extending in a direction (x direction) perpendicular to the longitudinal direction (y direction) of the contact hole 16 on the first source electrode 10a side. The recess 19 between adjacent second source electrodes 10b is filled with an insulating film 26. By providing the insulating layer 26 in the source electrode 10 in this manner, it is possible to uniformly provide a thick region of the surface electrode composed of the first source electrode 10a and the second source electrode 10b and a region where the surface electrode has a normal thickness. The thickness, material, etc. of the first source electrode 10a and the second source electrode 10b are the same as those of the first embodiment.
[0064] Furthermore, the thickness T1 of the insulating film 25 in the active region 50 and the active region outer periphery 55 is preferably 1 μm or more and 5 μm or less (see FIG. 12). Furthermore, the thickness T2 of the second source electrode 10b on the insulating film 25 is preferably 0.5 to 5 times the width W2 (the distance between adjacent insulating layers 26) of the contact hole 17 in the insulating layer 26 (see FIG. 14). By setting the thickness within this range when filling the metal film 34 using the sidewall between the insulating films 26 as described later, the metal film 34 can be filled in the contact hole 17 without voids, and the second source electrode 10b can be formed in the contact hole 17.
[0065] Thus, in the second embodiment, as in the first embodiment, there is a thick region that is about twice as thick as a normal source electrode, and the current flowing through the thick region increases, thereby reducing the resistance of the surface electrode.
[0066] (Method of Manufacturing a Semiconductor Device According to the Second Embodiment) Next, a method for manufacturing a semiconductor device according to a second embodiment will be described. FIGS. 15 to 25 are cross-sectional views showing a state during the manufacturing process of the semiconductor device according to the second embodiment. As in the first embodiment, first, n + The n-type drain layer + A semiconductor substrate 1 is prepared, an n-type drift layer 2 and a p-type base layer 5 are formed, and an n-type semiconductor layer is formed in the p-type base layer 5. + Type source region 6, p ++ A trench MOS structure is formed, which is composed of the type contact region 33, the trench 18, the gate insulating film 7 and the gate electrode 8. Next, as in the first embodiment, an interlayer insulating film 9 is formed on the MOS structure, and a contact structure in which the contact plug 14 is embedded is formed.
[0067] Next, a metal film of aluminum or an alloy mainly composed of aluminum, or an alloy mainly composed of copper, etc. is formed by sputtering or the like. Next, the metal film is separated into electrodes in the active region 50 and the edge termination region 60 to form the first source electrode 10a and the gate metal electrode 13. The state up to this point is shown in FIG. 15. In FIGS. 15 to 25, it is referred to as a semiconductor substrate 30, and detailed descriptions of the internal MOS structure are omitted.
[0068] Next, an insulating film 26 is formed on the first source electrode 10a, the gate metal electrode 13, and the interlayer insulating film 9, and a resist 35 is applied onto the insulating film 26 to form a mask 36 having an opening in the region where the second source electrode 10b contacts the first source electrode 10a, and exposure 37 is performed. This opening is formed so that its longitudinal direction is perpendicular to the longitudinal direction of the contact hole 16. The insulating layer 26 is formed of, for example, inorganic SiO2, SiN, or organic polyimide resin (PI). The state up to this point is shown in FIG.
[0069] Next, the resist 35 is patterned and removed from the region where the second source electrode 10b contacts the first source electrode 10a. The state up to this point is shown in FIG. 17. Next, the insulating film 26 is etched to partially expose the first source electrode 10a. The state up to this point is shown in FIG. 18. Next, the resist 35 is peeled off to expose the insulating film 26. This forms the insulating film 26 whose longitudinal direction is perpendicular to the longitudinal direction of the contact hole 16. The state up to this point is shown in FIG. 19.
[0070] Next, a metal film 34 of aluminum or an alloy mainly composed of aluminum is formed on the insulating film 26 and the first source electrode 10a by sputtering or the like. In the opening of the insulating film 26, the metal film 34 is formed on the first source electrode 10a. The state up to this point is shown in FIG.
[0071] Next, a resist 35 is applied onto the metal film 34. The state up to this point is shown in FIG. 21. Next, a mask 36 having an opening in a region corresponding to the active region outer periphery 55 is formed, and exposure 37 is performed. The state up to this point is shown in FIG. 22. Next, the resist 35 is patterned to form an opening in a region corresponding to the active region outer periphery 55. The state up to this point is shown in FIG. 23. Next, the metal film 34 is separated into electrodes in the active region 50 and the edge termination region 60 to form the second source electrode 10b and the gate metal electrode 13. The state up to this point is shown in FIG. 24. Next, the resist 35 is peeled off to expose the second source electrode 10b and the gate metal electrode 13. The state up to this point is shown in FIG. 25.
[0072] Thus, in the second embodiment, a patterned insulating film 26 is formed, a metal film 34 is embedded in the insulating film 26, and a sidewall between the insulating films 26 is used to form a second source electrode 10b having a recess 19 extending in a direction perpendicular to the longitudinal direction of the contact hole 16 on the first source electrode 10a, thereby forming a thick region about twice as thick as a normal source electrode. Thereafter, a back electrode 11 is formed in the same manner as in the first embodiment. This completes the trench MOSFET 70 shown in FIGS. 12 to 14.
[0073] In the manufacturing method of the second embodiment described above, the gate metal electrode 13 is also formed to have the same structure as the source electrode 10, and is a two-layer electrode having a recess 19 with the insulating film 26 sandwiched between the upper electrode, but the gate metal electrode 13 may be a single layer having the same thickness as the first source electrode 10a. This is because the gate metal electrode 13 does not pass a large current like the source electrode 10.
[0074] As described above, according to the second embodiment, the second source electrode has a recess extending in a direction perpendicular to the longitudinal direction of the contact hole on the first source electrode side, and the recess between adjacent second source electrodes is filled with an insulating film. Therefore, it is possible to uniformly provide a thick region of the surface electrode and a region where the surface electrode has a normal thickness.
[0075] In the above, the present invention has been described with reference to an example in which a MOS gate structure is formed on the first main surface of a silicon substrate, but the present invention is not limited to this and can be modified in various ways with respect to the type of semiconductor (e.g., silicon carbide (SiC) and the like), the surface orientation of the main surface of the substrate, and the like. In addition, the present invention has been described with reference to an example of a trench-type MOSFET, but the present invention is not limited to this and can be applied to MOS-type semiconductor devices such as planar-type MOSFETs and IGBTs, and semiconductor devices of various configurations such as diodes. In addition, in each embodiment of the present invention, the first conductivity type is n-type and the second conductivity type is p-type, but the present invention is similarly valid even if the first conductivity type is p-type and the second conductivity type is n-type. [Industrial Applicability]
[0076] INDUSTRIAL APPLICABILITY As described above, the semiconductor device and the method for manufacturing the semiconductor device according to the present invention are useful for high-voltage semiconductor devices used in power conversion devices and power supply devices for various industrial machines. [Explanation of symbols]
[0077] 1n + Semiconductor Substrate 2 n-type drift layer 5 p-type base layer 6n + Type Source Area 7 Gate insulating film 8. Gate electrode 9 Interlayer insulating film 10 Source electrode 10a First source electrode 10b Second source electrode 11 Back electrode 13 Gate metal electrode 14 Contact plug 15 Barrier Metal 16 Contact Hole 17 Contact hole in insulating film 18 Trench 19 Recess 20 Field oxide 22 Conductive Film 23 Channel Stopper 24 pages- Type RESURF region 25 Wire 26 Insulating Film 30 Semiconductor substrate 33 p ++ Mold Contact Area 34 Metal Film 35 Resist 36 Mask 37 Exposure 50 active area 55 Active area outer periphery 60 Edge Termination Area 70 Semiconductor Devices x Extension direction of the recess y Longitudinal direction of the contact hole I current
Claims
1. a semiconductor substrate of a first conductivity type; a drift layer of a first conductivity type provided on a first main surface of the semiconductor substrate; a second conductivity type base layer provided on a surface layer of the drift layer; a first conductivity type source region selectively provided in a surface layer of the base layer; a gate electrode provided on a surface of the base layer and the source region via a gate insulating film; an interlayer insulating film covering the source region and the gate electrode; a contact hole provided in the interlayer insulating film on a surface of the source region, the contact hole having a longitudinal direction in a first direction; a front surface electrode provided on the interlayer insulating film; Equipped with The semiconductor device is characterized in that the front surface electrode is composed of a lower electrode on the interlayer insulating film and an upper electrode on the lower electrode, and the upper electrode has a recess extending in a second direction perpendicular to the first direction.
2. 2. The semiconductor device according to claim 1, wherein the upper electrode is in the form of a stripe having a longitudinal direction in the second direction.
3. 2. The semiconductor device according to claim 1, wherein the contact holes are in a stripe shape having a longitudinal direction in the first direction.
4. A conductive wire is further provided which is connected to the front surface electrode.
2. The semiconductor device according to claim 1, wherein the wire is connected in the first direction.
5. 5. The semiconductor device according to claim 4, wherein the width of the recess in the short side direction is smaller than the diameter of the wire.
6. 2. The semiconductor device according to claim 1, wherein a surface of said lower electrode that contacts said upper electrode is flatter than a surface of said interlayer insulating film.
7. 2. The semiconductor device according to claim 1, wherein the lower electrode is made of Al--Si, Al--Si--Cu, or Al--Cu.
8. 2. The semiconductor device according to claim 1, wherein the upper electrode is made of Al, Al--Si, Al--Si--Cu, Al--Cu, Al, or Cu.
9. the recess is provided on a surface of the upper electrode that contacts the lower electrode, 2. The semiconductor device according to claim 1, wherein the recess is filled with an insulating film.
10. 10. The semiconductor device according to claim 9, wherein the thickness of the upper electrode on the insulating film is 0.5 to 5 times the distance between adjacent insulating films.
11. The insulating film is made of inorganic SiO 2 10. The semiconductor device according to claim 9, wherein the semiconductor device is made of SiN or an organic polyimide resin.
12. a first step of forming a drift layer of a first conductivity type on a first main surface of a semiconductor substrate of a first conductivity type; a second step of forming a base layer of a second conductivity type on a surface layer of the drift layer; a third step of selectively forming a source region of a first conductivity type in a surface layer of the base layer; a fourth step of forming a gate electrode on a surface of the base layer and the source region via a gate insulating film; a fifth step of forming an interlayer insulating film covering the source region and the gate electrode; a sixth step of forming a contact hole having a longitudinal direction in a first direction in the interlayer insulating film on a surface of the source region; a seventh step of forming a front surface electrode on the interlayer insulating film; Including, The seventh step comprises: forming a lower electrode on the interlayer insulating film; forming an upper electrode on the lower electrode, the upper electrode having a recess extending in a second direction perpendicular to the first direction; 2. A method for manufacturing a semiconductor device comprising the steps of:
13. The seventh step comprises: forming the lower electrode on the interlayer insulating film; forming a resist on the lower electrode; forming an opening in the resist that reaches the lower electrode; forming a metal film on the resist and the opening; removing the metal film on the resist and the resist to form the upper electrode on the lower electrode; 13. The method for manufacturing a semiconductor device according to claim 12, further comprising:
14. The seventh step comprises: forming the lower electrode on the interlayer insulating film; forming an insulating film on the lower electrode; forming an opening in the insulating film reaching the lower electrode; forming a metal film on the insulating film and in the opening to form the upper electrode on the lower electrode; 13. The method for manufacturing a semiconductor device according to claim 12, further comprising:
Citation Information
Patent Citations
Method of manufacturing semiconductor device
JP2003101024A
Semiconductor device and its manufacturing method