Improved welding method for laser welding of battery foil stacks, welding method, laser processing system, and related computer program products
The method of remelting weld seam edges with reduced heat input addresses the cracking issue in welding multilayer aluminum foil stacks, enhancing the strength and quality of weld seams in lithium ion batteries.
Patent Information
- Application Number
- JP2024529192
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-16
- Filing Date
- 2022-11-14
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2042-11-14
AI Technical Summary
Lithium ion battery manufacturing faces challenges in directly welding multilayer aluminum foil stacks to battery components due to thin aluminum foils prone to cracking, especially at the weld seam edges, caused by oxide layers and high tensile stress, leading to deformation and cracking during laser welding.
A method involving remelting the weld seam edges of multilayer aluminum foil stacks with a laser beam using lower heat input, multiple times, to reduce internal stresses and prevent cracking, forming a stronger and higher-quality weld seam.
Reduces cracking in the weld seam edges by minimizing internal stresses through controlled remelting, resulting in a more robust and continuous weld seam.
Smart Images

Figure 2024543514000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an improved method for improving a weld seam, a welding method for welding a multi-layer aluminum foil stack of a battery current collector to a battery component, a laser processing system, a control device for a laser processing system and a computer program product.The present invention relates in particular to the field of lithium ion batteries and laser welding.
[0002] Background technology Lithium-ion batteries are superior in many respects to other types of batteries and are therefore widely used in a variety of fields.
[0003] In lithium-ion batteries, the positive electrode comprises a current collector made of lithium cobalt oxide (or lithium nickel cobalt manganate, lithium manganate, lithium iron phosphate, etc.) and aluminum foil, and the negative electrode comprises a current collector made of graphitized carbon material and copper foil. Aluminum foil is also used as the current collector of the positive electrode. Multilayer aluminum foil stacks are used in lithium-ion batteries to obtain a larger aluminum foil surface that can be coated with more active material. To manufacture the battery, the multilayer aluminum foil stack needs to be effectively connected to the poles. Since the aluminum foil is very thin, ultrasonic welding is usually suitable for the connection. Since the poles are usually irregular in shape, a connector, usually in the form of a sheet, is added between the aluminum foil stack and the poles. In this case, the aluminum foil stack and the connector are first connected by ultrasonic welding, and then the connector, which is less likely to cause welding cracks, is connected to the poles by laser welding.
[0004] However, in order to reduce the weight of the battery cells and to enable ultra-fast charging, the goal is to eliminate the connector. In this case, it is required to directly weld the multi-layer aluminum foil stack to the pole. However, the thin aluminum foil is very susceptible to cracking during welding, especially at the interface edge of the fusion. This is mainly due to the following reasons: the surface of the aluminum foil is often covered with an Al2O3 oxide layer, and the melting point and hardness of this oxide layer are significantly higher than those of the aluminum foil as the base material, so that parts of the oxide layer cannot be completely melted during the welding process and gather at the weld seam edge, which significantly increases the hardness of the weld seam edge and is prone to cracking; due to the thin thickness of the aluminum foil, the aluminum foil near the heat-affected zone of the molten pool is easily deformed significantly under the action of high temperature, and the tensile stress generated by this process also increases the risk of molten pool cracking; the temperature unevenness and material deformation caused by the laser energy input during welding also increase the risk of cracking.
[0005] Furthermore, since the weld seam is elongated in the feed direction, the molten pool of the weld seam is U-shaped when viewed in a cross section perpendicular to the feed direction, i.e., the edge profile of the molten pool is very steep, which causes the aluminum foil to be significantly deformed at the edge of the molten pool, and the resulting tensile stress makes it easy for continuous cracks to occur at the molten edge of the molten pool.
[0006] Disclosure Summary It is an object of the present invention to provide an improved method for improving weld seams that can reduce cracking when welding multi-layer aluminum foil stacks and provide high strength, high quality weld seams.
[0007] According to a first aspect of the present invention, there is provided an improved method for improving a weld seam formed by welding a multi-layer aluminum foil stack of a current collector of a battery and a component of the battery, the improved method comprising at least a remelting step of remelting a weld seam edge of the weld seam provided on a surface of the multi-layer aluminum foil stack at least once by a laser beam with a lower heat input than the heat input for forming the weld seam.
[0008] In this context, "part" is to be understood in particular as any component of the battery that is welded together with the multi-layer aluminum foil stack. "Weld seam" is to be understood in particular as any form of weld seam formed by welding the multi-layer aluminum foil stack to the part by means of a laser beam, in particular as an initial weld seam formed in a conventional manner. The weld seam can be formed by a linear, curved or similar trajectory of the laser beam on the multi-layer aluminum foil stack. "Weld seam edge of a weld seam provided on the surface of the multi-layer aluminum foil stack" is to be understood in particular as the contour line of the weld seam provided on the surface of the multi-layer aluminum foil stack or the boundary line between the weld seam and the aluminum foil as base material of this weld seam or the weld toe of the weld seam. The weld seam edge in particular defines the width of the weld seam. "Weld seam width" is to be understood in particular as the width of the weld seam transverse to the feed direction of the laser beam. After each remelting, in particular a new weld seam edge is formed on the surface of the multi-layer aluminum foil stack. In this specification, the term "weld seam edge" always refers in particular to the border between the weld seam and the aluminum foil as base material, and not to the internal line of the weld seam resulting from remelting. The feature "remelting the weld seam edge ... of a weld seam provided on the surface of a multi-layer aluminum foil stack" covers in particular the remelting of at least a part of the two weld seam edges of the weld seam, in particular the complete remelting of the two weld seam edges. Of course, when the weld seam edge is remelted, the molten pool formed by the laser beam is, for example, wider than the weld seam edge, so that the area near the weld seam edge is also melted at the same time. Furthermore, of course, after remelting, the melted area solidifies and thus a new weld seam edge is formed.
[0009] According to an optional embodiment of the present invention, in the remelting step, the weld seam edge of the weld seam provided on the surface of the multi-layer aluminum foil stack is remelted multiple times by the laser beam, the heat input used for the first remelting is lower than the heat input used to form the weld seam, the heat input used for each remelting after the first remelting is reduced compared to the previous remelting, and in each remelting, the weld seam edge formed by the previous remelting is remelted. The expression "multiple times" is particularly understood as "at least two times". Each remelting relates in particular to two weld seam edges of the weld seam provided on the surface of the multi-layer aluminum foil stack.
[0010] According to an optional embodiment of the invention, in the remelting step, the laser beam is moved relative to the multi-layer aluminum foil stack along the weld seam edge or in the vicinity of and parallel to the weld seam edge. Obviously, it is not essential that the focus of the laser beam must be along the weld seam edge, but it is sufficient if the weld seam edge is within the molten pool of the laser beam.
[0011] According to an optional embodiment of the invention, in order to achieve a lower heat input in the re-melting step, the laser power of the laser beam is reduced compared to the laser power for forming the weld seam and / or the movement speed of the laser beam relative to the multi-layer aluminum foil stack is increased compared to the movement speed for forming the weld seam.
[0012] In accordance with an optional embodiment of the present invention, the weld seam edge formed by each remelt is offset away from the weld seam edge formed by the immediately preceding remelt.
[0013] According to an optional embodiment of the invention, the lengths of the weld seam edges formed by the individual remelting are equal to each other, where "equal" is to be understood in particular to encompass "absolutely equal" and "substantially equal", with "substantially equal" particularly meaning to include a deviation within ±10%, in particular within ±5%.
[0014] According to an optional embodiment of the present invention, the depth of the molten pool at each remelt is decreased with increasing number of remelts and is less than the thickness of the multi-layer aluminum foil stack.
[0015] According to an optional embodiment of the present invention, the total number of remelts is selected such that the weld seam meets the requirements regarding cracking.
[0016] According to an optional embodiment of the invention, the battery is a lithium ion battery.
[0017] According to an optional embodiment of the invention, the component is a positive electrode of a battery.
[0018] According to a second aspect of the present invention, there is provided a welding method for welding a multi-layer aluminium foil stack of a current collector of a battery and a component of the battery, the welding method comprising an initial welding step of welding the multi-layer aluminium foil stack and the component by means of a laser beam, thereby forming a weld seam, and an improvement step of carrying out the improvement method described above on the weld seam.
[0019] According to an optional embodiment of the invention, in a first welding step a weld seam is formed on the surface of the multi-layer aluminum foil stack by a linear or curved trajectory of a laser beam.
[0020] According to an optional embodiment of the invention, the welding method is performed by scanning optics or a fixed welding head, which in particular refers to a welding head in which the laser beam does not move relative to the welding head.
[0021] According to an optional embodiment of the invention, prior to the welding process, the aluminum foils of the multi-layer aluminum foil stack were ultrasonically pre-welded to each other.
[0022] According to a third aspect of the present invention, there is provided a laser processing system comprising at least a laser device for generating a laser beam and a control device for controlling at least the laser device, the laser processing system being configured to perform the above-mentioned improvement or the above-mentioned welding method.
[0023] According to a fourth aspect of the present invention there is provided a controller for a laser processing system, the controller being configured to carry out the improvement described above or the welding method described above.
[0024] According to a fifth aspect of the present invention there is provided a computer program product comprising computer program instructions which, when executed by a processor, performs the improvement as defined above or the welding method as defined above.
[0025] The positive effects of the present invention are: by remelting the molten edge of the initial weld seam with lower power, the internal stresses in the molten edge area of the newly formed weld seam during the solidification process can be reduced, thereby reducing cracks in the molten edge area; by repeated remelting, the length of the crack can be reduced, and the crack becomes discontinuous with successive reductions in the welding energy.
[0026] The principles, features and advantages of the present invention may be better understood from the following more detailed description of the invention when taken in conjunction with the accompanying drawings. [Brief description of the drawings]
[0027] [Figure 1] FIG. 1 is a schematic partial cross-sectional view of an example battery. [Diagram 2] FIG. 1 is a schematic perspective view of an example laser processing system. [Diagram 3] FIG. 2 is a schematic plan view of an example of a weld seam and an area of the weld seam that is susceptible to cracking. [Figure 4] 4 is a schematic cross-sectional view of the molten pool of the weld seam shown in FIG. 3. [Diagram 5] 1 is a schematic plan view of a welded seam and an example of improving the welded seam according to the present invention; [Figure 6] 6 is a schematic cross-sectional view of the molten pool of the weld seam shown in FIG. 5.
[0028] Detailed Description of the Preferred Embodiments In order to make the technical problem to be solved by the present invention, the technical solution and the beneficial technical effects more clear, the present invention will be described in more detail below with reference to the accompanying drawings and several exemplary embodiments. Of course, the specific embodiments described herein are only used to explain the present invention, rather than to limit the protection scope of the present invention.
[0029] First, it is pointed out that for the purposes of clarity and brevity of the drawings, only one weld seam edge, only one weld seam edge formed by a crack or remelting of the weld seam and the like, is referenced.
[0030] FIG. 1 shows an example of a battery in a schematic partial cross-sectional view. In this specification, the battery is a lithium-ion battery by way of example. However, it is clear that the concept of the present invention is not limited to lithium-ion batteries, but may also be applied to other types of batteries, for example sodium-ion batteries. Furthermore, the concept of the present invention is not limited to batteries with a rectangular shell, but may also be applied to pouch-type batteries, cylindrical batteries, and batteries of other shapes with similar welded seams. The cells of the lithium-ion battery are formed, for example, by a multi-layer stack structure. In this multi-layer stack structure, a separator is provided between each aluminum foil and copper foil. Further materials required for manufacturing the battery are interposed between these layers. This is well known to those skilled in the art and will not be described in detail. These aluminum foil layers protrude at one end of the cell and are pre-welded by ultrasonics to form a current collector of the positive electrode. The multi-layer aluminum foil stack 10 of the current collector of the positive electrode comprises, for example, 20 to 130 aluminum foil layers. The positive electrode of the battery also comprises, for example, a positive electrode, a positive tab, and the like. The current collector of the positive electrode generally needs to be connected to the positive electrode, and possibly to the positive tab or another component of the battery. Such connection is usually achieved by welding. For example, the multi-layer aluminum foil stack 10 and the component 20 below the bottom aluminum foil layer of the multi-layer aluminum foil stack 10, such as the positive electrode, need to be welded by a laser beam 430 to form a weld seam 30.
[0031] FIG. 2 shows an example of a laser processing system 40 in a perspective view. For example, the laser processing system 40 is used for welding and / or improving the weld seam 30 of FIG. 1. For example, the laser processing system 40 includes a laser device 410 for generating a laser beam 430 and a control device 420 for controlling at least the laser device 410. The laser processing system 40 may further include a support table (shown diagrammatically as a plane in FIG. 2) for supporting the objects to be welded (i.e., the multi-layer aluminum foil stack 10 and the part 20) and / or a fixture and the like for holding the objects to be welded. The support table and / or fixture may be fixed or movable. The control device 420 may control the movement of the support table and / or fixture as required. The laser device 410 may include, for example, scanning optics or a fixed welding head.
[0032] When the multi-layer aluminum foil stack 10 of the current collector of the battery shown in FIG. 1 is welded, the weld seam 30 shown in FIG. 3 is typically used. In FIG. 3, this weld seam 30 is shown diagrammatically in a plan view. The length to width ratio is shown in FIG. 3 only for the sake of clarity, in reality the width may be significantly smaller than the length. The length of the weld seam 30 is, for example, 20 mm to 60 mm, and the width is, for example, 2 mm to 6 mm. The weld seam 30 is, for example, elongated in FIG. 3. To form such a weld seam 30, the laser beam 430 generally follows a linear trajectory relative to the multi-layer aluminum foil stack 10. However, it is also possible here to use other trajectories depending on the shape and size of the weldable area. For example, the laser beam 430 may additionally perform an oscillatory movement with a narrow amplitude transverse to the feed direction to the linear feed movement in the feed direction. The feed direction of the laser beam 430 is indicated in FIG. 3 by an arrow and by the symbol V. In Figure 3, a crack-prone region 340 in the weld seam 30 (i.e., the region near the initial weld seam edge 300) is shown by hatched diagonal lines. Although the weld seam 30 has two initial weld seam edges 300, only one of them is labeled for clarity and simplicity of the drawings. In Figure 4, a cross-section of the weld pool of the weld seam 30 shown in Figure 3 is shown diagrammatically. The crack-prone region 340 is also shown in Figure 4 by hatched diagonal lines. The cross-section of Figure 4 is shown diagrammatically in Figure 3 by dashed lines.
[0033] FIG. 5 shows a schematic plan view of a weld seam 30 and an example of improving the weld seam 30 according to the invention. The improvement method for improving the weld seam 30 is performed, for example, by the laser processing system 40 of FIG. 2. The improvement method for improving the weld seam 30 includes at least a remelting step. In this remelting step, the weld seam edge of the weld seam 30 provided on the surface of the multi-layer aluminum foil stack 10 is remelted at least once by a laser beam 430 with a lower heat input than the heat input for forming the weld seam 30. The initial weld seam 30 may be formed by the laser processing system 40 performing the improvement method. In this case, the laser processing system 40 performs a welding method for welding the multi-layer aluminum foil stack 10 of the battery current collector to the component 20 of the battery. The welding method includes an initial welding step and an improvement step. First, in the initial welding step, the multi-layer aluminum foil stack 10 and the component 20 are welded by the laser beam 430, thereby forming the weld seam 30. With regard to the initial weld seam 30 shown in Fig. 5, please refer in particular to the description of the initial weld seam 30 in Fig. 3 and Fig. 4. Afterwards, in an improvement step, the above-mentioned improvement method is carried out to improve the weld seam 30. In the improvement step, the welding method is carried out, for example, by means of scanning optics or a fixed welding head. However, the initial welding step and the improvement step can also be carried out by different laser processing systems 40. In this case, the two laser processing systems 40 can be located in different factories.
[0034] As used herein, the improvement or welding method of the present invention may be implemented, for example, by the controller 420 of Fig. 2. The controller 420 may include, for example, a corresponding computer program product, which includes computer program instructions that, when executed by a processor, control the laser processing system 40 of Fig. 2 to implement the improvement or welding method.
[0035] According to an optional embodiment of the present invention, in order to achieve a lower heat input in the remelting step, the laser power of the laser beam 430 is reduced compared to the laser power for forming the weld seam 30 and / or the movement speed of the laser beam 430 relative to the multi-layer aluminum foil stack 10 is increased compared to the movement speed for forming the weld seam 30.
[0036] According to an exemplary embodiment of the present invention, the laser power used for remelting is 5%-50% of the laser power used for welding. Other parameters of the laser beam 430 than the power used for remelting, such as the focal diameter, the feed rate, etc., may remain unchanged compared to the first welding, but may be changed. Furthermore, the parameters of the laser beam 430 may be changed during each remelting. For example, different laser beam parameters may be used for the rear section of the weld seam edge in each remelting than for the front section, since the rear section of the weld seam 30 along the length may have more cracks due to the heat accumulation effect.
[0037] According to an exemplary embodiment of the present invention, in the remelting step, the weld seam edge of the weld seam 30 provided on the surface of the multi-layer aluminum foil stack 10 is remelted multiple times by the laser beam 430. In this case, the heat input used for the first remelting is lower than the heat input used to form the weld seam 30, and the heat input used for each remelting after the first remelting is reduced compared to the previous remelting, and in each remelting, the weld seam edge formed by the previous remelting is remelted. In particular, each remelting is performed at least after the molten pool of the previous remelting has solidified. In FIG. 5, it is shown that the weld seam edge is remelted twice. In FIG. 5, the first weld seam 30 is represented by a thick solid black line, the first remelting is represented by a thin dashed line, and the second remelting is represented by a thinner dashed line. In Fig. 5, reference is made to the initial weld seam edge 300, the weld seam edge 311 formed by the first remelting and the weld seam edge 322 formed by the second remelting. In Fig. 6, a cross-section of the weld pool of the weld seam 30 shown in Fig. 5 is shown diagrammatically in Fig. 5 by a dashed-dotted line. In Fig. 6, reference is made to the initial weld seam 30, the weld pool 310 during the first remelting and the weld pool 320 during the second remelting. Naturally, they overlap each other.
[0038] According to an exemplary embodiment of the present invention, in the remelting step, the laser beam 430 is moved along or near and parallel to the weld seam edge relative to the multi-layer aluminum foil stack 10. However, other trajectories of the laser beam 430 relative to the surface of the multi-layer aluminum foil stack 10 for remelting are also possible, for example trajectories with additional lateral oscillatory movements.
[0039] According to an exemplary embodiment of the invention, the weld seam edge formed by each remelt is offset away from the weld seam 30 from the weld seam edge formed by the previous remelt. As shown in FIG. 5, the weld seam edge 322 formed by the second remelt is offset away from the weld seam 30 from the weld seam edge 311 formed by the first remelt. This can also be considered as a continuous widening of the weld seam 30. However, it is also possible that the weld seam edge formed by the remelt is identical to the initial weld seam edge 300, i.e. the width of the weld seam 30 remains constant.
[0040] According to an exemplary embodiment of the invention, the weld seam edges formed by the individual remelts are equal in length to each other, however, it is also possible for each remelt to produce a weld seam edge that is slightly shorter (see FIG. 5) or slightly longer than the previous remelt, etc.
[0041] According to an exemplary embodiment of the present invention, as shown in FIG. 6, the depth of the molten pool at each remelt is decreased with an increasing number of remelts and is less than the thickness of the multi-layer aluminum foil stack 10.
[0042] According to an exemplary embodiment of the present invention, the total number of remelts is selected so that the weld seam 30 meets cracking requirements.
[0043] Although specific embodiments of the invention have been described in detail herein, these embodiments have been presented for purposes of illustration only and should not be considered as limiting the scope of the invention. Various substitutions, modifications and alterations may be made without departing from the spirit and scope of the invention.
Claims
1. An improvement to improve a weld seam (30) formed by welding a multi-layer aluminum foil stack (10) of a current collector of a battery and a component (20) of said battery, comprising: The improved method includes at least a remelting step of remelting a weld seam edge of the weld seam (30) provided on the surface of the multilayer aluminum foil stack (10) at least once with a laser beam (430) at a heat input lower than the heat input for forming the weld seam (30).
2. in the remelting step, a weld seam edge of the weld seam (30) provided on the surface of the multilayer aluminum foil stack (10) is remelted a number of times by the laser beam (430), the heat input used for a first remelt is lower than the heat input used to form the weld seam (30), the heat input used for each remelt after the first remelt is reduced compared to the previous remelt, and in each remelt, the weld seam edge formed by the previous remelt is remelted, and / or and / or moving the laser beam (430) relative to the multi-layer aluminum foil stack (10) along or adjacent to a weld seam edge parallel to the weld seam edge during the remelting step; In order to achieve a lower heat input during the remelting step, the laser power of the laser beam (430) is reduced compared to the laser power for forming the weld seam (30) and / or the movement speed of the laser beam (430) relative to the multilayer aluminum foil stack (10) is increased compared to the movement speed for forming the weld seam (30). The improved method of claim 1.
3. offsetting the weld seam edge formed by each remelt away from the weld seam (30) from the weld seam edge formed by the previous remelt; and / or the weld seam edges formed by the individual remeltings are equal in length to one another, and / or the depth of the molten pool at each remelt is reduced with increasing number of remelts and is less than the thickness of the multi-layer aluminum foil stack (10); and / or The total number of remeltings is selected so that the weld seam (30) meets the requirements regarding cracking. The improved method of claim 2.
4. the battery is a lithium ion battery; and / or The component (20) is the positive electrode of the battery. Improved process according to any one of claims 1 to 3.
5. A welding method for welding a multi-layer aluminum foil stack (10) of a current collector of a battery to a component (20) of said battery, comprising the steps of: a first welding step of welding said multi-layer aluminum foil stack (10) and said component (20) by means of a laser beam (430), thereby forming a weld seam (30); performing an improvement step on the weld seam (30) according to any one of claims 1 to 4; , a welding method.
6. The welding method of claim 5, wherein in the first welding step, the weld seam (30) is formed on the surface of the multi-layer aluminum foil stack (10) by a linear or curved trajectory of the laser beam (430).
7. The welding method is carried out by scanning optics or a fixed welding head, and / or Prior to the welding process, the aluminum foils of the multi-layer aluminum foil stack (10) were pre-welded to each other by ultrasonics. The welding method according to claim 5 or 6.
8. A laser processing system (40), comprising: a laser device (410) for generating a laser beam (430); A control device (420) for controlling at least the laser device (410); At least It is adapted to carry out the improvement according to any one of claims 1 to 4 or the welding method according to any one of claims 5 to 7, A laser processing system (40).
9. A control device (420) for a laser processing system (40), the control device (420) being configured to carry out the improvement according to any one of claims 1 to 4 or the welding method according to any one of claims 5 to 7.
10. A computer program product comprising computer program instructions which, when executed by a processor, performs the improvement according to any one of claims 1 to 4 or the welding method according to any one of claims 5 to 7.
Citation Information
Patent Citations
Success / failure determination method of laser welding
JP2018111120A
Butt welded joint of welded structure, and method for manufacturing same
WO2011068155A1
Fillet arc welding joint and method for manufacturing same
WO2017018492A1
Cited By
Fluoroquinoxalinone derivatives that selectively inhibit PARP1