Window Cavity Wafer
Separate fabrication of window and spacer wafers before bonding, with pre-metallization and optical coating, addresses the high cost and defect issues in WCW production, enhancing efficiency and versatility.
Patent Information
- Application Number
- JP2024520691
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-10-05
- Filing Date
- 2022-10-04
- Publication Date
- 2024-10-23
AI Technical Summary
Current window cavity wafer (WCW) fabrication is costly due to multiple operations like metallization, patterning, and coating, which are complicated by the non-planar nature of the cavity surface, leading to high defect rates and waste.
A method involving separate fabrication of window and spacer wafers, followed by metallization and optical coating before bonding, allowing for a more efficient and defect-reduced process.
This approach reduces costs and improves yield by minimizing defects in optical coatings, enabling a wider range of cavity depths and material combinations, and avoiding incompatibilities with lithography chemistries.
Smart Images

Figure 2024538687000001_ABST
Abstract
Description
[Background technology]
[0001] (Related Applications) This international application claims the benefit of U.S. Provisional Application No. 63 / 252,327, filed October 5, 2021, which is incorporated by reference in its entirety.
[0002] Current window cavity wafers (WCW) are made from two wafers (such as silicon). One wafer is called the spacer wafer and the other wafer is called the window wafer. One or both wafers are oxidized and then the two wafers are bonded together to form a void-free oxide bond. The bonded wafer is an example of a silicon-on-insulator (SOI) bonded wafer.
[0003] The preferred method for drilling cavities into the spacer wafer is Deep Reactive Ion Etching, or DRIE, also known as the Bosch process. DRIE uses special AC plasma chemistry to etch Si with vertical sidewalls. Vertical sidewalls (anisotropic etching) are important to minimize the waste of xy area between cavities. The width of the web between the cavities must be maximized, which is achieved by DRIE of cavities with vertical sidewalls. The DRIE plasma chemistry is designed to stop etching when the cavity depth reaches the buried oxide layer, which acts as an etch stop. Thus, DRIE is used to etch cavities that are 100-500 μm deep as set by the thickness of the spacer wafer.
[0004] The top flat areas between the cavities must be metallized to support solder bonding of the WCW to the microbolometer / readout integrated circuit (ROIC) wafer. The metallization is in the form of a rectangular frame located just outside the boundary of each cavity. The metal can be a component of the solder formed during wafer bonding, the metal can be the solder itself, or the metal can be used for diffusion bonding to a matching metal frame on the ROIC wafer.
[0005] The total number of these numerous operations adds up to a significant cost for the WCW wafer, typically at least $1,400.00 per 200 mm WCW wafer. This is the cost of the input WCW, which must then be pattern coated with anti-reflective and blocking (long pass) coatings, followed by a getter thin film pattern coated in the cavity. The non-planar nature of the WCW cavity surfaces makes it difficult to pattern deposit the AR and blocking coatings and getter coatings, as the cavities make it more difficult to deposit, pattern, and lift off photoresist. The difficulty in treating the cavity surfaces leads to higher levels of defects in and on the AR and blocking coatings. Defects in the AR and blocking coatings are highly undesirable. Due to the high cost of the WCW input wafers, it is very costly to discard a WCW wafer due to defects in the AR and blocking coatings. Summary of the Invention [Means for solving the problem]
[0006] Provided herein is a window cavity wafer comprising a window wafer including a window wafer substrate and one or more optical coatings disposed on one or more sides of the window wafer substrate. The window cavity wafer also comprises a spacer wafer including a spacer wafer substrate. The spacer wafer is wafer bonded to the window wafer to form the window cavity wafer. The window cavity wafer includes a metal frame.
[0007] Provided herein is a method of forming a window cavity wafer, comprising fabricating a window wafer by providing a window wafer substrate having two sides, etching alignment features on one or more sides of the window wafer substrate, and applying one or more optical coatings on one or more sides of the window wafer substrate. The method further comprises fabricating a spacer wafer separate from the window wafer by providing a spacer wafer substrate having two sides and forming an array of through holes in the spacer wafer substrate. The method also includes bonding the spacer wafer to the window wafer to form a window cavity wafer, and forming a separate metal frame on the side of the window cavity wafer.
[0008] Also provided herein is a method of forming a window cavity wafer, comprising fabricating a window wafer by providing a window wafer substrate having two sides, etching one or more sides of the window wafer substrate, and applying one or more optical coatings onto one or more sides of the window wafer substrate. The method further comprises fabricating a spacer wafer separate from the window wafer by providing a spacer wafer substrate having two sides and forming a cavity on a side of the spacer wafer substrate. The method also includes bonding the spacer wafer to the window wafer to form the window cavity wafer, and forming a separate metal frame on the side of the window cavity wafer. [Brief description of the drawings]
[0009] The following is a brief description of the drawings, which are presented for the purpose of illustrating the exemplary embodiments disclosed herein, and not for the purpose of limiting them.
[0010] [Figure 1] FIG. 1 is a cross-sectional view of an exemplary embodiment of a window cavity wafer according to the present disclosure.
[0011] [Diagram 2] FIG. 2 is a cross-sectional view of an exemplary embodiment of a window wafer that constitutes a portion of the window cavity wafer of FIG.
[0012] [Diagram 3] 3A-3C each diagrammatically show a cross-sectional view of a spacer wafer that may form part of the window cavity wafer of FIG.
[0013] [Figure 4] FIG. 4 is a perspective view illustrating an example of wafer bonding between a window wafer and a spacer wafer to form a window cavity wafer according to the present disclosure.
[0014] [Diagram 5] FIG. 5 is a process flow diagram illustrating an exemplary implementation of a wafer-level processing (WLP) method for producing a window cavity wafer according to the present disclosure.
[0015] [Figure 6] 6A and 6B are flow diagrams illustrating an example implementation of a method for fabricating a window wafer according to the present disclosure.
[0016] [Figure 7-1] 7A-7E are flow diagrams illustrating an example implementation of a method for fabricating a spacer wafer according to the present disclosure. [Figure 7-2] 7A-7E are flow diagrams illustrating an example implementation of a method for fabricating a spacer wafer according to the present disclosure.
[0017] [Figure 8] FIG. 8 is a flow diagram illustrating an example implementation of a method for forming a window cavity wafer as shown in FIG. 1 by combining a window wafer and a spacer wafer, each fabricated according to the methods of FIGS. 6A-6B and 7A-7E, respectively, of the present disclosure.
[0018] [Figure 9] 9A-9C are cross-sectional views illustrating steps for forming a window cavity wafer by combining a window wafer and a spacer wafer, each of which is fabricated separately, in accordance with the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] A more complete understanding of the processes and apparatus disclosed herein can be obtained by reference to the accompanying drawings, which are schematic representations based merely on the convenience and ease of demonstrating existing technology and / or the present developments, and as such are not intended to indicate the relative sizes and dimensions of the assemblies or their components.
[0020] Although specific terms are used in the following description for the sake of clarity, these terms are intended to refer only to the particular structures of the embodiments selected for illustration in the drawings, and are not intended to define or limit the scope of the present disclosure. In the drawings and description below, it should be understood that like numerical designations refer to components of similar function.
[0021] The singular forms "a," "an," and "the" include plural referents unless the context clearly dictates otherwise.
[0022] As used herein and in the claims, the terms "comprise(s)," "include(s)," "having," "has," "can," "contain(s)," and variations thereof, as used herein, are intended to be open-ended transitional phrases, terms, or words that require the presence of the recited ingredients / steps and allow for the presence of other ingredients / steps. However, such descriptions should also be construed as describing compositions or processes as "consisting of" and "consisting essentially of the enumerated ingredients / steps," which allows for the presence of only the recited ingredients / steps, along with any unavoidable impurities that may result therefrom, and excludes other ingredients / steps.
[0023] Numerical values in the specification and claims of this application should be understood to include numerical values that are identical when reduced to the same number of significant digits, and numerical values that differ from the stated value by less than the experimental error of conventional measurement techniques of the type described herein to determine the value.
[0024] All ranges disclosed herein are inclusive of the recited endpoints and are independently combinable (e.g., the range "2 grams to 10 grams" includes the endpoints, 2 grams and 10 grams, and all intermediate values).
[0025] The modifier "about" used in connection with a quantity is inclusive of the stated value and has the meaning dictated by context (e.g., it includes at least the degree of error associated with measurement of the particular quantity). When used in conjunction with a specific value, it should also be considered to disclose that value. For example, the term "about 2" also discloses the value "2," and the range "from about 2 to about 4" also discloses the range "from 2 to 4."
[0026] The present disclosure provides, as a first step, an anti-reflection (AR) and / or long-pass blocking coating to be pattern-deposited on a window wafer having two planar sides. As an example, the window wafer can comprise a double-sided polished planar Si wafer with a front side and a back side. The cavity can be formed as a later step by wafer bonding a perforated spacer wafer having a thickness that is approximately the depth of the cavity. The present disclosure is also applicable / compatible with a variety of alternative window wafers (e.g., Si, Ge, glass, sapphire) and matching perforated spacer wafers (e.g., Si, glass, sapphire, ceramic, metal alloys) since the wafer bonding materials and methods can be tailored to the materials used for the window and spacer.
[0027] The fabrication method disclosed herein includes a novel sequence of operations that results in a window cavity wafer. Conventionally, fabrication of a window cavity wafer includes processing a silicon-on-insulator (SOI) bonded wafer in the following order: metallization of the frame in a grid pattern; then patterned deep reactive ion etching (DRIE) to create cavities in the wafer; then patterned deposition of an AR / barrier coating; and patterned deposition of a getter thin film. In the present disclosure, fabrication of the patterned AR / barrier coating on the window wafer occurs first, and then bonding of a metallized perforated spacer wafer to create an array of cavities follows. Getter deposition is performed on the window cavity wafer as a final step. As will be appreciated, the present technique provides a higher yield at a lower cost than conventional techniques.
[0028] The present disclosure offers numerous technical advantages, including, but not limited to: reduced cost and improved yield; a wider range of cavity depths; no incompatibility with lithography chemistries; and a wider range of window and spacer material combinations.
[0029] (Device / Equipment)
[0030] 1, an exemplary embodiment of a window cavity wafer (WCW) 100 is shown. The window cavity wafer 100 can include a window wafer 110 and a spacer wafer 130, each of which is individually fabricated and processed. At a later stage, the window wafer 110 and the spacer wafer 130 are bonded together, generally as represented by bond line 144, thereby resulting in the window cavity wafer 100.
[0031] 1-4, the window wafer 110 can include a window wafer substrate 112 and one or more optical coatings 114 and 116 disposed on the window wafer substrate 112. The window wafer substrate 112 can be double-sided (i.e., having a front side and a back side) and has two generally planar sides. In some embodiments, the window wafer substrate 112 can have a thickness between 300 μm and 1,000 μm and can be generally transparent to infrared light. As illustrative examples, the window wafer substrate 112 can include silicon (Si), germanium (Ge), glass (e.g., borofloat glass), and sapphire. In some embodiments, the window wafer substrate 112 can include a double-sided polished 200 mm (8 inch diameter) Si wafer having a thickness between 300 μm and 1,000 μm, such as about 400 μm. In another embodiment, the window wafer substrate 112 may include a double-sided polished 200 mm wafer of Borofloat 33 glass (eg, borosilicate glass, etc.) having a thickness between 300 μm and 1,000 μm.
[0032] One or more optical coatings 114 and 116 can be disposed on the window wafer substrate 112. The optical coating 114 is disposed over a front surface (i.e., front side) of the window wafer substrate 112, and the optical coating 116 is disposed over a rear surface (i.e., rear side) of the window wafer substrate 112. As illustrative examples, the optical coatings 114 and 116 can include an anti-reflective (AR) coating, an optical filter coating, or a blocking coating. Optionally, a diamond-like carbon (DLC) coating 118 can be disposed over the optical coating 116 on the rear side of the window wafer substrate 112.
[0033] In some embodiments, the window wafer substrate 112 is made of Si and includes an optical coating 116 (comprising a long-pass infrared (LWIR) optical coating) formed on its rear side and an optical coating 114 (comprising an LWIR AR coating) formed on its front side. In some embodiments, the window wafer 110 can optionally include a diamond-like carbon (DLC) coating 118 disposed over the optical coating 116, such as an AR coating, to prevent the optical coating 116 from being scratched during a subsequent wafer bonding process. In other embodiments, each of the optical coatings 114 and 116 on the respective front and rear sides of the Si window wafer substrate 112 includes an AR coating in the long-pass infrared (e.g., an LWIR AR coating) and a blocking coating. In yet another embodiment, the window wafer substrate 112 is made from Borofloat 33 glass and includes an optical coating 116 (e.g., a visible, near infrared (NIR), or short wave infrared (SWIR) AR coating or filter) formed on its rear side and an optical coating 114 (e.g., a visible, NIR or SWIR AR coating) formed on its front side.
[0034] The spacer wafer 130 can include a spacer wafer substrate 132 and one or more metal layers 134 and 136 (e.g., a seed layer (or stack) or an electroplated layer) disposed on the spacer wafer substrate 132. In some embodiments, a glass layer 142 can be disposed on the spacer wafer substrate 132. The spacer wafer 130 can be a perforated spacer wafer.
[0035] The spacer wafer substrate 132 can be double-sided (i.e., having a front side and a back side) and has two sides. In some embodiments, the spacer wafer substrate 132 can have a thickness between 100 μm and 700 μm, and in certain embodiments, can have a thickness between 100 μm and 500 μm. As illustrative examples, the spacer wafer substrate 132 can include glass, sapphire, ceramic, or a metal alloy. In some embodiments, the spacer wafer substrate 132 can include a double-sided polished 200 mm (8 inch diameter) Si wafer having a thickness between 100 μm and 700 μm. In some embodiments, the Si wafer can have a thickness between 100 μm and 500 μm, such as, for example, about 200 μm. In other embodiments, the spacer wafer substrate 132 can include a double-sided polished 200 mm borosilicate glass wafer or a perforated Invar wafer.
[0036] One or more metal layers 134 and 136 can be disposed on the spacer wafer substrate 132. In some embodiments, the metal layers 134, 136 can include a seed layer stack disposed on the back side of the spacer wafer substrate 132 (e.g., 136 in FIG. 3A) and / or a seed layer stack disposed on the front side of the spacer wafer substrate 132 (e.g., 134 in FIGS. 3A-3C). As illustrative examples, a standard seed layer stack can include Cr+Ni+Au or Ti+Pt+Au. In some embodiments, a top layer of sputtered gold (Au) in the seed layer stack can have a thickness of 100 nm to 300 nm to minimize costs. In other embodiments, the metal layers 134, 136 can include an electroplated layer of Ni (e.g., a wafer of Invar) disposed on the spacer wafer substrate 132. In those embodiments, the plated Ni layer can have a thickness of 1 to 2 μm.
[0037] In some embodiments, the spacer wafer 130 may further include a metal plating layer 138 disposed over the seed layer stack (e.g., 136 in FIGS. 1 and 3A) on the rear side of the spacer wafer substrate 132. The rear side of the spacer wafer substrate 132 may be electroplated with gold to a thickness of 1-4 μm to form the plating layer 138. In other embodiments, the spacer wafer 130 may further include a metal plating layer 138 (e.g., gold) having a thickness of 1-10 microns disposed over the plated Ni metal layer 136 on the rear side of the spacer wafer substrate 132.
[0038] In some embodiments, the spacer wafer 130 may further include a metal plating layer 140 disposed over the seed layer stack (e.g., 134 in FIG. 1 ) on the front side of the spacer wafer substrate 132. The front side of the spacer wafer substrate 132 may be electroplated with gold to a thickness of 1-4 μm to form the plating layer 140. In other embodiments, the spacer wafer 130 may further include a metal plating layer 140 (e.g., gold) having a thickness of 1-10 microns disposed over the plated Ni metal layer 134 on the rear side of the spacer wafer substrate 132.
[0039] In some embodiments, the glass layer 142 can be disposed on the spacer wafer substrate 132, as shown in Figure 3B. In these embodiments, a glass layer 142, such as a borosilicate glass (e.g., similar to Corning 7740), can be disposed on the spacer wafer substrate 132 (e.g., a Si wafer). The glass layer 142 can have a thickness of 3 μm to 10 μm.
[0040] 4, there is an example of wafer bonding between a window wafer 110 and a spacer wafer 130. The spacer wafer 130 is perforated. An array of cavities can be established by wafer bonding the window wafer 110 to the perforated spacer wafer 130, the perforated spacer wafer 130 having a thickness that is approximately the depth of the cavities. Various types of wafer bonding can be implemented in accordance with the present disclosure, including, but not limited to, one or more of anodic bonding, solder bonding (e.g., eutectic bonding), and laser bonding.
[0041] Under conventional techniques, cavities are excavated by DRIE. As a result, as the cavity depth increases, the cost and difficulty of creating an acceptable cavity increases. When excavating using DRIE, it is important that the sidewalls of the cavity are approximately vertical to minimize the consumption of lateral (xy) footprint.
[0042] The present disclosure recognizes advantages to increasing the cavity depth, such as reducing the sensitivity of the microbolometer array to defects in the AR coating on the window wafer that appear as "crop circle" defects in the images. In the present disclosure, the cavity depth is controlled by the thickness of the drilled spacer wafer 130, which may range from 100 μm to 700 μm, with minor differences in cost based on thickness. In some embodiments, the thickness of the drilled spacer wafer 130 may be 100 μm to 500 μm. For spacer wafers 130 made from materials such as glass, Si, and metal, cost can be minimized by creating through holes with wet chemicals, by laser or ultrasonic machining, or by abrasive polishing. A standard wafer bonder can align two 200 mm wafers at high temperature with an accuracy of ±1 μm prior to solder or anodic bonding. Thus, the present disclosure advantageously provides a greater range of cavity depths than conventional techniques and related structures.
[0043] (method)
[0044] The following is a description of an exemplary implementation of method 500 (FIG. 5) by which the exemplary window cavity wafer 100 of FIG. 1 as well as other window cavity wafers may be reliably and efficiently manufactured in large quantities using wafer level packaging (WLP) techniques disclosed herein. As illustrated in a top-level overview of the method in FIG. 5, in one implementation, the exemplary method 500 may begin at stage or step 1 (S1) with fabrication of a "window wafer" (e.g., 110 in FIG. 1) and at S2 with fabrication of a "spacer wafer" (e.g., 130 in FIG. 1), as described in further detail below. The method then proceeds at S3 with a WLP process that combines two wafers (e.g., window wafer 110 and spacer wafer 130 in FIG. 1) into an assembly and processes the assembly (e.g., through wafer bonding), which results in a "window cavity wafer" (e.g., 100 in FIG. 1).
[0045] The method provided herein advantageously provides a window cavity wafer that can be made from a wider range of window and spacer wafer material combinations. Because the window and spacer wafers are fabricated separately before being bonded together by wafer bonding at a later stage, a wider range of window and spacer wafer material combinations are available. Thus, the method disclosed herein provides an advantage over conventional techniques that require one-sided anisotropic etching of cavities into the bonded wafers (thereby limiting the window wafer to Si or glass).
[0046] For example, in one non-limiting example, the present disclosure provides a Si window wafer to be bonded to a Si, glass, or metal perforated spacer wafer for wafer level packaging of near infrared (NIR), mid-wave infrared (MWIR), and long-wave infrared (LWIR) detectors with focal plane arrays. In another non-limiting example, the present disclosure provides a silicate glass window wafer to be bonded to a Si, glass, or metal perforated spacer wafer for wafer level packaging of UV, visible, and NIR detectors with focal plane arrays. In another non-limiting example, the present disclosure provides a sapphire window wafer to be bonded to a glass, ceramic, or metal perforated spacer wafer for wafer level packaging of UV, visible, NIR, and short-wave infrared (SWIR) detectors with focal plane arrays. In another non-limiting example, the present disclosure provides a germanium (Ge) window wafer to be bonded to a glass, ceramic, or metal perforated spacer wafer for wafer level packaging of NIR, SWIR, MWIR, and LWIR detectors with focal plane arrays. In yet another non-limiting example, the present disclosure provides a chalcogenide glass window wafer to be bonded to a glass, ceramic, or metal perforated spacer wafer for wafer level packaging of NIR, MWIR, and LWIR detectors and focal plane arrays.
[0047] As illustrated in detail in Figures 6-8, the exemplary WLP method 500 includes two methods, namely, "window wafer" fabrication methods 600A and 600B and "spacer wafer" fabrication methods 700A-700E, the products of which are combined into a third "window cavity wafer assembly and bonding" method 800. The various steps depicted in Figures 6-8 are described in detail below with respect to one or more embodiments.
[0048] In one non-limiting exemplary implementation, Figures 6A, 7A, and 8 collectively provide a flow diagram illustrating a Si window wafer and a Si spacer wafer, each of which is fabricated separately and then bonded together at a later stage through solder bonding (e.g., eutectic bonding) to form a window cavity wafer. In another non-limiting exemplary implementation, Figures 6A, 7B, and 8 collectively provide a flow diagram illustrating a Si window wafer and a Si spacer wafer, each of which is fabricated separately and then bonded together at a later stage through anodic bonding to form a window cavity wafer. In yet another non-limiting exemplary implementation, Figures 6A, 7C, and 8 collectively provide a flow diagram illustrating a Si window wafer and a glass spacer wafer, each of which is fabricated separately and then bonded together at a later stage through anodic bonding to form a window cavity wafer. In another non-limiting exemplary implementation, Figures 6A, 7D, and 8 collectively provide a flow diagram illustrating a Si window wafer and an Invar 36 spacer wafer, each of which are fabricated separately and then bonded together at a later stage through solder bonding (e.g., eutectic bonding) or alternatively through diffusion bonding to form a window cavity wafer. In yet another non-limiting exemplary implementation, Figures 6B, 7E, and 8 collectively provide a flow diagram illustrating a Borofloat 33 glass window wafer and a Si spacer wafer, each of which are fabricated separately and then bonded together at a later stage through anodic bonding to form a window cavity wafer. In yet another non-limiting exemplary implementation, Figures 6A, 7E, and 8 collectively provide a flow diagram illustrating a Si window wafer and a Si spacer wafer, each of which are fabricated separately and then bonded together at a later stage through laser bonding to form a window cavity wafer. Figures 6A, 7C, and 8 collectively provide a flow diagram illustrating a Si window wafer and a glass spacer wafer, each of which are fabricated separately and then bonded together at a later stage through laser bonding to form a window cavity wafer. In yet another non-limiting exemplary implementation, Figures 6B, 7E, and 8 collectively provide a flow diagram illustrating a borofloat 33 glass window wafer and a Si spacer wafer, each of which are fabricated separately and then bonded together at a later stage through laser bonding to form a window cavity wafer. In yet another non-limiting exemplary implementation, Figures 6B, 7C, and 8 collectively provide a flow diagram illustrating a borofloat 33 glass window wafer and a glass spacer wafer, each of which are fabricated separately and then bonded together at a later stage through laser bonding to form a window cavity wafer.
[0049] 6A and 6B, there is a flow diagram illustrating an example implementation of methods 600A and 600B for fabricating a window wafer (eg, 110 in FIG. 2).
[0050] Referring initially to FIG. 6A, at 602A, a double-sided (i.e., front and back) window wafer substrate (e.g., 112 in FIG. 2) having two planar sides is provided. In this implementation, the window wafer substrate (e.g., 112 in FIG. 2) comprises a double-sided polished 200 mm Si wafer having a thickness of 300 μm to 1,000 μm. In other implementations, the window wafer substrate (e.g., 112 in FIG. 2) may comprise Ge, glass, or sapphire. At 604A, the Si wafer may be etched with shallow (less than 5 μm deep) fiducial (alignment) marks and source streets by wet or dry etching on one or both of the sides (i.e., front and back) of the Si wafer. The features to be etched may be defined by using lithography.
[0051] In 606A, one or more coatings (e.g., 114 and 116 in FIG. 2), such as an AR coating and a blocking coating, can be applied to the front and back sides of the Si wafer. In some implementations, the back side of the Si wafer can be blanket coated with a long-pass LWIR optical coating, while the front side of the Si wafer can be coated with an LWIR AR coating in a rectangular (e.g., or other shape) 2D array defined by lift-off lithography. In these implementations, an optional diamond-like carbon (DLC) coating (e.g., 118 in FIG. 2) can be deposited over the LWIR coating on the back side of the Si wafer.
[0052] In other implementations, both the front and back sides of the Si wafer are coated with an AR coating in the LWIR and a blocking coating with a wavelength kerf of 7-8 microns. In those implementations, the back side of the window wafer substrate is blanket coated with these AR and blocking coatings, while the front side of the window wafer substrate includes these coatings in a rectangular (e.g., or other shape) 2D array defined by lift-off lithography. In those implementations, an optional diamond-like carbon (DLC) coating (e.g., 118 in FIG. 2) can be deposited over the blanket LWIR AR coating on the back side of the Si wafer to prevent the coating from scratching during the subsequent two-wafer bonding process.
[0053] In 608A, the fabricated Si window wafer (e.g., 110 in FIG. 2) can be inspected for defects. For example, after the lift-off process, the front side of the window wafer (e.g., 110 in FIG. 2) can be inspected to ensure that all bare Si streets between the rectangles of AR coating are intact and free of any coating or photoresist residue. In another example, the arrays of AR and barrier coatings on both sides of the window wafer can be inspected for defects such as scratches, digs, and / or particles. If the window wafer is found to have too high a density or number of defects in the optical coating, the window wafer can either be discarded or stripped, repolished, and then reused. Thus, only if the quality and yield of the patterned AR, filter, and / or barrier coatings is high enough, further unit operations (i.e., bonding to a perforated spacer wafer, which may be a metallized perforated spacer wafer) will be performed on this planar window wafer.
[0054] Referring to FIG. 6B, at 602B, a double-sided (i.e., front and back) window wafer substrate (e.g., 110 in FIG. 2) having two planar sides is provided. In this implementation, the window wafer substrate (e.g., 110 in FIG. 2) is a double-sided polished 200 mm wafer of Borofloat 33 glass (e.g., borosilicate float glass, etc.) having a thickness of 300 μm to 1,000 μm. At 604B, the Borofloat 33 glass wafer can be etched with shallow (less than 5 μm deep) fiducial marks and source streets by wet or dry etching on one or both of the sides (i.e., front and back) of the Borofloat 33 glass wafer. In this implementation, the etched features can be defined by using lithography. In other implementations, the fiducial marks can be created by laser.
[0055] At 606B, one or more coatings (e.g., 114 and 116 in FIG. 2), such as an AR coating and an optical filter coating, can be applied to the front and back sides of the Borofloat 33 glass wafer. In some implementations, the back side of the Borofloat 33 glass wafer can be blanket coated with a visible, near infrared (NIR) or shortwave infrared (SWIR) AR coating or filter, while the front side of the Borofloat 33 glass wafer can be coated with a visible, NIR, or SWIR AR coating in a rectangular (e.g., or other shape) 2D array defined by lift-off lithography.
[0056] In 608B, the fabricated Borofloat 33 glass wafer (e.g., 110 in FIG. 2) can be inspected for defects. For example, after the lift-off process, the front side of the Borofloat 33 glass wafer (e.g., 110 in FIG. 2) can be inspected to ensure that all the streets between the rectangles of the AR coating are intact and free of any coating or photoresist residue. In another example, the arrays of AR and filter coatings on both sides of the window wafer can be inspected for defects such as scratches, digs, and / or particles. If the window wafer is found to have too high a density or number of defects in the optical coating, the window wafer can either be discarded or stripped, repolished, and then reused. Thus, only if the quality and yield of the patterned AR, filter, and / or blocking coatings is high enough, further unit operations (i.e., bonding to a perforated spacer wafer, which may be a metallized perforated spacer wafer) will be performed on this planar window wafer.
[0057] As disclosed herein, fabrication of the window wafer (e.g., 110 in FIG. 2) occurs prior to wafer bonding and metallization. Thus, any lithography steps required for deposition of AR and barrier coatings on the window wafer are completed prior to wafer bonding and metallization (if present). Advantageously, the present disclosure does not experience incompatibility with lithography chemicals since lithography chemicals are used prior to wafer bonding and metallization. Thus, the metallization is not exposed to lithography chemicals and does not experience any resulting corrosion from the lithography chemicals.
[0058] 7A-7E, there are flow diagrams illustrating example implementations of methods 700A, 700B, 700C, 700D, and 700E for fabricating a spacer wafer (eg, 130 in FIGS. 3A and 3B).
[0059] Referring to FIG. 7A, at 702A, a double-sided (i.e., front and back) spacer wafer substrate (e.g., 132 in FIG. 3A) having two sides is provided. In this implementation, the spacer wafer substrate (e.g., 132 in FIG. 3A) is a double-sided polished 200 mm Si wafer having a thickness of 100 μm to 700 μm, e.g., 100 μm to 500 μm. In other implementations, the spacer wafer substrate (e.g., 132 in FIG. 3A) may include glass, sapphire, ceramic, or metal alloy. At 704A, a standard seed layer stack (e.g., 134 and 136 in FIG. 3A) is blanket sputter deposited on both sides (e.g., front and back) of the Si wafer. The standard seed layer stack may include Cr+Ni+Au or Ti+Pt+Au. In some implementations, the sputtered gold (Au) top layer can have a thickness between 100 nm and 300 nm to minimize cost.
[0060] At 706A, an array of through-holes is formed in the Si spacer wafer according to a desired array. In some implementations, an array of rectangular through-holes is formed in the Si spacer wafer, although other shapes are contemplated by this disclosure. Methods for forming the through-holes are unencumbered by metallization on both sides of the spacer wafer substrate and can include wet etching, laser, water jet, or ultrasonic machining. At 708A, the back side of the spacer wafer is electroplated with gold to a thickness of 1 μm to 4 μm to form a plating layer (e.g., 138 in FIG. 3A), while the opposing front side is masked during electroplating.
[0061] Referring to FIG. 7B, at 702B, a double-sided (i.e., front and back) spacer wafer substrate (e.g., 132 in FIG. 3B) having two sides is provided. In this implementation, the spacer wafer substrate (e.g., 132 in FIG. 3B) is a double-sided polished 200 mm Si wafer having a thickness of 100 μm to 700 μm, e.g., 100 μm to 500 μm. In other implementations, the spacer wafer substrate (e.g., 132 in FIG. 3B) may include glass, sapphire, ceramic, or metal alloy. At 704B, a standard seed layer stack (e.g., 134 in FIG. 3B) is blanket metallized (e.g., sputter deposited) on the front side of the Si wafer. The standard seed layer stack may include Cr+Ni+Au or Ti+Pt+Au. In some implementations, the top layer of sputtered gold (Au) may have a thickness of 100 nm to 300 nm to minimize cost.
[0062] At 706B, an array of rectangular (e.g., or other shape) through-holes are formed in the Si spacer wafer in the desired array. Methods for forming the through-holes are unencumbered by metallization on one side of the spacer wafer substrate and can include wet etching, laser, water jet, or ultrasonic machining. At 708B, the backside of the spacer wafer is coated with a glass layer (e.g., 142 in FIG. 3B) such as borosilicate glass (e.g., similar to Corning 7740). In some non-limiting examples, the glass layer (e.g., 142 in FIG. 3B) can be deposited by evaporation, plasma-assisted evaporation (plasma-enhanced chemical vapor deposition), or sputtering to a thickness of 3 μm to 10 μm. The borosilicate glass contains a sufficient concentration of alkali ions (similar to Na+) to promote anodic bonding.
[0063] Referring to FIG. 7C, at 702C, a double-sided (i.e., front and back) spacer wafer substrate (e.g., 132 in FIG. 3A) having two sides is provided. In this implementation, the spacer wafer substrate (e.g., 132 in FIG. 3A) is a double-sided polished 200 mm borosilicate glass wafer having a thickness of 100 μm to 700 μm, e.g., 100 μm to 500 μm. It is advantageous that borosilicate glass has the same coefficient of thermal expansion (CTE) as silicon and a sufficient content of alkali ions to promote anodic bonding (e.g., Corning 7740 or Borofloat 33) when anodic bonding is used to bond the spacer wafer to the window wafer. At 704C, a standard seed layer stack (e.g., 134 in FIG. 3A) is blanket sputter deposited on the front side of the borosilicate glass wafer. The standard seed layer stack can include Cr+Ni+Au or Ti+Pt+Au. In some implementations, the sputtered gold top layer can have a thickness of 100 nm to 300 nm to minimize cost. It will be understood that metallization step 704C may not be included (i.e., is optional) if laser bonding is used to bond the spacer wafer to the window wafer (as direct laser bonding does not require a metal or metal seed layer for bonding).
[0064] At 706C, an array of rectangular (e.g., or other shaped) through-holes are formed in the glass spacer wafer in the desired array. Methods for forming the through-holes are unobstructed by the metallization on one side of the spacer wafer and can include wet etching, laser, water jet, or ultrasonic machining.
[0065] Referring to FIG. 7D, at 702D, a double-sided (i.e., front and back) spacer wafer substrate (e.g., 132 in FIG. 3A) having two sides is provided. In this implementation, the spacer wafer substrate (e.g., 132 in FIG. 3A) is a perforated wafer of Invar having a thickness of 100 μm to 700 μm, e.g., 100 μm to 500 μm. It is advantageous for the desired Invar alloy and temper to have a CTE as close as possible to that of Si. At 704D, one or more cavities are formed in the Invar by wet photoetching from both sides on the Invar sheet to keep the cavity sidewalls as vertical as possible.
[0066] At 706D, the Invar is electroplated with 1-2 microns of Ni to form a metal plating layer on both sides of the Invar (e.g., 134 and 136 in FIG. 3A), and then sintered to remove the plating salts. The Invar wafer is then masked on the front side so that the next electroplating step occurs only on the back side. At 708D, the back side of the Invar is then electroplated with Gold to a thickness of 1-10 microns to form a plating layer (e.g., 138 in FIG. 3A), while the opposite front side is masked during electroplating.
[0067] Referring to FIG. 7E, at 702E, a double-sided (i.e., front and back) spacer wafer substrate (e.g., 132 in FIG. 3A) having two sides is provided. In this implementation, the spacer wafer substrate (e.g., 132 in FIG. 3A) is a double-sided polished 200 mm Si wafer having a thickness of 100 μm to 700 μm, e.g., 100 μm to 500 μm. In other implementations, the spacer wafer substrate may include glass, sapphire, ceramic, or metal alloy. At 704E, a standard seed layer stack (e.g., 134 in FIG. 3A) is blanket metallized (e.g., sputter deposited) on the front side of the Si spacer wafer substrate. The standard seed layer stack may include Cr+Ni+Au or Ti+Pt+Au. In some implementations, the sputtered gold top layer may have a thickness of 100 nm to 300 nm to minimize cost. It will be understood that if laser bonding is used to bond the spacer wafer to the window wafer, then metallization step 704E may not be included (i.e., is optional) (as direct laser bonding does not require a metal or metal seed layer for bonding).
[0068] At 706E, an array of rectangular (e.g., or other shaped) through-holes are formed in the Si spacer wafer in the desired array. Methods for forming the through-holes are unobstructed by the metallization on one side of the Si spacer wafer and can include wet etching, laser, water jet, or ultrasonic machining.
[0069] 8, there is a flow diagram illustrating an example implementation of a method 800 of forming a window cavity wafer (e.g., 100 in FIG. 1) from a spacer wafer fabricated according to the method of FIGs. 7A-7E and a window wafer fabricated according to the method of FIGs. 6A and 6B. In particular, the "window cavity wafer", i.e., WCW, results from a spacer wafer that is hermetically bonded to a window wafer.
[0070] At 802, a spacer wafer (e.g., 130 in FIG. 1) is bonded to a window wafer (e.g., 110 in FIG. 1). In some implementations, the spacer wafer (fabricated by the method of FIG. 7A) and the window wafer (fabricated by the method of FIG. 6A) can be placed in a wafer bonder for vacuum bonding at 390-415° C. to form an Au / Si eutectic alloy between the back side of the spacer wafer and the front side of the window wafer. The Au / Si eutectic alloy bonds the spacer wafer and the window wafer together through an Au / Si eutectic bond. In other implementations, the spacer wafer (fabricated by the method of FIG. 7B-7C) and the window wafer (fabricated by the method of FIG. 6A) can be placed in a wafer bonder for anodic bonding at 390-450° C. in vacuum, where bonding occurs between Si and glass. In yet another implementation, the Invar spacer wafer (fabricated by the method of FIG. 7D) and the window wafer (fabricated by the method of FIG. 6A) can be placed in a wafer bonder for bonding at 390-450° C. to form AuSi solder between the Invar wafer and the window wafer. Alternatively, the matching streets on the window wafer can be coated with germanium (to form AuGe solder during bonding) or with electroplated gold (to form a gold-gold diffusion bond). In still another implementation, the bare silicon surface of the spacer wafer (fabricated by the method of FIG. 7E) and the patterned surface of the glass window wafer (fabricated by the method of FIG. 6B) are pressed together and then anodically bonded under vacuum at 350-400° C. In still another implementation, the Si spacer wafer (fabricated by the method of FIG. 7E) and the Si window wafer (fabricated by the method of FIG. 6A) are bonded together using direct laser bonding. It is conceivable that an infrared (IR) laser can be used to perform the laser bonding. In yet another implementation, a Si spacer wafer (fabricated by the method of FIG. 7E) and a glass window wafer (fabricated by the method of FIG. 6B) are bonded together using direct laser bonding.In yet another implementation, a glass spacer wafer (fabricated by the method of FIG. 7C) and a Si window wafer (fabricated by the method of FIG. 6A) are bonded together using direct laser bonding. In yet another implementation, a glass spacer wafer (fabricated by the method of FIG. 7C) and a glass window wafer (fabricated by the method of FIG. 6B) are bonded together using direct laser bonding.
[0071] It will be appreciated that bonding the window wafer to the spacer wafer via laser bonding offers many advantages. First, laser bonding can be performed at low temperatures, such as at room temperature, which advantageously mitigates heat-related damage to any previously formed optical coatings and other active layers. Thus, the window wafer and / or spacer wafer substrate can be coated prior to laser processing. Laser bonding offers minimal heat load since the heat-affected area (i.e., the laser processing area) is very small, e.g., only a few microns. In addition, low heating allows for the use of less bulk / material, and thus thinner materials. Second, direct laser bonding provides bonding between the spacer wafer and the window wafer without requiring additional materials, such as adhesives, and without leaving gaps between the window wafer and the spacer wafer. The absence of adhesives means there is no outgassing, and it will be further appreciated that direct laser bonding does not require metal or metal seed layers for bonding. It is conceivable that an infrared (IR) laser can be used as the laser light source to bond the Si spacer wafer to the Si window wafer.
[0072] It can be difficult to anodically bond glass wafers thinner than 400 μm (e.g., perforated borosilicate glass wafers) to silicon wafers without excessive warping and potential fracturing of the glass. Therefore, an alternative strategy is to temporarily bond the thin glass wafer to a silicon backing wafer to reduce or prevent warping and fracturing of the borosilicate glass wafer during anodic bonding. The adhesive between the thin glass wafer and the Si backing wafer can be easily removed after anodic bonding.
[0073] At 804, a verification of the bond between the spacer wafer and the window wafer is performed. In some implementations, the verification includes evaluating the Au / Si eutectic bond between the spacer wafer and the window wafer. In these implementations, a C-mode scanning acoustic microscope or an X-ray camera can be used to verify the low void Au / Si eutectic bond between the spacer wafer and the window wafer. In other implementations, the verification includes evaluating the anodic bond between the spacer wafer (e.g., comprising borosilicate glass) and the window wafer. In these implementations, a C-mode scanning acoustic microscope or an X-ray camera can be used to verify the void-free glass bond between the spacer wafer and the window wafer. In still other implementations, the verification includes evaluating the solder bond between the Invar spacer wafer and the window wafer. In these implementations, a C-mode scanning acoustic microscope or an X-ray camera can be used to verify the void-free solder bond between the Invar spacer wafer and the window wafer. In still other implementations, the verification includes evaluating the anodic bond between the spacer wafer (e.g., comprising Si) and the Borofloat 33 glass window wafer. In these implementations, a C-mode scanning acoustic microscope or an X-ray camera can be used to verify the low void anode bond between the spacer wafer and the window wafer.
[0074] At 806, separate metal frames suitable for wafer bonding are formed on the top surface (i.e., cavity side) of the WCW. In some implementations, each metal frame sits on the periphery of each cavity. In some implementations, the streets between the cavities can be electroplated with gold, gold-tin, or copper. At 808, a getter thin film is deposited inside the cavities of the WCW. In some non-limiting examples, the getter can be deposited by sputtering or evaporation through a shadow mask. The getter thin film can be configured to maintain a sufficient vacuum level despite degassing of the device by absorbing outgassed gases.
[0075] At 810, the WCW can be bonded to the ROIC / microbolometer wafer under vacuum by applying pressure and a temperature of 290-320° C. to form an array of gas-tight AuSn solder joints. Advantageously, the temperature treatment for AuSn solder formation and reflow will not cause reflow of the AuSi solder joints previously formed between the spacer wafer and the window wafer. The temperature required for AuSn solder formation and reflow will not reflow the anode glass joints previously formed between the Si spacer wafer and the window wafer. If the WCW is overplated with Cu, the WCW can be bonded to the ROIC / microbolometer wafer under vacuum by applying pressure and a temperature of 290-350° C. to form an array of gas-tight CuSn solder joints. The temperature required for CuSn solder formation and reflow will not cause reflow of the anode glass joints previously formed between the spacer wafer and the window wafer.
[0076] 9A-9C show steps for forming a window cavity wafer by laser bonding together a window wafer and a spacer wafer, each fabricated separately. In FIG. 9A, the window wafer 110 is positioned over the perforated spacer wafer 130. In FIG. 9B and 9C, encapsulated devices such as electrical components are positioned between the spaces in the perforated spacer wafer 130 and hermetically sealed therein by bonding of another wafer substrate 160 to the perforated spacer wafer 130, whereby the electrical components 150 are hermetically sealed between the window wafer 110, the spacer wafer 130, and the additional wafer substrate 160. Laser bonding of the spacer wafer 130 to the window wafer 110 is performed by laser processing at a laser processing location 170.
[0077] It will be understood that various of the above-disclosed and other features and functions, or alternatives thereof, may be desirably combined into many other different systems or applications, and it will be further understood that various presently unforeseen or unanticipated alternatives, modifications, variations, or improvements therein may subsequently be made by those skilled in the art, which are also intended to be covered by the following claims.
Claims
1. 1. A window cavity wafer, comprising: a window wafer comprising a window wafer substrate and one or more optical coatings disposed on one or more surfaces of the window wafer substrate; a spacer wafer including a spacer wafer substrate; Equipped with The spacer wafer is wafer bonded to the window wafer to form the window cavity wafer, the window cavity wafer including a metal frame.
2. The window cavity wafer of claim 1 , wherein the one or more optical coatings comprise one or more of an anti-reflective coating, an optical filter coating, and a long-pass blocking coating.
3. 10. The window cavity wafer of claim 1, wherein the window wafer substrate comprises one of silicon (Si), germanium (Ge), borofloat glass, and sapphire.
4. The window cavity wafer of claim 3, wherein the window wafer substrate has a thickness between 300 μm and 1,000 μm.
5. 10. The window cavity wafer of claim 1, further comprising a diamond-like carbon (DLC) coating disposed over one of the optical coating layers.
6. The window cavity wafer of claim 1 , wherein one or more metal layers are disposed on one or more surfaces of the spacer wafer substrate.
7. The one or more metal layers may comprise a seed layer stack, the seed layer stack comprising: (i) Cr+Ni+Au, or (ii) Ti+Pt+Au 7. The window cavity wafer of claim 6, comprising one of:
8. 10. The window cavity wafer of claim 1, wherein the spacer wafer substrate comprises one of glass, sapphire, ceramic, silicon (Si), and a metal alloy.
9. The window cavity wafer of claim 1 , wherein the spacer wafer substrate has a thickness between 100 μm and 500 μm.
10. The window cavity wafer of claim 1 , wherein said spacer wafer substrate is perforated.
11. The window cavity wafer of claim 6 further comprising a metal plating layer disposed over one of said metal layers.
12. The window cavity wafer of claim 1 further comprising a glass layer disposed on said spacer wafer substrate.
13. 10. The window cavity wafer of claim 1, further comprising a getter disposed inside the cavity of the window cavity wafer.
14. 1. A method of forming a window cavity wafer, the method comprising: Fabricating a window wafer, the fabricating of the window wafer comprising: Providing a window wafer substrate having two sides; Etching one or more sides of the window wafer substrate; applying one or more optical coatings onto one or more surfaces of the window wafer substrate; By, fabricating a spacer wafer separate from the window wafer, the fabricating of the separate spacer wafer comprising: Providing a spacer wafer substrate having two sides; forming an array of through holes in said spacer wafer substrate; By, bonding the spacer wafer to the window wafer to form the window cavity wafer; forming a separate metal frame on a surface of said window cavity wafer; A method comprising:
15. The method of claim 14 , further comprising depositing one or more metal layers on one or more surfaces of the spacer wafer substrate.
16. depositing a getter inside the cavity of said window cavity wafer; bonding said window cavity wafer to a readout integrated circuit; The method for forming a window cavity wafer of claim 15 further comprising:
17. The method of claim 14 , wherein the applied one or more optical coatings include one or more of an anti-reflective coating, an optical filter coating, and a long-pass blocking coating.
18. 15. The method of claim 14, wherein the provided window wafer substrate is one of silicon (Si), germanium (Ge), borofloat glass, and sapphire.
19. The method of claim 18, wherein the provided window wafer substrate has a thickness between 300 μm and 1,000 μm.
20. The method of claim 14 , further comprising depositing a diamond-like carbon (DLC) coating over one of the optical coating layers.
21. The method of claim 15 , wherein the deposited one or more metal layers comprise a seed layer stack.
22. The deposited seed layer stack comprises: (i) Cr+Ni+Au, or (ii) Ti+Pt+Au, 22. The method of claim 21, comprising one of:
23. 15. The method of claim 14, wherein the provided spacer wafer substrate comprises one of glass, sapphire, ceramic, and a metal alloy.
24. The method of claim 23, wherein the spacer wafer substrate has a thickness between 100 μm and 500 μm.
25. The method of claim 15 further comprising depositing a metal plating layer over one of the metal layers.
26. The method of claim 14 further comprising disposing a glass layer on one side of the spacer wafer substrate.
27. 1. A method of forming a window cavity wafer, the method comprising: Fabricating a window wafer, the fabricating of the window wafer comprising: Providing a window wafer substrate having two sides; Etching one or more sides of the window wafer substrate; applying one or more optical coatings onto one or more surfaces of the window wafer substrate; By, fabricating a spacer wafer separate from the window wafer, the fabricating of the separate spacer wafer comprising: Providing a spacer wafer substrate having two sides; forming a cavity on a surface of the spacer wafer substrate; By, bonding the spacer wafer to the window wafer to form the window cavity wafer; forming a separate metal frame on a surface of said window cavity wafer; A method comprising:
Citation Information
Patent Citations
Silicon optical package with 45°-reflecting mirror
JP2006324658A
Housing for infrared-emitting microdevices and method for manufacturing the housing.
JP2012530257A
Hermetically sealed package