Method for identifying optical wavelength using semiconductor optical sensor

The phototransistor with a double diffusion layer in a Si semiconductor substrate addresses the complexity and cost issues of conventional sensors by using potential peaks to separate photovoltaic currents, enabling precise wavelength identification and intensity analysis without optical filters.

JP2024162009APending Publication Date: 2024-11-21TOYOHASHI UNIVERSITY OF TECHNOLOGY
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023077131
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-09
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

Conventional optical sensors for fluorescence observation are complex, costly, and unable to accurately determine light intensity at each wavelength, especially when fluorescence has multiple wavelengths, leading to incomplete analysis of biological and cell samples.

Method used

A phototransistor with a double diffusion layer in a Si semiconductor substrate, utilizing a potential peak to separate photovoltaic currents into two paths, allowing for wavelength identification through current ratios without the need for optical filters or diffraction gratings.

Benefits of technology

Enables accurate and compact wavelength identification with a single photodetector, simplifying the configuration and reducing manufacturing costs while providing detailed light intensity analysis for each wavelength.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024162009000001_ABST
    Figure 2024162009000001_ABST
Patent Text Reader

Abstract

To solve a problem in which, in a semiconductor optical sensor used in a fluorescence microscope, which is used to observe living cells, the photocurrent generated depends on the wavelength and intensity of the incident light, so it is not possible to determine the wavelength from the photocurrent alone.SOLUTION: A potential peak is formed in a photoelectric conversion region of a semiconductor optical sensor, and a photoelectric current is split into two paths by this barrier and detected. Taking advantage of the fact that the ratio of the detected photoelectric currents does not depend on the intensity of the incident light, the position of the potential peak is identified in advance using a reference incident light, and the wavelength is identified from the photoelectric current ratio of the unknown incident light.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for identifying a wavelength of light using a phototransistor or a photodiode. [Background technology]

[0002] Fluorescence observation is often used as a method for observing the activity of living cells. This method involves irradiating living cells with a laser beam or the like having a specific wavelength as excitation light, measuring the wavelength and intensity of the fluorescence emitted by the fluorescent substance labeled in the living cells, and analyzing the activity of the living cells. Semiconductor phototransistors or the like are used to detect the fluorescence.

[0003] Here, the light intensity of the fluorescence is weaker than the excitation light, and the intensity of the excitation light reflected by the living cells themselves is generally strong. In the fluorescence observation method, since the wavelengths of the excitation light and the fluorescence are different, an optical system combining an optical filter that blocks the wavelength corresponding to the excitation light and an optical filter that passes only the wavelength band of the fluorescence is required, and the observation equipment becomes large. Furthermore, if the fluorescent substance is changed or if fluorescence of multiple wavelengths occurs in response to the excitation light, the optical filter needs to be replaced and multiple observations are required. Here, if the wavelength of the fluorescence can be identified, the intensity can be identified for each wavelength, so the activity state of the living cells can be observed by irradiating the excitation light once.

[0004] Intensity detection using a phototransistor is based on the penetration depth of light, which changes depending on the wavelength. In a phototransistor using a Si semiconductor substrate with a forbidden band width of 1.11 eV, the light intensity φ0 at the Si surface and the light intensity φ at a depth w are W The relationship between the amount of light at depth w and the amount of light g is expressed by equation (2). W is expressed by equation (3). φ W =φ0exp(-αw) (2) g W =φ0{1-exp(-αw)} (3) Here, α is the light absorption coefficient and depends on the wavelength λ. The light absorption coefficient is evaluated for each material. Therefore, if the light absorption coefficient α can be obtained, the wavelength λ can be determined. The specific light absorption coefficient of Si semiconductors is disclosed in Non-Patent Document 2. Non-Patent Document 2 discloses absorption coefficients in 10 nm increments in the light wavelength range of 250 to 1450 nm, and the absorption coefficient of a fractional wavelength can be supplemented from the absorption coefficients of the wavelengths before and after it.

[0005] By multiplying the amount of light by the elementary charge q and the light-receiving area S, the current value generated by the incident light absorbed from the surface to a depth w can be obtained. I=-(φ0qSλ / hc)·{1-exp(-λw)} (4) where h is Planck's constant and c is the speed of light.

[0006] In fluorescence observation, when a semiconductor laser or LED is used as a light source of excitation light, the wavelength spectrum of the excitation light is not steep and has a certain half-width. Furthermore, the fluorescence or phosphorescence emitted from a living body or cell sample may have multiple peak wavelengths in the wavelength spectrum. For this reason, in fluorescence observation, the general analytical method is to correlate the centroid wavelength with the total light intensity. Centroid wavelength λ C is the wavelength obtained by integrating the product of the light intensity φ(λ) at wavelength λ and wavelength l, and dividing the integral by the total amount of light, and is expressed by equation (5). λ C =[∫λφ(λ)dλ] / [∫φ(λ)dλ] (5) [Prior art documents] [Patent documents]

[0007] [Patent Document 1] Japanese Patent Application Publication No. 7-326790 [Patent Document 2] Patent Publication No. 2022-012325 [Non-patent literature]

[0008] [Non-Patent Document 1] Yong-Joon Choi and et.al, "Demonstrating a filter-free wavelength sensor with double-well structure and its application," biosensors 2022, 12(11), 1033. [Non-Patent Document 2] MA Green, "Self-consistent optical parameters of intrinsic silicon at 300 K including temperature coefficients," Solar Energy Materials and Solar Cells, vol. 92, pp. 1305-1310, 2008. Summary of the Invention [Problem to be solved by the invention]

[0009] Patent Document 1 discloses a photodiode structure in which multiple n-type regions are formed at different depths in a p-type silicon substrate, and each n-type region is connected to an electrode provided on the surface of the silicon substrate. It is shown that the photodiode can measure the intensity of incident light by reading out the photoelectromotive current value of each n-type region.

[0010] Patent Document 2 discloses an optical sensor structure having a p-type silicon substrate with a light incident surface, a region that generates carriers by absorbing incident light, a pair of driving electric field application electrodes that move carriers from the region in a direction oblique to the light incident direction, and a number of detection electrodes provided at different positions in a direction perpendicular to the light incident direction.

[0011] However, the optical sensor shown in Patent Document 1 has an epitaxial layer structure for providing the same functionality as a plurality of photodiodes connected in parallel, which results in a complex element structure and high manufacturing costs.In addition, the depth at which each n-type region is formed is fixed, so it is not always possible to form the n-type region at a depth suitable for the wavelength of the incident light, making it difficult to achieve precise separation.

[0012] In the optical sensor shown in Patent Document 2, the longer the wavelength of incident light, the deeper it penetrates, so the shorter the distance that is affected by the driving electric field, and the larger the photovoltaic current detected by the detection electrode positioned perpendicular to the incident light. On the other hand, the shorter the wavelength of light, the shallower the region in which carriers are generated, so the longer the distance that is affected by the driving electric field, and the smaller the photovoltaic current detected by the detection electrode positioned perpendicular to the incident light. It has been shown that this phenomenon can be used to measure the intensity of incident light from the photovoltaic current at each detection electrode.

[0013] In the structure of the above-mentioned optical sensor, light is incident on the surface of the p-type silicon substrate, but it is necessary to provide a driving electric field application electrode in a direction perpendicular to the light, i.e., on the side of the p-type silicon substrate, and a detection electrode must also be provided on the back surface of the p-type silicon substrate, making the manufacturing process complicated.

[0014] In order to solve the problems in Patent Documents 1 and 2, Non-Patent Document 1 has been proposed. Non-Patent Document 1 discloses a structure having a double diffusion layer in which an n-type diffusion region is formed in a p-type silicon substrate and a p-type diffusion region is formed in a predetermined region of the n-type diffusion region. It shows that the intensity of incident light can be determined from the current ratio by generating a potential saddle in the n-type diffusion region, distributing the charge according to the penetration depth, and extracting the photovoltaic current from different electrodes. In Non-Patent Document 1, the wavelength of the incident light is normalized by the centroid wavelength.

[0015] When the fluorescence emitted from a biological or cellular sample has multiple wavelengths, the light intensity at each wavelength is not specified even in the detection method of Non-Patent Document 1. In this way, when using the centroid wavelength, there is a problem that the wavelength spectrum information of the excitation light having multiple wavelengths and the fluorescence from the biological or cellular sample is lost, making it unsuitable for detailed observation of life science phenomena.

[0016] Non-Patent Document 1 shows that in a photogate transistor having a double diffusion layer, if the wavelength of incident light is constant, the ratio of the photocurrent detected from the photogate electrode to the photocurrent detected from the semiconductor substrate side is constant regardless of the light intensity. However, it is not possible to identify the wavelength of unknown incident light.

[0017] In the conventional technology, it is not possible to obtain the light intensity for each wavelength of incident light having multiple wavelengths. The method shown in the conventional technology is applied on the premise that the wavelength components contained in the incident light are known. [Means for solving the problem]

[0018] In consideration of the above circumstances, the inventors of the present application have discovered a method of using a phototransistor having a double diffusion layer in a Si semiconductor substrate to generate a potential peak in the diffusion region of the phototransistor, detecting a photocurrent generated by incident light by separating it into two paths by the potential peak, and identifying the wavelength of any incident light from the ratio of the photocurrents. Here, the potential peak refers to an extreme value of the potential in the potential distribution formed in the diffusion region.

[0019] A first aspect of the present invention is a light-emitting diode having a photoelectric conversion region that generates electric charges in response to incident light and that includes a transparent electrode provided via an insulating film in a predetermined region on a semiconductor substrate, A semiconductor photosensor is used, which provides a potential distribution that divides charge discharge from the photoelectric conversion region into two paths, a first and a second charge discharge path, the first and the second charge discharge paths being connected to first and second photovoltaic current detection electrodes, and has a means for detecting first and second photovoltaic currents detected from the first and second photovoltaic current detection electrodes, applying a predetermined photogate potential to the transparent electrode under incident light having a specified wavelength to obtain a current ratio between the first and second photocurrents, and determining a depletion layer depth for the photogate potential from the current ratio; The present invention is characterized in that an absorption coefficient of the light to be identified is calculated from the current ratio and the depletion layer depth determined by incident light having a wavelength of the light to be identified, and the wavelength of the light to be identified is determined from the absorption coefficient.

[0020] A second aspect of the present invention is a light-charge conversion region that generates charges in response to incident light and that includes a transparent electrode provided via an insulating film in a predetermined region on a semiconductor substrate, a potential distribution is provided that divides a charge discharge path from the photoelectric conversion region into two paths, the first and second charge discharge paths are connected to first and second photovoltaic current detection electrodes, and a current ratio of the first and second photovoltaic currents detected from the first and second photovoltaic current detection electrodes is defined by the following formula: I1 / I2={exp(-αW)-exp(-αW pn )} / {1-exp(-αW)} (1), (I1 is the first photocurrent, I2 is the second photocurrent, a is the absorption coefficient, W is the position of the potential peak, W pn is the deepest position of the potential peak) a semiconductor photosensor having a means for determining said current ratio, applying a predetermined photogate potential to the transparent electrode under incident light having a predetermined wavelength to obtain a current ratio between the first and second photocurrents, and calculating a depletion layer depth for the photogate potential from the current ratio using equation (1); The present invention is characterized in that an absorption coefficient of the light to be identified is calculated from the current ratio and the depletion layer depth determined by incident light having a wavelength to be identified, and the wavelength of the light to be identified is determined from the absorption coefficient.

[0021] A third aspect of the present invention is characterized in that, in the second aspect, the semiconductor substrate has a first conductivity type, the photocharge generation region has the first conductivity type, the first charge discharge path has a second conductivity type, and the second charge discharge path is a part of the photocharge generation region and has the first conductivity type.

[0022] A fourth aspect of the present invention is characterized in that, in the second aspect, the semiconductor substrate has a second conductivity type, the photocharge generation region has a first conductivity type, the first charge discharge path is part of the semiconductor substrate and has the second conductivity type, and the second charge discharge path is part of the photocharge generation region and has the first conductivity type.

[0023] When a potential peak exists in the photoelectric conversion region, the first and second photoelectric currents detected from the first and second photoelectric current detection electrodes are expressed by the formulas (2) and (3). The ratio of the formulas (5) and (6) is expressed by the formula (1). Here, W is the depth at which the potential peak exists. Also, W pn is the depth of the pn junction formed between the first and second diffusion layers, and is determined by the position where the pn junction is formed. The position W of the potential peak is W pn It doesn't get any deeper than that. I1=-(φ0qSλ / hc)·{exp(-αW)-exp(-αW pn )} (7) I2=-(φ0qSλ / hc)·{1-exp(-αW)} (6) I1 / I2={exp(-αW)-exp(-αW pn )} / {1-exp(-αW)} (1)

[0024] The sum of I1 and I2 is expressed by equation (8) and does not fluctuate even if the photogate potential, that is, the position W of the potential peak, changes. I1+I2=-(φ0qSλ / hc)·{1-exp(-αW pn )} (8)

[0025] Equation (1) indicates that the current ratio is constant regardless of the light intensity. On the other hand, since the light absorption coefficient α depends on the wavelength λ, if the position W of the potential peak is unknown, the wavelength cannot be specified. Here, if the wavelength λ0 of the incident light is known, the corresponding absorption coefficient α0 can be specified, and the current ratio I1 / I2 and photogate potential V in equation (1) can be determined. PG The position W of the potential peak can be calculated from the photogate potential V PG By recording the position W of the potential peak corresponding to the photogate potential V PG Since the position W of the potential peak does not change, the absorption coefficient of the unknown incident light can be obtained, and the wavelength of the unknown incident light can be identified. Effect of the Invention

[0026] According to the present invention, a wavelength can be identified using a single photodetector without using a diffraction grating or optical filter as in conventional spectroscopic devices, and a method for identifying a wavelength that is highly accurate, compact, and has a simple configuration can be provided. [Brief description of the drawings]

[0027] [Figure 1] 1 is a schematic cross-sectional view of a semiconductor device used in a first embodiment. [Diagram 2] FIG. 11 is a schematic cross-sectional view of a semiconductor device used in a second embodiment. [Diagram 3] FIG. 11 is a schematic cross-sectional view of a semiconductor device used in a third embodiment. [Figure 4] 2A to 2C are explanatory views showing first to third steps in the manufacture of the semiconductor device according to the first embodiment. [Diagram 5] 5A to 5C are explanatory views showing a fourth step and a fifth step in the manufacture of the semiconductor device according to the first embodiment. [Figure 6]5A to 5C are explanatory views showing a sixth step and a seventh step in the manufacture of the semiconductor device according to the first embodiment. [Figure 7] 8A to 8C are explanatory diagrams showing eighth and ninth steps in the manufacture of the semiconductor device according to the first embodiment; [Figure 8] FIG. 2 is a plan view of the semiconductor device used in the first embodiment. [Figure 9] 13 is a simulation result illustrating a potential distribution in a semiconductor device used in the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0028] Hereinafter, embodiments will be described with reference to the drawings. <First embodiment> A schematic cross-sectional view of a semiconductor device 101 according to this embodiment is shown in Fig. 1. The semiconductor device 101 of this embodiment is a photogate type transistor having a transparent electrode 7 as a gate electrode, and has a function of controlling the outflow path of charges generated in the semiconductor by the incidence of light by the photogate potential.

[0029] The semiconductor device 101 shown in Fig. 1 has a structure with a double diffusion layer, and includes a first diffusion layer 2 that serves as a first charge transport path in a predetermined region of a semiconductor substrate 1, a second diffusion layer 3 that serves as a photoelectric conversion region in a predetermined region of the first diffusion layer 2, and a transparent electrode 7 that applies a photogate potential via an insulating film 6 on the region of the second diffusion layer 3. The first and second diffusion layers 2 and 3 are of opposite conductivity types. If the conductivity type of the semiconductor substrate 1 is p-type, the first diffusion layer 2 is n-type and the second diffusion layer 3 is p-type.

[0030] The semiconductor substrate 1 is divided into a first potential fixed electrode 11 connected to the semiconductor substrate 1, a first photoinduced current detection electrode 13 connected to the first diffusion layer 2, a second potential fixed electrode 12 connected to the second diffusion layer 3, a photogate electrode 14 connected to the transparent electrode 7, and a second photoinduced current detection electrode 15. The first and second potential fixed electrodes 11 and 12 and the first photoinduced current detection electrode 13 have contact regions 5a, 5b, and 5c made of a high concentration and the same conductivity type as the connected region, and are in ohmic contact. The connection between the second photoinduced current detection electrode 15 and the second diffusion layer 3 has a contact region 5d made of a conductivity type of the opposite polarity, and is a diode contact to prevent charge inflow from the outside.

[0031] The second diffusion layer 3 functions as a photoelectric charge conversion region. In the photoelectric charge conversion region, electron-hole pairs are generated by incident light. A predetermined potential is applied to the first and second photocurrent detection electrodes 13, 15 to detect the generated electrons, and the generated holes reach the first and second potential fixed electrodes 11, 12 which are fixed to the ground potential. In this case, the holes are not detected as a photoelectric current.

[0032] In the first embodiment, the semiconductor substrate 1 has a concentration of 2×10 14 cm -3 The first diffusion layer 2, which is an n-type diffusion layer, has a concentration of 1×10 12 cm -3 The diffusion depth is 6.5 μm, and the p-type diffusion layer, which is the second diffusion layer 3, has a concentration of 2×10 12 cm -3 The diffusion depth is 2.5 μm. The impurity distribution is analyzed separately by secondary ion mass spectrometry, and the diffusion depth is the position where the carrier concentration is the same as that of the adjacent opposite conduction type region. The concentration of the p-type and n-type contact regions is 4×10 18 cm -3The thickness is about 100 nm. The gate insulating film 6 is made of SiO2 and has a thickness of 60 nm. The transparent electrode 7 is made of poly-Si and has a thickness of 300 nm, so that the incident light is sufficiently transmitted and reaches the photoelectric conversion region 3. The transparent electrode 7 may be made of ITO (indium tin oxide). The electrode material is Al and has a thickness of 0.7 μm.

[0033] <Second embodiment> 2 has a structure with a single diffusion layer 3a, and the diffusion layer 3a serving as a photoelectric conversion region is provided in a predetermined region of the semiconductor substrate 1, and a transparent electrode 7 is provided on a predetermined region of the diffusion layer 3a via an insulating film 6. The semiconductor substrate 1 and the diffusion layer 3a are of opposite conductivity types. If the conductivity type of the semiconductor substrate 1 is n-type, the diffusion layer 3a is p-type.

[0034] A first photoinduced current detection electrode 13 connected to the semiconductor substrate 1, a potential fixed electrode 11a connected to the diffusion layer, a photogate electrode 14 connected to the transparent electrode 7, and a second photoinduced current detection electrode 15 connected to the diffusion layer 3a are defined on the semiconductor substrate 1. The first photoinduced current detection electrode 11a and the potential fixed electrode 13 have contact regions 5a, 5c made of a high concentration and the same conductivity type as the diffusion layer 3a to which they are connected, and are in ohmic contact. The second photoinduced current detection electrode 15 is connected to the diffusion layer 3a through a contact region 5d made of a conductivity type of the opposite polarity, and is in diode contact to prevent inflow of charge from the outside.

[0035] In the second embodiment, the semiconductor substrate 1 has a concentration of 5.0×10 13 cm -3 The p-type diffusion layer 3a has a concentration of 2.5×10 13 cm -3 The diffusion depth is 3 μm. The impurity concentration of the contact regions 5a, 5c, and 5d is 10 18 cm -3 The gate insulating film 6 was made of SiO2 and had a thickness of 60 nm. The transparent electrode 7 was made of poly-Si and had a thickness of 300 nm. The electrode material and the transparent electrode material were the same as those in the first embodiment.

[0036] <Third embodiment> 3 has a structure including an epitaxial growth layer 3b, which is a photoelectric charge conversion region, in a predetermined region of a semiconductor substrate 1, a transparent electrode 7 is provided on a predetermined region of the epitaxial growth layer 3b via an insulating film 6, and a first photovoltaic current detection electrode 13 is provided on the back surface of the semiconductor substrate 1. If the conductivity type of the semiconductor substrate 1 is n-type, the epitaxial growth layer 3b is p-type.

[0037] In the third embodiment, a potential fixed electrode 11a connected to the epitaxial growth layer 3b, a photogate electrode 14 connected to the transparent electrode 7, and a second photovoltaic current detection electrode 15 connected to the epitaxial growth layer 3a are defined on the semiconductor substrate 1, and a first photovoltaic current detection electrode 13 is defined on the back surface of the semiconductor substrate 1.

[0038] Generally, the thickness of a Si semiconductor substrate is about several hundreds of μm to 1 mm. In the third embodiment, the depth of the epitaxial growth layer 3b functioning as a photoelectric conversion region can be set deep, so that the region for collecting photovoltaic current can be made deep. In other words, the detection range can be expanded to a wavelength band (about 1050 nm) with a small absorption coefficient for the Si semiconductor substrate 1.

[0039] In the third embodiment, the photoelectric conversion region is formed as an epitaxial growth layer 3b, but may be formed as a diffusion layer. In the third embodiment, it is convenient to detect a substrate current as the first photovoltaic current from the back surface of the semiconductor substrate 1. <Method of Manufacturing a Semiconductor Device According to the First Embodiment>

[0040] A manufacturing method of the semiconductor device 101 of the first embodiment will be described with reference to Figures 4 to 7. The first and second steps are steps of forming a double diffusion layer, the third to fifth steps are a step of forming a channel stopper, a step of isolating elements, a step of forming a gate insulating film, and a step of forming a photogate, and the sixth to ninth steps are a step of forming a contact region, a step of forming a contact hole, a step of forming an electrode, a step of forming an interlayer insulating film, and a step of forming a light-shielding layer.

[0041] The first step is a step of forming a first diffusion layer 2. As a specific example, the conductivity type of the Si semiconductor substrate 1 is p-type, and the carrier concentration is 2.24×10 -14 cm -3 The sheet resistance is 60 ohm·cm, and the crystal plane orientation is (100).

[0042] First, an oxide film 10a is formed to protect the Si semiconductor substrate 1. As a specific example, a SiO2 film with a thickness of 50 nm is formed by thermal oxidation at 1050°C. Next, an n-type diffusion layer 2 is formed by ion implantation. The region in which the n-type diffusion layer 2 is to be formed is defined by photolithography using a resist. Specifically, a rectangular region of 500 μm x 500 μm is defined, and P (phosphorus) ionized from PH3 gas as an n-type impurity is implanted at an acceleration voltage of 150 keV and a dose of 1×10 12 cm -2 After ion implantation, the resist is removed. Drive-in diffusion is performed to recover the crystal defects caused by ion implantation and to expand the impurity diffusion depth. As a specific example, heat treatment was performed at 1150°C for 1530 min (25 hours 30 min) in a N2 gas atmosphere.

[0043] The second step is a step of forming the second diffusion layer 3. The region in which the p-type diffusion layer 3 is to be formed is partitioned by photolithography. As a specific example, a region of 400 μm×400 μm is partitioned, and B (boron) ionized from BF3 gas as a p-type impurity is ionized at an acceleration voltage of 80 keV and a dose of 2×10 12 cm -2After the ion implantation, drive-in diffusion is performed in a N2 gas atmosphere. As a specific example, heat treatment was performed at 1150°C for 270 minutes (4 hours and 30 minutes). Figure 4 shows the shape after the double diffusion layer was formed.

[0044] The third process is a channel stopper formation process. After the double diffusion layer is formed, it is desirable to provide a channel stopper in a part of the diffusion region that will become the contact region. An n-type channel stopper 4b is formed on the p-type semiconductor substrate 1, and a p-type channel stopper 4a is formed on the n-type semiconductor substrate 1. As a specific example, the n-type channel stopper 4b is formed by doping P as an n-type impurity with an acceleration voltage of 60 keV and a dose of 6.0×10 13 cm -2 The p-type channel stopper 4a is implanted with B as a p-type impurity at an acceleration voltage of 60 keV and a dose of 6.0×10 13 cm -2 The activation process is carried out during the subsequent oxide film formation process.

[0045] The fourth process is an element isolation process. As a specific example, wet oxidation is performed at 1050° C. for 55 min (4 hours) to grow a SiO2 film that will become the field oxide film 10b. The film thickness of the field oxide film 10b is set to 400 nm. The field oxide film 10b is removed from the region where each electrode and the photogate electrode 14 are to be formed by selective etching using a photolithography method.

[0046] The fifth step is a transparent electrode formation step. First, a gate insulating film 6 is formed on the entire surface. As a specific example, wet oxidation is performed at 950°C for 15 minutes. The thickness of the gate insulating film 6 is 70 nm. Poly-Si is used as the transparent electrode material. A poly-Si film is deposited on the entire surface by a CVD (Chemical Vapor Deposition) method or the like, and unnecessary poly-Si regions are removed by selective etching using a photolithography method. As a specific example, the poly-Si film thickness is 70 nm, and reactive ion etching using XeF2 gas is used for selective etching. The section of the transparent electrode 7 is 300 μm x 300 μm.

[0047] The sixth step is a contact region formation step. The contact surface between the p-type diffusion layer 3 and the second photovoltaic current detection electrode 15 is doped with n-type impurities to form a diode contact. The contact surface between the n-type diffusion layer 2 and the first photovoltaic current detection electrode 13 is doped with n-type impurities, the contact surface between the p-type diffusion layer 3 and the second potential fixed electrode 12 is doped with p-type impurities, and the contact surface between the p-type semiconductor substrate 1 and the first potential fixed electrode 11 is doped with p-type impurities, and these contact surfaces are in ohmic contact. It is desirable to perform ion implantation of the contact surfaces with a high concentration and shallow doping. As a specific example, P is doped as an n-type impurity at a dose of 4×10 15 cm -2 The implantation was performed at an acceleration voltage of 60 keV, and B was implanted as a p-type impurity at a dose of 4 × 10 15 cm -2 The ions were implanted at an acceleration voltage of 60 keV. After the ion implantation, a tetraethyl orthosilicate (TEOS) film, which serves as an insulating film, is formed by CVD or the like. Activation annealing is performed at 1000°C for 20 minutes.

[0048] The seventh process is a contact hole forming process, in which the TEOS film 10 at the contact hole opening and the SiO2 layer formed when the gate insulating film 6 is formed are removed by photolithography.

[0049] The eighth step is the electrode formation step. Al is used as the electrode material and formed over the entire surface by sputtering, and the area other than the electrodes is removed by RIE. Alternatively, the film can be formed by vacuum deposition, and etching can also be done by wet etching. After that, a PE-TEOS (Plasma Enhanced CVD TEOS) film that will become the interlayer insulating layer 16 is deposited.

[0050] The ninth step is the light-shielding layer formation step. Here, Tokyo Ohka Kogyo's black resist BK-8310 is used, and only the photogate area is opened by lithography. The light-shielding layer 17 has a thickness of 1.5 μm. Alternatively, Al can be used as the light-shielding material.

[0051] 8 is a plan view of the semiconductor device 101 according to the embodiment 1. A photogate electrode 14, a second potential fixed electrode 12, a first photoinduced current detection electrode 13, and a first potential fixed electrode 11 are formed around the rectangular photogate region at the center, joining and separating at a predetermined interval toward the outer periphery, with a portion left unfinished. A second photoinduced current detection electrode 15 is connected to the region where these electrodes do not wrap around. The region where the transparent electrode 7 is formed is partitioned into 300 μm × 300 μm.

[0052] <Electric potential distribution in the diffusion layer> The potential distribution in the diffusion layer 3a will be described by taking the second embodiment as an example. Fig. 9 shows the results of calculations of the diffusion layer depth and the potential distribution in the diffusion layer 3a using the photogate potential as a parameter based on the formation conditions of the diffusion layer 3a described in paragraphs 0033 to 0035. The calculations were performed using the device simulator SPECTRA manufactured by Link Research.

[0053] If the conduction type of the Si semiconductor substrate 1 is n-type, the conduction type of the diffusion layer 3a which is the photoelectric conversion region is p-type. DD The diffusion layer 3a is connected to a ground potential, and 0V is applied to the photogate electrode 14. The surface side of the diffusion layer 3a is connected to 0V, and the inside of the Si semiconductor substrate 1 is connected to V DD The voltage near the pn junction interface ranges from 0V to V DD Here, the potential of the outermost surface is shifted slightly to the positive side due to the influence of the Si surface. When a positive potential is applied to the photogate electrode 14, the surface side of the diffusion layer 3a becomes a positive potential, the potential in the diffusion layer 3a temporarily decreases to near 0 V, and the potential on the Si semiconductor substrate 1 side changes to V DD That is, the potential distribution peak is formed in the diffusion layer 3a.

[0054] In the example of Figure 9, at a photogate potential of -1 V, the minimum value is -0.34 V at the outermost surface, at a photogate potential of 3 V, the minimum value is 0.53 V at a depth of 1.46 μm, and at a photogate potential of 5 V, the minimum value is 1.86 V at a depth of 1.56 μm, indicating that the depth of the potential peak becomes deeper as the photogate potential is increased.

[0055] Electrons generated by the incidence of light on the surface side of the peak of the potential distribution flow out to the second photoinduced current detection electrode 15, and electrons generated on the Si semiconductor substrate 1 side of the peak of the potential distribution flow out to the first photoinduced current detection electrode 11a. If the photogate potential is further increased, the potential on the surface side of the diffusion layer 3a increases, and since there is no significant change in the electric field strength, the peak of the potential distribution generated in the diffusion layer 3a moves from the surface side to a deeper position. The amount of charge flowing out to the first and second photoinduced current detection electrodes 11a, 15 can be varied by the photogate potential.

[0056] In the first embodiment, a p-type semiconductor substrate 1, an n-type diffusion layer 2, and a p-type diffusion layer 3 are formed, and the p-type diffusion layer 3 serves as a photoelectric charge conversion region. The p-type semiconductor substrate 1 is fixed to the ground potential, but the potential distribution in the p-type diffusion layer 3 is the same as in the second embodiment. Also in the third embodiment, the potential distribution in the photoelectric charge conversion region can be explained in the same way as in the second embodiment.

[0057] <Specifying the light wavelength> The procedure for identifying the wavelength of unknown incident light will be described. The optical absorption coefficient of Si semiconductor is the value described in Non-Patent Document 2. The tunable wavelength laser light source LDTLS (registered trademark) manufactured by Tokyo Instruments Inc. was used as the light source for the experiment.

[0058] In the first step, light with a specified reference wavelength is irradiated. Here, light with a wavelength of 600 nm is irradiated, and the first and second photocurrents are measured. The position of the potential peak is determined using equation (1), but equation (2) can also be used. The intensity of the incident light on the surface is converted into the sum of the photocurrents (I1+I2), and the intensity of the incident light at depth w is converted into the first photocurrent (I1), so equation (9) holds. φ W =φ0·exp(-α 600 w) (2) φ W / φ0=I1 / (I1+I2) (9) where φ0 is the intensity at the surface of the diffusion layer, and φ w is the intensity at depth w. α 600 is the optical absorption coefficient of Si at a wavelength of 600 nm, and 4175 cm -1 At a photogate potential of 3 V, the first photoelectric current I1 is 514.519 nA, the second photoelectric current I2 is 354.092 nA, the current ratio according to formula (1) is 1.453, and the current ratio according to formula (9) is 0.5923. In addition, the absorption coefficient α 600 Using equation (2), the depth w of the diffusion layer is calculated to be 1.254 μm.

[0059] In the second step, when incident light of unknown wavelength is irradiated, the first photocurrent I1 is measured to be 1490.93 nA, and the second photocurrent I2 is measured to be 414.74 nA. The current ratio according to equation (9) is 0.7824. The absorption coefficient is calculated from equation (2) to be 1957 cm -1 The wavelength can be determined to be approximately 697.1 nm. Since the wavelength of the tunable laser light source was set to 700 nm in advance, it was confirmed that the wavelength of the incident light could be determined with an error of 5 nm or less.

[0060] In the third step, the intensity of the incident light is calculated using equation (4). In equation (4), the second photovoltaic current I2 is 414.74 nA, and the elementary charge q is 1.602 × 10 -19 C, the light receiving area S is 0.3 mm × 0.3 mm, the wavelength of the incident light is 697.1 nm, and the absorption coefficient is 1957 cm -1 , the depth of the diffusion layer w is 1.254×10 -4 cm, Planck constant h is 6.62×10 -34 m 2 kg / s, the speed of light c is 3×10 8 m / s, the intensity of the incident light at the surface, f0, is 3.77mW / cm 2 It becomes.

[0061] In this way, the wavelength and intensity of unknown incident light can be identified. The present invention is not limited to the above-mentioned embodiments and examples. Various modifications that do not deviate from the spirit of the claims and that can be easily conceived by a person skilled in the art are also included in the present invention. [Explanation of symbols]

[0062] 1. Semiconductor substrate, silicon substrate 2 First diffusion layer 3 Second diffusion layer, photoelectric conversion region 3a Diffusion layer, photoelectric conversion region 3b Epitaxial growth layer, photoelectric conversion region 4. Channel stopper layer 4a: Channel stopper layer formed on the first diffusion layer 4b: A channel stopper layer formed on the semiconductor substrate and the second diffusion layer 5 Contact Area 5a Contact region formed on semiconductor substrate 5b Contact region formed on first diffusion layer 5c: a contact region formed on the second diffusion layer or the photoelectric conversion region 5d. A reverse-conducting contact region formed on the second diffusion layer or the photoelectric conversion region. 6 Gate insulating film 7 Transparent electrode 10. Insulating film 10a Oxide film 10b Field oxide 11 First potential clamp electrode 11a Potential fixing electrode 12 Second potential clamp electrode 13 First photovoltaic current detection electrode 14 Photogate electrode 15 Second photovoltaic current detection electrode 16 Interlayer insulating film 17 Light blocking layer 101, 102, 103 Semiconductor device

Claims

1. a photoelectric conversion region that generates electric charges in response to incident light and that is provided with a transparent electrode via an insulating film in a predetermined region on a semiconductor substrate; A semiconductor photosensor is used, which provides a potential distribution that divides charge discharge from the photoelectric conversion region into two paths, a first and a second charge discharge path, the first and the second charge discharge paths being connected to first and second photovoltaic current detection electrodes, and has a means for detecting first and second photovoltaic currents detected from the first and second photovoltaic current detection electrodes, applying a predetermined photogate potential to the transparent electrode under incident light having a specified wavelength to obtain a current ratio between the first and second photocurrents, and determining a depletion layer depth for the photogate potential from the current ratio; A method for identifying a wavelength of light, comprising the steps of: determining an absorption coefficient of light to be identified from a current ratio and the depletion layer depth determined by incident light having a wavelength of the light to be identified; and identifying the wavelength of the light to be identified from the absorption coefficient.

2. a photoelectric conversion region that generates electric charges in response to incident light and that is provided with a transparent electrode via an insulating film in a predetermined region on a semiconductor substrate; a potential distribution is provided that divides a charge discharge path from the photoelectric conversion region into two paths, the first and second charge discharge paths are connected to first and second photovoltaic current detection electrodes, and a current ratio of the first and second photovoltaic currents detected from the first and second photovoltaic current detection electrodes is defined by the following formula: I 1 / I 2 ={exp(-αW)-exp(-αW pn )} / {1-exp(-αW)} (1)、 (I 1 is the first photovoltaic current, I 2 is the second photocurrent, α is the absorption coefficient, W is the position of the potential peak, W pn is the deepest position of the potential peak) a semiconductor photosensor having a means for determining said current ratio, applying a predetermined photogate potential to the transparent electrode under incident light having a specified wavelength to obtain a current ratio between the first and second photocurrents, and determining a depletion layer depth for the photogate potential from the current ratio; A method for identifying a light wavelength, comprising: determining an absorption coefficient of light to be identified from a current ratio and the depletion layer depth determined by incident light having a wavelength of the light to be identified; and identifying the wavelength of the light from the absorption coefficient.

3. 3. The method for identifying a wavelength of light according to claim 2, wherein the semiconductor substrate has a first conductivity type, the photocharge generation region has a first conductivity type, the first charge discharge path has a second conductivity type, and the second charge discharge path is a part of the photocharge generation region and has the first conductivity type.

4. 3. The method for identifying a wavelength of light according to claim 2, wherein the semiconductor substrate has a second conductivity type, the photocharge generation region has a first conductivity type, the first charge discharge path is a part of the semiconductor substrate and has the second conductivity type, and the second charge discharge path is a part of the photocharge generation region and has the first conductivity type.

5. 5. The method of claim 4, wherein the photocharge generating region is an epitaxially grown layer.

6. Either the absorption coefficient α or the position w of the potential peak is determined by the first photovoltaic current I 1 and the second photovoltaic current I 2 Using this, from equation (10), I 1 / (I 1 +I 2 )= exp(-αw) (10)、 6. The method for identifying a light wavelength according to claim 2, further comprising the step of determining the other of the two wavelengths.

Citation Information

Patent Citations

  • Semiconductor optical sensor

    JP1995326790A

  • Optical sensor and spectrometer using the same

    JP2022012325A