Manufacturing method of polypropylene for secondary battery separator with excellent mechanical and thermal properties
A bimodal process with adjusted catalyst and electron donor ratios improves the mechanical and thermal properties of polypropylene films for secondary battery separation membranes, addressing limitations in conventional methods and enhancing processing fluidity.
Patent Information
- Application Number
- JP2024529298
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-19
- Filing Date
- 2022-11-04
- Publication Date
- 2024-10-31
AI Technical Summary
Conventional methods for producing polypropylene films for secondary battery separation membranes fail to maximize mechanical properties and thermal properties, limiting their effectiveness in secondary batteries.
A bimodal process is applied in the production of polypropylene for secondary battery separation membranes, adjusting the ratio of a Ziegler-Natta catalyst and electron donor to achieve a specific molecular weight distribution and incorporating a cocatalyst, resulting in high molecular weight and low molecular weight polypropylene blends.
The method enhances mechanical properties and thermal stability, improving fluidity during processing and enhancing the performance of the separation membranes.
Smart Images

Figure 2024540466000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing polypropylene, and more particularly to a method for producing polypropylene for use in a dry separator for a secondary battery.
[0002] This application claims priority to and the benefit of Korean Patent Application No. 10-2021-0160619, filed on November 19, 2021, the entire text of which is incorporated herein by reference. [Background technology]
[0003] Polymer matrices commonly used in the manufacture of secondary battery separators include polyethylene and polypropylene, which are inexpensive and have favorable pore formation properties.
[0004] Polypropylene has the advantages of having low thermal shrinkage and excellent mechanical properties compared to polyethylene. Patent Documents 1, 2, and 3 disclose methods for producing polypropylene films for secondary battery separators by dry methods that are excellent in heat resistance and cost competitive, but the conventional methods do not show satisfactory results in terms of either mechanical properties or thermal properties.
[0005] Meanwhile, in Patent Document 4, the applicant proposed polypropylene for use in a separator for a secondary battery having high heat resistance and high strength, which has excellent physical properties in terms of stereoregularity, crystallinity, melting temperature, and flexural modulus by applying a catalyst prepared in a specific manner and a bimodal process, but there was a limit to maximizing the mechanical properties and thermal properties. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] U.S. Patent No. 5,385,777 [Patent Document 2] U.S. Patent No. 5,480,745 [Patent Document 3] Korean Patent Publication No. 2003-0080007 [Patent Document 4] Korean Patent No. 1711261 Summary of the Invention [Problem to be solved by the invention]
[0007] The present invention provides a method for producing polypropylene for a separator for a secondary battery, which has maximized mechanical and thermal properties and improved resin fluidity compared to conventional materials. [Means for solving the problem]
[0008] In order to achieve the above object, the present invention provides a method for producing polypropylene for a separator for a secondary battery by polymerizing propylene monomer in the presence of a Ziegler-Natta catalyst, the polymerization reaction of the propylene monomer includes the steps of a) obtaining a high molecular weight polypropylene having a weight average molecular weight of 450,000 to 650,000 g / mol from a first reactor, and b) obtaining a low molecular weight polypropylene having a weight average molecular weight of 150,000 to 300,000 g / mol from a second reactor, and the molar ratio of the co-catalyst and the electron donor added in step a) is adjusted to 2 to 25 to produce polypropylene for a separator for a secondary battery.
[0009] The co-catalyst is at least one selected from the group consisting of trimethylaluminum, triethylaluminum, triisobutylaluminum, and trioctylaluminum, and the electron donor is at least one selected from the group consisting of cyclohexylmethyldimethoxysilane, dicyclopentyldimethoxysilane, diisopropyldimethoxysilane, vinyltriethoxysilane, triethylmethoxysilane, trimethylethoxysilane, dicyclopentyldiethoxysilane, ethyltrimethoxysilane, methyltriethoxysilane, diphenyldiethoxysilane, phenylpropyldimethoxysilane, The polypropylene for use in a secondary battery separator is at least one selected from the group consisting of dimethoxysilane, phenyltrimethoxysilane, tert-butyltrimethoxysilane, cyclohexylethyldimethoxysilane, cyclohexylmethyldimethoxysilane, cyclopentyltriethoxysilane, diisobutyldiethoxysilane, diisobutyltriethoxysilane, normal propyltrimethoxysilane, isopropyltrimethoxysilane, cycloheptylmethyldiethoxysilane, and dicycloheptyldiethoxysilane.
[0010] In addition, the polypropylene for the secondary battery separator has a weight average molecular weight of 300,000 to 500,000 g / mol, a molecular weight distribution (Mw / Mn) of 6 or more, a meltdown temperature of 166° C. or more, a xylene soluble content of 3 wt % or less, and a tensile strength of 1,300 kgf / cm, as measured by the following method. 2 The present invention provides a method for producing polypropylene for use in secondary battery separators, which is characterized by having a puncture strength of 220 gf or more. [Method of measuring molecular weight characteristics] The weight average molecular weight and molecular weight distribution (Mw / Mn) are measured using Gel Permeation Chromatography (GPC, Agilent) according to ASTM D3536. [Method for measuring xylene solubles] According to the ASTM D5492 standard, the sample is dissolved in boiling xylene, and the insoluble portion is crystallized from the solution to separate and measure the soluble portion. [Method of measuring meltdown temperature] The polypropylene for the separator is extruded in a T-die manner at 220 to 250° C. using a twin-screw extruder to form a sheet, and then sequentially stretched in MD and TD directions in a stretching machine to produce a single-layer porous film with a thickness of 15 μm. A lithium ion secondary battery manufactured using the porous film is heated in an oven at a rate of 2° C. / min while measuring the resistance in real time. The temperature at which the resistance exceeds 10,000 Ω is evaluated as the shutdown temperature, and the temperature at which the resistance rapidly decreases after the shutdown temperature is evaluated as the meltdown temperature. [Method of measuring tensile strength] The prepared porous film specimen (ASTM D638 Type IV standard) is measured using a universal material testing machine according to ASTM D638 under the condition of 50 mm / min. [Method of measuring drilling strength] A 15μm thick separator is cut to a size of 50×50mm, and a specimen is placed on a plate with a 10mm diameter circular hole. A probe with a diameter of 1mm (radius of curvature 0.5mm) is lowered at a speed of 0.05cm / sec to measure the force at which the specimen opens. Effect of the Invention
[0011] According to the present invention, a method for producing polypropylene for a dry separator of a secondary battery, in which a bimodal process is applied and ideal conditions are set for the input ratio of a cocatalyst and an electron donor, can be provided to maximize mechanical properties and thermal properties while improving fluidity during processing of the separator. [Brief description of the drawings]
[0012] [Figure 1] 4 is a photograph showing a processing state during production of a porous film in a test example of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] The present invention will be described in detail below through preferred embodiments. Prior to this, the terms and words used in this specification and claims should not be interpreted in their ordinary or dictionary sense, but should be interpreted in their meaning and concept consistent with the technical idea of the present invention, based on the principle that the inventor can appropriately define the concept of the term to best describe his / her invention. Therefore, the configuration of the embodiment described in this specification is merely one of the most preferred embodiments of the present invention, and does not fully represent the technical idea of the present invention, so it should be understood that there may be various equivalents and modifications that can replace them at the time of this application.
[0014] The present inventors applied a bimodal process in the manufacture of polypropylene for dry separators of secondary batteries in a situation where it was necessary to develop a material with maximized conventional mechanical and thermal properties. However, they discovered that a specific ratio of promoter and electron donor can maximize mechanical and thermal properties while improving fluidity during separator processing, and thus arrived at the present invention.
[0015] The present invention discloses a method for producing polypropylene for a separator for a secondary battery by polymerizing propylene monomer in the presence of a Ziegler-Natta catalyst, the polymerization reaction of the propylene monomer includes a) obtaining a high molecular weight polypropylene having a weight average molecular weight of 450,000 to 650,000 g / mol from a first reactor, and b) obtaining a low molecular weight polypropylene having a weight average molecular weight of 150,000 to 300,000 g / mol from a second reactor, and the molar ratio of the co-catalyst and the electron donor added in step a) is adjusted to 2 to 25 to produce polypropylene for a separator for a secondary battery.
[0016] In the present invention, the Ziegler-Natta catalyst is a solid catalyst prepared by, for example, reacting a magnesium compound with an alkanediol having 3 to 15 carbon atoms, which may or may not be substituted with an alkyl group having 1 to 5 carbon atoms, and a benzoyl halide compound to prepare a magnesium compound solution, reacting the magnesium compound solution with a transition metal compound to prepare a support, and reacting the support with a transition metal compound. For a specific preparation method, Korean Patent No. 1711261 in the name of the present applicant is cited as a reference.
[0017] In the manufacture of polypropylene for secondary battery separators according to the present invention, propylene monomer is polymerized in the presence of the solid catalyst, and a bimodal process is applied, that is, the polymerization reaction of the propylene monomer includes a) a step of obtaining high molecular weight polypropylene having a weight average molecular weight of 450,000 to 650,000 g / mol from a first reactor, and b) a step of obtaining low molecular weight polypropylene having a weight average molecular weight of 150,000 to 300,000 g / mol from a second reactor, thereby obtaining highly crystalline polypropylene.
[0018] In the present invention, the propylene polymerization reaction may be in a gas phase, a liquid phase, or a solution phase. When the polymerization reaction is carried out in a liquid phase, a hydrocarbon solvent may be used, or propylene itself may be used as a solvent. The temperature of the polymerization reaction may be 0 to 200°C, preferably 50 to 150°C. If the reaction temperature is less than 0°C, the activity of the catalyst may decrease, and if it exceeds 200°C, the stereoregularity may decrease. The pressure condition during polymerization may be 1 to 100 atm, preferably 2 to 30 atm. If the pressure exceeds 100 atm, it is not preferable from an industrial and economical point of view. The polymerization reaction may be carried out in any of batch, semi-continuous, and continuous modes. In the present invention, a continuous bimodal process is applied to produce a high molecular weight polypropylene having a weight average molecular weight of 450,000 to 650,000 g / mol from the first reactor and a low molecular weight polypropylene having a weight average molecular weight of 150,000 to 300,000 g / mol from the second reactor in a weight ratio of 8:2 to 4:6, preferably a high molecular weight polypropylene having a weight average molecular weight of 500,000 to 600,000 g / mol from the first reactor. From the first reactor, low molecular weight polypropylene having a weight average molecular weight of 180,000 to 240,000 g / mol is produced in a weight ratio of 7:3 to 5:5, and the final polypropylene has a weight average molecular weight of 300,000 to 500,000 g / mol and a molecular weight distribution (Mw / Mn) of 6 to 10, preferably a weight average molecular weight of 350,000 to 450,000 g / mol and a molecular weight distribution (Mw / Mn) of 6.5 to 8, more preferably a molecular weight distribution (Mw / Mn) of 6.5 to 7. In other words, low molecular weight and high molecular weight polypropylene are uniformly contained, and by applying the input ratio of a specific cocatalyst / electron donor described later, the mechanical properties and thermal properties of polypropylene are maximized while the fluidity during separation membrane processing can be improved.
[0019] Here, in the first reactor, a co-catalyst and an external electron donor are introduced, and as the transition metal compound is reduced by the solid catalyst, some of the internal electron donors present in the solid catalyst are removed, and the external electron donor is bound to the vacant space to carry out the polymerization reaction. In the present invention, it has been confirmed that the mechanical and thermal properties of polypropylene produced by the bimodal process are dramatically improved by applying a lower ratio of the electron donor to the co-catalyst introduced in the present invention compared to the conventional method.
[0020] That is, in the present invention, the molar ratio of the co-catalyst and the electron donor added in step a) may be 2-25, preferably 3-16, and more preferably 4-6.
[0021] The co-catalyst and the electron donor are not particularly limited as long as they are components used in the manufacture of polypropylene for a typical dry separator for a secondary battery. For example, the co-catalyst may be trimethylaluminum, triethylaluminum, triisobutylaluminum, trioctylaluminum, etc., and the electron donor may be cyclohexylmethyldimethoxysilane, dicyclopentyldimethoxysilane, diisopropyldimethoxysilane, vinyltriethoxysilane, triethylmethoxysilane, trimethylethoxysilane, dicyclopentyldiethoxysilane, ethyltrimethoxysilane, methyltriethoxysilane, diphenyldiethoxysilane, etc. Examples of the cocatalyst that can be used include phenylpropyldimethoxysilane, phenyltrimethoxysilane, tert-butyltrimethoxysilane, cyclohexylethyldimethoxysilane, cyclohexylmethyldimethoxysilane, cyclopentyltriethoxysilane, diisobutyldiethoxysilane, diisobutyltriethoxysilane, normalpropyltrimethoxysilane, isopropyltrimethoxysilane, cycloheptylmethyldiethoxysilane, and dicycloheptyldiethoxysilane. Preferably, triethylaluminum (TEAL) is used as the cocatalyst and dicyclopentyldimethoxysilane is used as the electron donor.
[0022] Generally, the crystallinity of general-purpose polypropylene is about 50 to 52%, but the polyolefin produced by the present invention is a highly crystalline polypropylene with a crystallinity of 55% or more. In addition, since the stereoregularity is very high at 97% or more, it has a melting temperature of 167°C or more, exhibits high crystallization temperature characteristics, and has excellent mechanical properties and thermal properties.
[0023] The polymerized polypropylene may further be added with an antioxidant, a neutralizing agent, a nucleating agent, etc. during the kneading process, and the extruded sheet may be stretched to dry produce a porous film. The method used to produce a separator using the dry process for the above polypropylene may be a method in which the polymer crystalline portion is oriented in a certain direction, and then the relatively weak amorphous portion is ruptured by cold stretching to form pores. In addition, it may be produced depending on the difference in the shape of the polymer crystals and the difference in crystallization temperature, and when produced by such a method, a nucleating agent is added. Therefore, it is believed that the properties of the produced microporous membrane are determined not only by the degree of orientation of the polymer crystalline portion and the shape of the polymer crystals, but also by the additives and modifiers added.
[0024] For example, in the present invention, the separator may be manufactured by extruding the polypropylene in a twin-screw extruder in a T-die manner at a temperature of 200 to 230°C to form a sheet, and then simultaneously or sequentially stretching in the MD and TD directions in a stretching machine to form a porous film. In order to be used as a separator for a secondary battery, the porosity of the film is required to be at least 30%, and mechanical properties such as puncture strength and tensile strength are important factors that determine whether the film can be used. As confirmed in the following examples, the polypropylene for a separator for a secondary battery according to the present invention has improved mechanical properties, thermal properties and fluidity (processability) of the film used as a material for a separator for a secondary battery, and has an improved meltdown temperature.
[0025] In detail, the polypropylene for secondary battery separator according to the present invention has a meltdown temperature of 166° C. or higher, preferably 168° C. or higher, a xylene soluble content of 3% by weight or lower, preferably 1.5% by weight or lower, more preferably 1.2% by weight or lower, and a tensile strength of 1,300 kgf / cm 2 More than 1,400kgf / cm 2 or more, and the puncture strength may be 220 gf or more, preferably 230 gf or more. EXAMPLES
[0026] The present invention will now be described in more detail with reference to specific examples and comparative examples.
[0027] [Example 1] A 2L pressure-resistant glass reactor equipped with an agitator and an oil circulation heater was thoroughly ventilated with nitrogen, and anhydrous magnesium dichloride, 2,4-pentanediol, and decane were added under a nitrogen atmosphere and stirred at 130°C and 500 rpm. After the magnesium compound was completely dissolved to form a homogeneous solution and aged for 1 hour, benzoyl chloride was added for 30 minutes, aged for 1 hour at 130°C, and the temperature of the reactor was lowered to 25°C to prepare a magnesium compound solution. Next, a glass reactor equipped with an agitator and an oil circulation heater was thoroughly ventilated with nitrogen, and 800L of hexane and 800L of titanium tetrachloride were added under nitrogen reflux conditions, and the temperature of the reactor was lowered to -20°C while stirring at 300 rpm to prepare a mixed solvent. The prepared magnesium dichloride solution was added to the reactor containing the titanium compound dispersed in the hexane solvent for 4 hours. After the magnesium compound solution was added and maintained for 1 hour, the temperature of the reactor was raised at a rate of 0.25°C / min until the temperature reached 20°C. After the temperature of the reactor reached 20°C, it was aged for 1 hour, and the temperature of the reactor was raised at a rate of 1°C / min to 73°C. After reaching 73°C, the reactor underwent an aging process for 2 hours, and the supernatant liquid excluding the precipitated solid in the reactor was removed to produce a solid support. Next, titanium tetrachloride was added to the prepared solid support, stirred, and heated at a rate of 1°C / min, and 2,2'-diisobutyl phthalate and 1,3-diether mixed in a 1:1 molar ratio at 110°C were added. Next, the mixture was aged for 1 hour to further precipitate the solid catalyst, and the supernatant liquid was removed. The solid catalyst from which the supernatant liquid had been removed was washed once more with titanium tetrachloride, cooled to 63°C, and washed 7 times with 1L of hexane to obtain a final slurry solid catalyst. The final catalyst slurry was dried with nitrogen to obtain a solid catalyst for polypropylene polymerization.
[0028] Polypropylene polymerization was carried out by applying a bimodal process to the bulk polymerization method using the solid catalyst and propylene as a solvent. First, the first reactor was heated to 120°C and filled with 2L of nitrogen. Under the nitrogen atmosphere, the temperature of the reactor was lowered to 25°C and propylene was used to ventilate the reactor and maintain the reactor in a propylene atmosphere. 2mmol of triethylaluminum (TEAL) diluted in decane solvent at 1 molar concentration was added to the reactor maintained in a propylene gas atmosphere, and dicyclopentyldimethoxysilane (Donor) diluted in decane solvent was added so that the molar ratio (dicyclopentyldimethoxysilane / triethylaluminum) was 4.4 to 5. The catalyst was diluted in decane solvent and added at 0.005g, 1,000mL of hydrogen was added, and then 500g of propylene was added, and the prepolymerization was carried out for 5 minutes by operating the stirrer. After prepolymerization, the reactor temperature was heated to 70°C, and polymerization was carried out at 70°C for 1 hour. Unreacted propylene was discharged to the atmosphere, and the reactor temperature was lowered to room temperature to produce a high molecular weight polypropylene having a relatively low melt index and a weight average molecular weight of about 550,000 g / mol. The same method was carried out in the second reactor, but the polymerization time was adjusted to produce a low molecular weight polypropylene having a relatively low melt index and a weight average molecular weight of about 210,000 g / mol, and the high molecular weight polypropylene and low molecular weight polypropylene produced were polymerized in a weight ratio of about 6:4. The produced polypropylene was obtained after drying in a vacuum oven at 50°C for 10 hours.
[0029] [Example 2, Comparative Examples 1 to 3] Polypropylene was produced in the same manner as in Example 1, except that the polymerization process and TEAL / Donor ratio were adjusted as shown in Table 1 below. In the case of the monomodal process, only the first reactor was used to produce polypropylene having the weight average molecular weight shown in Table 1 below.
[0030] [Test example] The prepared polypropylene was extruded in a twin-screw extruder at 220 to 250° C. in a T-die manner to prepare a sheet, and then sequentially stretched in the MD and TD directions in a stretching machine to prepare a monolayer porous film having a thickness of 15 μm. The molecular weight characteristics, meltdown temperature, xylene solubles, tensile strength, puncture strength, and fluidity of the polypropylene and film were measured or evaluated by the following methods, and the results are shown in Table 1 and FIG. 1. [Measurement method] (1) Molecular weight characteristics The weight average molecular weight and molecular weight distribution (Mw / Mn) were measured using gel permeation chromatography (GPC, Agilent) according to ASTM D3536. Polystyrene was used as a standard in chloroform solvent. (2) Meltdown temperature The lithium ion secondary battery manufactured using the porous film was heated in an oven at a rate of 2°C / min, and the resistance was measured in real time. The temperature at which the resistance exceeded 10,000Ω was evaluated as the shutdown temperature, and the temperature at which the resistance dropped sharply after the shutdown temperature was evaluated as the meltdown temperature. "Shutdown" refers to the property of partially melting the film at a certain temperature or higher to close the pores. A short circuit in which the positive and negative electrodes of a secondary battery are directly connected due to thermal deformation of the film at high temperatures is the main cause of explosions and fires, but this can be prevented by shutting down. In this case, "meltdown" (or "film rupture") refers to the phenomenon in which the film melts at a certain temperature or higher and partially breaks the film. If this phenomenon occurs, a short circuit in which the positive and negative electrodes of the secondary battery are connected may cause accidents such as fires or explosions. (3) Xylene solubles The samples were dissolved in boiling xylene according to ASTM D5492, and the insoluble portion was then crystallized from the solution to separate the soluble portion and measured. (4) Tensile strength The specimens (ASTM D638 Type IV standard) were measured using a universal material testing machine according to ASTM D638 at a speed of 50 mm / min. (5)Punching strength A 15 μm thick separator was cut to a size of 50 × 50 mm, and a specimen was placed on a plate with a circular hole of 10 mm in diameter. A probe of 1 mm in diameter (radius of curvature 0.5 mm) was lowered at a speed of 0.05 cm / sec to measure the force at which the specimen opened. (6) Liquidity The prepared polypropylene was extruded in a twin-screw extruder at 220°C using a T-die method, and the extrudate was passed through a T-die to check whether melt fracture or defects occurred in the extrudate.
[0031] [Table 1]
[0032] Referring to Table 1 and FIG. 1, in the production of polypropylene for a dry separator of a secondary battery, when a bimodal process according to the present invention is applied and a specific cocatalyst and electron donor are added at a specific ratio, it can be seen that the mechanical properties and thermal properties are maximized compared to the conventional art, and the fluidity during the processing of the separator is improved.
[0033] In contrast, when polypropylene is produced using a monomodal process (Comparative Examples 1 and 2), the molecular weight distribution is narrow and the fluidity of the resin is reduced, resulting in defects such as melt fracture in the extrudate (see the red square in Figure 1), which results in poor processability.Even when polypropylene is produced using a bimodal process, when the TEAL / Donor input ratio is the same as that of the conventional method (Comparative Example 3), it is found that the mechanical properties and thermal properties are reduced, such as a decrease in meltdown temperature.
[0034] The preferred embodiments of the present invention have been described in detail above. The description of the present invention is for illustrative purposes only, and those skilled in the art will understand that the present invention can be easily modified into other specific forms without changing the technical concept or essential features of the present invention.
[0035] Therefore, the scope of the present invention is defined by the claims set forth below rather than the above detailed description, and all modifications and variations that fall within the meaning, scope and equivalent concept of the claims should be interpreted as being included within the scope of the present invention.
Claims
1. A method for producing polypropylene for a secondary battery separator by polymerizing a propylene monomer in the presence of a Ziegler-Natta catalyst, The polymerization reaction of the propylene monomer includes the steps of: a) obtaining a high molecular weight polypropylene having a weight average molecular weight of 450,000 to 650,000 g / mol from a first reactor; and b) obtaining a low molecular weight polypropylene having a weight average molecular weight of 150,000 to 300,000 g / mol from a second reactor. The molar ratio of the cocatalyst and the electron donor added in step a) is adjusted to 2 to 25 to prepare polypropylene for a separator of a secondary battery.
2. The co-catalyst is at least one selected from the group consisting of trimethylaluminum, triethylaluminum, triisobutylaluminum, and trioctylaluminum, and the electron donor is at least one selected from the group consisting of cyclohexylmethyldimethoxysilane, dicyclopentyldimethoxysilane, diisopropyldimethoxysilane, vinyltriethoxysilane, triethylmethoxysilane, trimethylethoxysilane, dicyclopentyldiethoxysilane, ethyltrimethoxysilane, methyltriethoxysilane, diphenyldiethoxysilane, phenylpropyldimethoxysilane, 2. The method for producing a polypropylene for a secondary battery separator according to claim 1, wherein the polypropylene is at least one selected from the group consisting of butyltrimethoxysilane, phenyltrimethoxysilane, tert-butyltrimethoxysilane, cyclohexylethyldimethoxysilane, cyclohexylmethyldimethoxysilane, cyclopentyltriethoxysilane, diisobutyldiethoxysilane, diisobutyltriethoxysilane, normal propyltrimethoxysilane, isopropyltrimethoxysilane, cycloheptylmethyldiethoxysilane, and dicycloheptyldiethoxysilane.
3. The polypropylene for the secondary battery separator has a weight average molecular weight of 300,000 to 500,000 g / mol, a molecular weight distribution (Mw / Mn) of 6 or more, a meltdown temperature of 166° C. or more, a xylene soluble content of 3 wt % or less, and a tensile strength of 1,300 kgf / cm, as measured by the following method. 2 and a puncture strength of 220 gf or more. [Method of measuring molecular weight characteristics] The weight average molecular weight and molecular weight distribution (Mw / Mn) are measured using Gel Permeation Chromatography (GPC, Agilent) according to ASTM D3536. [Method for measuring xylene solubles] According to ASTM D5492, the sample is dissolved from boiling xylene, and the insoluble portion is crystallized from the solution to separate and measure the soluble portion. [Method of measuring meltdown temperature] The polypropylene for the separator is extruded in a twin-screw extruder at 220 to 250° C. in a T-die manner to form a sheet, and then sequentially stretched in MD and TD directions in a stretching machine to produce a single-layer porous film having a thickness of 15 μm. A lithium ion secondary battery manufactured using the porous film is heated in an oven at a rate of 2° C. / min while measuring the resistance in real time. The temperature at which the resistance exceeds 10,000Ω is evaluated as the shutdown temperature, and the temperature at which the resistance rapidly decreases after the shutdown temperature is evaluated as the meltdown temperature. [Method of measuring tensile strength] The prepared porous film specimen (ASTM D638 Type IV standard) is measured using a universal material testing machine according to ASTM D638 under the condition of 50 mm / min. [Method of measuring puncture strength] A 15 μm thick separator was cut to a size of 50 × 50 mm, and a specimen was placed on a plate with a circular hole of 10 mm in diameter. A probe of 1 mm in diameter (radius of curvature 0.5 mm) was lowered at a speed of 0.05 cm / sec to measure the force at which the specimen opened.
Citation Information
Patent Citations
Olefin polymer and method for producing olefin polymer
CN111378058A
Olefin polymer and method for producing olefin polymer
EP3674331A1
Olefin polymerization and copolymerization
JP1993105722A
Crystalline polypropylene
JP1996092321A
Olefin polymer, and production method of olefin polymer
JP2020105484A