Metal oxide film
A metal oxide film with alternating crystal structures and controlled deposition methods addresses grain boundary and oxygen vacancy issues, enhancing stability and reliability in semiconductor devices.
Patent Information
- Application Number
- JP2024151312
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-09-03
- Publication Date
- 2024-11-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing semiconductor devices using metal oxide films face challenges in achieving stable physical properties and reliable performance due to grain boundaries and oxygen vacancies, which affect electrical characteristics and device reliability.
A metal oxide film with a novel structure is developed, featuring alternating regions with different periodic crystal structures and shared layers, minimizing grain boundaries and reducing oxygen vacancies through controlled deposition and heat treatment processes.
The novel metal oxide film achieves high structural stability, reducing defects and fluctuations in electrical properties, leading to highly reliable semiconductor devices with improved performance.
Smart Images

Figure 2024161184000001_ABST
Abstract
Description
[Technical field]
[0001] One embodiment of the present invention relates to a metal oxide film. Regarding placement.
[0002] In this specification and the like, a semiconductor device is a device that can function by utilizing semiconductor characteristics. Refers to devices in general, including transistors, semiconductor circuits, memory devices, imaging devices, electro-optical devices, and power generation devices. Devices (including thin-film solar cells, organic thin-film solar cells, etc.) and electronic devices can also be considered semiconductor devices. do. [Background technology]
[0003] A technology for constructing transistors using semiconductor films formed on substrates with insulating surfaces The transistor is used in integrated circuits (ICs) and image display devices (also known simply as display devices). These are widely used in electronic devices such as semiconductors that can be used in transistors. Silicon-based semiconductor materials are widely known as semiconductor films, but other materials with semiconductor properties are also available. Metal oxides (oxide semiconductors) that exhibit this property have been attracting attention.
[0004] For example, amorphous oxides containing In, Zn, Ga, Sn, etc. are used as oxide semiconductors. Patent Document 1 discloses a technique for fabricating a transistor using this method. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2006-165529 A Summary of the Invention [Problem to be solved by the invention]
[0006] An object of one embodiment of the present invention is to provide a metal oxide film having a novel structure. .
[0007] Another object of one embodiment of the present invention is to provide a metal oxide film having highly stable physical properties. It shall be one.
[0008] Another embodiment of the present invention provides a highly reliable semiconductor device to which the above-described metal oxide is applied. One of our goals is to provide
[0009] The description of these problems does not preclude the existence of other problems. It is not necessary for one embodiment to solve all of these problems. The subject matter will be self-evident from the description, drawings, claims, etc. Other issues can be extracted from the drawings, claims, etc. [Means for solving the problem]
[0010] One aspect of the present invention is a crystal that contains In, Ga, and Zn, and in a cross-sectional observation image, In atoms are periodically arranged. and a second layer in which Ga atoms or Zn atoms are periodically arranged. A first region is observed, the first region having a pair of first layers and n (n is a natural number) second layers between the pair of first layers; a second region having m (m is a natural number other than n) second layers between another pair of first layers; The metal oxide film has the following structure:
[0011] In the metal oxide film, the first region and the second region are parallel to the first layer. and at the boundary between the first region and the second region, one of the first regions is adjacent to the first region in the vertical direction. It is preferred that the layers are shared.
[0012] Alternatively, the first region and the second region are adjacent to each other in a direction parallel to a plane parallel to the first layer. It is preferable that one first layer is continuous at the boundary between the first region and the second region. stomach.
[0013] In the first region or the second region of the metal oxide film, the first layer is a coating. It is preferably parallel to the forming surface.
[0014] In addition, no grain boundary is observed between the first region and the second region in the metal oxide film. It is preferable that
[0015] Further, one aspect of the present invention is a semiconductor device comprising any one of the above metal oxide films, a gate electrode, and a metal oxide A gate insulating layer is provided between the film and the gate electrode, and a source electrode and a and a drain electrode, and a channel is formed in the metal oxide film. .
[0016] In this specification, the term "plane A is parallel to plane B" refers to the angle between the normal to plane A and the normal to plane B. In this specification, the C-plane is defined as a plane having an angle of -20° or more and 20° or less. Perpendicular to surface B means that the angle between the normal line of surface C and the normal line of surface B is between 70° and 110°. In addition, in this specification, the expression "line C is approximately perpendicular to surface B" refers to the normal between line C and surface B. This refers to a state in which the angle between the lines is between -20° and 20°. Effect of the Invention
[0017] According to the present invention, it is possible to provide a metal oxide film having a novel structure. Alternatively, a highly reliable metal oxide film using the above-mentioned metal oxide can be provided. A semiconductor device can be provided. [Brief description of the drawings]
[0018] [Figure 1] 1A to 1C are diagrams illustrating a metal oxide film according to an embodiment; [Diagram 2] 1A to 1C are diagrams illustrating a metal oxide film according to an embodiment; [Diagram 3] 1A to 1C are diagrams illustrating a crystal structure of a metal oxide according to an embodiment; [Figure 4] 1A to 1C are diagrams illustrating a crystal structure contained in a metal oxide film according to an embodiment; [Diagram 5] 1A to 1C illustrate examples of the structure of a transistor according to an embodiment. [Figure 6] 1A to 1C illustrate an example of a method for manufacturing a transistor according to an embodiment. [Figure 7] 1A to 1C illustrate examples of the structure of a transistor according to an embodiment. [Figure 8] 1A to 1C are diagrams illustrating a structure of a display panel according to an embodiment. [Figure 9] 1A to 1C are block diagrams illustrating electronic devices according to an embodiment. [Figure 10] 1A to 1C are diagrams illustrating external views of electronic devices according to an embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] The embodiment will be described in detail with reference to the drawings. However, the present invention is not limited to the following description. The present invention is not limited to the above embodiment, and various changes and modifications may be made in the form and details without departing from the spirit and scope of the present invention. It will be easily understood by those skilled in the art that the present invention can be realized by the following embodiments. The present disclosure should not be construed as being limited to the contents of the preceding paragraph.
[0020] In the configuration of the invention described below, the same parts or parts having similar functions are The same reference numerals are used in common between different drawings, and the repeated explanations are omitted. When referring to a function, the hatch pattern may be the same and no particular symbol may be used.
[0021] In each figure described in this specification, the size, layer thickness, or area of each component is indicated by the following formula: The figures may be exaggerated for clarity and are not necessarily limited to scale. stomach.
[0022] (Embodiment 1) In this embodiment, a metal oxide film according to one embodiment of the present invention will be described with reference to drawings. .
[0023] [Crystal structure of metal oxide film] The metal oxide film of one embodiment of the present invention has a metal oxide containing two or more different metal elements. In addition, the metal oxide is an oxide whose crystal structure can have a layered structure, and Alternatively, an oxide that can exhibit a different periodic structure due to differences in composition can be used.
[0024] Various periodic structures that appear due to differences in composition are also called homologous phases. When the crystal structure is a layered structure in which layer A containing metal A and layer B containing metal B are arranged in layers, In this case, the number of B layers sandwiched between a pair of A layers changes continuously depending on the composition. As a result, different periodic structures are realized depending on the composition. A structure that can have different periodic structures depending on the composition is called a homologous structure.
[0025] For example, In-Ga-Zn oxide is InGaO_3(ZnO). m (m is a natural number) The homologous structure shown in Fig. 3 is an example of the crystal structure of an In-Ga-Zn oxide. The crystal structure shown in FIG. 3(A) is InGaO_3(ZnO) m(m=1) The crystal structure shown in FIG. 3(B) is that of InGaO_3(ZnO). m The crystal structure shown in FIG. 3(C) is InGa O_3(ZnO) m This is the crystal structure represented as (m=3).
[0026] The metal oxide film according to one embodiment of the present invention has regions having different crystal structures (periodic structures) in the film. It is characterized by a mixture of regions.
[0027] For example, when In-Ga-Zn oxide is used as the metal oxide, the A layer made of an oxide of Ga and Zn (Ga, Zn It has a layered structure in which two layers, the crystalline layer (also written as the crystalline layer) and the crystalline layer (also called the crystalline layer O), are arranged in layers.
[0028] Furthermore, the number of (Ga, Zn)O layers sandwiched between a pair of InO2 layers can be varied. For example, the structure shown in FIG. 4(A) has a layer of (Ga,Zn) between a pair of InO2 layers. )O layers. The structure shown in FIG. 4(B) has two (Ga The structure shown in FIG. 4(C) has a Ga, Zn)O layer (also called a (Ga, Zn)2O2 layer). The structure is a pair of InO2 layers, with three (Ga, Zn)O layers (also called (Ga, Zn)3O3 layers) between them. (hereinafter referred to as "the Company").
[0029] In this way, the metal oxide film of one embodiment of the present invention uses an In-Ga-Zn-based oxide. In the case of the metal oxide film, the number of (Ga, Zn)O layers between a pair of InO2 layers is It contains two or more different crystalline regions.
[0030] Crystal regions contained in metal oxides can be seen, for example, by a transmission electron microscope (TEM). It can be observed by using a scanning electron microscope (STEM) or other methods. In addition, the crystalline regions observed by TEM were further analyzed using techniques such as electron diffraction. The crystal structure can also be identified by analyzing the crystal.
[0031] Here, for example, a scanning transmission electron microscope (STEM) is used to observe the cross section of a metal oxide film. canning Transmission Electron Microscopy ) Therefore, it is difficult to observe oxygen atoms, which are a light element, when observing at high resolution. Only the arrangement of metal atoms can be confirmed.
[0032] Next, FIG. 1 shows a cross-sectional observation image of a metal oxide film according to one embodiment of the present invention.
[0033] Here, as an example of a metal oxide film, an In-Ga-Zn oxide film is formed on a quartz glass substrate. The metal oxide film shown in Fig. 1 was formed under the following conditions: In Sputtering using an oxide target with an atomic ratio of Ga:Zn=1:1:1 According to the method, under oxygen atmosphere (flow rate 45sccm), pressure 0.4Pa, direct current (DC) power supply power The power was 0.5 kW, and the substrate temperature during film formation was room temperature. The metal oxide film after the heat treatment was subjected to ion milling. The specimens were then sliced by a microscope to prepare samples for cross-sectional observation.
[0034] Cross-sectional observation was performed using a transmission electron microscope (Hitachi High-Technologies Corporation: HD-2700) with accelerating current. The voltage was 200 kV and the magnification was 12 million times. Annular Dark-Field Scanning Transmissio The electron microscopy images were observed.
[0035] As shown in Figure 1, in the metal oxide film, there are atoms (specifically, electrons) that are observed to have high brightness. ) and layers with periodic arrangement of atoms that are observed to have low brightness. Here, the atoms observed to have high brightness are In atoms, and the atoms observed to have low brightness are In atoms. The electrons are Ga or Zn atoms.
[0036] An enlarged view of the region 1 enclosed by the dashed line in FIG. 1(A) is shown in FIG. 1(B). Between the layers in which Ga atoms or Zn atoms are periodically arranged, there are two layers in which Ga atoms or Zn atoms are periodically arranged. It can be confirmed that it exists.
[0037] As mentioned above, the O atoms that make up the metal oxide cannot be directly observed in the cross-sectional observation images. Therefore, it is difficult to know the composition of O atoms and the bonding state between O atoms and metal atoms from cross-sectional observation images. Therefore, in the following, we will focus on the periodic arrangement of atoms obtained from the cross-sectional observation image. The layer of electrons (specifically, electrons) is an InO2 layer or a (Ga, Zn)O layer in an actual crystal structure. This will be noted separately from layers such as
[0038] Specifically, in the cross-sectional observation image, a layer in which pairs of In atoms are periodically arranged is In the cross-sectional observation image, Ga atoms or Zn atoms are A layer in which atoms are periodically arranged is referred to as the (Ga, Zn) layer, or the second layer.
[0039] In addition, when metal oxides other than In-Ga-Zn oxides were used, Among the multiple layers that are periodically arranged and observed, the brightest atom (those with equal brightness) The first layer is the first one, the second layer is the second one, the third layer is the third one, and so on. This will be expressed as layer etc.
[0040] Next, an enlarged view of the area 2 enclosed by the dashed line in FIG. 1(A) is shown in FIG. 1(C). It can be seen that there are three (Ga, Zn) layers between the In layers.
[0041] In this way, in the cross-sectional observation image of the metal oxide film according to one embodiment of the present invention, a pair of first A first region having n layers (n is a natural number) of second layers between the first layers, and another pair of first layers between the first layers. and a second region having m (m is a natural number other than n) layers in the first region. Let us assume that.
[0042] The types of crystal structures in the crystal regions contained in the metal oxide film are limited to two types. The crystal structure may include three or more crystalline regions having different types of crystal structures.
[0043] In addition, in Fig. 1(A), regions 1 and 2 are stacked in a direction perpendicular to the direction parallel to the In layer. Furthermore, when we look at the boundary between region 1 and region 2, we can see that one In You can see that they share layers.
[0044] In this way, regions with different crystal structures are stacked, and one of them shares an In layer. By providing two regions so that the grain boundaries do not occur between these regions, high structural integrity is achieved. Furthermore, defects in the metal oxide film caused by the presence of grain boundaries are reduced. It is possible.
[0045] In addition, as shown in FIG. 1, the upper layer of region 1 has a pair of In layers between them, just like region 2. There are three (Ga, Zn) layers in the region, and one In layer is also present between them. You can see that they share layers.
[0046] In this way, multiple regions with different crystal structures are stacked while sharing the In layer. As a result, structural stability is obtained over a wide range in the metal oxide film, A metal oxide film with reduced defects can be achieved.
[0047] FIG. 2 is a cross-sectional observation image of another portion of the above sample.
[0048] In the cross-sectional image shown in Figure 2, two (Ga, Zn) layers exist between a pair of In layers. Region 3 is mixed with region 4, which has three (Ga, Zn) layers between another pair of In layers. Regions 3 and 4 are adjacent to each other in the direction parallel to the plane parallel to the In layer. is.
[0049] Furthermore, in FIG. 2, one In layer constituting region 3 extends to region 4, and the I In other words, one In layer exists continuously between region 3 and region 4. is doing.
[0050] In this way, the In layers exist continuously between adjacent regions having different crystal structures. As a result, no grain boundaries are formed between these regions, realizing high structural stability. Furthermore, defects in the metal oxide film caused by the presence of grain boundaries can be reduced.
[0051] A metal oxide film according to one embodiment of the present invention is a metal oxide film that has high structural stability. By applying such a metal oxide film to a semiconductor layer in which a transistor channel is formed, As a result, a highly reliable transistor can be realized.
[0052] Furthermore, in the metal oxide film according to one embodiment of the present invention, the crystalline regions are continuous and the crystalline regions are Since there are no grain boundaries between the regions, the metal oxide film has reduced defects. By applying a metal oxide film to the semiconductor layer of a transistor, carrier transport due to defects can be prevented. The transistor has suppressed wrapping, high field effect mobility, and suppressed fluctuations in electrical properties. A transistor can be realized.
[0053] Note that a structural example of a transistor including a metal oxide film of one embodiment of the present invention will be described later. This will be described in the following embodiment.
[0054] [Method of forming metal oxide film] The method for forming a metal oxide film according to this embodiment will be described below.
[0055] The metal oxide film of this embodiment is formed by sputtering in an atmosphere containing oxygen. The film can be formed by performing a heat treatment after the film is formed in an atmosphere containing oxygen. By using the atmosphere, oxygen vacancies in the metal oxide film are reduced, and the crystallization is promoted by the subsequent heat treatment. It may be a membrane that includes a region.
[0056] In the metal oxide film of the present embodiment, by reducing oxygen vacancies, the film has stable physical properties. In particular, as the metal oxide film of this embodiment, a metal oxide film exhibiting semiconductor characteristics can be used. When a semiconductor device is manufactured by using a nitride film (oxide semiconductor film), The oxygen vacancies caused by the oxygen vacancies are a factor in the fluctuation of the electrical characteristics of the semiconductor device. By manufacturing a semiconductor device using an oxide semiconductor film, a highly reliable semiconductor device can be obtained. This can be done.
[0057] In the metal oxide film of this embodiment, when the oxygen partial pressure in the film formation atmosphere is increased, oxygen More specifically, the oxygen partial pressure in the film formation atmosphere is preferably It is preferable to set it to 33% or more.
[0058] The target used in the sputtering method is not limited to In-Ga-Zn oxide. In addition, multi-component metal oxides that can have a homologous structure can be used. For example, In-M -Zn-based oxide (M is Al, Ti, Ga, Y, Zr, La, Ce, Nd or Hf, etc.) It can be used.
[0059] In addition, the composition of the metal oxide contained in the target used in the sputtering method is homologous. There is no particular limitation as long as the composition can have a lattice structure. For example, in the case of an In-Ga-Zn oxide In this case, if the Ga composition is larger than Zn, it is easier to form a spinel structure rather than a layered structure. Therefore, it is preferable to have a Zn content higher than Ga content. When the Zn content in the formed metal oxide film decreases due to sublimation during film formation using this method, Therefore, it is necessary to use a target having a higher Zn content than the desired metal oxide film composition. is preferred.
[0060] In addition, when forming a metal oxide film by sputtering, the surface on which the film is to be formed is not heated. The film may be formed at room temperature or may be heated. When heating, the film is heated at 150° C. or higher for 3 hours. 00°C or higher, or 450°C or higher, for example.
[0061] After the metal oxide film is formed, a heat treatment is performed. The atoms in the film are rearranged by the heat treatment. This results in the formation of crystalline regions in the metal oxide film.
[0062] At this time, since the degree of dynamic freedom is relatively high near the membrane surface, the initial stage is The rearrangement of the adjacent atoms occurs, and a layer approximately parallel to the film surface is formed near the film surface. Then, as the crystallization progresses from the film surface toward the depth direction, multiple layers are formed approximately parallel to the film surface. A crystalline region having a multi-layer structure is formed. The first layer and the second layer are aligned in a direction parallel to the membrane surface.
[0063] Here, in the metal oxide film before the heat treatment, a distribution occurs in the metal element concentration. During the atomic rearrangement during the heat treatment, a pair of In atoms is formed in the region where the concentration of In atoms in the film is relatively high. It is believed that regions with fewer (Ga, Zn) layers between the In layers are formed. In the region where the concentration of In atoms in the film is relatively low, the (Ga,Zn As a result, regions with a higher number of crystalline layers are formed in the film. This process can be used to form a metal oxide film. The same applies to multi-component metal oxides that can have homologous structures other than the above-mentioned oxides.
[0064] For example, the film is formed at room temperature or below without heating the surface to be formed. By this, it is possible to form a metal oxide film having regions with different concentrations of metal elements. Cut.
[0065] The heat treatment is carried out at a temperature of 550° C. or higher, preferably 600° C. or higher, and more preferably 650° C. or higher. For example, heat treatment at 650°C for 1 hour is sufficient. The higher the heat treatment temperature, the better the The longer the time, the greater the proportion of crystalline regions in the metal oxide film. .
[0066] The heat treatment can be carried out, for example, in a nitrogen atmosphere or a reduced pressure atmosphere. By performing a heat treatment in an atmosphere, hydrogen in the metal oxide film can be effectively desorbed. In addition, oxygen may be released from the metal oxide film during the heat treatment. It is preferable to subsequently carry out a heat treatment in an oxygen atmosphere to reduce oxygen vacancies in the film. stomach.
[0067] In the above manner, the metal oxide film of one embodiment of the present invention can be formed.
[0068] This embodiment may be implemented in appropriate combination with other embodiment modes described in this specification. This can be done.
[0069] (Embodiment 2) In this embodiment, a metal oxide film according to one embodiment of the present invention, which has semiconductor characteristics, is A semiconductor device using a nitride semiconductor film (oxide semiconductor film) will be described with reference to the drawings. Here, a configuration example of a transistor will be described as an example of a semiconductor device.
[0070] [Transistor configuration example] FIG. 5A is a schematic cross-sectional view of a transistor 100 to be described below. The transistor 100 shown is a bottom-gate transistor.
[0071] The transistor 100 includes a gate electrode 102 provided on a substrate 101 and a An insulating layer 103 is provided on the gate electrode 102, and the gate electrode 102 is provided on the insulating layer 103. The oxide semiconductor layer 104 is provided so as to overlap with the upper surface of the oxide semiconductor layer 104. The insulating layer 103 and the oxide semiconductor layer 10 4. An insulating layer 106 covering the pair of electrodes 105a and 105b, and an insulating layer 10 on the insulating layer 106. 7 is provided.
[0072] The oxide semiconductor film of one embodiment of the present invention is applied to the oxide semiconductor layer 104 of the transistor 100. It can be used.
[0073] [Substrate 101] There is no particular restriction on the material of the substrate 101, but it should be strong enough to withstand the subsequent heat treatment. For example, a glass substrate, a ceramic substrate, a quartz substrate, a surface treatment substrate, etc. A fiber substrate, a YSZ (yttria stabilized zirconia) substrate, etc. are used as the substrate 101. In addition, a single crystal semiconductor substrate such as silicon or silicon carbide, a polycrystalline semiconductor substrate, It is also possible to use compound semiconductor substrates such as silicon germanium, SOI substrates, etc. .
[0074] In addition, a semiconductor substrate or an SOI substrate on which a semiconductor element is provided is referred to as a substrate 101. In this case, the transistor 100 is formed on the substrate 101 via an interlayer insulating layer. At this time, the gate of the transistor 100 is connected to a connection electrode embedded in the interlayer insulating layer. At least one of the electrodes 102, 105a, and 105b is electrically connected to the semiconductor element. The transistor 10 may be electrically connected to the semiconductor element via an interlayer insulating layer. By providing 0, the increase in area due to the addition of the transistor 100 is suppressed. It is possible.
[0075] A flexible substrate such as plastic is used as the substrate 101. Alternatively, the transistor 100 may be formed by connecting the substrate 101 and the transistor 100. A release layer may be provided between the semiconductor device and the semiconductor substrate. The release layer is a layer on which a part or the whole of a transistor is formed. After the formation, the semiconductor device can be separated from the substrate 101 and can be transferred to another substrate. As a result, the transistor 100 can be mounted on a substrate having poor heat resistance or a flexible substrate.
[0076] [Gate electrode 102] The gate electrode 102 may be made of any of aluminium, chromium, copper, tantalum, titanium, molybdenum, tantalum, etc. or an alloy containing the above-mentioned metals or It can be formed by using a combination of alloys, etc. Also, manganese, zirconium, etc. The gate electrode 102 may be made of a single metal. The film may have a layer structure or a laminate structure of two or more layers. For example, an aluminum film containing silicon A single-layer structure of titanium on an aluminum film, a two-layer structure of titanium on a titanium nitride film, Two-layer structure with a tungsten film laminated on a titanium nitride film, two-layer structure with a tungsten film laminated on a titanium nitride film, A two-layer structure in which a tungsten film is laminated on a titanium film or a tungsten nitride film, a titanium film, A three-layer structure in which an aluminum film is layered on the titanium film, and a titanium film is then formed on top of that. Aluminum, titanium, tantalum, tungsten, molybdenum, chromium, etc. An alloy film made by combining one or more metals selected from aluminum, neodymium, and scandium, Alternatively, a nitride film of these may be used.
[0077] The gate electrode 102 is made of indium tin oxide or indium containing tungsten oxide. Oxide, indium zinc oxide with tungsten oxide, indium oxide with titanium oxide Indium tin oxide, indium zinc oxide, silicon oxide, etc. A light-transmitting conductive material such as doped indium tin oxide can also be used. Alternatively, the light-transmitting conductive material and the metal may be laminated together.
[0078] In addition, an In-Ga-Zn-based oxynitride semiconductor is provided between the gate electrode 102 and the insulating layer 103. film, In-Sn-based oxynitride semiconductor film, In-Ga-based oxynitride semiconductor film, In-Zn-based oxynitride semiconductor film Semiconductor film, Sn-based oxynitride semiconductor film, In-based oxynitride semiconductor film, metal nitride film (InN These films have a work energy of 5 eV, preferably 5.5 eV or more. function, which is larger than the electron affinity of an oxide semiconductor. The threshold voltage of the transistor can be shifted to the positive side, and the so-called normally-off characteristic can be improved. For example, a switching element with high conductivity can be realized by using an In-Ga-Zn-based oxynitride semiconductor film. In this case, the nitrogen concentration is at least higher than that in the oxide semiconductor layer 104, specifically, 7 atomic % or more. The semiconductor layer is an In-Ga-Zn oxynitride semiconductor film.
[0079] [Insulating layer 103] The insulating layer 103 functions as a gate insulating film.
[0080] The insulating layer 103 is made of, for example, silicon oxide, silicon oxynitride, silicon nitride oxide, silicon nitride, or silicon oxide. Silicon, aluminum oxide, hafnium oxide, gallium oxide or Ga-Zn-based metal oxide The insulating film may be formed of a single layer or a laminated layer.
[0081] The insulating layer 103 is made of hafnium silicate (HfSiO x ), nitrogen is added Hafnium silicate (HfSi x O y N z ), nitrogen-doped hafnium aluminate (HfAl x O y N z ), high-k materials such as hafnium oxide and yttrium oxide The use of this material can reduce gate leakage of transistors.
[0082] [Pair of electrodes 105a, 105b] The pair of electrodes 105a and 105b are the source and drain electrodes of the transistor. It functions as such.
[0083] The pair of electrodes 105a and 105b are made of a conductive material such as aluminum, titanium, chromium, Nickel, copper, yttrium, zirconium, molybdenum, silver, tantalum, or tungsten A single metal made of stainless steel or an alloy containing stainless steel as the main component is used in a single-layer structure or a multi-layer structure. For example, a single layer structure of an aluminum film containing silicon, Two-layer structure with titanium film laminated on tungsten film, two-layer structure with titanium film laminated on tungsten film , a two-layer structure in which a copper film is laminated on a copper-magnesium-aluminum alloy film, a titanium film or A titanium nitride film and an aluminum film or a copper film overlaid on the titanium film or the titanium nitride film. A three-layer structure in which a titanium film or titanium nitride film is formed on top of the molybdenum A molybdenum film or molybdenum nitride film is laminated on the molybdenum film or molybdenum nitride film. A aluminum or copper film is laminated, and then a molybdenum or molybdenum nitride film is laminated on top of it. A three-layer structure is formed. An electrically conductive material may also be used.
[0084] [Insulating layers 106, 107] The insulating layer 106 is an oxide insulating film containing more oxygen than the oxygen required for the stoichiometric composition. It is preferable to use an oxide insulating material containing more oxygen than the oxygen required for the stoichiometric composition. When the film is heated, some oxygen is desorbed. The oxide insulating film containing The amount of oxygen released, calculated as oxygen atoms, was 1 .0×10 18 atoms / cm 3 More than 3.0×10 20 atoms / cm 3 The oxide insulating film is as described above.
[0085] For example, the insulating layer 106 can be made of silicon oxide, silicon oxynitride, or the like. Cut.
[0086] The insulating layer 106 is formed to cover the oxide semiconductor layer 1 when the insulating layer 107 is formed later. It also functions as a damage mitigation membrane for 04.
[0087] In addition, an oxide film that transmits oxygen is provided between the insulating layer 106 and the oxide semiconductor layer 104. Good too.
[0088] As the oxide film that transmits oxygen, silicon oxide, silicon oxynitride, etc. can be used. In this specification, the silicon oxynitride film is a film containing less than nitrogen as a component. A silicon nitride film is a film that contains more oxygen than silicon dioxide. This also refers to a film with a high nitrogen content.
[0089] The insulating layer 107 may be an insulating film having a blocking effect against oxygen, hydrogen, water, etc. By providing the insulating layer 107 over the insulating layer 106, the oxide semiconductor layer 104 can be prevented from being oxidized. In order to prevent the diffusion of elements to the outside and the intrusion of hydrogen, water, and the like into the oxide semiconductor layer 104 from the outside, Examples of insulating films that have a blocking effect against oxygen, hydrogen, water, etc. include silicon nitride, Silicon oxide nitride, aluminum oxide, aluminum oxynitride, gallium oxide, oxynitride Gallium, yttrium oxide, yttrium oxynitride, hafnium oxide, hafnium oxynitride Examples include Um.
[0090] [Example of how to make a transistor] Next, an example of a method for manufacturing the transistor 100 illustrated in FIG. .
[0091] First, as shown in FIG. 6(A), a gate electrode 102 is formed on a substrate 101. An insulating layer 103 is formed on the electrode 102 .
[0092] Here, a glass substrate is used as the substrate 101 .
[0093] [Formation of Gate Electrode] The method of forming the gate electrode 102 will be described below. First, a sputtering method, a CVD method, A conductive film is formed by a deposition method or the like, and a photolithography is performed on the conductive film using a first photomask. A resist mask is formed by a photolithography process. Next, a portion of the conductive film is The portion is etched to form the gate electrode 102. Then, the resist mask is removed. .
[0094] The gate electrode 102 may be formed by electrolytic plating, printing, inkjet printing, or the like instead of the above-mentioned method. It may be formed by a jet method or the like.
[0095] [Formation of Gate Insulating Layer] The insulating layer 103 is formed by a method such as sputtering, CVD, or vapor deposition.
[0096] The insulating layer 103 may be a silicon oxide film, a silicon oxynitride film, or a silicon nitride oxide film. In the case of forming the above-mentioned, a deposition gas containing silicon and an oxidizing gas are used as a source gas. Representative examples of deposition gases containing silicon include silane, disilane, trisilane, and tetrasilane. Examples of oxidizing gases include oxygen, ozone, nitrous oxide, and Nitric oxide, etc.
[0097] In addition, when forming a silicon nitride film as the insulating layer 103, a two-stage formation method is used. First, a mixture gas of silane, nitrogen, and ammonia is used as a raw material gas. A first silicon nitride film with few defects is formed by the plasma CVD method used. Next, The source gas is switched to a mixture of silane and nitrogen, and hydrogen concentration is low and hydrogen is not blown. A second silicon nitride film capable of rocking is formed. The insulating layer 103 is made of silicon nitride, which has few defects and a hydrogen blocking property. A film can be formed.
[0098] In addition, when a gallium oxide film is formed as the insulating layer 103, MOCVD (Metal Organic Chemical Vapor Deposition (OCVD) method It can be achieved.
[0099] [Formation of Oxide Semiconductor Layer] Next, as shown in FIG. 6B, the oxide semiconductor layer 104 is formed over the insulating layer 103.
[0100] A method for forming the oxide semiconductor layer 104 will be described below. First, Then, a second photomask is formed on the oxide semiconductor film. A resist mask is formed by a photolithography process using the resist mask. The oxide semiconductor film is partly etched using a mask to form the oxide semiconductor layer 104. The resist mask is then removed.
[0101] Note that the heat treatment described in Embodiment 1 may be performed immediately after the oxide semiconductor film is formed. Alternatively, the etching may be performed after part of the oxide semiconductor film is etched.
[0102] Here, the oxide semiconductor has a large energy gap of 3.0 eV or more. The oxide semiconductor film obtained by processing the substrate under appropriate conditions and sufficiently reducing the carrier density is In the applied transistor, the leakage current between the source and drain in the off state (on The current (flash current) is extremely low compared to conventional silicon-based transistors. can be done.
[0103] When a large amount of hydrogen is contained in the oxide semiconductor film, the hydrogen is bonded to the oxide semiconductor. Some of the elements become donors and generate electrons, which are carriers. This causes a transistor Therefore, the threshold voltage of the oxide semiconductor film is shifted in the negative direction. After that, dehydration treatment (dehydrogenation treatment) is performed to remove hydrogen or moisture from the oxide semiconductor film. It is preferable to remove the impurities to obtain a high purity so that the impurities are not included as much as possible.
[0104] Note that the oxide semiconductor film is dehydrated (dehydrogenated) to At the same time, oxygen may also decrease. The oxygen that was reduced by the oxidation process is added to the oxide semiconductor, or oxygen is added to the oxide semiconductor. It is preferable to supply oxygen to fill oxygen vacancies in the oxide semiconductor film. Supplying oxygen to a semiconductor film may be referred to as oxygen addition treatment.
[0105] In this manner, the oxide semiconductor film is dehydrated by dehydration treatment (dehydrogenation treatment). By removing oxygen and filling the oxygen vacancies with oxygen addition treatment, the i-type (intrinsic) or The oxide semiconductor film can be an oxide semiconductor film that is nearly i-type and is substantially i-type (intrinsic). Note that the term "substantially intrinsic" means that the number of carriers derived from donors in the oxide semiconductor film is extremely small. (close to zero), carrier density is 1×10 17 / cm 3 Below, 1×10 16 / cm 3 below , 1×10 15 / cm 3 Below, 1×10 14 / cm 3 Below, 1×10 13 / cm 3 Below It says something.
[0106] In addition, a transistor including an i-type or substantially i-type oxide semiconductor film can be For example, a transistor using an oxide semiconductor film can be The drain current per 1 μm of channel width when the transistor is off is 1×10 -18 A or less, preferably 1×10 -21 A or less, more preferably 1×10 -24 A or less, or 1 x 10 at 85°C -15 A or less, preferably 1×10 -18 After A or less, and more preferably 1×10 -21 A or less. In the case of an n-channel transistor, the off state is when the gate voltage is sufficiently higher than the threshold voltage. Specifically, the gate voltage is 1V or more, 2V or more, lower than the threshold voltage. Or, if it is 3V or more smaller, the transistor is turned off.
[0107] [Formation of a pair of electrodes] Next, as shown in FIG. 6(C), a pair of electrodes 105a and 105b are formed.
[0108] The method for forming the pair of electrodes 105a and 105b will be described below. First, a sputtering method A conductive film is formed by a CVD method, a vapor deposition method, or the like. Next, a third photomask is used on the conductive film. Then, a resist mask is formed by a photolithography process. The conductive film is partially etched using a dummy mask to form a pair of electrodes 105a and 105b. Thereafter, the resist mask is removed.
[0109] Note that as shown in FIG. 6C, when the conductive film is etched, the top of the oxide semiconductor layer 104 is Therefore, a part of the oxide semiconductor layer 104 may be etched and thinned. When the oxide semiconductor film is formed, the thickness of the oxide semiconductor film is preferably set to be large in advance.
[0110] [Formation of insulating layer] Next, as shown in FIG. 6D, the oxide semiconductor layer 104 and the pair of electrodes 105a and 10 An insulating layer 106 is formed on 5b, and then an insulating layer 107 is formed on insulating layer 106.
[0111] When a silicon oxide film or a silicon oxynitride film is formed as the insulating layer 106, the raw material gas As the gas, it is preferable to use a deposition gas containing silicon and an oxidizing gas. Representative examples of deposition gases containing silane include silane, disilane, trisilane, and fluorosilane. Oxidizing gases include oxygen, ozone, nitrous oxide, and nitrogen dioxide.
[0112] For example, a substrate placed in a vacuum-evacuated processing chamber of a plasma CVD device is heated to 180° C. or higher. The temperature is kept at 260° C. or less, and more preferably at 200° C. or more and 240° C. or less. By introducing gas, the pressure in the processing chamber is set to 100 Pa or more and 250 Pa or less, and more preferably The pressure is between 100 Pa and 200 Pa, and the pressure applied to the electrodes in the treatment chamber is 0.17 W / cm 2 Below Upper 0.5W / cm 2 Less than or equal to 0.25 W / cm 2 More than 0.35W / cm 2 Silicon oxide film or silicon oxynitride film is formed by supplying the following high frequency power. Complete.
[0113] As a film formation condition, high frequency power with the above power density is supplied in a reaction chamber with the above pressure. This increases the efficiency of decomposition of the source gas in the plasma, increases the number of oxygen radicals, and increases the amount of oxygen in the source gas. As a result, the oxygen content in the oxide insulating film becomes higher than the stoichiometric ratio. However, when the substrate temperature is the above temperature, the bond between silicon and oxygen is weak, so the bonding strength is reduced by heating. As a result, the mixture contains more oxygen than the stoichiometric composition. In addition, an oxide insulating film from which part of oxygen is released by heating can be formed.
[0114] In addition, when an oxide insulating film is provided between the oxide semiconductor layer 104 and the insulating layer 106, In the process of forming the edge layer 106, the oxide insulating film serves as a protective film for the oxide semiconductor layer 104. As a result, damage to the oxide semiconductor layer 104 can be reduced while a high frequency with high power density can be achieved. Electrical power may be used to form the insulating layer 106 .
[0115] For example, a substrate placed in a vacuum-evacuated processing chamber of a plasma CVD device is heated to 180° C. or higher. The temperature is kept at 400° C. or lower, and more preferably at 200° C. or higher and 370° C. or lower. By introducing gas, the pressure in the processing chamber is set to 20 Pa or more and 250 Pa or less, and more preferably 1 The pressure is set to 0.00 Pa or more and 250 Pa or less, and high-frequency power is supplied to the electrode installed in the treatment chamber. Depending on the conditions, a silicon oxide film or a silicon oxynitride film may be formed as the oxide insulating film. In addition, by setting the pressure in the treatment chamber to 100 Pa or more and 250 Pa or less, the oxide When an insulating layer is formed, damage to the oxide semiconductor layer 104 can be reduced. .
[0116] As the source gas for the oxide insulating film, a deposition gas containing silicon and an oxidizing gas are used. Representative examples of deposition gases containing silicon include silane, disilane, trisilane, and tetrasilane. Examples of oxidizing gases include oxygen, ozone, nitrous oxide, and Nitric oxide, etc.
[0117] The insulating layer 107 can be formed by a sputtering method, a CVD method, or the like.
[0118] When a silicon nitride film or a silicon nitride oxide film is formed as the insulating layer 107, the raw material As the gas, a deposition gas containing silicon, an oxidizing gas, and a gas containing nitrogen are used. Representative examples of deposition gases containing silicon include silane, disilane, trisilane, and Examples of oxidizing gases include oxygen, ozone, nitrous oxide, and dioxygen. Nitrogen ions, etc. Nitrogen-containing gases include nitrogen and ammonia.
[0119] After the insulating layers 106 and 107 are formed, heat treatment is preferably performed. The oxygen released from the insulating layer 106 is supplied to the oxide semiconductor layer 104, and the oxide semiconductor layer 1 It is possible to reduce oxygen vacancies in 04.
[0120] Through the above steps, the transistor 100 can be formed.
[0121] [Modifications of Transistor 100] Below, an example of a transistor configuration that is partially different from the transistor 100 will be described. .
[0122] [Variation 1] FIG. 5B is a schematic cross-sectional view of a transistor 110, which will be described below as an example. The transistor 110 differs from the transistor 100 in the structure of the oxide semiconductor layer.
[0123] The oxide semiconductor layer 114 of the transistor 110 is an oxide semiconductor layer 114a and an oxide The insulating layer 114 is formed by laminating a first insulating layer 114b and a second insulating layer 114c.
[0124] Note that the boundary between the oxide semiconductor layer 114a and the oxide semiconductor layer 114b may be unclear. Therefore, in figures such as FIG. 5(B), these boundaries are shown by dashed lines.
[0125] Either one or both of the oxide semiconductor layer 114a and the oxide semiconductor layer 114b The oxide semiconductor film of one embodiment of the present invention can be applied to the above-mentioned.
[0126] For example, the oxide semiconductor layer 114a is typically made of In-Ga oxide or In-Zn oxide. , In-M-Zn oxide (M is Al, Ti, Ga, Y, Zr, La, Ce, Nd, or When the oxide semiconductor layer 114a is an In-M-Zn oxide, I The atomic ratio of n to M is preferably such that In is less than 50 atomic % and M is less than 50 atomic %. ic% or more, more preferably, In is less than 25 atomic % and M is 75 atomic %. % or more. For example, the oxide semiconductor layer 114a has an energy gap of 2 eV or more. A material having a surface area of preferably 2.5 eV or more, and more preferably 3 eV or more, is used.
[0127] For example, the oxide semiconductor layer 114b contains In or Ga, typically In-Ga Oxide, In-Zn oxide, In-M-Zn oxide (M is Al, Ti, Ga, Y, Zr, La, Ce, Nd, or Hf) and has a lower conduction band than the oxide semiconductor layer 114a. The energy of the oxide semiconductor layer 114b is close to the vacuum level, and is typically at the bottom of the conduction band of the oxide semiconductor layer 114b. The difference between the energy of the lower end of the conduction band of the oxide semiconductor layer 114a and the energy of the lower end of the conduction band of the oxide semiconductor layer 114a is 0.05 eV or more, 0.07eV or more, 0.1eV or more, or 0.15eV or more and 2eV or more It is preferable that the electron transport angle is set to 1 eV or less, 0.5 eV or less, or 0.4 eV or less.
[0128] For example, when the oxide semiconductor layer 114b is an In-M-Zn oxide, the In and M The atomic ratio is preferably 25 atomic % or more of In and less than 75 atomic % of M. More preferably, In is 34 atomic % or more and M is less than 66 atomic %. do.
[0129] The oxide semiconductor layer 114a may be formed of, for example, In:Ga:Zn=1:1:1 or 3:1: In-Ga-Zn oxide having an atomic ratio of 1:1 can be used. 14b, for example, In:Ga:Zn=1:3:4, 1:3:6, 1:6:8, or An In-Ga-Zn oxide having an atomic ratio of 1:6:10 can be used. The atomic ratios of the semiconductor layer 114a and the oxide semiconductor layer 114b are each calculated by subtracting the above from the atomic ratio of the oxide semiconductor layer 114a and the oxide semiconductor layer 114b. This includes a variation of ±20% in the atomic ratio.
[0130] The oxide semiconductor layer 114b provided in the upper layer has a higher stability than the oxide semiconductor layer 114a. By using an oxide with a high Ga content that functions as a riser, the oxide semiconductor layer 1 This can suppress release of oxygen from the oxide semiconductor layers 14a and 114b.
[0131] In addition, the semiconductor characteristics and electrical characteristics (field effect) of the required transistors are not limited to these. It is sufficient to use a material with an appropriate composition depending on the characteristics of the device (e.g., the mobility, threshold voltage, and variation). In order to obtain required semiconductor characteristics of a transistor, the oxide semiconductor layer 114a and the oxide The carrier density, impurity concentration, defect density, atomic ratio of metal elements to oxygen in the semiconductor layer 114b, It is preferable to make the interatomic distance, density, etc. appropriate.
[0132] Note that in the above description, the oxide semiconductor layer 114 has a structure in which two oxide semiconductor layers are stacked. However, a structure in which three or more oxide semiconductor layers are stacked may be used.
[0133] [Modification 2] FIG. 5C is a schematic cross-sectional view of a transistor 120, which will be described below as an example. The transistor 120 is different from the transistor 100 in the structure of the oxide semiconductor layer. It is different from 10.
[0134] The oxide semiconductor layer 124 of the transistor 120 includes an oxide semiconductor layer 124a and an oxide The organic semiconductor layer 124b and the oxide semiconductor layer 124c are laminated in this order.
[0135] The oxide semiconductor layer 124a and the oxide semiconductor layer 124b are stacked on the insulating layer 103. The oxide semiconductor layer 124c is formed on the upper surface of the oxide semiconductor layer 124b and on a pair of The electrodes 105a and 105b are provided in contact with the upper and side surfaces of the electrodes 105a and 105b.
[0136] Among the oxide semiconductor layer 124a, the oxide semiconductor layer 124b, and the oxide semiconductor layer 124c, The oxide semiconductor film of one embodiment of the present invention is used for any one, any two, or all of the above. It is possible.
[0137] For example, the oxide semiconductor layer 124b may be the oxide semiconductor layer 11 exemplified in the first modification. For example, the oxide semiconductor layers 124a and 124b may have a similar structure to that of the oxide semiconductor layers 124a and 124b. The oxide semiconductor layer 114c may have a structure similar to that of the oxide semiconductor layer 114b illustrated in the first modification. can.
[0138] For example, the oxide semiconductor layer 124a provided under the oxide semiconductor layer 124b and the oxide semiconductor layer 124b provided over the oxide semiconductor layer 124a are The oxide semiconductor layer 124c provided in the layer has a content of Ga functioning as a stabilizer. By using a large amount of oxide, the oxide semiconductor layer 124a, the oxide semiconductor layer 124b, and In addition, release of oxygen from the oxide semiconductor layer 124c can be suppressed.
[0139] In addition, when a channel is mainly formed in the oxide semiconductor layer 124b, for example, The semiconductor layer 124b is made of an oxide containing a large amount of In. By providing the pair of electrodes 105a and 105b, the on-current of the transistor 120 is increased. It can be made bigger.
[0140] [Other examples of transistor configurations] A top-gate transistor to which the oxide semiconductor film of one embodiment of the present invention can be applied will be described below. An example of the configuration of the star will be described.
[0141] In the following, components having the same configuration or function as those described above will be referred to as follows: The same symbols are used and duplicate content is omitted.
[0142] [Configuration example] FIG. 7A is a schematic cross-sectional view of a top-gate transistor 150 as an example. .
[0143] The transistor 150 includes an oxide semiconductor layer 10 on a substrate 101 on which an insulating layer 151 is provided. 4, a pair of electrodes 105a and 105b in contact with the upper surface of the oxide semiconductor layer 104, A conductor layer 104, an insulating layer 103 provided on a pair of electrodes 105a and 105b, and an insulating layer 1 A gate electrode 102 overlapping with an oxide semiconductor layer 104 is provided on the insulating layer 103. An insulating layer 152 is provided over the gate electrode 102 and the semiconductor layer 103 .
[0144] The oxide semiconductor film described in Embodiment 1 can be used as the oxide semiconductor layer 104.
[0145] The insulating layer 151 has a function of suppressing the diffusion of impurities from the substrate 101 to the oxide semiconductor layer 104. In addition, the oxide semiconductor layer 104 has a function of supplying oxygen by heating. For example, the insulating layer 106 or the insulating layer 107 may have the same structure as the insulating layer 106 or the insulating layer 107. It may be a laminated structure.
[0146] The insulating layer 152 is an insulating layer from which oxygen is released by heating, and the oxide semiconductor layer 104 is For example, the insulating layer 106 may have the same structure as the insulating layer 106. .
[0147] The insulating layer 153 is an insulating layer that has a blocking effect against oxygen, hydrogen, water, etc. For example, it may have the same structure as the insulating layer 107 described above.
[0148] The insulating layer 152 is an insulating layer having a blocking effect against oxygen, hydrogen, water, etc. In that case, the insulating layer 153 does not have to be provided.
[0149] [Modification 3] Below, an example of a transistor configuration that is partially different from the transistor 150 will be described. do.
[0150] FIG. 7B is a schematic cross-sectional view of a transistor 160, which will be described below as an example. The transistor 160 differs from the transistor 150 in the structure of the oxide semiconductor layer.
[0151] The oxide semiconductor layer 164 of the transistor 160 includes an oxide semiconductor layer 164a and an oxide The organic semiconductor layer 164b and the oxide semiconductor layer 164c are laminated in this order.
[0152] Among the oxide semiconductor layer 164a, the oxide semiconductor layer 164b, and the oxide semiconductor layer 164c, Any one, any two, or all of the oxide semiconductor films may be any of the oxide semiconductor films described in Embodiment 1. can be applied.
[0153] For example, the oxide semiconductor layer 164b may be the oxide semiconductor layer 11 exemplified in the first modification. For example, the oxide semiconductor layer 164a may have a structure similar to that of the oxide semiconductor layer 4a. The semiconductor layer 164c has a structure similar to that of the oxide semiconductor layer 114b illustrated in the first modification. can be used.
[0154] For example, the oxide semiconductor layer 164a provided under the oxide semiconductor layer 164b and the oxide semiconductor layer 164b provided over the oxide semiconductor layer 164a are The oxide semiconductor layer 164c provided in the layer has a content of Ga functioning as a stabilizer. By using an oxide having a large amount of oxide, the oxide semiconductor layer 164a, the oxide semiconductor layer 164b, and the oxide This can suppress the release of oxygen from the compound semiconductor layer 164c.
[0155] [Modification 4] In the following, transistors that are partially different from transistor 150 and transistor 160 will be described. A configuration example of the above will be described.
[0156] The transistor 170 illustrated in FIG. 7C includes an oxide semiconductor layer, a gate insulating layer, and the like. The transistor 150 and the transistor 160 are different in different respects.
[0157] In the oxide semiconductor layer 164 included in the transistor 170, the oxide semiconductor layer 164c The oxide semiconductor layer 164b and the electrodes 105a and 105b are provided to cover the oxide semiconductor layer 164b and the ends of the electrodes 105a and 105b. It is being done.
[0158] In addition, the end portions of the oxide semiconductor layer 164c and the insulating layer 103 are in contact with the end portions of the gate electrode 102. The same photomask was used to process the patterns so that they were almost identical to each other.
[0159] The insulating layer 152 is provided in contact with the side surfaces of the insulating layer 103 and the oxide semiconductor layer 164c. It is being done.
[0160] The transistor exemplified in this embodiment has a semiconductor layer in which a channel is formed. The metal oxide film shown in 1 is applied. Therefore, the trapping of carriers due to defects is prevented. The effect of the ion exchange is suppressed, high field effect mobility is achieved, and the fluctuation of electrical characteristics is suppressed, resulting in high reliability. It is a high performance transistor.
[0161] This embodiment may be implemented in appropriate combination with other embodiment modes described in this specification. This can be done.
[0162] (Embodiment 3) In this embodiment, a structure example of a display panel according to one embodiment of the present invention will be described.
[0163] [Configuration example] FIG. 8A is a top view of a display panel according to one embodiment of the present invention, and FIG. A pixel circuit that can be used when a liquid crystal element is applied to a pixel of a display panel of one embodiment is described. FIG. 8C is a circuit diagram for explaining a pixel of a display panel according to one embodiment of the present invention. FIG. 1 is a circuit diagram for explaining a pixel circuit that can be used when an organic EL element is applied. do.
[0164] The transistor disposed in the pixel portion can be formed according to the second embodiment. Since the transistor can be easily made into an n-channel type, the n-channel transistor in the driver circuit can be easily made into an n-channel type. A part of the driver circuit can be configured with a transistor of the same type as the transistor of the pixel part. In this manner, the transistor described in Embodiment 2 is formed in the pixel portion or the driver circuit. By using the same, a highly reliable display device can be provided.
[0165] An example of a block diagram of an active matrix display device is shown in FIG. On a substrate 500, a pixel section 501, a first scanning line driving circuit 502, a second scanning line driving circuit The pixel portion 501 includes a signal line driver circuit 503 and a signal line driver circuit 504. A first scanning line driving circuit 502 extends from the first scanning line driving circuit 504. The scanning line driving circuit 503 is arranged to extend from the scanning line driving circuit 503. In each region, pixels each having a display element are arranged in a matrix. The substrate 500 is a connection board for FPC (Flexible Printed Circuit) etc. It is connected to a timing control circuit (also called a controller or control IC) via .
[0166] In FIG. 8A, a first scanning line driver circuit 502, a second scanning line driver circuit 503, a signal line The driver circuit 504 is formed on the same substrate 500 as the pixel portion 501. Since the number of components such as the drive circuits to be mounted is reduced, the cost can be reduced. 00When an external driver circuit is provided, it becomes necessary to extend the wiring, and the number of connections between the wiring increases. When a driving circuit is provided on the same substrate 500, the number of connections between the wirings can be reduced. Therefore, it is possible to improve reliability or yield.
[0167] [Liquid crystal panel] An example of the circuit configuration of a pixel is shown in FIG. 8(B). 4 shows a pixel circuit that can be applied to the pixel.
[0168] This pixel circuit can be applied to a configuration in which one pixel has multiple pixel electrode layers. The pixel electrode layer is connected to different transistors, and each transistor is driven by a different gate signal. This allows individual pixels of the multi-domain design to be The signals applied to the electrode layers can be controlled independently.
[0169] A gate wiring 512 of a transistor 516 and a gate wiring 513 of a transistor 517 The data lines are separated so that different gate signals can be applied. The source electrode layer or drain electrode layer 514 functioning as a transistor 516 is The transistors 516 and 517 are used in common. The transistors described in the second embodiment can be appropriately used. A display panel can be provided.
[0170] A first pixel electrode layer electrically connected to the transistor 516 and a second pixel electrode layer electrically connected to the transistor 517 The shape of the second pixel electrode layer that is electrically connected to the first pixel electrode layer will be described. The shape of the pixel electrode layer is separated by slits. The first pixel electrode layer spreads in a V shape. The second pixel electrode layer is formed so as to surround the outside of the first pixel electrode layer.
[0171] The gate electrode of the transistor 516 is connected to the gate wiring 512, and the transistor 517 The gate electrode of the gate electrode 512 is connected to the gate wiring 513. 3, different gate signals are applied to transistors 516 and 517. By varying the thickness, the alignment of the liquid crystal can be controlled.
[0172] In addition, the capacitance wiring 510, the gate insulating film functioning as a dielectric, and the first pixel electrode layer Alternatively, a storage capacitor may be formed by a capacitor electrode electrically connected to the second pixel electrode layer.
[0173] The multi-domain structure has a first liquid crystal element 518 and a second liquid crystal element 519 in one pixel. The first liquid crystal element 518 is composed of a first pixel electrode layer, a counter electrode layer, and a liquid crystal layer therebetween. The second liquid crystal element 519 is composed of a second pixel electrode layer, a counter electrode layer, and a liquid crystal layer therebetween. can be.
[0174] Note that the pixel circuit shown in FIG. 8B is not limited to this. Pixels can be equipped with new switches, resistors, capacitors, transistors, sensors, or logic circuits. may be added.
[0175] [Organic EL Panel] Another example of the circuit configuration of a pixel is shown in FIG. 8(C). The pixel structure of the panel is shown.
[0176] In an organic EL element, when a voltage is applied to the light-emitting element, electrons are emitted from one of a pair of electrodes. and holes are injected from the other side into the layer containing the light-emitting organic compound, causing a current to flow. The electrons and holes recombine to form an excited state in the light-emitting organic compound, When the excited state returns to the ground state, light is emitted. The optical element is called a current-excited light-emitting element.
[0177] FIG. 8C is a diagram showing an example of an applicable pixel circuit. An example in which two transistors are used in one pixel is shown. The film can be used for the channel formation region of an n-channel transistor. The pixel circuit can apply digital time gray scale driving.
[0178] Regarding the configuration of an applicable pixel circuit and the operation of a pixel when digital time gray scale driving is applied, I will explain it below.
[0179] The pixel 520 includes a switching transistor 521, a driving transistor 522, and a light emitting The switching transistor 521 has a gate element 524 and a capacitor element 523. The gate electrode layer is connected to the scanning line 526, and the first electrode (one of the source electrode layer and the drain electrode layer) The second electrode (the other of the source electrode layer and the drain electrode layer) is connected to a signal line 525. It is connected to the gate electrode layer of the driving transistor 522. The gate electrode layer is connected to a power supply line 527 via a capacitance element 523, and the first electrode is connected to the power supply line 527, and the second electrode is connected to the first electrode (pixel electrode) of the light-emitting element 524. The second electrode of the light emitting element 524 corresponds to a common electrode 528. It is electrically connected to a common potential line formed thereon.
[0180] The switching transistor 521 and the driving transistor 522 are the same as those in the second embodiment. The transistors described below can be used appropriately. This makes it possible to realize a highly reliable organic EL display. A display panel can be provided.
[0181] The potential of the second electrode (common electrode 528) of the light emitting element 524 is set to a low power supply potential. The low power supply potential is a potential lower than the high power supply potential set in the power supply line 527. For example, D, 0V, etc. can be set as the low power supply potential. The high power supply potential and the low power supply potential are set so that the potential difference is equal to or greater than the threshold voltage of the light emitting element 52. By applying a voltage to the light emitting element 524, a current flows through the light emitting element 524, causing it to emit light. The forward voltage in 24 refers to the voltage required to achieve the desired brightness, and should be at least 100%. Includes threshold voltage.
[0182] The capacitance element 523 is substituted for the gate capacitance of the driving transistor 522. The gate capacitance of the driving transistor 522 can be omitted. A capacitance may be formed between the gate electrode layer and the gate electrode layer.
[0183] Next, a signal input to the driving transistor 522 will be described. In the case of the above method, the driving transistor 522 is in two states, that is, fully on or off. A video signal that satisfies the above requirement is input to the driving transistor 522. In order to operate the actuator 522 in a linear region, a voltage higher than the voltage of the power supply line 527 is applied to the driving A gate electrode layer of the transistor 522 is connected to a signal line 525. A voltage equal to or greater than the threshold voltage Vth of the driving transistor 522 is applied.
[0184] When analog gradation driving is performed, the gate electrode layer of the driving transistor 522 is connected to the light emitting element 5 A voltage equal to or greater than the sum of the forward voltage of 24 and the threshold voltage Vth of the driving transistor 522 is applied. In addition, a video signal is input so that the driving transistor 522 operates in the saturation region. A current flows through the light emitting element 524. In addition, the driving transistor 522 is operated in a saturation region. In order to achieve this, the potential of the power supply line 527 is set higher than the gate potential of the driving transistor 522. By converting the video signal into an analog signal, a current corresponding to the video signal is passed through the light emitting element 524. Moreover, analog gray scale driving can be performed.
[0185] The configuration of the pixel circuit is not limited to the pixel configuration shown in FIG. C) The pixel circuit includes a switch, a resistor, a capacitor, a sensor, a transistor, or a logic circuit. Roads etc. may be added.
[0186] This embodiment may be implemented in appropriate combination with other embodiment modes described in this specification. This can be done.
[0187] (Embodiment 4) In this embodiment, a semiconductor device and an electronic device using a metal oxide film according to one embodiment of the present invention will be described. A configuration example will be described.
[0188] FIG. 9 is a block diagram of an electronic device including a semiconductor device to which a metal oxide film of one embodiment of the present invention is applied. This is a diagram.
[0189] FIG. 10 illustrates the appearance of an electronic device including a semiconductor device to which a metal oxide film of one embodiment of the present invention is applied. FIG.
[0190] The electronic device shown in FIG. 9 includes an RF circuit 901, an analog baseband circuit 902, a digital A baseband circuit 903, a battery 904, a power supply circuit 905, an application processor 906, flash memory 910, display controller 911, memory circuit 91 2. Display 913, touch sensor 919, audio circuit 917, keyboard 918, etc. It is composed of:
[0191] The application processor 906 includes a CPU 907, a DSP 908, and an interface The memory circuit 912 is composed of an SRAM or a DRAM. It is possible.
[0192] By applying the transistor described in Embodiment 2 to the memory circuit 912, It is possible to provide a highly reliable electronic device capable of writing and reading information.
[0193] In addition, the transistor described in the second embodiment may be included in the CPU 907 or the DSP 908. By applying this to registers, etc., the reliability of being able to write and read information is improved. It is possible to provide a highly reliable electronic device.
[0194] In addition, when the off-leak current of the transistor described in the second embodiment is extremely small, Long-term memory retention is possible, and power consumption is sufficiently reduced. In addition, during the power-gated period, The CPU 907 or DSP 90 can store the state before loading in a register or the like. 8 can be provided.
[0195] The display 913 includes a display unit 914, a source driver 915, and a gate driver 9 It is composed of 16.
[0196] The display unit 914 has a plurality of pixels arranged in a matrix. The pixel circuit is electrically connected to a gate driver 916 .
[0197] The transistor described in Embodiment 2 is appropriately provided in the pixel circuit or the gate driver 916. This makes it possible to provide a highly reliable display.
[0198] The electronic device may be, for example, a television device (television or television receiver) (also called "computer monitors"), digital cameras, digital video cameras, etc. digital photo frames, mobile phones (also called mobile phones or mobile phone devices), These include large game machines such as small game machines, portable information terminals, audio playback devices, and pachinko machines. can be.
[0199] FIG. 10A shows a portable information terminal, which includes a main body 1001, a housing 1002, a display unit 1003, and a The display unit 1003b is a touch panel. By touching the keyboard button 1004 displayed on the display unit 1003b, Of course, the display unit 1003a can be configured as a touch panel. The transistor described in Embodiment 2 may be used as a switching element in a liquid crystal panel. By fabricating an organic light-emitting panel and applying it to the display units 1003a and 1003b, It is possible to provide a highly useful portable information terminal.
[0200] The portable information terminal shown in FIG. 10(A) displays various information (still images, videos, text images, etc.). Functions that display calendars, dates, or times on the display, functions that display Ability to manipulate or edit displayed information, processed by various software (programs) In addition, the rear and side of the housing may be provided with terminals for external connection. It may also be configured to include a connector (such as an earphone jack or USB port) and a recording medium insertion section.
[0201] The portable information terminal shown in FIG. 10A is configured to be capable of wirelessly transmitting and receiving information. The desired book data can be purchased and downloaded wirelessly from an electronic book server. It is also possible to configure the device to perform this function.
[0202] FIG. 10B shows a portable music player. The main body 1021 has a display unit 1023 and an earphone. The device has a fixing part 1022 for mounting to an external device, a speaker, an operation button 1024, and an external memory slot. The transistor shown in the second embodiment is used as a switching element. By manufacturing a liquid crystal panel or an organic light-emitting panel as a display unit 1023, This makes the portable music player more reliable.
[0203] Furthermore, the portable music player shown in FIG. 10(B) is equipped with an antenna, a microphone function, and a wireless function. If you carry it with you and connect it to your mobile phone, you can enjoy wireless hands-free driving while driving a car. Conversation in Lee is also possible.
[0204] FIG. 10C shows a mobile phone, which is composed of two housings, a housing 1030 and a housing 1031. The housing 1031 includes a display panel 1032, a speaker 1033, a microphone, and the like. a phone 1034, a pointing device 1036, a camera lens 1037, an external connection terminal The housing 1030 also includes a solar cell for charging the mobile phone. The device is equipped with a cell 1040, an external memory slot 1041, and the like. The transistor described in the second embodiment is built in the display panel 103. By applying this to 2, a highly reliable mobile phone can be achieved.
[0205] The display panel 1032 is equipped with a touch panel, and an image is displayed on the display panel 1032 as shown in FIG. The operation keys 1035 are shown by dotted lines. It also includes a boost circuit to boost the input voltage to the voltage required by each circuit.
[0206] For example, the power transistor used in a power supply circuit such as a boost circuit is also described in the second embodiment. The thickness of the metal oxide film of the transistor to be described is set to 2 μm or more and 50 μm or less. It is possible.
[0207] The display direction of the display panel 1032 changes appropriately depending on the usage mode. The camera lens 1037 is located on the same surface as the lens 1032, so video calls are possible. The speaker 1033 and the microphone 1034 are not limited to voice calls, but are also used for video calls. , recording, playback, etc. are possible. Furthermore, the housing 1030 and the housing 1031 can be slid apart, As shown in Figure 10(C), the device can be folded from the unfolded state to the overlapped state, making it easy to carry. Suitable miniaturization is possible.
[0208] The external connection terminal 1038 can be connected to various cables such as AC adapters and USB cables. It is possible to charge the battery and to communicate data with a personal computer, etc. By inserting a recording medium into the external memory slot 1041, it is possible to store and transfer a larger amount of data. Cut.
[0209] In addition to the above functions, it also has infrared communication function, TV reception function, etc. Good too.
[0210] FIG. 10D shows an example of a television device. The television device 1050 is A display unit 1053 is built into the housing 1051. The display unit 1053 displays an image. In addition, the CPU is built into the stand 1055 that supports the housing 1051. The transistor described in the second embodiment is applied to the display unit 1053 and the CPU. By using this, a highly reliable television device 1050 can be obtained.
[0211] The television device 1050 can be operated using an operation switch provided on the housing 1051 or a separate remote control. This can be done by a remote control device. A display unit for displaying information output from the input unit may be provided.
[0212] The television device 1050 includes a receiver, a modem, and the like. This allows reception of general television broadcasts, and can also be used for wired or wireless reception via a modem. By connecting to a network, communication can be one-way (sender to receiver) or two-way It is also possible to communicate information in both directions (between sender and receiver, or between receivers). .
[0213] The television device 1050 also includes an external connection terminal 1054 and a storage medium playback / recording unit 1055. 052, and an external memory slot. The external connection terminal 1054 is a It can be connected to any type of cable, enabling data communication with a personal computer, etc. In the storage medium playback and recording unit 1052, a disk-shaped recording medium is inserted and It is possible to read the stored data and write it to the recording medium. Images and videos stored in the external memory 1056 inserted in the reslot It is also possible to display it on the display unit 1053.
[0214] In addition, when the off-leak current of the transistor described in embodiment 2 is extremely small, By applying this transistor to the external memory 1056 and the CPU, power consumption is sufficiently reduced. This results in a highly reliable television apparatus 1050 with reduced noise. [Explanation of symbols]
[0215] 100 Transistors 101 Substrate 102 Gate electrode 103 Insulating layer 104 Oxide semiconductor layer 105a electrode 105b electrode 106 Insulating Layer 107 Insulating layer 110 Transistor 114 Oxide semiconductor layer 114a Oxide semiconductor layer 114b Oxide semiconductor layer 120 Transistor 124 Oxide semiconductor layer 124a Oxide semiconductor layer 124b Oxide semiconductor layer 124c Oxide semiconductor layer 150 Transistors 151 Insulating layer 152 Insulating layer 153 Insulating Layer 160 Transistors 164 Oxide semiconductor layer 164a Oxide semiconductor layer 164b Oxide semiconductor layer 164c Oxide semiconductor layer 170 Transistors 500 boards 501 Pixel section 502 Scanning line driver circuit 503 Scanning line driver circuit 504 Signal line driver circuit 510 Capacitance wiring 512 Gate wiring 513 Gate wiring 514 Drain electrode layer 516 Transistor 517 Transistor 518 Liquid crystal element 519 Liquid crystal element 520 pixels 521 Switching Transistors 522 Driving Transistor 523 Capacitive element 524 Light emitting element 525 Signal Line 526 scan lines 527 Power line 528 Common electrode 901 RF circuit 902 Analog Baseband Circuit 903 Digital Baseband Circuit 904 Battery 905 Power supply circuit 906 Application Processor 907 CPU 908 DSP 910 Flash Memory 911 Display Controller 912 Memory Circuit 913 Display 914 Display section 915 Source Driver 916 Gate Driver 917 Voice Circuit 918 Keyboard 919 Touch Sensor 1001 Main unit 1002 Case 1003a Display section 1003b Display section 1004 Keyboard Buttons 1021 Main unit 1022 Fixed part 1023 Display section 1024 operation buttons 1025 external memory slot 1030 Case 1031 Case 1032 Display Panel 1033 Speaker 1034 Microphone 1035 Operation Key 1036 Pointing Device 1037 Camera Lenses 1038 External connection terminal 1040 Solar Cell 1041 External memory slot 1050 Television Equipment 1051 Case 1052 Storage media playback and recording unit 1053 Display section 1054 External connection terminal 1055 Stand 1056 External Memory
Claims
[Claim 1] Contains In, Ga, and Zn; In the cross-sectional observation image, a first layer in which In atoms are periodically arranged and a second layer in which Ga atoms or Zn atoms are periodically arranged are observed, a first region having n layers of the second layer (n is a natural number) between a pair of the first layers; a second region having m (m is a natural number other than n) layers of the second layer between another pair of the first layers; Metal oxide film.
Citation Information
Patent Citations
Oxide semiconductor film and semiconductor device
JP2011100979A
Method of manufacturing oxide semiconductor
JP2012099661A
Metal Oxide Film
JP7550948B2
Amorphous oxide and field effect transistor
JP2006165529A