Stacked nanosheet transistors with defect-free channels
The novel nanosheet fabrication technique addresses the challenge of defect-free channels in conventional methods by using sacrificial silicon-germanium layers, enabling higher channel layers and improved performance in nanosheet transistors.
Patent Information
- Application Number
- JP2024531089
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-12-02
- Filing Date
- 2022-11-28
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2042-11-28
AI Technical Summary
Conventional nanosheet transistor fabrication methods face limitations in achieving defect-free channels, particularly due to the critical thickness constraint of silicon-germanium layers, which hinders the fabrication of laminated nanosheet devices with arbitrary height and compromises computational power and performance.
A novel nanosheet fabrication technique is employed where all initial silicon and silicon-germanium layers are sacrificial, allowing for the growth of defect-free semiconductor layers after removing the silicon-germanium layers, ensuring the thickness of SiGe layers remains within critical dimensions without defects, enabling more channel layers and improved device performance.
The method ensures defect-free channels, allowing for increased channel layers within the structure without compromising device scaling, thereby enhancing computational power per unit area and performance.
Smart Images

Figure 2024541485000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates generally to methods for fabricating semiconductor devices and the resulting structures, and more particularly to improved methods for fabricating nanosheet transistors having defect-free channels and the resulting structures. [Background technology]
[0002] Known metal-oxide-semiconductor field-effect transistor (MOSFET) fabrication techniques include process flows for constructing planar field-effect transistors (FETs). A planar FET includes a substrate (also called a silicon slab), a gate formed on top of the substrate, source and drain regions formed on either side of the gate, and a channel region near the surface of the substrate below the gate. The channel region electrically connects the source region to the drain region, while the gate controls the current in the channel. The gate voltage controls whether the path from drain to source is an open circuit ("off") or a resistive path ("on").
[0003] In recent years, research has been directed towards the development of non-planar transistor architectures. For example, nanosheet FETs include non-planar architectures that offer higher device density and somewhat higher performance than lateral devices. In nanosheet FETs, in contrast to conventional planar FETs, the channel is implemented as multiple stacked and spaced apart nanosheets. The gate stack wraps around the entire periphery of each nanosheet, thus allowing for more complete depletion of the channel region, resulting in steeper subthreshold swing (SS) and smaller drain induced barrier lowering (DIBL), thus reducing short channel effects. Summary of the Invention
[0004] An embodiment of the present invention is directed to a method for forming a nanosheet transistor having a defect-free channel. A non-limiting example of the method includes forming a nanosheet stack on a substrate. The nanosheet stack includes alternating first and second sacrificial layers. One of the first sacrificial layers has a thickness greater than the remaining first sacrificial layers. The first sacrificial layers are removed and a semiconductor layer is formed on a surface of the second sacrificial layer. The semiconductor layer includes a first set of semiconductor layers and a second set of semiconductor layers. The second sacrificial layer is removed and an isolation dielectric is formed between the first set of semiconductor layers and the second set of semiconductor layers.
[0005] An embodiment of the present invention is directed to a semiconductor structure. A non-limiting example of the semiconductor structure includes a nanosheet stack on a substrate. The nanosheet stack includes a first set of semiconductor layers and a second set of semiconductor layers. An isolation dielectric is disposed between the first set of semiconductor layers and the second set of semiconductor layers. A first source and drain region is formed on a sidewall of the first set of semiconductor layers and a second source and drain region is formed on a sidewall of the second set of semiconductor layers. The first source and drain region includes a first dopant type and the second source and drain region includes a second dopant type. A lower source and drain contact is formed on the sidewall of the first source and drain region and an upper source and drain contact is formed on a top surface of the second source and drain region.
[0006] Additional technical features and advantages are realized by the techniques of the present invention. Embodiments and aspects of the present invention are described in detail herein and are considered a part of the claimed subject matter. For a better understanding, reference should be made to the detailed description and drawings.
[0007] The particulars of the exclusive rights set forth herein are particularly pointed out and distinctly claimed in the concluding claims of this specification. The foregoing and other features and advantages of embodiments of the present invention will become apparent from the following detailed description taken in conjunction with the accompanying drawings. [Brief description of the drawings]
[0008] [Figure 1] 1A-1C are top and cross-sectional views of a semiconductor structure taken along line X in the top and cross-sectional views of the ... after a first series of processing operations in accordance with one or more embodiments of the present invention. [Figure 2A] 1 is a cross-sectional view of a semiconductor structure taken along line X of the reference figure in accordance with one or more embodiments of the present invention. [Figure 2B] FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y1 of reference figure in accordance with one or more embodiments of the present invention. [Figure 3A] 1 is a cross-sectional view of a semiconductor structure taken along line X of the reference figure in accordance with one or more embodiments of the present invention. [Figure 3B] FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y1 of reference figure in accordance with one or more embodiments of the present invention. [Figure 4A] 1 is a cross-sectional view of a semiconductor structure taken along line X of the reference figure in accordance with one or more embodiments of the present invention. [Figure 4B] FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y1 of reference figure in accordance with one or more embodiments of the present invention. [Figure 5A] 1 is a cross-sectional view of a semiconductor structure taken along line X of the reference figure in accordance with one or more embodiments of the present invention. [Figure 5B] FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y1 of reference figure in accordance with one or more embodiments of the present invention. [Figure 6A] 1 is a cross-sectional view of a semiconductor structure taken along line X of the reference figure in accordance with one or more embodiments of the present invention. [Figure 6B] FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y1 of reference figure in accordance with one or more embodiments of the present invention. [Figure 7A] 1 is a cross-sectional view of a semiconductor structure taken along line X of the reference figure in accordance with one or more embodiments of the present invention. [Figure 7B] FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y1 of reference figure in accordance with one or more embodiments of the present invention. [Figure 8]FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y2 of reference figure in accordance with one or more embodiments of the present invention. [Figure 9] FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y2 of reference figure in accordance with one or more embodiments of the present invention. [Figure 10] FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y2 of reference figure in accordance with one or more embodiments of the present invention. [Figure 11] FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y2 of reference figure in accordance with one or more embodiments of the present invention. [Figure 12] FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y2 of reference figure in accordance with one or more embodiments of the present invention. [Figure 13] FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y2 of reference figure in accordance with one or more embodiments of the present invention. [Figure 14] FIG. 2 is a cross-sectional view of a semiconductor structure taken along line Y2 of reference figure in accordance with one or more embodiments of the present invention. [Figure 15] 1 is a flow diagram illustrating a method according to one or more embodiments of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] The diagrams depicted herein are exemplary. There may be many variations to the diagrams or operations described herein without departing from the scope of the invention. For example, actions may be performed in a different order, or actions may be added, deleted, or modified.
[0010] In the accompanying drawings and the following detailed description of the described embodiments of the invention, various elements illustrated in the drawings are given two or three digit reference numbers. With few exceptions, the left-most digit of each reference number corresponds to the figure in which the element is first shown.
[0011] Although exemplary embodiments of the present invention are described with reference to particular transistor architectures, it should be understood in advance that embodiments of the present invention are not limited to the particular transistor architectures or materials described herein. Rather, embodiments of the present invention may be implemented in conjunction with any other type of transistor architecture or material now known or later developed.
[0012] For the sake of brevity, conventional techniques associated with the manufacture of semiconductor devices and integrated circuits (ICs) may or may not be described in detail herein. Additionally, various tasks and process steps described herein may be incorporated into a more comprehensive procedure or process having additional steps or functions not described in detail herein. In particular, the various steps in the manufacture of semiconductor devices and semiconductor-based ICs are well known, and thus, for the sake of brevity, many conventional steps are only briefly mentioned herein or omitted entirely without providing details of the well-known processes.
[0013] Turning now to an overview of technologies more specifically related to aspects of the present invention, several candidates exist for scaling non-planar transistors beyond the 7 nm node, each currently limited by various factors. One candidate is the nanosheet transistor architecture. To increase the available computing power per unit area, nanosheet devices stack channels vertically on a shared substrate footprint.
[0014] Currently, for nanosheet devices, in the early stages of fabrication, each channel is predefined by growing alternating silicon and silicon-germanium (Si / SiGe) layers. One of the Si or SiGe layers is a sacrificial layer that is removed to expose the surface of the remaining layers that define the channel. However, because selective removal between the two materials (Si vs. SiGe) is required, the minimum percentage of germanium used is about 25% (lower Ge% reduces the removal selectivity between Si and SiGe). At this germanium concentration, the bulk critical thickness of a stable SiGe film grown epitaxially on Si is 10 nm; below this thickness (sometimes called the critical thickness), the Si / SiGe can remain defect-free, and above this thickness (the critical thickness), defects can form and become prevalent. This imposes a practical limit on the maximum height of the nanosheet stack and, ultimately, on the computational power and performance. It is therefore difficult, if not impossible, to fabricate stacked nanosheet devices of any height with defect-free channels using conventional nanosheet fabrication processes.
[0015] Turning now to an overview of aspects of the invention, one or more embodiments of the invention address the above-mentioned shortcomings of known nanosheet structures and fabrication methods by providing a new nanosheet structure and fabrication method thereof that guarantees defect-free channels for any number of channels at any stack height. According to embodiments of the invention, a new nanosheet fabrication technique is utilized in which all of the initial Si and SiGe layers are sacrificial layers. The final channels are grown on the defect-free silicon layers after removal of the silicon-germanium sacrificial layers.
[0016] The nanosheet structure thus formed offers several technical advantages over conventional nanosheets. For example, the thickness of the SiGe layers can be kept within the critical dimension threshold without compromising the total number of channels or channel height and without introducing defects into the stack. By ensuring defect-free channels, the proposed structure allows more channel layers to be included in the structure, without compromising the scaling of device performance. This provides a way to further increase the bits / area for future technology nodes.
[0017] Turning now to a more detailed description of the fabrication operations and resulting structures according to embodiments of the present invention, Figures 1-14 show a semiconductor structure 100 after various fabrication operations according to embodiments of the present invention. It should be understood that the cross-sectional views shown in Figures 1-14 are of two-dimensional structures, whereas the cross-sectional views shown in Figures 1-14 represent three-dimensional structures. A top view reference diagram 101 shown in Figure 1 provides a reference point for the various cross-sectional views, namely, the X cross-sectional view (across the gate of the channel region), the Y1 cross-sectional view (along the gate of the channel region), and the Y2 cross-sectional view (along the gate of the source / drain regions) shown in Figures 1-14.
[0018] 1 shows a cross-sectional view of a semiconductor structure 100 taken along line X of reference figure 101 after an initial set of fabrication operations have been applied as part of a method for producing a final semiconductor device according to one or more embodiments of the present invention. In some embodiments of the present invention, one or more nanosheet stacks 102 are formed on a substrate 104.
[0019] The substrate 104 may be made of any suitable substrate material, such as, for example, single crystal Si, silicon germanium (SiGe), a III-V compound semiconductor, a II-VI compound semiconductor, or a semiconductor-on-insulator (SOI). III-V compound semiconductors include materials having at least one group III element and at least one group V element, such as, for example, one or more of aluminum gallium arsenide (AlGaAs), aluminum gallium nitride (AlGaN), aluminum arsenide (AlAs), aluminum indium arsenide (AlInAs), aluminum nitride (AlN), gallium antimony (GaSb), gallium aluminum antimony (GaAlSb), gallium arsenide (GaAs), gallium arsenide antimony (GaAsSb), gallium nitride (GaN), indium antimony (InSb), indium arsenide (InAs), indium gallium arsenide (InGaAs), indium gallium arsenide phosphide (InGaAsP), indium gallium nitride (InGaN), indium nitride (InN), indium phosphide (InP), and alloy combinations including at least one of the foregoing materials. Alloy combinations can include binary alloys (two elements, e.g., gallium(III) arsenide (GaAs)), ternary alloys (three elements, e.g., InGaAs), and quaternary alloys (four elements, e.g., aluminum gallium indium phosphide (AlInGaP)).
[0020] In some embodiments of the present invention, the substrate 104 may include a buried oxide layer (not shown separately) in a silicon-on-insulator (SOI) configuration. The buried oxide layer may be made of any suitable dielectric material, such as, for example, silicon oxide. In some embodiments of the present invention, the buried oxide layer is formed to a thickness of about 10-200 nm, although other thicknesses are within the contemplated scope of the present invention. In some embodiments of the present invention, the semiconductor structure 100 may be formed without a buried oxide layer. In that case, a shallow trench isolation (STI) is formed to provide isolation between devices.
[0021] In some embodiments of the invention, each of the nanosheet stacks 102 may include one or more first sacrificial layers 106 interleaved with one or more second sacrificial layers 108. In some embodiments of the invention, one of the first sacrificial layers 106 is formed or grown to a greater thickness than the remaining first sacrificial layers 106 to define a thick sacrificial layer 110. In some embodiments of the invention, the thick sacrificial layer 110 is grown from the centermost layer of the first sacrificial layers 106 (as shown), although other relative positioning is possible. The inclusion of the thick sacrificial layer 110 later allows for separation between the channels of the two stacked FETs (described in more detail below with respect to FIG. 5A).
[0022] In some embodiments of the present invention, the first sacrificial layer 106 and the second sacrificial layer 108 are epitaxially grown layers. For ease of discussion, reference will be made to operations performed on a nanosheet stack having four first sacrificial layers 106, four second sacrificial layers 108, and a thick sacrificial layer 110. However, it will be understood that the nanosheet stack 102 can include any number of semiconductor layers alternating with a corresponding number of sacrificial layers, and may or may not include a thick semiconductor layer. For example, the nanosheet stack 102 can include two semiconductor layers, five semiconductor layers, eight semiconductor layers, thirty semiconductor layers, or any number of semiconductor layers, along with a corresponding number of sacrificial layers (i.e., alternating while taking into account thick semiconductor layers, if present).
[0023] The first sacrificial layer 106 (and the thick sacrificial layer 110) can be made of any suitable material, such as, for example, single crystal silicon. Alternative materials are possible, so long as the material exhibits etch selectivity to silicon germanium and can be deposited or grown to the required height without introducing defects. In some embodiments of the invention, the first sacrificial layer 106 has a thickness of about 4 nm to about 10 nm, e.g., 6 nm, although other thicknesses are within the contemplated range of the invention. In some embodiments of the invention, the thick sacrificial layer 110 has a thickness of about 10 nm to about 50 nm, e.g., 25 nm, although other thicknesses are within the contemplated range of the invention. In some embodiments of the invention, the substrate 104 and the first sacrificial layer 106 can be made of the same semiconductor material. In other embodiments of the invention, the substrate 104 can be made of a first semiconductor material and the first sacrificial layer 106 can be made of a second semiconductor material. The thick sacrificial layer 110 can be the same material as the first sacrificial layer 106 or a different material. In some embodiments, the bottom layer of the sacrificial layer 106 can be a silicon layer on a starting silicon-on-insulator (SOI) substrate.
[0024] In some embodiments of the present invention, the second sacrificial layer 108 is a silicon-germanium layer having a germanium concentration greater than the germanium concentration of the first sacrificial layer 106 (if present). For example, if the first sacrificial layer 106 is a silicon-germanium layer having a germanium concentration of 5 percent (sometimes referred to as SiGe5), the second sacrificial layer 108 may be a silicon-germanium layer having a germanium concentration of about 25 percent (SiGe25), although other germanium concentrations are within the contemplated scope of the present invention. In embodiments in which the first sacrificial layer 106 is a silicon layer, the second sacrificial layer 108 may include a silicon-germanium layer having a germanium concentration of about 5% to about 60%. Advantageously, the second sacrificial layer 108 has a maximum thickness below the critical thickness for SiGe defects, e.g., less than about 10 nm.
[0025] 2A and 2B show cross-sectional views of the semiconductor structure 100 taken along lines X and Y1 of reference figure 101 after processing operations according to one or more embodiments of the present invention. As shown in cross-section X of FIG. 2A, a portion of the nanosheet stack 102 can be removed to expose the surface of the substrate 104 and define the width of the nanosheet stack. This process is sometimes referred to as fin-cutting. In some embodiments of the present invention, the width of the nanosheet stack 102 after fin-cutting is about 10-100 nm, although other widths are within the contemplated scope of the present invention.
[0026] As shown in FIG 2B, a dielectric layer 202 is formed on each end of the nanosheet stack 102 on the substrate 104. The dielectric layer 202 can be made of any suitable dielectric material, such as, for example, oxides, low-k dielectrics, nitrides, silicon nitride, silicon oxide, SiON, SiC, SiOCN, and SiBCN. Any known method of forming the dielectric layer 202 can be utilized, such as, for example, CVD, PECVD, ALD, flowable CVD, spin-on dielectric, or PVD.
[0027] 3A and 3B show cross-sectional views of the semiconductor structure 100 taken along lines X and Y1 of reference figure 101 after processing operations according to one or more embodiments of the present invention. As shown in cross-sectional view X of FIG. 3A, the first sacrificial layer 106 and the thick sacrificial layer 110 are removed to expose the surface of the second sacrificial layer 108. In some embodiments of the present invention, the first sacrificial layer 106 and the thick sacrificial layer 110 are selectively removed relative to the second sacrificial layer 108. The first sacrificial layer 106 and the thick sacrificial layer 110 can be selectively removed using wet etching, dry etching, or a combination of wet etching or dry etching or both. For example, a chemical reaction of an aqueous hydroxide solution containing ammonium hydroxide and potassium hydroxide can be used to selectively remove silicon relative to silicon germanium. As shown in FIG. 3B, a dielectric layer 202 on each end of one or more nanosheet stacks 102 anchors each of the nanosheet stacks 102 onto the substrate 104.
[0028] 4A and 4B show cross-sectional views of the semiconductor structure 100 taken along lines X and Y1 of reference figure 101 after processing operations according to one or more embodiments of the present invention. As shown in cross-sectional view X of FIG. 4A, a semiconductor layer 402 (also referred to as a channel layer) is formed on the exposed surfaces (top and bottom) of the second sacrificial layer 108. In some embodiments of the present invention, the semiconductor layer 402 is epitaxially grown from the surface of the second sacrificial layer 108. As previously mentioned, the thickness of the second sacrificial layer 108 can be kept below a critical thickness for defects to ensure a defect-free surface on which the semiconductor layer 402 can be epitaxially grown.
[0029] The semiconductor layer 402 can be made of any suitable semiconductor material, such as, for example, single crystal silicon or silicon germanium. Alternative materials are possible, so long as the materials exhibit etch selectivity to silicon germanium at the germanium concentration present in the second sacrificial layer 108. In some embodiments of the invention, the first sacrificial layer 106 has a thickness of about 4 nm to about 10 nm, for example, 6 nm, although other thicknesses are within the contemplated scope of the invention. In some embodiments of the invention, the semiconductor layer 402, the substrate 104, and / or the first sacrificial layer 106 can be made of the same semiconductor material. In other embodiments of the invention, the semiconductor layer 402 is made of a different semiconductor material.
[0030] 5A and 5B show cross-sectional views of the semiconductor structure 100 taken along lines X and Y1 of reference figure 101 after processing operations according to one or more embodiments of the present invention. As shown in cross-sectional view X of Figure 5A, the second sacrificial layer 108 is removed to expose a surface of the semiconductor layer 402. In embodiments of the present invention having a thick sacrificial layer 110, a first portion 502 of the semiconductor layer 402 is separated from a second portion 504 of the semiconductor layer 402 by a stack separation distance that can be increased or decreased by varying the thickness of the thick sacrificial layer 110 (see Figure 2A).
[0031] In some embodiments of the present invention, the second sacrificial layer 108 is selectively removed with respect to the semiconductor layer 402. The second sacrificial layer 108 can be selectively removed using wet etching, dry etching, or a combination of wet etching, dry etching, or both. For example, hydrogen chloride (HCl) gas or an aqueous solution containing a mixture of ammonia and hydrogen peroxide can be used to remove silicon germanium selectively with respect to silicon. As shown in FIG. 5B, the dielectric layer 202 on each end of the semiconductor layer 402 secures each semiconductor layer 402 of the nanosheet stack 102 onto the substrate 104.
[0032] 6A and 6B show cross-sectional views of the semiconductor structure 100 taken along lines X and Y1 of reference figure 101 after processing operations according to one or more embodiments of the present invention. As shown in cross-sectional view X of FIG. 6A, a dielectric layer 602 is formed on the exposed surface of the semiconductor layer 402. The stack separation distance is reduced by about two times the thickness of the dielectric layer 602, but is not eliminated completely. This makes room for the isolation dielectric to be formed later (see FIG. 7B).
[0033] The dielectric layer 602 can be made of any suitable dielectric material, such as, for example, oxides, low-k dielectrics, nitrides, silicon nitride, silicon oxide, SiON, SiC, SiOCN, and SiBCN. Any known method of forming the dielectric layer 202 can be utilized, such as, for example, CVD, PECVD, and ALD. In some embodiments of the invention, the dielectric layer 602 is conformally deposited over the semiconductor layer 402, for example, using ALD. In some embodiments of the invention, the dielectric layer 602 is an ALD silicon oxide layer. The dielectric layer 602 can be formed to a thickness of about 2 nm to about 15 nm, for example, 5 nm, although other thicknesses are within the contemplated scope of the invention.
[0034] 7A and 7B show cross-sectional views of the semiconductor structure 100 taken along lines X and Y1 of reference figure 101 after processing operations according to one or more embodiments of the present invention. As shown in cross-sectional view X of FIG. 7A, an isolation dielectric 702 is formed on the dielectric layer 602. In particular, the isolation dielectric 702 fills the remaining space (defined by the stack separation distance) between the first portion 502 and the second portion 504 of the semiconductor layer 402. In this manner, the isolation dielectric 702 serves to electrically isolate the first portion 502 from the second portion 504, allowing these portions to later function as separate FETs (see, for example, FIG. 14). Moreover, the isolation dielectric 702 surrounds the semiconductor layer 402, but is physically separated from them by the presence of the dielectric layer 602. As a result, the isolation dielectric 702 acts as a dielectric shell that advantageously ensures a uniform gate stack during downstream RMG processes (i.e., uniform spacing for the gate dielectric and gate work function metal around the nanosheets 402 when the dielectric layer 602 is replaced by the gate dielectric and gate work function metal as described with respect to FIG. 13).
[0035] In some embodiments of the present invention, a shallow trench isolation (STI) 704 is formed over the remaining portion of the substrate 104. The STI 704 may be made of any suitable isolation material, such as, for example, silicon nitride, silicon oxide, SiON, SiC, SiOCN, and SiBCN. In some embodiments of the present invention, the semiconductor structure 100 is planarized, for example, using a chemical mechanical planarization (CMP) process.
[0036] 8 illustrates a cross-sectional view of the semiconductor structure 100 taken along line Y2 of reference diagram 101 after processing operations according to one or more embodiments of the present invention. In some embodiments of the present invention, the sidewalls of the nanosheet stack 102 are released (exposed) and a sacrificial gate 802 (sometimes referred to as a dummy gate) is formed on top of the nanosheet stack 102.
[0037] The portion of the nanosheet stack where the gate is formed is called the channel region. The sacrificial gate 802 can be made of any suitable material, such as amorphous silicon or polysilicon. Any known method for patterning the sacrificial gate can be used, such as wet etching, dry etching, or a combination of successive wet or dry etching or both.
[0038] In some embodiments of the present invention, a hard mask 804 is formed on the sacrificial gate 802. In some embodiments of the present invention, the sacrificial gate 802 is formed by patterning the hard mask 804 and selectively removing the portions of the sacrificial gate 802 that are not covered by the patterned hard mask 804 using a wet or dry etching process. The hard mask 804 may be made of any suitable material, such as, for example, silicon nitride. In some embodiments of the present invention, a second hard mask (not shown) is formed on the hard mask 804 to form a bilayer hard mask. In some embodiments, the second hard mask comprises an oxide, such as, for example, silicon dioxide.
[0039] FIG. 9 illustrates a cross-sectional view of the semiconductor structure 100 taken along line Y2 of reference FIG. 101 after processing operations according to one or more embodiments of the present invention. In some embodiments of the present invention, spacers 902 (also known as sidewall spacers or gate spacers) are formed on the sidewalls of the sacrificial gate 802. In some embodiments of the present invention, the spacers 902 are formed using CVD, PECVD, UHVCVD, RTCVD, MOCVD, LPCVD, LRPCVD, ALD, PVD, chemical solution deposition, MBE, or other similar processes in combination with wet or dry etching processes. For example, a spacer material can be conformally deposited on the semiconductor structure 100 and selectively removed using RIE to form the spacers 902.
[0040] Spacers 902 may be made of any suitable material, such as, for example, a low-k dielectric, nitride, silicon nitride, silicon oxide, SiON, SiC, SiOCN, or SiBCN. In some embodiments of the invention, spacers 902 include silicon nitride. Spacers 902 may be formed to a thickness of about 5-40 nm, although other thicknesses are within the contemplated scope of the invention.
[0041] In some embodiments of the invention, a portion of the nanosheet stack 102 may be removed (also called a stack recess) to expose the surface of the substrate 104 (or the buried oxide layer, if present). The nanosheet stack 102 may be patterned using, for example, wet etching, dry etching, or a combination of wet etching or dry etching or both. In some embodiments of the invention, the nanosheet stack 102 is patterned using RIE. In some embodiments of the invention, the nanosheet stack 102 is selectively patterned with respect to the spacers 902.
[0042] In some embodiments of the invention, the dielectric layer 602 can be recessed and the inner spacers 904 can be formed on the recessed sidewalls of the dielectric layer 602. For example, the sidewalls of the dielectric layer 602 can be recessed to form cavities (not shown) in the nanosheet stack 102. In some embodiments of the invention, the inner spacers 904 are formed on the recessed sidewalls of the dielectric layer 602 by filling these cavities with a dielectric material. In some embodiments of the invention, the portions of the inner spacers 904 that extend beyond the sidewalls of the nanosheet stack 102 are removed using, for example, an isotropic etching process. In this way, the sidewalls of the inner spacers 904 are coplanar with the sidewalls of the semiconductor layer 402. In some embodiments of the invention, the inner spacers 904 are formed using CVD, PECVD, ALD, PVD, chemical solution deposition, or other similar processes in combination with wet or dry etching processes. The inner spacers 904 may be made of any suitable material, such as, for example, a low-k dielectric, a nitride, silicon nitride, silicon dioxide, SiON, SiC, SiOCN, or SiBCN.
[0043] 10 illustrates a cross-sectional view of the semiconductor structure 100 taken along line Y2 of reference figure 101 after processing operations according to one or more embodiments of the present invention. In some embodiments of the present invention, source and drain regions 1002 are formed on exposed sidewalls of the semiconductor layer 402. In some embodiments of the present invention, a gap 1004 remains between the upper (1002a) and lower (1002b) portions of the source and drain regions 1002 due to the presence of the isolation dielectric 702, which does not provide a surface for epitaxial growth. The gap 1004 can later be filled with a dielectric to ensure device isolation (see, for example, FIG. 11).
[0044] The source and drain regions 1002 may be epitaxially grown using, for example, vapor phase epitaxy (VPE), molecular beam epitaxy (MBE), liquid phase epitaxy (LPE), or other suitable processes. The source and drain regions 1002 may be epitaxially grown semiconductor material from gaseous or liquid precursors. In some embodiments of the invention, the gas source for epitaxial deposition of the semiconductor material includes a silicon-containing gas source, a germanium-containing gas source, or a combination thereof. For example, the silicon layer may be epitaxially deposited (or grown) from a silicon gas source selected from the group consisting of silane, disilane, trisilane, tetrasilane, hexachlorodisilane, tetrachlorosilane, dichlorosilane, trichlorosilane, methylsilane, dimethylsilane, ethylsilane, methyldisilane, dimethyldisilane, hexamethyldisilane, and combinations thereof. The germanium layer may be epitaxially deposited from a germanium gas source selected from the group consisting of germane, digermane, halogermane, dichlorogermane, trichlorogermane, tetrachlorogermane, and combinations thereof. Combinations of such gas sources may be utilized to epitaxially form silicon-germanium alloy layers. Carrier gases such as hydrogen, nitrogen, helium, and argon may be used. In some embodiments of the invention, the epitaxial semiconductor material includes carbon-doped silicon (Si:C). This Si:C layer may be grown in the same chamber used for the other epitaxy steps or in a dedicated Si:C epitaxy chamber. Si:C may contain carbon ranging from about 0.2 percent to about 3.0 percent.
[0045] Epitaxially grown silicon and silicon germanium can be doped by adding n-type dopants (e.g., P or As) or p-type dopants (e.g., Ga, B, BF2, or Al). In some embodiments of the invention, the source and drain regions 1002 can be epitaxially formed and doped by a variety of methods, such as, for example, in situ doped epitaxy (doped during deposition), doping after epitaxy, or implantation and plasma doping. The dopant concentration in the doped regions can be greater than 1×10 19 cm -3 ~2×10 21 cm -3 , or 1 × 10 20 cm -3 ~1×10 21 cm -3 The range may be:
[0046] In some embodiments of the present invention, the source and drain regions 1002 are made of silicon or silicon germanium. In some embodiments of the present invention, the source and drain regions 1002 are p-type source / drain regions made of silicon germanium doped with boron to a boron concentration of about 1 to about 15 percent, e.g., 2 percent, although other boron concentrations are within the contemplated scope of the present invention.
[0047] 11 illustrates a cross-sectional view of semiconductor structure 100 taken along line Y2 of reference figure 101 after processing operations according to one or more embodiments of the present invention. In some embodiments of the present invention, a liner 1102 is formed over source and drain regions 1002. In some embodiments of the present invention, liner 1102 fills gap 1004 (i.e., contacts the sidewalls of isolation dielectric 702).
[0048] In some embodiments of the invention, the liner 1102 is conformally deposited over the semiconductor structure 100. In some embodiments of the invention, the liner 1102 has a thickness sufficient to completely fill the gap 1004, for example, from about 10 nm to about 60 nm, although other thicknesses are within the contemplated scope of the invention.
[0049] In some embodiments of the invention, the liner 1102 is formed using chemical vapor deposition (CVD), plasma enhanced chemical vapor deposition (PECVD), ultra-high vacuum chemical vapor deposition (UHVCVD), rapid thermal chemical vapor deposition (RTCVD), metal organic chemical vapor deposition (MOCVD), low pressure chemical vapor deposition (LPCVD), limited reaction processing CVD (LRPCVD), atomic layer deposition (ALD), physical vapor deposition (PVD), chemical solution deposition, molecular beam epitaxy (MBE), or other similar processes in combination with wet or dry etching processes. The liner 1102 can be made of any suitable dielectric material, for example, silicon nitride, although other materials are within the contemplated scope of the invention.
[0050] As further shown in FIG. 11, an interlayer dielectric (ILD) 1104 is formed over the substrate 104. The ILD 1104 can be made of any suitable dielectric material, such as, for example, oxide, low-k dielectric, nitride, silicon nitride, silicon oxide, SiON, SiC, SiOCN, and SiBCN. In some embodiments of the invention, the ILD 1104 is deposited over the semiconductor structure 100 and then recessed to expose the tops 1002a of the source and drain regions 1002 (as shown). In some embodiments of the invention, the ILD 1104 is recessed selectively to the liner 1102.
[0051] 12 illustrates a cross-sectional view of the semiconductor structure 100 taken along line Y2 of reference figure 101 after processing operations according to one or more embodiments of the present invention. In some embodiments of the present invention, exposed portions of the liner 1102 (e.g., portions above the isolation dielectric 702) are removed to expose surfaces of the upper portions 1002a of the source and drain regions 1002. In some embodiments of the present invention, the liner 1102 is removed selectively with respect to the ILD 1104 and / or the spacers 902. The liner 1102 can be selectively removed using a wet etch, a dry etch, or a combination of a wet etch, a dry etch, or both.
[0052] Once exposed, the upper portions 1002a of the source and drain regions 1002 are removed and replaced with source and drain regions 1202. The upper portions 1002a of the source and drain regions 1002 may be removed using, for example, hydrogen chloride (HCl) gas or an aqueous solution containing a mixture of ammonia and hydrogen peroxide. Once removed, the source and drain regions 1202 may be formed on the sidewalls of the semiconductor layer 402 in a manner similar to the source and drain regions 1002. For example, the source and drain regions 1202 may be epitaxially grown from the sidewalls of the semiconductor layer 402.
[0053] In some embodiments of the invention, source and drain regions 1202 have an opposite doping type than source and drain region 1002. For example, in embodiments in which source and drain region 1002 is a p-type region, such as silicon germanium doped with boron (SiGe:B), source and drain region 1202 can comprise an n-type region, such as silicon doped with phosphorus (Si:P). Similarly, if source and drain region 1002 is an n-type region, source and drain region 1202 can be a p-type region. The dopant concentration can range from about 1 to about 15 percent, such as 2 percent, although other dopant concentrations are within the contemplated scope of the invention.
[0054] 13 illustrates a cross-sectional view of semiconductor structure 100 taken along line Y2 of reference figure 101 after processing operations according to one or more embodiments of the present invention. In some embodiments of the present invention, a liner 1302 is formed over source and drain regions 1202. Liner 1302 may be formed in a similar manner and from similar materials as liner 1102. Liner 1302 may be made of the same dielectric as liner 1102 or a different dielectric.
[0055] In some embodiments of the invention, the height of the ILD 1104 is increased by depositing additional dielectric over the semiconductor structure 100. In some embodiments of the invention, the ILD 1104 is planarized, for example, using CMP. In some embodiments of the invention, the ILD 1104 is planarized to the surface of the spacers 902.
[0056] 13, the hard mask 804, sacrificial gate 802, and dielectric layer 602 are removed to release the semiconductor layer 402 (not shown separately). The hard mask 804, sacrificial gate 802, and dielectric layer 602 may then be replaced with an active gate 1304 (sometimes referred to as a metal gate or conductive gate). In some embodiments of the invention, the gate 1304 includes a first portion 1304a and a second portion 1304b (as shown).
[0057] The gate 1304 can be, for example, a high-k metal gate (HKMG) formed using the known replacement metal gate (RMG) process, or the so-called gate-first process, on the channel region of the nanosheet stack 102. As used herein, "channel region" refers to the portion of the semiconductor layer 402 on which the gate 1304 is formed and through which current passes from source to drain in the final device.
[0058] In some embodiments of the invention, the first portion 1304a of the gate 1304 includes a PFET gate stack and the second portion 1304b of the gate 1304 includes an NFET gate stack (or vice versa). For example, the first portion 1304a and the second portion 1304b of the gate 1304 may include a known gate dielectric (not shown) and a known work function metal stack (not shown) suitable for an NFET device or a PFET device.
[0059] In some embodiments of the invention, the gate dielectric is a high-k dielectric film formed on the surface (sidewall) of the semiconductor layer 402. The high-k dielectric film can be made of, for example, silicon oxide, silicon nitride, silicon oxynitride, boron nitride, high-k materials, or any combination of these materials. Examples of high-k materials include, but are not limited to, metal oxides such as hafnium oxide, hafnium silicon oxide, hafnium silicon oxynitride, lanthanum oxide, lanthanum aluminum oxide, zirconium oxide, zirconium silicon oxide, zirconium silicon oxynitride, tantalum oxide, titanium oxide, barium strontium titanium oxide, barium titanium oxide, strontium titanium oxide, yttrium oxide, aluminum oxide, lead scandium tantalum oxide, and lead zinc niobate. The high-k material can further include dopants such as lanthanum and aluminum. In some embodiments of the invention, the high-k dielectric film can have a thickness of about 0.5 nm to about 4 nm. In some embodiments of the present invention, the high-k dielectric film comprises hafnium oxide and has a thickness of about 1 nm, although other thicknesses are within the contemplated scope of the present invention.
[0060] In some embodiments of the invention, one or more work function layers are disposed between the high-k dielectric film and the bulk gate material. In some embodiments of the invention, the gate 1304 includes one or more work function layers but does not include a bulk gate material.
[0061] If present, the work function layer can be made from, for example, aluminum, lanthanum oxide, magnesium oxide, strontium titanate, strontium oxide, titanium nitride, tantalum nitride, hafnium nitride, tungsten nitride, molybdenum nitride, niobium nitride, hafnium silicon nitride, titanium aluminum nitride, tantalum silicon nitride, titanium aluminum carbide, tantalum carbide, and combinations thereof. The work function layer can serve to modify the work function of the gate 1304, allowing for tuning of the threshold voltage of the device. The work function layer can be formed to a thickness of about 0.5-6 nm, although other thicknesses are within the contemplated scope of the invention. In some embodiments of the invention, each of the work function layers can be formed to different thicknesses.
[0062] In some embodiments, the gate 1304 comprises a body formed from a bulk conductive gate material deposited on the work function layer and / or gate dielectric. The bulk gate material can include any suitable conductive material, such as, for example, a metal (e.g., tungsten, titanium, tantalum, ruthenium, zirconium, cobalt, copper, aluminum, lead, platinum, tin, silver, gold), a conductive metal compound material (e.g., tantalum nitride, titanium nitride, tantalum carbide, titanium carbide, titanium aluminum carbide, tungsten silicide, tungsten nitride, ruthenium oxide, cobalt silicide, nickel silicide), conductive carbon, graphene, or any suitable combination of these materials. The conductive gate material can further include a dopant incorporated during or after deposition.
[0063] 14 illustrates a cross-sectional view of semiconductor structure 100 taken along line Y2 of reference figure 101 after processing operations according to one or more embodiments of the present invention. In some embodiments of the present invention, portions of ILD 1104 are removed (patterned) to form source / drain contact trenches (not shown) that may be filled with a conductive material. In some embodiments of the present invention, the source / drain contact trenches expose surfaces of source and drain regions 1002b as well as surfaces of source and drain regions 1202. ILD 1104 may be patterned using a wet etch, a dry etch, or a combination of successive wet or dry etches or both.
[0064] In some embodiments of the invention, lower source / drain contacts 1402 are formed or deposited in the source / drain contact trenches to make electrical contact with source and drain region 1002b. Similarly, upper source / drain contacts 1404 are formed or deposited in the source / drain contact trenches to make electrical contact with source and drain region 1202.
[0065] The source / drain contacts 1402 / 1404 can be formed from conductive materials including copper or metals other than copper (e.g., tungsten, titanium, tantalum, ruthenium, zirconium, cobalt, aluminum, platinum), alloys thereof, conductive metal compound materials (e.g., tantalum nitride, titanium nitride, tantalum carbide, titanium carbide, titanium aluminum carbide, tungsten silicide, tungsten nitride, cobalt silicide, nickel silicide), conductive carbon, or any suitable combination of these materials. In some embodiments of the invention, the source / drain contacts 1402 / 1404 are formed from the same conductive material, e.g., cobalt, copper, ruthenium, or tungsten. In some embodiments of the invention, the source / drain contacts 1402 / 1404 are made from different conductive materials. In some embodiments of the present invention, source / drain contacts 1402 / 1404 each include a barrier liner (sometimes called a metal liner or barrier metal liner) to prevent diffusion into the surrounding dielectric (not shown).
[0066] 15 illustrates a flow diagram 1500 illustrating a method for forming a semiconductor device according to one or more embodiments of the present invention. As shown in block 1502, a nanosheet stack is formed on a substrate. The nanosheet stack can include an alternating first sacrificial layer and a second sacrificial layer. In some embodiments of the present invention, the first sacrificial layer includes silicon and the second sacrificial layer includes silicon germanium. In some embodiments of the present invention, a maximum thickness of the second sacrificial layer is below a defect critical thickness.
[0067] In some embodiments of the present invention, one of the first sacrificial layers is formed to a thickness greater than the remaining first sacrificial layers, in some embodiments of the present invention, the one layer having the greater thickness is a central-most layer of the first sacrificial layers.
[0068] At block 1504, the first sacrificial layer is removed to expose a surface of the second sacrificial layer. At block 1506, a semiconductor layer is formed on the exposed surface of the second sacrificial layer. The semiconductor layer includes a first set of semiconductor layers and a second set of semiconductor layers. In some embodiments of the present invention, the semiconductor layer is epitaxially grown from the exposed surface of the second sacrificial layer.
[0069] The second sacrificial layer is removed at block 1508. An isolation dielectric is formed between the first and second sets of semiconductor layers at block 1510. The method may further include forming a dielectric layer on exposed surfaces of the semiconductor layers.
[0070] In some embodiments of the invention, a first source and drain region is formed on the sidewalls of a first set of semiconductor layers and a second source and drain region is formed on the sidewalls of a second set of semiconductor layers. In some embodiments of the invention, the first source and drain region comprises a first dopant type and the second source and drain region comprises a second, different dopant type. In some embodiments of the invention, the first source and drain region comprises a p-type dopant and the second source and drain region comprises an n-type dopant.
[0071] In some embodiments of the invention, a first dielectric liner is formed over the first source and drain regions and a second dielectric liner is formed over the second source and drain regions, hi some embodiments of the invention, the second dielectric liner is formed directly on top of the first dielectric liner.
[0072] In some embodiments of the invention, lower source and drain contacts are formed on sidewalls of the first source and drain region. In some embodiments of the invention, upper source and drain contacts are formed on a top surface of the second source and drain region.
[0073] In some embodiments of the invention, a gate is formed over a channel region of the semiconductor layer. In some embodiments of the invention, the gate comprises a first portion and a second portion. In some embodiments of the invention, the first portion comprises a p-type gate stack and the second portion comprises an n-type gate stack.
[0074] The methods and resulting structures described herein can be used in the manufacture of IC chips. The resulting IC chips can be distributed by manufacturers in raw wafer form (i.e., as a single wafer with multiple unpackaged chips), as bare die, or in packaged form. In the latter case, the chips are mounted in single-chip packages (such as a plastic carrier with leads secured to a motherboard or other higher level carrier) or multi-chip packages (such as a ceramic carrier with either surface interconnects or embedded interconnects or both). In either case, the chips are integrated with other chips, discrete circuit elements or other signal processing devices, or a combination thereof, as part of either (a) an intermediate product such as a motherboard, or (b) a final product. The final product can be any product that contains the IC chip, ranging from toys and other low-end applications to advanced computer products with displays, keyboards or other input devices, and a central processor.
[0075] Various embodiments of the present invention are described herein with reference to the associated drawings. Alternative embodiments may be devised without departing from the scope of the present invention. Although various connections and relationships (e.g., above, below, adjacent, etc.) are described between elements in the following description and drawings, those skilled in the art will recognize that many of the relationships described herein are orientation independent if the described functionality is maintained even if the orientation is changed. These connections and / or relationships may be direct or indirect unless otherwise specified, and the present invention is not intended to be limited in this respect. Similarly, the term "coupled" and variations thereof describe having a communication path between two elements and do not imply a direct connection between elements with no intervening elements / connections between them. All of these variations are considered part of this specification. Thus, coupling of entities can refer to either direct or indirect coupling, and the relationship between entities can be direct or indirect. As an example of an indirect positional relationship, a reference herein to forming layer "A" on layer "B" includes the situation where one or more intermediate layers (e.g., layer "C") are between layers "A" and "B," so long as the relevant properties and functionality of layers "A" and "B" are not substantially altered by the intermediate layers.
[0076] The following definitions and abbreviations are used for interpretation of the claims and the specification. As used herein, the terms "comprises," "comprising," "includes," "including," "has," "having," "contains," or "containing," or any other variation thereof, are intended to cover a non-exclusive inclusion. For example, a composition, mixture, process, method, article, or device that includes a list of elements is not necessarily limited to only those elements and can include other elements not expressly listed or inherent to such composition, mixture, process, method, article, or device.
[0077] Moreover, the term "exemplary" is used herein to mean "serving as an example, instance, or illustration." Any embodiment or design described herein as "exemplary" is not necessarily to be construed as preferred or advantageous over other embodiments or designs. The terms "at least one" and "one or more" are understood to include any integer number greater than or equal to one, i.e., 1, 2, 3, 4, etc. The term "multiple" is understood to include any integer number greater than or equal to two, i.e., 2, 3, 4, 5, etc. The term "connected" can include indirect and direct "connected."
[0078] References herein to "one embodiment," "embodiment," "exemplary embodiment," and the like indicate that the embodiment being described may include a particular feature, structure, or characteristic, but that all embodiments may or may not include the particular feature, structure, or characteristic. Moreover, such phrases do not necessarily refer to the same embodiment. Furthermore, when a particular feature, structure, or characteristic is described in connection with an embodiment, it is submitted that it is within the knowledge of one of ordinary skill in the art to affect such feature, structure, or characteristic in connection with other embodiments, whether or not explicitly described.
[0079] For purposes of the following description, the terms "top", "bottom", "right", "left", "vertical", "horizontal", "upper", "lower" and their derivatives shall refer to the structures and methods described as oriented in the drawings. The terms "overlying", "atop", "on top", "positioned on" or "positioned atop" mean that a first element, such as a first structure, is on a second element, such as a second structure, and that an intervening element, such as an interface structure, may be between the first and second elements. The term "direct contact" means that a first element, such as a first structure, and a second element, such as a second structure, are connected without an intermediate conductive, insulating or semiconducting layer at the interface of the two elements.
[0080] Spatially relative terms, such as "below," "down," "lower," "upper," "above," and the like, are used herein to describe the relationship of one element or feature to another element or feature as shown in the figures for ease of description. It will be understood that the spatially relative terms are intended to encompass different orientations of the device during use or operation in addition to the orientation shown in the figures. For example, if the device in the figures is turned over, an element described as "below" or "below" the other element or feature would be oriented "above" the other element or feature. Thus, the term "down" can encompass both an orientation of above and below. The device can be otherwise oriented (e.g., rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein should be interpreted accordingly.
[0081] The terms "about," "substantially," "approximately," and variations thereof are intended to include the degree of error associated with the measurement of a particular quantity based on the equipment available at the time of filing this application. For example, "about" can include a range of ±8% or 5% or 2% of a given value.
[0082] For example, the phrase "selective to," such as "a first element selective to a second element," means that the first element may be etched and the second element may act as an etch stop.
[0083] The term "conformal" (e.g., conformal layer or conformal deposition) means that the thickness of a layer is substantially the same on all surfaces or that the thickness variation is less than 15% of the nominal thickness of the layer.
[0084] The terms "epitaxially grown and / or deposited" and "epitaxially formed and / or grown" refer to the growth of one semiconductor material (a crystalline material) on a deposition surface of another semiconductor material (a crystalline material) where the semiconductor material grown (the crystalline overlayer) has substantially the same crystalline properties as the semiconductor material of the deposition surface (the seed material). In an epitaxial deposition process, the chemical reactants provided by the source gases can be controlled and system parameters can be set so that the deposition atoms arrive at the deposition surface of the semiconductor substrate with sufficient energy to move around on the surface such that the deposition atoms are oriented in the crystalline arrangement of the atoms of the deposition surface. The epitaxially grown semiconductor material can have substantially the same crystalline properties as the deposition surface on which the epitaxially grown material is formed. For example, <100> Epitaxially grown semiconductor material deposited on an oriented crystalline surface is <100> In some embodiments of the present invention, the epitaxial growth and / or deposition process may be selective to formation on semiconductor surfaces and may or may not deposit material on other exposed surfaces, such as silicon dioxide or silicon nitride surfaces.
[0085] As used herein, "p-type" refers to the addition of impurities to an intrinsic semiconductor that creates a valence electron deficiency. In silicon-containing substrates, examples of p-type dopants, or impurities, include, but are not limited to, boron, aluminum, gallium, and indium.
[0086] As used herein, "n-type" refers to the addition of an impurity that provides free electrons to an intrinsic semiconductor. In silicon-containing substrates, examples of n-type dopants, or impurities, include, but are not limited to, antimony, arsenic, and phosphorus.
[0087] As noted earlier herein, for the sake of brevity, conventional techniques relating to the manufacture of semiconductor devices and integrated circuits (ICs) may or may not be described in detail herein. However, by way of background, a more general description of a semiconductor device manufacturing process that may be utilized in practicing one or more embodiments of the present invention is now provided. While the specific manufacturing operations used in practicing one or more embodiments of the present invention may be individually known, the described combination of operations and / or resulting structures of the present invention is unique. Thus, the unique combination of operations described in connection with the manufacture of semiconductor devices in accordance with the present invention utilizes a variety of individually known physical and chemical processes performed on a semiconductor (e.g., silicon) substrate, some of which are described in the immediately following paragraphs.
[0088] In general, the various processes used to form microchips that are packaged into ICs fall into four general categories: film deposition, removal / etching, semiconductor doping, and patterning / lithography. Deposition is any process that grows, coats, or otherwise transfers material onto a wafer. Available techniques include physical vapor deposition (PVD), chemical vapor deposition (CVD), electrochemical deposition (ECD), molecular beam epitaxy (MBE), and, more recently, atomic layer deposition (ALD), among others. Removal / etching is any process that removes material from a wafer. Examples include etching processes (either wet or dry), chemical mechanical planarization (CMP), and others. For example, reactive ion etching (RIE) is a type of dry etching that uses a chemically reactive plasma to remove material, such as semiconductor material, in a masked pattern by exposing the material to a bombardment of ions that remove some of the material from the exposed surface. The plasma is typically generated by an electromagnetic field under low pressure (vacuum). Semiconductor doping is the modification of electrical properties, for example by doping the source and drain of a transistor, typically by diffusion or ion implantation or both. These doping processes are followed by furnace anneals or rapid thermal anneals (RTA). The annealing serves to activate the implanted dopants. Films, both conductors (e.g., polysilicon, aluminum, copper, etc.) and insulators (e.g., various forms of silicon dioxide, silicon nitride, etc.), are used to connect and separate transistors and their components. By selectively doping various areas of a semiconductor substrate, the conductivity of the substrate can be changed by the application of a voltage. By creating structures of these various components, millions of transistors can be constructed and wired together to form the complex circuits of modern microelectronic devices. Semiconductor lithography is the formation of a three-dimensional relief image or pattern on a semiconductor substrate and the subsequent transfer of that pattern to a substrate. In semiconductor lithography, the pattern is formed by a light-sensitive polymer called a photoresist.To build the intricate structures that make up the transistors and the numerous wires that connect the circuit's millions of transistors, lithography and etch pattern transfer steps are repeated multiple times. Each pattern printed on the wafer is aligned with a previously formed pattern, and conductors, insulators and selectively doped regions are gradually built up to form the final device.
[0089] The flow charts and block diagrams in the figures illustrate possible implementations of manufacturing and / or operational methods according to various embodiments of the present invention. Various functions / operations of the method are represented in the flow charts by blocks. In some alternative implementations, the functions noted in the blocks may be performed in an order different from that noted in the figures. For example, two blocks shown in succession may in fact be executed substantially simultaneously, or the blocks may sometimes be executed in the reverse order, depending on the functionality involved.
[0090] The description of various embodiments of the present invention is presented for illustrative purposes, but is not intended to be exhaustive or limited to the described embodiments. Many modifications and variations will be apparent to those skilled in the art without departing from the scope of the described embodiments. The terms used herein are selected to best explain the principles of the embodiments, practical applications, or technical improvements to the technology found in the market, or to enable other skilled in the art to understand the embodiments described herein.
Claims
1. 1. A method for forming a semiconductor device, comprising: forming a nanosheet stack on a substrate, the nanosheet stack including alternating first and second sacrificial layers, one of the first sacrificial layers having a thickness greater than the remaining first sacrificial layers; removing the first sacrificial layer; forming a semiconductor layer on a surface of the second sacrificial layer, the semiconductor layer including a first set of semiconductor layers and a second set of semiconductor layers; removing the second sacrificial layer; forming an isolation dielectric between the first set of semiconductor layers and the second set of semiconductor layers; A method comprising:
2. The method of claim 1 , wherein the first sacrificial layer comprises silicon and the second sacrificial layer comprises silicon germanium.
3. The method of claim 1 , wherein the one layer having the greater thickness comprises a central most layer of the first sacrificial layer.
4. The method of claim 1 , wherein a maximum thickness of the second sacrificial layer is below a defect critical thickness.
5. The method of claim 4 , wherein the semiconductor layer is epitaxially grown from an exposed surface of the second sacrificial layer.
6. The method of claim 1 further comprising forming a dielectric layer on an exposed surface of the semiconductor layer.
7. 2. The method of claim 1, further comprising forming first source and drain regions on sidewalls of the first set of semiconductor layers and forming second source and drain regions on sidewalls of the second set of semiconductor layers.
8. 8. The method of claim 7, wherein the first source and drain regions comprise a first dopant type and the second source and drain regions comprise a second dopant type.
9. 9. The method of claim 8, wherein the first source and drain regions comprise a p-type dopant and the second source and drain regions comprise an n-type dopant.
10. 8. The method of claim 7, further comprising forming a first dielectric liner over the first source and drain regions and forming a second dielectric liner over the second source and drain regions.
11. The method of claim 10 , wherein the second dielectric liner is on top of the first dielectric liner.
12. The method of claim 10 further comprising forming lower source and drain contacts on sidewalls of the first source and drain regions.
13. 13. The method of claim 12, further comprising forming upper source and drain contacts on a top surface of the second source and drain regions.
14. The method of claim 1 , further comprising forming a gate over a channel region of the semiconductor layer.
15. 15. The method of claim 14, wherein the gate comprises a first portion and a second portion, the first portion comprising a p-type gate stack and the second portion comprising an n-type gate stack.
16. a nanosheet stack on a substrate, the nanosheet stack including a first set of semiconducting layers and a second set of semiconducting layers; an isolation dielectric between the first set of semiconductor layers and the second set of semiconductor layers; first source and drain regions on sidewalls of the first set of semiconductor layers and second source and drain regions on sidewalls of the second set of semiconductor layers, the first source and drain regions comprising a first dopant type and the second source and drain regions comprising a second dopant type; lower source and drain contacts on sidewalls of the first source and drain regions; upper source and drain contacts on the upper surface of the second source and drain regions; A semiconductor device comprising:
17. 17. The semiconductor device of claim 16, wherein the first source and drain regions comprise a p-type dopant and the second source and drain regions comprise an n-type dopant.
18. 17. The semiconductor device of claim 16, further comprising a gate, a first portion of the gate formed over a channel region of the first set of semiconductor layers and a second portion of the gate formed over a channel region of the second set of semiconductor layers.
19. 17. The semiconductor device of claim 16, wherein the isolation dielectric comprises a dielectric shell that surrounds but physically separates the first and second sets of semiconductor layers.
20. 17. The semiconductor device of claim 16, further comprising a dielectric liner between the first source and drain regions and the second source and drain regions.
Citation Information
Patent Citations
Gate-all-around nanowire device and method for manufacturing such a device
US20170040321A1
Vertically stacked nfets and pfets with gate-all-around structure
US20190131396A1
Vertically-integrated two-dimensional (2D) semiconductor slabs in complementary field effect transistor (CFET) cell circuits, and method of fabricating
US20200235098A1
Gate-all-around integrated circuit structures having source or drain structures with epitaxial nubs
US20200303502A1
Stacked Nanosheet CFET with Gate All Around Structure
US20210265345A1