Solar cell, photovoltaic module, and method for manufacturing photovoltaic module
The solar cell design with widened grid lines and adhesive dots on the first surface addresses the low yield issue in photovoltaic modules by improving welding tensile force and efficiency, reducing defects, and enhancing module reliability.
Patent Information
- Application Number
- JP2023100460
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-05-23
- Filing Date
- 2023-06-20
- Publication Date
- 2024-12-05
- Estimated Expiration
- 2043-06-20
AI Technical Summary
Conventional photovoltaic modules have low yield due to issues such as welding defects and fragmentation during the welding process of PV ribbons, which are exacerbated by the high melting point of solder and large warping deformation of solar cells.
The solar cell design incorporates first and second grid lines with widened portions on opposite surfaces, enhancing the welding tensile force and efficiency by increasing the surface welding area and reducing the covered area on the first surface, while the PV ribbon is connected to these widened portions and secured with adhesive dots on the first surface.
This design improves the welding effect and yield of photovoltaic modules by increasing the welding tensile force and reducing the risk of defects, thereby enhancing the overall efficiency and reliability of the solar cells.
Smart Images

Figure 2024169256000001_ABST
Abstract
Description
[Technical field]
[0001] FIELD OF THE DISCLOSURE Embodiments of the present invention relate to the field of photovoltaics, and more particularly to solar cells, photovoltaic modules and methods of manufacture thereof. [Background technology]
[0002] A solar cell is a device that converts light energy directly into electrical energy through photoelectric or photochemical effects. A single cell cannot generate electricity directly. It can only be used after multiple cells are connected in series or parallel by PV ribbons and packaged strictly as a module. A solar cell module (also called a solar panel) is the core of a photovoltaic power generation system and is also the most important part of the system. The role of a solar cell module is to convert solar energy into electrical energy, send it to a battery for storage, and drive the operation of the equipment.
[0003] The cells are very fragile, and in order to protect the battery cells, it is generally necessary to install adhesive films and cover plates on the upper and lower surfaces of the battery module. The cover plate is generally photovoltaic glass, which cannot be directly attached to the upper surface of the battery cell, and the adhesive film needs to play an adhesive role in it. The connection between the battery cells usually requires PV ribbons to collect current, and ordinary PV ribbons require alloying between the PV ribbon and the thin grid by welding during welding. However, the melting point of the solder in the PV ribbon is generally high, and in the actual welding process, the welding temperature is more than 20°C higher than the melting point of the solder. The battery cell has a large warp deformation during welding, so there is a high risk of hidden cracks after welding and a high rate of fragmentation. Under the above background, low-temperature PV ribbon and main gridless technology have been born to improve the welding quality, but there are still many factors that affect the yield of the module, such as the welding effect and welding yield between the PV ribbon and the thin grid. Summary of the Invention [Problem to be solved by the invention]
[0004] In the embodiments of the present application, a solar cell, a photovoltaic module, and a manufacturing method thereof are provided, which are advantageous in improving at least the yield of photovoltaic modules. [Means for solving the problem]
[0005] According to some embodiments of the present application, in one aspect of the embodiment of the present application, a solar cell is provided, the solar cell including: a substrate having a first surface and a second surface opposite to each other; a plurality of first grid lines sequentially arranged along a first direction, the first grid lines being located on the first surface of the substrate, wherein at least one first grid line located on an edge of the substrate among the plurality of first grid lines along the first direction has a first widening portion; and a plurality of second grid lines sequentially arranged along the first direction, the second grid lines being located on the second surface of the substrate, wherein at least one second grid line located on an edge of the substrate among the plurality of second grid lines along the first direction has a second widening portion, wherein a dimension of the second widening portion is larger than a dimension of the first widening portion.
[0006] In some embodiments, along the first direction, the first grid line includes two first electrodes located at an edge of the substrate and a plurality of second electrodes located between the two first electrodes, the first electrodes including a first widening portion, the second electrodes including a third widening portion, the third widening portion facing the first widening portion along the first direction, and a dimension of the third widening portion being smaller than a dimension of the first widening portion.
[0007] In some embodiments, along the first direction, the second grid lines include third electrodes arranged at intervals and a plurality of fourth electrodes located between two of the third electrodes, the third electrodes including a second widening portion, the fourth electrode including a fourth widening portion, the fourth widening portion facing the second widening portion along the first direction, and a dimension of the fourth widening portion being smaller than a dimension of the second widening portion.
[0008] In some embodiments, the fourth widened portion has a smaller dimension than the first widened portion.
[0009] In some embodiments, the number of the third electrodes in the same second surface is 2-20.
[0010] In some embodiments, the range of the second width of the second widened portion in the first direction is 0.2 mm to 1.0 mm.
[0011] In some embodiments, the substrate further includes a passivation layer located on a surface of the substrate, the first widened portion and / or the second widened portion are located on a surface of the passivation layer and do not burn through the passivation layer, and the first grid lines further include first sub-grid lines located on either side of the first widened portion, the first sub-grid lines burn through the passivation layer and protrude from the passivation layer.
[0012] In some embodiments, the first grid lines are integrally formed structures and the second grid lines are integrally formed structures.
[0013] According to some embodiments of the present application, in another form of the embodiment of the present application, a photovoltaic module is provided, the photovoltaic module including: a cell string, in which a plurality of solar cells are electrically connected by PV ribbons, the PV ribbons are electrically connected to each first grid line and / or each second grid line, and any of the PV ribbons is in electrical contact with a first widened portion or a second widened portion; an encapsulation layer for covering a surface of the cell string; and a cover plate for covering a surface of the encapsulation layer away from the cell string.
[0014] In some embodiments, there are M first overlapping areas between the same PV ribbon and the plurality of first grid lines, and further includes N adhesive dots, each of which covers the first overlapping area, and the adhesive dots are also located on the first widening portions, where N is smaller than M and equal to or greater than the number of the first widening portions, and the sealing layer is located on the surfaces of the adhesive dots.
[0015] In some embodiments, N is less than or equal to the number of second widening portions.
[0016] In some embodiments, N satisfies 2≦N≦20.
[0017] In some embodiments, the encapsulation layer is located on a surface of the second grid lines, the PV ribbons corresponding to the second surface are in direct contact with the encapsulation layer, and the second surface is free of the adhesive dots.
[0018] According to some embodiments of the present application, in another form of the embodiment of the present application, a method for manufacturing a photovoltaic module is provided, the method for manufacturing the photovoltaic module includes: providing a plurality of battery cells and a PV ribbon; performing a welding process on the PV ribbon and the battery cells so that an alloy layer is formed between the PV ribbon and a first grid line and between the PV ribbon and a second grid line, the battery cells and the PV ribbon after the welding process constitute a cell string; providing a sealing layer and a cover plate, the sealing layer is used to cover a surface of the cell string and the cover plate is used to cover a surface of the sealing layer away from the cell string; and performing a lamination process on the cell string, the sealing layer and the cover plate.
[0019] In some embodiments, there are M first overlapping areas between the same PV ribbon and the first grid line, and after performing the welding process, the method further includes applying adhesive to a portion of the first overlapping area of the battery cell to have N adhesive dots on a surface of the battery cell, each of the adhesive dots covering the first overlapping area, and the adhesive dots are also located in a first widening portion, where N is less than M and greater than or equal to the number of the first widening portions. Effect of the Invention
[0020] The technical solutions provided in the embodiments of the present application have at least the following advantages:
[0021] In the technical solution provided in the embodiment of the present application, the substrate has a first surface and a second surface facing each other, the first grid line located on the first surface has a first widening portion, and the second grid line located on the second surface has a second widening portion, so that the first widening portion and the second widening portion can increase the welding tensile force between the first grid line and the PV ribbon and the welding tensile force between the second grid line and the PV ribbon, and thus improve the welding effect between the first grid line and the PV ribbon and the welding effect between the second grid line and the PV ribbon. The dimension of the first widening portion is larger than that of the second widening portion, and the dimension of the first widening portion on the first surface and the dimension of the second widening portion on the second surface are changed, i.e., the dimension of the first widening portion on the first surface is ensured to be small, so that the coverage area of the first surface can be reduced, and the cell efficiency of the solar cell can be improved. The second widening portions of the second surface are located at least at the end of the substrate, i.e., the number of the second widening portions is equal to or greater than the number of the first widening portions. By increasing the number of the second widening portions, the welding area of the second surface can be increased, and the welding tensile force between the battery and the PV ribbon can be increased. [Brief description of the drawings]
[0022] One or more embodiments are illustratively described in the figures in the corresponding attached drawings, but these illustrative descriptions are not intended to limit the embodiments, and unless otherwise specified, the figures in the attached drawings do not form a proportional limit. In order to more clearly describe the embodiments of the present application or the technical solutions in the prior art, the following will briefly describe the drawings necessary for the embodiments. Obviously, the drawings in the following description are only some embodiments of the present disclosure, and those skilled in the art can also obtain other drawings based on these drawings without paying creative labor. [Figure 1] FIG. 1 is a diagram showing a first configuration of a first surface of a solar cell according to an embodiment of the present application. [Diagram 2] FIG. 2 is a diagram showing a first type sectional configuration along the A1-A2 section of FIG. [Diagram 3] FIG. 3 is a diagram showing a second type sectional configuration along the A1-A2 section of FIG. [Figure 4] FIG. 4 is a diagram showing a first type sectional configuration along the B1-B2 cross section of FIG. [Diagram 5] FIG. 5 is a diagram showing a local configuration of a first widened portion of a solar cell according to an embodiment of the present application. [Figure 6] FIG. 6 is a diagram showing a first configuration of a second surface of a solar cell according to an embodiment of the present application. [Figure 7] FIG. 7 is a diagram showing a local configuration of a second widened portion of a solar cell according to an embodiment of the present application. [Figure 8] FIG. 8 is a diagram showing a second configuration of the first surface of a solar cell according to an embodiment of the present application. [Figure 9] FIG. 9 is a diagram showing a local configuration of a third widened portion of a solar cell according to an embodiment of the present application. [Figure 10] FIG. 10 is a diagram showing a second configuration of the second surface of the solar cell according to an embodiment of the present application. [Figure 11] FIG. 11 is a diagram showing a local configuration of a fourth widened portion of a solar cell according to an embodiment of the present application. [Figure 12] FIG. 12 is a diagram showing a third configuration of the first surface of a solar cell according to an embodiment of the present application. [Figure 13]FIG. 13 is a diagram showing a configuration in which a PV ribbon is formed on a first surface of a photovoltaic module according to an embodiment of the present application. [Figure 14] FIG. 14 is a diagram showing a configuration in which a PV ribbon is formed on the second surface of a photovoltaic module according to an embodiment of the present application. [Figure 15] FIG. 15 is a diagram showing a configuration in which adhesive dots are formed on a first surface of a photovoltaic module according to an embodiment of the present application. [Figure 16] FIG. 16 is a diagram showing the configuration of a photovoltaic module according to an embodiment of the present application. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0023] As can be seen from the background art, the yield of conventional photovoltaic modules is not high.
[0024] In the solar cell according to the embodiment of the present application, the substrate has a first surface and a second surface facing each other, and the first grid line located on the first surface has a first widening portion, and the second grid line located on the second surface has a second widening portion, so that the first widening portion and the second widening portion can increase the welding tensile force between the first grid line and the PV ribbon and the welding tensile force between the second grid line and the PV ribbon, and thus improve the welding effect between the first grid line and the PV ribbon and the welding effect between the second grid line and the PV ribbon. The size of the first widening portion is larger than the size of the second widening portion, and the size of the first widening portion on the first surface and the size of the second widening portion on the second surface are changed, i.e., the size of the first widening portion on the first surface is ensured to be small, so that the coverage area of the first surface is reduced, and the cell efficiency of the solar cell can be improved. The second widening portions of the second surface are located at least at the end of the substrate, i.e., the number of the second widening portions is equal to or greater than the number of the first widening portions. By increasing the number of the second widening portions, the welding area of the second surface can be increased, and the welding tensile force between the battery and the PV ribbon can be increased.
[0025] Hereinafter, each embodiment of the present application will be described in detail with reference to the drawings. However, as will be understood by those skilled in the art, many technical details are proposed in each embodiment of the present application in order to allow the reader to understand the present application better, but the technical solution claimed for protection by the present application can be realized without these technical details and various changes and modifications based on the following embodiments.
[0026] FIG. 1 is a diagram showing a first type configuration of a first surface of a solar cell according to an embodiment of the present application. FIG. 2 is a diagram showing a first type cross-sectional configuration along the A1-A2 section of FIG. 1. FIG. 3 is a diagram showing a second type cross-sectional configuration along the A1-A2 section of FIG. 1. FIG. 4 is a diagram showing a first type cross-sectional configuration along the B1-B2 section of FIG. 1. FIG. 5 is a diagram showing a local configuration of a first widening portion of a solar cell according to an embodiment of the present application. FIG. 6 is a diagram showing a first type configuration of a second surface of a solar cell according to an embodiment of the present application. FIG. 7 is a diagram showing a local configuration of a second widening portion of a solar cell according to an embodiment of the present application. FIG. 8 is a diagram showing a second type configuration of a first surface of a solar cell according to an embodiment of the present application. FIG. 9 is a diagram showing a local configuration of a third widening portion of a solar cell according to an embodiment of the present application. FIG. 10 is a diagram showing a second type configuration of a second surface of a solar cell according to an embodiment of the present application. FIG. 11 is a diagram showing a local configuration of a fourth widening portion of a solar cell according to an embodiment of the present application. FIG. 12 is a diagram showing a third type configuration of a first surface of a solar cell according to an embodiment of the present application. Here, in order to explain the relative positional relationship between the first widening portion and the PV ribbon, the PV ribbon is also shown in Figures 2 and 3. Note that in order to show the regions of the first widening portion and the second widening portion, the second widening portion is shown in the region surrounded by the dotted line in Figure 12.
[0027] As can be understood, the cross-sectional view between the second widening portion and the second grid line on the second surface can be seen by reference to the positional relationship between the first widening portion and the first grid line in Figures 2 to 4, and here the cross-sectional view of the second surface is not shown, only the cross-sectional view of the first surface side is shown.
[0028] As shown in FIGS. 1 to 12 , according to some embodiments of the present application, a solar cell is provided, the solar cell including: a substrate 100 having a first surface 11 and a second surface 12 opposite to each other; a plurality of first grid lines 21 sequentially arranged along a first direction Y, the first grid lines 21 being located on the first surface 11 of the substrate 100, where at least one of the first grid lines 21 located on an end of the substrate 100 along the first direction Y has a first widening portion 111; and a plurality of second grid lines 22 sequentially arranged along the first direction Y, the second grid lines 22 being located on the second surface 12 of the substrate 100, where at least one of the second grid lines 22 located on an end of the substrate along the first direction Y has a second widening portion, where a dimension of the second widening portion 211 is larger than a dimension of the first widening portion 111.
[0029] The solar cell may be any of the following: a regular TOPCON (Tunnel Oxide Passivated Contact) cell, a PERC (Passivated emitter and real cell), a heterojunction cell, etc. In some embodiments, the solar cell may be a compound cell, where the compound includes, but is not limited to, materials such as silicon germanium, silicon carbide, gallium arsenide, indium gallide, perovskite, cadmium telluride, copper indium selenide, etc.
[0030] The solar cell includes a substrate and a passivation layer, which are stacked in sequence. The material of the substrate 100 may be an elemental semiconductor material. Specifically, the elemental semiconductor material is made of a single element, for example, silicon. Here, the elemental semiconductor material may be in a single crystalline state, a polycrystalline state, an amorphous state, or a microcrystalline state (a state having both a single crystalline state and an amorphous state is called a microcrystalline state), for example, the silicon may be at least one of single crystalline silicon, polycrystalline silicon, amorphous silicon, or microcrystalline silicon.
[0031] In some embodiments, the material of the substrate 100 may be a compound semiconductor material. Common compound semiconductor materials include, but are not limited to, materials such as silicon germanium, silicon carbide, gallium arsenide, indium gallide, perovskites, cadmium telluride, copper indium selenide, etc. The substrate 100 may be a sapphire substrate, a silicon-on-insulator substrate, or a germanium-on-insulator substrate.
[0032] In some embodiments, the substrate 100 may be an N-type semiconductor substrate or a P-type semiconductor substrate. In an N-type semiconductor substrate, an N-type doping element is doped, which may be any of the group V elements, such as phosphorus (P), bismuth (Bi), antimony (Sb), or arsenic (As). In a P-type semiconductor substrate, an P-type doping element is doped, which may be any of the group III elements, such as boron (B), aluminum (Al), gallium (Ga), or indium (In).
[0033] In some embodiments, the solar cell further includes a passivation layer 101 located on the surface of the substrate 100. The material of the passivation layer 101 includes any one or more of the following materials: silicon oxide, silicon nitride, silicon oxynitride, silicon oxycarbonitride, titanium oxide, hafnium oxide, or aluminum oxide.
[0034] The solar cell includes an emitter and a first passivation layer located on a first surface 11 of the substrate 100, and a second passivation layer located on a second surface 12 of the substrate 100, with first grid lines 21 penetrating the first passivation layer to make electrical contact with the emitter and second grid lines 22 penetrating the thickness of the second passivation layer to make electrical contact with the second surface 12. The passivation layer 101 includes a first passivation layer and a second passivation layer.
[0035] In some embodiments, when the solar cell is a TOPCON cell, the solar cell further includes a stacked tunnel dielectric layer and a doped conductive layer, the tunnel dielectric layer being located on the second surface 12 of the substrate 100, and the second gridlines 22 burning through the second passivation layer and making electrical contact with the doped conductive layer.
[0036] In some embodiments, the first grid lines 21 and the second grid lines 22 are both sub-grid lines of a solar cell, and the sub-grid lines may be formed by firing a burn-through paste. A method for forming the first grid lines 21 and the second grid lines 22 includes printing a metal paste on a surface of a portion of a passivation layer using a screen printing process. The metal paste may include at least one of silver, aluminum, copper, tin, gold, lead, or nickel. In the process of firing the metal paste, in some embodiments, the metal paste includes a highly corrosive component such as glass, so that the corrosive component corrodes the passivation layer during the sintering process, and the metal paste penetrates into the passivation layer 101 to make electrical contact with the substrate 100.
[0037] In some embodiments, along the first direction Y, the first grid lines 21 include two first electrodes 110 located at the ends of the substrate 100 and a plurality of second electrodes 120 located between the two first electrodes 110, where the first electrodes 110 include a first widened portion 111. The first electrodes 110 further include first sub-grid lines 112 located on both sides of the first widened portion 111. The first sub-grid lines 112 burn through the passivation layer 101 and protrude from the passivation layer 101.
[0038] 2, the first widened portion 111 is located on the surface of the passivation layer 101 and does not burn through the passivation layer 101, i.e., the material composition of the first widened portion 111 is different from the material composition of the first sub-grid lines 112. For example, the first widened portion 111 is made from a main grid line printing paste, and the first sub-grid lines 112 are made from a sub-grid line printing paste, in which the sub-grid line printing paste has a high silver content, thereby burning through the passivation layer, and the main grid line printing paste has a low silver content and a high aluminum content.
[0039] In some embodiments, the first length L1 of the first widened portion 111 in the second direction X is in the range of 0.5 mm to 1.5 mm. The first length L1 may be in the range of 0.5 mm to 0.8 mm, 0.58 mm to 1.39 mm, 0.6 mm to 1.5 mm, 0.9 mm to 1.48 mm, 0.5 mm to 1 mm, 0.6 mm to 1.3 mm, or 0.69 mm to 0.8 mm. The first length L1 may be 0.53 mm, 0.58 mm, 0.77 mm, 0.98 mm, 1.19 mm, 1.28 mm, 1.33 mm, 1.42 mm, or 1.5 mm.
[0040] In some embodiments, the first width W1 of the first widened portion 111 in the first direction Y is in the range of 0.1 mm to 0.5 mm. The first width W1 may be 0.1 mm to 0.16 mm, 0.16 mm to 0.28 mm, 0.28 mm to 0.41 mm, 0.41 mm to 0.5 mm, 0.14 mm to 0.45 mm, 0.16 mm to 0.28 mm, or 0.19 mm to 0.36 mm. The first width W1 may be 0.12 mm, 0.18 mm, 0.21 mm, 0.33 mm, 0.35 mm, 0.42 mm, 0.46 mm, or 0.5 mm.
[0041] In some embodiments, the fifth width W5 of the first sub-grid lines 112 in the first direction is in the range of 10 um to 45 um. The fifth width W5 may be 11 um to 15 um, 15 um to 20 um, 20 um to 38 um, 38 um to 45 um, 10 um to 25 um, 18 um to 32 um, or 14 um to 37 um. The fifth width W5 may be 10.3 um, 16.8 um, 21.7 um, 33.6 um, 35.8 um, 41.1 um, 42.3 um, or 45 um.
[0042] In some embodiments, as shown in FIG. 3, the first grid lines 21 are integrally formed, i.e., the first widened portions 111 and the first sub-grid lines 112 of the first electrode 110 are integrally formed, and the first widened portions 111 and the first sub-grid lines 112 can be manufactured in the same manufacturing process using the same printing paste, and the first widened portions 111 and the first sub-grid lines 112 both burn through the passivation layer 101. This allows the width of the area of the first grid lines 21 located at the end of the battery cell to be large, which can reduce the welding stress of the first electrode 110 and form a good contact between the PV ribbons 40 and the battery cell. In addition, the first widened portions 111 can improve the transport ability of carriers and provide the battery cell with a large transport area for collecting current.
[0043] In some embodiments, along the first direction, the second grid lines 22 include third electrodes 210 arranged at intervals and a plurality of fourth electrodes 220 located between two third electrodes 210, and the third electrodes 210 include second widened portions 211. The third electrodes 210 further include second sub-grid lines 212 located on both sides of the second widened portions 211. The second sub-grid lines 212 burn through the passivation layer 101 and protrude from the passivation layer 101.
[0044] In some embodiments, within the same second surface 12, the number of third electrodes 210 is 2 to 20. The number of third electrodes 210 is the number of second widened portions 211, and the number of second widened portions 211 is equal to or greater than the number of first widened portions 111. This can reduce the shielding area of the first surface 11 and improve the battery efficiency of the battery cell. By increasing the number of second widened portions 211 to increase the welding area of the second surface, the welding tensile force between the battery and the PV ribbon can be increased.
[0045] In some embodiments, the second width W2 of the second widened portion 211 in the first direction Y is in the range of 0.2 mm to 1.0 mm. The second width W2 may be in the range of 0.21 mm to 0.8 mm, 0.2 mm to 0.8 mm, 0.38 mm to 0.78 mm, 0.25 mm to 0.94 mm, 0.29 mm to 0.99 mm, 0.5 mm to 0.82 mm, 0.86 mm to 1.0 mm, or 0.19 mm to 0.69 mm. The second width W2 may be 0.21 mm, 0.38 mm, 0.41 mm, 0.53 mm, 0.65 mm, 0.78 mm, 0.89 mm, or 0.98 mm.
[0046] In some embodiments, the second length L2 of the second widened portion 211 in the second direction X is in the range of 0.5 mm to 1.5 mm. The second length L2 may be in the range of 0.5 mm to 0.8 mm, 0.54 mm to 1.39 mm, 0.6 mm to 1.5 mm, 0.9 mm to 1.48 mm, 0.5 mm to 1 mm, 0.6 mm to 1.3 mm, or 0.56 mm to 0.8 mm. The second length L2 may be 0.53 mm, 0.58 mm, 0.77 mm, 0.98 mm, 1.19 mm, 1.28 mm, 1.33 mm, 1.42 mm, or 1.5 mm.
[0047] In some embodiments, the second widened portion 211 is located on the surface of the passivation layer 101 and does not burn through the passivation layer 101, i.e., the material composition of the second widened portion 211 is different from the material composition of the second sub-grid lines 212. For example, the second widened portion 211 is made from a main grid line printing paste and the second sub-grid lines are made from a sub-grid line printing paste.
[0048] In some embodiments, the second grid lines 22 are integrally formed, i.e., the second widened portion 211 and the second sub-grid lines 212 of the third electrode 210 are also integrally formed, and the second widened portion 211 and the second sub-grid lines 212 can be manufactured in the same manufacturing process using the same printing paste, and both the second widened portion 211 and the second sub-grid lines 212 are burned through the passivation layer 101. This increases the width of the area of the second grid lines 22 located at the end of the battery cell, which can reduce the welding stress of the third electrode 210 and provide good contact between the PV ribbons and the cell. The second widened portion 211 also increases the carrier transport capacity and provides the battery cell with a large transport area for collecting current.
[0049] In some embodiments, the sixth width W6 of the second sub-grid lines 212 is in the range of 14 um to 60 um. The sixth width W6 may be in the range of 15 um to 20 um, 20 um to 28 um, 28 um to 35 um, 35 um to 49 um, 49 um to 52 um, 52 um to 60 um, or 18 um to 39 um. The sixth width W6 may be 14.3 um, 24.8 um, 35.7 um, 41.8 um, 47.8 um, 52.1 um, 59.6 um, or 60 um.
[0050] 8, the second electrode 120 includes a third widened portion 121, which faces the first widened portion 111 along the first direction Y and has a smaller dimension than the first widened portion 111. The second electrode 120 further includes third sub-grid lines 122 located on both sides of the third widened portion 121. The third sub-grid lines 122 burn through the passivation layer 101 and protrude from the passivation layer 101.
[0051] In some embodiments, the third widened portion 121 is located on the surface of the passivation layer 101 and does not burn through the passivation layer 101, i.e., the material composition of the third widened portion 121 is different from the material composition of the third sub-grid lines 122. For example, the third widened portion 121 is made from a main grid line printing paste and the third sub-grid lines 122 are made from a sub-grid line printing paste.
[0052] In some embodiments, as shown in Fig. 9, the third length L3 of the third widened portion 121 in the second direction X is in the range of 0.5 mm to 1.5 mm. The range of the third length L3 may be 0.5 mm to 0.8 mm, 0.58 mm to 1.39 mm, 0.6 mm to 1.5 mm, 0.9 mm to 1.48 mm, 0.5 mm to 1 mm, 0.6 mm to 1.3 mm, or 0.69 mm to 0.8 mm. The third length L3 may be 0.53 mm, 0.58 mm, 0.77 mm, 0.98 mm, 1.19 mm, 1.28 mm, 1.33 mm, 1.42 mm, or 1.5 mm.
[0053] In some embodiments, the third width W3 of the third widened portion 121 in the first direction Y is in the range of 0.02 mm to 0.2 mm. The third width W3 may be in the range of 0.02 mm to 0.1 mm, 0.08 mm to 0.18 mm, 0.02 mm to 0.14 mm, 0.09 mm to 0.19 mm, 0.05 mm to 0.12 mm, 0.16 mm to 0.2 mm, or 0.09 mm to 0.19 mm. The third width W3 may be 0.02 mm, 0.08 mm, 0.11 mm, 0.13 mm, 0.15 mm, 0.18 mm, 0.19 mm, or 0.2 mm.
[0054] In some embodiments, the seventh width W7 of the third sub-grid lines 122 in the first direction is in the range of 10 um to 45 um. The seventh width W7 may be in the range of 11 um to 15 um, 15 um to 20 um, 20 um to 38 um, 38 um to 45 um, 10 um to 25 um, 18 um to 32 um, or 14 um to 37 um. The seventh width W7 may be 10.3 um, 16.8 um, 21.7 um, 33.6 um, 35.8 um, 41.1 um, 42.3 um, or 45 um.
[0055] In some embodiments, the first grid lines 21 are integral structures, i.e., the third widened portion 121 and the third sub-grid lines 122 of the third electrode 120 are also integral structures, and the third widened portion 121 and the third sub-grid lines 122 can be manufactured in the same manufacturing process by using the same printing paste, and the third widened portion 121 and the third sub-grid lines 122 both burn through the passivation layer 101. The third widened portion 121 and the third sub-grid lines 122 can improve the carrier transport ability and provide the battery cell with a large transport area for collecting current.
[0056] In some embodiments, as shown in FIG. 10 , the fourth electrode 220 includes a fourth widening portion 221, which faces the second widening portion 211 along the first direction Y, and the dimensions of the fourth widening portion 221 are smaller than the dimensions of the second widening portion 211.
[0057] In some embodiments, the fourth widened portion has a smaller dimension than the first widened portion. The fourth electrode 220 further includes a fourth sub-grid line 222 located on either side of the fourth widened portion 221. The fourth sub-grid line 222 burns through the passivation layer 101 and protrudes from the passivation layer 101.
[0058] In some embodiments, the fourth width W4 of the fourth widened portion 221 in the first direction Y is in the range of 0.02 mm to 0.2 mm. The fourth width W4 may be in the range of 0.02 mm to 0.1 mm, 0.08 mm to 0.18 mm, 0.02 mm to 0.14 mm, 0.09 mm to 0.19 mm, 0.05 mm to 0.12 mm, 0.16 mm to 0.2 mm, or 0.09 mm to 0.19 mm. The fourth width W4 may be 0.02 mm, 0.08 mm, 0.11 mm, 0.13 mm, 0.15 mm, 0.18 mm, 0.19 mm, or 0.2 mm.
[0059] In some embodiments, the fourth length L4 of the fourth widened portion 221 in the second direction X is in the range of 0.5 mm to 1.5 mm. The fourth length L4 may be in the range of 0.5 mm to 0.8 mm, 0.54 mm to 1.39 mm, 0.6 mm to 1.5 mm, 0.9 mm to 1.48 mm, 0.5 mm to 1 mm, 0.6 mm to 1.3 mm, or 0.56 mm to 0.8 mm. The fourth length L4 may be 0.53 mm, 0.58 mm, 0.77 mm, 0.98 mm, 1.19 mm, 1.28 mm, 1.33 mm, 1.42 mm, or 1.5 mm.
[0060] In some embodiments, the fourth widened portion 221 is located on the surface of the passivation layer 101 and does not burn through the passivation layer 101, i.e., the material composition of the fourth widened portion 221 is different from the material composition of the fourth sub-grid lines 222. For example, the fourth widened portion 221 is made from a main grid line printing paste and the fourth sub-grid lines are made from a sub-grid line printing paste.
[0061] In some embodiments, the second grid line 22 is an integrally molded structure, i.e., the fourth widened portion 221 and the fourth sub-grid line 222 of the fourth electrode 220 are also integrally molded structures, and the fourth widened portion 221 and the fourth sub-grid line 222 can be manufactured in the same manufacturing process by using the same printing paste, and the fourth widened portion 221 and the fourth sub-grid line 222 are both burned through the passivation layer 101. This increases the width of the area of the second grid line 22 located at the end of the battery cell, which can relieve the welding stress of the third electrode 220 and form a good contact between the PV ribbon and the battery cell. In addition, the fourth widened portion 221 can increase the carrier transport capacity and provide the battery cell with a large transport area for collecting current.
[0062] In some embodiments, the solar cell is a split battery. In some embodiments, the split battery is a half-split battery, which can be understood as a half-cut battery or a two-split battery. In other embodiments, the split battery can be a three-split battery, a four-split battery, or an eight-split battery, etc.
[0063] Experimental example 0: The first widened portion and the second widened portion were not provided, that is, each grid line was a completely uniform grid line.
[0064] Example 1: The number of first widening portions and second widening portions is equal, there are no adhesive dots on the first surface, the dimensions of the second widening portions are larger than the dimensions of the first widening portions, the first width W1 of the first widening portion is 0.3 mm, the first length L1 of the first widening portion is 0.8 mm, the second width W2 of the second widening portion is 0.3 mm, the second length L2 of the second widening portion is 1.0 mm, the number of first widening portions is 2, and the number of second widening portions is 2.
[0065] Example 2: The number of first widening portions is less than the number of second widening portions, there are no adhesive dots on the first surface, the dimensions of the second widening portions are greater than the dimensions of the first widening portions, the first width W1 of the first widening portion is 0.3 mm, the first length L1 of the first widening portion is 0.8 mm, the second width W2 of the second widening portion is 0.3 mm, the second length L2 of the second widening portion is 1.0 mm, the number of first widening portions is 2 and the number of second widening portions is 4.
[0066] Example 3: The number of first widening portions is less than the number of second widening portions, there are adhesive dots on the first surface, the dimensions of the second widening portions are greater than the dimensions of the first widening portions, the first width W1 of the first widening portion is 0.3 mm, the first length L1 of the first widening portion is 0.8 mm, the second width W2 of the second widening portion is 0.3 mm, the second length L2 of the second widening portion is 1.0 mm, the number of adhesive dots is 2, the number of first widening portions is 2, and the number of second widening portions is 4.
[0067] Example 4: The number of first widening portions is equal to the number of second widening portions, there are adhesive dots on the first surface, the dimensions of the second widening portions are larger than the dimensions of the first widening portions, the first width W1 of the first widening portion is 0.3 mm, the first length L1 of the first widening portion is 0.8 mm, the second width W2 of the second widening portion is 0.3 mm, the second length L2 of the second widening portion is 1.0 mm, the number of first widening portions is 2, the number of second widening portions is 2, the number of adhesive dots is 4, and the first surface and the second surface have third widening portions and fourth widening portions.
[0068] Table 1 JPEG2024169256000002.jpg5597
[0069] As can be seen from Table 1, setting the quantity and dimensions of the second widening parts can increase the welding pull-off force between the PV ribbons and the battery cells. Here, according to the ratio of the welding pull-off force of each embodiment and Experimental Example 0, it can be seen that when adhesive dots are provided between the PV ribbons on the first surface and the battery cells, the welding pull-off force is good.
[0070] In the solar cell according to the embodiment of the present application, the substrate has a first surface and a second surface facing each other, and the first grid line located on the first surface has a first widening portion, and the second grid line located on the second surface has a second widening portion, so that the first widening portion and the second widening portion can increase the welding tensile force between the first grid line and the PV ribbon and the welding tensile force between the second grid line and the PV ribbon, and thus improve the welding effect between the first grid line and the PV ribbon and the welding effect between the second grid line and the PV ribbon. The size of the first widening portion is larger than the size of the second widening portion, and the size of the first widening portion on the first surface and the size of the second widening portion on the second surface are changed, i.e., the size of the first widening portion on the first surface is ensured to be small, so that the coverage area of the first surface is reduced, and the cell efficiency of the solar cell can be improved. The second widening portions of the second surface are located at least at the end of the substrate, i.e., the number of the second widening portions is equal to or greater than the number of the first widening portions. By increasing the number of the second widening portions, the welding area of the second surface can be increased, and the welding tensile force between the battery and the PV ribbon can be increased.
[0071] FIG. 13 is a diagram showing a configuration in which a PV ribbon is formed on a first surface of a photovoltaic module according to an embodiment of the present application; FIG. 14 is a diagram showing a configuration in which a PV ribbon is formed on a second surface of a photovoltaic module according to an embodiment of the present application; FIG. 15 is a diagram showing a configuration in which adhesive dots are formed on a first surface of a photovoltaic module according to an embodiment of the present application; and FIG. 16 is a diagram showing the configuration of a photovoltaic module according to an embodiment of the present application.
[0072] According to some embodiments of the present application, in another form of the embodiment of the present application, there is further provided a photovoltaic module, which includes a cell string in which a plurality of solar cells 50 are electrically connected by PV ribbons 40, the PV ribbons 40 are electrically connected to each of the first grid lines 21 and / or each of the second grid lines 22, and any of the PV ribbons 40 is in electrical contact with the first widened portion 111 or the second widened portion 211, a sealing layer 51 for covering a surface of the cell string, and a cover plate 52 for covering a surface of the sealing layer 51 away from the cell string.
[0073] Specifically, in some embodiments, the cell strings may be electrically connected by the PV ribbon 40. FIG. 16 shows only the positional relationship between one solar cell 50. That is, in the solar cell 50, the electrodes having the same polarity are arranged in the same direction, or the electrodes of each battery cell having a positive polarity are arranged on the same side, so that the conductive tape is connected to the different sides of two adjacent battery cells. In some embodiments, the solar cell 50 can have electrodes of different polarities facing the same side. That is, the electrodes of the adjacent battery cells are arranged in the order of the first polarity, the second polarity, and the first polarity, and the conductive tape connects the two adjacent battery cells on the same side.
[0074] In some embodiments, there is no spacing between the solar cells 50, i.e., the solar cells 50 overlap each other.
[0075] In some embodiments, the cross-sectional shape of PV ribbons 40 may be circular, as shown in Figures 2 and 3, because circular PV ribbons are free of orientation and alignment problems and are easier to mass-produce. To increase the contact area between the PV ribbons and the reinforcing grid and reduce misalignment problems between PV ribbons 40 and the reinforcing grid, in some embodiments, the cross-sectional shape of PV ribbons 40 may be triangular or any other shape.
[0076] In some embodiments, the dimensions of the PV ribbon 40 are between 160 and 300 um, and the number of PV ribbons in one battery cell is between 12 and 30. The dimensions of the PV ribbon 40 are between 160 and 180 um, 180 and 200 um, 200 and 220 um, 220 and 240 um, 240 and 280 um, and 280 and 300 um.
[0077] In some embodiments, there are M first overlapping regions between the same PV ribbon 40 and the first grid lines 110, and N adhesive dots 102 are further included, each adhesive dot 102 covering a first overlapping region, and the adhesive dots 102 are also located on the first widened portions 111, where N is less than M and equal to or greater than the number of the first widened portions 111, and the sealing layer 51 is located on the surface of the adhesive dots 102. In this way, the adhesive dots 101 position the PV ribbon 40 and precisely position the positional relationship between the PV ribbon 40 and the first grid lines 21, which ensures good contact between the PV ribbon 40 and the battery in the subsequent welding or lamination process, increases the welding pull force, and maximizes the battery efficiency.
[0078] In some embodiments, the adhesive dots completely cover the first overlap region, and the dimensions of the adhesive dots are at least 1.5 times the dimensions of the first overlap region, so that the PV ribbons are firmly positioned on the surface of the battery cell, and the welding tension between the battery and the PV ribbons is increased. The adhesive dots can also prevent problems such as PV ribbon misalignment during subsequent lamination processes.
[0079] In some embodiments, N is equal to or less than the number of second widened portions 211. N satisfies 2≦N≦20.
[0080] In some embodiments, the encapsulation layer 51 is located on the surface of the second grid lines 22, the PV ribbons 40 corresponding to the second surface 12 are in direct contact with the encapsulation layer 51, and no adhesive dots are provided on the second surface 12. By not providing adhesive dots on the second surface and increasing the quantity and size of the second widening portion, the welding pull force between the battery cells and the PV ribbons can be increased, which can avoid the adhesive application process and reduce the process difficulty.
[0081] In some embodiments, the encapsulating layer 51 includes a first encapsulating layer covering one of the front and back surfaces of the solar cell 50, and a second encapsulating layer covering the other of the front and back surfaces of the solar cell 50. Specifically, at least one of the first encapsulating layer or the second encapsulating layer may be an organic encapsulating adhesive film such as a polyvinyl butyral (abbreviated as PVB) adhesive film, an ethylene vinyl acetate copolymer (EVA) adhesive film, a polyethylene-octene copolymer (POE) adhesive film, or a polyethylene terephthalate (PET) adhesive film, or may be an EPE (a co-extruded adhesive film of one layer of EVA, one layer of POE, and one layer of EVA) or an EP (a co-extruded adhesive film of one layer of EVA and one layer of POE).
[0082] As can be understood, before lamination processing, there is a boundary between the first sealing layer and the second sealing layer, and after lamination processing, when the photovoltaic module is formed, the concepts of the first sealing layer and the second sealing layer disappear, and the first sealing layer and the second sealing layer are integrated to form sealing layer 51.
[0083] In some embodiments, the cover plate 52 may be a cover plate having a light transmitting function, such as a glass cover plate, a plastic cover plate, etc. Specifically, the surface of the cover plate 52 facing the sealing layer 51 may be an uneven surface, which can improve the utilization rate of the incident light. The cover plate 52 includes a first cover plate facing the first sealing layer and a second cover plate facing the second sealing layer.
[0084] According to some embodiments of the present application, in another aspect of the embodiments of the present application, there is further provided a method for manufacturing a photovoltaic module, the method including: providing a plurality of battery cells and PV ribbons; performing a welding process on the PV ribbons and the battery cells, such that alloy layers are formed between the PV ribbons and a first grid line and between the PV ribbons and a second grid line, the battery cells and the PV ribbons after the welding process constitute a cell string; providing a sealing layer and a cover plate, the sealing layer is used to cover a surface of the cell string, and the cover plate is used to cover a surface of the sealing layer remote from the cell string; and performing a lamination process on the cell string, the sealing layer, and the cover plate.
[0085] In some embodiments, there are M first overlapping areas between the same PV ribbon and the first grid line, and after performing the welding process, the method further includes applying adhesive to a portion of the first overlapping area of the battery cell, such that there are N adhesive dots on a surface of the battery cell, each adhesive dot covering the first overlapping area, and the adhesive dots are also located in the first widening portion, where N is less than M and greater than or equal to the number of the first widening portions.
[0086] Although the present application has been disclosed as above in the preferred embodiment, it does not limit the scope of the claims, and since a person skilled in the art can make some possible variations and modifications without departing from the idea of the present application, the scope of protection of the present application should be in accordance with the scope defined by the claims of the present application. In addition, the examples and drawings of the present application are merely illustrative and do not cover the entire scope of protection provided by the claims of the present application.
[0087] Those skilled in the art will understand that the above embodiments are specific examples for implementing the present application, but various changes in form and details are possible in practice without departing from the spirit and scope of the present application. Since any person skilled in the art can make changes and modifications without departing from the spirit and scope of the present application, the scope of protection of the present application should be based on the scope limited by the claims.
Claims
1. a substrate having opposing first and second surfaces; a plurality of first grid lines sequentially arranged along a first direction, the first grid lines being located on a first surface of the substrate, and at least one of the first grid lines located at an end of the substrate along the first direction has a first widening portion; a plurality of second grid lines sequentially arranged along the first direction, the second grid lines being located on a second surface of the substrate, and at least one second grid line located at an end of the substrate among the plurality of second grid lines along the first direction has a second widening portion, and a dimension of the second widening portion is larger than a dimension of the first widening portion. A solar cell characterized by:
2. Along the first direction, the first grid line includes two first electrodes located at an end of the substrate and a plurality of second electrodes located between the two first electrodes, the first electrodes include a first widened portion, the second electrodes include a third widened portion, the third widened portion faces the first widened portion along the first direction, and a dimension of the third widened portion is smaller than a dimension of the first widened portion, The solar cell according to claim 1 .
3. Along the first direction, the second grid lines include third electrodes arranged at intervals and a plurality of fourth electrodes located between two of the third electrodes, the third electrodes include second widened portions, the fourth electrodes include fourth widened portions, the fourth widened portions face the second widened portions along the first direction, and a dimension of the fourth widened portions is smaller than a dimension of the second widened portions.
3. The solar cell according to claim 1 or 2.
4. The fourth widening portion has a smaller dimension than the first widening portion. The solar cell according to claim 3 .
5. Within the same second surface, the number of the third electrodes is 2 to 20. The solar cell according to claim 3 .
6. The second width of the second widening portion in the first direction is in a range of 0.2 mm to 1.0 mm. The solar cell according to claim 1 .
7. the first grid line further includes first sub-grid lines located on both sides of the first widening portion, the first sub-grid lines burn through the passivation layer and protrude from the passivation layer; and The solar cell according to claim 1 .
8. the first grid lines are integrally molded structures and the second grid lines are integrally molded structures; The solar cell according to claim 1 .
9. a cell string in which a plurality of solar cells are electrically connected by PV ribbons, the PV ribbons being electrically connected to each of the first grid lines and / or each of the second grid lines, and any of the PV ribbons being in electrical contact with the first widened portion or the second widened portion; a sealing layer for covering a surface of the cell string; a cover plate for covering a surface of the sealing layer away from the cell string. A photovoltaic module comprising:
10. Between the same PV ribbon and the first grid line, there are M first overlapping regions, and further includes N adhesive dots, each of which covers the first overlapping region, and the adhesive dots are also located on the first widening portion, where N is smaller than M and equal to or greater than the number of the first widening portions, and the sealing layer is located on the surface of the adhesive dots.
10. The photovoltaic module of claim 9.
11. The N is equal to or less than the number of the second widening portions.
11. The photovoltaic module of claim 10.
12. The N satisfies 2≦N≦20, 11. The photovoltaic module of claim 10.
13. the encapsulation layer is located on a surface of the second grid lines, the PV ribbons corresponding to the second surface are in direct contact with the encapsulation layer, and the second surface is free of the adhesive dots; 10. The photovoltaic module of claim 9.
14. providing a plurality of battery cells and a PV ribbon; performing a welding process on the PV ribbon and the battery cell such that an alloy layer is formed between the PV ribbon and a first grid line and between the PV ribbon and a second grid line, and the battery cell and the PV ribbon after the welding process constitute a cell string; providing a sealing layer and a cover plate, the sealing layer being used to cover a surface of the cell string, and the cover plate being used to cover a surface of the sealing layer that is remote from the cell string; and performing a lamination process on the cell string, the sealing layer, and the cover plate. A method for producing a photovoltaic module comprising the steps of:
15. M first overlap regions between the same PV ribbon and the first grid line; After performing the welding process, the method further includes applying adhesive to a part of the first overlapping region of the battery cell so as to have N adhesive dots on a surface of the battery cell, each of the adhesive dots covering the first overlapping region, the adhesive dots also being located in a first widening portion, and N being smaller than M and equal to or greater than the number of the first widening portions. The method for producing a photovoltaic module according to claim 14 .
Citation Information
Patent Citations
Solar cell
JP2015070260A
Solar cell module and method for manufacturing the same
JP2016018997A
Ultrasonic soldering method and ultrasonic soldering device
JP2017080753A
Solar cell and its manufacturing method
JP2022550638A
Photovoltaic solar cell, cell module and manufacturing process
JP2023033059A
Cited By
Solar cell and photovoltaic module
JP2025120086A
Solar Cells and Photovoltaic Modules
JP7719911B1
Solar cell and photovoltaic module
US12707760B2