Three-color 3D DRAM stack and method for fabricating it
A three-color process with doped SiGe and silicon layers addresses wafer warpage and etch selectivity issues in 3D DRAM manufacturing, enhancing fabrication accuracy and reducing complexity.
Patent Information
- Application Number
- JP2024519291
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-09-28
- Filing Date
- 2022-09-28
- Publication Date
- 2024-10-16
- Estimated Expiration
- 2042-09-28
AI Technical Summary
Current 3D DRAM manufacturing processes face challenges with wafer warpage and reduced etch selectivity due to lattice mismatch stress, which hinder accurate lithography and increase process complexity and cost.
A three-color process using doped SiGe and silicon layers with varying Si:Ge ratios and dopant concentrations to form a stack with controlled stress and etch selectivity, reducing wafer bow and enabling selective etching.
The method achieves reduced wafer bow and improved etch selectivity, allowing for accurate lithography and simplified process steps in 3D DRAM fabrication.
Smart Images

Figure 2024537776000001_ABST
Abstract
Description
[Technical field]
[0001] FIELD OF THE DISCLOSURE Embodiments of the present disclosure generally relate to methods for forming 3D DRAM stacks and 3D DRAM devices, and more particularly, to methods for forming 3D DRAM devices using a 3-color process. [Background technology]
[0002] There is an interest in the semiconductor manufacturing industry to increase the bit density of memory devices. One approach to fabricating 3D DRAM devices involves epitaxially growing a multi-layer stack that includes an epitaxial silicon channel layer and two or more sacrificial epitaxial layers. Subsequent process steps require recessing the sacrificial layers to form access gates and capacitors.
[0003] To scale the density of 3D DRAM beyond the 10 nm node, the number of silicon channel and sacrificial layer stacks needs to increase to more than 100, which can result in 400 epitaxial layers. One issue with the increase in the number of layers is wafer warpage when the stacks increase beyond 150 μm. It is believed that lattice mismatch induced stress in the silicon channel / sacrificial layer stacks results in this wafer warpage. Generally, wafer warpage of more than 150 μm will prevent subsequent processes such as lithography from being performed accurately.
[0004] During device formation, the sacrificial layer is etched selectively to the silicon channel, and conventional layer stack designs designed to reduce wafer bow result in poor etch selectivity. Summary of the Invention [Problem to be solved by the invention]
[0005] Current state-of-the-art processes require the additional deposition of a stress relieving film on the backside of the wafer to counteract the wafer bow. This only partially alleviates the wafer bow problem because the bow returns when the top stack is etched or during thermal processes. In addition, the removal of the backside film increases process complexity and cost.
[0006] Therefore, there is a need for 3D DRAM devices and methods of forming 3D DRAM devices that have reduced wafer bow and / or improved etch selectivity. [Means for solving the problem]
[0007] One or more embodiments of the present disclosure are directed to a method for reducing wafer bow in a 3D DRAM device. A plurality of film stacks are formed on a substrate surface. Each of the film stacks includes a first doped SiGe layer, a second doped SiGe layer, and a doped silicon layer. The first doped SiGe layer has an empirical formula of Si 1-x Ge x where x is in the range of 0 to 0.5. A second doped SiGe layer is on the first doped SiGe layer and has an empirical formula Si 1-y Ge y where y is in the range >0 to 0.5. A doped silicon layer overlies a second doped SiGe layer. The first doped SiGe layer and the second doped SiGe layer have one or more of different doping amounts or different Si:Ge ratios.
[0008] An additional embodiment of the present disclosure is directed to a method of fabricating a 3D DRAM device. At least 100 film stacks are formed on a substrate surface. Each of the film stacks includes a first doped SiGe layer, a second doped SiGe layer, and a doped silicon layer. The first doped SiGe layer has an empirical formula of Si 1-x Ge xwhere x is in the range of 0 to 0.5. A second doped SiGe layer is on the first doped SiGe layer and has an empirical formula Si 1-y Ge y where y is in the range >0 to 0.5. The first doped SiGe layer and the second doped SiGe layer have one or more of different doping amounts or different Si:Ge ratios. A doped silicon layer is on the second doped SiGe layer. A channel is formed through the film stack to the substrate. One or more of the first doped SiGe layer or the second doped SiGe layer are selectively removed through the channel.
[0009] A further embodiment of the present disclosure is directed to a method of fabricating a 3D DRAM device with reduced wafer bow. At least 100 film stacks are formed on a substrate surface. Each of the film stacks includes an epitaxially grown first doped SiGe layer, an epitaxially grown second doped SiGe layer, and an epitaxially grown doped silicon layer. The epitaxially grown first doped SiGe layer has an empirical formula Si 1-x Ge x where x is in the range of 0 to 0.5. A second epitaxially grown doped SiGe layer is on the first doped SiGe layer and has an empirical formula of Si 1-y Ge ywhere y is in the range >0-0.5. The first doped SiGe layer and the second doped SiGe layer have one or more of different doping amounts or different Si:Ge ratios. An epitaxially grown doped silicon layer is on the second doped SiGe layer. The first doped SiGe layer, the second doped SiGe layer, and the doped silicon layer independently include a dopant selected from carbon or boron in the range of 0.5-2.5%. The stress of the second doped SiGe layer is more tensile than the stress of the first doped SiGe layer, and the stress of the first doped SiGe layer is more tensile than the stress of the Si layer. Each of the first doped SiGe layer, the second doped SiGe layer, and the doped silicon layer has an etch selectivity of greater than 200:1 relative to the other layer when using a halide-based etchant. A channel is lithographically formed through all of the stack down to the substrate surface, and one or more of the first doped SiGe layer or the second doped SiGe layer are selectively etched from all of the film stack through the channel.
[0010] In order that the features of the present disclosure may be understood in detail, a more detailed description of the present disclosure briefly summarized above may be made by referring to embodiments, some of which are illustrated in the accompanying drawings. It should be noted, however, that the accompanying drawings only illustrate typical embodiments of the present disclosure, and therefore should not be considered as limiting the scope of the present disclosure, since the present disclosure may admit of other equally effective embodiments. The embodiments described herein are shown by way of example and are not limited to the figures of the accompanying drawings, in which like reference designations indicate like elements. [Brief description of the drawings]
[0011] [Figure 1] 1 is a schematic diagram of a 3D DRAM device being formed by a three-color process in accordance with one or more embodiments of the present disclosure. [Diagram 2] FIG. 2 is an enlarged view of region II of FIG. 1 after formation of a channel through the membrane stack. [Diagram 3] FIG. 3 is an enlarged view of FIG. 2 after selective removal of one of the layers of the three-color process. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Before describing some example embodiments of the present disclosure, it is to be understood that the disclosure is not limited to the details of construction or process steps set forth in the following description as the disclosure is capable of other embodiments and of being practiced or carried out in various ways.
[0013] The term "substrate" as used herein and in the appended claims refers to a surface or a portion of a surface on which a process acts. Those skilled in the art will understand that a reference to a substrate may also refer to only a portion of the substrate, unless the context clearly indicates otherwise. In addition, a reference to depositing on a substrate may refer to both a bare substrate and a substrate having one or more films or features deposited or formed thereon.
[0014] As used herein, "substrate" refers to any substrate or material surface formed on a substrate on which a film treatment is performed during a manufacturing process. For example, substrate surfaces on which treatment can be performed include materials such as silicon, silicon oxide, strained silicon, silicon-on-insulator (SOI), carbon-doped silicon oxide, amorphous silicon, doped silicon, germanium, gallium arsenide, glass, sapphire, and any other materials such as metals, metal nitrides, alloys, and other conductive materials, depending on the application. Substrates include, but are not limited to, semiconductor wafers. Substrates may be exposed to pretreatment processes to polish, etch, reduce, oxidize, hydroxylate, anneal, UV cure, e-beam cure, and / or bake the substrate surface. In addition to film treatment directly on the surface of the substrate itself, in this disclosure, any of the disclosed film treatment steps may also be performed on an underlayer formed on the substrate as disclosed in more detail below, and the term "substrate surface" is intended to include such underlayers as the context indicates. Thus, for example, when a film / layer or partial film / layer is deposited on a substrate surface, the exposed surface of the newly deposited film / layer becomes the substrate surface for further processing.
[0015] According to one or more embodiments, the term "on" in reference to a film or layer of a film includes the film or layer being directly on a surface, e.g., a substrate surface, as well as the presence of one or more underlayers between the film or layer and a surface, e.g., a substrate surface. Thus, in one or more embodiments, the phrase "on a substrate surface" is intended to include one or more underlayers. In other embodiments, the phrase "directly on" refers to a layer or film that contacts a surface, e.g., a substrate surface, without an intervening layer. Thus, the phrase "a layer directly on the substrate surface" refers to a layer that directly contacts the substrate surface without an intermediate layer.
[0016] One or more embodiments of the present disclosure advantageously provide a three-color method for forming a 3D DRAM device with a film stack having reduced or neutral bow. When used in this manner, a three-color process means that three etch selective materials are used. Some embodiments advantageously provide a 3D DRAM film stack including epitaxial silicon (Si) and silicon germanium (SiGe) with reduced or neutral bow. Some embodiments advantageously provide an epi Si / SiGe stack with reduced bow using carbon (C) or boron (B) doping.
[0017] 1-3, one or more embodiments of the present disclosure are directed to a method for reducing wafer bow in a 3D DRAM device 100 using a three-color process. A plurality of film stacks 120 are formed on a substrate 110 having a substrate surface 112. The film stacks 120 may also be referred to as three-color stacks. The embodiment shown in FIG. 1 shows five film stacks 120 (including film stacks 120a, 120b). Those skilled in the art will recognize that this is merely representative and that there may be more or fewer film stacks 120. In some embodiments, there are more than 50, 100, 150, or 200 film stacks 120.
[0018] At least a portion of the film stacks 120, or each of the film stacks 120, includes a first doped SiGe layer 122, a second doped SiGe layer 124, and a doped silicon layer 126. Those skilled in the art will recognize that the first doped SiGe layer 122 in the first stack 120a is formed on the substrate surface 112 or directly on the substrate surface 112. The first doped SiGe layer 122 of the subsequent film stack 120b is formed on the surface 127 of the doped silicon layer 126 of the previous film stack 120a or directly on the surface 127 of the doped silicon layer 126 of the previous film stack 120a.
[0019] The first doped SiGe layer 122 has the empirical formula Si 1-x Ge x In some embodiments, x is in the range of from greater than 0 (>0) to 0.5. In some embodiments, x is in the range of from greater than 0 to 0.4, or from greater than 0 to 0.3, or from greater than 0 to 0.2. In some embodiments, x is in the range of 0.05, 0.1, 0.15, 0.2, or 0.25 to 0.5.
[0020] The first doped SiGe layer 122 includes a dopant having a concentration in the range of 0.5 atomic % to 2.5 atomic %. In some embodiments, the first doped SiGe layer 122 has a dopant concentration in the range of 0.5, 0.6, 0.7, 0.8, 0.9, 1.0, 1.1, 1.2, 1.3, 1.4, or 1.5 atomic % to 2.5 atomic %. In some embodiments, the first doped SiGe layer 122 has a dopant concentration in the range of 0.5 atomic % to 1.5, 1.6, 1.7, 1.8, 1.9, 2.0, 2.1, 2.2, 2.3, 2.4, or 2.5 atomic %.
[0021] The second doped SiGe layer 124 has the empirical formula Si 1-y Ge y In some embodiments, y is in the range of 0 to 0.5. In some embodiments, y is in the range of 0 to 0.4, or in the range of 0 to 0.3, or in the range of 0 to 0.2. In some embodiments, x is in the range of 0.05, 0.1, 0.15, 0.2, or 0.25 to 0.5. In some embodiments, x from the first doped layer 122 and y of the second doped layer 124 differ by 0.1, 0.2, 0.3, 0.4, or 0.5 or more. In some embodiments, x is greater than y. In some embodiments, y is greater than x.
[0022] The second doped SiGe layer 124 includes a dopant having a concentration in the range of 0.5 atomic % to 2.5 atomic %. In some embodiments, the second doped SiGe layer 124 has a dopant concentration in the range of 0.5, 0.6, 0.7, 0.8, 0.9, 1.0, 1.1, 1.2, 1.3, 1.4, or 1.5 atomic % to 2.5 atomic %. In some embodiments, the second doped SiGe layer 124 has a dopant concentration in the range of 0.5 atomic % to 1.5, 1.6, 1.7, 1.8, 1.9, 2.0, 2.1, 2.2, 2.3, 2.4, or 2.5 atomic %.
[0023] The doped silicon layer 126 includes a dopant having a concentration in the range of 0.5 atomic % to 2.5 atomic %. In some embodiments, the doped silicon layer 126 has a dopant concentration in the range of 0.5, 0.6, 0.7, 0.8, 0.9, 1.0, 1.1, 1.2, 1.3, 1.4, or 1.5 atomic % to 2.5 atomic %. In some embodiments, the doped silicon layer 126 has a dopant concentration in the range of 0.5 atomic % to 1.5, 1.6, 1.7, 1.8, 1.9, 2.0, 2.1, 2.2, 2.3, 2.4, or 2.5 atomic %.
[0024] The dopant in either the first doped SiGe layer 122, the second doped SiGe layer 124, or the doped silicon layer 126 can be any suitable dopant known to one of skill in the art. In some embodiments, the dopant comprises a III-V group element. In some embodiments, the dopant comprises one or more of carbon or boron. In some embodiments, the dopant consists essentially of one or more of carbon or boron. As used in this manner, the term "consists essentially of" means that the composition of the subject component is 95%, 98%, 99%, or 99.5% or more of the stated material. For example, a dopant consisting essentially of carbon and / or boron means that of all dopant atoms, 95% or more are carbon or boron. In some embodiments, the dopant comprises carbon or consists essentially of carbon. In some embodiments, the dopant comprises boron or consists essentially of boron.
[0025] In some embodiments, the first doped SiGe layer and the second doped SiGe layer independently include a dopant in the range of 0.5-2.5%. In some embodiments, the first doped SiGe layer, the second doped SiGe layer, and the doped silicon layer independently include a dopant in the range of 0.5-2.5%. The dopant may be the same or different in the different layers.
[0026] In some embodiments, the x of the first doped SiGe layer 122 and the y of the second doped SiGe layer 124 are the same or within 0.1 of each other, and the dopant concentrations of each of the first doped SiGe layer 122 and the second doped SiGe layer 124 differ by more than 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, or 1.0 atomic percent.
[0027] The various layers described may be formed by any suitable technique known to one of skill in the art. For example, one or more of the films may be formed by epitaxial growth, chemical vapor deposition, atomic layer deposition, physical vapor deposition, ion implantation, etc. In some embodiments, each of the first doped SiGe layer 122, the second doped SiGe layer 124, and the doped silicon layer 126 are epitaxially grown. In some embodiments, each of the first doped SiGe layer 122, the second doped SiGe layer 124, and the doped silicon layer 126 are independently grown at a temperature in the range of 500° C. to 800° C.
[0028] The stress of the membrane stack 120 is adjusted by the doped layers. In some embodiments, the stress of the second doped SiGe layer 124 is more tensile than the stress of the first doped SiGe layer 122. The stress of the membrane stack 120 is adjusted by the doped layers. In some embodiments, the stress of the second doped SiGe layer 124 is more tensile than the stress of the first doped SiGe layer 122, which is more tensile than the stress of the doped silicon layer 126. In some embodiments, the stress of the first doped SiGe layer 122 and the second doped SiGe layer 124 is more tensile than the stress of the doped silicon layer 126.
[0029] In some embodiments, the overall bow of the wafer is neutral after formation of 100 film stacks 120. In some embodiments, the overall bow of the wafer is neutral after formation of 125, 150, 175, or 200 film stacks 120. The term "neutral" as used in this manner means that the bow across the wafer surface is no greater than 150 μm, 125 μm, 100 μm, 75 μm, 50 μm, or 25 μm. Some embodiments provide a method of doping epi films in a controlled manner that reduces the wafer bow to about 30 μm for 1 μm talk stacks to enable 5 μm or larger DRAM stacks.
[0030] In the three-color process shown in the figure, the first doped SiGe layer 122 and the second doped SiGe layer 124 differ from each other in the way that makes the two etches selective to each other. In some embodiments, the first doped SiGe layer 122 and the second doped SiGe layer 124 have similar Si:Ge ratios at different doping levels. In some embodiments, the first doped SiGe layer 122 and the second doped SiGe layer 124 have different Si:Ge ratios at similar doping levels. Stated differently, in some embodiments, the first doped SiGe layer 122 and the second doped SiGe layer 124 have one or more of different doping amounts or different Si:Ge ratios.
[0031] The first doped SiGe layer 122, the second doped SiGe layer 124, and the doped silicon layer 126 are etch selective relative to one another. In some embodiments, the first doped SiGe layer 122 and the doped silicon layer 126 have an etch selectivity of greater than 200:1 when using a halide-based etchant (e.g., 1% HF, NF3 plasma). The halide-based etchant includes a wet etchant or a gas-phase etchant. In some embodiments, the halide-based etchant is a gas-phase etchant that includes fluorine atoms. In some embodiments, the second doped SiGe layer 124 and the doped silicon layer 126 have an etch selectivity of greater than 200:1 when using a halide-based etchant. In some embodiments, the first doped SiGe layer 122 and the second doped SiGe layer 124 have an etch selectivity of greater than 200:1 when using a halide-based etchant. In some embodiments, the first doped SiGe layer 122, the second doped SiGe layer 124, and the doped silicon layer 126 each have an etch selectivity of greater than 200:1 relative to the other layers when using a halide-based etchant.
[0032] While the embodiments and illustrations discuss a three-color method, one skilled in the art will recognize that the doped Si and doped SiGe layers can be configured to provide a four or more color system, with the additional colors (SiGe layers) being etch selective due to one or more of a different dopant amount or a different Si:Ge ratio compared to the first doped SiGe layer 122, the second doped SiGe layer 124, and the doped silicon layer 126.
[0033] 2 and 3 show a portion of the 3D DRAM device 100 in region II of FIG. 1. In some embodiments, the method further includes forming a channel 140 by lithography through all of the film stack 120 to the substrate surface 112 (or a distance within the substrate 110). Those skilled in the art will understand how to form the channel 140 using lithography. After forming the channel 140, one or more of the first doped SiGe layer 122 or the second doped SiGe layer 124 are selectively etched from the film stack 120 through the channel 140. FIG. 3 shows that the first doped SiGe layer 122 has been removed, leaving behind the second doped SiGe layer 124 and the doped silicon layer 126. Those skilled in the art will appreciate that the second doped SiGe layer 124 may be removed through the channel 140 while leaving the first doped SiGe layer 122 and the doped silicon layer 126.
[0034] References throughout this specification to "one embodiment," "a particular embodiment," "one or more embodiments," or "an embodiment" mean that a particular feature, structure, material, or characteristic described in connection with an embodiment is included in at least one embodiment of the present disclosure. Thus, the appearances of phrases such as "in one or more embodiments," "in a particular embodiment," "in one embodiment," or "in one embodiment" in various places throughout this specification do not necessarily refer to the same embodiment of the present disclosure. Furthermore, particular features, structures, materials, or characteristics may be combined in any suitable manner in one or more embodiments.
[0035] Although the disclosure of this specification has been described with reference to specific embodiments, those skilled in the art will understand that the described embodiments are merely illustrative of the principles and applications of the present disclosure. It will be apparent to those skilled in the art that various modifications and variations may be made to the disclosed method and apparatus without departing from the spirit and scope of the present disclosure. Thus, the present disclosure can include modifications and variations within the scope of the appended claims and their equivalents.
Claims
1. 1. A method for reducing wafer bow in a 3D DRAM device, the method comprising: forming a plurality of film stacks on a substrate surface, each of the film stacks comprising: Empirical formula: Si 1-x Ge x where x is in the range of >0 to 0.5; and a second doped SiGe layer on the first doped SiGe layer, the second doped SiGe layer having an empirical formula of Si 1-y Ge y where y is in the range of >0 to 0.5; and a doped silicon layer on the second doped SiGe layer; and Including, forming the first doped SiGe layer and the second doped SiGe layer having one or more of different doping amounts or different Si:Ge ratios; A method comprising:
2. The method of claim 1, wherein the first doped SiGe layer comprises a dopant in the range of 0.5 to 2.5%.
3. The method of claim 2, wherein the dopant is a Group III-V element.
4. The method of claim 3 , wherein the dopant is one or more of carbon or boron.
5. The method of claim 1, wherein the second doped SiGe layer comprises a dopant in the range of 0.5 to 2.5%.
6. The method of claim 5, wherein the dopant is a Group III-V element.
7. The method of claim 6 , wherein the dopant is one or more of carbon or boron.
8. The method of claim 1 , wherein the doped silicon layer comprises a dopant in the range of 0.5 to 2.5%.
9. The method of claim 1 , wherein each of the first doped SiGe layer, the second doped SiGe layer, and the doped silicon layer is epitaxially grown.
10. 10. The method of claim 9, wherein each of the first doped SiGe layer, the second doped SiGe layer, and the doped silicon layer is independently grown at a temperature in the range of 500°C to 800°C.
11. 2. The method of claim 1 , wherein a stress of the second doped SiGe layer is more tensile than a stress of the first doped SiGe layer, and the stress of the first doped SiGe layer is more tensile than a stress of the doped silicon layer.
12. The method of claim 1 , wherein the wafer warps by an amount less than 150 μm when 100 film stacks are present.
13. 2. The method of claim 1 , wherein the first doped SiGe layer, the second doped SiGe layer, and the doped silicon layer each have an etch selectivity of greater than 200:1 relative to other layers when using a halide-based etchant.
14. 10. The method of claim 1, further comprising: lithographically forming a channel through all of the stacks to the substrate surface; and selectively etching one or more of the first doped SiGe layer or the second doped SiGe layer through the channel from all of the film stacks.
15. 1. A method of fabricating a 3D DRAM device, the method comprising: forming at least 100 film stacks on a substrate surface, each of the film stacks comprising: Empirical formula: Si 1-x Ge x where x is in the range of >0 to 0.5; and a second doped SiGe layer on the first doped SiGe layer, the second doped SiGe layer having an empirical formula of Si 1-y Ge y a second doped SiGe layer, where y is in the range of >0 to 0.5, and the first doped SiGe layer and the second doped SiGe layer have one or more of different doping amounts or different Si:Ge ratios; a doped silicon layer on the second doped SiGe layer; and forming, forming a channel through the film stack to the substrate; selectively removing one or more of the first doped SiGe layer or the second doped SiGe layer through the channel; A method comprising:
16. 16. The method of claim 15, wherein the first doped SiGe layer, the second doped SiGe layer, and the doped silicon layer independently comprise a dopant in the range of 0.5 to 2.5%.
17. 16. The method of claim 15, wherein each of the first doped SiGe layer, the second doped SiGe layer, and the doped silicon layer is epitaxially grown.
18. 16. The method of claim 15, wherein a stress of the second doped SiGe layer is more tensile than a stress of the first doped SiGe layer, and the stress of the first doped SiGe layer is more tensile than a stress of the doped silicon layer.
19. The method of claim 1 , wherein the wafer warps by an amount less than 150 μm when 100 film stacks are present.
20. 1. A method for fabricating a 3D DRAM device with reduced wafer bow, the method comprising: forming at least 100 film stacks on a substrate surface, each of the film stacks comprising: Empirical formula: Si 1-x Ge x where x is in the range of >0 to 0.5; and a second doped SiGe layer epitaxially grown on the first doped SiGe layer, the second doped SiGe layer having an empirical formula of Si 1-y Ge y an epitaxially grown second doped SiGe layer, where y is in the range of >0 to 0.5, and the first doped SiGe layer and the second doped SiGe layer have one or more of different doping amounts or different Si:Ge ratios; a doped silicon layer epitaxially grown on the second doped SiGe layer; and Including, the first doped SiGe layer, the second doped SiGe layer, and the doped silicon layer independently comprise a dopant selected from carbon or boron in the range of 0.5-2.5%; a stress of the second doped SiGe layer is more tensile than a stress of the first doped SiGe layer, the stress of the first doped SiGe layer being more tensile than a stress of the silicon layer; forming the first doped SiGe layer, the second doped SiGe layer, and the doped silicon layer, each of which has an etch selectivity relative to other layers of greater than 200:1 when using a halide-based etchant; forming a channel through all of the stacks to the substrate surface by lithography; selectively etching one or more of the first doped SiGe layer or the second doped SiGe layer from all of the film stack through the channel; A method comprising:
Citation Information
Patent Citations
Semiconductor wafer and method for manufacturing semiconductor device
JP2007036134A
Semiconductor device and method for manufacturing the same
JP2010225694A
Nonvolatile semiconductor memory device and method for manufacturing same
JP2011060991A
Crystalline layer stack for forming conductive layers in a three-dimensional memory structure
US20160268209A1
Semiconductor devices comprising multiple channels and method of making same
US20170025314A1
Cited By
Substrate processing method and substrate processing device
WO2026191615A1