Metal-filled resin formulations, 3D printing methods, and additively manufactured parts

A metal-filled resin formulation for 3D printing addresses the challenge of producing complex, thin-walled radiation-absorbing parts by using photopolymerization, achieving high precision and cost-effective manufacturing with improved part performance.

JP2024540250AActive Publication Date: 2024-10-31SIEMENS HEALTHINEERS AG +1
View PDF 14 Cites 0 Cited by

Patent Information

Application Number
JP2024525956
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-27
Filing Date
2022-10-25
Publication Date
2024-10-31
Estimated Expiration
2042-10-25

AI Technical Summary

Technical Problem

Conventional manufacturing methods struggle to produce complex, thin-walled radiation-absorbing parts cost-effectively, as they face challenges with mechanical strength and processing complexity, especially when using high-density metal fillers.

Method used

A metal-filled resin formulation based on photopolymerizable matrix components with high-density metal fillers is used in a 3D printing method, allowing layer-by-layer photopolymerization to create parts with precise geometries and high radiation absorption, using SLA or DLP techniques.

Benefits of technology

The method enables the production of ultra-fine, complex geometries with high radiation absorption and mechanical strength, offering improved part performance and cost-effective on-demand manufacturing of spare parts with high precision and surface quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024540250000001_ABST
    Figure 2024540250000001_ABST
Patent Text Reader

Abstract

The present invention relates to a metal-filled resin formulation for the production of parts, in particular for 3D printing methods, based on layer-by-layer photopolymerization, which contains a photopolymerizable matrix component, a dense metal filler with a specific minimum volume fraction, and a photopolymerization initiator. By selective layer-by-layer curing of the metal-filled resin formulation, the parts are additively produced using light irradiation. The present invention particularly relates to the high-precision production of radiation-absorbing parts based on lithographic additive methods such as SLA, where wall thicknesses of up to less than 100 μm are possible, despite good radiation hardness and good surface quality, based on the special selection of the formulations used.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a metal-filled resin formulation, in particular for a 3D printing method, as well as a 3D printing method in which such a metal-filled resin formulation is used to manufacture a part. The present invention also relates to a part manufactured using such a 3D printing method. The present invention is further directed to the additive manufacturing of three-dimensionally formed parts, in particular for absorbing electromagnetic radiation, such as X-ray radiation. [Background technology]

[0002] In several technical application fields, radiation absorbing materials and parts manufactured from them are increasingly used in a wide variety of and partly complex shapes. Lead, previously standard for such applications, has been successively replaced by other metals and polymer / metal composites. In the case of polymer / metal composites, today often a metal filler with high density or high atomic number (e.g. tungsten) is embedded in a thermoplastic matrix (e.g. polyamide). This material is typically processed into industrial parts using conventional polymer molding processes such as injection molding or extrusion (see for example US Pat. No. 5,393,633; US Pat. No. 5,493,623; and US Pat. No. 5,493,623).

[0003] With a higher percentage of metal fillers, a higher density and therefore a better part performance in terms of radiation absorption can be achieved, but in some cases, a reduction in mechanical strength must be accepted, which can make such materials difficult to process. Basically, with the above-mentioned conventional approaches, complex geometric shapes can only be realized at high cost and effort, if at all. However, with the increasing miniaturization or development of application fields, the demand for the manufacture of highly complex shapes with thin walls and high precision is increasing, and conventional molding methods are increasingly reaching their limits.

[0004] In generative or additive manufacturing methods, also commonly called 3D printing processes, one or more starting materials are successively deposited and hardened in layers on the basis of a digitized geometric model of the object. For example, in stereolithography (SL or SLA), the part is built up layer by layer from light-curable resin formulations (lichthaerbare Harzformulierung), for example acrylic, epoxy or vinylester resins. For this, the respective resin formulation is prepared in a bath in liquid form (typically with a viscosity in the range of <2 Pa·s) and hardened into a material (e.g. synthetic resin or composite material) in selected areas of the surface by polymerization with laser radiation, the so-called photopolymerization. After each step, the thin material layer thus formed is lowered a few millimeters into the liquid and returned to a position where it is one layer thick below the previous one. The liquid resin mixture on top of the material is then evenly distributed by a wiper or squeegee, after which the laser is again moved over the liquid surface, resulting in the step-by-step creation of a three-dimensional part.

[0005] 3D printing offers enormous design freedom and makes it possible to produce at a reasonable cost objects that could not be produced by conventional methods or that could only be produced at a considerable cost. For this reason, 3D printing methods are now very widespread in industrial design, medical technology, the automotive industry, the aerospace industry or in general industrial product development, where resource-efficient process chains are used for the demand-based small-scale and large-scale production of individualized parts, and in some cases also for the flexible, on-demand production of necessary spare parts.

[0006] For example, "Electronics for Laser Scanning Laser Beam Melting" (2003) describes the use of additive beam melting processes to fabricate thin collimator structures made of tungsten.

[0007] Certain additive manufacturing techniques, such as, for example, SLA, LCD (liquid crystal display) processes, digital light processing (DLP) or other light-emitting processes using active light masks, or combinations of these, are characterized by a surprisingly high precision and therefore offer particularly promising solutions for the production of ultra-fine feature components.

[0008] For example, US Pat. No. 5,999,366 describes a two-step process for producing a collimator made of tungsten, in which after the SLA step, a layer of radiation-absorbing metal is deposited on the polymeric layer by cathodic sputtering. This metal layer is then lifted off the SLA layer and retained as a layer part of the collimator. This procedure is repeated accordingly to produce the final collimator from tungsten as a layer process. However, directly producing a collimator from a radiation-absorbing material using SLA would be a substantially simplified and more economical process solution.

[0009] Furthermore, patent document 6 describes the use of colloids of polymer macromolecules in a solvent as a matrix material, into which metal particles can be mixed. In a productive manufacturing process, first a green part is produced using this material, which is then dried under the effect of temperature in a subsequent step.

[0010] US Patent No. 5,399,633 describes additive manufacturing of radiation absorbing and metal-containing radiological phantoms using lithographic processes, where nanometer-sized metal particles are used.

[0011] Patent document 8 describes a method for producing a dental prosthesis or restoration. Suitable photoinitiators for initiating the required photoreaction are described, for example, in Non-Patent Document 2. [Prior art documents] [Patent documents]

[0012] [Patent Document 1] German Patent Application Publication No. 102004027158 [Patent Document 2] US Patent Application Publication No. 2008 / 0023636 [Patent Document 3] German Patent Application Publication No. 102007028231 [Patent Document 4] International Patent Application Publication No. 2012 / 034879 [Patent Document 5] US Patent Application Publication No. 2020 / 0077966 [Patent Document 6] International Patent Application Publication No. 2020 / 198404 [Patent Document 7] International Patent Application Publication No. 2020 / 141519 [Patent Document 8] International Patent Application Publication No. 2019 / 048963 [Patent Document 9] International Patent Application Publication No. 2018 / 032022 [Patent Document 10] US Patent Application Publication No. 2020 / 0024394 [Non-patent literature]

[0013] [Non-Patent Document 1] ATSidambe et al. “Laser powder bed fusion of a pure tungsten ultra-fine single pinhole collimator for use in gamma ray detector characterization” International Journal of Refractory Metals and Hard Materials, Volume 84, 2019 [Non-Patent Document 2] W. Arthur Green “Industrial Photoinitiators: A Technical Guide” Taylor & Francis Group, 2010, ISBN: 978-1-2745-1 Summary of the Invention [Problem to be solved by the invention]

[0014] Against this background, the present invention is based on the problem of finding a precise and practical solution for the production of radiation-absorbing components, which preferably can be produced cost-effectively even with complex thin-walled structures. [Means for solving the problem]

[0015] According to the invention, this problem is solved by a metal-filled resin formulation (hereinafter also referred to as "metal-filled resin formulation") having the features of claim 1, a 3D printing method having the features of claim 9 and an additively manufactured part having the features of claim 11.

[0016] That is, the following solutions are proposed: - a metal-filled resin formulation, preferably radiation-absorbent, for layer-by-layer photopolymerization-based, in particular for 3D printing methods for the production of parts, the resin formulation comprising a photopolymerizable matrix component, the photopolymerizable matrix component comprising at least one of the monomers, oligomers and prepolymers from the group consisting of monofunctional and / or polyfunctional radically and / or cationic polymerizable compounds, and a metal filler, the metal filler having a density of at least 8.5 g / cm 3 , preferably at least 10 g / cm 3 the photopolymerizable matrix component has a volume fraction of 5 to 80 vol. %, preferably 5 to 70 vol. %, particularly preferably 5 to 60 vol. %, based on the total of the photopolymerizable matrix component and the metal filler, the metal filler has a volume fraction of 20 to 95 vol. %, preferably 30 to 95 vol. %, particularly preferably 40 to 95 vol. %, based on the total of the photopolymerizable matrix component and the metal filler, a photopolymerization initiator is included, which is adapted to the photopolymerizable matrix component and to the light wavelength used for the photopolymerization, the photopolymerization initiator has a content of 0.05 to 10 phr, preferably 0.1 to 5 phr, particularly preferably 0.3 to 3 phr, based on the photopolymerizable matrix component, and the metal filler comprises a fine particle fraction of less than 10% having a particle size of less than 1 micrometer. - a 3D printing method based on layer-by-layer photopolymerization for the production of parts, in particular radiation-absorbent parts, using a metal-filled resin formulation according to the invention, which comprises providing a metal-filled resin formulation in a production bath, on a production bed and / or as a wet layer, and selectively hardening the metal-filled resin formulation layer-by-layer by polymerization in the production bath, on the production bed and / or in the wet layer using selective light irradiation to form the part. - Additively manufactured parts, in particular radiation-absorbing parts, produced using the 3D printing method according to the invention.

[0017] The idea underlying the present invention is to incorporate high density metal materials into photocurable resin formulations and form the composites into virtually any complex part shape by a light-based and therefore particularly accurate additive method. For this purpose, the present invention uses metal-filled resin formulations, which integrate a polymerizable matrix component with one or more metal fillers. In this case, a photoinitiator initiates a rapid photoreaction, which gives the composite, in combination with the matrix component, sufficient green strength to maintain the desired shape fidelity during the 3D printing process and during post-processing. In this case, light irradiation can be applied directly to the surface of the resin formulation, or can be introduced into the resin formulation through a carrier medium transparent to light irradiation.

[0018] In addition to guaranteeing ultra-fine and complex geometries with wall or structure thicknesses in the 100 μm range and at the same time high resolution of up to 10 μm as well as the precision of 3D parts in printing methods with adequate surface quality, the cured composite is in a state in particular to be able to absorb radiation doses with energies in the keV range or even above at a specified wall thickness. This is achieved by the use of radiation-absorbing metals, which preferably have a density comparable to or greater than that of lead, reaching a filler content in the composite of at least 20% by volume. The resulting density of the photopolymerized composite is thus likewise sufficiently high, for example 4.5 g / cm. 3 It can also be set to a value greater than 0.

[0019] As a result, the effectiveness and performance of technical 3D parts produced in this way can also be significantly improved, for example, the directionality of light in radiation collimators is improved. The ability to quickly and efficiently mass-produce and provide replacement parts for new and existing applications is another major benefit of the 3D printing technology used. Here, light-based technology is particularly advantageous here, since it allows, due to its precision, to produce parts with a consistent surface quality compared to traditional manufacturing methods such as injection molding. This also brings the desired backward compatibility for the cost-efficient on-demand production of spare parts in existing fields of application.

[0020] Existing material solutions consist of metal-filled composites with the desired radiation absorption properties that can be produced by conventional methods and are based on a thermoplastic matrix. However, additive processing methods that can be used are limited to extrusion-based 3D printing methods (e.g. fused filament fabrication) or powder bed methods (e.g. laser powder bed fusion), which are significantly below the potential of light-based 3D printing techniques in terms of their achievable resolution or future size (achievable part resolution above 50 μm, minimum wall thickness above 150 μm). These limitations become even more pronounced, especially when composite materials are used.

[0021] Another advantage of producing composites via SLA-based techniques is the efficient use of materials, since all of the formulation that is not polymerized can be reused in the printing process.

[0022] The digital manufacturing aspect of light-based 3D printing methods allows, among other things, tool-free manufacturing of target shapes. This reduces the production risk of new shapes many times over, since start-up costs for a new production campaign do not have to be procured in advance and waiting times for tool manufacturing do not have to be considered. Without such production risks, shape and product iteratives can be quickly and cost-effectively transferred to field testing, so that product optimization can be continuously advanced.

[0023] Advantageous embodiments and developments are evident from the dependent claims and the description with reference to the drawings.

[0024] According to one development, the photopolymerizable matrix component may comprise acrylates, in particular methacrylates, acrylamides, in particular methacrylamides, vinyl esters, vinyl ethers and / or cyclic ethers, and the like.

[0025] In principle, however, any photocurable matrix component or correspondingly behaving material is of interest here, which is structurally crosslinked and hardened by a photochemical process under irradiation with light, in particular in the presence of a suitable photoinitiator system.

[0026] According to one development, the photopolymerizable matrix component can be adapted to cure under irradiation with light of wavelengths between 150 and 1000 nm, preferably between 200 and 550 nm.

[0027] The photopolymerizable matrix components may therefore be curable not only with near infrared and visible light, but also in particular with UV light. The photoinitiator or photoinitiators are adjusted accordingly to these wavelengths. The achievable through-curing depth of the additional structure and thus the layer thickness defined may be, for example, in the range of 10 to 500 μm, preferably 40 to 300 μm, particularly preferably 70 to 250 μm.

[0028] According to one development, the metal filler may comprise tungsten, molybdenum and / or tantalum or another suitable metal.

[0029] As a rule here, at least 8.5 g / cm 3 , preferably at least 10 g / cm 3 Of interest is any metal, any metallic material and / or any combination of metallic materials, particularly preferably having a density comparable to or greater than the density of lead.

[0030] According to one development, the corresponding resin formulation has a viscosity of at least 4.5 g / cm 3 , preferably at least 6 g / cm 3 , particularly preferably at least 8 g / cm 3 The density of the powder may be 0.01 to 0.01.

[0031] In accordance with the present invention, the metal filler comprises less than 10% fine particle fraction having a particle size of less than 1 micrometer.

[0032] The strong absorption of the metal fillers used, especially in the spectral range of 150-1000 nm, can limit the achievable curable layer thickness. This limit depends heavily on the filler level and the particle size, particle shape, particle distribution. The higher the filler level and / or the smaller the particle size, the stronger the obstacle to light entering the formulation and allowing the photopolymerization and associated structuring of the photopolymerizable matrix component. For this reason, it is advantageous to have a small particulate component.

[0033] According to one development, the metal filler may have a particle size distribution where D10>2 μm and D90<100 μm.

[0034] In addition to the average particle size, the particle size distribution is also important. The particle size distribution of a sample can be measured, for example, by laser diffraction and can be characterized using several indices Dxx. For example, D50 means that 50% of the particles are smaller than the specified value. Other important parameters include D10 as a measure of the smallest particles in the sample, and D90, and sometimes D95, D99 and / or D100, for larger particles. For example, the closer D10 and D90 are, the narrower the particle size distribution.

[0035] Here, the particle size of the smallest particles is considered to be substantially greater than 2 μm (index D10). The upper particle size limit D90 is limited by the desired wall thickness and the required surface roughness (for example less than 100 μm).

[0036] According to one development, the metal filler may not only have a monomodal particle size distribution, but also a bimodal or polymodal particle size distribution.

[0037] Particle size distributions with multiple maxima in the density distribution are called multimodal, i.e. bimodal, trimodal, etc. Multimodal distributions are preferred to achieve high loading levels or to facilitate the processability of metal-filled resin formulations. The density distribution of the metal-filled particles may thus in this case only have a single maximum, or at best two or more maxima.

[0038] According to one development, the metal filler may comprise rounded and / or round particles.

[0039] For example, rounded and / or round metal particles in the resin formulation according to the invention result in increased flowability or reduced wear behavior during processing, which has an advantageous effect on the processing of the resin formulation.

[0040] According to one development, the metal-filled resin formulation may further contain rheological additives, nanoparticle fillers with a particle size of less than 1 micrometer, light absorbers, adhesion promoters, defoamers, leveling additives and / or thermal initiators. In particular, each additive may be present in a content of 0.01 to 20 phr with respect to the photopolymerizable matrix component.

[0041] For example, metal particles of a metal filler can be stabilized within a matrix component by the addition of a rheological additive, which prevents the particles from sinking in the matrix component by forming a network of physical bonds.

[0042] Alternatively or additionally, nanoparticles may be added to prevent settling.

[0043] The metal-filled resin formulations used preferably have suitable settling stability (e.g., greater than 4 weeks at room temperature and / or greater than 2 days at process temperature) to ensure storage stability of the resin product and isotropic filler distribution in the layers of the part produced during the 3D printing process.

[0044] When particles are at risk of light scattering during the 3D printing process, the addition of light absorbing substances (e.g. UV absorbers, HALS) can prevent curing outside of the desired exposed areas.

[0045] Additionally, other substances or mixtures can be added to facilitate curing (e.g., UV cured adhesion promoters, defoamers to reduce air void content, leveling additives for a stable resin layer on the production bed, etc.).

[0046] According to one development, the 3D printing method can include process types SLA (e.g. laser), LCD process (e.g. display), active light mask from DLP (e.g. projector) and / or other suitable light emitting process with active light mask, where it is understood that the skilled person can combine suitable processes.

[0047] Much more precise additive manufacturing processes are light-based techniques such as stereolithography (SLA) or digital light processing (DLP), in which so-called photopolymerizable resin formulations (mainly acrylate- or epoxy-based) are used. With these techniques, the resin formulations used can be locally and precisely cured layer by layer by light excitation, which allows the production of 3D parts with a resolution of up to 10 μm (for SLA) and part features of up to less than 100 μm. In addition, such 3D printing methods are advantageous over material extrusion or powder bed methods based on their high material efficiency, reduced energy consumption, achievable part density, and good scalability.

[0048] For example, so-called hot lithography can be used as a special form of SLA (see, for example, US Pat. No. 5,399,633), which is intended for the processing of highly filled formulations by targeted heating of the process zone in combination with the layer doctor technique, as a result of which particularly good material resistance and also smooth surfaces are achieved. Hot lithography is therefore particularly suitable for processing filled material systems, such as the metal-filled resin formulations according to the invention, and therefore for the production of technical 3D parts from composite materials with high precision and good surface quality.

[0049] According to one development, the component may be designed to absorb electromagnetic radiation having an energy of at least 1 keV, in particular at least 50 keV.

[0050] For example, the component may be configured to absorb electromagnetic radiation having an energy in the range of 50 keV to about 300 keV, and the wall thickness may therefore be selected depending on the radiation energy, for example in the range of 100±50 μm or more.

[0051] According to one development, the part may have a wall thickness of less than 150 μm.

[0052] The minimum wall thickness can therefore in particular be less than 100 μm.

[0053] According to one development, the part has a density of at least 4.5 g / cm 3 , preferably at least 6 g / cm 3 , particularly preferably at least 8 g / cm 3 It is.

[0054] The resulting density of the photopolymerized composite material can therefore be in the range of lead or even higher.

[0055] According to one development, the organic components can be fired in a separate step from the part (green part) by heat treatment (e.g. in a convection oven), and the resulting brown part is fed to a sintering process to form a metal, metal oxide shaped part or a combination of metal and metal oxide shaped parts.

[0056] According to one development, the fired part can furthermore be infiltrated with a metallic and / or non-metallic matrix, which makes it possible to adjust the properties (eg radiation absorption rate, strength, etc.).

[0057] The above configurations and developments can be combined with each other in any way, as long as it is reasonable. Further possible embodiments, developments and implementations of the invention also include combinations of the features of the invention described above or in the following specification in relation to the examples, but not explicitly described. In particular, the skilled person can add individual aspects as improvements or supplements to each basic form of the invention. [Brief description of the drawings]

[0058] The invention will be explained in more detail below with reference to an embodiment presented in the schematic diagrams of the drawing.

[0059] [Figure 1] 1 shows a schematic diagram of a 3D printing apparatus for performing a 3D printing method according to one embodiment of the present invention. [Diagram 2] 2 shows a detailed view of a part produced using the 3D printing apparatus of FIG. 1 based on a metal-filled resin formulation according to one embodiment of the present invention. [Diagram 3] A schematic flow chart of the 3D printing method used is shown in Figures 1 and 2.

[0060] The accompanying drawings are intended to provide a further understanding of embodiments of the present invention. They serve to illustrate embodiments and clarify the principles and concepts of the present invention. Other embodiments and many of the described advantages are apparent with reference to the drawings. Elements in the drawings are not necessarily shown to scale relative to each other.

[0061] In the figures, identical, functionally identical and identically acting elements, features and components are given the same reference numerals, respectively, unless otherwise specified. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0062] 1 shows a schematic diagram of a 3D printing apparatus 100 for performing a 3D printing method M according to an embodiment of the present invention. A schematic flow chart of process M is shown in FIG.

[0063] The process M is used in the embodiment described below for the manufacture of a radiation absorbing component 10. The component 10 is, for example, a scattered radiation collimator, which is used to suppress unwanted scattered radiation for a radiation detector in a transmission tomography device, for example an X-ray computed tomography device. During an examination, for example in X-ray computed tomography, such scattered radiation can occur due to interaction with an object. To prevent unwanted artifacts in the captured image, such scattered light radiation is usually stopped before entering the detector by a corresponding collimator element made of a suitably dense metallic or metal composite material.

[0064] For this and other radiation absorbing structures, polymer / metal composites are often formed today by conventional polymer forming techniques such as injection molding or extrusion, using metal fillers with high density and / or high atomic number, such as tungsten, such that the density of the resulting composite is at least 4.5 g / cm. 3 , which corresponds to a tungsten loading of more than 18.5% by volume, although a higher loading would be ideal to achieve a density similar to or higher than that of lead. It should be noted that although a higher density improves the part performance in terms of radiation absorption, the lower mechanical strength of the composite must be taken into account, which may lead to brittleness of the finished part. Furthermore, the processing of such composites is difficult with a higher percentage of metal loading, and complex shapes can no longer be realized. The polymer matrix must therefore be targeted and optimized to ensure good processability and the required (thermo)mechanical properties.

[0065] Due to the increasingly required miniaturization of applications or development efforts, there is also a great demand for the production of highly complex geometries (e.g. wall thicknesses below 100 μm and resolution or accuracy down to 10 μm to increase the sensitivity of collimators), which are not feasible with conventional molding processes. Furthermore, with the above mentioned mass production methods, on-demand production of degradable spare parts is either economically unfeasible or must be mitigated by sufficient storage capacities at the current state of the art.

[0066] For the manufacture of such precise radiation-absorbent shaped parts, it is therefore currently proposed to use additive manufacturing techniques, namely 3D printing. However, 3D printing methods realized up to now, such as those directly processing metallic materials (e.g. laser powder bed fusion, see the opening mentioned non-patent document 1) or those using thermoplastic-based metal composites on par with injection molding or extrusion methods (e.g. fused filament fabrication, see e.g. patent document 10), are very limited in terms of achievable part resolution (>50 μm) and achievable minimum wall thickness (>150 μm). Such limitations are even more pronounced, especially when composite materials are used.

[0067] For this reason, an innovative approach is currently being pursued, in which metal-filled resin formulations are structured locally and precisely freeform by photoexcitation, layer by layer, with high precision, part features down to <100 μm or resolution down to 10 μm, using stereolithographic 3D printing methods such as SLA. In this case, the metal-filled resin formulation is required to have a density of at least 4.5 g / cm in order for the final part 10 to absorb radiation with an energy of, for example, more than 50 keV. 3The 3D printing method is selected to have a material density of 1000 nm or more. Access to complex geometries and low wall thicknesses allows for improved part performance in many applications (e.g., improved light directionality in collimators). In addition, such 3D printing methods are advantageous over material extrusion or powder bed processing methods based on their high material efficiency, their reduced energy consumption, achievable part densities, and their high scalability.

[0068] Process M thus optionally comprises, in M1, providing a metal-filled resin formulation 1 in a production bath and / or on a production bed 6 and / or generally by providing a wet layer of metal-filled resin formulation 1. Process M further comprises, in M2, selectively curing the metal-filled resin formulation 1 layer by layer in the production bath and / or on a production bed 6 and / or in the provided wet layer using selective light irradiation to form a part. The light irradiation can be applied directly to the surface of the resin formulation as required (FIG. 1) or can be introduced into the resin formulation through a support medium transparent to the light irradiation.

[0069] A corresponding exemplary structure for the "top-down" method is shown in Fig. 1. A metal-filled resin formulation 1 is present in a production bath 6. A control device 7, e.g. a computer, controls on the one hand a laser 8, which moves a laser beam 9 selectively over the surface of the resin formulation 1 in the production bath 6 via a deflection mirror 11. On the other hand, the control device 7 controls a lowering device 13 in the production bath 6 for gradually lowering a work table 12, on which a part 10 is built up by the hardening of the resin formulation 1 caused layer by layer by means of a laser beam.

[0070] Formulation 1 as used herein comprises a mixture of a photostructurable matrix component (component A) and one or more metal fillers (component B). Formulation 1 is constructed as follows: - photopolymerizable matrix component A: monomers, oligomers, prepolymers or mixtures thereof, consisting of the group of monofunctional and / or polyfunctional radically and / or cationically polymerizable compounds, such as (meth)acrylates, (meth)acrylamides, vinyl esters, vinyl ethers, cyclic ethers, etc., having a volume fraction of 5 to 80% by volume, preferably 5 to 70% by volume, particularly preferably 5 to 60% by volume, based on the sum of components A and B. - Metal fillers (component B), especially radiation-absorbing, such as refractory metals: 8.5 g / cm 3 or more, preferably at least 10 g / cm 3 or more, and a volume fraction of 20 to 95 volume %, preferably 30 to 95 volume %, particularly preferably 40 to 95 volume %, based on the total of component A and component B, preferably tungsten, molybdenum or tantalum, preferably with a low fine particle fraction (less than 1 μm, less than 10%), D10>2 μm and D90<100 μm, preferably with a unimodal or bimodal distribution, preferably with a rounded or round particle shape. - Photopolymerization initiator: adjusted to the photopolymerizable component A and the wavelength of light used for curing, and has a content of 0.05 to 10 phr, preferably 0.1 to 5 phr, particularly preferably 0.3 to 3 phr, relative to component A.

[0071] The photopolymerizable component A is cured by targeted irradiation with light of wavelengths of 150-1000 nm, preferably 200-550 nm, using a tailored photoinitiator. The achievable through-curing depths, and therefore layer thicknesses, are in the range of 10-500 μm, preferably 40-300 μm, particularly preferably 70-250 μm. The matrix component A together with the photoinitiator allows for a fast photoreaction and provides the composite with sufficient green strength, which therefore maintains the desired shape fidelity during the 3D printing process and during post-treatment.

[0072] Optionally, additional components such as rheological additives, fillers with a particle size of less than 1 μm, absorbents, adhesion promoters, defoamers, leveling additives, thermal initiators, etc., may be included in the formulation, each in a content of 0.01 to 20 phr relative to component A.

[0073] FIG. 2 shows a detailed view from FIG. 1 of part 10 in manufacture.

[0074] In the lower region of the part 10, the metal-filled resin formulation 1 has already been transformed into a hardened material 5. Above that there is a thin layer of not yet hardened metal-filled resin formulation 1, i.e. of a photopolymerizable matrix component 2 with metal-filled material 3 dispersed therein, with a layer thickness 14 determined by the position of the sinking device 13. By selective laser irradiation this layer can be targeted and hardened in specific areas and the part 10 can thus be expanded layer by layer upwards.

[0075] The presented resin formulation and photopolymer composites produced by SLA have the following material properties: 3 , or sufficient radiation resistance of the matrix), in combination with the described geometrical freedom of the producible 3D parts (minimum wall thickness down to less than 100 μm), the achievable part resolution (down to 10 μm) and the resulting surface quality, offer decisive quality and performance improvements of the corresponding technical 3D parts (e.g. improved directionality of light in radiation collimators).

[0076] Resin formulations can be detected, for example, by particle determination (density, REM, particle size determination, RFA), matrix determination by Fourier transform IR spectroscopy, NMR spectroscopy, GPC, LC / GC-MS, UV / VIS spectroscopy and / or UV exposure testing.

[0077] The part 10 produced by lithography can be analyzed, for example, by microscopy of the SLA layer structure and by the particle size, particle shape and / or particle distribution used. Via the particle distribution, for example, the approximate filler content can be estimated. Energy dispersive X-ray spectroscopy (EDS) can be used, for example, for the analysis of the fillers used, and via density measurements and ATR-IR spectroscopy, for example, the base matrix and the filler content can be determined, including the information obtained by EDS. The associated radiation absorption can be measured in relation to pure tungsten or lead, whereby a defined radiation intensity can be applied to the plaque and can be measured by radiation transmission. Finally, the absorption of scattered light radiation as well as possible artifacts / radiation arising from the material are important and can be tested in the respective application.

[0078] In other words, a part 10 manufactured using this process M can be distinguished, both in terms of its material composition and in terms of its structuring (wall thickness, etc.), from conventionally manufactured structures by appropriate measurement processes.

[0079] In the foregoing detailed description, various features are shown together in one or more examples to improve the consistency of the description. However, it is clear that the above description is merely illustrative and in no way limiting in nature. It covers all alternatives, modifications, and equivalents of the different features and exemplary embodiments. Many other examples will be immediately and directly apparent to those skilled in the art in light of the above description based on their technical knowledge.

[0080] The embodiments have been selected and described so as to best illustrate the principles underlying the invention and its practical applicability, thereby enabling those skilled in the art to best modify and utilize the invention and its various embodiments for its intended use. In the claims and the specification, the terms "containing" and "having" are used as linguistically neutral terms for the corresponding term "comprising". Furthermore, the use of the singular terms "ein", "einer" and "eine" is not intended to exclude, in principle, a plurality of features and a plurality of components described with the term. [Explanation of symbols]

[0081] 1 Metal-filled resin formulation 2. Photopolymerizable matrix components 3 Metal fillers 4. Photopolymerized matrix components 5 Curing material 6 Manufacturing bath, manufacturing floor 7 Control device 8 Laser 9. Laser Light 10 parts 11 Deflecting mirror 12 Workbench 13. Sinking device 14 layer thickness 100 3D printing equipment M Process M1, M2 process steps

Claims

1. A metal-filled resin formulation (1) for the production of a part (10), in particular a radiation-absorbing part, in particular for a 3D printing method (M) based on photopolymerization, said resin formulation (1) comprising: a photopolymerizable matrix component (2) comprising at least one of the monomers, oligomers and prepolymers from the group consisting of monofunctional and / or polyfunctional radically and / or cationic polymerizable compounds, The metal filler (3) has a density of at least 8.5 g / cm 3 , preferably at least 10 g / cm 3 the photopolymerizable matrix component (2) has a volume fraction of 5 to 80 volume %, preferably 5 to 70 volume %, particularly preferably 5 to 60 volume %, based on the total of the photopolymerizable matrix component (2) and the metal filler (3); the metal filler (3) has a volume fraction of 20 to 95 volume %, preferably 30 to 95 volume %, particularly preferably 40 to 95 volume %, based on the total of the photopolymerizable matrix component (2) and the metal filler (3); a photopolymerization initiator, which is adapted to the photopolymerizable matrix component (2) and the light wavelength used for photopolymerization, the photopolymerization initiator having a content of 0.05 to 10 phr, preferably 0.1 to 5 phr, particularly preferably 0.3 to 3 phr, relative to the photopolymerizable matrix component (2); The metal filler comprises less than 10% fine particle fraction having a particle size of less than 1 micrometer. Metal-filled resin formulation.

2. The photopolymerizable matrix component (2) comprises at least one of acrylates, in particular methacrylates, acrylamides, in particular methacrylamides, vinyl esters, vinyl ethers and cyclic ethers.

2. The resin formulation of claim 1.

3. characterised in that the photopolymerisable matrix component (2) is adapted to cure under irradiation with light of wavelengths between 150 and 1000 nm, preferably between 200 and 550 nm, A resin formulation according to at least one of the preceding claims.

4. The metal filler (3) comprises at least one of tungsten, molybdenum, and tantalum. A resin formulation according to at least one of the preceding claims.

5. The metal filler (3) has a particle size distribution of D10>2 μm and D90<100 μm. A resin formulation according to at least one of the preceding claims.

6. The metal filler (3) has a monomodal or bimodal particle size distribution. A resin formulation according to at least one of the preceding claims.

7. The metal filler (3) has rounded and / or round particles, A resin formulation according to at least one of the preceding claims.

8. the metal-filled resin formulation (1) further comprises at least one of the following: rheological additives, nanoparticle fillers with a particle size of less than 1 micrometer, light absorbers, adhesion promoters, defoamers, leveling additives, and thermal initiators, in particular each in a content of 0.01 to 20 phr with respect to the photopolymerizable matrix component (2); A resin formulation according to at least one of the preceding claims.

9. 9. A 3D printing method (M) based on photopolymerization for the production of a part (10), in particular a radiation-absorbing part, using the metal-filled resin compound (1) according to any one of claims 1 to 8, comprising: Providing (M1) said metal-filled resin formulation (1) in a production bath, on a production bed (6) and / or as a wet layer; and selectively curing (M2) the metal-filled resin formulation (1) layer by layer by polymerization in the production bath, on the production bed (6) and / or in the wet layer using selective light irradiation to form the part (10); 3D printing method comprising:

10. The 3D printing method (M) is characterized in that it includes at least one active light mask from the process types of stereolithography, liquid crystal display process and digital light processing; 10. The 3D printing method of claim 9.

11. Additively manufactured part (10), in particular a radiation absorbing part, manufactured using the 3D printing method (M) according to claim 9 or 10.

12. characterised in that the component (10) is designed to absorb electromagnetic radiation having an energy of at least 1 keV, in particular at least 50 keV. The component of claim 11.

13. characterised in that the part (10) has a wall thickness of less than 150 μm, 13. A part according to claim 11 or 12.

14. The part (10) has a hardness of at least 4.5 g / cm 3 , preferably at least 6 g / cm 3 , particularly preferably at least 8 g / cm 3 , characterized in that it has a density of 14. A component according to any one of claims 11 to 13.

Citation Information

Patent Citations

  • Photocurable composition for photo-shaping, metal shaped article, and method for producing the same

    JP2009084388A

  • Composite articles made using radiation curable compositions and additive manufacturing processes

    JP2020533449A

  • Additive manufacturing of radioactive phantoms

    JP2022518362A

  • Monomer formulations and methods for 3D printing of preceramic polymers

    US20180148380A1

  • Synthesis and 3D printing of photocurable colloids

    WO2020198404A1