Casting device

The casting apparatus aligns cast pins with intersecting axes and uses a convex-recessed design to manage stress, preventing pin deformation and burrs, thus reducing manufacturing costs and ensuring efficient lubrication passage formation in engine cylinder blocks.

JP2024163674APending Publication Date: 2024-11-22MAZDA MOTOR CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023079493
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-12
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The formation of main galleries in cylinder blocks of engines, especially in multi-cylinder engines, leads to high manufacturing costs due to separate machining after casting, and the use of cast pins on the molten metal inlet side risks deformation from direct hits and thermal expansion, causing burrs in the casting passageway.

Method used

A casting apparatus that aligns first and second cast pins with intersecting axial directions, featuring a convex portion and a recessed non-contact portion to reduce the contact area and increase surface pressure without increasing the butt load, using a circular groove to concentrate stress on the contact surface.

Benefits of technology

This configuration prevents the opening of the abutting portions of the cast pins during molten metal pouring, eliminating the need for additional machining and ensuring the formation of lubrication oil passages without deformation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024163674000001_ABST
    Figure 2024163674000001_ABST
Patent Text Reader

Abstract

To provide a casting device to form a core passage with a pair of core pins butted against, in which butt portions are inhibited from opening without increasing the load of butting.SOLUTION: A casting device includes a melt inlet port arranged such that a direction of flow of melt into a cavity from the melt inlet port intersects with an axial direction of a first core pin 11 and a second core pin 12. Tips of the first and second core pins 11, 12 are butted against each other upon clamping a mold to thereby make up a core for forming a communication hole to become a lubrication-oil passage in a cylinder block. At least one of the tips of the first and second core pins 11, 12 has a contact face 11c to contact the other of the tips upon clamping the mold and a circular groove 11b, as a non-contact portion, disposed in a position adjacent to the contact face 11c and recessed in a manner to avoid a contact with the other of the tips.SELECTED DRAWING: Figure 7
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a casting apparatus. [Background technology]

[0002] A structure in which a main gallery for oil passage is formed in an engine cylinder block is known. The main gallery is a long passage extending along the cylinder arrangement direction that supplies lubricating oil to the crankshaft inside the engine and the oil jets facing the back surface of the pistons. In the case of a cylinder block that is long in the cylinder arrangement direction, such as an in-line multi-cylinder engine (e.g., six or more cylinders), the main gallery is generally formed by machining, such as with a drill, after the cylinder block is cast. However, in this case, manufacturing costs are high because machining is performed separately from casting.

[0003] Therefore, it is considered to form a main gallery using a core pin during casting to suppress the increase in costs. During casting, the main gallery is formed by a pair of core pins that are butted against each other in the cylinder arrangement direction. In this case, however, when molten metal is injected from a direction perpendicular to the cylinder arrangement direction, the core pin may be directly hit by the molten metal and deformed. Therefore, the core pin is arranged at a position away from the molten metal inlet side through which the molten metal is injected into the cavity inside the mold, specifically, at a position opposite the molten metal inlet across each cylinder liner, to prevent the molten metal from directly hitting the core pin.

[0004] In recent years, a technology has been proposed that changes the number of main galleries used depending on the operating conditions in order to improve engine fuel efficiency and emissions. In the case of a cylinder block with two or more main galleries, it is necessary to add a main gallery on the molten metal inlet side. Therefore, the shot pin that forms the main gallery on the molten metal inlet side cannot avoid being hit directly by the molten metal, and there is a risk that the shot pin will be deformed.

[0005] As a prior art for preventing such deformation of core pins, Patent Document 1 discloses a casting device in which the tips of a pair of core pins are butted together, with a convex part formed on the tip surface of one of the core pins and a concave part having a shape corresponding to the convex part formed on the tip surface of the other core pin. In this structure, the fitting of the convex part and the concave part at the butted tips prevents deformation of the core pins due to direct impact with molten metal. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] JP 2019-089075 A Summary of the Invention [Problem to be solved by the invention]

[0007] However, even with the above structure, the molten metal during casting hits the butt joint of the pair of core pins on the molten metal inlet side directly, and the butt joint is subjected to bending load due to the collision of the molten metal from the perpendicular direction. This causes rapid thermal expansion (specifically, thermally biased expansion on the side closer to the molten metal inlet and the side farther from it). Therefore, even if the convex and concave parts of the pair of core pins are fitted together, the butt joint may open up. If the butt joint opens up when the molten metal is poured, it can cause burrs to appear in the core passage of the cylinder block after casting.

[0008] In order to prevent the butt joints from opening when the molten metal is poured, it is possible to increase the butt joint load between the pair of core pins. However, if the butt joint load is too large, the core pins may be plastically deformed and break, so it is difficult to increase the butt joint load too much.

[0009] The present invention has been made in consideration of the above-mentioned circumstances, and has an object to suppress the opening of the butt portion without increasing the butt load in a casting device in which a pair of cast-out pins are butted together to form a cast-out passage. [Means for solving the problem]

[0010] In order to solve the above problems, the casting apparatus of the present invention is a casting apparatus for casting a casting having a communicating hole, and is provided with a first side die having a first core pin, a second side die arranged opposite to the first side die and having a second core pin extending along the same axis as the first core pin, and a third die which, together with the first and second side dies, forms a cavity when clamped, and is provided with a molten metal inlet for injecting molten metal into the cavity, and the molten metal inlet is provided with a molten metal inlet that is inclined relative to the first side die and is inclined relative to the first side die. The present invention is characterized in that the axial direction of the first core pin and the second core pin intersect, and the first core pin and the second core pin form a core for forming the communicating hole of the casting by butting their tips together when the mold is closed, and at least one of the tips of the first core pin and the second core pin has a contact surface that contacts the other tip when the mold is closed, and a non-contact portion that is positioned adjacent to the contact surface and is recessed in the opposite direction to the butt direction to become non-contact with the other tip.

[0011] According to this configuration, at least one of the tips of the first core pin and the second core pin that are butted against each other has a contact surface that contacts the tip of the other when the molds are closed, and a non-contact portion that is recessed in the opposite direction to the butting direction to be out of contact with the tip of the other. Therefore, the contact area of ​​the tip of one with the tip of the other is reduced, so that it is possible to increase the surface pressure when the first core pin and the second core pin are butted together without increasing the butt load. As a result, it is possible to prevent the butt portions of the first core pin and the second core pin from opening due to the bending load caused by the impact of the molten metal during casting and the thermal expansion caused by the heat of the molten metal.

[0012] In the above-mentioned casting apparatus, it is preferable that the tip of the first core pin has a convex portion protruding in the axial direction of the first core pin, the tip of the second core pin has a concave portion that can fit into the convex portion when the mold is closed, and the contact surface and the non-contact portion are positioned at the tip of the first core pin so that the non-contact portion is located between the contact surface and the convex portion.

[0013] According to this configuration, by fitting the convex portion at the tip of the first core pin into the concave portion at the tip of the second core pin, the first core pin and the second core pin can be centered when the tips of the first core pin and the second core pin are butted against each other during mold closing. In this configuration, the contact surface and non-contact portion are located at the tip of the first core pin, which has a convex portion, so that the non-contact portion can be located close to the convex portion, making it possible to concentrate stress on the contact surface during mold closing.

[0014] In addition, the tip of the second core pin has a recess that fits with the protrusion, but does not have a non-contact portion, so that the tip of the second core pin can have a width of the recess that can stably guide the protrusion.

[0015] In the above casting apparatus, the non-contact portion is preferably a circular groove surrounding the protrusion.

[0016] According to this configuration, since the non-contact portion is a circular groove, it is easy to process the non-contact portion at the tip of the first core pin, and it is possible to form the non-contact portion over a wide area. Accordingly, it is possible to reliably reduce the area of ​​the contact surface at the tip of the first core pin, so that it is possible to increase the compressive strain due to the increase in compressive stress at the contact surface when the mold is closed. As a result, it is possible to reliably suppress the opening of the butt portion.

[0017] In the above casting apparatus, the circular groove is preferably formed on the periphery of the protrusion.

[0018] According to this configuration, since the circular groove is formed on the periphery of the protrusion, the contact surface is arranged continuously in a circular shape on the outer periphery side of the circular groove at the tip of the first core pin. Therefore, since the contact surface is not divided by the circular groove (i.e., the contact surface is not dispersed), it is possible to reliably increase the compressive strain of the contact surface and reliably suppress the opening of the butted portion.

[0019] In the above casting apparatus, it is preferable that the casting is a cylinder block of an engine, and the communication hole is a lubricating oil passage.

[0020] With this configuration, it is possible to form the lubricating oil passage by using the first core pin and the second core pin on the molten metal inlet side where the molten metal hits directly when molding the cylinder block, which eliminates the need for additional machining to form the lubricating oil passage. Effect of the Invention

[0021] As described above, according to the casting apparatus of the present invention, in a casting apparatus in which a pair of core pins are butted together to form a core passage, it is possible to suppress the opening of the butted portions without increasing the butt load. [Brief description of the drawings]

[0022] [Figure 1] 1 is a perspective view showing an overall configuration of a casting device according to an embodiment of the present invention; [Diagram 2] 2 is an enlarged perspective view showing the arrangement of first to fourth core pins in the cavity of FIG. 1. FIG. [Diagram 3] 2 is an enlarged plan view showing the arrangement of first to fourth core pins in the cavity of FIG. 1. FIG. [Figure 4] 4 is an explanatory view showing a state in which molten metal collides with a butt portion where the tip portions of the first core pin and the second core pin in FIG. 3 are butted against each other. FIG. [Diagram 5] 5 is an enlarged perspective view showing the tip portions of the first core pin and the second core pin in FIG. 4. FIG. [Figure 6]FIG. 5 is a vertical sectional view of a tip portion of the first core pin of FIG. 4. [Figure 7] 4 is a vertical cross-sectional view of a butted portion where the tip ends of the first core pin and the second core pin in FIG. 3 are butted against each other. FIG. [Figure 8] 2 is a perspective explanatory view showing a lubricating oil passage inside an engine having a cylinder block cast by the casting apparatus of FIG. 1, the lubricating structure having two main galleries. FIG. [Figure 9] FIG. 6 is an enlarged perspective view showing the tip portions of a first core pin having no circular groove, which is a comparative example of the present invention, and the second core pin of FIG. 5. [Figure 10] 10(a) is a cross-sectional diagram showing a schematic diagram of the butt load F1, the bending load F2 due to the molten metal collision, the temperature T1 of the molten metal collision side, the temperature T2 of the back side of the molten metal collision side, the resultant strain ε1 of the molten metal collision side, and the resultant strain ε2 of the back side of the molten metal collision side when molten metal collides with the butt portion of the first core pin and the second core pin that do not have a circular groove in FIG. 9, and FIG. 10(b) is a cross-sectional diagram showing the state in which the butt portion of the first core pin and the second core pin that do not have a circular groove is open. [Figure 11] 10(a) is a cross-sectional view showing a schematic diagram of a butt compression strain εF1 generated by a butt load F1 at the butt joint between a first core pin and a second core pin not having a circular groove in FIG. 10(a), (b) is a cross-sectional view showing a schematic diagram of a molten metal collision bending strain εF2 generated by a bending load F2 due to molten metal collision at the butt joint in FIG. 10(a), and (c) is a cross-sectional view showing a schematic diagram of a thermal expansion bending strain εT1 due to a temperature T1 on the molten metal collision side at the butt joint in FIG. 10(a) and a thermal expansion bending strain εT2 due to a temperature T2 on the back side of the molten metal collision side. [Figure 12] 6 is a flowchart showing an example of a procedure for determining an interference m, which is the area of ​​the contact surface of FIG. 5. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0023] Hereinafter, a casting apparatus according to an embodiment of the present invention will be described in detail with reference to the drawings.

[0024] Hereinafter, a preferred embodiment of the present invention will be described in detail with reference to the accompanying drawings.

[0025] The casting apparatus 1 shown in Fig. 1 is an apparatus for casting a cylinder block B of an engine 50 (see Fig. 8) as an example of a casting having a communicating hole. The shape of the cylinder block B cast by the casting apparatus 1 is not particularly limited in the present invention, but for example, a cylinder block B for an in-line multi-cylinder engine (four cylinders in this embodiment) is produced by the casting apparatus 1.

[0026] (Explanation of molds 2 to 7) As shown in Figures 1 to 3, the casting apparatus 1 is equipped with six dies, namely, a first side die 2, a second side die 3, a lower die 4 (corresponding to the third die of the present invention), a front die 5, a rear die 6, and an upper die 7, in order to form a cavity 9 which is a space corresponding to the shape of the cylinder block B. These six dies 2 to 7 are combined when clamped to form a sealed cavity 9. In Figure 1, the front die 5 and the upper die 7 are simply shown by using two-dot chain lines to make the cavity 9 visible.

[0027] The first side die 2 and the second side die 3 are arranged facing each other with a space between them in the cylinder arrangement direction X of the cylinder block B. The lower die 4 and the upper die 7 are arranged facing each other with a space between them in the vertical direction Z. The front die 5 and the rear die 6 are arranged facing each other with a space between them in the width direction Y perpendicular to the cylinder arrangement direction X. The front die 5 is arranged above a molten metal inlet 10 described later.

[0028] The lower die 4 is formed with a molten metal inlet 10 for forcing molten metal into the cavity 9. The molten metal inlet 10 is a through hole that penetrates the lower die 4 in the vertical direction Z. The molten metal inlet 10 communicates with the cavity 9 through an inlet gate 16. The inlet gate 16 is formed by the opposing surfaces of the lower die 4 and the front die 5, and is a passage that extends obliquely upward.

[0029] Molten metal formed by melting a metal such as an aluminum alloy is injected under high temperature and pressure from the molten metal inlet 10 through the inflow gate 16 into the cavity 9, thereby casting (specifically, die casting) a cylinder block B corresponding to the shape of the cavity 9. The remaining molten metal and air that flowed into the cavity 9 are discharged to the outside of the cavity 9 through a vent (not shown). The vents are formed at locations away from the inflow gate 16, for example, between the lower die 4 and the rear die 6, between the front die 5 and the upper die 7, and between the rear die 6 and the upper die 7.

[0030] (Explanation of core pins 11 to 14) The casting apparatus 1 further includes four core pins, namely, a first core pin 11, a second core pin 12, a third core pin 13, and a fourth core pin 14, for forming a first main gallery 25 and a second main gallery 26 (see FIG. 8) as two lubricating oil passages in the cylinder block B.

[0031] The first main gallery 25 is a lubricating oil passage on the side closer to the inflow gate 16, and is a passage that supplies lubricating oil to an oil jet (injection part) that injects lubricating oil onto the back surface of a piston inside the engine mainly during high-speed operation or high temperature. The second main gallery 26 (see FIG. 8) is a lubricating oil passage on the side farther from the inflow gate 16, and is a passage that constantly supplies lubricating oil to the crank journal and the oil jet inside the engine while the engine is running. The first main gallery 25 and the second main gallery 26 are supplied with lubricating oil stored in the crankcase CC shown in FIG. 8 through a first supply passage 42 after being filtered by an oil filter 41. At the same time, the lubricating oil is also supplied to an oil gallery 44 for a valve opening and closing mechanism in the cylinder head CH through a second supply passage 43.

[0032] The first core pin 11 shown in Figures 1 to 4 is one part of a core for forming a first main gallery 25 (see Figure 8) close to the inlet gate 16, and is provided on the surface facing the cavity 9 of the first side mold 2 so as to protrude inside the cavity 9 in the cylinder arrangement direction X.

[0033] 1 to 4 is the other part of the core for forming the above-mentioned first main gallery 25, and is provided on the surface of the second side die 3 facing the cavity 9 so as to protrude inward of the cavity 9 in the cylinder arrangement direction X. The second core pin 12 extends along the same axis as the first core pin 11 (in this embodiment, along the axis extending in the cylinder arrangement direction X).

[0034] The first core pin 11 and the second core pin 12 constitute a core for forming the first main gallery 25, which serves as a passage for the flow of lubricating oil in the cylinder block B, by having their tips butt together when the mold is closed (i.e., forming the butt portion 17 in Figures 2 to 4 and 7).

[0035] The third core pin 13 shown in Figures 1 to 3 is one part of a core for forming a second main gallery 26 (see Figure 8) that is far from the inlet gate 16, and is provided on the surface facing the cavity 9 in the first side mold 2 so as to protrude inside the cavity 9 in the cylinder arrangement direction X.

[0036] 1 to 3 is the other part of the core for forming the second main gallery 26, and is provided on the surface of the second side die 3 facing the cavity 9 so as to protrude inward of the cavity 9 in the cylinder arrangement direction X. The fourth core pin 14 extends along the same axis as the third core pin 13 (in this embodiment, along the axis extending in the cylinder arrangement direction X).

[0037] The third core pin 13 and the fourth core pin 14 constitute a core for forming the second main gallery 26, which serves as a passage for the flow of lubricating oil in the cylinder block B, by having their tips butt together when the mold is closed (forming the butt portion 18 in Figures 2 and 3).

[0038] The third core pin 13 and the fourth core pin 14 are located on the opposite side to the first core pin 11 and the second core pin 12 across the cylinder forming region 9a of the cavity 9 shown in FIG.

[0039] Here, when looking at the position of the above-mentioned molten metal inlet 10 with reference to the first core pin 11 and the second core pin 12, as shown in Figures 1-2 and 4, the molten metal inlet 10 is positioned so that the flow direction of the molten metal M from the molten metal inlet 10 to the cavity 9 intersects (orthogonal in Figures 1-2) with the axial direction of the first core pin 11 and the second core pin 12 (the same direction as the cylinder arrangement direction X).

[0040] As shown in Figures 5 to 7, the tip of the first core pin 11 has, on its tip surface facing the tip of the second core pin 12, a convex portion 11a protruding in the axial direction of the first core pin 11, a circular groove 11b which is a non-contact portion that does not contact the second core pin 12, and an annular contact surface 11c which contacts the second core pin 12.

[0041] The protrusion 11a is disposed at the axial center of the tip end of the first cast core pin 11 and is a cone-shaped projection that protrudes in the axial direction.

[0042] The circular groove 11b is a non-contact portion that is recessed in the opposite direction to the butting direction and is not in contact with the tip of the second core pin 12. The circular groove 11b is formed concentrically with the protruding portion 11a. Specifically, the circular groove 11b is formed so as to surround the protruding portion 11a along the periphery 11a1 of the protruding portion 11a.

[0043] Arc-shaped chamfered portions 11b1 are formed at the radially outer and inner corners of the inner peripheral surface of the circular groove 11b. These chamfered portions 11b1 make it possible to disperse stress acting on the corners of the inner peripheral surface of the groove 11b when the tips of the first core pin 11 and the second core pin 12 are butted against each other.

[0044] The contact surface 11c is formed concentrically with the above-mentioned protrusion 11a and the circular groove 11b. Specifically, the contact surface 11c is formed continuously in an annular shape along the outer periphery of the circular groove 11b. Therefore, the circular groove 11b is adjacent to the inside of the annular contact surface 11c. The contact surface 11c faces the butting direction of the first core pin 11 and the second core pin 12 (the axial direction of the first core pin 11).

[0045] As shown in Figure 7, when the tip ends of the first core pin 11 and the second core pin 12 are butted together during mold clamping (when butt portion 17 is formed), the contact surface 11c comes into surface contact with the outer peripheral edge of the tip end of the second core pin 12 at butt portion 17, specifically, the outer peripheral edge of the opposing surface 12b.

[0046] In this embodiment, it is sufficient that at least one of the tip portions of the first core pin 11 and the second core pin 12 has, on the tip surface facing the other tip portion, a contact surface that comes into contact with the other tip portion when the mold is closed, and a non-contact portion (circular groove 11b in the above embodiment) that is positioned adjacent to the contact surface and is recessed in the opposite direction to the butt direction to thereby become non-contact with the other tip portion.

[0047] The non-contact portion may be any recessed portion adjacent to the contact surface, and may be at least one dot-like or circular depression (dimple) or semicircular groove other than the circular groove 11b as described above.

[0048] In this embodiment, the circular groove 11b is disposed so as to be located between the contact surface 11c and the protrusion 11a, so that it is possible to concentrate stress on the contact surface 11c when the mold is clamped.

[0049] The tip of the second core pin 12 has, at its tip surface facing the tip of the first core pin 11, a recess 12a that can fit into the protrusion 11a of the first core pin 11 when the mold is closed, and an opposing surface 12b that faces the contact surface 11c and circular groove 11b (non-contact portion) of the first core pin 11.

[0050] The recess 12a is a cone-shaped recess that is disposed at the axial center of the tip of the second core pin 12, recessed in the axial direction, and has a shape corresponding to the above-mentioned protrusion 11a. The recess 12a plays the role of a guide for aligning the centers of the first core pin 11 and the second core pin 12 while fitting with the protrusion 11a when the first core pin 11 and the second core pin 12 are butted together during mold clamping. Therefore, when the butting is completed, the protrusion 11a and the recess 12a are fitted together in a loose fit state (a state allowing clearance), and no pressing force is generated between the inner peripheral surfaces of the protrusion 11a and the recess 12a.

[0051] The opposing surface 12b is an annular surface that is the portion other than the recess 12a on the tip surface of the second core pin 12. The opposing surface 12b has an area opposing the entire surfaces of the annular contact surface 11c and the circular groove 11b (non-contact portion).

[0052] (Features of this embodiment) (1) In the casting apparatus 1 of this embodiment, the tip of the first core pin 11, which is one of the tips of the first core pin 11 and the second core pin 12 that are butted against each other, has a contact surface 11c that contacts the tip of the other when the molds are closed, and a circular groove 11b as a non-contact portion that is recessed in the opposite direction to the butting direction to be non-contact with the tip of the second core pin 12. Therefore, the contact area of ​​the tip of the first core pin 11 with the tip of the second core pin 12 is small. (Specifically, when considering the contact area of ​​the first core pin 11 and the second core pin 12 of this embodiment excluding the areas occupied by the convex portion 11a and the concave portion 12a for centering, the circular groove 11b is not involved in the contact between the core pins 11 and 12, and is only the area of ​​the annular contact surface 11c.)

[0053] 7, it is possible to increase the surface pressure σF1 at the contact surface 11c when the first core pin 11 and the second core pin 12 are butted together without increasing the butt load F1 at which the tips of the first core pin 11 and the second core pin 12 are butted together. In other words, it is possible to increase the butt compressive strain εF1 at the contact surface 11c due to the butt load F1. As a result, it is possible to prevent the butt portion 17 of the first core pin 11 and the second core pin 12 from opening due to the bending load caused by the impact of the molten metal during casting and the thermal expansion caused by the heat of the molten metal.

[0054] <Detailed explanation of the phenomenon of the butt joint 17 opening> The phenomenon in which the butt joint portion 17 of the first core pin 11 and the second core pin 12 opens will be described in detail below.

[0055] Here, a comparative sample shown in Fig. 9 is used as a sample that exhibits the phenomenon in which the butt portion 17 opens. Fig. 9 is an enlarged perspective view showing the tip portions of a first core pin 111 that does not have the circular groove 11b (Figs. 5 to 7) and the second core pin 12 of Fig. 5, which are comparative examples of the present invention. In Fig. 9, the tip surface of the first core pin 111 that does not have the circular groove 11b is entirely a contact surface 111c, except for the protrusion 111a. The contact surface 111c can come into contact with the entire surface of the opposing surface 12b of the second core pin 12.

[0056] As shown in Figure 10(a), when molten metal collides with the butt portion 17 of the first core pin 111 and the second core pin 12, which do not have a circular groove 11b, the first core pin 111 and the second core pin 12 are butted together under an butt load F1, and high-temperature molten metal M collides with the butt portion 17 from a direction perpendicular to the butt portion 17.

[0057] At this time, the portion 111cα of the contact surface 111c of the first core pin 111 on the molten metal collision side and the portion 111cβ on the back side of the molten metal collision side are subjected to strains, i.e., composite strains ε1 and ε2, caused by three factors: the butt load F1, the bending load F2 due to the molten metal collision, and the thermal expansion due to the temperature difference (T1>T2) between the temperature T1 on the molten metal collision side and the temperature T2 on the back side of the molten metal collision side.

[0058] 10(b), when the resultant strain ε2 in the portion 111cβ on the back side of the molten metal collision side becomes 0 or less, it is believed that the butt portion 17 of the first core pin 11 and the second core pin 12 opens (a gap G occurs). If the butt portion 17 opens, it will cause burrs during casting, so it is necessary to suppress the opening of the butt portion 17.

[0059] As shown in Fig. 11(a), the butt compression strain εF1 caused by the butt load F1 is considered to be uniformly generated in the portion 111cα of the contact surface 111c on the molten metal collision side and the portion 111cβ on the back side of the molten metal collision side. The contact surface 111c of the comparative example shown in Fig. 11(a) is larger than the contact surface 11c of the first core pin 11 having the circular groove 11b in Fig. 7 of the above embodiment by the area of ​​the circular groove 11b. Therefore, the surface pressure on the contact surface 111c of the comparative example cannot be increased, and the butt compression strain εF1 caused by the butt load F1 cannot be increased.

[0060] Furthermore, as shown in FIG. 11(b), it is believed that the strain εF2 generated by the bending load F2 due to the collision of the molten metal occurs in the compression direction in the portion 111cα of the contact surface 111c on the molten metal collision side, and in the tension direction in the portion 111cβ on the back side of the molten metal collision side.

[0061] Furthermore, as shown in Figure 11(c), the strain generated by thermal expansion due to the temperature difference (T1>T2) between the temperature T1 on the molten metal collision side and the temperature T2 on the back side of the molten metal collision side is considered to be such that a thermal expansion strain εT1 due to temperature T1 occurs in the portion 111cα of the contact surface 111c on the molten metal collision side, and a thermal expansion strain εT2 due to temperature T2 occurs in the portion 111cβ on the back side of the molten metal collision side (εT1>εT2).

[0062] <How to determine the interference (contact area, groove depth)> In order to suppress the opening of the butt portion 17 shown in Figure 10(b) above, in this embodiment, a circular groove 11b is formed in the tip surface of the first cast pin 11 shown in Figures 5 to 7, and the contact surface 11c is narrowed.

[0063] The contact area (specifically, the area of ​​the contact surface 11c) of the first core pin 11 and the depth of the groove 11b, which can suppress the opening of the butt portion 17, are determined by the steps in the flowchart shown in Figure 12 below, as an example of a method for determining them.

[0064] First, as shown in step S1 of FIG. 12, the bending deflection δ1 of the first core pin 11 due to the collision of the molten metal (the maximum amount of displacement due to bending due to collision) is calculated.

[0065] Next, as shown in step S2, the thermal expansion deflection δ2 (maximum displacement due to thermal expansion) of the first core pin 11 caused by the thermal bias expansion at the time of collision with the molten metal is calculated.

[0066] Next, as shown in step S3, a butt compression deflection δ3 (i.e., the amount of compressive displacement at the contact surface 11c caused by the butt of the first core pin 11 and the second core pin 12) required to offset the bending deflection δ1 due to the collision of the molten metal and the thermal expansion deflection δ2 is calculated. Specifically, the butt compression deflection δ3 is set to be larger than the sum of the bending deflection δ1 and the thermal expansion deflection δ2 (i.e., δ3>δ1+δ2).

[0067] Finally, as shown in step S4, the contact area (specifically, the area of ​​the contact surface 11c) and the depth of the groove 11b of the first core pin 11 are determined based on the calculated butt compression deflection δ3. That is, the first core pin 11 may be designed and manufactured so that the area of ​​the contact surface 11c and the depth of the groove 11b provide the calculated butt compression deflection δ3.

[0068] By manufacturing the first core pin 11 in this way, even if the butt load F1 is the same, the contact area between the first core pin 11 and the second core pin 12 can be reduced to increase the surface pressure of the butt portion 17, thereby increasing the butt compression deflection δ3. This butt compression deflection δ3 can offset the combined deflection of the deflection δ1 due to the bending load acting on the butt portion 17 due to the impact of the molten metal during casting, and the deflection δ2 due to thermal expansion caused by the heat of the molten metal. As a result, it becomes possible to prevent the butt portion 17 from opening.

[0069] In addition, it is preferable that the depth of the groove 11b is as shallow as possible in order to suppress a decrease in the rigidity of the butted portion 17.

[0070] (2) 5 to 7, in the casting apparatus 1 of this embodiment, the tip of the first core pin 11 has a protrusion 11a that protrudes in the axial direction of the first core pin 11. The tip of the second core pin 12 has a recess 12a that can fit into the protrusion 11a when the mold is closed. The contact surface 11c and the circular groove 11b, which is a non-contact portion, are disposed at the tip of the first core pin 11 such that the circular groove 11b is located between the contact surface 11c and the protrusion 11a.

[0071] According to this configuration, by fitting the convex portion 11a at the tip of the first core pin 11 with the concave portion 12a at the tip of the second core pin 12, the first core pin 11 and the second core pin 12 can be centered when the tips of the first core pin 11 and the second core pin 12 are butted against each other during mold closing. In this configuration, the contact surface 11c and the circular groove 11b are located at the tip of the first core pin 11 having the convex portion 11a, so that the circular groove 11b can be located close to the convex portion 11a, and stress can be concentrated on the contact surface 11c during mold closing.

[0072] The tip of the second core pin 12 has a recess 12a that fits with the above-mentioned protrusion 11a, but does not have a non-contact portion (such as a groove). Therefore, at the tip of the second core pin 12, it is possible to ensure the width of the recess 12a that can stably guide the protrusion 11a.

[0073] In addition, when a groove is formed in the second core pin 12 having the guide recess 12a, the groove is difficult to machine and there is a risk that a predetermined butt load cannot be obtained. In addition, there is a risk that the butt load will open the recess 12a. Considering these points, it is preferable that the first core pin 11 having the protrusion 11a has the groove 11b.

[0074] (3) In the casting apparatus 1 of this embodiment, the non-contact portion of the first core pin 11 is a circular groove 11b surrounding the protrusion 11a. With this configuration, since the non-contact portion is a circular groove 11b, it is easy to process the non-contact portion at the tip of the first core pin 11, and it is possible to form the non-contact portion over a wide area. Accordingly, it is possible to reliably reduce the area of ​​the contact surface 11c at the tip of the first core pin 11, so that it is possible to increase the compressive strain associated with the increase in compressive stress at the contact surface 11c when the mold is closed. As a result, it is possible to reliably suppress the opening of the butted portion.

[0075] (4) In the casting apparatus 1 of this embodiment, the circular groove 11b is formed on the periphery of the protrusion 11a, so that the contact surface 11c is circumferentially and continuously disposed on the outer periphery side of the circular groove 11b at the tip of the first core pin 11. Therefore, the contact surface 11c is not divided by the circular groove 11b (i.e., the contact surface 11c is not dispersed), so that it is possible to reliably increase the compressive strain of the contact surface 11c and reliably suppress the opening of the butted portion.

[0076] (5) The casting produced by the casting apparatus 1 of this embodiment is a cylinder block B of an engine 50, and the communication hole formed by the first core pin 11 and the second core pin 12 is a first main gallery 25 serving as a lubricating oil passage. This makes it possible to mold the first main gallery 25 of the cylinder block B using the first core pin 11 and the second core pin 12 on the molten metal inlet 10 side where the molten metal directly hits when molding the cylinder block B. This eliminates the need for additional machining to form the communication hole.

[0077] The casting apparatus of the present invention can be widely applied to the casting of castings having communicating holes, and can manufacture products or parts other than the engine cylinder block of the above embodiment. [Explanation of symbols]

[0078] 1 Casting equipment 2 First side mold 3. Second side mold 4 Lower mold (third mold) 5 Front mold 6 Rear mold 7 Upper mold 9 Cavity 10 Molten metal inlet 11 First core pin 11a Convex part 11b Circular groove (non-contact part) 11c Contact surface 12 Second core pin 12a Recess 12b Opposite surface 16 Inlet Gate 17 Butt joint 25 First Main Gallery 26 Second Main Gallery 50 Engine B. Cylinder block

Claims

1. A casting apparatus for casting a casting having a communicating hole, comprising: a first side die having a first core pin; a second side die disposed opposite the first side die and including a second core pin extending along the same axis as the first core pin; a third mold that forms a cavity together with the first side mold and the second side mold when the molds are clamped, and that has a molten metal inlet formed therein for injecting molten metal into the cavity; It is equipped with the molten metal inlet is disposed such that a direction in which the molten metal flows from the molten metal inlet to the cavity intersects with an axial direction of the first core pin and the second core pin; the first core pin and the second core pin constitute a core for forming the communication hole of the casting by butting their tip ends against each other when the mold is closed, At least one tip end of the first core pin and the second core pin has a contact surface that contacts the other tip end when the molds are closed, and a non-contact portion that is disposed adjacent to the contact surface and is recessed in a direction opposite to the butt direction to be out of contact with the other tip end. A casting apparatus comprising:

2. 2. The casting apparatus according to claim 1, A tip end of the first core pin has a protrusion protruding in an axial direction of the first core pin, a tip end of the second core pin has a recess that can be fitted into the protrusion when the mold is closed, the contact surface and the non-contact portion are disposed at a tip portion of the first core pin such that the non-contact portion is located between the contact surface and the protrusion. The casting device is characterized by:

3. 3. The casting apparatus according to claim 2, The non-contact portion is a circular groove surrounding the protrusion. A casting apparatus comprising:

4. The casting apparatus according to claim 3, The circular groove is formed on the periphery of the protrusion. A casting apparatus comprising:

5. The casting apparatus according to any one of claims 1 to 4, In the above-mentioned casting apparatus, the casting product is a cylinder block of an engine, The communication hole is a lubricating oil passage. A casting apparatus comprising:

Citation Information

Patent Citations

  • Die casting device

    JP2019089075A