Semiconductor Device Package

Thin-form-factor semiconductor device packages with silicon core frames and advanced manufacturing techniques address scaling and thermal issues, achieving efficient power distribution and signal transmission, thus improving performance and reducing costs.

JP2024543400APending Publication Date: 2024-11-21APPLIED MATERIALS INC

Patent Information

Application Number
JP2024527518
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-11-11
Filing Date
2022-10-26
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

Conventional semiconductor device packages face challenges in maintaining device scaling and performance due to limitations of organic package substrates, particularly in forming fine features and managing thermal expansion mismatch, leading to high costs and inefficient power usage.

Method used

The development of thin-form-factor semiconductor device packages using a silicon core frame with integrated silicon interposers and advanced manufacturing processes, including microblasting and laser patterning, to create high-density interconnects and reduce mechanical defects, enabling efficient power distribution and signal transmission.

Benefits of technology

This approach allows for reduced package size, improved electrical performance, and cost-effectiveness by overcoming the limitations of traditional packaging materials, enhancing bandwidth and power efficiency while maintaining structural integrity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024543400000001_ABST
    Figure 2024543400000001_ABST
Patent Text Reader

Abstract

The present disclosure relates to a method and apparatus for forming a thin form factor semiconductor device package. In certain embodiments, a glass or silicon substrate is patterned by laser ablation to form structures for subsequent formation of interconnects through the glass or silicon substrate. The substrate is then utilized as a frame for forming a semiconductor device package, which may have one or more embedded double-sided dies within the semiconductor device package. In certain embodiments, a pre-structured insulating film is laminated onto the substrate to form an insulating layer on the substrate. The insulating film may be pre-structured by laser ablation to form structures in the insulating film, followed by selective hardening of the sidewalls of the formed structures.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD OF THE DISCLOSURE Embodiments of the present disclosure relate generally to semiconductor device packages and methods of forming the same. More particularly, embodiments described herein relate to thin-form-factor semiconductor device package structures and methods of forming the same. [Background technology]

[0002] Ongoing trends in the development of semiconductor device technology are resulting in semiconductor components having reduced size and increased circuit density. In keeping with the demands for continually scaling semiconductor devices while simultaneously improving performance, these components and circuits are integrated into complex 3D semiconductor device packages that facilitate a significant reduction in device footprint and allow shorter and faster connections between components. Such packages may, for example, integrate a semiconductor chip and multiple other electronic components for mounting on a circuit board of an electronic device.

[0003] Semiconductor device packages have historically been fabricated on organic package substrates due to the ease of forming features and connections in the substrate and the relatively low package manufacturing costs associated with organic composites. However, as circuit density increases and semiconductor devices become smaller, the use of organic package substrates becomes impractical due to limitations in material structuring solutions to maintain device scaling and associated performance requirements.

[0004] More recently, 2.5D and / or 3D packages have been fabricated utilizing passive silicon interposers as redistribution layers to compensate for some of the limitations associated with organic package substrates. The potential for high bandwidth density, lower power chip-to-chip communication and heterogeneous integration requirements in advanced packaging applications is driving the use of silicon interposers. Furthermore, it remains difficult and costly to form features such as through silicon vias (TSVs) in silicon interposers. In particular, high aspect ratio silicon via etching, chemical mechanical planarization and semiconductor back-end-of-line (BEOL) interconnects impose high costs.

[0005] Thus, there is a need in the art for improved semiconductor device package structures and methods of forming same for advanced packaging applications. Summary of the Invention

[0006] SUMMARY OF THE DISCLOSURE Embodiments of the present disclosure relate to structures for thin form factor semiconductor device packages and methods of forming the same.

[0007] In certain embodiments, a package assembly is provided. The package assembly includes a core frame having a first surface opposite a second surface, the core frame being formed of a core frame material including silicon. The core frame further includes at least one cavity, in which a semiconductor die is disposed, the semiconductor die having electrical contacts disposed on two opposing sides of the semiconductor die, and a via including a via surface, the via defining an opening extending through the core frame from the first surface to the second surface. An insulating layer is disposed on the first surface and the second surface, the insulating layer contacting at least a portion of each side of the semiconductor die, an electrical interconnect disposed in the via, and an insulating layer disposed between the via surface and the electrical interconnect.

[0008] So that the above-listed features of the present disclosure may be understood in detail, a more particular description of the present disclosure briefly outlined above may be had by reference to embodiments, some of which are illustrated in the accompanying drawings, which should be noted, however, that the accompanying drawings represent only exemplary embodiments and therefore should not be considered as limiting the scope of the present disclosure, which may embrace other embodiments that are equally effective. [Brief description of the drawings]

[0009] [Figure 1] 4 is a flow diagram of a process for forming a semiconductor device package according to embodiments described herein. [Diagram 2] 4 is a flow diagram of a process for structuring a substrate to form a semiconductor device package according to embodiments described herein. [Figure 3A] 3A-3C are schematic cross-sectional views of the substrate at different stages of the substrate structuring process shown in FIG. 2 according to embodiments described herein. [Figure 3B] 3A-3C are schematic cross-sectional views of the substrate at different stages of the substrate structuring process shown in FIG. 2 according to embodiments described herein. [Figure 3C] 3A-3C are schematic cross-sectional views of the substrate at different stages of the substrate structuring process shown in FIG. 2 according to embodiments described herein. [Figure 3D] 3A-3C are schematic cross-sectional views of the substrate at different stages of the substrate structuring process shown in FIG. 2 according to embodiments described herein. [Figure 4A] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 4B] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 4C]1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 4D] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 4E] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 4F] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 5A] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 5B] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 5C] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 5D] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 5E] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 5F] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 6A] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 6B] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 6C]1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 6D] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 6E] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 7A] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 7B] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 7C] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 7D] 1A-1D are schematic cross-sectional views of a substrate at different stages of feature formation and subsequent damage removal according to embodiments described herein. [Figure 8] Schematic top view of a substrate structured using the processes shown in Figures 2, 3A-3D, 4A-4F, 5A-5F, 6A-6E and 7A-7D according to embodiments described herein. [Figure 9] 4 is a process flow diagram for forming an embedded die assembly having through-assembly vias and contact holes according to embodiments described herein. [Figure 10A] 10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 10B] 10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 10C]10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 10D] 10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 10E] 10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 10F] 10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 10G] 10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 10H] 10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 10I] 10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 10J] 10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 10K] 10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 10L] 10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 10M] 10A-10C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 9 according to embodiments described herein. [Figure 11]4 is a process flow diagram for forming an embedded die assembly having through-assembly vias and contact holes according to embodiments described herein. [Figure 12A] 12A-12C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 11 according to embodiments described herein. [Figure 12B] 12A-12C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 11 according to embodiments described herein. [Figure 12C] 12A-12C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 11 according to embodiments described herein. [Figure 12D] 12A-12C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 11 according to embodiments described herein. [Figure 12E] 12A-12C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 11 according to embodiments described herein. [Figure 12F] 12A-12C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 11 according to embodiments described herein. [Figure 12G] 12A-12C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 11 according to embodiments described herein. [Figure 12H] 12A-12C are schematic cross-sectional views of the embedded die assembly at different stages of the process shown in FIG. 11 according to embodiments described herein. [Figure 13] 4 is a flow diagram of a process for forming an interconnect in a embedded die assembly according to embodiments described herein. [Figure 14A] 14A-14C are schematic cross-sectional views of the embedded die assembly at different stages of the interconnect formation process shown in FIG. 13 according to embodiments described herein. [Figure 14B]14A-14C are schematic cross-sectional views of the embedded die assembly at different stages of the interconnect formation process shown in FIG. 13 according to embodiments described herein. [Figure 14C] 14A-14C are schematic cross-sectional views of the embedded die assembly at different stages of the interconnect formation process shown in FIG. 13 according to embodiments described herein. [Figure 14D] 14A-14C are schematic cross-sectional views of the embedded die assembly at different stages of the interconnect formation process shown in FIG. 13 according to embodiments described herein. [Figure 14E] 14A-14C are schematic cross-sectional views of the embedded die assembly at different stages of the interconnect formation process shown in FIG. 13 according to embodiments described herein. [Figure 14F] 14A-14C are schematic cross-sectional views of the embedded die assembly at different stages of the interconnect formation process shown in FIG. 13 according to embodiments described herein. [Figure 14G] 14A-14C are schematic cross-sectional views of the embedded die assembly at different stages of the interconnect formation process shown in FIG. 13 according to embodiments described herein. [Figure 14H] 14A-14C are schematic cross-sectional views of the embedded die assembly at different stages of the interconnect formation process shown in FIG. 13 according to embodiments described herein. [Figure 15] 4 is a flow diagram of a process for forming a redistribution layer on an embedded die assembly and subsequent package singulation according to embodiments described herein. [Figure 16A] 16A-16C are schematic cross-sectional views of an embedded die assembly at different stages of forming a redistribution layer and subsequent package singulation as shown in FIG. 15 according to embodiments described herein. [Figure 16B] 16A-16C are schematic cross-sectional views of an embedded die assembly at different stages of forming a redistribution layer and subsequent package singulation as shown in FIG. 15 according to embodiments described herein. [Figure 16C]16A-16C are schematic cross-sectional views of an embedded die assembly at different stages of forming a redistribution layer and subsequent package singulation as shown in FIG. 15 according to embodiments described herein. [Figure 16D] 16A-16C are schematic cross-sectional views of an embedded die assembly at different stages of forming a redistribution layer and subsequent package singulation as shown in FIG. 15 according to embodiments described herein. [Figure 16E] 16A-16C are schematic cross-sectional views of an embedded die assembly at different stages of forming a redistribution layer and subsequent package singulation as shown in FIG. 15 according to embodiments described herein. [Figure 16F] 16A-16C are schematic cross-sectional views of an embedded die assembly at different stages of forming a redistribution layer and subsequent package singulation as shown in FIG. 15 according to embodiments described herein. [Figure 16G] 16A-16C are schematic cross-sectional views of an embedded die assembly at different stages of forming a redistribution layer and subsequent package singulation as shown in FIG. 15 according to embodiments described herein. [Figure 16H] 16A-16C are schematic cross-sectional views of an embedded die assembly at different stages of forming a redistribution layer and subsequent package singulation as shown in FIG. 15 according to embodiments described herein. [Figure 16I] 16A-16C are schematic cross-sectional views of an embedded die assembly at different stages of forming a redistribution layer and subsequent package singulation as shown in FIG. 15 according to embodiments described herein. [Figure 16J] 16A-16C are schematic cross-sectional views of an embedded die assembly at different stages of forming a redistribution layer and subsequent package singulation as shown in FIG. 15 according to embodiments described herein. [Figure 16K] 16A-16C are schematic cross-sectional views of an embedded die assembly at different stages of forming a redistribution layer and subsequent package singulation as shown in FIG. 15 according to embodiments described herein. [Figure 16L]16A-16C are schematic cross-sectional views of an embedded die assembly at different stages of forming a redistribution layer and subsequent package singulation as shown in FIG. 15 according to embodiments described herein. [Figure 17A] 1A-16L are schematic cross-sectional views of an exemplary stack device including multiple semiconductor device packages formed using the process illustrated in FIGS. 1-16L according to embodiments described herein. [Figure 17B] 1A-16L are schematic cross-sectional views of an exemplary stack device including multiple semiconductor device packages formed using the process illustrated in FIGS. 1-16L according to embodiments described herein. [Figure 18A] 1A-1D are various schematic diagrams of an exemplary semiconductor device having a stiffening frame according to embodiments described herein. [Figure 18B] 1A-1D are various schematic diagrams of an exemplary semiconductor device having a stiffening frame according to embodiments described herein. [Figure 18C] 1A-1D are various schematic diagrams of an exemplary semiconductor device having a stiffening frame according to embodiments described herein. [Figure 18D] 1A-1D are various schematic diagrams of an exemplary semiconductor device having a stiffening frame according to embodiments described herein. [Figure 19] 1 is a flow diagram of a process for forming a stiffening frame on a buried die assembly according to embodiments described herein. [Figure 20A] 20A-20C are schematic cross-sectional views of an embedded die assembly at different stages of forming a stiffening frame as shown in FIG. 19 according to embodiments described herein. [Figure 20B] 20A-20C are schematic cross-sectional views of an embedded die assembly at different stages of forming a stiffening frame as shown in FIG. 19 according to embodiments described herein. [Figure 20C] 20A-20C are schematic cross-sectional views of an embedded die assembly at different stages of forming a stiffening frame as shown in FIG. 19 according to embodiments described herein. [Figure 20D] 20A-20C are schematic cross-sectional views of an embedded die assembly at different stages of forming a stiffening frame as shown in FIG. 19 according to embodiments described herein. [Figure 20E] 20A-20C are schematic cross-sectional views of an embedded die assembly at different stages of forming a stiffening frame as shown in FIG. 19 according to embodiments described herein. [Figure 20F] 20A-20C are schematic cross-sectional views of an embedded die assembly at different stages of forming a stiffening frame as shown in FIG. 19 according to embodiments described herein. [Figure 20G] 20A-20C are schematic cross-sectional views of an embedded die assembly at different stages of forming a stiffening frame as shown in FIG. 19 according to embodiments described herein. [Figure 20H] 20A-20C are schematic cross-sectional views of an embedded die assembly at different stages of forming a stiffening frame as shown in FIG. 19 according to embodiments described herein. [Figure 20I] 20A-20C are schematic cross-sectional views of an embedded die assembly at different stages of forming a stiffening frame as shown in FIG. 19 according to embodiments described herein. [Figure 20J] 20A-20C are schematic cross-sectional views of an embedded die assembly at different stages of forming a stiffening frame as shown in FIG. 19 according to embodiments described herein. [Figure 21] 1 is a schematic cross-sectional view of an exemplary device having a stiffening frame and one or more heat exchangers according to embodiments described herein. [Figure 22A] 1 is a schematic cross-sectional view of an exemplary device having a stiffening frame according to embodiments described herein. [Figure 22B] 1 is a schematic cross-sectional view of an exemplary device having a stiffening frame according to embodiments described herein. [Figure 23A] 1 is a schematic cross-sectional view of an exemplary device having a heat exchanger according to embodiments described herein. [Figure 23B]1 is a schematic cross-sectional view of an exemplary device having a heat exchanger according to embodiments described herein. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] For ease of understanding, wherever possible, identical reference numerals have been used to designate identical elements common to the figures. It is contemplated that elements and features of one embodiment may be beneficially incorporated in other embodiments without additional description.

[0011] The present disclosure relates to methods and apparatus for forming thin form factor semiconductor device packages. In certain embodiments, a substrate is structured or shaped by microblasting to allow for the formation of interconnects through the substrate. In other embodiments, the substrate is structured by direct laser patterning. The substrate is then utilized as a package frame or core frame for forming one or more semiconductor device packages with dies disposed therein. In yet other embodiments, the substrate is utilized as a core frame for a semiconductor device stack, such as a dynamic random access memory (DRAM) stack.

[0012] The methods and apparatus disclosed herein further include novel thin form factor semiconductor device packages intended to replace more conventional package structures utilizing fiberglass filled epoxy frames and silicon interposers as redistribution layers. In general, the scalability of current packages is limited by the stiffness and planarity of the materials (e.g., epoxy molding compounds, FR-4 and FR-5 grade woven fiberglass cloth with epoxy resin binders, etc.) utilized to form the various package structures. The inherent properties of these materials make it difficult to pattern fine (e.g., less than 50 μm) features in these materials. Furthermore, the thermal properties of current package materials can result in a coefficient of thermal expansion (CTE) mismatch between the packaging substrate, molding compound, and any semiconductor die integrated therein, such that current package structures require larger solder bumps with greater spacing to mitigate any warpage caused by the CTE mismatch. Thus, conventional packages are characterized by low die-to-package area ratios and low package through-bandwidth, resulting in low overall power efficiency. The methods and apparatus disclosed herein provide a semiconductor device package that overcomes many of the above-mentioned disadvantages associated with conventional package architectures.

[0013] 1 shows a flow diagram of an exemplary method 100 of forming a thin form factor semiconductor device package. Method 100 includes a number of operations 110, 120, 130, and 140, each of which will be described in more detail with reference to FIGS. 2-16L. The method may include one or more additional operations performed before any of the stated operations, between two of the stated operations, or after all of the stated operations (unless the context precludes this possibility).

[0014] Generally, the method 100 includes structuring a substrate for use as a core frame in operation 110. This operation is further described in more detail with reference to FIGS. 2, 3A-3D, 4A-4F, 5A-5F, 6A-6E, 7A-7D, and 8. In operation 120, an embedded die assembly is formed having one or more embedded dies and an insulating layer. This operation is described in more detail with reference to FIGS. 9 and 10A-10M, and 11 and 12A-12H. In operation 130, one or more interconnects for interconnecting the embedded die-frame set are formed within and / or through the embedded die assembly. This operation is described in more detail with reference to FIGS. 13 and 14A-14H. In operation 140, a first redistribution layer is formed on the embedded die assembly for relocating contacts of the interconnects to desired lateral positions on a surface of the embedded die assembly. In some embodiments, prior to singulating the individual packages from the embedded die assembly, one or more additional redistribution layers may be formed in addition to the first redistribution layer, which will be described in more detail with reference to Figures 15 and 16A-16L.

[0015] Figure 2 illustrates a flow diagram of an exemplary method 200 for structuring a substrate for use as a core frame during the formation of a semiconductor device package. Figures 3A-3D illustrate schematic cross-sectional views of a substrate 302 at different stages of the substrate structuring process 200 illustrated in Figure 2. Thus, for clarity, Figures 2 and 3A-3D will be discussed together herein.

[0016] The method 200 begins with operation 210 and corresponding FIG. 3A. A substrate 302 may be formed of a material such as, but not limited to, a III-V compound semiconductor material, silicon, crystalline silicon (e.g., Si <100> Or Si <111> The frame 302 may be formed of any suitable frame material, including silicon oxide, silicon germanium, doped or undoped silicon, doped or undoped polycrystalline silicon, silicon nitride, quartz, borosilicate glass, glass, sapphire, alumina, and ceramic. In certain embodiments, the substrate 302 is a monocrystalline p-type or n-type silicon substrate. In certain embodiments, the substrate 302 is a polycrystalline p-type or n-type silicon substrate. In another embodiment, the substrate 302 is a p-type or n-type silicon solar substrate. The substrate 302 may further have a polygonal or circular shape. For example, the substrate 302 may comprise a substantially square silicon substrate with or without chamfered edges having a lateral dimension between about 120 mm and about 180 mm. In another example, the substrate 302 may comprise a circular silicon-containing wafer having a diameter between about 20 mm and about 700 mm, such as between about 100 mm and about 500 mm, for example about 300 mm.

[0017] Unless otherwise specified, the embodiments and examples described herein are implemented on a substrate having a thickness of between about 50 μm and about 1000 μm, such as between about 90 μm and about 780 μm. For example, the substrate 302 has a thickness of between about 100 μm and about 300 μm, such as between about 110 μm and about 200 μm. In another example, the substrate 302 has a thickness of between about 60 μm and about 160 μm, such as between about 80 μm and about 120 μm.

[0018] Prior to operation 210, the substrate 302 may be sliced ​​and separated from the bulk material by wire sawing, scribing and breaking, mechanical abrasive sawing, or laser cutting. Slicing typically results in mechanical defects or deformations of the substrate surface formed by slicing, such as scratches, microcracks, chipping, and other mechanical defects. Thus, in operation 210, the substrate 302 is subjected to a first damage removal process to smooth and planarize the surface of the substrate 302 and remove any mechanical defects in preparation for subsequent structuring and packaging operations. In some embodiments, the substrate 302 may be further thinned by adjusting process parameters of the first damage removal process. For example, the thickness of the substrate 302 may be reduced by further exposure to the first damage removal process.

[0019] The damage removal process in operation 210 includes subjecting the substrate 302 to a substrate polishing process and / or an etching process, followed by a rinsing process and a drying process. In some embodiments, operation 210 includes a chemical mechanical polishing (CMP) process. In certain embodiments, the etching process is a wet etching process, including a buffered etch process that is selective to the removal of desired materials (e.g., contaminants and other undesirable compounds). In other embodiments, the etching process is a wet etching process that utilizes an isotropic aqueous etching process. Any suitable wet etchant or combination of wet etchants may be used for the wet etching process. In certain embodiments, the substrate 302 is immersed in an aqueous HF etching solution for etching. In another embodiment, the substrate 302 is immersed in an aqueous KOH etching solution for etching.

[0020] In some embodiments, during the etching process, the etching solution is heated to a temperature between about 30° C. and about 100° C., such as between about 40° C. and about 90° C. For example, the etching solution is heated to a temperature of about 70° C. In yet other embodiments, the etching process in operation 210 is a dry etching process. Examples of dry etching processes include plasma-based dry etching processes. The thickness of the substrate 302 is adjusted by controlling the time the substrate 302 is exposed to an etchant (e.g., an etching solution) used during the etching process. For example, the final thickness of the substrate 302 may be reduced by increasing the exposure to the etchant. Alternatively, the final thickness of the substrate 302 may be increased by decreasing the exposure to the etchant.

[0021] In operations 220 and 230, the now planarized substantially defect-free substrate 302 has one or more features, such as vias 303 and cavities 305, patterned and smoothed into the substrate 302 (one cavity 305 and four vias 303 are shown in cross-section of the underside of the substrate 302 in FIG. 3B). The vias 303 are utilized to form direct contact electrical interconnects through the substrate 302, and the cavities 305 are utilized to receive and encapsulate (i.e., embed) one or more semiconductor dies within the cavities 305. FIGS. 4A-4C, 5A-5C, 6A-6C, and 7A-7B generally illustrate cross-sectional views of the substrate 302 at different stages of a feature formation and damage or defect removal (e.g., smoothing) process according to embodiments described herein. Accordingly, operations 220 and 230 will now be described in more detail with reference to Figures 4A-4C, 5A-5C, 6A-6C and 7A-7B.

[0022] In embodiments in which the substrate 302 has a thickness of less than about 200 μm, such as about 100 μm or about 50 μm, the substrate 302 may first be bonded to an optional carrier plate 406, as shown in FIGS. 4A and 5A. The carrier plate 406 provides mechanical support to the substrate 302 during the substrate structuring process 200 and prevents the substrate 302 from breaking. The carrier plate 406 is formed of any suitable highly rigid material that is chemically and thermally stable, including but not limited to glass, ceramic, metal, and the like. The carrier plate 406 has a thickness of between about 1 mm and about 10 mm, such as between about 2 mm and about 5 mm. In certain embodiments, the carrier plate 406 has a textured structure. In other embodiments, the carrier plate 406 has a polished or smoothed surface.

[0023] The substrate 302 may be bonded to the carrier plate 406 via an adhesive layer 408. The adhesive layer 408 is formed of any suitable temporary bonding material, including, but not limited to, wax, glue, or similar bonding materials. The adhesive layer 408 is applied onto the carrier plate 406 by mechanical rolling, pressing, lamination, spin coating, or doctor-blading. In certain embodiments, the adhesive layer 408 is a water-soluble or solvent-soluble adhesive layer. In other embodiments, the adhesive layer 408 is a UV-release adhesive layer. In yet other embodiments, the adhesive layer 408 is a thermal-release adhesive layer. In such embodiments, the bonding properties of the adhesive layer 408 are degraded by subjecting it to a heat treatment, for example, by exposing the adhesive layer 408 to a temperature greater than 110° C., such as greater than 150° C. The adhesive layer 408 may further include one or more layers of additional films (not shown), such as liners, base films, pressure-sensitive films, and other suitable layers.

[0024] In some embodiments, after bonding the substrate 302 to the carrier plate 406, a resist film is applied to the substrate 302 to form the resist layer 404 shown in Figures 4A and 5A. In embodiments in which the substrate 302 has a thickness greater than about 200 μm, such as about 250 μm, the resist layer 404 is formed on the substrate 302 without first bonding the substrate 302 to the carrier plate 406. The resist layer 404 is used to transfer a desired pattern to the substrate 302 on which the resist layer 404 is formed during subsequent processing operations. After being patterned, the resist layer 404 protects selected areas of the substrate 302 underneath it during subsequent structuring operations.

[0025] The substrate 302 generally has a substantially planar surface on which the resist layer 404 is formed. In some embodiments, such as the embodiment shown in FIG. 5A, the resist layer 404 is bonded to the substrate 302 via a resist adhesive layer 409. The resist adhesive layer 409 is formed of any suitable temporary bonding material, including, but not limited to, polyvinyl alcohol, triesters including 2-ethyl-2-(hydroxymethyl)-1,3-propanediol, and other water-soluble or solvent-soluble materials. In certain embodiments, the resist adhesive layer 409 is formed of a material different from the adhesive layer 408. In certain embodiments, the composition of the resist adhesive layer 409 is substantially similar to the composition of the adhesive layer 408. The resist adhesive layer 409 is applied onto the substrate 302 by mechanical rolling, pressing, lamination, spin coating, or doctor blading. In other embodiments, the resist layer 404 is formed of a temporary bonding material, such as polyvinyl alcohol, and thus the resist layer 404 can be directly applied and bonded to the surface of the substrate 302. The resist layer 404 may include one or more layers, such as a first resist layer and a second resist layer (not shown).

[0026] In certain embodiments, such as the embodiment shown in FIG. 4A, the resist layer 404 is a photosensitive layer (e.g., photoresist). The resist layer 404 may include a solvent, a photoresist resin, and a photoacid generator. The photoresist resin may be any positive or negative photoresist resin. Exemplary photoresist resins include acrylates, novolac resins, poly(methyl methacrylate), and poly(olefin sulfone). Other photoresist resins may be used. The photoacid generator generates charged species, such as acid cations and anions, upon exposure to electromagnetic radiation. The photoacid generator may generate polarized species. The photoacid generator increases the sensitivity of the resin to electromagnetic radiation. Exemplary photoacid generators include sulfonic acid compounds, such as, for example, sulfonated salts, sulfonated esters, and sulfonyloxyketones. Other suitable photoacid generators include onium salts, such as aryl diazonium salts, halonium salts, aromatic sulfonium salts, and sulfoxonium salts, or selenium salts. Other representative photoacid generators include nitrobenzyl esters, s-triazine derivatives, ionic iodonium sulfonates, perfluoroalkanesulfonates, aryl triflates and their derivatives and analogs, pyrogallol derivatives, and alkyl disulfones. Other photoacid generators may also be used. In certain embodiments, such as the embodiment shown in FIG. 5A, the resist layer 404 is a laser-sensitive resist.

[0027] After forming the resist layer 404, the substrate 302 having the resist layer 404 formed thereon is exposed to electromagnetic radiation to pattern the resist layer 404 shown in FIG. 4B and FIG. 5B. In the embodiment shown by FIG. 4B, the substrate 302 having the resist layer 404 formed thereon is exposed to electromagnetic radiation in the ultraviolet (UV) range. Portions of the resist layer 404 are selectively exposed to UV radiation and portions of the resist layer 404 are selectively not exposed to UV radiation. Upon exposure to UV radiation, the selectively exposed portions of the resist layer 404 are structurally weakened (shown as hatched areas) while the non-selectively exposed portions maintain their structural integrity. In certain embodiments, prior to UV radiation exposure, a mask 412 having a desired pattern is formed on or adjacent to the photosensitive resist layer 404. In other embodiments, the mask 412 is a reticle disposed between the resist layer 404 and a UV radiation source. Mask 412 is configured to transfer a desired UV radiation pattern into resist layer 404. Mask 412 is formed from any suitable polymeric material, including, but not limited to, PTFE, PVDF, FEP, polyimide, and the like.

[0028] In the embodiment illustrated by FIG. 5B, the substrate 302 having a laser-sensitive resist layer 404 formed thereon is exposed to electromagnetic radiation generated by a laser source 307 instead of a UV radiation source. Thus, patterning is performed by targeted laser ablation without the use of a mask. The laser source 307 may be any type of laser suitable for patterning the resist layer 404. In some examples, the laser source 307 is a femtosecond green laser. In other examples, the laser source 307 is a femtosecond UV laser. The laser source 307 generates a continuous or pulsed laser beam 310 for patterning the resist layer 404. For example, the laser source 307 may generate a pulsed laser beam 310 having a frequency between 100 kHz and 1200 kHz, such as between about 200 kHz and about 1000 kHz. The laser source 307 is generally configured to form any desired pattern in the resist layer 404. It is further contemplated that the electromagnetic radiation during operation may alternatively include an electron beam or an ion beam instead of a laser beam.

[0029] The resist layer 404 may be formed of any material that has a suitable hardness after patterning the resist layer 404, such as after exposing a negative photoresist to electromagnetic radiation to crosslink the resist material. Generally, the resist layer 404 should have one or more desired mechanical properties after patterning (e.g., depositing, exposing, and developing) the resist layer 404. In certain embodiments, the resist layer 404 is formed of a material that has a Shore A scale hardness value of between 40 and 90, such as between 60 and 70, after patterning. For example, the resist layer 404 is formed of a material that has a Shore A scale hardness value of about 65 after patterning. In certain embodiments, the resist layer 404 is formed of a material that has a tensile strength of between about 0.5 MPa and about 10 MPa, such as between about 1 MPa and about 8 MPa, after patterning. For example, the resist layer 404 may be formed of a material that has a tensile strength of about 7 MPa after patterning. In certain embodiments, resist layer 404 is formed of a polydimethylsiloxane material, while in other embodiments, resist layer 404 is formed of polyvinyl alcohol, triesters including 2-ethyl-2-(hydroxymethyl)-1,3-propanediol, and the like.

[0030] Following patterning of the resist layer 404, the substrate 302 having the resist layer 404 formed thereon is microblasted to form the desired pattern on the substrate 302, as shown in Figures 4C and 5C. During this microblasting, a stream of powder particles 309 is propelled toward the substrate 302 by use of a high pressure carrier gas to remove exposed portions of the substrate 302 and / or layers formed thereon. This microblasting process is carried out using any suitable substrate ablading system.

[0031] The microblasting process is determined by the material properties of the powder particles 309, the momentum of the powder particles striking the exposed surface of the substrate 302, and the material properties of the substrate 302 and, when applicable, the selectively exposed portions of the resist layer 404. To achieve the desired substrate patterning characteristics, the type and size of the powder particles 309, the size of the ablading system's applicator nozzle and its distance to the substrate 302, the pressure of the carrier gas utilized to propel the powder particles 309, which pressure correlates with the carrier gas velocity and flow rate, and the density of the powder particles 309 in the fluid stream are adjusted. For example, the desired fluid pressure of the carrier gas used to propel the powder particles 309 towards the substrate 302 for a fixed desired nozzle orifice size of the microblasting device is determined based on the material of the substrate 302 and the powder particles 309. In certain embodiments, carrier gas and particle velocities between about 300 and about 1000 meters per second (m / s), and / or a flow rate of about 0.001 to about 0.002 cubic meters per second (m / s) are used. 3 The fluid pressure utilized to microblast the substrate 302 ranges between about 50 psi and about 150 psi, such as between about 75 psi and about 125 psi, to achieve a flow rate of between about 2350 m / s. For example, the fluid pressure of the inert gas (e.g., nitrogen (N2), CDA, argon) utilized to propel the powder particles 309 during microblasting is about 95 psi to achieve a carrier gas and particle velocity of about 2350 m / s. In certain embodiments, the applicator nozzle utilized to microblast the substrate 302 has an inner diameter between about 0.1 and about 2.5 millimeters (mm) and is disposed at a distance of between about 1 mm and about 5 mm, such as between about 2 mm and about 4 mm, from the substrate 302. For example, the applicator nozzle is disposed at a distance of about 3 mm from the substrate 302 during microblasting.

[0032] Typically, the microblasting process is performed with powder particles 309 that have sufficient hardness and a high melting point to prevent the particles from adhering when in contact with the substrate 302 and / or any layers formed on the substrate 302. For example, the microblasting process is performed with powder particles 309 formed of a ceramic material. In certain embodiments, the powder particles 309 utilized in the microblasting process are formed of aluminum oxide (Al2O3). In another embodiment, the powder particles 309 are formed of silicon carbide (SiC). Other suitable materials for the powder particles 309 are also contemplated. The particle size of the powder particles 309 generally ranges between about 15 μm and about 60 μm in diameter, such as between about 20 μm and about 40 μm in diameter. For example, the powder particles 309 have an average particle size of about 27.5 μm in diameter. In another example, the powder particles 309 have an average particle size of about 23 μm in diameter.

[0033] The effectiveness of the microblasting process in operation 220 shown in Figures 4C and 5C further depends on the material properties of the resist layer 404. Utilizing a material having too high a Shore A scale hardness may result in unnecessary bouncing of the powder particles 309 between the sidewalls of the resist layer 404, thus reducing the rate at which the powder particles 309 impact the substrate 302, and ultimately reducing the effectiveness of the powder particles 309 in eroding or removing exposed areas of the substrate 302. Conversely, utilizing a material having too low a Shore A scale hardness may result in unnecessary adhesion of the powder particles 309 to the resist layer 404. As mentioned above, it is contemplated to utilize a Shore A scale hardness value between about 40 and about 90 for the material of the resist layer 404.

[0034] In embodiments where the resist layer 404 is a photoresist, such as the embodiment shown in FIG. 4C, the substrate 302 remains unexposed at the start of the microblasting process. Thus, the powder particles 309 first impinge on the surface of the photoresist, thereby dislodging and removing material from the UV-exposed and structurally weakened portions of the photoresist. Eventually, the powder particles 309 penetrate and remove the weak UV-exposed portions, forming voids in the resist layer 404 and exposing the desired areas of the substrate 302, while other areas of the substrate 302 remain protected by the portions of the photoresist that were not UV-exposed. Microblasting then continues until the powder particles 309 dislodge and remove the desired amount or depth of material from the exposed areas of the substrate 302, forming the desired pattern in the substrate 302. In embodiments where the resist layer 404 is patterned by laser ablation, such as the embodiment shown in FIG. 5C, the desired areas of the substrate 302 are already exposed through the voids in the resist layer 404 prior to the microblasting process. Therefore, it is contemplated to minimize removal of the resist layer 404 during microblasting, or not remove the resist layer 404 at all during the microblasting process.

[0035] The above-described process in operation 220 for forming features in the substrate 302 may result in unwanted mechanical defects, such as chipping and cracking, in the surface of the substrate 302. Therefore, after performing operation 220 to form desired features in the substrate 302, in operation 230, the substrate 302 is subjected to a second damage removal and cleaning process to smooth the surface of the substrate 302 and remove unwanted debris, followed by stripping the resist layer 404 and optionally peeling the substrate 302 from the carrier plate 406. Figures 4D-4F and 5D-5F show schematic cross-sectional views of the substrate 302 at different stages of the second damage removal, cleaning, resist stripping and substrate stripping process according to embodiments described herein. Therefore, operation 230 will now be described in more detail with reference to Figures 4D-4F and 5D-5F.

[0036] The second damage removal process in operation 230 is substantially similar to the first damage removal process in operation 210 and includes subjecting the substrate 302 to an etching process, followed by rinsing and drying. The etching process continues for a predetermined time to smooth the surface of the substrate 302, particularly the surface that was subjected to the microblasting process. In another embodiment, the etching process is utilized to remove undesirable debris left by the microblasting process. Residual powder particles adhering to the substrate 302 may be removed during the etching process. Figures 4D and 5D show schematic views of the substrate 302 after the debris has been removed and the surface has been smoothed.

[0037] In certain embodiments, the etching process is a wet etching process utilizing a buffered etching process that preferentially etches the substrate surface over the material of the resist layer 404. For example, the buffered etching process is selective to polyvinyl alcohol. In other embodiments, the etching process is a wet etching process utilizing an aqueous etching process. Any suitable wet etchant or combination of wet etchants may be used for the wet etching process. In certain embodiments, the substrate 302 is immersed in an aqueous HF etching solution for etching. In another embodiment, the substrate 302 is immersed in an aqueous KOH etching solution for etching. Additionally, during the etching process, the etching solution may be heated to a temperature between about 40° C. and about 80° C., such as between about 50° C. and about 70° C. For example, the etching solution is heated to a temperature of about 60° C. The etching process may be isotropic or anisotropic. In yet other embodiments, the etching process in operation 230 is a dry etching process. An example of a dry etching process includes a plasma-based dry etching process.

[0038] After removing the debris and smoothing the substrate surface, the substrate 302 is subjected to a resist stripping process. As shown in FIG. 4E and FIG. 5E, this stripping process is utilized to strip the resist layer 404 from the substrate 302. In certain embodiments, a wet process is used to strip the resist layer 404 from the substrate 302 by dissolving / solubilizing the resist adhesive layer 409. Other types of etching processes to release the resist adhesive layer 409 are also contemplated. In certain embodiments, a mechanical rolling process is used to physically strip the resist layer 404 or the resist adhesive layer 409 from the substrate 302. In certain embodiments, an ashing process is used to remove the resist layer 404 from the substrate 302, for example, by using an oxygen plasma assisted process.

[0039] After the resist stripping process, the substrate 302 is subjected to an optional carrier stripping process, as shown in Figures 4F and 5F. The use of the carrier stripping process depends on whether the substrate 302 is bonded to a carrier plate 406 and the type of bonding material used to bond the substrate 302 and the carrier plate 406. As described above and shown in Figures 4A-4F and 5A-5F, in embodiments in which the substrate 302 has a thickness of less than about 200 μm, the substrate 302 is bonded to the carrier plate 406 for mechanical support during feature formation in operation 220. The substrate 302 is bonded to the carrier plate 406 via an adhesive layer 408. Thus, after microblasting and subsequent substrate etching and resist stripping, the substrate 302 bonded to the carrier plate 406 is subjected to a carrier stripping process to release the adhesive layer 408 and thereby strip the substrate 302 from the carrier plate 406.

[0040] In certain embodiments, adhesive layer 408 is released by subjecting substrate 302 to a bake process. Substrate 302 is exposed to a temperature between about 50° C. and about 300° C., such as between about 100° C. and about 250° C. For example, to release adhesive layer 408, substrate 302 is exposed to a temperature between about 150° C. and about 200° C., such as about 160° C., for a desired period of time. In other embodiments, adhesive layer 408 is released by exposing substrate 302 to UV radiation.

[0041] Figures 4F and 5F show substrate 302 in a schematic manner after operations 210-230 have been completed. The cross-section of substrate 302 in Figures 4F and 5F shows a single cavity 305 formed through substrate 302 with two vias 303 on either side of it. A schematic top view of substrate 302 after the operations described with reference to Figures 4A-4F and 5A-5F have been completed is shown in Figure 8, which will be described in more detail below.

[0042] 6A-6E show schematic cross-sectional views of substrate 302 during an alternative sequence for operations 220 and 230 similar to those described above. This alternative sequence shown for operations 220 and 230 includes patterning two major surfaces on either side of substrate 302 as opposed to patterning only one surface, thus increasing efficiency during structuring substrate 302. The embodiment shown in FIGS. 6A-6E includes substantially all of the processes described with reference to FIGS. 4A-4F and 5A-5F. For example, FIG. 6A corresponds to FIGS. 4A and 5A, FIG. 6B corresponds to FIGS. 4B and 5B, FIG. 6C corresponds to FIGS. 4C and 5C, FIG. 6D corresponds to FIGS. 4D and 5D, and FIG. 6E corresponds to FIGS. 4F and 5F. Unlike the previous embodiments, however, the embodiment of operation 220 illustrated in Figures 6A-6E includes a substrate 302 having two resist layers 404 formed on opposite major surfaces 606, 608 of the substrate 302, as opposed to a substrate 302 having one resist layer 404 formed on a single surface. Thus, the processes performed during operations 210-230 must be performed at the same time (i.e., simultaneously) or one after the other (i.e., sequentially) on both sides of the substrate during each operation. Although Figures 6A-6E only show the formation of vias 303, the processes described herein can also be used to form cavities 305, or to form cavities 305 and vias 303.

[0043] Thus, after the resist layer 404 on one side of the substrate 302, such as the side including surface 608, is exposed to electromagnetic radiation for patterning, the substrate 302 may optionally be flipped over so that the resist layer 404 on the opposite surface 606 is also exposed to electromagnetic radiation for patterning, as shown in Figure 6B. Similarly, after a microblasting process is performed on surface 608 of the substrate 302, the substrate 302 may optionally be flipped over so that microblasting can be performed on the opposite surface 606, as shown in Figure 6C. The substrate 302 is then subjected to a second damage removal and cleaning process and a resist stripping process, as shown in Figures 6D-6E. By utilizing two resist layers 404 on opposite major surfaces 606, 608 of the substrate 302 and performing a microblasting process on both surfaces 606 and 608, potential tapering of features formed in the substrate 302 by the microblasting process can be reduced or eliminated, and the efficiency of the process used to structure the substrate 302 can be increased.

[0044] 7A-7D show schematic cross-sectional views of substrate 302 during another alternative sequence for operations 220 and 230 to form a desired pattern on substrate 302 by direct laser ablation. As shown in FIG. 7A, substrate 302, such as a solar substrate or even a semiconductor wafer, is placed on a stand 706 of a laser ablation system (not shown). Stand 706 may be any suitable rigid flat or textured (e.g., structured) surface to provide mechanical support to substrate 302 during laser ablation. In some embodiments, stand 706 includes an electrostatic chuck for electrostatically chucking substrate 302 to stand 706. In some embodiments, stand 706 includes a vacuum chuck for vacuum chucking substrate 302 to stand 706. After substrate 302 is placed on stand 706, a desired pattern is formed on substrate 302 by laser ablation as shown in FIG. 7B.

[0045] The laser ablation system may include any type of laser source 307 suitable for patterning the substrate 302. In some examples, the laser source 307 is an infrared (IR) laser. In some examples, the laser source 307 is a picosecond UV laser. In other examples, the laser source 307 is a femtosecond UV laser. In yet other examples, the laser source 307 is a femtosecond green laser. The laser source 307 generates a continuous or pulsed laser beam 310 for patterning the substrate 302. For example, the laser source 307 may generate a pulsed laser beam 310 having a frequency between 5 kHz and 500 kHz, such as between 10 kHz and about 200 kHz. In one example, the laser source 307 is configured to provide a pulsed laser beam with an output power between about 10 Watts and about 100 Watts with a wavelength between about 200 nm and about 1200 nm and a pulse duration between about 10 ns and about 5000 ns. Laser source 307 is configured to form any desired patterns and features in substrate 302 , including cavities 305 and vias 303 .

[0046] Similar to microblasting, the process of direct laser patterning of substrate 302 can introduce unwanted mechanical defects, including chipping and cracking, into the surface of substrate 302. Therefore, after forming the desired features in substrate 302 by direct laser patterning, substrate 302 is subjected to a second damage removal and cleaning process substantially similar to the embodiment described above. Figures 7C-7D show structured substrate 302 before and after performing the second damage removal and cleaning process, which results in a smoothed substrate 302 having cavity 305 and four vias 303 formed in substrate 302.

[0047] 2 and 3D, after removing mechanical defects in the substrate 302 in operation 230, in certain embodiments, the substrate 302 may be subjected to an oxidation process in operation 240 to grow or deposit an insulating oxide film (i.e., layer) 314 on desired surfaces of the substrate 302. For example, the oxide film 314 may be formed on all surfaces of the substrate 302 in a manner that surrounds the substrate 302. The insulating oxide film 314 acts as a passivating layer on the substrate 302 and provides an outer protective barrier that resists corrosion and other forms of damage. In certain embodiments, the oxidation process is a thermal oxidation process. The thermal oxidation process is performed at a temperature between about 800° C. and about 1200° C., such as between about 850° C. and about 1150° C. For example, the thermal oxidation process is performed at a temperature between about 900° C. and about 1100° C., such as between about 950° C. and about 1050° C. In certain embodiments, the thermal oxidation process is a wet oxidation process utilizing water vapor as an oxidizing agent. In certain embodiments, the thermal oxidation process is a dry process utilizing molecular oxygen as an oxidizing agent. It is contemplated that in operation 240, the substrate 302 may be subjected to any suitable oxidation process to form an oxide film 314 on the substrate 302. The oxide film 314 generally has a thickness between about 100 nm and about 3 μm, such as between about 200 nm and about 2.5 μm. For example, the oxide film 314 has a thickness between about 300 nm and about 2 μm, such as about 1.5 μm.

[0048] In certain embodiments, in operation 240, the substrate 302 is subjected to a metallization process to form a metal clad layer 316 on one or more surfaces of the substrate 302. In certain embodiments, the metal clad layer 316 is formed on substantially all of the outer surfaces of the substrate 302 in such a manner that the metal clad layer 114 substantially surrounds the substrate 302. The metal clad layer 316 acts as a reference layer (e.g., a ground layer or a voltage supply layer), the metal clad layer 316 is disposed on the substrate 302 to protect subsequently formed interconnects from electromagnetic interference, and further to shield electrical signals from the semiconductor material (Si) used to form the substrate 302. In certain embodiments, the metal clad layer 316 comprises a conductive metal layer comprising nickel, aluminum, gold, cobalt, silver, palladium, tin, or the like. In certain embodiments, the metal clad layer 316 comprises a metal layer comprising an alloy or pure metal comprising nickel, aluminum, gold, cobalt, silver, palladium, tin, or the like. Metal cladding layer 316 typically has a thickness between about 50 nm and about 10 μm, such as between about 100 nm and about 5 μm.

[0049] In certain examples, at least a portion of the metal cladding layer 316 comprises a deposited nickel (Ni) layer formed on the surface of the substrate 302 (e.g., an n-Si substrate or a p-Si substrate) by direct displacement plating or displacement plating. For example, the substrate 302 is exposed to a nickel displacement plating bath having a composition including 0.5M NiSO4 and NH4OH at a temperature between about 60°C and about 95°C and a pH of about 11 for about 2 minutes to about 4 minutes. Exposure of the silicon substrate 302 to an aqueous electrolyte loaded with nickel ions without a reducing agent causes a localized oxidation / reduction reaction at the surface of the substrate 302, thus plating metallic nickel on the surface of the substrate 302. Thus, nickel displacement plating allows for selective formation of a thin and pure nickel layer on the silicon material of the substrate 400 utilizing a stable solution. Moreover, the process is self-limiting, and thus the reaction stops once the entire surface of the substrate 302 is plated (e.g., when no silicon remains on which nickel can form). In certain embodiments, the nickel metal clad layer 316 may be utilized as a seed layer for plating additional metal layers, such as nickel or copper by electroless and / or electrolytic plating processes. In a further embodiment, to promote adhesion of the nickel metal clad layer 316 to the substrate 302, the substrate 302 is exposed to an SC-1 pre-clean solution and an HF oxide etch solution prior to the nickel displacement plating bath.

[0050] In a subsequent packaging operation, the metal clad layer 316 may be bonded to one or more connection points, e.g., interconnects, formed in the resulting semiconductor device package to connect the metal clad layer 316 to a common ground. For example, interconnects may be formed on one or both sides of the resulting semiconductor device package to connect the metal clad layer 316 to ground. Alternatively, the metal clad layer 316 may be connected to a reference voltage, such as a power supply voltage.

[0051] FIG. 8 illustrates a schematic top view of an exemplary structured substrate 302, according to one embodiment. Substrate 302 may be structured as described above with reference to FIGS. 2, 3A-3D, 4A-4F, 5A-5F, 6A-6E, and 7A-7D during operations 210-240. Substrate 302 is shown as having two quadrilateral cavities 305, each of which is surrounded by a number of vias 303. In certain embodiments, each cavity 305 is surrounded by two rows 801, 802 of vias 303 disposed along each side 306a-d of quadrilateral cavity 305. Although ten vias 303 are shown in each row 801, 802, it is contemplated that any desired number of vias 303 may be formed in a row. Additionally, any desired number and arrangement of cavities 305 and vias 303 may be formed in the substrate 302 during operation 220. For example, the substrate 302 may have more than two or fewer than two cavities 305 formed in the substrate 302. In another example, the substrate 302 may have more than two or fewer than two rows of vias 303 formed along each side 306a-d of the cavity 305. In another example, the substrate 302 may have two or more rows of vias 303, where the vias 303 in each row are staggered and not aligned with the vias 303 in the other rows.

[0052] In certain embodiments, the cavities 305 and vias 303 have a depth equal to the thickness of the substrate 302, thus forming holes on both surfaces of the substrate 302 (e.g., holes penetrating the thickness of the substrate 302). For example, the cavities 305 and vias 303 formed in the substrate 302 may have a depth between about 50 μm and about 1 mm, such as between about 100 μm and about 200 μm, such as between about 110 μm and about 190 μm, depending on the thickness of the substrate 302. In other embodiments, the cavities 305 and / or vias 303 may have a depth equal to or less than the thickness of the substrate 302, thus forming holes on only one surface (e.g., one side) of the substrate 302.

[0053] In certain embodiments, each cavity 305 has a lateral dimension ranging between about 3 mm and about 50 mm, such as between about 8 mm and about 12 mm, such as between about 9 mm and about 11 mm, depending on the size of one or more semiconductor dies 1026 (shown in FIG. 10B) to be embedded in the cavity 305 during package fabrication (described in more detail below). A semiconductor die typically includes a plurality of integrated electronic circuits formed on and / or within a substrate material, such as a strip of semiconductor material. In certain embodiments, the cavity 305 is sized to have a lateral dimension substantially similar to the lateral dimension of the die 1026 to be embedded in the cavity 305. For example, each cavity 305 is formed to have a lateral dimension that is less than about 150 μm, such as less than about 120 μm, such as less than 100 μm, larger than the lateral dimension of the die 1026. A smaller difference in size between the cavity 305 and the die 1026 to be filled into the cavity 305 reduces the amount of fill material subsequently used.

[0054] In certain embodiments, each via 303 has a diameter ranging between about 50 μm and about 200 μm, such as between about 60 μm and 130 μm, such as between about 80 μm and 110 μm. The minimum pitch 807 between the center of a via 303 in row 801 and the center of an adjacent via 303 in row 802 is between about 70 μm and about 200 μm, such as between about 85 μm and about 160 μm, such as between about 100 μm and 140 μm. Although the embodiment is described with reference to FIG. 8, the substrate structuring process described above with respect to operations 210-240 and FIGS. 2, 3A-3B, 4A-4C, 5A-5C, 6A-6C, and 7A-7B may be utilized to form patterned features in substrate 302 having desired depths, lateral dimensions, and morphologies.

[0055] After structuring the substrate 302, one or more packages are formed around the substrate 302 by utilizing the substrate 302 as a core frame. Figures 9 and 11 respectively show flow diagrams of representative methods 900 and 1100 for manufacturing an intermediate embedded die assembly 1002 around the substrate 302 prior to final package formation. Figures 10A-10M show schematic cross-sectional views of the substrate 302 at different stages of the method 900 shown in Figure 9, and Figures 12A-12H show schematic cross-sectional views of the substrate 302 at different stages of the method 1100 shown in Figure 11. For clarity, Figures 9 and 10A-10M will be discussed together herein, and Figures 11 and 12A-12H will be discussed together herein.

[0056] Generally, the method 900 begins with operation 902 and FIG. 10A, in which a first side 1075 of the substrate 302 having desired features formed thereon (e.g., surface 606, which may have an oxide layer or a metal clad layer formed thereon) is placed on a first insulating film 1016a. In certain embodiments, the first insulating film 1016a includes one or more layers formed of a polymer-based dielectric material. For example, the first insulating film 1016a includes one or more layers formed of a flowable build-up material. In the embodiment shown in FIG. 10A, the first insulating film 1016a includes a flowable layer 1018a. The flowable layer 1018a may be formed of a ceramic-filled epoxy resin, such as an epoxy resin filled with silica (SiO2) particles (e.g., including SiO2 particles). Other examples of ceramic fillers or particles that may be utilized to form the flowable layer 1018a and other layers of the insulating film 1016a include aluminum nitride (AlN), aluminum oxide (Al2O3), silicon carbide (SiC), silicon nitride (Si3N4), Sr2Ce2Ti5O 16 , Zirconium silicate (ZrSiO4), Wollastonite (CaSiO3), Beryllium oxide (BeO), Cerium dioxide (CeO2), Boron nitride (BN), Calcium copper titanium oxide (CaCu3Ti4O12 ), magnesium oxide (MgO), titanium dioxide (TiO2), zinc oxide (ZnO), and the like. In some examples, the ceramic filler utilized to form the flowable layer 1018a has particles having a particle size ranging from about 40 nm to about 1.5 μm, such as between about 80 nm to about 1 μm. For example, the ceramic filler utilized to form the flowable layer 1018a has particles having a particle size ranging from about 200 nm to about 800 nm, such as between about 300 nm to about 600 nm. In some embodiments, the ceramic filler utilized to form the flowable layer 1018a includes particles having a particle size less than about 25% of the width or diameter of a desired feature (e.g., a via, a cavity, or a through assembly via), such as a particle size less than about 15% of the width or diameter of the desired feature.

[0057] The flowable layer 1018a typically has a thickness of less than about 60 μm, such as between about 5 μm and about 50 μm. For example, the flowable layer 1018a has a thickness of between about 10 μm and about 25 μm. In certain embodiments, the insulating film 1016a further comprises one or more support layers. For example, the insulating film 1016a comprises a polyethylene terephthalate (PET) or similar lightweight plastic support layer 1022a. However, any suitable combination of layers and insulating materials is contemplated for the insulating film 1016a. In some embodiments, the insulating film 1016a as a whole has a thickness of less than about 120 μm, such as less than about 90 μm.

[0058] Additionally, for mechanical support during subsequent processing operations, the substrate 302, with its first side 1075 bonded to the insulating film 1016a, specifically the flowable layer 1018a of the insulating film 1016a, may optionally be placed on a carrier 1024. The carrier is made of any suitable mechanically and thermally stable material. For example, the carrier 1024 is made of polytetrafluoroethylene (PTFE). In another example, the carrier 1024 is made of PET.

[0059] In operation 904, one or more semiconductor dies 1026 are placed in the cavity 305 formed in the substrate 302, as shown in FIG. 10B (a single semiconductor die 1026 is shown in FIG. 10B). The die 1026 is placed in the cavity 305, for example using a vacuum gripper, and positioned on the surface of the insulating film 1016a exposed through the cavity 305. To secure the die 1026 in place, in certain embodiments, the die 1026 is placed on an adhesive layer (not shown) disposed on or formed on the insulating film 1016a. In certain embodiments, the substrate 302 and / or the insulating film 1016a are heated during placement of the semiconductor die 1026 to provide additional adhesion between the semiconductor die 1026 and the insulating film 1016a, thus reducing movement of the semiconductor die 1026 during placement of the semiconductor die 1026. For example, in certain embodiments, the carrier 1024 may be heated during placement of the semiconductor die 1026.

[0060] In certain embodiments, the die 1026 comprises an active multi-purpose die having one or more integrated circuits formed thereon. For example, in such embodiments, the die 1026 may include one or more signal contacts 1030 for interconnects carrying signals formed on the front side 1028a of the die 1026. In further embodiments, the die 1026 may further include a backside power delivery network including power contacts 1031 formed on the backside 1028b of the die 1026. Such a die may be referred to as a "double-sided" die. An exemplary double-sided die is shown in FIG. 10M and will be described later. However, in still other embodiments, the die 1026 may include passive die or passive components such as capacitors, resistors, inductors, RF components, and the like.

[0061] After the die 1026 is placed in the cavity 305, a first protective film 1060 is placed on the second side 1077 (e.g., surface 608) of the substrate 302 in operation 906 and FIG. 10C. The protective film 1060 is bonded to the second side 1077 of the substrate 302 opposite the first insulating film 1016a in such a manner that the protective film 1060 contacts and covers the active surface 1028 of the die 1026 disposed in the cavity 305. In certain embodiments, the protective film 1060 is formed of a material similar to that of the support layer 1022a. For example, the protective film 1060 is formed of PET, such as biaxial PET. However, the protective film 1060 may be formed of any suitable protective material. In some embodiments, the protective film 1060 has a thickness between about 50 μm and about 150 μm.

[0062] Next, the substrate 302, with a first side 1075 attached to the insulating film 1016a and a second side 1077 attached to the protective film 1060, and further having a die 1026 disposed therein, is subjected to a lamination process in operation 908. During this lamination process, the substrate 302 is exposed to high temperatures, thereby softening the flowable layer 1018a of the insulating film 1016a and causing the flowable layer 1018a to flow into open voids or volumes between the insulating film 1016a and the protective film 1060, such as the gaps 1051 between the inner walls of the vias 303 and the cavity 305 and the die 1026. Thus, the semiconductor die 1026 is at least partially embedded in the material of the insulating film 1016a and the substrate 302, as shown in FIG.

[0063] In certain embodiments, the lamination process is a vacuum lamination process that may be performed in an autoclave or other suitable device. In certain embodiments, the lamination process is performed by using a hot press process. In certain embodiments, the lamination process is performed at a temperature between about 80° C. and about 140° C. for about 5 seconds to about 1.5 minutes, such as about 30 seconds to about 1 minute. In some embodiments, the lamination process includes applying a pressure between about 1 psig and about 50 psig while subjecting the substrate 302 and the insulating film 1016a to a temperature between about 80° C. and about 140° C. for about 5 seconds to about 1.5 minutes. For example, the lamination process is performed at a pressure between about 5 psig and about 40 psig, a temperature between about 100° C. and about 120° C., and a time between about 10 seconds to about 1 minute. For example, the lamination process is performed at a temperature of about 110° C. for about 20 seconds.

[0064] In operation 910, the protective film 1060 is removed, and then the substrate 302 with the laminated insulating material of the flowable layer 1018a at least partially surrounding the substrate 302 and one or more dies 1026 is placed on a second protective film 1062. As shown in FIG. 10E, the second protective film 1062 is bonded to the first side 1075 of the substrate 302 in such a manner that the second protective film 1062 is disposed against (e.g., adjacent to) the support layer 1022a of the insulating film 1016a. In some embodiments, the substrate 302 bonded to the protective film 1062 may then be placed on a carrier 1024, optionally for additional mechanical support of the first side 1075. In some embodiments, the protective film 1062 is then placed on the carrier 1024 before bonding the protective film 1062 to the substrate 302 with the laminated insulating film 1016a. Generally, the composition of protective film 1062 is substantially similar to the composition of protective film 1060. For example, protective film 1062 may be formed of PET, such as biaxial PET. However, protective film 1062 may be formed of any suitable protective material. In some embodiments, protective film 1062 has a thickness between about 50 μm and about 150 μm.

[0065] After bonding the substrate 302 to the second protective film 1062, in operation 912 and FIG. 10F, a second insulating film 1016b substantially similar to the first insulating film 1016a is placed on the second side 1077 of the substrate 302. Thus, the second insulating film 1016b replaces the protective film 1060. In certain embodiments, the second insulating film 1016b is disposed on the second side 1077 of the substrate 302 in such a manner that the flowable layer 1018b of the second insulating film 1016b contacts and covers the active surface 1028 of the die 1026 in the cavity 305. In certain embodiments, by placing the second insulating film 1016b on the substrate 302, one or more voids may be formed between the insulating film 1016b and the already deposited insulating material of the flowable layer 1018a partially surrounding one or more dies 1026. The second insulating film 1016b may include one or more layers formed of a flowable polymer-based dielectric material. As shown in FIG. 10F, the second insulating film 1016b includes a flowable layer 1018b similar to the flowable layer 1018a described above. The second insulating film 1016b may further include a support layer 1022b formed of a material similar to the support layer 1022a, such as PET or other lightweight plastic material.

[0066] In operation 914, a third protective film 1064 is placed over the second insulating film 1016b, as shown in FIG. 10G. Generally, the composition of the protective film 1064 is substantially similar to the composition of the protective films 1060, 1062. For example, the protective film 1064 is formed of PET, such as biaxial PET. However, the protective film 1064 may be formed of any suitable protective material. In some embodiments, the protective film 1064 has a thickness between about 50 μm and about 150 μm.

[0067] The substrate 302, with its second side 1077 attached to the insulating film 1016b and support layer 1064, and its first side 1075 attached to the protective film 1062 and optional carrier 1024, is then subjected to a second lamination process in operation 916 and Figure 10H. Similar to the lamination process in operation 908, the substrate 302 is exposed to an elevated temperature, thereby softening the flowable layer 1018b of the insulating film 1016b and causing the flowable layer 1018b to flow into any open voids or volumes between the insulating film 1016b and the already deposited insulating material of the flowable layer 1018a, thus causing the flowable layer 1018b to integrate itself with the insulating material of the flowable layer 1018a. Thus, the cavity 305 and vias 303 are filled (eg, filled and sealed) with the insulating material, and the semiconductor die 1026 previously placed within the cavity 305 is completely embedded within the insulating material of the flowable layers 1018a, 1018b.

[0068] In certain embodiments, the lamination process is a vacuum lamination process that may be performed in an autoclave or other suitable device. In certain embodiments, the lamination process is performed by using a hot press process. In certain embodiments, the lamination process is performed at a temperature between about 80° C. and about 140° C. for about 1 minute to about 30 minutes. In some embodiments, the lamination process includes applying a pressure between about 10 psig and about 150 psig while subjecting the substrate 302 and the insulating film 1016b to a temperature between about 80° C. and about 140° C. for about 1 minute to about 30 minutes. For example, the lamination process is performed at a pressure between about 20 psig and about 100 psig, a temperature between about 100° C. and about 120° C., and a time between about 2 minutes to about 10 minutes. For example, the lamination process is performed at a temperature of about 110° C. for about 5 minutes.

[0069] After lamination, in operation 918, the substrate 302 is separated from the carrier 1024 and the protective films 1062, 1064 are removed, resulting in a laminated embedded die assembly 1002. As shown in FIG. 10I, the embedded die assembly 1002 includes a substrate 302 having one or more cavities 305 and / or vias 303 formed in the substrate 302 and filled with an insulating dielectric material of the flowable layers 1018a, 1018b, and an embedded die 1026 in the cavity 305. The insulating dielectric material of the flowable layers 1018a, 1018b encapsulates the substrate 302 in such a manner that the insulating material covers at least two surfaces or sides of the substrate 302, such as the two major surfaces 606, 608 and all sides of the embedded semiconductor die 1026. In some examples, in operation 918, the support layers 1022a, 1022b are also removed from the embedded die assembly 1002. Generally, the support layers 1022a and 1022b, the carrier 1024, and the protective films 1062 and 1064 are removed from the embedded die assembly 1002 by any suitable mechanical process, such as a peeling process.

[0070] After removing the support layers 1022a, 1022b and the protective films 1062, 1064, the embedded die assembly 1002 is subjected to a curing process to sufficiently cure (i.e., harden by chemical reaction and cross-linking) the insulating dielectric material of the flowable layers 1018a, 1018b, thus forming a cured insulating layer 1018. The insulating layer 1018 substantially surrounds the substrate 302 and the semiconductor die 1026 embedded in the substrate 302. For example, the insulating layer 1018 contacts or encapsulates at least the sides 1075, 1077 of the substrate 302 (including the surfaces 606, 608) and at least six sides or surfaces of each semiconductor die 1026. Each semiconductor die 1026 has the shape of a rectangular prism as shown in FIG. 10I (i.e., in the 2D view, only four surfaces 1028a, 10298b and 1029a, 1029b are shown).

[0071] In certain embodiments, the curing process is carried out at an elevated temperature to sufficiently cure the embedded die assembly 1002. For example, the curing process is carried out at a temperature between about 140° C. and about 220° C. for a period between about 15 minutes and about 45 minutes, such as between about 160° C. and about 200° C. for a period between about 25 minutes and about 35 minutes. For example, the curing process is carried out at a temperature of about 180° C. for about 30 minutes. In further embodiments, the curing process in operation 918 is carried out at or near ambient (e.g., atmospheric) pressure conditions.

[0072] After curing, in operation 920, one or more through-assembly vias 1003 are drilled through the embedded die assembly 1002 to form channels through the entire thickness of the embedded die assembly 1002 for subsequent interconnect formation. In some embodiments, the embedded die assembly 1002 may be placed on a carrier, such as carrier 1024, for mechanical support during the formation of the through-assembly vias 1003 and subsequent contact holes 1032. The through-assembly vias 1003 are drilled through vias 303 formed in the substrate 302 and subsequently filled with an insulating layer 1018. Thus, the periphery of the through-assembly vias 1003 may be surrounded by the insulating layer 1018 that fills the vias 303. By lining the walls of the vias 303 with the ceramic filler-containing epoxy resin material of the insulating layer 1018, capacitive coupling between the conductive silicon-based substrate 302 and the interconnects 1444 (described with reference to FIG. 13 and FIG. 14E-14H), and therefore between adjacently located vias 303 and / or redistribution connections 1644 (described with reference to FIG. 15 and FIG. 16K-16L), of the completed package 1602, is significantly reduced compared to other conventional interconnect structures utilizing conventional via insulating liners or via dielectric films. Additionally, the flowability of the epoxy resin material allows for more consistent and reliable encapsulation and insulation, thus enhancing electrical performance by minimizing leakage current of the completed package 1602.

[0073] In certain embodiments, the through assembly via 1003 has a diameter of less than about 100 μm, such as less than about 75 μm. For example, the through assembly via 1003 has a diameter of less than about 60 μm, such as less than about 50 μm. In certain embodiments, the through assembly via 1003 has a diameter of between about 25 μm and about 50 μm, such as between about 35 μm and about 40 μm. In certain embodiments, the through assembly via 1003 is formed using any suitable mechanical process. For example, the through assembly via 1003 is formed using a mechanical drilling process. In certain embodiments, the through assembly via 1003 is formed through the embedded die assembly 1002 by laser ablation. For example, the through assembly via 1003 is formed using an ultraviolet laser. In certain embodiments, the laser source utilized for laser ablation has a frequency of between about 5 kHz and about 500 kHz. In certain embodiments, the laser source is configured to provide a pulsed laser beam with a pulse duration between about 10 ns and about 100 ns and a pulse energy between about 50 microjoules (μJ) and about 500 μJ. Utilizing an epoxy resin material with small ceramic filler particles further facilitates more precise and accurate laser patterning of small diameter vias, such as via 1003, because the small ceramic filler particles in the epoxy resin material exhibit reduced laser light reflection, scattering, diffraction, and transmission away from the area where the via is to be formed during the laser ablation process.

[0074] In operation 922 and FIG. 10K, one or more contact holes 1032 are drilled through the insulating layer 1018 on the second side 1077 of the embedded die assembly to expose one or more signal contacts 1030 formed on the front side 1028a of each embedded die 1026. The contact holes 1032 are drilled through the insulating layer 1018 by laser ablation to leave all outer surfaces of the semiconductor die 1026 covered and surrounded by the insulating layer 1018 and to expose the signal contacts 1030. Thus, the signal contacts 1030 are exposed by the formation of the contact holes 1032 in operation 922. In certain embodiments, the laser source may generate a pulsed laser beam having a frequency between about 100 kHz and about 1000 kHz. In certain embodiments, the laser source is configured to provide a pulsed laser beam having a wavelength between about 100 nm and about 2000 nm, a pulse duration between about 10E-4 ns and about 10E-2 ns, and a pulse energy between about 10 μJ and about 300 μJ. In certain embodiments, the contact holes 1032 are drilled using a CO2, green, or UV laser. In certain embodiments, the contact holes 1032 have a diameter between about 5 μm and about 60 μm, such as a diameter between about 20 μm and about 50 μm.

[0075] In embodiments in which the die 1026 is a double-sided die, in operation 924 and FIG. 10L, the embedded die assembly 1002 is flipped over and one or more contact holes 1032 are drilled through the insulating layer 1018 on the first side 1075 of the embedded die assembly to expose one or more power contacts 1031 formed on the backside 1028b of each embedded die 1026. The contact holes 1032 may be formed in a manner substantially similar to that described with respect to operation 922, such as by laser ablation, and may have substantially similar dimensions.

[0076] After all desired contact holes 1032 are formed, the embedded die assembly 1002 is subjected to a de-smear process to remove any unwanted residue and / or debris caused by laser ablation during the formation of the through-assembly vias 1003 and contact holes 1032. This de-smear process thus cleans the through-assembly vias 1003 and contact holes 1032 and fully exposes the contacts 1030 on the active surface 1028 of the embedded die 1026 in preparation for subsequent metallization. In certain embodiments, this de-smear process is a wet de-smear process. Any suitable aqueous etchant, solvent and / or combination thereof may be utilized for this wet de-smear process. In one example, a potassium permanganate (KMnO4) solution may be utilized as the etchant. Depending on the thickness of the residue, the embedded die assembly 1002 may be subjected to a wet de-smear process in operation 922 at varying amounts. In another embodiment, this de-smear process is a dry de-smear process. For example, the desmear process may be a plasma desmear process using a O2:CF4 gas mixture. The plasma desmear process may include generating a plasma by applying a power of about 700 W for about 60 seconds to about 120 seconds and flowing O2:CF4 at a ratio of about 10:1 (e.g., 100:10 sccm). In a further embodiment, the desmear process is a combination of a wet process and a dry process.

[0077] After this desmear process, the embedded die assembly 1002 is ready for forming interconnect paths within the embedded die assembly 1002, as described below with reference to Figures 13 and 14A-14H.

[0078] FIG. 10M illustrates in schematic form an exemplary double-sided die 1026 that may be utilized with the semiconductor device packaging structures and methods described herein. More conventional semiconductor chips typically have all of the interconnects (power and signal) along with the transistors on a single side of the silicon substrate or core. Thus, as transistors continue to get smaller, the interconnects connecting the transistors to other devices or device elements must be packed closer together and made finer and finer, especially since they share space with the power interconnects. This can lead to increased resistance, RC-related limitations, and power losses, which can create chip design and device packaging challenges. By utilizing a double-sided chip such as the example of FIG. 10M, the power distribution interconnects and the signal routing interconnects can be separated onto different sides of the chip, thus allowing more lateral space for larger power connections to facilitate providing more power to the transistors, while at the same time allowing more space for signal interconnects.

[0079] As shown in FIG. 10M, the double-sided die 1026 includes a core 1080 having a signal portion 1094 formed on a first side of the core 1080 and a power delivery portion 1096 formed on an opposing second side of the core 1080. The core 1080 is generally made of silicon, crystalline silicon (e.g., Si <100> Or Si <111> Core 1080 may be formed of any suitable silicon-containing material, including those materials described with respect to 302, such as silicon oxide, silicon germanium, doped or undoped silicon, doped or undoped polycrystalline silicon, silicon nitride, single crystal p-type or n-type silicon, polycrystalline p-type or n-type silicon, etc. Core 1080 may alternatively be formed of any suitable silicon-containing glass material.

[0080] The signal portion 1096 includes one or more integrated circuits having transistors (represented by fins 1082) and signal interconnects 1084 that are conductively coupled to signal contacts 1030 on a first surface 1028a of the die 1026. In certain embodiments, the transistors 1082 and signal interconnects 1084 are disposed within a dielectric insulating layer 1092, such as silicon dioxide or other oxide insulator, formed over the core 1080. The signal interconnects 1084 may be formed of any suitable conductive material, including copper, cobalt, ruthenium, nickel, aluminum, gold, silver, palladium, tin, molybdenum, and the like.

[0081] The power delivery portion 1096 includes a network of one or more power interconnects 1090 (e.g., a power delivery network or "PDN") that extend from the second side of the core 1080 to power contacts 1031 on the second surface 1028b of the die 1026. Like the signal interconnects, the power interconnects 1090 may be formed of any suitable conductive material, including copper, cobalt, ruthenium, nickel, aluminum, gold, silver, palladium, tin, molybdenum, etc., and may be disposed within a dielectric insulating layer 1092 formed of an oxide insulator.

[0082] One or more buried power rails 1086 may be formed through at least a portion of the core 1080 and connected to the transistors 1082 and / or signal interconnects 1084 to electrically couple the transistors 1082 and / or signal interconnects 1084 to a power supply portion 1096 (e.g., power interconnects 1090). The buried power rails 1086 provide power connections that pass under the transistors, through the core 1080, and extend toward the power supply portion 1096, thus allowing more space on the first side of the core 1080 for integrating circuitry. In particular, the buried power rails 1086 facilitate more space for interconnects carrying signals above the transistors, thus allowing increased circuit density and improved performance of the die 1027.

[0083] In certain embodiments, a buried power rail 1086 extends from the signal portion 1096 across the entire thickness of the core 1080 and couples to the power interconnect 1090. In certain other embodiments, the buried power rail 1086 extends across a portion of the thickness of the core 1080, as shown in FIG. 10M. In such embodiments, the buried power rail may be electrically coupled to a through silicon interconnect 1088, which may in turn be coupled to the power interconnect 1090, which may extend from the power supply portion 1096 into the core 1088.

[0084] As discussed above, Figures 9 and 10A-10M illustrate an exemplary method 900 for forming an intermediate embedded die assembly 1002. Figures 11 and 12A-12H illustrate an alternative method 1100 that is substantially similar to method 900 but includes fewer operations than method 900. Method 1100 generally includes seven operations 1110-1180. However, operations 1110, 1120, 1160, 1170, and 1180 of method 1100 are substantially similar to operations 902, 904, 920, 922, and 924, respectively, of method 900. Thus, for clarity, only operations 1130, 1140, and 1150, shown in Figures 12C, 12D, and 12E, respectively, are described herein.

[0085] After placing one or more semiconductor dies 1026 on the surface of the insulating film 1016a exposed through the cavity 305, and prior to lamination, a second insulating film 1016b is disposed on the second side 1077 (e.g., surface 608) of the substrate 302 in operation 1130 and FIG. 12C. In some embodiments, the second insulating film 1016b is disposed on the second side 1077 of the substrate 302 in such a manner that the flowable layer 1018b of the second insulating film 1016b contacts and covers the active surface 1028 of the die 1026 in the cavity 305. In some embodiments, a second carrier 1025 is attached to the support layer 1022b of the second insulating film 1016b for additional mechanical support during subsequent processing operations. As shown in FIG. 12C, one or more voids 1050 are formed between the insulating films 1016a and 1016b, penetrating the via 303, forming a gap 1051 between the semiconductor die 1026 and the inner wall of the cavity 305.

[0086] Next, in operation 1140 and FIG. 12D, the substrate 302 having the die 1026 attached to the insulating films 1016a and 1016b and disposed therein is subjected to a single lamination process. During this single lamination process, the substrate 302 is exposed to high temperatures, thereby softening the flowable layers 1018a and 1018b of both insulating films 1016a, 1016b and causing the flowable layers 1018a and 1018b to flow into open voids or volumes between the insulating films 1016a, 1016b, such as the via 303 and the gap 1051 between the inner wall of the cavity 305 and the die 1026. Thus, the semiconductor die 1026 is embedded in the material of the insulating films 1016a, 1016b and the via 303 is filled with the material of the insulating films 1016a, 1016b.

[0087] Similar to the lamination process described with reference to Figures 9 and 10A-10K, the lamination process in operation 1140 may be a vacuum lamination process that may be performed in an autoclave or other suitable device. In another embodiment, the lamination process is performed by using a hot press process. In certain embodiments, the lamination process is performed at a temperature between about 80°C and about 140°C for about 1 minute to about 30 minutes. In some embodiments, the lamination process includes applying a pressure between about 1 psig and about 150 psig while subjecting the substrate 302 and the insulating film 1016a, 1016b layers to a temperature between about 80°C and about 140°C for about 1 minute to about 30 minutes. For example, the lamination process is performed at a pressure between about 10 psig and about 100 psig and a temperature between about 100°C and about 120°C for about 2 minutes to about 10 minutes. For example, the lamination process is performed at a temperature of about 110°C for about 5 minutes.

[0088] In operation 1150, one or more supporting layers of insulating films 1016a and 1016b are removed from the substrate 302, resulting in a stacked embedded die assembly 1002. As shown in FIG. 12E, the embedded die assembly 1002 includes a substrate 302 having one or more cavities 305 and / or vias 303 formed in the substrate 302 and filled with an insulating dielectric material of the flowable layers 1018a, 1018b, and an embedded die 1026 in the cavity 305. The insulating material encapsulates the substrate 302 in such a manner that the insulating material covers at least two surfaces or sides of the substrate 302, e.g., surfaces 606, 608. In one example, the supporting layers 1022a, 1022b are removed from the embedded die assembly 1002, thus separating the embedded die assembly 1002 from the carriers 1024, 1025. Generally, the support layers 1022a, 1022b and carriers 1024, 1025 are removed from the embedded die assembly 1002 by any suitable mechanical process, such as a peeling process.

[0089] After removing the support layers 1022a, 1022b, the embedded die assembly 1002 is subjected to a curing process to fully harden the insulating dielectric material of the flowable layers 1018a, 1018b. The hardening of the insulating material results in the formation of a hardened insulating layer 1018. As shown in Figure 12E, the insulating layer 1018 substantially surrounds the substrate 302 and the semiconductor die 1026 embedded in the substrate 302, similar to operation 918 corresponding to Figure 10I.

[0090] In certain embodiments, the curing process is carried out at an elevated temperature to sufficiently cure the embedded die assembly 1002. For example, the curing process is carried out at a temperature between about 140° C. and about 220° C. for a period between about 15 minutes and about 45 minutes, such as between about 160° C. and about 200° C. for a period between about 25 minutes and about 35 minutes, etc. For example, the curing process is carried out at a temperature of about 180° C. for about 30 minutes. In further embodiments, the curing process in operation 1150 is carried out at or near ambient (e.g., atmospheric) pressure conditions.

[0091] After curing at operation 1150, method 1100 is substantially similar to operations 920-924 of method 900. For example, embedded die assembly 1002 has one or more through-assembly vias 1003 and one or more contact holes 1032 drilled through insulating layer 1018. Subsequently, embedded die assembly 1002 is subjected to a desmear process after which embedded die assembly 1002 is ready for forming interconnect paths therein, as described below.

[0092] Figure 13 illustrates a flow diagram of an exemplary method 1300 of forming electrical interconnects through an embedded die assembly 1002. Figures 14A-14H illustrate schematic cross-sectional views of the embedded die assembly 1002 at different stages of the process of the method 1300 illustrated in Figure 13. Thus, for clarity, Figure 13 and Figures 14A-14H will be described together herein.

[0093] In certain embodiments, the electrical interconnects formed through the embedded die assembly 1002 are formed of copper. Thus, the method 1300 may optionally begin with operation 1310 and FIG. 14A, where the embedded die assembly 1002 having the through assembly vias 1003 and contact holes 1032 formed therein has an adhesion layer 1440 and / or a seed layer 1442 formed thereon. For reference, an enlarged partial view of the adhesion layer 1440 and the seed layer 1442 formed on the embedded die assembly 1002 is shown in FIG. 14H. An adhesion layer 1440 may be formed on desired surfaces of the insulating layer 1018, such as the major surfaces 1005, 1007 of the embedded die assembly 1002, as well as the active surfaces 1028 of the contact holes 1032 on each die 1026 and the inner walls of the through-assembly vias 1003, to help promote adhesion and inhibit diffusion of the subsequently formed seed layer 1442 and copper interconnects 1444. Thus, in certain embodiments, the adhesion layer 1440 acts as an adhesion layer, and in other embodiments, the adhesion layer 1440 acts as a barrier layer. However, hereinafter, in both embodiments, the adhesion layer 1440 will be described as an "adhesion layer."

[0094] In certain embodiments, optional adhesion layer 1440 is formed of titanium, titanium nitride, tantalum, tantalum nitride, manganese, manganese oxide, molybdenum, cobalt oxide, cobalt nitride, or any other suitable material, or combinations thereof. In certain embodiments, adhesion layer 1440 has a thickness between about 10 nm and about 300 nm, such as between about 50 nm and about 150 nm. For example, adhesion layer 1440 has a thickness between about 75 nm and about 125 nm, such as about 100 nm. Adhesion layer 1440 is formed by any suitable deposition process, including, but not limited to, chemical vapor deposition (CVD), physical vapor deposition (PVD), plasma enhanced chemical vapor deposition (PECVD), atomic layer deposition (ALD), and the like.

[0095] An optional seed layer 1442 may be formed on the adhesion layer 1440 or directly on the insulating layer 1018 (e.g., without forming an adhesion layer 1440). The seed layer 1442 is formed of a conductive material, such as copper, tungsten, aluminum, silver, gold, or any other suitable material, or combinations thereof. In certain embodiments, the seed layer 1442 has a thickness between about 50 nm and about 500 nm, such as between about 100 nm and about 300 nm. For example, the seed layer 1442 has a thickness between about 150 nm and about 250 nm, such as about 200 nm. In certain embodiments, the seed layer 1442 has a thickness between about 0.1 μm and about 1.5 μm. Similar to the adhesion layer 1440, the seed layer 1442 is formed by any suitable deposition process, such as CVD, PVD, PECVD, a dry ALD process, a wet electroless plating process, or the like. In certain embodiments, a molybdenum adhesion layer 1440 is formed on the embedded die assembly in combination with a copper seed layer 1442. The combination of the Mo adhesion layer and the Cu seed layer allows for improved adhesion to the surface of the insulating layer 1018 and reduces undercutting of the conductive interconnect lines during a subsequent seed layer etching process in operation 1370.

[0096] In operations 1320 and 1330, corresponding to Figures 14B and 14C, respectively, a spin-on / spray-on or dry resist film 1450, such as photoresist, is applied to both major surfaces 1005, 1007 of the embedded die assembly 1002 and subsequently patterned. In certain embodiments, the resist film 1450 is patterned by selective exposure to UV radiation. In certain embodiments, an adhesion promoter (not shown) is applied to the embedded die assembly 1002 prior to forming the resist film 1450. The adhesion promoter improves the adhesion of the resist film 1450 to the embedded die assembly 1002 by creating an interfacial bonding layer for the resist film 1450 and by removing any moisture from the surface of the embedded die assembly 1002. In some embodiments, the adhesion promoter is formed of bis(trimethylsilyl)amine or hexamethyldisilizane (HMDS) and propylene glycol monomethyl ether acetate (PGMEA).

[0097] In operation 1340 and FIG. 14D, the embedded die assembly 1002 is subjected to a resist film developing process. As shown in FIG. 14D, the resist film 1450 is developed, thereby exposing the through assembly via 1003 and the contact hole 1032 having the adhesion layer 1440 and the seed layer 1442 formed thereon. In certain embodiments, the film developing process is a wet process, such as a wet process that includes exposing the resist to a solvent. In certain embodiments, the film developing process is an aqueous etching process that utilizes an aqueous etching process. In other embodiments, the film developing process is a wet etching process that utilizes a buffered etching process that is selective to the desired material. Any suitable wet solvent or any suitable combination of wet etchants may be used for the resist film developing process.

[0098] In operations 1350 and 1360, corresponding to Figures 14E and 14F, respectively, interconnects 1444 are formed through the exposed through-assembly vias 1003 and contact holes 1032, and thereafter the resist film 1450 is removed. The interconnects 1444 are formed by any suitable method, including electroplating and electroless deposition. In certain embodiments, the resist film 1450 is removed by a wet process. As shown in Figures 14E and 14F, the formed interconnects 1444 fill the through-assembly vias 1003 and contact holes 1032 and / or cover the inner peripheral walls of the through-assembly vias 1003 and contact holes 1032, and protrude from the surfaces 1005, 1007, and 1028 of the embedded die assembly 1002 after removal of the resist film 1450. In certain embodiments, the interconnects 1444 are formed of copper. In other embodiments, the interconnects 1444 may be formed of any suitable conductive material, including, but not limited to, aluminum, gold, nickel, silver, palladium, tin, or the like.

[0099] In operation 1370 and FIG. 14G, the embedded die assembly 1002 having the interconnects 1444 formed therein is subjected to an adhesion and / or seed layer etching process to remove the adhesion layer 1440 and the seed layer 1442. In certain embodiments, the seed layer etching is a wet etching process that includes rinsing and drying the embedded die assembly 1002. In certain embodiments, the seed layer etching process is a buffered etching process that is selective to a desired material, such as copper, tungsten, aluminum, silver, or gold. In other embodiments, the etching process is an aqueous etching process. Any suitable wet etchant or any suitable combination of wet etchants may be used for the seed layer etching process.

[0100] Following the seed layer etching process in operation 1370, one or more electrically functional packages may be singulated from the embedded die assembly 1002. Alternatively, the embedded die assembly 1002 may have one or more redistribution layers 1658 and / or 1660 (shown in FIGS. 16K-16L) formed thereon, as needed, to enable rerouting of the contacts of the interconnects 1444 to desired locations on the surface of the embedded die assembly 1002. FIG. 15 illustrates a flow diagram of an exemplary method 1500 of forming a redistribution layer 1658 on the embedded die assembly 1002. FIGS. 16A-16L illustrate schematic cross-sectional views of the embedded die assembly 1002 at different stages of the method 1500 shown in FIG. 15. Thus, for clarity, FIGS. 15 and 16A-16L will be described together herein.

[0101] Method 1500 is substantially similar to methods 900, 1100, and 1300 described above. Generally, method 1500 begins with operation 1502 and FIG. 16A, which places an insulating film 1616 on a desired side of embedded die assembly 1002 followed by lamination. Insulating film 1616 may be substantially similar to insulating film 1016 and includes one or more layers formed of a polymer-based flowable dielectric material. In certain embodiments, insulating film 1616 includes a flowable layer 1618 and one or more support layers 1622, as shown in FIG. 16A. In certain embodiments, insulating film 1616 may include a ceramic filler-containing epoxy resin flowable layer 1618 and one or more support layers 1622. In another example, insulating film 1616 may include a photodefinable polyimide flowable layer 1618 and one or more support layers 1622. The material properties of photodefinable polyimide allow for the formation of smaller (e.g., thinner) vias through interconnect layers formed from photodefinable polyimide. However, any suitable combination of layers and insulating materials is contemplated for the insulating layer 1616. For example, the insulating layer 1616 may include a flowable layer 1618 of non-photosensitive polyimide, polybenzoxazole (PBO), silicon dioxide, and / or silicon nitride. Examples of suitable materials for the support layer(s) 1622 include PET and polypropylene (PP).

[0102] In some examples, the flowable layer 1618 includes a different polymer-based flowable dielectric material than the flowable layers 1018a, 1018b described above. For example, the flowable layer 1018 may include a ceramic-filled epoxy resin, and the flowable layer 1618 may include a photodefinable polyimide. In another example, the flowable layer 1618 is formed from a different inorganic dielectric material than the flowable layers 1018a, 1018b. For example, the flowable layers 1018a, 1018b may include a ceramic-filled epoxy resin, and the flowable layer 1618 may include a silicon dioxide layer.

[0103] The insulating film 1616 has a thickness of less than about 200 μm, such as between about 10 μm and about 180 μm. For example, the insulating film 1616 including the flowable layer 1618 and the PET support layer 1622 has a total thickness of between about 50 μm and about 100 μm. In certain embodiments, the flowable layer 1618 has a thickness of less than about 60 μm, such as between about 5 μm and about 50 μm, such as about 20 μm. The insulating film 1616 is disposed on a surface, such as the major surface 1005, of the embedded die assembly 1002 having exposed interconnects 1444 coupled to contacts 1030 of the active surface 1028 of the die 1026 and / or exposed interconnects 1444 coupled to metallized through-assembly vias 1003.

[0104] After depositing the insulating film 1616, the embedded die assembly 1002 is subjected to a lamination process substantially similar to that described with reference to operations 908, 916, and 1140. The embedded die assembly 1002 is exposed to an elevated temperature to soften the flowable layer 1618. The flowable layer 1618 is then bonded to the insulating layer 1018 already formed on the embedded die assembly 1002. Thus, in certain embodiments, the flowable layer 1618 merges with the insulating layer 1018 to form an extension of the insulating layer 1018. The merger of the flowable layer 1618 and the insulating layer 1018 results in an extended and merged insulating layer 1018 covering the previously exposed interconnects 1444. Thus, the combined flowable layer 1618 and insulating layer 1018 are collectively referred to herein as the insulating layer 1018. However, in other embodiments, deposition and subsequent curing of the flowable layer 1618 forms a second insulating layer (not shown) over the insulating layer 1018. In some examples, this second insulating layer is formed of a different layer of material than the insulating layer 1018.

[0105] In certain embodiments, the lamination process is a vacuum lamination process that may be performed in an autoclave or other suitable device. In certain embodiments, the lamination process is performed by using a hot press process. In certain embodiments, the lamination process is performed at a temperature between about 80° C. and about 140° C. for about 1 minute to about 30 minutes. In some embodiments, the lamination process includes applying a pressure between 10 psig and about 100 psig while subjecting the substrate 302 and the insulating film 1616 to a temperature between about 80° C. and about 140° C. for about 1 minute to about 30 minutes. For example, the lamination process is performed at a pressure between about 30 psig and about 80 psig and a temperature between about 100° C. and about 120° C. for about 2 minutes to about 10 minutes. For example, the lamination process is performed at a temperature of about 110° C. for about 5 minutes. In a further example, the lamination process is performed at a pressure between about 30 psig and about 70 psig, such as about 50 psig.

[0106] In operation 1504 and FIG. 16B, the support layer 1622 and the carrier 1624 are removed from the embedded die assembly 1002 by a mechanical process. After removing the support layer 1622 and the carrier 1624, the embedded die assembly 1002 is subjected to a curing process to fully cure the newly extended insulating layer 1018. In certain embodiments, the curing process is substantially similar to the curing process described with respect to operations 918 and 1150. For example, the curing process is performed at a temperature between about 140° C. and about 220° C. for a period between about 15 minutes and about 45 minutes, such as at a temperature between about 160° C. and about 200° C. for a period between about 25 minutes and about 35 minutes. For example, the curing process is performed at a temperature of about 180° C. for about 30 minutes. In further embodiments, the curing process in operation 1504 is performed at or near ambient pressure conditions.

[0107] The embedded die assembly 1002 is then selectively patterned by laser ablation in operation 1506 and FIG. 16C. The laser ablation in operation 1506 forms redistribution vias 1603 through the newly expanded insulating layer 1018 and exposes the desired interconnects 1444 for redistribution of their contact points. In certain embodiments, the redistribution vias 1603 have a diameter between about 5 μm and about 60 μm, such as between about 10 μm and about 50 μm, such as between about 20 μm and about 45 μm. In certain embodiments, the laser ablation process in operation 1506 is performed using a CO2 laser. In certain embodiments, the laser ablation process in operation 1506 is performed using a UV laser. In another embodiment, the laser ablation process in operation 1506 is performed using a green laser. For example, the laser source may generate a pulsed laser beam having a frequency between about 100 kHz and about 1000 kHz. In one example, the laser source is configured to provide a pulsed laser beam having a wavelength between about 100 nm and about 2000 nm, a pulse duration between about 10E-4 ns and about 10E-2 ns, and a pulse energy between about 10 μJ and about 300 μJ.

[0108] After the embedded die assembly 1002 is patterned, the embedded die assembly 1002 is subjected to a desmear process substantially similar to the desmear process in operations 922 and 1170. During the desmear process in operation 1506, any unwanted residue and debris formed by laser ablation during the formation of the redistribution vias 1603 is removed from the redistribution vias 1603 to clean (e.g., wash) the surfaces of the redistribution vias 1603 for subsequent metallization. In certain embodiments, the desmear process is a wet process. Any suitable aqueous etchant, solvent, and / or combination thereof may be utilized for the wet desmear process. In one example, a KMnO4 solution may be utilized as the etchant. In another embodiment, the desmear process is a dry desmear process. For example, the desmear process may be a plasma desmear process using an O2 / CF4 gas mixture. In a further embodiment, the desmear process is a combination of a wet process and a dry process.

[0109] In operation 1508 and FIG. 16D, an optional adhesion layer 1640 and / or seed layer 1642 is formed on the insulating layer 1018. In certain embodiments, the adhesion layer 1640 is formed from titanium, titanium nitride, tantalum, tantalum nitride, manganese, manganese oxide, molybdenum, cobalt oxide, cobalt nitride, or any other suitable material, or combinations thereof. In certain embodiments, the adhesion layer 1640 has a thickness between about 10 nm and about 300 nm, such as between about 50 nm and about 150 nm. For example, the adhesion layer 1640 has a thickness between about 75 nm and about 125 nm, such as about 100 nm. The adhesion layer 1640 may be formed by any suitable deposition process, including, but not limited to, CVD, PVD, PECVD, ALD, and the like.

[0110] The optional seed layer 1642 is formed from a conductive material, such as copper, tungsten, aluminum, silver, gold, or any other suitable material, or combinations thereof. In certain embodiments, the seed layer 1642 has a thickness between about 50 nm and about 500 nm, such as between about 100 nm and about 300 nm. For example, the seed layer 1642 has a thickness between about 150 nm and about 250 nm, such as about 200 nm. In certain embodiments, the seed layer 1642 has a thickness between about 0.1 μm and about 1.5 μm. Similar to the adhesion layer 1640, the seed layer 1642 may also be formed by any suitable deposition process, such as CVD, PVD, PECVD, a dry ALD process, a wet electroless plating process, or the like. In certain embodiments, the molybdenum adhesion layer 1640 and the copper seed layer 1642 are formed on the embedded die assembly 1002 to reduce undercutting of the conductive interconnect lines during a subsequent seed layer etching process in operation 1520.

[0111] In operations 1510, 1512, and 1514, which correspond to Figures 16E, 16F, and 16G, respectively, a spin-on / spray-on or dry resist film 1650, such as photoresist, is applied over the adhesive and / or seed surface of the embedded die assembly 1002, followed by patterning and development. In certain embodiments, an adhesion promoter (not shown) is applied to the embedded die assembly 1002 before the resist film 1650 is applied. The resist film 1650 is exposed and developed, which results in the opening of the redistribution vias 1603. Thus, the patterning of the resist film 1650 may be performed by selectively exposing portions of the resist film 1650 to UV radiation, and the subsequent development of the resist film 1650 may be performed by a wet process, such as a wet etching process. In certain embodiments, the resist film development process is a wet etching process that utilizes a buffered etching process that is selective to the desired material. In other embodiments, the resist film development process is a wet etching process that utilizes an aqueous etching process. Any suitable wet etchant or any suitable combination of wet etchants may be used for this resist film development process.

[0112] In operations 1516 and 1518, corresponding to Figures 16H and 16I, respectively, redistribution connections 1644 are formed through the exposed redistribution vias 1603, followed by removal of the resist film 1650. The redistribution connections 1644 are formed by any suitable method, including electroplating and electroless deposition. In certain embodiments, the resist film 1650 is removed by a wet process. As shown in Figures 16H and 16I, the redistribution connections 1644 fill the redistribution vias 1603, and after removal of the resist film 1650, the redistribution connections 1644 protrude from the surface of the embedded die assembly 1002. In certain embodiments, the redistribution connections 1644 are formed of copper. In other embodiments, the redistribution connections 1644 may be formed of any suitable conductive material, including, but not limited to, aluminum, gold, nickel, silver, palladium, tin, and the like.

[0113] In operation 1520 and FIG. 16J, the embedded die assembly 1002 having the redistribution connections 1644 formed thereon is subjected to a seed layer etching process substantially similar to the process of operation 1370. In certain embodiments, the seed layer etching is a wet etching process that includes rinsing and drying the embedded die assembly 1002. In certain embodiments, the seed layer etching process is a wet etching process that utilizes a buffered etching process that is selective to the desired material of the seed layer 1642. In other embodiments, the etching process is a wet etching process that utilizes an aqueous etching process. Any suitable wet etchant or any suitable combination of wet etchants may be used for the seed layer etching process.

[0114] In operation 1522, one or more completed packages 1602 are singulated from the embedded die assembly 1002, as shown in FIG. 16K and FIG. 16L. However, prior to operation 1522, additional redistribution layers may be formed on the embedded die assembly 1002, as shown in FIG. 16L, utilizing the sequence and process described above (FIG. 16K shows the completed package 1602 with one additional redistribution layer 1658). For example, one or more additional redistribution layers 1660 may be formed on an opposite side or surface of the embedded die assembly 1002 from the first additional redistribution layer 1658, such as on the major surface 1007. Alternatively, one or more additional redistribution layers 1660 may be formed on the same side or surface as the first additional redistribution layer 1658 (not shown), such as on the major surface 1005. The completed packages 1602 may then be singulated from the embedded die assembly 1002 after all desired redistribution layers have been formed.

[0115] The packaging structures, e.g., intermediate embedded die assembly 1002 and / or packages 1602, formed by the methods described above may be used in any suitable packaging application and in any suitable configuration. In one exemplary embodiment, shown generally in FIG. 17A, four packages 1602 are used to form a stack structure 1700, e.g., a DRAM stack. Accordingly, each package 1602 includes a double-sided die 1026 (e.g., a memory or similar chip) embedded in a substrate 302 and encapsulated by (e.g., a portion of each side is in contact with) an insulating layer 1018. One or more interconnects 1444 are formed through the entire thickness of each package 1602, and the interconnects 1444 are in direct contact with one or more solder bumps 1746 disposed between the major surface 1005 and the major surface 1007 of an adjacent (i.e., stacked above or below) package 1602. For example, as shown in stack structure 1700, four or more solder bumps 1746 are disposed between adjacent packages 1602 to bridge (e.g., connect, couple) the interconnects 1444 of each package 1602 to the interconnects 1444 of an adjacent package 1602.

[0116] In certain embodiments, to enhance the reliability of the solder bumps 1746, an encapsulant material 1748 fills the voids between adjacent packages 1602 connected by the solder bumps 1746. The encapsulant material 1748 may be any suitable type of encapsulant or underfill. In one example, the encapsulant material 1748 includes a pre-assembly underfill material, such as a no-flow underfill (NUF) material, a nonconductive paste (NCP) material, and a nonconductive film (NCF) material. In one example, the encapsulant material 1748 includes a post-assembly underfill material, such as a capillary underfill (CUF) material, and a molded underfill (MUF) material. In certain embodiments, the encapsulant material 1748 includes a SiO2, AlN, Al2O3, SiC, Si3N4, Sr2Ce2Ti5O 16 , ZrSiO4, CaSiO3, BeO, CeO2, BN, CaCu3Ti4O 12 , low expansion filled resins such as epoxy resins filled with (e.g., including) MgO, TiO2, ZnO, and the like.

[0117] In certain embodiments, the solder bumps 1746 are formed of one or more intermetallic compounds, such as a combination of tin (Sn) with lead (Pb), silver (Ag), Cu, or any other suitable combination of metals. For example, the solder bumps 1746 are formed of a solder alloy, such as Sn-Pb, Sn-Ag, Sn-Cu, or any other suitable material or combination thereof. In certain embodiments, the solder bumps 1746 include C4 (controlled collapse chip connection) bumps. In certain embodiments, the solder bumps 1746 include C2 (chip connection, such as Cu pillar with solder cap) bumps. The use of C2 solder bumps allows for smaller pitch between contact pads and improved thermal and / or electrical properties for the stack structure 1700. In some embodiments, the solder bumps 1746 have a diameter between about 10 μm and about 150 μm, such as between about 50 μm and about 100 μm in diameter. The solder bumps 1746 may also be formed by any suitable wafer bumping process, including, but not limited to, electrochemical deposition (ECD) and electroplating.

[0118] In another exemplary embodiment, shown generally in Figure 17B, four packages 1602 are stacked together and one or more interconnects 1444 of each package 1602 are directly bonded to the interconnects 1444 of one or more adjacent packages 1602 to form a stack structure 1701. As shown, the packages 1602 may be bonded by hybrid bonding, whereby the major surfaces 1005 and 1007 of adjacent packages are planarized and in full contact with one another. Thus, the one or more interconnects 1444 of each package 1602 are formed through the entire thickness of the respective package 1602 and directly contact one or more interconnects 1444 of at least another adjacent package 1602.

[0119] The stacked structures 1700 and 1701 offer numerous advantages over conventional stacked package structures. Such advantages include a thin form factor and high die-to-package volume ratio, which enable greater I / O scaling to meet the ever-increasing bandwidth and power efficiency demands of artificial intelligence (AI) and high performance computing (HPC). The utilization of a structured silicon core frame provides optimal material stiffness and thermal conductivity for improved electrical performance, thermal management and reliability of three-dimensional integrated circuit (3D IC) architectures. Additionally, the fabrication methods for assembly through-via and via-in-via structures described herein provide high performance and flexibility for 3D integration at relatively low manufacturing costs compared to conventional TSV technology.

[0120] In certain embodiments of the present disclosure, the disclosed devices and methods are intended to replace more conventional flip chip ball grid array (fcBGA) packaging structures that are limited by the inherent properties of materials typically utilized to form these various structures. In particular, conventional fcBGA packaging structures can exhibit greater mechanical stresses due to thermal expansion mismatch between components of the packaging structure, resulting in high rates of bending, warping, and / or collapse of the substrate. Scaling the substrates for these devices to improve signal integrity and power delivery further amplifies such stresses, resulting in reduced structural stability of the devices. Accordingly, the devices disclosed herein can be integrated with stiffening frames, thus providing semiconductor package devices that address many of the above-mentioned disadvantages associated with conventional fcBGA packaging structures.

[0121] 18A-18B show schematic side cross-sectional views of different configurations of device 1800 including package 1602 integrated with stiffening frame 1810, according to certain embodiments of the present disclosure. In certain examples, device 1800 may be utilized for structural support and electrical interconnection of additional semiconductor packages or other devices in a stacked configuration, which may be mounted to device 1800 using any suitable technique, such as flip chip or wafer bumping. In certain examples, device 1800 may be utilized as a carrier structure for surface mounted devices, such as chips or graphics cards, in addition to semiconductor die 1026.

[0122] 18A-18B, the device 1800 includes a stiffening frame 1810 formed on the first side 1007 and / or the second side 1007 of the device 1800. The stiffening frame 1810 provides additional rigidity to the overall structure of the device 1800, thus reducing or eliminating the risk of warping or collapse of, for example, the substrate 302 or the package 1602 during integration of the device 1800 into a high density integrated device (e.g., stacked semiconductor packages, PCB assemblies, PCB spacer assemblies, chip carrier assemblies, intermediate carrier assemblies, memory stacks, etc.). Thus, integrating the stiffening frame 1810 with the package 1602 allows for the utilization of a thinner substrate 302, which facilitates improved signal integrity (e.g., lower insertion loss) and improved power delivery (e.g., lower power loss) between components on either side of the substrate 302. In certain embodiments, the stiffening frame 1810 may further provide a shielding effect for one or more semiconductor dies or devices, such as the semiconductor die 1026 or 1820 shown in Figures 18A-18B, embedded or stacked with the package 1602.

[0123] In general, the stiffening frame 1810 has a polygonal or circular ring-like shape and is formed from a patterned substrate comprising any suitable substrate material. In certain embodiments, the stiffening frame 1810 may be formed from a substrate comprising a material substantially similar to that of the substrate 302, and thus matching the coefficient of thermal expansion (CTE) of the substrate 302 to reduce or eliminate the risk of warping during assembly. For example, the stiffening frame 1810 may be formed from a substrate comprising a material substantially similar to that of the substrate 302, and thus matching the coefficient of thermal expansion (CTE) of the substrate 302, to reduce or eliminate the risk of warping during assembly. For example, the stiffening frame 1810 may be formed from a substrate comprising a material substantially similar to that of the substrate 302, and thus matching the coefficient of thermal expansion (CTE) of the substrate 302 ... <100> Or Si <111> ), silicon oxide, silicon germanium, doped or undoped silicon, undoped high resistivity silicon (e.g., float zone silicon having a lower dissolved oxygen content and a resistivity between about 5000 and about 10000 ohm-cm), doped or undoped polycrystalline silicon, silicon nitride, silicon carbide (e.g., silicon carbide having a conductivity of about 500 W / mK), quartz, glass (e.g., borosilicate glass), sapphire, alumina, and / or ceramic materials. In certain embodiments, the stiffening frame 1810 comprises monocrystalline p-type or n-type silicon. In certain embodiments, the stiffening frame 1810 comprises polycrystalline p-type or n-type silicon.

[0124] The stiffening frame 1810 has a thickness T between about 50 μm and about 1500 μm, such as a thickness T between about 100 μm and about 1200 μm. For example, the stiffening frame 1810 has a thickness T between about 200 μm and about 1000 μm, such as a thickness T between about 400 μm and about 800 μm, such as a thickness T of about 775 μm. In another example, the stiffening frame 1810 has a thickness T between about 100 μm and about 700 μm, such as a thickness T between about 200 μm and about 500 μm. In another example, the stiffening frame 1810 has a thickness T between about 800 μm and about 1400 μm, such as a thickness T between about 1000 μm and about 1200 μm. In yet another example, the stiffening frame 1810 has a thickness T greater than about 1200 μm.

[0125] The stiffening frame 1810 may be attached to the package 1602 by any suitable method. For example, as shown in FIGS. 18A-18B, the stiffening frame 1810 may be attached to the package 1602 by an adhesive 1811, which may include a laminate adhesive material, a die attach film, an adhesive film, glue, wax, or the like. In certain embodiments, the adhesive 1811 is a layer of uncured dielectric material, such as an epoxy resin material with ceramic fillers, similar to the dielectric material of the insulating layer 1018. In certain embodiments, the stiffening frame 1810 is attached directly to the insulating layer 1018 of the major surface 1005 or 1007 (FIG. 18A). In certain other embodiments, the stiffening frame 110 is attached directly to the substrate 302 or to a passivating layer or metal clad layer formed on the substrate 302 (FIG. 18B). In such embodiments, desired portions of the insulating layer 1018 may be removed, for example by laser ablation, to allow for attachment of the stiffening frame 1810 to the substrate 302 .

[0126] The stiffening frame 1810 may be patterned to form one or more openings 1877 therethrough, which in certain embodiments may receive one or more semiconductor dies 1820 (or other devices) therein. The openings 1877 thus allow for direct integration (e.g., stacking) of the semiconductor dies 1820 either on the insulating layer 1018 of the package 1602 or on the substrate 302 without requiring further extension of the interconnects through the stiffening frame 1810. In further embodiments, the stiffening frame 1810 may further provide mechanical and / or electrical shielding for the dies 1820. For example, as shown in FIGS. 18A-18B, the stiffening frame 1810 may include a metal clad layer 1812 formed thereon and connected to ground (not shown), which may provide electromagnetic interference (EMI) shielding for the die 1820 disposed in the opening 1877 or the die 1026 embedded in the package 1602. In such an embodiment, the metal clad layer 1812 may include substantially the same material as the metal clad layer 316 described above and may be formed by a substantially similar process as the metal clad layer 316. For example, the metal clad layer 1812 may be formed by nickel displacement plating or other electroless or electrolytic plating processes. In certain embodiments, the stiffening frame 1810 is formed of high resistivity silicon and acts as an insulator for the device 1800. In such an embodiment, the stiffening frame 1810 may be attached to the package 1602 by soldering. For example, a metal or surface layer (eg, a nickel or copper layer) may be formed on the package 1602 and then the stiffening frame 1810 may be soldered onto the package 1602 .

[0127] The one or more openings 1877 may generally have any shape and dimensions suitable for accommodating, for example, a semiconductor die 1820 or other desired device in the one or more openings 1877. For example, in certain embodiments, the openings 1877 may have a substantially quadrilateral or polygonal shape. In certain embodiments, the openings 1877 may have a substantially circular shape or an irregular shape. In certain embodiments, one or more of the openings 1877 have substantially tapered (i.e., angled) sidewalls 1821 as shown in FIGS. 18A-B, or substantially vertical (e.g., at a right angle, e.g., perpendicular to the surface 1005) sidewalls 1821.

[0128] In certain embodiments, the one or more openings 1877 have a lateral dimension D in the range between about 0.5 mm and about 50 mm, such as a lateral dimension D in the range between about 3 mm and about 12 mm, such as a lateral dimension D in the range between about 8 mm and about 11 mm, where the lateral dimension D may be determined by the size and number of semiconductor die 1820 or other devices to be placed in the one or more openings 1877 during manufacturing of the package or system. In certain embodiments, the openings 1877 are sized to have a lateral dimension substantially similar to the lateral dimension of the semiconductor die 1820 to be placed in the openings 1877. For example, each opening 1877 may be formed to have a lateral dimension that is less than about 150 μm, such as less than about 120 μm, such as less than 100 μm, larger than the lateral dimension of the semiconductor die 1820.

[0129] The semiconductor die 1820 may be any suitable type of die, chip, or semiconductor device, including a memory die, a microprocessor, a complex system on chip (SoC), a standard die, or a passive semiconductor device. In certain embodiments, the semiconductor die 1820 is a DRAM die or a NAND flash die. In certain embodiments, the semiconductor die 1820 includes a digital die, an analog die, or a mixed die. In certain embodiments, the semiconductor die 1820 includes passive semiconductor devices, such as capacitors, inductors, resistors, RF elements, etc., which may be electrically coupled to power contacts 1031 of the semiconductor die 1026 embedded in the package 1602 to enable a more stable power supply across the device 1800. For example, the semiconductor die 1820 may include a decoupling capacitor, a trench capacitor, or a planar capacitor. In certain embodiments, the semiconductor die 1820 may be formed of a material substantially similar to the material of the substrate 302, the die 1026, and / or the stiffening frame 1810, such as a silicon material. Utilizing the semiconductor die 1820 formed from the same or similar material as that of the substrate 302, the die 1026 and / or the stiffening frame 1810 may facilitate matching the CTE therebetween and may essentially eliminate the occurrence of warpage during assembly.

[0130] 18A-18B, each semiconductor die 1820 may be disposed adjacent one of the major surfaces 1005, 1007 of the package 1602 and has contacts 1822 electrically coupled to one or more redistribution connections 1644 via solder bumps 1824. In certain embodiments, the contacts 1822 and / or solder bumps 1824 are formed of a material substantially similar to the material of the interconnects 1444 and the redistribution connections 1644. For example, the contacts 1822 and solder bumps 1824 may be formed of a conductive material such as copper, tungsten, aluminum, silver, gold, or any other suitable material, or combinations thereof.

[0131] In certain embodiments, the solder bumps 1824 comprise C4 solder bumps. In certain embodiments, the solder bumps 1824 comprise C2 (Cu pillar with solder cap) solder bumps. The use of C2 solder bumps may allow for smaller pitch lengths and improved thermal and / or electrical properties for the device 1800. The solder bumps 1824 may be formed by any suitable wafer bumping process, including, but not limited to, electrochemical deposition (ECD) and electroplating.

[0132] 18C-E show top views of different configurations of the device 1800, according to certain embodiments of the present disclosure. In particular, FIG. 18C-E show different configurations / arrangements of the stiffening frame 1810.

[0133] In Figure 18C, device 1800 includes a squircular (e.g., rectangular with rounded corners) ring-shaped stiffening frame 1810 that surrounds semiconductor die 1820 disposed within opening 1877 and substantially follows the lateral perimeter of device 1800 (and thus package 1602 disposed below). Thus, the outer dimensions of stiffening frame 1810 are substantially similar to the outer dimensions of package 1602. Note that while stiffening frame 1810 in Figure 18C is shown as having rounded corners, chamfered or square corners are also contemplated.

[0134] 18D, a stiffening frame 1810 formed on a device 1800 has an irregular polygonal shape to accommodate multiple semiconductor dies 1820 of different sizes. A single opening 1877 is formed in the stiffening frame 1810, but in different lateral dimensions around each of the semiconductor dies 1820.

[0135] In FIG. 18E, the stiffening frame 1810 has a rectangular ring-like shape bounded by one or more transverse ribs 1830 that extend across the surface of the device 1800 (and thus the underlying package 1602). The ribs 1830 thus form a plurality of openings 1877 for receiving a plurality of semiconductor dies 1820. Forming the ribs 1830 in the stiffening frame 1810 may provide additional mechanical support / rigidity to the device 1800. In certain embodiments, the ribs 1830 may be arranged in a crisscross or cross pattern on the device 1800. It should be noted that while the stiffening frame 1810 in FIG. 18E is shown as a rectangle with right angle corners, other overall shapes and / or corner types are contemplated.

[0136] 18C-18E, in certain embodiments, the stiffening frame 1810 may have lateral dimensions that are substantially consistent with or substantially similar to the package 1602. Thus, in such embodiments, the outer lateral dimensions L1 and L2 are within about 500 μm, such as within about 300 μm, of the outer lateral dimensions of the package 1602. In certain embodiments, the lateral dimensions L1 and L2 are substantially equal to one another.

[0137] Figure 19 illustrates a flow diagram of an exemplary method 1900 of forming a packaging structure, e.g., an fcBGA type device, having a stiffening frame 2010, utilizing, e.g., the embedded die assembly 1002 described above, in accordance with certain embodiments of the present disclosure. Figures 20A-20J illustrate schematic cross-sectional views of the embedded die assembly 1002 at different stages of the method 1900. For clarity, Figure 19 and Figures 20A-20J are described herein together for clarity.

[0138] 19 and 20A-20J are described as utilizing embedded die assembly 1002, the methods of Figures 19 and 20A-20J may similarly be performed on previously singulated packages 1602. Additionally, while Figures 19 and 20A-20J are described with respect to forming a stiffening frame on an fcBGA type packaging structure, the operations described below may be performed on other types of devices, such as PCB assemblies, PCB spacer assemblies, chip carrier and mid-carrier assemblies (e.g., for graphics cards), memory stacks, etc.

[0139] The method 1900 generally begins with operation 1902 and FIG. 20A, in which a solder mask 2066a is applied to a "front side" or "device side" surface of the intermediate core assembly 1002. For example, the solder mask 2066a is applied to the major surface 1005 of the embedded die assembly 1002. Typically, the solder mask 2066a has a thickness between about 10 μm and about 100 μm, such as between about 15 μm and about 90 μm. For example, the solder mask 2066a has a thickness between about 20 μm and about 80 μm.

[0140] In certain embodiments, the solder mask 2066a is a thermally curable epoxy liquid silk screened onto the insulating layer 1018 on the device side of the embedded die assembly 1002 through a patterned woven mesh. In certain embodiments, the solder mask 2066a is a liquid photo-imageable solder mask (LPSM) or liquid photo-imageable ink (LPI) silk screened or sprayed onto the device side of the embedded die assembly 1002. The liquid photo-imageable solder mask 2066a is then exposed and developed in a subsequent operation to form the desired pattern. In other embodiments, the solder mask 2066a is a dry film photo-imageable solder mask (DFSM) that is vacuum laminated to the device side of the embedded die assembly 1002 and then exposed and developed in a subsequent operation. In such embodiments, a thermal or UV cure is performed after the pattern is defined in the solder mask 2066a.

[0141] In operation 1904 and FIG. 20B , the embedded die assembly 1002 is flipped over and a second solder mask 2066b is applied to the “backside” or “non-device side” surface of the embedded die assembly 1002. For example, the solder mask 2066b is applied to the major surface 1007 of the embedded die assembly 1002. Generally, the solder mask 2066b is substantially similar to the solder mask 2066a, although in certain embodiments the solder mask 2066b is of a different type or material than the solder mask 2066a, selected from among the solder mask types / materials discussed above.

[0142] In operation 1906 and FIG. 20C, the embedded die assembly 1002 is flipped over again and the solder mask 2066a is patterned to form vias 2003a in the solder mask 2066a. The vias 2003a expose the desired interconnects 1444 and / or redistribution connections 1644 on the device side of the embedded die assembly 1002 for designated signal routing to the outer surface of the package during fabrication.

[0143] In certain embodiments, the solder mask 2066a may be patterned by the methods described above. In yet other embodiments, the solder mask 2066a may be patterned, for example, by laser ablation. In such embodiments, the laser ablation patterning process may be performed utilizing a CO2 laser, a UV laser, or a green laser. For example, the laser source may generate a pulsed laser beam having a frequency between about 100 kHz and about 1000 kHz. In one example, the laser source is configured to provide a pulsed laser beam having a wavelength between about 100 nm and about 2000 nm, a pulse duration between about 10E-4 ns and about 10E-2 ns, and a pulse energy between about 10 μJ and about 300 μJ.

[0144] In operation 1908 and FIG. 20D, the embedded die assembly 1002 is again flipped over and the solder mask 2066b is patterned to form vias 2003b in the solder mask 2066b. Similar to the vias 2003a, the vias 2003b also expose the desired interconnects 1444 and / or redistribution connections 1644 on the embedded die assembly 1002 for designated signal routing to the outer surface of the package during fabrication. In general, the solder mask 2066b may be formed by any of the methods described above, including laser ablation.

[0145] After both sides of the embedded die assembly 1002 are patterned, the embedded die assembly 1002 is transferred to a curing rack and the embedded die assembly 1002 with the solder masks 2066a, 2066b attached thereto is fully cured in operation 1910 and FIG. 20E. In certain embodiments, the curing process is carried out at a temperature between about 80° C. and about 200° C. for a period between about 10 minutes and about 80 minutes, such as between about 90° C. and about 200° C. for a period between about 20 minutes and about 70 minutes. For example, the curing process is carried out at a temperature of about 180° C. for a period of about 30 minutes, or at a temperature of about 100° C. for a period of about 60 minutes. In further embodiments, the curing process in operation 1910 is carried out at or near ambient (e.g., atmospheric) pressure conditions.

[0146] In operation 1912 and Figure 20F, a plating process is performed on both the device side and the non-device side of the embedded die assembly 1002 to form conductive layers 2070a and 2070b, respectively, on the device side (e.g., the side shown facing up including surface 1005) and the non-device side (e.g., the side shown facing down including surface 1007) of the embedded die assembly 1002. As shown in Figure 20F, the plated conductive layers 2070a, 2070b extend the interconnects 1444 and / or redistribution connections 1644 through the device-side vias 2003a and the non-device-side vias 2003b to facilitate electrical connection of the interconnects 1444 and / or redistribution connections 1644 to other devices and / or packaging structures.

[0147] Each conductive layer 2070a and 2070b is formed of one or more metal layers formed by electroless plating. For example, in certain embodiments, each conductive layer 2070a and 2070b includes an electroless nickel plating layer covered with a thin layer of gold and / or palladium formed by electroless nickel immersion gold (ENIG) or electroless nickel electroless palladium immersion gold (ENEPIG). However, other metal materials and plating techniques are also contemplated, including soft ferromagnetic metal alloys and highly conductive pure metals. In certain embodiments, the conductive layers 2070a and / or 2070b are formed of one or more layers of copper, chromium, tin, aluminum, nickel chromium, stainless steel, tungsten, silver, etc.

[0148] In certain embodiments, on the device or non-device side of the embedded die assembly 1002, each conductive layer 2070a and / or 2070b has a thickness between about 0.2 μm and about 20 μm, such as between about 1 μm and about 10 μm. During plating of the conductive layers 2070a and 2070b, the exposed interconnects 1444 and / or redistribution connections 1644 are further extended outwardly from the embedded die assembly 1002 through the solder masks 2066a, 2066b to facilitate further bonding with additional devices in subsequent manufacturing operations.

[0149] In operation 1914 and FIG. 20G, a solder-on-pad (SOP) process is performed on both the device side and non-device side of the embedded die assembly 1002 to form solder pads 1280a and 1280b, respectively, on the device side and non-device side of the embedded die assembly 1002. For example, in certain embodiments, solder is applied to the vias 2003a, 2003b and then reflowed, followed by a planarization process such as coining to form a substantially flat surface for the solder pads 2080a, 2080b.

[0150] In operation 1916 and FIG. 20H, a bonding layer 2090 is applied to the desired areas / surfaces of the solder mask 2066a (e.g., device side) onto which the stiffening frame 2010 is to be attached. In certain embodiments, the bonding layer 2090 comprises a laminating adhesive material, a die attach film, an adhesive film, glue, wax, etc. In certain embodiments, the bonding layer 2090 is a layer of dielectric material, such as an epoxy resin material with ceramic fillers, similar to the dielectric material of the insulating layer 1018. In certain embodiments, the bonding layer 2090 is a solder layer. The bonding layer 2090 may be applied to the solder mask 2066a by mechanical rolling, pressing, laminating, spin coating, doctor blading, etc.

[0151] However, in certain embodiments, rather than applying the bonding layer 2090 to the solder mask 2066a, the bonding layer 2090 may be applied directly to the stiffening frame 2010, which may then be attached to the solder mask 2066a of the embedded die assembly 1002. When a die attach or adhesive film is used as the bonding layer 2090 in such embodiments, the film may be trimmed to the lateral dimensions of the stiffening frame 2010 when the stiffening frame 2010 is structured / patterned.

[0152] After application of the bonding layer 2090 to the embedded die assembly 1002, a stiffening frame 2010 is attached to the bonding layer 2090 in operation 1918 and FIG. 20I. As shown, the stiffening frame 2010 includes one or more openings 2017 into which a semiconductor die may be attached in a subsequent operation. To form the openings 2017, prior to operation 1916, the stiffening frame 2010 may be patterned by the methods described above with reference to FIGS. 2-7D.

[0153] In operation 1920 and FIG. 20J, one or more semiconductor dies 2020 are electrically coupled to the solder pads 2080a exposed through the openings 2017 on the device side of the embedded die assembly 1002 via solder bumps 2024, ball grid arrays (BGAs) 2040 are mounted to the solder pads 2080b on the non-device side, and the embedded die assembly 1002 is singulated into one or more electrically functional devices 2000 (further singulation is not required in embodiments where the operations of FIG. 19 and FIG. 20A-FIG. 20J are performed on the singulated package 1602). In certain embodiments, the BGAs 2040 are formed by electrochemical deposition to form C4 or C2 type bumps. In certain embodiments, the semiconductor die 2020 is bonded to the solder pads 2080a by a flip chip die attach process that flips the semiconductor die 2020 over and connects the contact or bond pads 2022 of the semiconductor die 2020 to the solder pads 2080a. In certain examples, the connection between the contacts 2022 and the solder pads 2080a is performed by mass reflow or thermo-compression bonding (TCB). In such examples, a capillary underfill, a non-conductive paste or a non-conductive film may be laminated between the semiconductor die 2020 and the embedded die assembly 1002. In certain embodiments, the semiconductor die 2020 and / or the BGA 2040 are bonded to the embedded die assembly 1002 before attaching the stiffening frame 1810 and then singulating the embedded die assembly 1002.

[0154] After singulation, each singulated device 2000 may then be integrated with other semiconductor devices and packages in a variety of 2.5D and 3D configurations and architectures, such as homogeneous or heterogeneous 3D stacked systems. Generally, when a stiffening frame, such as stiffening frame 2010, is incorporated into a device 2000 that is then integrated into a larger stacked system, the beneficial reduction in warpage of the device 2000 is further extended to the entire system. That is, increasing the structural integrity of the device 2000 reduces the likelihood of warpage or collapse of the entire integrated system.

[0155] 21 is a schematic side cross-sectional view of an exemplary stack system 2100 according to an embodiment described herein, which integrates a device 2000 with a stiffening frame 1810 formed thereon, thereby improving the structural integrity of the system 2100. As shown, in addition to the device 2000, the exemplary system 2100 further includes one or more PCBs 2120, which may be vertically stacked or arranged side-by-side, a high bandwidth memory (HBM) module 2130 with a large parallel interconnect density between the memory die and a central processing unit (CPU) core or logic die, and one or more heat exchangers 2110. In the example of FIG. 21, the semiconductor die 2020 of the device 2000 may represent a graphics processing unit (GPU) electrically coupled to the HBM 2130 via the interconnects 1444 arranged through the package 1602 as well as solder bumps 2024 and BGA 2040. The device 2000 may be electrically connected to the PCB 2120 via, for example, redistribution connections 1644 formed on the non-device side of the device 2000 and pin-type connectors 2122 formed on the PCB 2120 .

[0156] The integration of a heat exchanger 2110, such as a heat sink, improves the heat dissipation and thermal performance of the device 2000, and thus the system 2100, by transferring heat, for example, heat conducted by the semiconductor die 2020, the embedded die 1026, the HBM 2130, and / or the silicon substrate 302. The improved heat dissipation further reduces the likelihood of warping. Suitable types of heat exchangers 2110 include pin heat sinks, straight heat sinks, flared heat sinks, and the like, which may be formed of any suitable material, such as aluminum or copper. In certain embodiments, the heat exchanger 2110 is formed of extruded aluminum. In certain embodiments, the heat exchanger 2110 is directly attached to one or more semiconductor dies integrated within the system 2100, such as the semiconductor die 2020 and one or more dies of the HBM module 2130, as shown in FIG. 21. In other embodiments, the heat exchanger 2110 is attached directly to the substrate 302 or indirectly to the substrate 302 through an insulating layer 1018. Such an arrangement is particularly beneficial over conventional PCBs formed from fiberglass reinforced epoxy laminates, which have low thermal conductivity. The addition of a heat exchanger to a conventional PCB would be of little value.

[0157] 22A-22B each show schematic side cross-sectional views of additional device configurations 2200 and 2201 of device 2000 according to embodiments described herein. As shown in FIG. 22A, a stiffening frame 2010 is attached with a lid 2210, which covers a semiconductor die 2020 stacked on and electrically coupled to device 2000. Some conventional integrated circuits, such as microprocessors or GPUs, generate a significant amount of heat during operation that must be carried away to avoid device damage or device shutdown. For such devices, the lid 2210 serves as a protective cover and a heat transfer path. Additionally, the lid 2210 provides additional structural reinforcement to the device 2000 that already includes the stiffening frame 2010 formed thereon. Thus, the device configuration 2200 facilitates improved heat dissipation and thermal performance as well as improved structural integrity when compared to conventional packaging structures.

[0158] Generally, the lid 2210 has a polygonal or circular ring-like shape and is formed from a patterned substrate comprising any suitable substrate material. In certain embodiments, the lid 2210 may be formed from a substrate that comprises a material substantially similar to that of the stiffening frame 2010 and the substrate 302, and thus matches the coefficient of thermal expansion (CTE) of the stiffening frame 2010 and the substrate 302, reducing or eliminating the risk of warping of the device configuration 2200 during assembly. For example ... III-V compound semiconductor material, silicon (e.g., silicon having a resistivity between about 1 and about 10 Ohm-com, or a conductivity of about 100 W / mK), crystalline silicon (e.g., Si <100> Or Si <111> ), silicon oxide, silicon germanium, doped or undoped silicon, undoped high resistivity silicon (e.g., float zone silicon having a lower dissolved oxygen content and a resistivity between about 5000 and about 10000 ohm-cm), doped or undoped polycrystalline silicon, silicon nitride, silicon carbide (e.g., silicon carbide having a conductivity of about 500 W / mK), quartz, glass (e.g., borosilicate glass), sapphire, alumina, and / or ceramic materials. In certain embodiments, the lid 2210 comprises monocrystalline p-type or n-type silicon. In certain embodiments, the lid 2210 comprises polycrystalline p-type or n-type silicon.

[0159] The lid 2210 has a thickness T of about 50 μm to about 1500 μm, such as a thickness T of about 100 μm to about 1200 μm. For example, the lid 2210 has a thickness T of about 200 μm to about 1000 μm, such as a thickness T of about 300 μm to about 775 μm, such as a thickness T of about 750 μm or 775 μm. In another example, the lid 2210 has a thickness T of about 100 μm to about 700 μm, such as a thickness T of about 200 μm to about 500 μm. In another example, the lid 2210 has a thickness T of about 800 μm to about 1400 μm, such as a thickness T of about 1000 μm to about 1200 μm. In yet another example, the lid 2210 has a thickness T of more than about 1200 μm.

[0160] The lid 2210 is attached to the stiffening frame 2010 by any suitable method. For example, as shown in FIG. 22A, the lid 2210 may be attached to the stiffening frame 2210 by a bonding layer 2290, which may include a lamination adhesive material, a die attach film, an adhesive film, glue, wax, etc. In certain embodiments, the bonding layer 2290 is a layer of uncured dielectric material, such as an epoxy resin material with ceramic fillers, similar to the dielectric material of the insulating layer 1018.

[0161] In addition to being attached to the stiffening frame 2010, the lid 2210 is also indirectly attached to the semiconductor die 2020 via a thermal interface material (TIM) layer 2292 to provide a thermal transfer path to the semiconductor die 2020. Generally, the TIM layer 2292 eliminates voids or spaces between the semiconductor die 2020 and the lid 2020 to maximize heat transfer and dissipation, eliminating voids or spaces from the interface between the semiconductor die 2020 and the lid 2020 that act as thermal insulators. In certain embodiments, the TIM layer 2292 comprises a thermal paste, a thermal adhesive (e.g., glue), a thermal tape, an underfill material, or a potting compound. In certain embodiments, the TIM layer 2292 is a thin layer of a flowable dielectric material substantially similar to the flowable dielectric material of the insulating layer 1018, such as a flowable epoxy resin with an aluminum oxide or nitride filler.

[0162] 22B illustrates another device configuration 2201 that integrates a lid 2210 with the device 2000. In this example, the lid 2210 and stiffening frame 2010 are both metallized. As shown, the lid 2210 includes a metal layer 2296 and the stiffening frame 2010 includes a metal layer 2212. The metal layers 2212, 2296 may be formed of any suitable metallic material and may be formed by any suitable method, including the materials and methods described above with respect to the metal cladding layer 316 described above. For example, in certain embodiments, the metal layer 2212 and / or the metal layer 2296 include a conductive metal layer including nickel (e.g., formed by immersion plating), aluminum, gold, cobalt, silver, palladium, tin, or the like. In certain embodiments, the metal layer 2212 and / or the metal layer 2296 include a metal layer including an alloy or pure metal including nickel, aluminum, gold, cobalt, silver, palladium, tin, or the like. In certain embodiments, metal layer 2212 and metal layer 2296 are formed of the same material, while in other embodiments, metal layer 2212 and metal layer 2296 are formed of different materials.

[0163] As shown in FIG. 22B, the metal layer 2212 and the metal layer 2296 may be electrically coupled to one another utilizing one or more solder balls 2294 disposed between the lid 2210 and the stiffening frame 2010. In such embodiments, the bonding layer 2290 may be formed around the solder balls 2294, such that the solder balls 2294 are substantially embedded in the bonding layer 2290. In certain embodiments, the metal layer 2212 and / or the metal layer 2296 are further electrically coupled to ground, e.g., via the solder balls 2294, thus providing a grounded lid 2210 and stiffening frame 2010. In certain embodiments, the metal layer 2212 and / or the metal layer 2296 are further coupled to the metallized substrate 302, e.g., via the solder balls 2294 and the interconnects 1444 and / or the redistribution connections 1644.

[0164] 23A-23B each show schematic side cross-sectional views of exemplary devices 2300 and 2301 according to embodiments described herein, including a package 1602 having a double-sided die 1026 embedded therein. In the example of FIGS. 23A-23B, the package 1602 is further integrated with a heat exchanger 2330. The integration of a heat exchanger 2330, such as a heat sink, improves the heat dissipation and thermal properties of the packaged device 1602, and thus the devices 2300 and 2301, by transferring heat, e.g., generated by the semiconductor die 1026 and / or the substrate 302, or conducted by, e.g., the semiconductor die 1026 and / or the substrate 302. The improved heat dissipation further reduces the possibility of warping, improving the performance of the devices 2300 and 2301. Such an arrangement is particularly beneficial over conventional PCBs made of fiberglass reinforced epoxy laminates, which have low thermal conductivity. The addition of a heat exchanger to a conventional PCB would be of little value. Types of heat exchangers 2330 suitable for use with the embodiments described herein include pin heat sinks, straight heat sinks, flared heat sinks, and the like, which may be made of any suitable material, such as aluminum or copper. In certain embodiments, the heat exchanger 2330 is made of extruded aluminum.

[0165] In general, the heat exchanger 2330 may be added to one or both sides of the device 2300 or 2301. In certain embodiments, the heat exchanger 2330 is mounted directly on the substrate 302 or indirectly through the insulating layer 1018. To achieve such a configuration, the desired area of ​​the insulating layer 1018 of the package 1602 (or embedded die assembly 1002) may be laser ablated to form a pocket, after which the heat exchanger 2330 may be mounted on the substrate 302. For example, an area of ​​the insulating layer 1018 having lateral dimensions corresponding to those of the heat exchanger 2330 may be removed by a CO2, UV or IR laser configured to ablate only the dielectric material of the insulating layer 10018 and leave the substrate 302 intact. The heat exchanger 2330 may then be placed in the opening and mounted on the substrate 302 by any suitable mounting method. The substrate 302 may include an oxide layer or a metal clad layer. In certain embodiments, an adhesive or interface layer may be placed between the heat exchanger 2330 and the substrate 302 .

[0166] In other embodiments, the heat exchanger 2330 is attached directly to one or more semiconductor dies stacked with the device 2300 or 2301, such as the semiconductor die 1820 described above. In further embodiments, the heat exchanger 2330 may be placed on the embedded semiconductor die 1026 and the substrate 302, or may be attached to the insulating layer 1018 or another layer disposed on the insulating layer 1018, as shown in FIG. 23A. For example, the device 2300 includes a metallization plane 2310 and an interface layer 2320 disposed between the package 1600 and the heat exchanger 2330. The metallization plane 2310 may include a conductive metal layer formed of any suitable metal material, including copper, nickel, aluminum, gold, cobalt, silver, palladium, tin, and the like, and may be connected to ground. In certain embodiments, the metallization plane 2310 includes a metal layer formed of an alloy or pure metal, including copper, nickel, aluminum, gold, cobalt, silver, palladium, tin, and the like. In certain embodiments, the metallized plane 2310 comprises a metal mesh or grid formed of the materials described above. In certain embodiments, the interface layer 2320 comprises a thermal interface material (TIM) material, such as a thermal adhesive or potting compound. In certain embodiments, the interface layer 2320 is a thin layer of a flowable dielectric material substantially similar to the material of the insulating layer 1018.

[0167] In another exemplary device 2301 shown in FIG. 23B, one or more capacitors 2340 or other passive devices are disposed between the heat exchanger 2330 and the package 1602 to enable a more stable power supply to the semiconductor die 1026. In such an embodiment, the capacitors may be embedded or disposed within one or more layers disposed above the semiconductor die 1026, including the insulating layer 1018, and may be electrically connected to the semiconductor die 1026 by the interconnects 1444 and / or redistribution connections 1644. FIG. 23B shows two capacitors 2340 disposed above the semiconductor die 1026 and surrounded by a metallized plane 2310, an interface layer 2320, and a heat spreader layer 2350. In certain embodiments, the heat spreader layer 2350 is formed of a metallic material suitable for conducting and spreading heat, including copper, nickel, aluminum, gold, cobalt, silver, palladium, tin, combinations or alloys thereof, and the like. In certain embodiments, an additional interface layer 2360, such as another TIM layer, may be formed between the heat spreader layer 2350 and the heat exchanger 2330, and the additional interface layer 2360 may further be in contact with or formed on the capacitor 2340.

[0168] Advantageously, the embodiments described herein provide improved methods of substrate structuring and die assembly for manufacturing advanced integrated circuit packages. By utilizing the methods described above, high aspect ratio features can be formed on glass and / or silicon substrates, thus enabling the economical formation of thinner and narrower semiconductor device packages. The thin, small form factor packages manufactured by utilizing the methods described above provide the benefits of high I / O density and improved bandwidth and power, as well as higher reliability due to a package architecture that allows for lower stress due to reduced weight / inertia and flexible solder ball distribution. Further advantages of the methods described above include economical manufacturing with two-sided metallization capability and high production yields due to the elimination of flip-chip attachment and overmolding steps that are prone to damaging features in the high volume manufacturing of conventional and advanced packages.

[0169] While the foregoing is directed to embodiments of the present disclosure, other and further embodiments of the present disclosure may be devised without departing from the basic scope thereof, the scope of the disclosed embodiments being determined by the claims.

Claims

1. a core frame having a first surface opposite a second surface; A frame material including silicone; at least one cavity, a semiconductor die disposed within the at least one cavity, the semiconductor die having electrical contacts disposed on two opposing sides of the semiconductor die; and a via including a via surface, the via defining an opening extending through the core frame from the first surface to the second surface; A core frame further comprising: an insulating layer disposed over the first surface and the second surface, the insulating layer in contact with at least a portion of each side of the semiconductor die; an electrical interconnect disposed within the via, the insulating layer being disposed between a surface of the via and the electrical interconnect; Package assembly including:

2. The package assembly of claim 1 , wherein the at least one cavity has a lateral dimension of between about 3 mm and about 50 mm.

3. 3. The package assembly of claim 2, wherein the lateral dimensions of the at least one cavity are less than about 150 μm larger than the lateral dimensions of the semiconductor die.

4. 10. The package assembly of claim 1, wherein the semiconductor die includes an integrated circuit formed on a first side and a power delivery network formed on a second side opposite the first side.

5. The package assembly of claim 1 , further comprising an oxide layer formed on the core frame.

6. The package assembly of claim 1 , further comprising a metal layer formed on the core frame.

7. The package assembly of claim 6 , wherein the metal layer comprises nickel.

8. The package assembly of claim 1 , wherein the insulating layer comprises an epoxy resin.

9. The package assembly of claim 8 , wherein the epoxy resin comprises ceramic particles.

10. The package assembly of claim 9 , wherein the ceramic particles comprise silica particles.

11. The package assembly of claim 1 , further comprising an adhesion or seed layer disposed between the electrical interconnect and the insulating layer.

12. The package assembly of claim 11 , wherein the adhesion layer comprises molybdenum and the seed layer comprises copper.

13. The package assembly of claim 1 , further comprising a capacitor disposed on the insulating layer and electrically coupled to one or more contacts of the semiconductor die.

14. 10. The package assembly of claim 1, further comprising a stiffening frame formed on said insulating layer, said stiffening frame comprising a silicone material, said stiffening frame having an opening formed therein.

15. 15. The package assembly of claim 14, further comprising a capacitor disposed on the insulating layer and within the opening of the stiffening frame, the capacitor being electrically coupled to one or more contacts of the semiconductor die.

16. a buried die assembly, A core frame containing silicon, an oxide layer disposed on a surface of the core frame; one or more semiconductor dies disposed within the core frame, the one or more semiconductor dies having an integrated circuit formed on a first side and a power delivery network formed on a second side opposite the first side; and an insulating layer formed on the oxide layer, the insulating layer comprising an epoxy resin material, the epoxy resin material having ceramic particles disposed in the epoxy resin material; a buried die assembly including: one or more metal interconnects disposed within a portion of the embedded die assembly; Package including assembly.

17. The core frame further comprises: one or more cavities formed in the core frame, the one or more cavities having the one or more semiconductor dies disposed within the one or more cavities; and 17. The package assembly of claim 16, comprising: one or more vias formed in the core frame, the one or more metal interconnects passing through the one or more vias.

18. 17. The package assembly of claim 16, further comprising a molybdenum adhesion layer and a copper seed layer disposed between each of the one or more metal interconnects and the insulating layer.

19. a buried die assembly, A core frame containing silicon, one or more semiconductor dies disposed within the core frame, the one or more semiconductor dies having electrical contacts disposed on two opposing sides of the one or more semiconductor dies; a first insulating layer formed on the core frame, the first insulating layer including an epoxy resin material including ceramic particles; and One or more electrical interconnects disposed through the core frame or the first insulating layer. a buried die assembly including: a redistribution layer formed on the embedded die assembly; the redistribution layer comprising: a second insulating layer formed on the first insulating layer; and one or more electrical redistribution connections disposed through the second insulating layer; Including, package assembly.

20. 20. The package assembly of claim 19, wherein the second insulating layer is formed of the same material as the first insulating layer.

Citation Information

Patent Citations

  • Multilayer wiring board and manufacturing method there for

    JP2003204011A

  • Electronic device

    JP2014216509A

  • Semiconductor package

    JP2019161214A

  • Stacked silicon package assembly with improved stiffeners - Patents.com

    JP2019501534A

  • Backside drilling embedded die substrate

    JP2019511120A

Cited By

  • Fabrication of embedded die packaging comprising laser drilled vias