Liquid processing method, liquid processing apparatus, and program

The liquid processing apparatus addresses inefficiencies in drying semiconductor wafers by adjusting the cup opening and controlling airflow, enhancing drying efficiency and preventing edge defects, thus improving throughput.

JP2024165518APending Publication Date: 2024-11-28TOKYO ELECTRON LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023081779
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-17
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

Existing methods for processing liquids on semiconductor wafers lack flexibility in adjusting the drying rate and distribution of processing liquids, leading to inefficiencies and potential defects due to residual liquid at the wafer's edge.

Method used

A liquid processing apparatus with a cup that adjusts its opening area using a moving member to control airflow, enhancing drying by increasing airflow velocity over the wafer's edge, and a control system to manage the rotational speed and nozzle movements for precise liquid application and drying.

Benefits of technology

The apparatus improves drying efficiency, reduces residual liquid on the wafer edge, prevents defects, and increases throughput by optimizing the drying process through controlled airflow and rotational speed adjustments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024165518000001_ABST
    Figure 2024165518000001_ABST
Patent Text Reader

Abstract

To increase the degree of freedom in adjusting the dryness of a processing liquid supplied to a substrate.SOLUTION: A liquid processing method according to the present disclosure includes an accommodating step of accommodating a substrate in a cup with the opening area of the cup set as a first area, a processing step of supplying a processing liquid to the substrate held in a substrate holding portion provided in the cup, and then rotating the substrate together with the substrate holding portion to remove the processing liquid and dry the substrate, and a changing step of changing the opening area of the cup such that a period is formed during the processing step during which the opening area of the cup becomes a second area smaller than the first area.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a liquid processing method, a liquid processing apparatus, and a program. [Background technology]

[0002] In the manufacturing process of semiconductor devices, various processing liquids are supplied to a semiconductor wafer (hereinafter, referred to as a wafer) as a substrate to perform processing. Patent Document 1 shows that when resist is supplied to the wafer to form a resist film, gas is supplied to the peripheral portion of the wafer to increase the drying speed of the resist film and adjust the film thickness of the peripheral portion. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2008-60462 A Summary of the Invention [Problem to be solved by the invention]

[0004] The present disclosure provides a technique that allows for greater freedom in adjusting the degree of dryness of a processing liquid supplied to a substrate. [Means for solving the problem]

[0005] The liquid processing method of the present disclosure includes a step of accommodating a substrate in a cup, the opening area of ​​the cup being set to a first area; a processing step of supplying a processing liquid to the substrate held by a substrate holder provided in the cup, and then rotating the substrate together with the substrate holder to remove the processing liquid and dry the substrate; a changing step of changing the opening area of ​​the cup so that a period during which the opening area of ​​the cup has a second area smaller than the first area is formed during the processing step; Equipped with. Effect of the Invention

[0006] The present disclosure can increase the degree of freedom in adjusting the dryness of a processing liquid supplied to a substrate. [Brief description of the drawings]

[0007] [Figure 1] 1 is a vertical sectional side view of a cleaning device according to a first embodiment of a liquid processing apparatus of the present disclosure. [Diagram 2] FIG. [Diagram 3] FIG. 4 is a plan view showing an arrangement of moving members in the cleaning device. [Figure 4] FIG. 4 is a plan view showing an arrangement of moving members in the cleaning device. [Diagram 5] FIG. 11 is a chart showing changes in the rotation speed of a wafer during a cleaning process. [Figure 6] 3A to 3C are explanatory views showing processing steps in the cleaning device. [Figure 7] 3A to 3C are explanatory views showing processing steps in the cleaning device. [Figure 8] 3A to 3C are explanatory views showing processing steps in the cleaning device. [Figure 9] 5A to 5C are explanatory diagrams showing an example of control of a moving member in the cleaning device. [Figure 10] 6A to 6C are explanatory views showing other processing steps in the cleaning device. [Figure 11] 6A to 6C are explanatory views showing other processing steps in the cleaning device. [Figure 12] 11 is a vertical sectional side view of a resist film forming apparatus according to a second embodiment of the liquid processing apparatus. FIG. [Figure 13] FIG. 2 is a plan view of the resist film forming apparatus. [Figure 14] FIG. 11 is a chart showing changes in the rotation speed of a wafer during a film formation process. [Figure 15] 3A to 3C are explanatory views showing processing steps in the resist film forming apparatus. [Figure 16] 3A to 3C are explanatory views showing processing steps in the resist film forming apparatus. [Figure 17] 3A to 3C are explanatory views showing processing steps in the resist film forming apparatus. [Figure 18] 6A to 6C are explanatory views showing other processing steps in the resist film forming apparatus. [Figure 19] 10A to 10C are explanatory views showing still another processing step in the resist film forming apparatus. [Figure 20] 10A to 10C are explanatory views showing still another processing step in the resist film forming apparatus. [Figure 21] FIG. 2 is a block diagram of a system including the resist film forming apparatus. [Figure 22] 5A to 5C are explanatory diagrams showing an example of control of a moving member in the resist film forming apparatus. [Figure 23] FIG. 11 is a perspective view showing another example of the moving member. [Figure 24] FIG. 4 is a plan view showing an arrangement of the moving members. [Diagram 25] FIG. 4 is a plan view showing an arrangement of the moving members. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] [First embodiment] A cleaning apparatus 1 according to a first embodiment of the present disclosure will be described with reference to a vertical cross-sectional side view in Fig. 1 and a plan view in Fig. 2. The cleaning apparatus 1 is an example of a liquid processing apparatus, and performs a cleaning process by supplying a cleaning liquid as a processing liquid to the front and back surfaces of a wafer W, which is a circular substrate. The cleaning liquid is, for example, pure water. The wafer W transported to the cleaning apparatus 1 has, for example, a resist film formed on its front surface. This resist film has been exposed to light according to a predetermined circuit pattern and is in a pre-development state.

[0009] The configuration of the device will be described below using an XYZ Cartesian coordinate system. The X and Y directions are horizontal, and the Z direction is vertical. The X direction may be described as the front-back direction, and the Y direction as the left-right direction. The cleaning device 1 includes a nozzle moving mechanism 2, a cup 3, a spin chuck 11, a rotation mechanism 13, and a wafer W delivery mechanism 15, and performs a cleaning process on the wafer W contained and surrounded by the cup 3 that is open at the top.

[0010] A spin chuck 11 is provided in the cup 3. The spin chuck 11 is a circular substrate holder that sucks the center of the lower surface (rear surface) of the placed wafer W and holds the wafer W horizontally. The spin chuck 11 is connected to a rotation mechanism 13 via a shaft 12 extending in the Z direction. The rotation mechanism 13 rotates the spin chuck 11 and the wafer W held by the spin chuck 11 around a vertical axis. Point P in FIG. 2 is the rotation center point of the spin chuck 11. The wafer W is placed so that its center overlaps with the rotation center point of the spin chuck 11, so point P is also the center point of the wafer W placed on the spin chuck 11.

[0011] The wafer transfer mechanism 15 includes three pins 16 and a lifting mechanism 17. The three pins 16 each extend in the Z direction surrounding the shaft 12, and are raised and lowered by the lifting mechanism 17. The upper ends of the pins 16 protrude above the cup 3 when raised, allowing the wafer W to be transferred between the spin chuck 11 and a transfer mechanism (not shown). For this transfer, the transfer mechanism can move from the front side relative to the cup 3 to the rear side, and position itself above the cup 3.

[0012] Next, the nozzle moving mechanism 2 will be described. The nozzle moving mechanism 2, which is a processing liquid supply mechanism, includes a nozzle 21, a pure water supply unit 22, an arm 23, a moving mechanism 24, and a guide rail 25. The nozzle 21 ejects pure water pressure-fed from the pure water supply unit 22 vertically downward. The pure water supply unit 22 includes a pump and a valve, and can pressure-fed pure water to the nozzle 21 at a desired timing. The nozzle 21 is supported on the tip side (rear end side) of the arm 23, and the base end side of the arm 23 is connected to the moving mechanism 24. The moving mechanism 24 is capable of moving in the Y direction along the guide rail 25, and can raise and lower the arm 23.

[0013] Further, a standby section 26 forming a container that opens upward is provided outside the cup 3 in a plan view, and the nozzle 21 waits in the standby section 26 when not in use. The above-mentioned moving mechanism 24 allows the nozzle 21 to move between the standby section 26 and the inside of the cup 3. The nozzle 21 also moves above the wafer W in the radial direction of the wafer W, and is capable of supplying pure water to a region from the center to the periphery of the wafer W. In addition, reference numeral 27 in Fig. 1 denotes an air supply section, which is provided above the cup 3 so as not to interfere with the movement of the arm 23 and the nozzle 21, and supplies clean air downward.

[0014] Next, the cup 3 will be described. The cup 3 is composed of a cup body 31 and two opening changing units 5. As will be described in detail later, the opening changing unit 5 forms the opening 30 of the cup 3 and includes a moving member 61 that moves relative to the cup body 31, forming a mechanism for changing the opening of the cup 3. By moving the moving member 61, the opening area of ​​the cup 3 in a plan view is changed.

[0015] The cup body 31 includes a guide portion 32, a cylindrical portion 33, a bottom portion 34, a side wall 35, and an upper wall 36. The guide portion 32 is a circular member in a plan view that is disposed below the wafer W, and the shaft 12 penetrates the center portion. The guide portion 32 has a mountain-shaped cross section and a peripheral portion that extends downward so that the cleaning liquid that flows down from the wafer W during processing can be guided to the bottom portion 34 of the wafer W. A backside nozzle 41 is provided on the guide portion 32. Pure water is supplied to the backside nozzle 41 from the above-mentioned pure water supply unit 22, and the pure water is discharged from the backside nozzle 41 toward the peripheral portion of the back side (lower surface) of the wafer W. The pure water supply unit 22 can supply pure water to each of the backside nozzle 41 and the nozzle 21 individually.

[0016] The central part of the guide part 32 in the radial direction is extended downward to form the tube part 33. The lower end of the tube part 33 is extended outward from the cup 3 to form the bottom part 34 of the cup 3. The bottom part 34 is provided with a drainage port 42 and an upright exhaust pipe 43. During operation of the apparatus, exhaust from the exhaust pipe 43 and air supply from the air supply part 27 are performed, and mist generated around the wafer W by processing is carried by the exhaust flow of the air toward the exhaust pipe 43 inside the cup 3 and flows into the exhaust pipe 43 and is removed. The processing liquid that flows down into the cup 3 is removed by flowing into the drainage port 42.

[0017] The periphery of the bottom 34 extends vertically upward to form an upright cylindrical side wall 35, which surrounds the spin chuck 11 and the wafer W held by the spin chuck. The upper end of the side wall 35 extends generally horizontally toward the center of the cup 3 to form an annular upper wall 36, and a circular opening formed by the upper wall 36 is shown as an upper wall opening 37. The center point of the upper wall opening 37 in a plan view coincides with the rotation center point P of the spin chuck 11. The upper wall opening 37 is formed slightly larger than the wafer W in a plan view so that the wafer W can be loaded and unloaded into the cup 3.

[0018] Next, the aperture changing unit 5 will be described. The aperture changing unit 5 is composed of a moving mechanism 51 and a moving member 61, and two aperture changing units 5 are provided in the cup 3. The aperture changing units 5 are provided on the left and right sides of the cup 3, respectively. The left aperture changing unit 5 and the right aperture changing unit 5 are disposed symmetrically with respect to a virtual straight line L that passes through the rotation center point P of the spin chuck 11 and runs along the X-axis in a plan view. The moving mechanism 51 of each aperture changing unit 5 is provided on the upper surface of the center part in the front-rear direction of the upper wall 36. A moving member 52 is provided on the upper wall opening 37 side of the moving mechanism 51 and is connected to the moving mechanism 51.

[0019] The moving mechanism 51 is configured as, for example, a single-acting air cylinder, and a moving member 61 is connected to a piston 55 provided in a space within the moving mechanism 51 via a rod 53 extending horizontally in the left-right direction (Y direction). The moving member 61 moves horizontally in the left-right direction due to the movement of the piston 55. The piston 55 is urged toward the periphery of the cup 3 by a spring 56 provided within the moving mechanism 51. If the peripheral side of the cup 3 with respect to the piston 55 in the space within the moving mechanism 51 is defined as a pressure chamber 57, one end of pipes 58 and 59 is connected to the pressure chamber 57. The other ends of the pipes 58 and 59 are connected to an air supply source 18 and an exhaust source 19, respectively, of a semiconductor manufacturing factory in which the cleaning device 1 is installed, and the moving mechanism 51 operates by supplying and exhausting air to the moving mechanism 51 using the power utility of the factory. Air is supplied from the air supply source 18. The exhaust source 19 is configured, for example, by an exhaust path of the factory in which negative pressure is generated.

[0020] Electromagnetic valves 65 are provided in the pipes 58 and 59, and the opening and closing of each electromagnetic valve 65 allows air to be supplied to and exhausted from the pressure chamber 57. This supply and exhaust changes the pressure in the pressure chamber 57, and the piston 55 moves to a position corresponding to the pressure of the pressure chamber 57 against the biasing force of the spring 56. This allows the moving member 56 to be stopped at any position in the left-right direction. In addition, an adjustment unit 66 for adjusting the flow rate of air supplied to the pressure chamber 57 is provided downstream of the electromagnetic valve 65 in the pipe 58, and by adjusting the flow rate of air, the moving speed of the moving member 61 toward the center of the cup 3 can be set to a desired speed. The supply flow rate by this adjustment unit 66 can be changed by the control unit 10.

[0021] The moving member 61 is composed of a base 62 and a hanging part 63. The base 62 is in contact with or close to the upper surface of the upper wall 36, and is formed in a plate shape extending along the upper surface from the outer periphery of the upper wall opening 37 toward the peripheral edge of the upper wall opening 37, and is disposed in the center of the cup 3 in the front-to-rear direction. The hanging part 63 is formed in a plate shape with the tip side of the base 62 bent vertically downward, and enters the upper wall opening 37. The lower end of the hanging part 63 is located below the height H of the lower end of the upper wall opening 37 (the height of the lower end at the tip of the upper wall 36).

[0022] The moving mechanism 51 moves the moving member 61 between a position (reference position) where the hanging portion 63 contacts the edge of the upper wall opening 37 and does not overlap the wafer W in a plan view, and a position (airflow control position) where the hanging portion 63 is separated from the edge of the upper wall opening 37 and overlaps the wafer W in a plan view. When the moving member 61 is positioned at the airflow adjustment position, the lower end of the hanging portion 63 is close to the upper surface of the wafer W and is formed in an arc shape so as to follow the circumference of the wafer W below it in a plan view. FIG. 3 is a plan view of the moving members 61 positioned at the reference position, and FIG. 4 is a plan view of the moving members 61 positioned at the airflow control position. Thus, in a plan view, the airflow control position is closer to the center of the wafer W than the reference position.

[0023] Note that there is no difference in the distance between the moving mechanism 51 and the moving member 61 at the reference position and the airflow control position between the left opening changing unit 5 and the right opening changing unit 5. Therefore, the left and right moving members 61 shown in Figures 3 and 4 are disposed symmetrically with respect to the above-mentioned imaginary straight line L. Note that in this example, the hanging portion 63 of the moving member 61 located at the airflow control position is set to be located slightly closer to the center of the wafer W than the position of the peripheral edge of the wafer W, but is not limited to this setting, and the airflow control position may be set to be located on the peripheral edge, for example.

[0024] Since the moving member 61 is configured as described above, the area of ​​the circular upper wall opening 37 provided in the cup body 31 that does not overlap with the moving member 61 in a plan view is the opening 30 of the cup 3, and the opening 30 is formed by the upper wall 36 of the cup body 31 and the moving member 61. The moving member 61 is located at a reference position, which is a first position, when transferring the wafer W between the inside of the cup 3 and a transfer mechanism for the wafer W so as not to interfere with the transfer, and is located at an airflow control position, which is a second position, to control the airflow on the peripheral portion of the wafer W when processing the wafer W in the cup 3. Note that the processing of the wafer W here is not limited to supplying a processing liquid, but includes a drying process of the wafer W after supplying the processing liquid.

[0025] Compared with the opening area (first area) when the movable member 61 is located at the reference position, the opening area (second area) when the movable member 61 is located at the airflow control position is smaller because a part of the periphery of the opening 30 protrudes toward the center of the opening 30. In other words, the opening area of ​​the opening 30 in a plan view is reduced by moving the movable member 61 to the airflow control position. The part of the periphery of the opening 30 protruding toward the center of the opening 30 covers the periphery of the wafer W, and the hanging portion 63 comes close to the upper surface of the wafer W as described above.

[0026] The reason why the peripheral portion of the wafer W is covered by the moving member 61 in this manner is to increase the drying speed at the peripheral portion of the wafer W. To be more specific, the air flowing into the cup 3 during processing by exhausting the inside of the cup 3 as described above flows from the center side to the peripheral portion side on the upper surface of the wafer W rotating for processing. When a member for covering the wafer W is disposed above the wafer W, the smaller the gap between the covering member and the wafer W, the faster the speed of the air flow flowing over the upper surface of the wafer W toward the peripheral portion side, and the faster the drying speed. It has been confirmed that when the wafer W is rotated and dried after cleaning, liquid residue is relatively likely to occur on the peripheral portion of the wafer W. In order to prevent the liquid residue, the cleaning apparatus 1 covers the peripheral portion of the wafer W with the moving member 61 described above. In order to reduce the gap formed on the peripheral portion of the wafer W and increase the drying speed, the moving member 61 is formed with a hanging portion 63.

[0027] In addition, a camera 29 serving as an imaging unit is provided at a position above the cup 3 and outside the cup 3 in a plan view. The optical axis of the camera 29 is directed obliquely downward so as to be inclined with respect to each of the X direction, the Y direction, and the Z direction, and can image the inside of the cup 3 at a depression angle. Therefore, it is possible to image the upper surface of the wafer W and the nozzle 21 arranged on the wafer W. Image data acquired by imaging with the camera 29 is transmitted to the control unit 10 described later. The control unit 10 can determine the presence or absence of an abnormality in the surface of the wafer W or an abnormality in the operation of the nozzle 21 from this image data. In addition, as described later, this image data can also be used for feedback control of the operation of the opening changing unit 5.

[0028] The cleaning apparatus 1 includes a control unit 10. The control unit 10 is configured by a computer and includes a program. A group of steps is incorporated in the program so that a series of operations in the cleaning apparatus 1 can be performed. The control unit 10 outputs a control signal to each part of the cleaning apparatus 1 by the program, and the operation of each part is controlled. Specifically, each operation, such as the number of rotations of the spin chuck 11 by the rotation mechanism 13, the raising and lowering of the pins 16 by the lifting mechanism 17, the supply of pure water from the pure water supply unit 22 to the nozzle 21 and the back side nozzle 41, the movement of the nozzle 21 by the moving mechanism 24, the movement of the moving member 61 by opening and closing the electromagnetic valve 65, and the adjustment of the supply flow rate of air to the pressure chamber 57 by the adjustment unit 66, is controlled by the above control signal, and processing is performed on the wafer W as described below. In addition, detection and judgment performed on the wafer W in image data for performing feedback control described below are also performed by the program. The program is stored in a storage medium such as a compact disc, a hard disk, or a DVD, and installed in the control unit 10.

[0029] Next, the processing of the wafer W by the cleaning apparatus 1 will be described with reference to Fig. 5 to Fig. 8. Fig. 5 is a chart showing the change in the rotation speed of the wafer W during processing, and Fig. 6 to Fig. 8 are explanatory diagrams showing the operation of the cleaning apparatus 1. Note that the arrows around the wafer W in Fig. 6 to Fig. 8 indicate airflow.

[0030] With the movable member 61 of each opening changing unit 5 positioned at the reference position, the wafer W is transported by the transport mechanism to above the cup 3, and the wafer W is placed on the spin chuck 11 and held by suction by the vertical movement of the pins 16. The nozzle 21 moves from the waiting section 28 to above the center of the wafer W, and when the wafer W starts to rotate and reaches a predetermined rotation speed R1, the nozzle 21 and the back-side nozzle 41 start to discharge the pure water L1 onto the front and back surfaces of the wafer W (time t1 in the chart). The nozzle 21 moves toward the peripheral portion of the wafer W while discharging the pure water L1, and the cleaning process progresses (FIG. 6).

[0031] Thereafter, the discharge of the pure water L1 from the nozzle 21 and the back surface side nozzle 41 stops (time t2), and the nozzle 21 moves toward the waiting section 28. Then, in order to shake off the pure water L1 from the wafer W, the rotation speed of the wafer W increases (time t3) and reaches a predetermined rotation speed R2. By increasing the rotation speed in this manner, the pure water L1 flows on the wafer W from the center side toward the periphery of the wafer W, and is scattered and removed from the wafer W (FIG. 7).

[0032] Then, after a predetermined time has elapsed from time t3, the moving member 61 moves toward the airflow control position, the opening area of ​​the opening 30 of the cup 3 becomes smaller (time t4), and the hanging part 63 is positioned above the peripheral portion of the wafer W (FIG. 8). This increases the flow rate of the airflow above the peripheral portion of the wafer W, and the drying speed at the peripheral portion increases. Thereafter, the rotation speed of the wafer W decreases (time t5), while the moving member 61 moves toward the reference position. Then, the rotation of the wafer W stops (time t6), and the wafer W is carried out of the cup 3 in the reverse order to the operation when it was accommodated in the cup 3, and is transferred to the transfer mechanism. The period from time t1 when the supply of pure water starts to time t6 when the drying ends and the rotation stops corresponds to the processing step.

[0033] According to this cleaning apparatus 1, in order to dry the wafer W, the rotation speed of the wafer W is increased from R1 when the cleaning liquid is supplied to R2, and then the movable member 61 is moved to reduce the opening area of ​​the opening 30 of the cup 3, and the hanging portion 63 of the movable member 61 is disposed on the peripheral portion of the wafer W. This increases the drying speed at the peripheral portion of the wafer W, and prevents the pure water L1 from remaining on the peripheral portion after the processing is completed. This prevents a decrease in the yield of semiconductor products manufactured from the wafer W. Furthermore, such an increase in the drying speed prevents a long time from being required to complete the drying of the pure water L1, and improves the throughput of the apparatus.

[0034] In the process described in the above chart, a predetermined interval (the interval between times t3 and t4) is provided between the time when the rotation speed is increased to R2 in order to dry the wafer W and the time when the moving member 61 starts moving toward the airflow control position. This is to prevent the occurrence of defects due to the pure water L1 remaining on the wafer W immediately after the rotation speed is increased. Specifically, when the moving member 61 moves to the airflow control position in a state where a large amount of the pure water L1 remains on the wafer W, the pure water L1 scattered from the wafer W by the centrifugal force of the rotation of the wafer W collides with the side wall 35 of the cup 3, bounces off, adheres to the moving member 61, and falls as droplets. When the moving member 61 is in the airflow control position, there is a risk that the droplets will fall onto the periphery of the wafer W and become foreign matter. Therefore, the above-mentioned interval is provided, and the moving member 61 is moved after the removal of the pure water L1 has progressed, thereby preventing the occurrence of such defects and further preventing a decrease in the yield of semiconductor products.

[0035] In addition, a predetermined interval is provided between the timing when the nozzle 21 stops spraying pure water L1 and the timing when the moving member 61 starts moving toward the airflow control position (the interval between times t2 and t4), and this interval is utilized to retract the nozzle 21 and the arm 23 supporting the nozzle 21 from the cup 3 so as not to interfere with the moving member 61.

[0036] However, if the timing at which the movable member 61 starts moving to the airflow control position is too early, there is a risk of liquid dripping onto the peripheral portion of the wafer W as described above. However, in order to sufficiently dry the peripheral portion of the wafer W, it is preferable to move the movable member 61 to the airflow control position at an early timing. In the above-mentioned chart processing, the time t4 at which the movable member 61 starts moving to the airflow control position can be made more appropriate by performing feedback control using image data from the camera 29. The method will be described below with reference to FIG. 9. The wafer W that is first transported to the cleaning apparatus 1 for processing and the wafer W that is subsequently transported to the cleaning apparatus 1 for processing are referred to as wafer W1 and wafer W2, respectively.

[0037] First, the wafer W1 is processed as described with reference to Fig. 5 to Fig. 8. During this process, at least after time t3 when the rotation speed of the wafer W1 increases, an image is captured by the camera 29. Due to the rotation of the wafer W1 after time t3, a liquid film of pure water L1 moves on the surface of the wafer W1 toward the peripheral edge of the wafer W. The control unit 10 detects the time (assumed to be t4') when this liquid film reaches the peripheral edge of the wafer W and disappears from the acquired image data.

[0038] Then, the wafer W2 accommodated in the cup 3 is processed in the same manner as the wafer W1, but the time t4 at which the moving member 61 is moved toward the airflow control position is shifted from the time t4 at which the wafer W1 is processed so as to coincide with the time t4'. Therefore, when the wafer W1 is processed, if the time t4' is later than the time t4, the time t4 at which the wafer W2 is processed is delayed from the time at which the wafer W1 is processed, thereby lengthening the interval between the time t3 at which the rotation speed is increased and the time t4 (right side of FIG. 9). On the other hand, when the wafer W1 is processed, if the time t4' is earlier than the time t4, the time t4 at which the wafer W2 is processed is advanced from the time at which the wafer W1 is processed, thereby shortening the interval between the time t3 at which the rotation speed is increased and the time t4 (left side of FIG. 9). Even if the time t4 is shifted in this way, the interval between the time t3 at which the rotation speed is increased and the time t5 at which the rotation speed is decreased is kept constant and is not changed. By the above feedback control, the peripheral edge of the wafer W can be sufficiently dried while preventing dripping onto the peripheral edge of the wafer W.

[0039] After the wafer W is accommodated in the cup 3, the movable member 61 may be moved from the reference position to a position slightly closer to the center of the wafer W. Then, at time t4, the movable member 61 may be moved from the position closer to the center to the airflow control position. When the above feedback control is performed, the moving speed from the position closer to the center may be controlled.

[0040] In the above example, the left and right opening changing units 5 perform the same operation, but different operations may be performed. With reference to Figs. 10 to 11, differences from the process described in Figs. 5 to 8 will be mainly described. At time t1, the nozzle 21 is moved to the peripheral edge of the wafer W while the pure water L1 is discharged from the nozzle 21 and the back side nozzle 41. At this time, if the nozzle 21 is moved to the right, the moving member 61 of the left opening changing unit 5 is moved to the airflow control position. The moving member 61 of the right opening changing unit 5 is kept at the reference position to prevent interference with the nozzle 21 and the arm 23 (Fig. 10).

[0041] Then, the discharge of the pure water L1 from the nozzle 21 is stopped, the nozzle 21 is retracted from the cup 3, and then the left-side movable member 61 is moved to the airflow control position at time t4 after the rotation speed of the wafer W has increased (FIG. 11). Therefore, the left-side movable member 61 is moved to the airflow control position at the same timing as in FIGS. 5 to 8.

[0042] 10 and 11 in detail, the reason why the movable member 61 is moved from the reference position to the airflow control position after the start of the process as described above is also to prevent interference with the nozzle 21 and the arm 23. Of the left and right opening changing units 5, the movable member 61 on the opposite side to the moving direction of the nozzle 21 moving in the radial direction of the wafer W is moved to the airflow control position before the movable member 61 in the moving direction, since the above-mentioned interference does not occur even if the nozzle 21 is positioned in the cup 3. As a result, after the discharge of the pure water L1 onto the wafer W is stopped, drying of the peripheral portion of the wafer W by the relatively high-speed airflow starts promptly, and the peripheral portion can be dried reliably in a shorter time.

[0043] Second Embodiment A resist film forming apparatus 7 according to the second embodiment will be described with reference to the vertical cross-sectional side view of Fig. 12 and the plan view of Fig. 13, focusing on the differences from the cleaning apparatus 1. The resist film forming apparatus 7 applies thinner and resist in that order to the surface of the wafer W by spin coating to form a resist film. The thinner is a modifying liquid that is applied to the surface of the wafer W before the resist is applied, thereby increasing the wettability of the surface of the wafer W with respect to the resist. In addition, the resist film forming apparatus 7 supplies thinner to the peripheral portion of the rotating wafer W after the resist film is formed, thereby performing a process of removing the resist film limited to the peripheral portion, called EBR (Edge Bead Remover).

[0044] The nozzle moving mechanism 2 in the resist film forming apparatus 7 will be described. Nozzles 71 and 72 are supported on the tip side of the arm 23 instead of the nozzle 21, and the nozzle 71 is connected to a resist supply unit 73, and the nozzle 72 is connected to a thinner supply unit 74. The resist supply unit 73 and the thinner supply unit 74 have substantially the same configuration as the pure water supply unit 22, but instead of pure water, they pressure-feed resist and thinner to the nozzles 71 and 72, respectively. The nozzles 71 and 72 can each move above the center of the wafer W, and can eject resist and thinner to the center. The thinner supply unit 74 can also pressure-feed thinner to the backside nozzle 41 and the EBR nozzle 76 described later, and pressure-feeding thinner to these backside nozzle 41, nozzle 72, and EBR nozzle 76 can be performed individually.

[0045] The resist film forming apparatus 7 is also provided with a nozzle moving mechanism 75 having a configuration substantially similar to that of the nozzle moving mechanism 2. The nozzle moving mechanism 75 is provided to perform EBR, and a difference from the nozzle moving mechanism 2 is that the arm 23 is provided with a nozzle 76 for EBR instead of the nozzles 71 and 72. The nozzle 76 for EBR is connected to a thinner supplying unit 74, and thinner is pressure-fed from the thinner supplying unit 74 to the nozzle 76 for EBR. The nozzle 76 for EBR can move to the periphery of the wafer W and supply thinner to the periphery. The nozzles 71 and 72 wait in the waiting unit 26 when not in use. The resist film forming apparatus 7 is also provided with a waiting unit 77 for waiting the nozzle 76 for EBR when not in use. The waiting unit 77 is provided outside the cup 3 in a plan view, similar to the waiting unit 26.

[0046] Next, the processing of the wafer W by the resist film forming apparatus 7 will be described with reference to Fig. 14 to Fig. 17. Fig. 14 is a chart showing the change in the rotation speed of the wafer W, similar to Fig. 5, and Fig. 15 to Fig. 17 are explanatory diagrams showing the operation of the resist film forming apparatus 7. Note that the operation of the apparatus at time t11' shown in the chart is not performed in this example, and this operation will be described later as the operation of another processing example.

[0047] With the moving member 61 of each opening changing unit 5 positioned at the reference position, the wafer W is suction-held on the spin chuck 11, the nozzle 72 is positioned above the center of the wafer W, and the thinner is discharged. When the thinner discharge is stopped, the wafer W rotates, and the thinner spreads and is applied to the entire surface of the wafer W. Next, with the nozzle 71 positioned above the center of the wafer W and the rotation speed of the wafer W at a predetermined rotation speed R11 (first rotation speed), the resist L2 as the processing liquid is discharged from the nozzle 71 (time t11), and the resist L2 is applied so as to spread to the entire surface of the wafer W (FIG. 15). Next, as the discharge of the resist L2 is completed, the rotation speed of the wafer W is reduced (time t12) to the predetermined rotation speed R12 (second rotation speed). By rotating the wafer W at a relatively low rotation speed in this manner, the film thickness distribution of the resist L2 on the wafer W in the radial direction of the wafer W is made uniform.

[0048] After that, the rotation speed of the wafer W increases (time t13) to a predetermined rotation speed R13 (third rotation speed), and the increase in the rotation speed advances the drying of the resist L2, forming a resist film L3, which is a coating film. The rotation speed R13 is lower than the rotation speed R11. Meanwhile, the nozzles 71 and 72 located in the cup 3 move from above the wafer W toward the waiting section 28. Next, each moving member 61 moves toward the airflow control position (time t14), and the flow rate of the airflow around the periphery of the wafer W increases, and the drying of the resist film L3 at the periphery progresses quickly (FIG. 16). Also, as the drying progresses in this way, the thickness of the resist film L3 on the periphery side of the wafer W becomes larger than when the moving member 61 is not disposed at the airflow control position.

[0049] Thereafter, the rotational speed of the wafer W decreases, and the moving member 61 moves toward the reference position (time t15), and the rotational speed becomes a predetermined rotational speed R14. This rotational speed R14 is greater than the rotational speed R12. While the rotational speed is changing in this manner, the EBR nozzle 76 moves from the waiting section 77 to above the peripheral portion of the wafer W, and the thinner L4 starts to be discharged from the EBR nozzle 76 and the backside nozzle 41 (time t16), and the EBR nozzle 76 moves along the radial direction of the wafer W toward the peripheral edge of the wafer W. As a result, the discharge position of the thinner L4 on the front surface of the wafer W moves toward the peripheral edge of the wafer W, and unnecessary portions of the resist film L3 on the peripheral edge of the wafer W are removed (FIG. 17). The thinner L4 discharged from the backside nozzle 41 cleans the back surface of the wafer W. Thereafter, the ejection of thinner from the EBR nozzle 76 and the back surface side nozzle 41 stops (time t17), and the EBR nozzle 76 returns to the standby section 77 while the rotation of the wafer W continues, and drying of the peripheral portion of the wafer W progresses. Thereafter, the rotation of the wafer W stops (time t18), and the wafer W is carried out of the cup 3. Note that in this example, the period from time t11 when the supply of resist starts to time t15 when the drying of the resist ends and the rotation speed is changed for the next process, EBR, corresponds to the processing step.

[0050] In this way, even when the processing liquid is a coating liquid for forming a coating film such as a resist, it is possible to promote drying at the peripheral portion of the wafer W, thereby improving the throughput of the device. Furthermore, when a coating liquid is used as the processing liquid, the moving member 61 is disposed at the airflow control position to increase the drying speed at the peripheral portion of the wafer W, and this can be utilized to adjust the film thickness distribution of the resist film L3 within the surface of the wafer W.

[0051] In this processing example, the movable member 61 is positioned at the airflow control position during the period when the wafer W rotates at the rotation speed R11 and from a point in time (t14) during the period when the wafer W rotates at the rotation speed R13 onward, so that the opening area is set to the relatively small second area. Then, during the period when the wafer W rotates at the rotation speed R12 and until a point in time (t14) during the period when the wafer W rotates at the rotation speed R13, the movable member 61 is positioned at a reference position, which is a position when the wafer W is loaded into and unloaded from the cup 3, so that the opening area is made larger than the second area. However, the movable member 61 is not limited to being positioned at the reference position, and may be positioned at a position slightly closer to the airflow control position than the reference position as long as there is no effect on the processing of the wafer W.

[0052] Next, another processing example of the resist film forming apparatus 7 will be described with reference to the chart of FIG. 14, focusing on the differences from the processing example described in FIG. 15 to FIG. 17. When the nozzle 71 is positioned above the center of the wafer W and the rotation speed of the wafer W is a predetermined rotation speed R11, the resist L2 is discharged from the nozzle 71 (time t11), and during this discharge, the moving member 61 is moved toward the air flow adjustment position (time t11′, FIG. 18). By reducing the opening area of ​​the opening 30 in this manner, the mist scattered by the collision of the discharged resist L2 with the wafer W is more reliably prevented from leaking outside the cup 3. At the next time t12, in addition to stopping the discharge of the resist L2 from the nozzle 71 and reducing the rotation speed, the moving member 61 is moved toward the reference position. After that, the processing proceeds in the same manner as the processing described in FIG. 15 to FIG. 17. Therefore, after time t12, the moving member 61 moves again between the air flow adjustment position and the reference position.

[0053] The moving member 61 may be placed at the airflow control position before the discharge of the resist L2 at time t11, but immediately after the start of discharge, there may be relatively large disturbances in the liquid flow of the discharged resist L2, and it is considered that the resist L2 may bounce off the surface of the wafer W and adhere to the moving member 61 that has moved to the airflow control position. If this happens, there is a risk that the resist L2 will turn into droplets and fall onto the wafer W as foreign matter, so it is preferable to move the moving member 61 after the start of discharge of the resist L2, as described above.

[0054] 18, the moving member 61 moved to the airflow control position is returned to the reference position at time t12 in order to suppress scattering of mist after time t12 when the discharge of the resist L2 from the nozzle 71 stops, and also to ensure sufficient fluidity of the resist film L3 at times t12 to t13 when the film thickness distribution of the resist film L3 is adjusted. Specifically, if the peripheral portion of the wafer W is covered by the moving member 61 for too long from the time when the resist L2 is applied to the entire surface of the wafer W to the time t13 when the adjustment of the film thickness distribution in the wafer W is completed, the fluidity of the resist L2 at the peripheral portion decreases. As a result, there is a risk that the adjustment of the film thickness distribution cannot be performed sufficiently, so the moving member 61 is returned to the reference position at time t12 as described above to ensure the fluidity of the resist L2.

[0055] The movement of the moving member 61 to the airflow control position when discharging the resist L2 shown in Fig. 18 is referred to as movement for mist, and the movement of the moving member 61 to the airflow control position for drying the resist film L3 shown in Fig. 16 is referred to as movement for drying. The movement speed (first speed) of the moving member 61 in the movement for mist and the movement speed (second speed) of the moving member 61 in the movement for drying may be different. Specifically, the movement speed in the movement for mist is set to be higher than the movement speed during the movement for drying.

[0056] The reason for changing the moving speed in this way will be explained. During the mist movement, the resist L2 is being discharged, the drying of the resist L2 has not progressed to a great extent, and the resist L2 has high fluidity. Therefore, even if the airflow around the resist film is disturbed by the movement of the moving member 61, the effect on the surface shape and film thickness of the resist film L3 is small. The moving speed of the moving member 61 is made relatively large from the viewpoint of such small effect of the airflow and of quickly preventing the mist from leaking out of the cup 3. During the drying movement, the drying of the resist film L3 has progressed to a certain extent, and the surface shape of the resist film is easily affected by the surrounding airflow. Therefore, in order to suppress the disturbance of the airflow, the moving speed of the moving member 61 is made relatively small. From the above, it is effective to make the moving speed during the mist movement larger than the moving speed during the drying movement.

[0057] In addition, the airflow control position (first airflow control position) to which the moving member 61 faces during the movement for mist and the airflow control position (second airflow control position) to which the moving member 61 faces during the movement for drying may be different. The above-mentioned Figs. 16 and 18 show the moving member 61 moved to such different airflow control positions, and the first airflow control position is closer to the center of the upper wall opening 37 of the cup body 31 (closer to the center of the wafer W in a plan view) than the second airflow control position. Therefore, the opening area of ​​the opening 30 of the cup 3 is smaller when the moving member 61 is positioned at the first airflow control position than when the moving member 61 is positioned at the second airflow control position. The opening area of ​​the opening 30 when the moving member 61 is positioned at the second airflow control position by the movement for drying is one area, and the opening area of ​​the opening 30 when the moving member 61 is positioned at the first airflow control position by the movement for mist is another area.

[0058] The reason for changing the airflow control position in this way will be described. The second airflow control position is set so as to be located above the portion where the film thickness of the resist film L3 is the smallest at the peripheral portion of the wafer W when processing is performed with the moving member 61 positioned at the reference position. In other words, the desired position of the second airflow control position is determined according to the film thickness distribution formed on the wafer W. On the other hand, in the mist movement, in order to prevent mist from leaking from the opening 30, the first airflow control position is preferably as close to the center of the opening 30 of the cup 3 as possible, and is set, for example, to a position closest to the center of the upper wall opening 37 within the movable range of the moving member 61. From the above, it is preferable to set the first airflow control position as a position where the opening area of ​​the cup 3 is smaller than that of the second airflow control position.

[0059] In addition, when performing EBR, the movable member 61 may be placed at the airflow control position to hasten drying of the thinner L4 supplied to the peripheral portion of the wafer W. In this case, as described as one example in the first embodiment, only one of the left and right movable members 61 is moved to the airflow control position to prevent interference with the nozzle and the arm. Specifically, if the movement direction of the EBR nozzle 76 that ejects the thinner is to the right as shown in FIG. 19 from time t16 to t17 in the chart of FIG. 14, the right movable member 61 of the left and right opening change units 5 is placed at the reference position to avoid interference with the EBR nozzle 76 and the arm 23 that supports the EBR nozzle 76, and the left movable member 61 is placed at the airflow control position.

[0060] By moving the left movable member 61 to the airflow control position in this manner, after the discharge of thinner from the EBR nozzle 76 stops at time t17, the peripheral portion of the wafer W can be quickly dried. When the discharge of thinner stops at time t17, the EBR nozzle 76 retreats from inside the cup 3 and no longer interferes with the EBR nozzle 76, the right movable member 61 can also be moved to the airflow control position as shown in FIG. 20 to further promote drying.

[0061] Next, referring to FIG. 21, a processing system 8 including a resist film forming device 7 will be described. In this processing system 8, feedback control is performed on the moving speed of the moving member 61 moving to the second airflow control position. The processing system 8 includes a stage on which a transfer container 81 storing a wafer W is placed, a transfer mechanism 83, and a film thickness measuring device 82. The transfer mechanism 83 transfers the wafer W taken out of the transfer container 81 to the resist film forming device 7 and the film thickness measuring device 82 in that order, and returns it to the transfer container 81. The solid arrows in the figure indicate the transfer path of the wafer W, and the dotted arrows indicate the exchange of data. The film thickness measuring device 82 includes a light projecting unit that irradiates light to various parts of the surface of the wafer W, and a light receiving unit that receives the light irradiated by the light projecting unit and reflected by the film on the surface of the wafer W, and the light receiving unit transmits a detection signal corresponding to the received light to the control unit 10. The control unit 10 performs film thickness measurement of the part irradiated with light based on the detection signal.

[0062] Here again, the wafer W that is accommodated in the cup 3 of the resist film forming apparatus 7 first and processed, and the wafer that is accommodated in the cup 3 later and processed will be described as W1 and W2, respectively. The resist film forming apparatus 7 forms a resist film L3 on the wafer W1, and the film thickness measuring device 82 transmits detection signals according to the film thickness of each portion to the control unit 10. The control unit 10 measures the film thickness of the resist film L3 at the peripheral portion from detection signals obtained by irradiating the peripheral portion of the resist film L3 with light. Then, when the wafer W2 is processed by the resist film forming apparatus 7, feedback control is performed on the moving speed of the moving member 61 toward the second airflow control position.

[0063] This feedback control will be described with a specific example. If the detected film thickness of the peripheral portion of the wafer W1 is smaller than a predetermined reference value, the moving member 61 is moved at a moving speed that is increased by a predetermined amount when the wafer W2 is processed, compared to the moving speed of the moving member 61 when moving to the second airflow control position when the wafer W1 is processed. By disposing the moving member 61 at the second airflow control position at an earlier timing than when the wafer W1 is processed, the film thickness of the peripheral portion of the wafer W2 is increased to be greater than the film thickness of the peripheral portion of the wafer W1. On the other hand, if the detected film thickness of the peripheral portion of the wafer W1 is larger than the predetermined reference value, the moving member 61 is moved at a moving speed that is decreased by a predetermined amount when the wafer W2 is processed, compared to the moving speed of the moving member 61 when moving to the second airflow control position when the wafer W1 is processed. By disposing the moving member 61 at the second airflow control position at an earlier timing than when the wafer W1 is processed, the film thickness of the peripheral portion of the wafer W2 is decreased to be less than the film thickness of the peripheral portion of the wafer W1.

[0064] Instead of changing the moving speed in this way, the timing (time t14 in FIG. 14) at which the moving member 61 starts moving toward the second airflow control position may be changed. In other words, the time t14 is shifted while times t13 to t15 in the chart explained in FIG. 14 remain constant. A specific explanation will be given with reference to FIG. 22 which shows the change in the number of rotations.

[0065] If the detected film thickness on the peripheral edge of wafer W1 is smaller than a predetermined reference value, the time t14 at which the movable member 61 moves to the second airflow control position during processing of wafer W1 is advanced by a predetermined time, as shown on the left side of Fig. 22. This lengthens the time that the movable member 61 is positioned at the second airflow control position, and causes the film thickness on the peripheral edge of wafer W2 to be greater than the film thickness on the peripheral edge of wafer W1.

[0066] On the other hand, if the detected film thickness on the peripheral edge of wafer W1 is greater than a predetermined reference value, the time t14 of the moving member 61 moving to the second airflow control position during processing of wafer W1 is delayed by a predetermined time, as shown on the right side of Fig. 22. This shortens the time that the moving member 61 is positioned at the second airflow control position, and the film thickness on the peripheral edge of wafer W2 is made lower than the film thickness on the peripheral edge of wafer W1. Note that feedback control may be performed to change not only one of the moving speed and the timing at which the moving member 61 starts moving (the time at which it is positioned at the second airflow control position), but also both.

[0067] In this resist film forming apparatus 7, after the wafer W is accommodated in the cup 3, the movable member 61 may be moved from the reference position to a position slightly closer to the center of the wafer W, and at time t14, the movable member 61 may be moved from the position closer to the center to the airflow control position. When the above feedback control is performed, it is only necessary to control the moving speed from the position closer to the center and / or the timing of starting the movement.

[0068] In the first and second embodiments, only one aperture changing unit 5 may be provided. However, from the viewpoint of improving the uniformity of processing in the circumferential direction of the wafer W, it is preferable to provide a plurality of aperture changing units 5 as described above, and to form and arrange the moving members 61 symmetrically with respect to the center of the wafer W in a plan view. Providing a plurality of aperture changing units 5 is also preferable from the viewpoint of covering the entire peripheral portion of the wafer W to further improve the uniformity of processing in the circumferential direction, as in the example of forming a circular ring 93 with the moving members described later. It is not limited to providing two aperture changing units 5 each having the moving members 61. For example, a total of four aperture changing units 5 may be provided on each of the front, rear, left and right sides of the rotation center point P of the spin chuck 11.

[0069] Furthermore, when providing two opening changing units 5, the opening changing units 5 are not limited to being provided on the left and right of the cup 3 as in the examples described above, but may be provided at the front and back of the cup 3. However, as already described, the transport mechanism for the wafer W moves in the front-back direction to be positioned above the cup 3. Providing the opening changing units 5 on the left and right of the cup 3 is preferable in that the overlapping area between the opening changing units 5 and the movement path of the transport mechanism can be made relatively small compared to providing them at the front and back, making it easier to design to suppress interference with each other at a limited height above the cup 3.

[0070] The movable member is not limited to the examples described above. Fig. 23 is a perspective view showing another example of the movable member. The movable member 91 shown in Fig. 23 differs from the movable member 61 in that it has a base 92 instead of the base 62. The base 92 is formed in a band shape forming an arc in a plan view, and a portion of the center of the band in the longitudinal direction near the center of the cup 3 protrudes downward to form the hanging portion 63.

[0071] 24 and 25 show the cup 3 equipped with the opening changing unit 5 in which the moving member 91 is provided instead of the moving member 61, and FIG. 24 shows the state in which the moving member 91 is located at the reference position, and FIG. 25 shows the state in which the moving member 91 is located at the airflow control position. When the moving member 91 is located at the reference position, it does not overlap the wafer W in a plan view, similar to the moving member 61 located at the reference position. When the moving members 91 are located at the airflow control position, the ends of the bases 92 of the moving members 91 come into contact with each other to form a ring 93. This ring 93 runs along the rim of the upper wall opening 37, and spans from a position closer to the center of the cup 3 than the rim to a position outside the rim in a plan view. Therefore, no gap is formed between the ring 93 and the upper wall opening 37 in a plan view.

[0072] In plan view, the entire peripheral portion of the wafer W is covered by this circular ring 93. By covering the entire peripheral portion in this manner, the drying speed can be increased, and it is preferable because it is possible to more reliably suppress processing variations in the circumferential direction when performing various processes on the wafer W using the processing liquid.

[0073] Incidentally, the movable member may be configured not to be provided with hanging portion 63. However, as described above, it is preferable to provide hanging portion 63 in order to increase the drying speed of the processing liquid on wafer W. When providing hanging portion 63, the example described above shows an example in which the lower end of hanging portion 63 is located below height H of the lower end of upper wall opening 37, but it may be at the same height as height H.

[0074] Moreover, the moving mechanism 51 of the opening changing unit 5 is not limited to an air cylinder, and may be configured with a hydraulic cylinder. A gas other than air may also be used. Therefore, the fluid that adjusts the pressure inside the moving mechanism 51 to move the moving member 61 is not limited to air. And it is not limited to a single-acting cylinder. Furthermore, the moving mechanism 51 is not limited to one that utilizes pressure changes caused by the supply and removal of a fluid, and the moving member 61 may be configured to be moved by a moving mechanism having a driving source that operates by electricity, such as a motor.

[0075] In the second embodiment, an example in which a resist film is formed as the coating film is shown, but the coating film is not limited to a resist film and may be, for example, an anti-reflection film or an insulating film. Therefore, the coating liquid forming each of these films can be used as the processing liquid. In the second embodiment, it is preferable to move the moving member 61 to the airflow control position after the start of the discharge of the resist L2 as described above, but after the movement to the airflow control position, the nozzle 71 may be moved in the Y direction from the waiting section 28 onto the wafer W so that the discharge of the resist L2 can be started. When the nozzle 71 is moved in this way, if the opening change units 5 are arranged side by side in the front-back direction (X direction) on the cup 3 as described above, the nozzle 71 moves between the opening change units 5 in a plan view. That is, there is no need to move above the opening change unit 5. From this point of view, interference between the opening change unit 5 and the nozzle 71 can be suppressed, and the device can be prevented from becoming larger.

[0076] Furthermore, in each embodiment, the substrate to be processed is not limited to a wafer, but may be, for example, a substrate for manufacturing a flat panel display or a mask substrate for manufacturing a mask for exposure. Therefore, a rectangular substrate may be processed.

[0077] The embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The above-described embodiments may be omitted, substituted, modified, and combined in various forms without departing from the scope and spirit of the appended claims. [Explanation of symbols]

[0078] W wafer 11 Spin chuck 3 cups L1 Pure water

Claims

1. a step of accommodating the substrate in a cup with an opening area of ​​the cup defined as a first area; a processing step of supplying a processing liquid to the substrate held by a substrate holder provided in the cup, and then rotating the substrate together with the substrate holder to remove the processing liquid and dry the substrate; a changing step of changing the opening area of ​​the cup so that a period during which the opening area of ​​the cup becomes a second area smaller than the first area is formed during the processing step; A liquid processing method comprising:

2. the cup comprises a cup body including a side wall surrounding the substrate holding portion and an upper wall extending from the side wall toward the center above the placement portion, and a moving member that moves relative to the cup body by a moving mechanism and forms an opening of the cup; The movable member is provided with a hanging portion that hangs down from an upper wall opening that is surrounded by an inner edge of the upper wall and has a lower end that is the same height as a lower end of the upper wall opening or lower than the lower end of the upper wall opening, The liquid processing method according to claim 1, wherein the change process includes a process of each moving a plurality of the movable members arranged opposite each other across the center of the substrate in a planar view from a first position forming the first area to a second position forming the second area closer to the center of the substrate than the first position in a planar view.

3. 3. The liquid processing method according to claim 1, wherein the changing step is performed after starting supply of the processing liquid to the substrate.

4. 3. The liquid processing method according to claim 1, wherein the processing liquid is supplied to the substrate while the opening area is set to the second area.

5. The second area includes one area and another area smaller than the one area.

3. The liquid processing method according to claim 1, wherein the change process includes a process of changing the opening area to another area while the processing liquid is being ejected onto the substrate, and changing the opening area to the one area after the processing liquid is ejected onto the substrate in order to dry the substrate.

6. the processing liquid is a coating liquid for forming a film on a surface of the substrate, The processing step comprises: setting a rotation speed of the substrate to a first rotation speed while the processing liquid is being discharged onto the substrate; Next, after the discharge of the processing liquid is completed, the rotation speed of the substrate is set to a second rotation speed which is lower than the first rotation speed; Subsequently, the rotation speed of the substrate is set to a third rotation speed that is higher than the second rotation speed, and the processing liquid is dried; The changing step includes: the opening area is set to the second area during a period from a midpoint in the period in which the rotor rotates at the first rotation speed and a period in which the rotor rotates at the third rotation speed, The liquid processing method according to claim 1 or 2, further comprising a step of making the opening area larger than the second area during a period from the period rotating at the second rotation speed to the midpoint of the period rotating at the third rotation speed.

7. The changing step includes: a first moving step of moving a moving member that is moved by a moving mechanism and forms an opening of the cup at a first speed to a position that forms the second area so that the processing liquid is discharged onto the substrate with the opening area being the second area; Next, a second moving step of moving the moving member from a position forming the second area so that the opening area becomes larger than the second area; Subsequently, a third moving step of moving the moving member to a position where the second area is formed at a second speed lower than the first speed so that the substrate is dried in a state where the second area is formed; The liquid processing method according to claim 1 or 2, comprising:

8. the substrates include a first substrate that is accommodated in the cup first and processed, and a second substrate that is accommodated in the cup after the first substrate and processed, the changing step includes a moving step of moving a moving member, which is moved by a moving mechanism and forms an opening of the cup, from a position where an opening area larger than the second area is formed after the supply of the processing liquid to the substrate, to a position where the second area is formed; capturing an image of the first substrate by an imaging unit while the processing step is being performed; determining a timing or a speed of movement of the moving member to a position where the second area is formed in the processing step of the second substrate based on the imaging result; The liquid processing method according to claim 1 or 2, comprising:

9. the substrate includes a first substrate that is first loaded into the cup and processed, and a second substrate that is loaded into the cup after the first substrate and processed, the changing step includes a moving step of moving a moving member, which is moved by a moving mechanism and forms an opening of the cup, from a position where an opening area larger than the second area is formed to a position where the second area is formed; the processing liquid is a coating liquid for forming a film on a surface of the substrate, a measuring step of measuring a thickness of the film formed on the first substrate; determining a timing or a speed of movement of the moving member to a position where the second area is formed in a processing step of the second substrate based on a measurement result obtained in the measuring step; The liquid processing method according to claim 1 or 2, comprising:

10. a cup having an opening area of ​​a first area for receiving the substrate; a substrate holder that holds and rotates the substrate within the cup; a processing liquid supply unit that supplies a processing liquid to the substrate held by the substrate holder; a change mechanism that changes the opening area of ​​the cup so that a period during which the opening area of ​​the cup becomes a second area smaller than the first area is generated, while supplying a processing liquid to the substrate held by a substrate holding part provided in the cup and subsequently rotating the substrate together with the substrate holding part to remove the processing liquid and dry the substrate; A liquid treatment device comprising:

11. a step of accommodating the substrate in a cup with an opening area of ​​the cup as a first area; a processing step of supplying a processing liquid to the substrate held by a substrate holder provided in the cup, and then rotating the substrate together with the substrate holder to remove the processing liquid and dry the substrate; a changing step of changing the opening area of ​​the cup so that a period during which the opening area of ​​the cup becomes a second area smaller than the first area is formed during the processing step; A program to implement the above.

Citation Information

Patent Citations

  • Coating method, program, computer-readable recording medium, and coater

    JP2008060462A