Composite textured yarn and woven or knitted fabric
The false twisted composite textured yarn with a core and presser yarn ratio addresses productivity and naturalness issues, offering a fabric with enhanced texture, comfort, and luxurious appearance while being environmentally friendly.
Patent Information
- Application Number
- JP2024161267
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2024-09-18
- Publication Date
- 2024-11-28
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing composite yarns and fabrics using cellulose filament yarns face issues with productivity, loss of naturalness, and weakened sense of swelling due to the use of twisted yarns, failing to meet consumer demands for improved texture, comfort, and environmental sustainability.
A false twisted composite textured yarn composed of cellulose filaments, with a core yarn and presser yarn ratio of 3:1 to 5:1, featuring a triple-wound slab and single-layer road structure, and a total fineness of 180 to 400 dtex, using acetate, rayon, or cupro fibers, and incorporating yarn length differences to enhance fullness and suppress bulging.
The solution provides an environmentally friendly woven or knitted fabric with excellent productivity, cool texture, supple drapability, luxurious coloring, and gloss, maintaining a natural slab-like appearance and enhancing drapability.
Abstract
Description
[Technical field]
[0001] The present invention relates to a composite textured yarn and a woven or knitted fabric. [Background technology]
[0002] Conventionally, various differentiated composite textured yarns have been proposed that combine the appearance and fluffy feel of a slub shape with the elegant luster of filament yarns.
[0003] In response to the recent diversification of consumer needs, there is a demand for composite textured yarns and woven / knitted fabrics containing such textured yarns that provide improved texture, comfort, and reduced environmental impact while maintaining traditional characteristics as much as possible.
[0004] In response to such demands, for example, Patent Document 1 proposes a woven fabric having a mild slub form using ply-twisted yarns in which the blend ratio of cellulosic filament yarns is 70% or more. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2010-037678 A Summary of the Invention [Problem to be solved by the invention]
[0006] However, the woven fabric described in Patent Document 1 requires the use of doubled and twisted cellulose filament yarns, which poses a problem in terms of productivity. In addition, the use of doubled and twisted cellulose filament yarns causes problems such as a loss of naturalness in the slub form and a reduced sense of volume.
[0007] The present invention aims to provide an environmentally friendly composite processed yarn and woven / knitted fabric that are highly productive and have a refreshing feel, supple drape, luxurious color development and luster. [Means for solving the problem]
[0008] The present invention has the following aspects. [1] A false twist slub yarn consisting of a core yarn and a presser yarn, which is composed only of cellulosic filaments, The ratio of the total fineness of the core yarn to the total fineness of the presser yarn is 3:1 to 5:1, A composite textured yarn in which a slub section in which the presser yarn is wound three times and a middle section in which the presser yarn is wound once around the core yarn are alternately formed in the longitudinal direction of the core yarn and the presser yarn. [2] The composite textured yarn according to [1], having a total fiber size of 180 to 400 dtex. [3] A composite textured yarn as described in [1] or [2], wherein the total fineness of the cellulose filaments of the presser yarn is 30 to 84 dtex and the single fiber fineness is 1.0 to 6.5 dtex. [4] A composite processed yarn described in any of [1] to [3], wherein the difference between the maximum length and the minimum length of the slub portion is 30 mm or more. [5] A composite textured yarn described in any one of [1] to [4], wherein the maximum length of the slub portion is 70 to 120 mm and the minimum length of the slub portion is 10 to 50 mm. [6] A composite processed yarn described in any of [1] to [5], wherein the cellulosic filament is acetate, rayon, or cupra. [7] The core yarn comprises two or more yarns, A composite textured yarn according to any one of [1] to [6], wherein at least one of the core yarns has a yarn length difference of 5 to 40% compared to the other core yarns. [8] The composite textured yarn according to any one of [1] to [7], A woven or knitted fabric, in which the blending ratio of the composite textured yarn is 25 to 100% by mass. [9] The woven or knitted fabric described in [8], which is wrinkled. Effect of the Invention
[0009] The composite textured yarn of the present invention makes it possible to provide environmentally friendly woven and knitted fabrics that are highly productive and have a refreshing feel, supple drape, luxurious color development and luster. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, an embodiment of the present invention will be described in detail. In the present invention, the term "woven or knitted fabric" refers to a woven fabric or a knitted fabric. In addition, the symbol "~" indicating a range of numerical values means that the numerical values before and after it are included as the lower limit and upper limit.
[0011] The composite textured yarn of the present invention (hereinafter also referred to as "the present composite textured yarn") is a false twist slub textured yarn consisting of a core yarn and a presser yarn, which are composed only of cellulosic filaments. This composite processed yarn has a ratio of the total fineness of the core yarn to the total fineness of the presser yarn of 3:1 to 5:1, and a slub section in which the presser yarn is wound three times and a middle section in which the presser yarn is wound once around the core yarn are alternately formed in the longitudinal direction of the core yarn and the presser yarn. In the present invention, the presser thread is a thread that constitutes a slub portion that is triple-wound. The presser thread is also called a sheath thread or a filament thread.
[0012] By using only cellulosic filaments for the core yarn and the presser yarn, the hygroscopicity of the composite processed yarn is maintained, and a refreshing texture can be imparted to the woven or knitted fabric. In addition, by specifying the ratio of the total fineness of the core yarn to the total fineness of the presser yarn when performing the composite processing, the convergence is improved, and a woven or knitted fabric having a natural slub-like appearance and excellent productivity can be obtained.
[0013] The ratio of the total fineness of the core yarn to the total fineness of the presser yarn when performing the composite processing is 3:1 to 5:1. If the total fineness ratio is 3:1 or more, the slub part where the presser yarn is wound three times is prevented from slipping, and the quality of the woven or knitted fabric during production is stabilized. Also, if the total fineness ratio is 5:1 or less, a natural slub-like appearance is easily obtained. From these viewpoints, the ratio of the total fineness of the core yarn to the total fineness of the presser yarn when performing composite processing is more preferably 3.5:1 to 4.5:1.
[0014] The composite textured yarn of the present invention preferably has a total fineness of 180 to 400 dtex. If the total fineness is 180 dtex or more, a natural slubby appearance and a fluffy feel are obtained, and weaving and knitting properties are stable. If the total fineness is 400 dtex or less, a delicate and luxurious product is obtained. From these viewpoints, the total fineness is more preferably 200 to 370 dtex, and even more preferably 220 to 350 dtex.
[0015] In the composite textured yarn of the present invention, the presser yarn preferably has a total fineness of the cellulosic filaments of 30 to 84 dtex and a single fiber fineness of 1.0 to 6.5 dtex. If the total fineness of the cellulose filaments of the presser thread is 30 dtex or more, a natural slubby appearance is obtained, and if it is 84 dtex or less, the slubby portion wound three times is prevented from collapsing, and the quality is stabilized. From these viewpoints, the total fineness of the cellulose filaments of the presser thread is more preferably 35 to 75 dtex, and even more preferably 40 to 65 dtex.
[0016] Furthermore, if the single fiber fineness of the cellulose multifilament of the pressing thread is 1.0 dtex or more, the slumping of the triple-wound slub section is suppressed, the quality is stabilized, and a refreshing feel is obtained, whereas if it is 6.5 dtex or less, a fluffy, soft feel is obtained. From these viewpoints, the single fiber fineness of the cellulose multifilament of the presser thread is more preferably 1.2 to 5.5 dtex, and further preferably 1.4 to 4.5 dtex.
[0017] A "slump" occurs when the triple-rotating presser thread changes its rotational state due to friction or other factors, causing the state of the slab to change.
[0018] In the composite textured yarn of the present invention, the difference between the maximum length and the minimum length of the slub portion is preferably 30 to 100 mm. If the difference between the maximum and minimum lengths of the slab portion is 30 mm or more, a natural appearance effect will be achieved, and if it is 100 mm or less, an appearance with a delicate texture will be achieved. From these viewpoints, the difference between the maximum length and the minimum length of the slab portion is more preferably from 40 to 90 mm, and further preferably from 50 to 80 mm.
[0019] In the composite textured yarn of the present invention, the maximum length of the slub portion is preferably 70 to 120 mm, and the minimum length is preferably 10 to 50 mm. If the maximum length of the slab section is 70 to 120 mm, it will produce a clear decorative effect, and if the minimum length is 10 to 50 mm, it will produce a rich, expressive effect reminiscent of the napped texture of linen.
[0020] The cellulose filaments used in the present invention are preferably acetate, rayon, cupra, or lyocell fibers. In particular, acetate fibers are more preferred because they have excellent color development due to their low refractive index, a luxurious luster, a soft and refreshing texture derived from cellulose, and heat setting properties. The cellulose filaments used in the present invention are not particularly limited in terms of the surface, cross-sectional shape, luster, etc. of the fibers, and may be selected arbitrarily in consideration of the expression of the woven or knitted fabric to be obtained.
[0021] The composite textured yarn of the present invention is composed of two or more core yarns, and at least one of the core yarns can have a yarn length difference of 5 to 40% compared to the other core yarns. By having at least one core yarn have a yarn length difference of 5 to 40% compared to the other core yarns, the sense of volume can be increased and the collapse of the triple-wound slub section can be further suppressed.
[0022] The difference in core yarn length is determined by cutting out a composite textured yarn, disassembling it into its individual yarns, measuring the length of each core yarn, and determining the difference in length. In addition, one method of creating a difference in yarn length between multiple core yarns is to supply multiple core yarns separately when producing composite textured yarn, and to create a difference in yarn length by adjusting the overfeed rate of core yarn 2 relative to core yarn 1.
[0023] The woven or knitted fabric of the present invention contains the above-mentioned composite textured yarn, and the blending ratio of the composite textured yarn is 25 to 100% by mass. When the content of the composite textured yarn in the woven or knitted fabric is 25% by mass or more, a fluffy texture, a natural texture, and a supple drape can be obtained. The blending ratio of the composite textured yarn in the woven or knitted fabric is more preferably in the range of 50% by mass or more, and even more preferably in the range of 70% by mass or more.
[0024] The woven or knitted fabric of the present invention is preferably wrinkled. The method of wrinkle processing is not particularly limited, and may be selected from among methods such as stuffing wrinkles by feeding a larger amount of fabric than usual into a liquid flow dyeing machine, or wrinkle processing by air currents such as a tumbler or air flow after dyeing, taking into consideration the desired appearance of the woven or knitted fabric. The wrinkle processing of the woven or knitted fabric of the present invention provides a natural appearance and a fluffy feel due to the kneading effect. EXAMPLES
[0025] Example 1 A cellulose triacetate fiber filament yarn (manufactured by Mitsubishi Chemical Corporation, Bright 220 dtex / 34 filament (hereinafter f), single yarn chrysanthemum cross section, moisture content 3.5%) was used as the core yarn, and a cellulose triacetate fiber filament yarn (61 dtex 15f, single yarn chrysanthemum cross section, moisture content 3.5%) was used as the pressing yarn. False twisting was performed under the following conditions to obtain a composite textured yarn. ·Number of false twists (T / m): 2000 ·False twist direction: Z -First heater temperature: 170℃ Second heater temperature: 190℃ - Distance between the core yarn and the twisting area: 200mm Overfeed rate of presser thread into false twist area of core thread: 65%
[0026] The obtained composite textured yarn was a slub yarn having a slub where the presser yarn was wrapped around the core yarn three times in the longitudinal direction, and a middle part where the presser yarn was wrapped around the core yarn once. The average fineness of the composite textured yarn was 335 dtex, and the length of the slub part was 10 mm to 100 mm.
[0027] The obtained composite processed yarn was used to weave a twill fabric with a warp density of 72 threads / inch and a weft density of 55 threads / inch. After scouring, the fabric was wrinkled using a liquid jet dyeing machine and then dyed at 120°C with a red disperse dye to produce a fabric with a warp density of 82 threads / inch and a weft density of 59 threads / inch.
[0028] The obtained woven fabric had luxurious coloring and luster, a design effect with natural slubby spots and a moderate sense of volume, as well as a refreshing, comfortable texture and supple drape characteristic of cellulosic fibers.
[0029] Example 2 A cellulose triacetate fiber filament yarn (manufactured by Mitsubishi Chemical Corporation, Bright 135 dtex / 33f, single yarn chrysanthemum cross section, moisture content 3.5%) was used as core yarn 1, a cellulose triacetate fiber filament yarn (50 dtex 34f, single yarn chrysanthemum cross section, moisture content 3.5%) was used as core yarn 2, and a cellulose triacetate fiber filament yarn (40 dtex 9f, single yarn chrysanthemum cross section, moisture content 3.5%) was used as presser yarn. False twisting was performed under the following conditions to obtain a composite textured yarn. ·Number of false twists (T / m): 2000 ·False twist direction: Z -First heater temperature: 170℃ Second heater temperature: 200℃ - Supply guide distance from the core yarn 1 false twisting area: 300 mm - OF rate of core yarn 2 in the false twist region of core yarn 1: 15% Overfeed rate of presser thread into false twist area of core thread 1: 75%
[0030] The obtained composite textured yarn was a slub yarn having a slub where the presser yarn was wrapped three times in the longitudinal direction of the core yarns 1 and 2, and a middle part where the presser yarn was wrapped once. The average fineness of the composite textured yarn was 265 dtex, and the length of the slub part was 15 mm to 110 mm. In addition, the difference in yarn length between core yarn 1 and core yarn 2 was 15%.
[0031] The obtained composite processed yarn was used to weave a plain weave fabric with a warp density of 56 threads / inch and a weft density of 47 threads / inch. After scouring, the fabric was wrinkled using a liquid jet dyeing machine and then dyed at 120°C using a red disperse dye to produce a woven fabric with a warp density of 68 threads / inch and a weft density of 52 threads / inch.
[0032] The obtained woven fabric had luxurious coloring and luster, a design effect with natural slubby spots and a moderate sense of volume, as well as a refreshing, comfortable texture and supple drape characteristic of cellulosic fibers.
[0033] Example 3 The composite textured yarn used in Example 2 was used as the warp and weft to weave a twill fabric. The grey fabric was scoured and dyed in the usual manner to give it a warp density of 95 threads / inch and a weft density of 65 threads / inch. The obtained woven fabric had luxurious coloring and luster, a design effect with natural slubby spots and a moderate sense of volume, as well as a refreshing, comfortable texture and supple drape characteristic of cellulosic fibers.
[0034] Example 4 The composite textured yarn used in Example 2 was used as the warp and weft to weave a matte fabric. The grey fabric was scoured and dyed in the usual manner to give it a warp density of 92 threads / inch and a weft density of 68 threads / inch. The obtained woven fabric had luxurious coloring and luster, a design effect with natural slubby spots and a moderate sense of volume, as well as a refreshing, comfortable texture and supple drape characteristic of cellulosic fibers.
[0035] Comparative Example 1 A polyester filament yarn (manufactured by Mitsubishi Chemical Corporation, Bright 167 dtex / 48 filament (f), single yarn triangle cross section, moisture content 0.2%) was used as the core yarn, and a polyester filament yarn (manufactured by Mitsubishi Chemical Corporation, Bright 33 dtex 12f, single yarn round cross section, moisture content 0.2%) was used as the presser yarn. False twisting was performed under the following conditions to obtain a composite textured yarn. ·Number of false twists (T / m): 2080T / M ·False twist direction: Z -First heater temperature: 165℃ - Second heater temperature: 175℃ - Distance between the core yarn and the twisting area: 350mm Overfeed rate of presser thread into false twist area of core thread: 80%
[0036] The obtained composite textured yarn was a slub yarn having a slub where the presser yarn was wrapped around the core yarn three times in the longitudinal direction, and a middle part where the presser yarn was wrapped around the core yarn once. The average fineness of the composite textured yarn was 250 dtex, and the length of the slub part was 50 mm to 110 mm.
[0037] The obtained composite processed yarn was used to weave a plain weave fabric with a warp density of 90 threads / inch and a weft density of 74 threads / inch. After scouring, the fabric was wrinkled using a liquid jet dyeing machine and then dyed at 120°C using a red disperse dye to obtain a woven fabric with a warp density of 95 threads / inch and a weft density of 83 threads / inch.
[0038] The resulting woven fabric had a slubby appearance, but had a slimy texture lacking in a refreshing feel, and a strong metallic luster, and was therefore unsatisfactory.
[0039] Comparative Example 2 A cellulose triacetate fiber filament yarn (manufactured by Mitsubishi Chemical Corporation, Bright 135 dtex / 33 f, single yarn chrysanthemum cross section, moisture content 3.5%) was used as the core yarn, and a cellulose triacetate fiber filament yarn (110 dtex 26 f, single yarn chrysanthemum cross section, moisture content 3.5%) was used as the pressing yarn. False twisting was performed under the following conditions to obtain a composite textured yarn. ·Number of false twists (T / m): 2000 ·False twist direction: Z -First heater temperature: 170℃ Second heater temperature: 190℃ - Distance between the core yarn and the twisting area: 200mm Overfeed rate of presser thread into false twist area of core thread: 70%
[0040] The composite textured yarn obtained was a slub yarn having a slub where the presser yarn is wrapped around the core yarn three times in the longitudinal direction, and a middle part where the presser yarn is wrapped around the core yarn once. The average fineness of the composite textured yarn was 325 dtex, and the length of the slub part was 10 mm to 90 mm.
[0041] The obtained composite processed yarn was used to weave a twill fabric with a warp density of 74 threads / inch and a weft density of 57 threads / inch. After scouring, the fabric was wrinkled using a liquid jet dyeing machine and then dyed at 120°C using a red disperse dye to produce a fabric with a warp density of 83 threads / inch and a weft density of 60 threads / inch.
[0042] The obtained woven fabric had a luxurious color and luster, and a refreshing and comfortable texture derived from cellulosic fibers, but there were many bumps in the triple-wound slub area and the appearance was not favorable.
Claims
1. A false twist slub textured yarn consisting of a core yarn and a presser yarn, which is composed only of cellulosic filaments, The total fineness of the cellulose filaments of the presser thread is 30 to 84 dtex, and the single fiber fineness is 1.0 to 6.5 dtex; A slub portion in which the presser thread is wound three times and a middle portion in which the presser thread is wound once around the core thread are alternately formed in the longitudinal direction of the core thread and the presser thread.
2. A false twist slub textured yarn consisting of a core yarn and a presser yarn, which is composed only of cellulosic filaments, a slub portion in which the presser yarn is wound three times and a middle portion in which the presser yarn is wound once around the core yarn are alternately formed in a longitudinal direction of the core yarn and the presser yarn; A composite textured yarn, wherein the difference between the maximum length and the minimum length of the slub portion is 30 mm or more.
3. The composite textured yarn according to claim 1 or 2, wherein the total fineness is 180 to 400 dtex.
4. 2. The composite textured yarn according to claim 1, wherein the difference between the maximum length and the minimum length of the slub portion is 30 mm or more.
5. A composite textured yarn according to any one of claims 1 to 4, wherein the maximum length of the slub portion is 70 to 120 mm, and the minimum length of the slub portion is 10 to 50 mm.
6. The composite textured yarn according to any one of claims 1 to 5, wherein the cellulosic filaments are acetate, rayon, or cupra.
7. The core yarn is composed of two or more yarns, A composite textured yarn according to any one of claims 1 to 6, wherein at least one of the core yarns has a yarn length difference of 5 to 40% compared to the other core yarns.
8. The composite textured yarn according to any one of claims 1 to 7 is included, The woven or knitted fabric has a mixing ratio of the composite textured yarn of 25 to 100% by mass.
9. The woven or knitted fabric according to claim 8, which has been wrinkled.
Citation Information
Patent Citations
Noil-like conjugated false twisting yarn and its production
JP1997291426A
Acetate processed yarn and its production
JP2001003237A
Slub-tone composite false-twisted yarn, woven or knit fabric produced by using the same, and method for producing slub-tone composite false-twisted yarn
JP2008190083A
Woven fabric having mild slub form
JP2010037678A