Microinductor coil and method of manufacturing same
The microinductor coil design addresses conductor damage and interlayer defects through N-layered open annular conductors connected by vias, enhancing performance and reducing AC loss in high-frequency applications.
Patent Information
- Application Number
- JP2023550142
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-11-10
- Filing Date
- 2023-03-06
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2043-03-06
AI Technical Summary
Conventional inductor coil manufacturing methods for power modules in power management systems face issues such as conductor damage and interlayer defects due to excessive tension and winding gaps, especially with small wire diameters, leading to performance degradation.
A microinductor coil design composed of N layers of open annular planar conductors connected via vias, avoiding excessive tension and defects by using etching and plating processes to form conductive vias within insulating layers.
The new design reduces conductor damage and interlayer defects, maintaining high performance and reducing AC loss at high frequencies by minimizing skin effect and conductor resistance.
Smart Images

Figure 2024543280000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to the technical field of inductor coils, in particular to H01F27 / 30, more particularly to a micro inductor coil and a method for manufacturing the same. [Background technology]
[0002] In the power management systems of communication and computing infrastructure, power module means are increasingly being used by equipment manufacturers. Power module means is a technology based on discrete switching power supplies, which converts the power bus of the equipment to each point of load (POL) in the infrastructure system through DC / DC, greatly reducing the power loss of the circuit. However, this technology places strict requirements on the high density and high integration of power modules, and designers need to balance high performance and miniaturization when selecting devices.
[0003] As an important component of a power module, the micro structure of an inductor depends on the coil design and manufacturing process. The traditional method of making an inductor coil is to pull a conductor by pulling it along the trajectory of a spindle, and then wind the conductor around a bobbin or magnetic core to form a multi-turn winding. For conductors with very small wire diameters or cross-sectional areas, this winding method is highly likely to cause defects such as enamel damage and conductor breakage due to excessive tension during winding of the conductor. In addition, during winding of the coil, winding gaps are inevitably generated in the conductor due to the crossing between turns, which causes interlayer defects, and the crossing between turns is also a factor that prevents the coil design from achieving the desired single coil. For example, Chinese patent CN202122097482 provides an inductor coil mechanism, which assembles multiple coils by installing lantern rings, and in this method, excessive tension during winding of a single coil conductor causes defects such as enamel damage and conductor judgment. Summary of the Invention [Means for solving the problem]
[0004] In response to some problems existing in the prior art, a first aspect of the present invention provides a microinductor coil comprising N layers of non-closed annular planar conductors, where N is greater than or equal to 2, vertically distributed and connected through vias, with a physical insulating layer formed between adjacent non-closed annular planar conductors outside the vias, and coil pins including a first coil pin provided on the bottom layer of the non-closed annular planar conductors and a second coil pin provided on the top layer of the non-closed annular planar conductors.
[0005] Compared with the conventional method of winding using a conductor coil, the microinductor coil of the present application is composed of N layers of open annular planar conductors, and the N layers of open annular planar conductors are connected through vias. This avoids defects such as enamel damage and conductor breakage caused by excessive tension when winding the conductor in the conventional winding method when the wire diameter or cross-sectional area is very small, and also avoids interlayer defects.
[0006] In one embodiment, the material of the physical insulating layer is an insulating material.
[0007] In one embodiment, the thickness of the annular planar conductor is less than or equal to six times the skin depth, preferably less than or equal to four times the skin depth, and more preferably less than or equal to two times the skin depth.
[0008] The formula for calculating the skin depth is Equation 1.
[0009]
number
[0010] More specifically, when the coil of the present invention is applied to frequencies of 300,000 Hz or more, the thickness of the annular planar conductor is 0.56 mm or less, preferably 0.28 mm or less, and when the coil of the present invention is applied to frequencies of 2,000,000 Hz or more, the thickness of the annular planar conductor is 0.1 mm or less, preferably 0.053 mm or less.
[0011] The applicant has accidentally discovered that when the thickness of the annular planar conductor is four times the skin depth or less, and particularly when it is twice the skin depth or less, the impact of the skin effect on the microinductor coil of the present invention is small, and resistance and inductance losses are reduced.
[0012] In the present application, the width of the annular planar conductor is not particularly limited, and can be appropriately selected by those skilled in the art as required, and examples of the width include 250 μm, 300 μm, and the like.
[0013] In one embodiment, the inner annular cross-sectional area A1 of the N-layer annular planar conductor is equal to or less than the peripheral cross-sectional area A2 of the annular planar conductor, specifically, A1 is the middle grey area and A2 is the peripheral grey area, as shown in FIG.
[0014] Applicant has fortuitously discovered that when the inner ring size of the annular planar conductor is controlled within the range of the present application, the inductance value is optimal.
[0015] In one embodiment, the vias are disposed in the physical insulation layers, and the number of vias in each physical insulation layer is 1 or more, preferably 2 or more, and the specific number can be appropriately selected by those skilled in the art. In addition, there is no particular limitation on the via hole diameter, and the hole diameter can be appropriately selected by those skilled in the art.
[0016] In the present invention, a via is a through hole having electrical conductivity.
[0017] A second aspect of the present invention provides a method for manufacturing the microinductor coil, comprising the steps of: (1) coating a layer of conductive material on a surface of an insulating material, etching to obtain an unclosed annular planar conductor and a first coil pin, then filling the etched portion with insulating material, coating a layer of insulating material on the top of the annular planar conductor, boring and plating to obtain a physical insulating layer including a via, repeating the above operations to obtain N layers of unclosed annular planar conductors, etching the last layer of the annular planar conductor to obtain a second coil pin, and coating an insulating material on the top surface of the etched and filled conductor; and (2) maintaining a predetermined insulating film thickness and removing excess insulating material on the inside and outside of the annular planar conductor by laser cutting.
[0018] In one embodiment, the method for manufacturing the microinductor coil comprises: (1) coating a layer of conductive material on a surface of an insulating material, etching the conductive material to form an open annular planar conductor, etching to obtain a first coil pin, filling the etched conductor portion with insulating material, coating a layer of insulating material on the surface of the conductor, and then boring and plating the insulating material to form a via through the insulating layer; (2) coating a layer of conductive material on the surface of the insulating material with the embedded vias, etching the conductive material to form an open annular planar conductor, filling the etched conductor portion with insulating material, coating the top surface of the etched and filled conductor with insulating material, boring and plating the insulating material to form a via penetrating the insulating layer, and repeating step (2) to obtain N layers of open annular planar conductors coated with insulating material; (3) coating a layer of conductive material on the surface of the top insulating material of step (2), etching the conductive material to form an open annular planar conductor and a second coil pin, filling the etched conductor portion with insulating material, and coating an insulating material on the top surface of the etched and filled conductor; (4) maintaining a predetermined insulating film thickness and removing excess insulating material inside and outside the annular planar conductor by laser cutting.
[0019] In one embodiment, the insulating material is selected from any one or more of polyimide, polyamide, and epoxy resin.
[0020] In the present application, the conductive material is a metallic material, preferably copper.
[0021] In the present application, the thickness of the insulating film is not particularly limited, and examples of the thickness include 20 μm, 25 μm, and 30 μm.
[0022] Compared with the prior art, the present invention has the following beneficial effects:
[0023] The manufacturing method of the microinductor coil of the present invention forms annular conductors by etching means, and the conductors of each layer are connected through plated conductive holes embedded in the insulating layer, thus avoiding the problem of interlayer crossover that occurs in the conventional coil winding process, and also avoiding the very high possibility of defects such as enamel damage and conductor breakage occurring due to excessive tension when winding the conductor in the conventional process when the wire diameter or cross-sectional area of the conductor is very small. [Brief description of the drawings]
[0024] [Figure 1] FIG. 1 is a manufacturing flow chart for a microinductor coil. [Diagram 2] FIG. 2 is a structural schematic diagram of a microinductor coil, in which 1 is the first coil pin, 2 is the second coil pin, and 3 is the annular planar conductor. [Diagram 3] FIG. 3 is a test diagram of AC resistance in Example 1 and Comparative Example 1. [Figure 4] FIG. 4 is a top perspective view of the microinductor coil in the first embodiment. [Diagram 5] FIG. 5 is a schematic diagram of the inner ring area of a microinductor coil. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0025] The present invention will now be described with reference to specific embodiments, but is not limited to the specific examples described below.
[0026] Example 1 As shown in FIG. 2, the micro-inductor coil includes six layers of non-closed annular planar conductors 3 and a coil pin, and the six layers of non-closed annular planar conductors 3 are vertically distributed and connected through vias, and a physical insulation layer is formed between adjacent non-closed annular planar conductors outside the vias with one layer of epoxy resin, and the thickness of the annular planar conductor is 48.5 μm and the width is 250 μm.
[0027] The coil pins include a first coil pin provided on the bottom layer of the non-closed annular planar conductor and a second coil pin provided on the top layer of the non-closed annular planar conductor. A top perspective view of the obtained microinductor coil is shown in FIG.
[0028] Regarding the manufacturing method of the microinductor coil, A copper piece coated with a surface of polyimide material with a size of 1400μm*1200μm*25μm was etched to obtain a six-layered open annular planar conductor coated with epoxy resin. Adjacent conductors were connected through two plated conductive holes with a hole diameter of 100μm, the thickness of the annular conductor was 48.5μm, the width was 250μm, and the inner ring size of the annular conductor was 450μm*650μm. The first coil pin was connected to the open end of the bottom layer annular planar conductor, and the second coil pin was connected to the open end of the top layer annular planar conductor. The excess polyimide material on the conductor surface was removed by laser cutting, and the insulation thickness of 25μm was maintained. The specific flow chart was shown in Figure 1.
[0029] The above coil is packaged in a magnetic material with a size of 1400*1200*1000, the relative permeability of the magnetic material is 30, and the cross-sectional area Ae of the magnetic core of the inductor is 0.2925mm 2 It was.
[0030] Example 2 The microinductor coil was similar to Example 1, except that the thickness of the annular planar conductor was 60 μm.
[0031] The manufacturing method of the microinductor coil was the same as in Example 1.
[0032] The above coil is packaged in a magnetic material with a size of 1400*1200*1000, the relative permeability of the magnetic material is 30, and the cross-sectional area Ae of the magnetic core of the inductor is 0.2925mm 2 It was.
[0033] Example 3 The microinductor coil was similar to Example 1, except that the thickness of the annular planar conductor was 25 μm.
[0034] The manufacturing method of the microinductor coil was the same as in Example 1.
[0035] The above coil is packaged in a magnetic material with a size of 1400*1200*1000, the relative permeability of the magnetic material is 30, and the cross-sectional area Ae of the magnetic core of the inductor is 0.2925mm 2 It was.
[0036] Example 4 The microinductor coil and the manufacturing method were the same as in the first embodiment.
[0037] The above coil is packaged in a magnetic material with a size of 1400*1200*1000, the relative permeability of the magnetic material is 30, and the cross-sectional area Ae of the magnetic core of the inductor is 0.5525mm 2 It was.
[0038] Example 5 The microinductor coil and the manufacturing method were the same as in the first embodiment.
[0039] The coil is packaged in a magnetic material with a size of 1400*1200*1000, the relative permeability of the magnetic material is 30, and the cross-sectional area Ae of the magnetic core of the inductor is 0.6825mm2 It was.
[0040] Inductance characteristics tests were conducted on Examples 1-5, and the results are shown in Table 1.
[0041] [Table 1]
[0042] As can be seen from the results of Examples 1 to 3, the thicker the annular conductor, the lower the inductance and resistance of the inductor. Also, as can be seen from the test results of Examples 1 to 5, when the inner ring size of the annular conductor, i.e., the cross-sectional area Ae of the magnetic core, increases within a certain range, the inductance value increases. When the inner ring size of the annular conductor increases to a certain value, the inductance value decreases.
[0043] Comparative Example 1 The copper wire was wound around a rectangular bobbin with a size of 450μm*650μm, the number of turns was 6, divided into 3 inner turns and 3 outer turns. The diameter of the copper wire was 120μm, the thickness of the enamel was 25μm, the first coil pin was formed by the inner coil in the opposite direction to the winding direction, and the second coil pin was formed by the outer coil in the unwinding direction.
[0044] An AC resistance test is carried out for Example 1 and Comparative Example 1, and the test results are shown in Figure 3. As can be seen from Figure 3, the resistance of the conductor in Example 1 of the present invention changes less with current, because the size of the conductor produced by the present invention is smaller, and therefore the skin depth effect is lower than that of the coil produced by traditional winding. This is advantageous in ensuring low AC loss of the inductor at high frequencies.
Claims
1. A micro inductor coil, N layers of non-closed annular planar conductors are vertically distributed and connected through vias, and a physical insulating layer is formed between adjacent non-closed annular planar conductors outside the vias, where N≧2; a first coil pin provided on the bottom layer of the open annular planar conductor; a second coil pin provided on a top layer of the non-closed annular planar conductor; A coil pin including: A microinductor coil comprising:
2. 2. The microinductor coil of claim 1, wherein the material of the physical insulating layer is an insulating material.
3. 3. The micro-inductor coil of claim 2, wherein the insulating material is selected from one or more of polyimide, polyamide, and epoxy resin.
4. A microinductor coil as claimed in any one of claims 1 to 3, characterized in that the thickness of the annular planar conductor is less than or equal to six times the skin depth.
5. 5. The microinductor coil of claim 4, wherein the thickness of the annular planar conductor is less than four times the skin depth, and preferably less than two times the skin depth.
6. The micro-inductor coil according to claim 4, characterized in that the calculation of the skin depth must satisfy Equation 1. [0010] where f is the frequency in Hz and Δ is the skin depth in mm.
7. 7. The microinductor coil of claim 6, wherein an inner cross-sectional area A1 of the N layers of the annular planar conductor is equal to or smaller than a peripheral cross-sectional area A2 of the annular planar conductor.
8. The microinductor coil of claim 7, characterized in that the vias are located in the physical insulating layers, and the number of vias in each physical insulating layer is greater than or equal to 1, and preferably greater than or equal to 2.
9. (1) Coating a layer of conductive material on the surface of an insulating material, etching to obtain an unclosed annular planar conductor and a first coil pin, then filling the etched portion with insulating material, coating a layer of insulating material on the top of the annular planar conductor, boring and plating to obtain a physical insulating layer including a via, repeating the above steps to obtain N layers of unclosed annular planar conductors, etching the last layer of the annular planar conductor to obtain a second coil pin, and coating insulating material on the top surface of the etched and filled conductor; (2) maintaining a predetermined insulating film thickness and removing excess insulating material on the inside and outside of the annular planar conductor by laser cutting.
Citation Information
Patent Citations
Laminated chip coil
JP1990256208A
Divided lamination type coil
JP1993121242A
Coil and its manufacture and wiring board for coil
JP1997035206A
Inductor built-in printed wiring board and its manufacturing method
JP2002324962A
Transformer and coil for transformer
JP2004349562A