Formation of bump structure
A novel bump formation technique using a metal adhesive layer and sintered conductive particles addresses the challenge of bonding bumps to pads of different materials, enhancing reliability and reducing costs by avoiding high-temperature processes.
Patent Information
- Application Number
- JP2024140843
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2019-10-23
- Filing Date
- 2024-08-22
- Publication Date
- 2024-12-04
- Estimated Expiration
- 2040-09-22
AI Technical Summary
Existing bump formation techniques face challenges in creating bonded bump structures on pads made of different conductive materials, particularly when using conductive materials like aluminum, leading to compromised adhesion and reliability issues due to electromigration.
A method involving the use of a metal adhesive layer on the pad, followed by sintering conductive particles to form a bump structure, which includes a solder cap, allowing the bumps to be firmly bonded to pads made of different conductive materials without high-temperature conditions.
The method ensures strong bonding between the bumps and pads, improving reliability and preventing electromigration, while eliminating the need for expensive electroplating processes and reducing manufacturing costs.
Smart Images

Figure 2024167912000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention generally relates to bump formation technology, and more particularly to a method for fabricating a bump structure, a bump structure, an electronic device including a bump structure, and a method for manufacturing an electronic device. [Background technology]
[0002] 3D and 2.5D chip packaging, which allows high bandwidth signal transmission and short wiring length, has been attracting attention to improve the performance of future computer systems. As the bump pitch and bump size in 3D and 2.5D packaging become finer compared to traditional flip-chip packaging, reliability issues arise due to stress concentration at solder joints and their interfaces and electromigration due to high current density.
[0003] IMS (Injection Molded Solder) technology is a bump formation technology that forms solder bumps on a substrate by directly injecting molten solder into the openings in a resist mask. IMS technology has the advantage of flexible solder alloy composition, which translates into improved fine pitch capability as well as mechanical properties and resistance to electromigration.
[0004] The recent trend in high density interconnects has led to the use of copper pillar (or post) bumps. However, to create the copper pillars under the solder cap, an expensive copper plating process is required. There is another technique that can create pillar bumps without using the expensive plating process, where the pillars are created by sintering conductive particles, typically provided in the form of a paste. Sintered pillars show good reliability when the pillars are created on contact pads made from the same material, i.e., sintered copper pillars are created on copper pads.
[0005] However, when a conductive material different from the pillars, especially aluminum, is used as the contact pad, the adhesion between the pillars and the contact pads is reduced even if the surface oxide of the aluminum pads is removed before bump formation.
[0006] Therefore, there is a need for a new bump formation technique that can produce a bump structure that includes a set of bumps formed on a substrate, in which the bumps made by sintering conductive particles are firmly bonded to pads made from a conductive material different from the conductive particles. Summary of the Invention
[0007] According to one embodiment of the present invention, a method for making a bump structure is provided. The method includes providing a substrate including a set of pads formed on a surface thereof, the pads including a first conductive material. The method also includes coating a metal adhesion layer on each pad. The method further includes forming a bump on each pad by sintering conductive particles with a mold layer, the conductive particles including a second conductive material different from the first conductive material.
[0008] This allows the creation of a bump structure that includes a set of bumps on a substrate, in which the bumps made by sintering conductive particles are firmly bonded to the pads of the substrate, even if the pads are made from a different conductive material than the conductive particles.
[0009] In one embodiment, the mold layer has a set of openings, each opening aligned with one of the pads. The method includes disposing the mold layer over the substrate and filling conductive particles into the openings of the mold layer while forming a bump on each pad. Sintering the conductive particles filled into the openings of the mold layer to provide a bump underlayer on each pad. The method further includes filling remaining space in each opening of the mold layer above the bump underlayer with a solder material to form a solder cap on each bump underlayer.
[0010] In one embodiment, the first conductive material includes Al and the second conductive material includes Cu, and since semiconductor devices typically use Al pads as the outermost layer, it is possible to create a practical sintered bump substrate that is firmly bonded to the pad.
[0011] In one embodiment, the conductive particles are provided in the form of a paste. The bump underlayer formed on each pad has a cup shape that fits the contour of the mold layer opening and has a bottom that is bonded to the pad by a metal adhesion layer. This allows for a sufficient amount of solder to be deposited on the bump underlayer even with smaller bump sizes compared to flat-topped pillar shapes. The cup-shaped bump underlayer also has an advantage in terms of resistance to electromigration because the current flow is distributed in bumps of this shape.
[0012] In one embodiment, the method further includes applying a resist layer on the surface of the substrate. The method also includes patterning the resist layer to create a mold layer. The method further includes depositing a metal adhesion material on the pads and the mold layer to conform to the contour of the mold layer, providing a metal adhesion layer coated on each pad. Since there is no removal process of the metal layer under the resist layer after resist stripping, undercutting of the base of the bump is prevented.
[0013] In one embodiment, the method includes dissolving the metal adhesive material deposited on the top surface of the mold layer into the solder material during filling with the solder material. This allows the excess metal adhesive material to be sufficiently removed while eliminating the process of removing the excess metal adhesive material. In this preferred embodiment, the metal adhesive material can be selected from the group consisting of Cu, Ni, Au, and any combination thereof. Cu, Ni, and Au are easily dissolved in the solder material, such as molten solder, during the solder material filling process.
[0014] In one embodiment, the method further includes peeling the mold layer from the substrate, washing off the mold layer, and lifting off and washing off the metal adhesive material on the top surface of the mold layer together with the mold layer. This allows the process of removing excess metal adhesive material to be omitted regardless of the composition of the metal adhesive material. Therefore, other functional materials such as Ti barrier can be used as the metal adhesive material even if they are insoluble in solder materials such as molten solder. Also, the metal adhesive material that conforms to the contour of the mold layer acts as a sidewall barrier to prevent short circuits between bumps due to ion migration.
[0015] In one embodiment, the method further includes removing the metal adhesive material deposited on the top surface of the mold layer by a technique selected from the group consisting of chemical mechanical polishing (CMP), mechanical polishing, fly-cutting, and chemical etching. The process of removing the excess metal adhesive material is performed, but the process of removing the metal layer after resist stripping, which causes undercuts at the base of the bumps, is omitted. Other functional materials, such as Ti barrier, can also be used as the metal adhesive material, even if they are insoluble in solder materials such as molten solder. Also, the metal adhesive material that conforms to the contours of the mold layer acts as a sidewall barrier to prevent short circuits between the bumps due to ion migration.
[0016] In one embodiment, the method further includes depositing a metal adhesion material on the surface of the substrate to have a first portion corresponding to the metal adhesion layer coated on each pad and a second portion formed in an outer region of the pad. The method includes applying a resist layer on the metal adhesion material. The method also includes patterning the resist layer to create a mold layer. The method includes peeling the mold layer from the substrate, thereby leaving the bumps on the substrate, each bump including a solder cap and a bump undercoat formed on the pad. The method further includes removing the second portion of the metal adhesion material exposed from the bump. Other functional materials, such as Ti barriers, can also be used as the metal adhesion material, even if the material is insoluble in a solder material such as molten solder. In this embodiment, the metal adhesion material can be selected from the group consisting of Cu, Ti, Ni, Au, and any combination thereof.
[0017] In one embodiment, filling the solder material includes injecting molten solder into each opening in the mold layer. In this embodiment, no electrolytic and electroless plating is required to create the set of bumps, thereby avoiding expensive pillar and solder cap creation processes, expensive equipment, and complex management of the plating process.
[0018] In one embodiment, the method includes removing surface oxides from the pads by reverse sputtering prior to coating of the metallic adhesion layer, the metallic adhesion layer being coated on each pad by sputtering. The combination of reverse sputtering and sputtering of the metallic adhesion layer is preferred to reduce the time interval between surface oxide removal and surface coating of the pads.
[0019] In one embodiment, the substrate includes a semiconductor device, and a set of pads is formed on at least an active surface of the semiconductor device. The method further includes interconnecting the semiconductor device to an external circuit using the bumps, and thus the method is a method for manufacturing an electronic device. The high temperature conditions of sintering contribute to strengthening the bond between the sintered pillars and the pads. However, semiconductor devices generally deteriorate under such high temperature conditions. This allows the bonding between the bump base and the pads to be improved without using high temperature conditions.
[0020] According to another embodiment of the present invention, a bump structure is provided. The bump structure includes a substrate including a set of pads formed on a surface thereof, the pads including a first conductive material. The bump structure also includes a set of bumps, each formed on one of the pads. Each bump includes a metal adhesion layer formed on the pad and a bump undercoat formed on the metal adhesion layer. The bump undercoat is a sintered body of conductive particles including a second conductive material different from the first conductive material.
[0021] The bump structure according to the embodiment of the present invention has a bump formed by sintering conductive particles and firmly bonded to the pad, so that the bump structure shows good reliability even if the pad is made of a conductive material different from the conductive particles. In addition, the bond between the bump base and the pad can be improved without using high temperature conditions. Therefore, the deterioration of the semiconductor device caused by the bump formation process can be prevented.
[0022] In one embodiment, each bump further includes a solder cap formed on the under-bump. The under-bump has a shape of a cup with a bottom bonded to the pad via a metal adhesion layer, and the cup is filled with the solder material of the solder cap. In a particular embodiment, the first conductive material can include Al, the second conductive material can include Cu, and the metal adhesion layer can include a material selected from the group consisting of Cu, Ti, Ni, Au, and combinations thereof.
[0023] In one embodiment, the metal adhesion layer covers the sides of the under-bump structure as a sidewall barrier, which prevents short circuits between the bumps due to ion migration.
[0024] In another embodiment of the invention, an electronic device is provided. The electronic device includes a semiconductor device including a set of pads formed on an active surface, the pads including a first conductive material. The electronic device also includes a set of bumps, each formed on one of the pads. Each bump includes a metal adhesion layer formed on the pad and a bump underlayer formed on the metal adhesion layer, the bump underlayer being a sintered body of conductive particles including a second conductive material different from the first conductive material. The electronic device further includes a circuit interconnected to the semiconductor device via the set of bumps.
[0025] Electronic devices according to embodiments of the present invention exhibit good durability because bumps made by sintering conductive particles are firmly bonded to pads, even if the pads are made of a conductive material different from the conductive particles used for the bump base.
[0026] In one embodiment, the metal adhesion layer covers the side of the under-bump as a sidewall barrier to prevent short circuits between the bumps due to ion migration.
[0027] In another embodiment of the invention, a method of manufacturing an electronic device is provided. The method includes providing a bumped semiconductor device. The bumped semiconductor device includes a substrate including a set of pads formed on a surface thereof, the pads including a first conductive material. The bumped semiconductor device also includes a set of bumps each formed on one of the pads, each bump including a metal adhesion layer formed on the pad and a bump underlayer formed on the metal adhesion layer, the bump underlayer being a sintered body of conductive particles including a second conductive material different from the first conductive material. The method further includes interconnecting the bumped semiconductor device to an external circuit via the set of bumps.
[0028] Electronic devices provided by the methods according to embodiments of the present invention exhibit good durability because the bumps made by sintering the conductive particles are firmly bonded to the pads, even if the pads are made of a conductive material different from the conductive particles used for the bump base.
[0029] Additional features and advantages are realized through the techniques of the present invention.Other embodiments and aspects of the invention are described in detail herein and are considered a part of the claimed invention.
[0030] The subject matter which is regarded as the invention is particularly pointed out and distinctly claimed in the concluding claims of this specification. The foregoing and other features and advantages of the invention will become apparent from the following detailed description taken in conjunction with the accompanying drawings. It should be noted that the sizes and relative positions of elements and layers in the drawings are not necessarily drawn to scale. Some of these elements or layers have been arbitrarily enlarged and positioned to improve the legibility of the drawings. [Brief description of the drawings]
[0031] [Figure 1A] 1 is a cross-sectional view of a bump structure according to an embodiment of the present invention; [Figure 1B] FIG. 2 is a top view of a bump structure according to one embodiment of the present invention. [Figure 2A] 1A-1C are cross-sectional views (1 / 2) of a structure obtained at a step of a bump formation process according to an embodiment of the present invention. [Figure 2B] 1A-1C are cross-sectional views (1 / 2) of a structure obtained at a step of a bump formation process according to an embodiment of the present invention. [Figure 2C] 1A-1C are cross-sectional views (1 / 2) of a structure obtained at a step of a bump formation process according to an embodiment of the present invention. [Figure 2D] 1A-1C are cross-sectional views (1 / 2) of a structure obtained at a step of a bump formation process according to an embodiment of the present invention. [Figure 2E]1A-1C are cross-sectional views (1 / 2) of a structure obtained at a step of a bump formation process according to an embodiment of the present invention. [Figure 3A] 2A-2C are cross-sectional views (2 / 2) of a structure obtained at a step of a bump formation process according to an embodiment of the present invention. [Figure 3B] 2A-2C are cross-sectional views (2 / 2) of a structure obtained at a step of a bump formation process according to an embodiment of the present invention. [Figure 3C] 2A-2C are cross-sectional views (2 / 2) of a structure obtained at a step of a bump formation process according to an embodiment of the present invention. [Figure 3D] 2A-2C are cross-sectional views (2 / 2) of a structure obtained at a step of a bump formation process according to an embodiment of the present invention. [Figure 4A] 1A-1C are cross-sectional views (1 / 2) of a structure obtained at a step of a bump formation process according to another embodiment of the present invention. [Figure 4B] 1A-1C are cross-sectional views (1 / 2) of a structure obtained at a step of a bump formation process according to another embodiment of the present invention. [Figure 4C] 1A-1C are cross-sectional views (1 / 2) of a structure obtained at a step of a bump formation process according to another embodiment of the present invention. [Figure 4D] 1A-1C are cross-sectional views (1 / 2) of a structure obtained at a step of a bump formation process according to another embodiment of the present invention. [Figure 5A] 2A-2C are cross-sectional views (2 / 2) of a structure obtained at a step of a bump formation process according to another embodiment of the present invention. [Figure 5B] 2A-2C are cross-sectional views (2 / 2) of a structure obtained at a step of a bump formation process according to another embodiment of the present invention. [Figure 5C] 2A-2C are cross-sectional views (2 / 2) of a structure obtained at a step of a bump formation process according to another embodiment of the present invention. [Figure 5D] 2A-2C are cross-sectional views (2 / 2) of a structure obtained at a step of a bump formation process according to another embodiment of the present invention. [Figure 6A] 3A-3C are cross-sectional views of structures obtained at steps of a bump formation process according to another embodiment of the present invention. [Figure 6B] 3A-3C are cross-sectional views of structures obtained at steps of a bump formation process according to another embodiment of the present invention. [Figure 6C] 3A-3C are cross-sectional views of structures obtained at steps of a bump formation process according to another embodiment of the present invention. [Figure 7A] 3A-3C are cross-sectional views of structures obtained at steps of a bump formation process according to another embodiment of the present invention. [Figure 7B] 3A-3C are cross-sectional views of structures obtained at steps of a bump formation process according to another embodiment of the present invention. [Figure 7C] 3A-3C are cross-sectional views of structures obtained at steps of a bump formation process according to another embodiment of the present invention. [Figure 7D] 3A-3C are cross-sectional views of structures obtained at steps of a bump formation process according to another embodiment of the present invention. [Figure 8A] 3A-3D are cross-sectional views of structures obtained at steps of a flip chip bonding process according to an embodiment of the present invention. [Figure 8B] 3A-3D are cross-sectional views of structures obtained at steps of a flip chip bonding process according to an embodiment of the present invention. [Figure 9A] A related bump formation process involves electroplating of both the pillars and the solder cap. [Figure 9B] A related bump formation process involves electroplating of both the pillars and the solder cap. [Figure 9C] A related bump formation process involves electroplating of both the pillars and the solder cap. [Figure 9D] A related bump formation process involves electroplating of both the pillars and the solder cap. [Figure 9E] A related bump formation process involves electroplating of both the pillars and the solder cap. [Figure 10A] Another related bump formation process involves electroplating of the pillars and IMS of the solder cap. [Figure 10B]Another related bump formation process involves electroplating of the pillars and IMS of the solder cap. [Figure 10C] Another related bump formation process involves electroplating of the pillars and IMS of the solder cap. [Figure 10D] Another related bump formation process involves electroplating of the pillars and IMS of the solder cap. [Figure 10E] Another related bump formation process involves electroplating of the pillars and IMS of the solder cap. [Figure 11A] Another related bump formation process involves electroless plating of the pillars and IMS of the solder cap. [Figure 11B] Another related bump formation process involves electroless plating of the pillars and IMS of the solder cap. [Figure 11C] Another related bump formation process involves electroless plating of the pillars and IMS of the solder cap. [Figure 11D] Another related bump formation process involves electroless plating of the pillars and IMS of the solder cap. [Figure 12A] Another related bump formation process is based on conductive paste sintering without the use of a metal adhesive layer (1 / 2). [Figure 12B] Another related bump formation process is based on conductive paste sintering without the use of a metal adhesive layer (1 / 2). [Figure 12C] Another related bump formation process is based on conductive paste sintering without the use of a metal adhesive layer (1 / 2). [Figure 12D] Another related bump formation process is based on conductive paste sintering without the use of a metal adhesive layer (1 / 2). [Figure 13A] Another related bump formation process is based on a sintering process that does not use a metal adhesion layer (2 / 2). [Figure 13B] Another related bump formation process is based on a sintering process that does not use a metal adhesion layer (2 / 2). [Figure 13C] Another related bump formation process is based on a sintering process that does not use a metal adhesion layer (2 / 2). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0032] The present invention will be described below with reference to specific embodiments, however, those skilled in the art will understand that the embodiments described below are referred to as examples only and are not intended to limit the scope of the present invention.
[0033] One or more embodiments according to the present invention are directed to methods of making a bump structure, an associated bump structure, an associated electronic device including the bump structure, and an associated method of manufacturing an electronic device including the bump structure, whereby a set of bumps are achieved that are firmly bonded to respective pads of a substrate.
[0034] A bump structure according to an exemplary embodiment of the present invention will be described below with reference to Figures 1A and 1B. Figure 1A shows a cross-sectional view of bump structure 100. Figure 1B shows a top view of bump structure 100. It should be noted that the cross-sectional view shown in Figure 1A corresponds to the cross-section indicated by "A" in the top view of Figure 1B.
[0035] 1 includes a substrate 110 that includes a set of pads 112 and a passivation layer 114 formed on a surface of the substrate 110. The bump structure 100 also includes a set of bumps 120, each of which is formed on a corresponding one of the pads 112. It should be noted that the reference numbers for the bumps 120 are shown for convenience only with respect to a representative bump and not all components.
[0036] The substrate 110 may be any substrate made of semiconductor materials. In a particular embodiment, the substrate 110 is a wafer (or panel) incorporating multiple electronic devices. In this particular embodiment, the wafer may eventually be separated into multiple chips (or dies). In another particular embodiment, the substrate 110 is a chip separated from the wafer. In the described embodiment, both the wafer and the chip are semiconductor devices. The wafer and the chip may be made of silicon, III-V or II-VI compound semiconductor materials, or other semiconductor materials. The wafer and the chip may be fabricated by any standard semiconductor process, including FEOL (Front End Of Line) and BEOL (Back End Of Line) processes. In the described embodiment, the substrate 110 is described as a semiconductor device, but any other substrate, such as a ceramic substrate, a glass substrate, a printed circuit board, etc., may be used as the substrate 110.
[0037] The pads 112 are made of a conductive material. Examples of the conductive material generally include metals such as aluminum (Al), copper (Cu), cobalt (Co) and other metallic materials. In the following, a case where the pads 112 are made of Al will be mainly described as an example to which the present bump formation technology can be applied. The pads 112 may be arranged on the surface of the substrate 110 at a specific pitch (e.g., 20 to 300 micrometers). The set of pads 112 is formed in a two-dimensional array as shown in FIG. 1B. The passivation layer 114 may include an insulating material such as silicon oxide (SiO2).
[0038] 1A-1B, in addition to the set of bumps 120, the substrate 110 may include electronic elements, optoelectronic elements such as photodiodes (PDs) and light emitting diodes (LEDs), and / or multiple wiring layers connected to the bumps 120. The substrate 110 may also include a stack of semiconductor substrates.
[0039] 1A also shows a more detailed structure of each bump 120. As shown in FIG 1A, each bump 120 includes a metal adhesion layer 126 formed on the pad 112 and a bump underlayer 122 formed on the pad 112 via the metal adhesion layer 126. Each bump 120 may further include a solder cap 124 formed on the bump underlayer 122. It should be noted that the metal adhesion layer 126 is a type of UBM (Under Bump Metallurgy).
[0040] The bump underlayer 122 is generally made of a conductive material that may include copper (Cu), nickel (Ni), silver (Ag), gold (Au), or other metal materials. Each bump underlayer 122 is made by sintering conductive particles using a mold layer or resist layer disposed on the substrate 110. Therefore, the bump underlayer 122 is a sintered body of conductive particles that includes a conductive material different from that of the pad 112. In the following, as an example to which the present bump formation technology can be applied, a case in which the bump underlayer 122 is made of copper will be mainly described. Therefore, the conductive particles are copper particles, and the bump underlayer 122 is a sintered body of copper particles.
[0041] In a preferred embodiment, copper nanoparticles, copper microparticles and mixtures thereof are used for the bump undercoat formation. The sintered body of the conductive particles has a porous morphology. The size of the particles may be in the range of 1 nm to 15 μm.
[0042] The under-bump 122 has the shape of a cup with a bottom that is bonded to the pad 112 via a metal adhesion layer 126. The cup of the under-bump 122 is filled with the solder material of a solder cap 124.
[0043] The metallic adhesion layer 126 is made of a metallic material selected from the group consisting of Cu, Ti, Ni, Au, and combinations of these elements. The metallic adhesion layer 126 can include a single layer or multiple layers (or stacks), each layer including the above-mentioned elements as pure metals or two or more of the above-mentioned elements as alloys. In certain embodiments, the metallic adhesion layer 126 is a stack of Ti / Cu, a layer or stack of Cu, Au, or Ni, or combinations thereof.
[0044] The solder material of the solder cap 124 can have any suitable composition. In one or more embodiments, any of the lead-free solder alloys including binary, ternary and quaternary systems of one or more elements selected from the group consisting of tin, bismuth, silver, indium, antimony, copper, zinc, nickel, aluminum, manganese and palladium may be used as the solder material. Examples of lead-free solder alloys may include Bi-Sn, Sn-Ag, Sn-Ag-Bi, Sn-Ag-Cu, Sn-Cu alloys, to name a few. The freedom in the solder composition allows any composition suitable for bump formation to be selected.
[0045] A bump formation process for producing a bump structure according to an exemplary embodiment of the present invention will now be described with reference to the series of Figures 2A-2E and 3A-3D, which show cross-sectional views of structures obtained at each step of the bump formation process for producing the bump structure 100 shown in Figures 1A and 1B.
[0046] As shown in FIG. 2A, the bump formation process can include preparing a substrate 110 including a set of pads 112 and a passivation layer 114 formed on a surface 110a of the substrate 110. In a particular embodiment, the bump formation process is performed as a wafer-level process, and the substrate 110 is a wafer incorporating multiple integrated circuits. Each pad 112 can include a conductive material. If the pads 112 are formed of an easily oxidized metal, such as Al, the bump formation process can also include removing surface oxides from the pads 112. Removal of the surface oxide can be accomplished by virtually any standard means, including, for example, reverse sputtering, etching with an acidic solution, etc.
[0047] As shown in FIG. 2B, the bump formation process can include depositing a metal adhesion material 128 on the surface 110a of the prepared substrate 110. The deposited metal adhesion material 128 can include a first portion 128a and a second portion 128b. The first portion corresponds to the metal adhesion layer 126 coated on the pad 112. The second portion 128b is formed on the outer region of the pad 112, where the passivation layer 114 may generally be formed. Any known seed layer typically used for electroplating pillars can be used as the metal adhesion material 128. The metal adhesion material is selected from the group consisting of Cu, Ti, Ni, Au, and combinations thereof. In a particular embodiment, the metal adhesion layer 126 is a stack of Ti / Cu, a layer or stack of Cu, Au, or Ni, or combinations thereof. The deposition of the metal adhesion material 128 can be performed by virtually any standard means, including, for example, sputtering, electroless plating. It should be noted that sputtering can provide a metal adhesion layer over the entire area, whereas electroless plating can provide a metal adhesion layer over a limited area, including pad 112 .
[0048] The removal of the surface oxide and the deposition of the metal adhesion material 128 can be performed by virtually any standard means, but when the pad 112 is formed of an easily and persistently oxidized metal such as Al, a combination of reverse sputtering and sputtering of the metal adhesion material is preferably employed to shorten the time interval between the removal of the surface oxide and the surface protection of the pad 112. A long time interval would cause deterioration of the bonding of the Al pad. Moreover, this combination is advantageous from the viewpoint of eliminating the plating process, which is generally expensive in itself and requires expensive equipment and complicated management of the plating process.
[0049] As shown in FIG. 2C, the bump formation process can also include applying a resist layer 130 onto the metal adhesion material 128. Any known liquid or film photoresist, positive or negative, can be used. The resist layer 130 can be applied by virtually any standard means, including spin coating, film lamination, etc.
[0050] As shown in FIG. 2D, the bump formation process may also include patterning the resist layer 130 to have a set of openings 130a formed therethrough. Each opening 130a is aligned with a corresponding pad 112. The openings 130a expose the surface of the metal adhesion material 128 on the pads 112. The patterned resist layer 130 may act as a mold layer to shape the material that fills the openings 130a. The openings 130a may have any shape, including but not limited to circular, square, and rounded square, to name a few. It should be noted that this resist patterning may be followed by electroless plating if electroless plating is employed to deposit the metal adhesion material 128.
[0051] The resist layer 130 can be patterned by virtually any standard means, including photolithography. In a particular embodiment, the patterning step can include the substeps of exposing a photoresist material with a photomask 131 and developing the exposed photoresist material to open openings 130a in positions aligned with the pads 112. In the embodiment shown in FIG. 2D, the photomask 131 is a dark field mask and the resist material is positive tone, but is not limited thereto.
[0052] The resist layer 130 may have a designed thickness that can provide sufficient height for bump formation. The diameter of the opening 130a may affect the size of the finally obtained bump 120. In one embodiment, the diameter of the opening 130a may be in the range of 5 micrometers to 150 micrometers. Also, the space of the opening 130a may provide a space to accommodate the conductive material to be filled by a subsequent filling step.
[0053] The bump formation process may include filling the openings 130a of the resist layer 130 with conductive particles 132, as shown in FIG. 2E. The conductive particles 132 may include a conductive material different from that of the pads 112. Examples of the conductive particles may include, for example, copper (Cu), nickel (Ni), silver (Ag), gold (Au), etc. In a preferred embodiment, the conductive particles may be copper (Cu) particles. Nanoparticles, microparticles, and mixtures thereof may be used as the conductive particles 132.
[0054] The conductive particles may have a diameter in the range of 1 nm to 15 μm.
[0055] In the described embodiment, the conductive particles are provided in the form of a paste. The filling of the conductive particles (hereinafter also referred to as conductive paste) 132 can be performed by virtually any standard means, including, for example, screen printing and injection techniques. The conductive particles may be immersed in an organic solvent. The viscosity of the conductive paste 132 and the particle fraction in the conductive paste 132 may be determined taking into account the shrinkage of the paste, in other words the thickness of the conductive layer obtained by the sintering in the next step.
[0056] As shown in FIG. 3A, the bump formation process can also include a step of sintering the conductive paste 132. The conductive paste 132 filled in each opening 130a of the resist layer 130 is sintered to form the bump underlayer 122 on each pad 112. The sintering of the conductive paste 132 in the opening 130a is performed by heating the conductive paste 132 in a nitrogen gas or formic acid atmosphere at 100 to 250° C. for 0.1 to 2.0 hours to prevent oxidation of the metal surface after sintering. When the sintering is performed in air, the oxide layer on the metal surface can be removed.
[0057] Sintering is a process of forming a solid mass of material by heat and / or pressure without melting the material to the liquidus point. In the sintering process, the conductive paste 132 shrinks, and as a result, the bump underlayer 122 is formed to cover the sidewall of the opening 130a of the resist layer 130 and the surface of the pad 112 (metal adhesive material 128), as shown in FIG. 3A. As a result, the bump underlayer 122 formed on each pad 112 has a cup shape that fits the contour of the opening 130a, and the bottom is firmly bonded to the pad 112 via the metal adhesive material 128. Since the solder filling is performed in the next step without additional coating of conductive paste, the volumetric shrinkage rate of the conductive paste 132 after sintering is optimized. The volumetric shrinkage rate of the conductive paste 132 depends on the design value of the bump diameter / height, and is, for example, preferably 50% or more.
[0058] The under-bump 122 corresponds to a metal pillar (or post). A space 136b remains above the under-bump 122, reaching the top of the opening 130a. The under-bump 122 has a cone-shaped surface, as shown in Figure 3A. The cross-section of the under-bump 122 has a conformal shape.
[0059] In the described embodiment, the step of filling the conductive paste 132 and the step of sintering the conductive paste 132 are each performed at one time. However, if the thickness of the central part of the under-bump 122 is thinner than the predetermined thickness, for example, in the range of 1 to 50 μm, the conductive paste filling step and the sintering step are alternately performed multiple times to form one or more additional conductive layers to ensure the predetermined thickness of the under-bump 122.
[0060] As shown in FIG. 3B, the bump formation process may also include filling a solder material into the remaining space 130b of each opening 130a above the bump underlayer 122 to form a solder cap 124 on each bump underlayer 122. In a preferred embodiment, the solder material may be filled by injecting molten solder into each opening 130a of the resist layer 130. Injecting the molten solder may be performed, for example, by an IMS process. The presence of the bump underlayer 122 covering the sidewalls of the opening 130a of the resist layer 130 facilitates filling the opening 130a with the solder material. In the IMS process, the molten solder is injected into each opening 130a by using a fill head under vacuum or reduced pressure conditions. The injected molten solder solidifies in each opening 130a. The fill head includes a reservoir of molten solder and a slot into which the molten solder is injected. The solder cap 124 may have a convex top surface.
[0061] As shown in FIG. 3C, the bump formation process may also include stripping the resist layer 130 from the substrate 110, thereby leaving the bumps 120 on the substrate 110.
[0062] 3D, the bump formation process can also include removing the second portion 128b of the metal adhesion material 128 exposed from the bump 120. Removal of the metal adhesion material 128 can be accomplished by any standard means, including wet or dry etching.
[0063] The bump structure 100 of Fig. 3D can be used as an embodiment of the present invention. When the substrate 110 is a wafer, the bump structure 100 may be used for flip-chip bonding after the substrate 110 is divided into multiple chips.
[0064] This bump formation process can produce a bump structure including a set of bumps 120 on a substrate 110, and the bumps 120 produced by sintering the conductive paste 132 are firmly bonded to the pads 112 of the substrate 110 even if the pads 112 are made of a conductive material (Al in this embodiment) different from the conductive particles for sintering (Cu in this embodiment). Generally, a semiconductor device includes an Al pad in the outermost layer. Therefore, it is possible to produce a practical sintered bump base 122 firmly bonded to the pads 112.
[0065] Furthermore, since the bump base 122 is fabricated by sintering the conductive particles 132 and the solder cap 124 is fabricated by injecting molten solder, electrolytic plating and electroless plating processes are not required to fabricate the main structure of the bump, thereby avoiding expensive pillar and solder cap fabrication processes, expensive equipment, and complex management of the plating process.
[0066] In the above-described embodiment, the removal of excess metal adhesive material is performed after resist stripping, however, in other embodiments, the removal of metal adhesive material may be omitted.
[0067] In the following, an improved bump formation process according to another embodiment of the invention in which removal of the metal adhesive material is omitted will be described with reference to the sequence of Figures 4A-4D and 5A-5D, which show cross-sectional views of the resulting structure at each step of the improved bump formation process.
[0068] 4A, the bump formation process can include providing a substrate 110 having a set of pads 112 and a passivation layer 114 formed thereon. As shown in FIG. 2B, the bump formation process can also include applying a resist layer 130 onto a surface 110a of the substrate 110.
[0069] 2C, the bump formation process may further include patterning the resist layer 130 to have a set of openings 130a aligned with the respective pads 112. The openings 130a expose the surfaces of the pads 112. The photoresist material is exposed using a photomask 131 and developed to open the openings 130a in the locations aligned with the pads 112. If the pads 112 are formed of an easily oxidized metal such as Al, the bump formation process may also include removing surface oxide from the pads 112.
[0070] 4D, the bump formation process can include depositing a metal adhesion material 128 over the surface of the pad 112 and the top surface of the resist layer 130. The metal adhesion material 128 is deposited to conform to the contours of the resist layer 130. In this embodiment, the metal adhesion material is selected from the group consisting of Cu, Ni, Au, and combinations thereof. In a particular embodiment, the metal adhesion layer 126 is a layer or stack of Cu, Au, or Ni, or combinations thereof.
[0071] If the pads 112 are made of an easily and persistently oxidized metal such as Al, then a combination of back sputtering and sputtering of a metal adhesive material is preferably employed, similar to the embodiment described above.
[0072] The bump formation process may include filling the openings 130a of the resist layer 130 with a conductive paste 132, as shown in FIG. 5A. The bump formation process may include sintering the conductive paste 132, as shown in FIG. 5B. The conductive paste 132 filled in the openings 130a is sintered to form the bump underlayer 122 on the pad 112. In the sintering process, the conductive paste 132 shrinks, and as a result, the bump underlayer 122 is formed to cover the sidewalls of the openings 130a and the surface of the pad 112, as shown in FIG. 5B, and both surfaces are covered with the metal adhesive material 128.
[0073] As shown in FIG. 5C, the bump formation process may include filling the remaining space 130b of each opening 130a on the bump underlayer 122 with a solder material. In the described embodiment, molten solder is injected into each opening 130a of the resist layer 130 to form a solder cap 124 on each bump underlayer 122. The injection of the molten solder may be performed, for example, by an IMS process. In the present embodiment, during the IMS process, the metal adhesion material 128 deposited on the top surface of the resist layer 130 dissolves in the molten solder because the metal adhesion material 128 does not contain a metal that is insoluble in the molten solder, such as Ti. A portion of the metal adhesion material 128 deposited on the sidewall of the opening 130a of the resist layer 130 (referred to as sidewall metal 129) may remain after the IMS process. In the present embodiment, the sidewall metal 129 surrounds the bump underlayer 122 and covers the side of the bump underlayer 122. The sidewall metal 129 can function as a sidewall barrier (eg, Ni) to prevent short circuits between the bumps due to ion migration.
[0074] As shown in Figure 5D, the bump formation process may also include stripping the resist layer 130 from the substrate 110, thereby leaving the bump 120 on the substrate 110. The step of removing the metal adhesion material 128 performed in the process shown in Figures 2A-2E and 3A-3D is omitted.
[0075] It should be noted that the stripping step may be omitted if a non-stripping type resist is used to form the resist layer 130. Thus, the structure shown in FIG. 5C can also be used in a subsequent flip-chip bonding process without removing the resist layer 130.
[0076] In the embodiment shown in FIG. 2A-FIG. 2E and FIG. 3A-FIG. 3D, since the removal of the metal adhesive material is introduced, there is an advantage that other functional materials such as Ti barriers can be used as the metal adhesive material even if the material is insoluble in the solder material such as molten solder. On the other hand, in the embodiment shown in FIG. 4A-FIG. 4D and FIG. 5A-FIG. 5D, if a material insoluble in the molten solder such as Ti is not used, it is possible to omit the removal of the metal adhesive material while sufficiently removing the excess metal adhesive material. Since the removal process of the metal layer under the resist layer after the resist peeling is eliminated, the undercut of the base of the bump is preferably prevented. In addition, the associated process cost can be reduced. Cu, Ni and Au are easily dissolved in the solder material such as molten solder during the filling process of the solder material.
[0077] In the following, an alternative bump formation process according to yet another embodiment of the invention will be described with reference to the sequence of Figures 6A-6C, which show cross-sectional views of the resulting structure at each step of the alternative bump formation process.
[0078] It should be noted that this bump formation process also includes the steps described in Figures 4A-4D and 5A, as in the above-described embodiment, and therefore the description will be given after the steps in Figure 5A are completed.
[0079] As shown in Fig. 6A, the bump formation process can include sintering the conductive paste 132. As shown in Fig. 6B, the bump formation process can include filling the remaining space 130b of each opening 130a above the bump underlayer 122 with a solder material to form a solder cap 124 on each bump underlayer 122. In this embodiment, the metal adhesion material 128 deposited on the top surface of the resist layer 130 remains even after the IMS process.
[0080] 6C, the bump formation process can include a step of stripping the resist layer 130 from the substrate 110. In this step, the metal adhesion material on the top surface of the resist layer 130 is lifted off and washed away together with the underlying resist layer 130 when the resist layer 130 is washed away. A separate step of removing the metal adhesion material 128 is omitted. In this embodiment, the metal adhesion material 128 is selected from the group consisting of Cu, Ti, Ni, Au, and combinations thereof.
[0081] In the embodiment shown in Figures 4A-4D, 5A and 6A-6C, the removal of the metal adhesive material can be omitted, regardless of the composition of the metal adhesive material, similar to the embodiment shown in Figures 4A-4D and 5A-5D. Therefore, undercutting of the base of the bump is preferably prevented. Also, the associated process cost can be reduced. Therefore, other functional materials such as Ti barrier can be used as the metal adhesive material. Furthermore, in this embodiment, the metal adhesive material that conforms to the contour of the mold layer can function as a sidewall barrier to prevent short circuits between the bumps due to ion migration.
[0082] Yet another alternative bump formation process according to another embodiment of the invention will now be described with reference to the sequence of Figures 7A-7D, which show cross-sectional views of the resulting structure at each step of the bump formation process.
[0083] It should be noted that the bump formation process also includes the steps described in Figures 4A-4D and 5A, as in the above-described embodiment, and therefore the description will be given after the steps in Figure 5A are completed.
[0084] As shown in Figure 7A, the bump formation process can include sintering the conductive paste 132 to form a bump undercoat 122 on each pad 112, similar to the above-described embodiment. As shown in Figure 7B, the bump formation process can include removing the metal adhesion material 128 deposited on the top surface of the resist layer 130. The removal of the metal adhesion material 128 can be performed by a technique selected from the group consisting of chemical mechanical polishing (CMP), mechanical polishing, fly-cutting, and chemical etching.
[0085] As shown in Figure 7C, the bump formation process may include filling the remaining space 130b in each opening 130a with a solder material to form a solder cap 124 on each under-bump 122. As shown in Figure 7D, the bump formation process may also include stripping the resist layer 130 from the substrate 110. In this embodiment, the metal adhesion material 128 is selected from the group consisting of Cu, Ti, Ni, Au, and combinations thereof.
[0086] In the embodiment shown in Figures 4A-4D, 5A and 7A-7D, even if the process of removing excess metal adhesive material is performed before resist stripping, the process of removing the metal layer after resist stripping, which causes undercuts at the base of the bumps, is eliminated. Other functional materials such as Ti barriers can also be used as metal adhesive materials. Furthermore, in this embodiment, the metal adhesive material that conforms to the contours of the mold layer can function as a sidewall barrier to prevent short circuits between the bumps due to ion migration.
[0087] In the following, an electronic device and a flip-chip bonding process for manufacturing the same according to an exemplary embodiment of the present invention will be described with reference to Figures 8A and 8B, which show cross-sectional views of the structure obtained at each step of the flip-chip bonding process.
[0088] 8A, the flip chip process may include providing a bumped semiconductor chip 310 including a set of bumps 320 formed on an active surface. The flip chip process may also include providing an organic substrate 350 including a set of contact pads 352 and a solder resist layer 354 formed on a surface of the organic substrate 350. The flip chip process may also include applying an underfill 356 onto the surface of the organic substrate 350.
[0089] The bumped semiconductor chip 310 prepared in this step is fabricated by any of the bump formation processes described above, followed by a dicing process if the bump formation process is performed at the wafer level. As already described with reference to Figures 1A and 1B, each bump 320 has a metal adhesion layer 326 formed on a pad 312, a bump underlayer 322 formed on the pad 312 via the metal adhesion layer 326, and a solder cap 324 formed on the bump underlayer 322.
[0090] 8B, the flip-chip process can include mounting the bumped semiconductor chip 310 on an organic substrate 350 such that the bumps 320 on the chip side are in contact with the contact pads 352 on the substrate side, respectively. The semiconductor chip 310 is flipped over so that its active side faces down and is positioned such that the bumps 320 are aligned with the respective pads 352 on the organic substrate 350.
[0091] 8B, the flip chip process may further include bonding the bumps 320 to the pads 352 to obtain flip chip joints 360. Depending on the desired size and pitch of the joints, either a mount reflow method or a thermocompression method may be used as appropriate. The flip chip process may also include curing the underfill 356 to firmly secure the semiconductor chip 310 to the organic substrate 350.
[0092] By performing the steps of mounting the bumped semiconductor chip 310 and bonding the bumps 320 to the pads 352, the bumped semiconductor chip 310 is interconnected to an organic substrate 350 that contains external circuitry.
[0093] Electronic devices manufactured by the above-described flip chip bonding process exhibit good durability because the bumps 320 made by sintering the conductive particles are firmly bonded to the pads 312, even if the pads 312 are made of a conductive material different from the conductive particles for the bumps.
[0094] Various related bump formation processes will now be described with reference to the series of Figures 9A-9E, 10A-10E, 11A-11D, 12A-12D and 13A-13C.
[0095] 9A-9E show cross-sectional views of the resulting structure at each step of the associated bump formation process, including electroplating of both the pillars and the solder cap.
[0096] As shown in FIG. 9A, a seed layer 516, such as a Ti / Cu layer, is formed on the surface of the prepared wafer 510. As shown in FIG. 9B, a resist mask 530 having a set of holes 530a is patterned on the wafer 510. As shown in FIG. 9C, Cu is electroplated on the seed layer 516 in the holes 530a to form Cu pillars partway through the holes 530a. As also shown in FIG. 9C, a solder layer 524 is deposited on the Cu pillars 522 by electroplating a solder material onto the upper limit of the holes 530b in the resist mask 530. As shown in FIG. 9D, the resist mask 530 is stripped from the wafer 510 and the seed layer 516 is etched. The solder layer 524 is then reflowed with flux to form solder-capped bumps 520 on the wafer 810, as shown in FIG. 9E.
[0097] However, in the related bump formation process shown in Figures 9A-9E, although Cu pillar bumps can be fabricated, it is difficult to adjust the composition of electroplated solder with a high degree of freedom. Only pure Sn or binary solder compositions are known to be stably fabricated by electroplating. In addition, both the pillar and the solder cap require expensive electroplating, expensive equipment and complex management of the plating process. In addition, removing the seed layer 516 after resist stripping will cause an undercut at the base of the bump 520.
[0098] 10A-10E show cross-sectional views of the resulting structure at each step of another related bump formation process including electroplating of the pillars and IMS of the solder cap.
[0099] As shown in FIG. 10A, a seed layer 616, such as a Ti / Cu layer, is formed on the surface of the wafer 610. As shown in FIG. 10B, a resist mask 630 having a set of holes 630a is patterned on the wafer 610. As shown in FIG. 10C, Cu is electrolytically plated on the seed layer 616 in the holes 630a to form Cu pillars halfway through the holes 630a. As shown in FIG. 10D, a solder material is filled into the remaining spaces of the holes 630a in the resist mask 630 by an IMS process to form solder caps 624 on the Cu pillars 622. As shown in FIG. 10E, the resist mask 630 is stripped from the wafer 610, and the seed layer 616 is etched.
[0100] 10A-10E, the electroplating of expensive solder material can be omitted, but it still requires expensive electroplating of Cu pillars, expensive equipment, and complex management of the plating process. Also, removing the seed layer 616 after resist stripping causes an undercut at the base of the bump 620.
[0101] 11A-11D show cross-sectional views of the resulting structures at various steps of yet another related bump formation process, including electroless plating of the pillars and IMS of the solder caps.
[0102] As shown in FIG. 11A, a resist mask 730 with a set of holes 730a is patterned on a wafer 710 including a set of pads 712 and a passivation layer 714. As shown in FIG. 11B, Ni is deposited on the pads 712 in the holes 730a by electroless plating to form Ni pillars 722 partway through the holes 730a, and an Au metal layer 728 is deposited on the Ni pillars 722. As shown in FIG. 11C, a solder material is filled into the remaining spaces of the holes 730a in the resist mask 730 by an IMS process to form solder caps 724 on the Ni pillars 722. As shown in FIG. 11D, the resist mask 730 is stripped from the wafer 710, leaving a set of Ni pillar bumps 720 including the Ni pillars 722 and the solder caps 724 on the wafer 710.
[0103] Although the removal of the seed layer after resist stripping can be omitted, it requires expensive electroless plating of Ni pillars, expensive equipment, and complicated management of the plating process.
[0104] 12A-12D and 13A-13C show cross-sectional views of the structures obtained at different steps of a related bump formation process based on conductive paste sintering without a metal adhesion layer.
[0105] As shown in Figure 12A, in a related bump formation process, a wafer 810 is provided, which includes a set of pads 812 and a passivation layer 814. As shown in Figure 12B, a resist mask 830 is formed on the surface of the wafer 810. As shown in Figure 12C, the resist mask 830 is patterned using a photomask 831 to have a set of holes 830a. Each hole 830a is aligned with a corresponding one of the pads 812.
[0106] As shown in FIG. 12D, the Cu paste 832 is filled into the holes 830a of the resist mask 830 up to the upper limit of the holes 830a. As shown in FIG. 13A, the Cu paste 832 filled into the holes 830a is cured to form the cup-shaped pillars 822 as sintered bodies of Cu particles. It should be noted that the present process does not require a seed layer, which is required for electrolytic plating of copper, since the sintering process is used to fabricate the copper pillars. Rather, such unnecessary steps, including the deposition of the seed layer and the removal of the seed layer after resist stripping, can be avoided from the viewpoint of cost. Moreover, the removal of the seed layer after resist stripping may cause undercuts at the base of the bumps.
[0107] Then, as shown in Fig. 13B, the remaining spaces of the holes 830a of the resist mask 830 above the cup-shaped pillars 822 are filled with solder material by an IMS process to form solder caps 824 on the cup-shaped pillars 822. As shown in Fig. 13C, the resist mask 830 is stripped from the wafer 810, leaving a set of Cu pillar bumps 820 on the wafer 810, each of which includes a cup-shaped pillar 822 and a solder cap 824.
[0108] The bump formation process shown in FIGS. 12A-12E and 13A-13C can avoid expensive plating of both Cu pillars and solder caps, expensive equipment, and complicated management of the plating process.
[0109] However, this process is limited to the case where the pad 812 and the pillar 822 are made of the same material, especially copper. After thorough research, the inventors have found that it is difficult to bond a sintered body of conductive paste to a pad made of a conductive material different from the conductive paste, for example, bonding sintered copper to an Al pad, under atmospheric pressure, even immediately after removing the native oxide film by reverse sputtering. It is expected that the high temperature condition of sintering contributes to strengthening the bond between the sintered pillar and the pad. However, semiconductor devices generally deteriorate under high temperature conditions, such as >300°C, which exceeds the temperature of a typical reflow process.
[0110] In contrast to the above-mentioned related bump formation process shown in Figures 12A-12D and 13A-13C, the technique according to one or more embodiments of the present invention allows for strengthening the bond between the bump underlayer and the pad without using high temperature conditions. The metal adhesion layer or UBM layer created between the pad 112 and the conductive paste 132 (or the sintered bump underlayer 122) maintains good bonding even when a conductive material different from the conductive particles is used as the pad material. Therefore, the degradation of the semiconductor device caused by the bump formation process can be prevented.
[0111] Additionally, in contrast to the related bump formation processes shown in Figures 9A-9E, 10A-10E, and 11A-11D described above, the bump formation process according to one or more embodiments of the present invention eliminates the need for expensive electroplating of both the bump substrate and the solder cap, as well as complex management of the plating process, thereby reducing the manufacturing costs of the bump.
[0112] As described above, in accordance with one or more embodiments of the present invention, a novel bump formation technique is provided that can produce a bump structure that includes a set of bumps formed on a substrate, where the bumps, made by sintering conductive particles, are firmly bonded to pads made from a conductive material different from the conductive particles.
[0113] The terms used herein are for the purpose of describing particular embodiments only and are not intended to limit the present invention. As used herein, the singular forms "a", "an" and "the" are intended to include the plural forms as well, unless the context clearly indicates otherwise. It will be further understood that the terms "comprises" and / or "comprising" as used herein specify the presence of stated features, steps, layers, elements, or components, or combinations thereof, but do not preclude the presence or addition of one or more features, steps, layers, elements, components, or groups thereof, or combinations thereof.
[0114] Corresponding structure, materials, acts, and equivalents of all means or steps in the following claims as well as functional elements are intended to include any structure, material, or acts for performing a function in combination with other claimed elements as specifically claimed, if any. The description of one or more aspects of the present invention has been presented for purposes of illustration and description, but is not intended to be exhaustive or limited to the invention in the form disclosed.
[0115] Many modifications and variations will be apparent to those skilled in the art without departing from the scope of the described embodiments. The terms used herein have been selected to best explain the principles of the embodiments, practical applications or technical improvements to technology found in the market, or to enable those skilled in the art to understand the embodiments disclosed herein.
Claims
1. 1. A method of making a bump structure, comprising: providing a substrate including a set of pads formed on a surface thereof, the pads comprising a first conductive material; coating a metallic adhesion layer on each of said pads; forming a bump on each of the pads by sintering conductive particles with a mold layer, the conductive particles comprising a second conductive material different from the first conductive material; A method comprising:
2. the molding layer having a set of openings each aligned with one of the pads and forming the bumps on each of the pads; disposing the mold layer on the substrate; filling conductive particles into the openings of the mold layer and sintering the conductive particles filled into the openings of the mold layer to provide a bump underlayer on each of the pads; filling a solder material into a remaining space in each of the openings in the mold layer above the under-bumps to form a solder cap on each under-bump; The method of claim 1 , comprising:
3. The method of claim 1 , wherein the first conductive material comprises Al and the second conductive material comprises Cu.
4. 3. The method of claim 2, wherein the conductive particles are provided in the form of a paste, and the under-bump formed on each of the pads has a cup shape that matches the contour of the opening in the mold layer and a bottom that is joined to the pad by the metal adhesion layer.
5. applying a resist layer onto the surface of the substrate; patterning the resist layer to form the mold layer; depositing a metallic adhesion material onto the pads and the mold layer so as to conform to a contour of the mold layer to provide the metallic adhesion layer coated on each of the pads; The method of claim 2 , further comprising:
6. Filling the solder material includes: dissolving a metallic adhesive material deposited on the top surface of the mold layer into a solder material; The method of claim 5 , comprising:
7. The method of claim 6 , wherein the metallic adhesive material is selected from the group consisting of Cu, Ni, Au and any combination thereof.
8. peeling the mold layer from the substrate and washing off the mold layer, lifting off and washing off the metallic adhesive material on the top surface of the mold layer along with the mold layer; The method of claim 5 further comprising:
9. removing the metallic adhesion material deposited on the top surface of the mold layer by a technique selected from the group consisting of chemical mechanical polishing (CMP), mechanical polishing, fly-cutting, and chemical etching; The method of claim 5 further comprising:
10. depositing a metallic adhesion material over the surface of the substrate to have a first portion corresponding to the metallic adhesion layer coated on each of the pads and a second portion formed in an outer region of the pads; applying a resist layer onto the metal adhesive material; patterning the resist layer to form the mold layer; peeling the mold layer from the substrate, thereby leaving the bumps on the substrate, each including the solder cap and the under-bump formed on the pad; removing the second portion of the metallic adhesive material exposed from the bump; The method of claim 2 , further comprising:
11. The method of claim 10, wherein the metallic adhesive material is selected from the group consisting of Cu, Ti, Ni, Au and any combination thereof.
12. Filling the solder material includes: injecting molten solder into each of the openings in the mold layer; The method of claim 2 , comprising:
13. 2. The method of claim 1, further comprising removing surface oxides from said pads by reverse sputtering prior to coating of said metallic adhesion layer, said metallic adhesion layer being coated onto each of said pads by sputtering.
14. the substrate includes a semiconductor device, the set of pads being formed on at least an active surface of the semiconductor device, and the method further comprising: and further comprising interconnecting the semiconductor device with an external circuit using the bumps, the method being a method for manufacturing an electronic device. The method of claim 1.
15. A bump structure, a substrate including a set of pads formed on a surface thereof, the pads including a first conductive material; a set of bumps, each of the bumps formed on one of the pads, each of the bumps including a metal adhesion layer formed on the pad and a bump undercoat formed on the metal adhesion layer, the bump undercoat being a sintered body of conductive particles including a second conductive material different from the first conductive material; A bump structure comprising:
16. 16. The bump structure of claim 15, wherein each of the bumps further includes a solder cap formed on the bump underlayer, the bump underlayer having a shape of a cup having a bottom joined to the pad via the metal adhesion layer, the cup being filled with the solder material of the solder cap.
17. The bump structure of claim 15 , wherein the metal adhesion layer covers the sides of the under-bump as a sidewall barrier.
18. 16. The bump structure of claim 15, wherein the first conductive material comprises Al, the second conductive material comprises Cu, and the metal adhesion layer comprises a material selected from the group consisting of Cu, Ti, Ni, Au, and combinations thereof.
19. 19. An electronic device comprising: a semiconductor device having a bump structure according to claim 15; and a circuit interconnected to the substrate via the set of bumps.
20. 20. The electronic device of claim 19, wherein each of the bumps further includes a solder joint connecting a respective bump substrate to a terminal contact of the circuit, the bump substrate having a shape of a cup having a bottom bonded to the pad via the metal adhesion layer, the cup being filled with a solder material of the solder cap.
21. 1. A method of manufacturing an electronic device, comprising: preparing a bumped semiconductor device, said preparing said bumped semiconductor device comprising a method for fabricating a bump structure according to any one of claims 1 to 14; interconnecting the bumped semiconductor device to an external circuit via the set of bumps; A method comprising:
Citation Information
Patent Citations
Semiconductor device and method for manufacturing the same
JP2010045234A
Semiconductor device and method of manufacturing the same
JP2011071175A
Pillar forming past, manufacturing method of pillar, manufacturing method of bump structure, pillar and bump structure
JP2016115846A
Method of forming metal pillar
US20120178251A1
Contact and solder ball interconnect
US20150311170A1