Interface preparation for tandem photovoltaic devices
By employing an interface with controlled roughness and refractive index mismatch in tandem photovoltaic devices, reflections are minimized, leading to improved light transmission and efficiency across submodules.
Patent Information
- Application Number
- JP2024529204
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-10-25
- Filing Date
- 2022-11-16
- Publication Date
- 2024-11-21
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The challenge in producing efficient tandem photovoltaic devices lies in providing interfaces between submodules with desired electrical, optical, physical, and thermal properties, leading to increased reflection and reduced performance.
The implementation of an interface between submodules in tandem photovoltaic devices, comprising a first layer with controlled roughness and refractive index mismatch, and a transparent layer to minimize reflections and enhance optical coupling.
This approach reduces reflections, improves light transmission, and enhances the overall efficiency of tandem photovoltaic devices by optimizing the use of light across submodules.
Smart Images

Figure 2024543515000001_ABST
Abstract
Description
[Technical field]
[0001]
[0001] The present technology relates to photovoltaic devices, and more particularly, to methods for preparing interfaces in tandem photovoltaic devices to minimize undesired reflections. [Background technology]
[0002]
[0002] This section provides background information related to the present disclosure that is not necessarily prior art.
[0003] Photovoltaic devices generate power by converting light into electricity using semiconductor materials that exhibit the photovoltaic effect. Certain semiconductor materials are more efficient at absorbing certain ranges of the electromagnetic spectrum. To improve the overall efficiency of a photovoltaic device, the device can incorporate stacked sub-modules, also called subcells, that utilize semiconductor materials with different absorption characteristics to form a tandem photovoltaic device.
[0003]
[0004] In an exemplary tandem photovoltaic device, solar radiation or light enters through the top submodule and a portion of the radiation passes from the top submodule to the bottom submodule. The top submodule can absorb more of the higher energy photons having shorter wavelengths, while the bottom submodule can absorb less energy photons having longer wavelengths. An interface exists between the top and bottom submodules.
[0004]
[0005] Laboratory experiments measuring the absorption efficiency in relevant spectral ranges of separate submodules have shown that there are promising submodules that may be used together to absorb a larger fraction of the incident radiation. However, as the complexity of tandem architectures increases, it may also be difficult to bridge the gap between actual and theoretical performance. A major challenge to producing tandem photovoltaic devices with good efficiency and manufacturability lies in providing interfaces between the submodules that have the desired electrical, optical, physical and thermal properties.
[0005]
[0006] Thus, a need exists for methods for preparing interfaces in tandem photovoltaic devices and for minimizing undesired reflections in tandem photovoltaic device architectures. Summary of the Invention [Means for solving the problem]
[0006]
[0007] In accordance with this disclosure, the present technology provides articles of manufacture, systems and methods relating to how to make and use tandem photovoltaic devices.
[0008] A tandem photovoltaic device is provided that can include a first sub-module, a second sub-module, and an interface between the first and second sub-modules. The interface can pass a portion of light, thus optically coupling the first and second sub-modules. The optical coupling of the first and second sub-modules can include reducing reflection of a portion of the light passing through the interface.
[0007]
[0009] Particular embodiments of the tandem photovoltaic device may include the following aspects: The interface may include a first layer of a first submodule, the first layer adjacent to a second submodule. The first layer may have a first surface having a root mean square average roughness of less than 170 nanometers. The interface may include a second layer of the first submodule, the second layer in contact with the first surface of the first layer. The second layer of the interface may be positioned between the first layer and the second submodule. The first layer and the second layer may have a refractive index mismatch of at least 0.75. The first layer of the interface may include an absorber layer having a II-VI semiconductor, and the second layer may include a transparent layer. The second layer may include a conductive layer.
[0008]
[0010] Particular embodiments of the tandem photovoltaic device may include the following aspects. The interface may include a first layer of the first submodule and a second layer of the first submodule. The first layer of the interface of the first submodule may be adjacent to the second layer of the interface of the first submodule, and the first layer of the first submodule may have a first surface having a root mean square average roughness of about 50 nanometers to about 200 nanometers. The second layer of the first submodule may contact the first surface of the first layer. The second layer of the first submodule may be positioned between the first layer of the first submodule and the second submodule, and the first layer of the first submodule and the second layer of the first submodule may have a refractive index mismatch of less than 0.2. The second layer of the interface of the first submodule may include a first surface and a second surface, and the first surface of the second layer may contact the first surface of the first layer. The second surface of the second layer may have a root mean square roughness of less than 170 nanometers. The first layer of the first submodule interface may include an absorber layer having a II-VI semiconductor and the second layer may include a transparent layer. The transparent layer may include titanium dioxide.
[0009]
[0011] Methods of making and using a tandem photovoltaic device are provided that include providing a first sub-module and a second sub-module, and forming an interface between the first sub-module and the second sub-module. The interface passes a portion of light such that the interface optically couples the first sub-module and the second sub-module. The optical coupling of the first sub-module and the second sub-module includes reducing reflection of a portion of the light.
[0010]
[0012] Particular embodiments of making and using tandem photovoltaic devices may include the following aspects. The interface may include a first layer of a first submodule, the first layer adjacent to a second submodule, the first layer having a first surface, the first surface may be polished to provide a root mean square average roughness of less than 170 nanometers. In other embodiments, the interface may include a first layer and may also include a second layer of an interface of the first submodule, the first layer adjacent to a second layer, the second layer adjacent to the second submodule, the second layer of the interface being between the first layer and the second submodule. The first layer has a first surface, the first surface has a defined surface roughness. In some embodiments, the root mean square average of the first surface roughness is between about 50 nanometers and about 200 nanometers. In some embodiments, the root mean square average of the first surface roughness is between about 175 nanometers and about 200 nanometers. In some embodiments, the second layer of the interface of the first sub-module may include at least one conductive layer and a transparent layer. In some embodiments, the second layer may contact the first surface of the first layer. In some embodiments, the second layer may be positioned between the first layer and the second sub-module, and the first layer and the second layer may have a refractive index mismatch of less than 0.2.
[0011]
[0013] Further areas of applicability will become apparent from the description provided herein. The description and specific examples in this summary are intended for purposes of illustration only and are not intended to limit the scope of the present disclosure.
[0012]
[0014] The drawings described herein are only for purposes of illustrating selected embodiments rather than all possible implementations and are not intended to limit the scope of the present disclosure. [Brief description of the drawings]
[0013] [Figure 1A]
[0015] FIG. 1A shows a scanning transmission electron micrograph of a cross-section of a CdSeTe absorber stack showing surface roughness. [Figure 1B]
[0016] FIG. 1B shows an optical diagram illustrating total internal reflection at rough surface "facets," such as those found in FIG. 1A with visible roughness. [Diagram 2]
[0017] FIG. 2A-2C are schematic diagrams illustrating cross-sectional views of a tandem photovoltaic device according to one or more embodiments shown and described herein. [Diagram 3]
[0018] 2A-2C are schematic diagrams illustrating example sub-modules of the photovoltaic device of FIG. 1 according to one or more embodiments shown and described herein. [Figure 4]
[0019] FIG. 3 is a schematic diagram illustrating a cross-sectional view of the photovoltaic sub-module of FIG. 2 along 3-3 according to one or more embodiments shown and described herein. [Diagram 5]
[0020] 1A and 1B illustrate schematic diagrams of a substrate according to one or more embodiments shown and described herein. [Figure 6]
[0021] FIG. 2 illustrates a schematic cross-sectional view of the tandem photovoltaic device of FIG. 1 according to one or more embodiments shown and described herein. [Figure 7A]
[0022] FIG. 7A is a schematic diagram illustrating a cross-sectional view of an exemplary interface according to one or more embodiments shown and described herein. [Figure 7B]
[0023] FIG. 7B is a schematic diagram illustrating a cross-sectional view of another example interface according to one or more embodiments shown and described herein. [Figure 8]
[0024] FIG. 2 illustrates an example of a method for making a tandem photovoltaic device according to one or more embodiments shown and described herein. [Figure 9]
[0025] FIG. 9 illustrates another exemplary method of making a tandem photovoltaic device according to one or more embodiments shown and described herein. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014]
[0026] The following description of the technology is merely exemplary in nature of the subject matter, manufacture and use of one or more inventions, and is not intended to limit the scope, application, or use of any particular invention claimed in this application, or in any other application that may be filed claiming priority to this application, or in any patent issued therefrom. With respect to the disclosed methods, the order of steps presented is exemplary in nature, and thus the order of steps may vary in various embodiments, including cases where certain steps may be performed simultaneously, unless expressly stated otherwise. As used herein, "a" and "an" indicate the presence of "at least one" of an item; where possible, a plurality of such items may be present. Unless otherwise expressly stated, all numerical quantities herein are understood to be modified by the word "about" in describing the broadest scope of the technology, and all geometric and spatial descriptors are understood to be modified by the word "substantially". When applied to a numerical value, "about" indicates that the calculation or measurement allows for some imprecision in the value (with some approximation to the precision of the value; roughly or reasonably close to the value; approximately). If for any reason the imprecision implied by "about" and / or "substantially" is not otherwise understood in the art to have its ordinary meaning, then "about" and / or "substantially" as used herein will at least account for the variation that can result from ordinary methods of measuring or using such parameters.
[0015]
[0027] All documents cited in this detailed description, including patents, patent applications, and scientific literature, are incorporated herein by reference unless expressly indicated otherwise. In the event that a conflict or ambiguity may exist between a document incorporated by reference and this detailed description, this detailed description will control.
[0016]
[0028] The open-ended term "comprising" is used herein to describe and claim embodiments of the present technology as a synonym for non-limiting terms such as including, containing, or having, although embodiments may alternatively be described using more restrictive terms such as "consisting of" or "consisting essentially of." Thus, for any given embodiment that describes a material, component, or process step, the present technology also specifically includes embodiments that consist of, or consist essentially of, such material, component, or process step, except for (if consisting of), any additional material, component, or process that affects a critical property of the embodiment, even if such additional material, component, or process is not explicitly described in this application. For example, a description of a composition or process that describes elements A, B, and C specifically contemplates an embodiment that consists essentially of A, B, and C, excluding element D, which may be described in the art, even if element D is not explicitly described herein as excluded.
[0017]
[0029] As referred to herein, the disclosure of a range includes all separate values and further divided ranges throughout the range, including the endpoints, unless otherwise specified. Thus, for example, a range of "A to B" or "about A to about B" includes A and B. The disclosure of a value and value range of a particular parameter (amount, weight percentage, etc.) does not exclude other values and value ranges useful herein. It is contemplated that two or more specific exemplified values for a given parameter may define the endpoints of a range of values that may be claimed for the parameter. For example, if a parameter X is exemplified herein as having a value A and also as having a value Z, then it is contemplated that the parameter X has a range of values from about A to about Z. Similarly, the disclosure of two or more value ranges for a parameter (whether such ranges are nested, overlapping, or separate) is contemplated to encompass all possible combinations of the ranges of values that may be claimed using the endpoints of the disclosed ranges. For example, if a parameter X is exemplified herein as having a value in the range of 1 to 10, or 2 to 9, or 3 to 8, it is contemplated that the parameter X may have other ranges of values, including 1 to 9, 1 to 8, 1 to 3, 1 to 2, 2 to 10, 2 to 8, 2 to 3, 3 to 10, 3 to 9, etc.
[0018]
[0030] When an element or layer is referred to as "resting," "engaged," "connected," or "coupled" with another element or layer, it may be directly resting, engaged, connected, or coupled with the other element or layer, or there may be intervening elements or layers. In contrast, when an element is referred to as "directly resting," "directly engaged," "directly connected," or "directly coupled" with another element or layer, there may not be intervening elements or layers. Other words used to describe relationships between elements should be interpreted similarly (e.g., "between" vs. "directly between," "adjacent" vs. "directly adjacent," etc.). As used herein, the term "and / or" includes any and all combinations of one or more of the associated listed items.
[0019]
[0031] Terms such as first, second, third, etc. may be used herein to describe various elements, components, regions, layers, and / or sections, but these elements, components, regions, layers, and / or sections should not be limited by these terms. These terms may be used only to distinguish one element, component, region, layer, or section from another region, layer, or section. Terms such as "first," "second," and other numerical terms, when used herein, do not imply any permutation or order unless clearly indicated by the context. Thus, a first element, component, region, layer, or section discussed below may be referred to as a second element, component, region, layer, or section without departing from the teachings of the exemplary embodiments.
[0020]
[0032] Spatially relative terms such as "inside," "outside," "lower," "below," "bottom," "upper," "top," and the like may be used herein for ease of description to describe the relationship of one element or feature shown in a figure to another element or feature. Spatially relative terms may be intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figure. For example, if a device in a figure is turned over, an element described as "below" or "below" the other element or feature would be oriented "above" the other element or feature. Thus, the exemplary term "lower" may encompass both an upper and lower orientation. A device may be oriented differently (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein may be interpreted accordingly.
[0021]
[0033] The term "light" may refer to various wavelengths in the electromagnetic spectrum, including, but not limited to, wavelengths in the ultraviolet (UV), infrared (IR), and visible portions of the electromagnetic spectrum. As used herein, "solar light" refers to light emitted by the sun.
[0022]
[0034] The term "layer" may refer to a thickness of material provided on a surface. A layer may cover all or a portion of a surface. A layer may include sublayers and may have a compositional gradient within the layer. A layer may include one or more functional layers of material. A layer may extend across substantially all of the full width and length of the module. A layer may be crossed, for example by a scribe.
[0023]
[0035] The present technology relates to a tandem photovoltaic device including a first sub-module and a second sub-module. However, it should be recognized that such a tandem photovoltaic device may include additional sub-modules, as well as additional arrangements of sub-modules. In the structure of the tandem photovoltaic device disclosed herein, an interface is provided between the first sub-module and the second sub-module, the interface passing a portion of the light. In this manner, the interface optically couples the first sub-module and the second sub-module, thereby reducing reflection of a portion of the light passing therethrough.
[0024]
[0036] In particular, the interface can reduce reflections compared to a substantially identical arrangement of the first and second sub-modules, but without the interface positioned therebetween. For example, reflections may cause a portion of the light to pass through the first sub-module and then reflect back to the first sub-module instead of passing onto the second sub-module. The interface may act accordingly on the reflection of such light, thereby improving the amount of light received by the second sub-module. Reflections may also include undesired scattering of light and polarization losses, each of which may be minimized by the interface. The optical coupling provided by the interface can optimize the performance of the tandem photovoltaic device by allowing each sub-module to receive a portion of the light to which they are conditioned, thus making better use of the available light.
[0025]
[0037] Tandem photovoltaic devices can generate electrical power by converting light into direct current electricity using semiconductor materials that exhibit the photovoltaic effect. The photovoltaic effect generates electrical power upon exposure to light because photons are absorbed in the semiconductor material, exciting electrons to a higher energy state. These excited electrons can move within the material, generating an electrical current. Semiconductor materials suitable for use in photovoltaic devices can include, for example, II-VI materials (including cadmium telluride alloys), I-III-VI materials (including CIGS and CIS materials), silicon, and perovskites.
[0026]
[0038] Tandem photovoltaic devices can achieve higher total conversion efficiencies than single photovoltaic devices by capturing a larger portion of the solar spectrum. Tandem devices may be formed using more than one p-n junction and materials with different bandgap properties that respond to different ranges or portions of the electromagnetic spectrum, including infrared, visible, and ultraviolet light. In devices where the primary light source is from above, the light incident top cell or upper submodule may have a large bandgap to capture high energy short wavelengths, while the bottom cell or lower submodule may use absorber materials with smaller bandgaps to capture longer wavelengths and reflected photons. Tandem devices may have two or more stacked subcells or submodules, with each submodule containing an active region formed from semiconductor materials with different absorption properties, including different types of semiconductor materials.
[0027]
[0039] The submodules of the tandem photovoltaic devices described herein may be stacked and separated by one or more interfaces. Incident electromagnetic radiation, i.e., light, enters the device through a first submodule (e.g., the front cell or top submodule). Light that is not absorbed by the first submodule reaches the interface. In certain embodiments, the interface may be configured to reflect some light energy, or photons, back to the first submodule and transmit additional photons of light to a second submodule (e.g., the back cell or bottom submodule). In most tandem devices, it is beneficial to minimize the reflection of light that has passed through one submodule back to another submodule. This is where optical coupling of the first and second submodules by an interface can have a substantial effect on the performance of the tandem photovoltaic device. Additionally, in photovoltaic devices with multiple stacked submodules, additional interfaces may be provided between each submodule. Tandem photovoltaic devices may also include bifacial devices configured to receive incident radiation through both the front and back surfaces. A bifacial tandem device may be configured to receive direct solar radiation on a top or front surface and receive radiation reflected from an external surface, including a portion of the light, such as visible and / or infrared light, on a back or rear surface. In such cases, the interface may affect the reflection of light passing from the first sub-module to the second sub-module, or vice versa.
[0028]
[0040] The backside of a typical thin-film solar cell absorber film stack is relatively rough due to the granular structure of such absorbers. The roughness may range from approximately 175 nm to 200 nm or more root-mean-square (RMS) average depending on the absorber grain size and deposition parameters. As described herein, roughness may be determined using a laser confocal scanning microscope (LCSM). Nanometer-level data may be collected by the LCSM and provided as RMS (Rq) or arithmetic mean (Ra). An exemplary LCSM system is a laser scanning microscope VK-X1000 by Keyence Corporation of America, Itasca, Illinois, USA.
[0029]
[0041] Applicants have discovered that this roughness can lead to an increase in the optical reflectance of light exiting the absorber. This is because the refractive index of materials used in thin film devices (e.g., absorber, back contact thin film) may be greater than the refractive index of a typical conductive layer, such as a transparent conductive oxide, or greater than the refractive index of one or more polymer encapsulants or a typical medium outside the cell, such as air. When such high-low refractive index steps are present, total internal reflection of light is possible at certain light incidence angles. The higher the surface roughness, the greater the local incidence angle of light at the rough surface, resulting in greater surface reflection, as shown in Figures 1A and 1B. Applicants have further discovered that the roughness of the absorber can affect the roughness of subsequently applied layers. For example, the refractive index of an absorber comprising CdTe may be substantially matched to the back contact comprising ZnTe. Thus, the interface between the absorber and the back contact may exhibit little reflection. In some embodiments, the conductive layer may be formed from a transparent material, such as, for example, a conformal transparent conductive oxide. It may be difficult to match the refractive index of such a conformal transparent conductive oxide to the back contact and the absorber. Furthermore, it may be difficult to match the refractive index of such conformal transparent conductive oxides with encapsulant materials. Thus, both interfaces of the conductive layer may be susceptible to reflection. The embodiments of the present disclosure may reduce the reflection at one or both interfaces of the conductive layer. For example, reducing the roughness of the absorber layer may reduce the roughness of the subsequently applied layer, reducing the reflection.
[0030]
[0042] A smooth (e.g., substantially zero roughness) tandem top cell absorber may be transparent to sunlight with energies below the band gap energy of the absorber. The light passing through may accordingly reach the bottom cell of the tandem photovoltaic device. However, light of these energies may be partially reflected by the rough top cell back surface, preventing it from reaching the bottom cell. The reflected light is then not absorbed by the top cell absorber and converted to electrical energy, reducing the performance of the entire tandem photovoltaic device. Thus, the rough surface of the absorber layer of a thin-film solar cell creates conditions that increase light reflection and reduce the transparency of the tandem top cell, which in turn reduces the performance of the tandem bottom cell.
[0031]
[0043] To overcome such roughness-related problems and improve optical coupling between cells or submodules of a tandem photovoltaic device, the present technology provides a present interface. The interface can reduce or minimize reflection by changing the structure between the respective submodules. The structural changes through the interface may include the addition of specific layers or coatings to maximize optical coupling of the submodules on either side of the interface as well as the removal and / or modification of surface structures. Without wishing to be bound by theory, the combination of layers of materials with controlled roughness in the described ranges may be beneficial to provide sufficient roughness to promote adhesion of adjacent layers and facilitate reflection or redirection of shorter wavelength light (e.g., λ≈400-800 nm) back into the first submodule for absorption while providing a surface roughness level low enough to promote transmission of longer wavelength light (e.g., λ≈800-1200 nm) through the interface, through any intervening layers, and into the second submodule.
[0032]
[0044] In certain embodiments, the interface includes a location where the thin film tandem top cell is polished to reduce the reflectivity of the absorber back surface and improve the performance of the tandem bottom cell. The tandem thin film top cell may be polished after deposition of one of the absorber stack layers. For example, polishing may be performed after CdTe deposition and before transparent back contact deposition. Similarly, other thin film semiconductor materials (e.g., II-VI materials, I-III-VI materials, and perovskites) may be polished before transparent back contact deposition. Polishing can reduce reflection at the back interface of the top cell and improve optical coupling between the tandem top and bottom cells, which can improve tandem cell efficiency. In other words, polishing the interface between the absorber and the back contact can improve the interface of the conductive layers. Polishing the back surface of the absorber layer may include mechanical polishing techniques, chemical polishing techniques, and combinations of mechanical and chemical polishing techniques. For example, mechanical polishing may be performed by vibrating a polishing pad that contacts the back surface of the absorber layer. Pressure can be applied to the polishing pad to remove material and reduce roughness. A slurry may be used during vibration. Optionally, the slurry may be chemically reactive with the surface. Inputs such as pad type, slurry composition, pressure, travel speed, rotation speed, etc. may be controlled to achieve the desired roughness. Chemical polishing may be performed by applying a chemical solution to the backside of the absorber layer. Material may be etched away to reduce the roughness. Inputs such as solvent, reagent, solubility, concentration, time, temperature, activation time, etc. may be controlled to achieve the desired roughness.
[0033]
[0045] In certain embodiments, the interface includes an optically transparent, planarizing, index-matched coating deposited on the back surface of the tandem thin-film top solar cell, which can reduce the reflectivity of the interface of the top cell back conductive layer and thus improve the performance of the tandem bottom cell. The coating may include an optical coating deposited on the surface of the top cell stack, which may be selected and configured to exhibit a particular effect. For example, the coating may planarize the top cell stack back surface such that surface roughness is reduced. The coating may have a refractive index substantially similar to that of the final top cell layer, such as the conductive layer. The coating may also be transparent at energies less than the band gap of the top cell absorber. Such a coating can reduce reflection at the top cell back surface, thereby improving the optical coupling between the tandem top and bottom cells and increasing the efficiency of the tandem photovoltaic device.
[0034]
[0046] In certain embodiments, the coating used at the interface may include a coating material based on titanium dioxide. In some embodiments, the transparent coating layer may consist essentially of titanium dioxide. The coating material may include titanium dioxide mixed with a solvent during application, may be highly transparent, and may have a refractive index ranging from about 1.7 to about 2.3 depending on the manufacturing process. In some embodiments, the transparent coating layer may have a single refractive index. In alternative embodiments, the coating material may have a gradient refractive index that varies from about 2.3 to about 1.7. Thus, the refractive index may be graded to transition from the conductive layer to the encapsulant material. Such a refractive index may be substantially matched to the refractive index of a typical thin film absorber layer. Surface planarization may be achieved by optimizing the coating thickness and the coating deposition process. In some embodiments, the interface coating layer, or transparent layer, has a thickness of greater than 50 nm, greater than 100 nm, greater than 150 nm, greater than 200 nm, greater than 250 nm, greater than 300 nm, greater than 400 nm, greater than 500 nm, or greater than 600 nm. In some embodiments, the transparent layer has a thickness of less than 2000 nm, less than 1800 nm, less than 1500 nm, less than 1250 nm, less than 1100 nm, less than 1000 nm, less than 900 nm, or less than 800 nm. Examples of coating deposition processes include wet coating methods, such as spray coating, roll coating, slot die coating, or spin coating. After application of the coating material, a drying and / or curing step may be performed. In this way, the coating can directly contact the back surface of the top cell transparent conductor layer and engage with any roughness or surface micro / nanostructures, and when dried / cured, effectively provide a flat or smooth new back surface. A gradient refractive index coating may be applied as multiple coating layers, with each layer having a different refractive index.The substantially identical refractive index between the transparent conductor layer and the coating provides an optimized transition of light through this new matched "bilayer" and out the new backside without the reflections previously exhibited solely by the roughness of the backside of the transparent conductor layer, thus reducing reflections at the interface between the top cell stack and the medium outside the cell, such as one or more polymer encapsulants or air.
[0035]
[0047] Thus, the present technology provides various methods of constructing a tandem photovoltaic module including a first submodule, a second submodule, and an interface between the first submodule and the second submodule. The interface can transmit a portion of the light. The interface can optically couple the first submodule and the second submodule, thereby reducing reflection of a portion of the light. The interface can be configured to optically couple the first submodule to the second submodule and transmit at least 60% of the light having a wavelength of about 800 nm to about 1200 nm therein. For example, light that has passed through the first submodule may reach the interface, and the interface reduces reflection of the light, allowing at least 60% of the light (λ≈800-1200 nm) to enter the second submodule. In some embodiments, the interface can be configured to optically couple the first submodule to the second submodule and transmit at least 90% of the light having a wavelength of about 800 nm to about 1200 nm therein.
[0036]
[0048] In certain embodiments, the interface may include the following aspects: The interface may include a first layer of the first submodule interface. The first layer may have a first surface having a root mean square average roughness less than 170 nanometers. For example, the first surface having a root mean square average roughness less than 170 nanometers may be the result of polishing the first surface, including using mechanical and / or chemical polishing techniques. The interface may include a second layer of the first submodule interface, the second layer may contact the first surface of the first layer. The second layer may be positioned between the first layer and the second submodule. The first layer and the second layer may have a refractive index mismatch of at least 0.75. The first layer may include an absorber layer having a II-VI semiconductor, a I-III-VI semiconductor, or a perovskite. The first layer may further include a back contact layer. The second layer may include a transparent layer. The second layer may also include a conductive layer, which may be transparent.
[0037]
[0049] In certain embodiments, the interface may include the following aspects: The interface may include a first layer of a first submodule, the first layer may be adjacent to a second submodule. The first layer may have a first surface having a root mean square average roughness of about 50 nanometers to about 200 nanometers, e.g., about 175 nanometers to about 200 nanometers. The interface may include a second layer of the first submodule, the second layer may contact the first surface of the first layer. The second layer may be between the first layer and the second submodule. The first layer and the second layer may have a refractive index mismatch of less than 0.2. The second layer may include a first surface and a second surface, the first surface of the second layer may contact the first surface of the first layer. The second surface of the second layer may have a roughness of less than 170 nanometers. The first layer may include an absorber layer having a thin film semiconductor (e.g., II-VI) and the second layer may include a transparent layer. The transparent layer may include titanium dioxide.
[0038]
[0050] The present technology further provides various methods of making a tandem photovoltaic device. Such methods include where a first sub-module and a second sub-module are provided and an interface is formed between the first sub-module and the second sub-module. The interface can pass a portion of light, thereby optically coupling the first sub-module and the second sub-module. The optical coupling of the first sub-module and the second sub-module can include reducing reflection of a portion of the light passing through the interface.
[0039]
[0051] In certain embodiments, the method may include the following aspects: The interface may include a first layer of the first submodule, the first layer may be adjacent to the second submodule, and the first layer may have a first surface. The first surface may be polished to provide a root mean square average roughness of less than 175 nanometers, such as, for example, in one embodiment, less than 160 nanometers, in another embodiment, less than 150 nanometers, in a further embodiment, less than 120 nanometers, or in yet another embodiment, less than 100 nanometers, or in yet a further embodiment, less than 25 nanometers. Polishing the first surface may include one or more mechanical polishing techniques and / or one or more chemical polishing techniques. The interface may include a second layer of the first submodule, the second layer contacting the first surface of the first layer, and the second layer being between the first layer and the second submodule. The first layer and the second layer may have a refractive index mismatch of at least 0.75. The first layer may include an absorber layer having a thin-film semiconductor (e.g., II-VI group), and the second layer may include a transparent layer. The second layer may include a conductive layer. Optionally, the second layer may include a transparent layer, which may include titanium dioxide. For example, a transparent layer may be provided on the second surface of the conductive layer and between the conductive layer and the encapsulant.
[0040]
[0052] In certain embodiments, the method may include the following aspects: The interface may include a first layer of a first submodule, the first layer adjacent to the second submodule, the first layer having a first surface having a root mean square average roughness of about 175 nanometers to about 200 nanometers. A second layer of the first submodule may be formed, the second layer may contact the first surface of the first layer. The second layer may be between the first layer and the second submodule, the first layer and the second layer having a refractive index mismatch of less than 0.2. Forming the second layer of the first module may include applying a coating composition by one of spray coating, roll coating, and spin coating. The applied coating composition may be dried and / or cured. The second layer may include a first surface and a second surface, the first surface of the second layer in contact with the first surface of the first layer, and the second surface of the second layer having a root mean square roughness of less than 25 nanometers. The first layer may include an absorber layer having a II-VI semiconductor, and the second layer may include a transparent layer, and the transparent layer may include titanium dioxide.
[0041]
[0053] In certain embodiments, the tandem photovoltaic device includes a first or top sub-module and a second or bottom sub-module. A plurality of backing layers of the top sub-module create a connection boundary region that provides an interface with the second sub-module. The boundary region of the first sub-module can facilitate the transmission of infrared light. In some embodiments, the boundary region includes a back or second surface of the absorber layer of the top module; a back contact layer; at least one conductive layer or transparent conductive oxide; and a transparent coating layer. An encapsulant intermediate layer may be provided between the boundary region and the second sub-module.
[0042]
[0054] In an exemplary embodiment, the absorber layer and back contact have a refractive index of about 2.8, the conductive layer has a refractive index of about 1.8, and the encapsulant interlayer has a refractive index of about 1.5. In some embodiments, the conductive layer has a refractive index mismatch to the absorber layer in the range of 0.75 to 1.0, and the conductive layer has a lower refractive index than the absorber layer. In some cases, a transparent coating layer is provided on the conductive layer, and the transparent layer and the conductive layer have a refractive index mismatch in the range of 0 to 0.2, and the transparent coating layer has a lower refractive index than the conductive layer. In some cases, the transparent coating layer has a refractive index in the range of 1.7 to 2.3.
[0043]
[0055] In some embodiments, the second surface of the absorber layer has a roughness RMS value in the range of 50 nm to 200 nm. In some embodiments, the interface includes a transparent layer or coating layer, the coating layer including titanium dioxide, provided on the absorber layer and including multiple layers therebetween. In some cases, the coating layer has a thickness in the range of 100 nm to 1000 nm. In some cases, the top or first surface of the coating layer is provided within 600 nm of the back or second surface of the absorber layer. In some cases, the first surface of the coating layer is provided within 200 nm of the second surface of the back contact layer. In some cases, the first surface of the coating layer is provided on the second surface of the absorber layer and including multiple layers therebetween, whereby the first surface of the coating layer is spaced 150 nm to 650 nm from the second surface of the absorber layer. In some cases, the second or back surface of the coating layer has a roughness RMS value in the range of 50 to 170 nm.
[0044]
[0056] In an exemplary embodiment, the interface includes: a second surface of the absorber layer of the first module, where the absorber is a II-VI semiconductor comprising cadmium and tellurium; a back contact layer on the absorber layer comprising zinc and tellurium; a barrier layer on the back contact layer comprising cadmium tin oxide; a conductive layer on the barrier layer comprising cadmium oxide; a cap layer on the conductive oxide layer comprising cadmium tin oxide; and a planarization and index matching layer or transparent coating layer on the cap layer, where the transparent coating layer comprises titanium dioxide.
[0045]
[0057] The tandem photovoltaic device may be subjected to various finishing processing steps, such as adding further encapsulation layers, bussing, etc., to produce a completed tandem photovoltaic device.
[0058] Aspects of the technology may be applied in various combinations, interdependencies, and multiple dependencies, as illustrated in the examples that follow.
[0046]
[0059] Provided is a first example of a tandem photovoltaic device including: a first sub-module; a second sub-module; an interface between the first sub-module and the second sub-module, the interface passing a portion of light, the interface optically coupling the first sub-module and the second sub-module, and the optically coupling the first sub-module and the second sub-module reducing reflection of the portion of the light.
[0047]
[0060] Provided is a second example of the first example, where the interface includes a first layer of a first sub-module, the first layer adjacent to a second sub-module, the first layer having a first surface, the first surface having a root mean square roughness of less than 170 nanometers. Optionally, the first surface may have a roughness of less than 160 nanometers. Optionally, the first surface may have a roughness of less than 150 nanometers. Optionally, the first surface may have a roughness of less than 120 nanometers. Optionally, the first surface may have a roughness of less than 100 nanometers.
[0048]
[0061] Provided is a third example of the second example, where the interface includes a second layer of the first sub-module, the second layer contacting the first surface of the first layer, and the second layer being between the first layer and the second sub-module.
[0049]
[0062] Provided is a fourth example of the third example, where the first layer and the second layer have a refractive index mismatch of at least 0.75. The first layer may include an absorber layer, a back contact layer, or both. The second layer may include a conductive layer. The conductive layer may include one or more layers of a conformal transparent conductive oxide.
[0050]
[0063] Provided is a fifth example of the third example or the fourth example, where the first layer includes an absorber layer having a II-VI semiconductor and the second layer includes a transparent layer.
[0064] Provided is a sixth example of the fifth example, where the second layer includes a conductive layer.
[0051]
[0065] Provided is a seventh example of the first example, where the interface includes a first layer of the first submodule, the first layer adjacent to the second submodule, the first layer having a first surface, the first surface having a root mean square roughness of less than 170 nanometers; the interface includes a second layer of the first submodule, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second submodule; the first layer and the second layer having a refractive index mismatch of at least 0.75; the first layer includes an absorber layer having a II-VI semiconductor, and the second layer includes a transparent layer; and the second layer includes a conductive layer.
[0052]
[0066] Provided is an eighth example of the first example, where the interface includes: a first layer of the first submodule, the first layer adjacent to the second submodule, the first layer having a first surface, the first surface having a root mean square average roughness of about 50 nanometers to about 200 nanometers; and a second layer of the first submodule, the second layer in contact with the first surface of the first layer, the second layer being between the first layer and the second submodule, the first layer and the second layer having a refractive index mismatch of less than 0.2.
[0053]
[0067] Provided is a ninth example of the eighth example, where the second layer includes a first surface and a second surface, the first surface of the second layer contacts the first surface of the first layer, and the second surface of the second layer has a root mean square average roughness of less than 170 nanometers.
[0054]
[0068] Provided is a tenth example of the eighth example or the ninth example, where the first layer includes an absorber layer having a II-VI semiconductor and the second layer includes a transparent layer.
[0069] Provided is an eleventh example of the tenth example, where the transparent layer comprises titanium dioxide.
[0055]
[0070] Provided is an interface comprising: a first layer of a first submodule, the first layer adjacent to a second submodule, the first layer having a first surface, the first surface having a root mean square roughness of about 175 nanometers to about 200 nanometers; a second layer of the first submodule, the second layer in contact with the first surface of the first layer, the second layer being between the first layer and the second submodule; A twelfth example of the first example, wherein the first layer and the second layer have a refractive index mismatch of less than 0.2, the second layer comprises a first surface and a second surface, the first surface of the second layer contacts the first surface of the first layer, and the second surface of the second layer has a root mean square roughness of less than 25 nanometers, the first layer comprises an absorber layer having a II-VI semiconductor, and the second layer comprises a transparent layer, the transparent layer comprises titanium dioxide.
[0056]
[0071] Provided is a thirteenth example of one of the first through twelfth examples, in which the interface is configured to transmit at least 60% of light having a wavelength between about 800 nm and about 1200 nm that passes through it.
[0057]
[0072] Provided is a fourteenth example of a method for making a tandem photovoltaic device, comprising: providing a first submodule and a second submodule; and forming an interface between the first submodule and the second submodule, wherein the interface passes a portion of light, wherein the interface optically couples the first submodule and the second submodule, and wherein optically coupling the first submodule and the second submodule comprises reducing reflection of the portion of the light.
[0058]
[0073] Provided is a fifteenth example of the fourteenth example, wherein the interface includes a first layer of a first submodule, the first layer adjacent to a second submodule, the first layer having a first surface; and forming an interface between the first submodule and the second submodule includes polishing the first surface to provide a root mean square average roughness of less than 170 nanometers.
[0059]
[0074] Provided is a sixteenth example of the fifteenth example, wherein polishing the first surface to result in a root mean square average roughness of less than 170 nanometers includes a member selected from the group consisting of mechanically polishing the first surface, chemically polishing the first surface, and combinations thereof.
[0060]
[0075] Provided is a seventeenth example of the sixteenth example, where the interface includes a second layer of the first submodule, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second submodule, the first layer and the second layer having a refractive index mismatch of at least 0.75, the first layer including an absorber layer having a II-VI semiconductor, the second layer including a transparent layer, and the second layer including a conductive layer.
[0061]
[0076] Provided is an 18th example of the 14th example, wherein the interface includes: a first layer of a first submodule, the first layer adjacent to the second submodule, the first layer having a first surface, the first surface having a root mean square average roughness of about 175 nanometers to about 200 nanometers; and the step of forming an interface between the first submodule and the second submodule includes forming a second layer of the first submodule, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second submodule, and the first layer and the second layer having a refractive index mismatch of less than 0.2.
[0062]
[0077] Provided is a 19th example of the 18th example, where forming the second layer of the first module includes applying the coating composition by one of spray coating, roll coating, slot die coating, and spin coating.
[0063]
[0078] Provided is a twentieth example of the nineteenth example, wherein the second layer comprises a first surface and a second surface, the first surface of the second layer contacts the first surface of the first layer, and the second surface of the second layer has a root mean square roughness of less than 170 nanometers; the first layer comprises an absorber layer having a II-VI semiconductor, and the second layer comprises a transparent layer; and the transparent layer comprises titanium dioxide. EXAMPLES
[0064]
[0079] Exemplary embodiments of the present technology are provided with reference to the figures enclosed herein.
[0080] 2 and 7, an embodiment of a tandem photovoltaic device 300 is shown. The tandem photovoltaic device 300 may be configured to receive light and convert the light into electrical energy as photons are absorbed from the light and converted into electrical current via the photovoltaic effect. For purposes of discussion and clarity, the tandem photovoltaic device 300 may define a front side 302 configured to face a primary light source, such as, for example, the sun. Additionally, the tandem photovoltaic device 300 may also define a back side 304 that is offset from the front side 302, such as by a functional layer of a plurality of materials.
[0065]
[0081] The tandem photovoltaic device 300 may have a first submodule 100, a second submodule 500, and an interface 400 therebetween. The first submodule 100 may also be referred to as a top cell or upper submodule. The second submodule 500 may also be referred to as a bottom cell or lower submodule. The interface 400 may include one or more treatments, treated portions, and / or one or more portions of the first submodule 100 and / or the second submodule 500, as well as a separate treatment, treated portion, and / or structure intervening between the first submodule 100 and the second submodule 500. In particular, the interface 400 allows a portion of light to pass from one of the first submodule 100 and the second submodule 500 to the other of the first submodule 100 and the second submodule 500. Thus, the interface 400 optically couples the first sub-module 100 and the second sub-module 500 and reduces reflection of light through the interface 400. Each of the first sub-module 100, the second sub-module 500, and the interface 400 may include multiple layers. Each of the first and second sub-modules 100, 500 of the tandem photovoltaic device 300 may include one or more absorber layers for converting light into charge carriers and conductive layers for collecting the charge carriers.
[0066]
[0082] The first sub-module 100 may have a first surface 102 that substantially faces the front side 302 of the tandem photovoltaic device 300, and a second surface 104 that substantially faces the back side 304 of the photovoltaic device 300. The interface 400 may have a first surface 402 that substantially faces the front side 302 of the photovoltaic device 300, and a second surface 404 that substantially faces the back side 304 of the photovoltaic device 300. The second sub-module 500 may have a first surface 502 that substantially faces the front side 302 of the photovoltaic device 300, and a second surface 504 that substantially faces the back side 304 of the photovoltaic device 300.
[0067]
[0083] As depicted in FIG. 2 , incident light (hv) 10 may enter the front side 302 of the tandem photovoltaic device 300 through the first submodule 100, a first portion 11 of the light energy may be absorbed by the first submodule 100, and a remaining portion 12 of the light energy may pass from the first submodule 100 to the interface 400. At the interface 400, the reflected light 13 may be directed back towards the absorbing region of the first submodule 100, and the transmitted light 14 may pass to the second submodule 500. However, the interface 400 is specifically configured to provide optical coupling of the first and second submodules 100, 500, thereby reducing the portion of the reflected light 13 that is directed back towards the first submodule 100. The interface 400 may reduce the portion of the reflected light 13 compared to a substantially identical arrangement of the first submodule 100 and the second submodule 500 between which the interface 400 is not positioned.
[0068]
[0084] Optionally, in a bi-lateral tandem device, backside light energy 16 may enter the backside 304 of the tandem photovoltaic device 300 toward the second sub-module 500. In many implementations, the backside light energy 16 may include externally reflected light and near infrared light. The first sub-module may absorb a first portion of light energy 11, which may include an absorbed combination of incident light 10 and reflected light 13 that was not minimized by the interface 400. The second sub-module may absorb a second portion of light energy 15, which includes transmitted light 14 and, optionally, backside light energy 16. The interface 400 effectively increases the amount of the second portion of light energy 15 absorbed in the second sub-module 500 by reducing the portion of reflected light 13.
[0069]
[0085] 3 and 4, an exemplary embodiment of a first submodule 100 of a tandem photovoltaic device 300 is shown. The first submodule 100 may include multiple layers disposed between a front side 102 and a back side 104. In some embodiments, the layers of the first submodule 100 may be divided into an array of photovoltaic cells 200. For example, the first submodule 100 may be scribed according to a plurality of series scribes 202 and a plurality of parallel scribes 204. The series scribes 202 may extend along the length Y of the first submodule 100 and partition the photovoltaic cells 200 along the length Y of the first submodule 100. Adjacent cells 200 of the photovoltaic cells may be connected in series along the width X of the first submodule 100. In other words, a monolithic interconnection of adjacent cells 200 may be formed, for example, adjacent to the series scribes 202. The parallel scribes 204 may extend along the width X of the first submodule 100 and section the photovoltaic cells 200 along the width X of the first submodule 100. In operation, current 205 may flow along the width X primarily through the photovoltaic cells 200 connected in series by the series scribes 202. In operation, the parallel scribes 204 may limit the ability of the current 205 to flow along the length Y. The parallel scribes 204 are optional and may be configured to separate the series connected photovoltaic cells 200 into groups 206 arranged along the length Y.
[0070]
[0086] 3, the parallel scribes 204 may electrically isolate groups 206 of photovoltaic cells 200 that are connected in series. In some embodiments, the groups 206 of photovoltaic cells 200 may be connected in parallel, for example, via an electrical bus connection. Optionally, the number of parallel scribes 204 may be configured to limit the maximum current generated by each group 206 of photovoltaic cells 200. In some embodiments, the maximum current generated by each group 206 may be about 200 milliamps (mA) or less, such as, for example, about 100 mA or less in one embodiment, about 75 mA or less in another embodiment, or about 50 mA or less in further embodiments.
[0071]
[0087] With particular reference to FIG. 4, the layers of the first sub-module 100 may include a thin film stack provided on a substrate 110. The substrate 110 may be configured to facilitate transmission of light into the first sub-module 100. The substrate 110 may be disposed on a front side 102 of the first sub-module 100. With reference collectively to FIGS. 3 and 4, the substrate 110 may have a first surface 112 that substantially faces the front side 102 of the first sub-module 100 and a second surface 114 that substantially faces the back side 104 of the first sub-module 100. One or more layers of material may be disposed between the first surface 112 and the second surface 114 of the substrate 110.
[0072]
[0088] 5, the substrate 110 may include a transparent layer 120 having a first surface 122 substantially facing the front side 102 of the first submodule 100 and a second surface 124 substantially facing the back side 104 of the first submodule 100. In some embodiments, the second surface 124 of the transparent layer 120 may form the second surface 114 of the substrate 110. The transparent layer 120 may be formed from a substantially transparent material, such as, for example, glass. Suitable glasses may include soda-lime glass or any glass with reduced iron content. The transparent layer 120 may have any suitable transmittance range, in some embodiments, including from about 250 nm to about 1,300 nm. The transparent layer 120 may also have any suitable transmittance percentage, including, for example, greater than about 50% in one embodiment, greater than about 60% in another embodiment, greater than about 70% in yet another embodiment, greater than about 80% in a further embodiment, or greater than about 85% in yet a further embodiment. In one embodiment, the transparent layer 120 may be formed from glass having a transmittance of about 90% or greater. Optionally, the substrate 110 may include a coating 126 applied to the first surface 122 of the transparent layer 120. The coating 126 may be configured to interact with light or improve the durability of the substrate 110, such as, but not limited to, an anti-reflective coating, an anti-soiling coating, or a combination thereof.
[0073]
[0089] 4 , the first sub-module 100 may include a barrier layer 130 configured to mitigate diffusion of contaminants (e.g., sodium) from the substrate 110 that may result in degradation or delamination of other layers of the photovoltaic stack. The barrier layer 130 may have a first surface 132 that substantially faces the front side 102 of the first sub-module 100 and a second surface 134 that substantially faces the back side 104 of the first sub-module 100. In some embodiments, the barrier layer 130 may be provided adjacent to the substrate 110. For example, the first surface 132 of the barrier layer 130 may be provided on the second surface 114 of the substrate 110.
[0074]
[0090] In general, the barrier layer 130 may be substantially transparent, thermally stable, have a low number of pinholes, have a high sodium blocking capability, and have good adhesion properties. Alternatively or additionally, the barrier layer 130 may be configured to apply color suppression to light. The barrier layer 130 may include one or more layers of suitable materials including, but not limited to, tin oxide, silicon dioxide, aluminum doped silicon oxide, silicon oxide, silicon nitride, or aluminum oxide. The barrier layer 130 may have any suitable thickness bounded by the first surface 132 and the second surface 134, including, for example, greater than about 10 nanometers in one embodiment, greater than about 15 nm in another embodiment, or less than about 20 nm in a further embodiment.
[0075]
[0091] With continued reference to FIG. 4, the first sub-module 100 may include a transparent conductive oxide (TCO) layer 140 configured to provide an electrical contact for transporting charge carriers generated by the first sub-module 100. The TCO layer 140 may have a first surface 142 that faces substantially the front side 102 of the first sub-module 100 and a second surface 144 that faces substantially the back side 104 of the first sub-module 100. In some embodiments, the TCO layer 140 may be provided adjacent to the barrier layer 130. For example, the first surface 142 of the TCO layer 140 may be provided on the second surface 134 of the barrier layer 130. In general, the TCO layer 140 may be formed from one or more layers of a substantially transparent, wide bandgap n-type semiconductor material. In particular, the wide bandgap may have a large energy value compared to the energy of the photons of light, thereby mitigating undesired absorption of light. The TCO layer 140 may include one or more layers of suitable materials, including, but not limited to, tin dioxide, doped tin dioxide (e.g., F-SnO2), indium tin oxide, or cadmium tin oxide (Cd2SnO4). In embodiments in which the TCO layer 140 includes cadmium stannate, the cadmium stannate may be provided in a crystalline form. For example, the cadmium stannate may be deposited as a film and then subjected to an annealing process that converts the thin film into a crystallized film.
[0076]
[0092] The first sub-module 100 may include a buffer layer 150 configured to provide an insulating layer between the TCO layer 140 and any adjacent semiconductor layers. The buffer layer 150 may have a first surface 152 that faces substantially the front side 102 of the first sub-module 100 and a second surface 154 that faces substantially the back side 104 of the first sub-module 100. In some embodiments, the buffer layer 150 may be provided adjacent to the TCO layer 140. For example, the first surface 152 of the buffer layer 150 may be provided on the second surface 144 of the TCO layer 140. The buffer layer 150 may be formed of any suitable material, including, but not limited to, intrinsic tin dioxide, zinc magnesium oxide (e.g., Zn 1-x Mgx The buffer layer 150 may comprise a material having a higher resistivity than the TCO layer 140, including silicon dioxide (SiO), silicon oxide (SiO), aluminum oxide (Al2O3), aluminum nitride (AlN), zinc tin oxide, zinc oxide, silicon tin oxide, or any combination thereof. In some embodiments, the material of the buffer layer 150 may be configured to substantially match the band gap of an adjacent semiconductor layer (e.g., absorber). The buffer layer 150 may have a suitable thickness between the first surface 152 and the second surface 154, including, for example, greater than about 10 nm in one embodiment, between about 10 nm and about 80 nm in another embodiment, or between about 15 nm and about 60 nm in further embodiments.
[0077]
[0093] With further reference to FIG. 4, the first submodule 100 may include an absorber layer 160 configured to cooperate with another layer to form a pn junction within the first submodule 100. Thus, absorbed photons of light can release electron-hole pairs and generate carrier flow, thereby resulting in electrical energy. The absorber layer 160 may have a first surface 162 that substantially faces the front side 102 of the first submodule 100, and a second surface 164 that substantially faces the back side 104 of the first submodule 100. A thickness of the absorber layer 160 may be defined between the first surface 162 and the second surface 164. The thickness of the absorber layer 160 may be, for example, from about 0.5 μm to about 10 μm, such as from about 1 μm to about 7 μm in one embodiment, or from about 1.5 μm to about 4 μm in another embodiment.
[0078]
[0094] The absorber layer 160 may be formed from a p-type semiconductor material that has an excess of positive charge carriers, i.e., holes or acceptors. The absorber layer 160 may include suitable p-type semiconductor materials, such as II-VI semiconductors, e.g., cadmium and tellurium. Further examples of II-VI absorber materials include, but are not limited to, semiconductor materials that include cadmium, zinc, tellurium, selenium, or any combination thereof. In some embodiments, the absorber layer 160 may include a ternary system of cadmium, selenium, and tellurium (e.g., CdSe x Te 1-x ), or a compound including cadmium, selenium, tellurium, and one or more additional elements (e.g., CdZnSeTe). The absorber layer 160 may further include one or more dopants. The first submodule 100 provided herein may include multiple absorber materials. In alternative embodiments, the absorber layer 160 may be formed from a I-III-VI semiconductor, or a perovskite semiconductor material.
[0079]
[0095] In embodiments in which the absorber layer 160 includes tellurium and cadmium, the average atomic percentage of tellurium in the absorber layer 160 may be greater than about 25 atomic percent and less than about 50 atomic percent, such as, for example, greater than about 30 atomic percent and less than about 50 atomic percent in one embodiment, greater than about 40 atomic percent and less than about 50 atomic percent in a further embodiment, or greater than about 47 atomic percent and less than about 50 atomic percent in yet another embodiment. Alternatively or additionally, the average atomic percentage of tellurium in the absorber layer 160 may be greater than about 45 atomic percent, such as, for example, greater than about 49 atomic percent in one embodiment. It should be noted that the average atomic percentages described herein represent the entirety of the absorber layer 160, and that the atomic percentage of material at a particular location within the absorber layer 160 may be graded through the thickness as compared to the overall composition of the absorber layer 160. For example, the absorber layer 160 may have a graded composition.
[0080]
[0096] In embodiments in which absorber layer 160 includes selenium and tellurium, the average atomic percent of selenium in absorber layer 160 may be greater than 0 atomic percent and less than or equal to about 25 atomic percent, such as, for example, greater than about 1 atomic percent and less than about 20 atomic percent in one embodiment, greater than about 1 atomic percent and less than about 15 atomic percent in another embodiment, or greater than about 1 atomic percent and less than about 8 atomic percent in a further embodiment. Note that the concentration of tellurium, selenium, or both may be graded through the thickness of absorber layer 160. For example, if absorber layer 160 includes a compound including a mole fraction of selenium of x and a mole fraction of tellurium of 1-x (Se x Te 1-x ), x may vary within the absorber layer 160 with distance from the first surface 162 of the absorber layer 160.
[0081]
[0097] 4, the absorber layer 160 may be doped with a dopant configured to manipulate the charge carrier concentration. In some embodiments, the absorber layer 160 may be doped with a Group VA (Group 15) dopant, such as, for example, arsenic, phosphorus, antimony, or a combination thereof. Alternatively or additionally, the absorber layer 160 may be doped with a Group IB (Group 11) dopant, such as, for example, copper, silver, gold, or a combination thereof. The total density of dopants in the absorber layer 160 may be controlled. Additionally, the amount of dopant may vary with distance from the first surface 162 of the absorber layer 160.
[0082]
[0098] FIG. 4 shows an exemplary layer structure, and the composition has been described with an example including II-VI materials. In other embodiments, the first submodule 100 of the tandem photovoltaic device 300 can use other photovoltaic materials with alternative layer structures to produce a photovoltaic submodule. In one example, the first submodule 100 may include a I-III-VI absorber material, such as, for example, copper indium gallium sulfide / selenide (CIGS), CuInSe2 (CIS), or GaAs, and may be provided as a thin film. In another example, the first submodule 100 may include a perovskite absorber. In a further example, the first submodule 100 may include a silicon absorber, which may include amorphous, polycrystalline, crystalline, or thin film silicon.
[0083]
[0099] According to embodiments provided herein, a p-n junction may be formed by providing an absorber layer 160 in sufficient proximity to a portion of the first submodule 100 that has an excess of negative charge carriers; e.g., electrons or donors. In some embodiments, the absorber layer 160 may be provided adjacent to an n-type semiconductor material. Alternatively, one or more intervening layers may be provided between the absorber layer 160 and the n-type semiconductor material. In some embodiments, the absorber layer 160 may be provided adjacent to the buffer layer 150. For example, the first surface 162 of the absorber layer 160 may be provided on the second surface 154 of the buffer layer 150.
[0084]
[0100] The first submodule 100 may include a back contact layer 170 configured to mitigate undesired alterations of the dopant and to provide electrical contact to the absorber layer 160. The back contact layer 170 may have a first surface 172 that substantially faces the front side 102 of the first submodule 100 and a second surface 174 that substantially faces the back side 104 of the first submodule 100. A thickness of the back contact layer 170 may be defined between the first surface 172 and the second surface 174. The thickness of the back contact layer 170 may be from about 5 nm to about 200 nm, such as from about 10 nm to about 50 nm in one embodiment.
[0085]
[0101] In some embodiments, the back contact layer 170 may be provided adjacent to the absorber layer 160. For example, the first surface 172 of the back contact layer 170 may be provided on the second surface 164 of the absorber layer 160. In some embodiments, the back contact layer 170 may include a combination of materials from groups I, II, VI, such as, for example, one or more layers including zinc and tellurium in various compositions. Further suitable materials include, but are not limited to, bilayers of cadmium zinc telluride and zinc telluride, or zinc telluride doped with a group V (group 15) dopant, such as nitrogen. The thin film junction 176 may be defined as the thin film stack that primarily contributes to the photovoltaic effect. For example, in some embodiments, the thin film junction 176 may include the transparent conductive oxide layer 140, the buffer layer 150, the absorber layer 160, the back contact layer 170, or a combination thereof.
[0086]
[0102] Referring to FIG. 4, the first submodule 100 may include a conductive layer 180, which may be transparent and configured to provide electrical contact with the back contact layer 170, the absorber layer 160, or both. In some embodiments, the conductive layer 180 may be formed toward the backside of the first submodule 100 relative to the absorber layer 160. When provided in a single junction device or as part of a lower or rear submodule (e.g., the second submodule 500), the conductive layer 180 may be disposed on the backside of the submodule (e.g., the second submodule 500) and may use a turbid opaque metal layer as a component. However, opaque layers may not be suitable for use as the conductive layer 180 of the first submodule 100, which is disposed between the junctions of a multijunction or tandem photovoltaic device. The conductive layer 180 may have a first surface 182 that substantially faces the front side 102 of the first submodule 100, and a second surface 184 that substantially faces the back side 104 of the first submodule 100. In some embodiments, the conductive layer 180 may be provided adjacent to the back contact layer 170 or the absorber layer 160. For example, the first surface 182 of the conductive layer 180 may be provided on the second surface 174 of the back contact layer 170 or the second surface 162 of the absorber layer 160. A thickness of the conductive layer 180 may be defined between the first surface 182 and the second surface 184. The thickness of the conductive layer 180 may be less than about 500 nm, such as, for example, from about 40 nm to about 400 nm, or from about 60 nm to about 350 nm in one embodiment.
[0087]
[0103] Optionally, the first sub-module 100 may have a back layer 199 on the back side 104 of the first sub-module 100. The back surface of the back layer 199 defines the front sub-module back surface 104. In some embodiments, the back layer 199 includes an electron reflector layer.
[0088]
[0104] In alternative embodiments, the back layer 199 may be omitted, i.e., the function of the back layer 199 may be replaced by a region of the conductive layer 180. For example, the conductive layer 180 may operate as a transparent tunnel junction. The tunnel junction may have a p+ subregion and an n+ subregion. In some embodiments, the tunnel junction may have a p++ subregion and an n++ subregion. For example, the conductive layer 180 may have a transparent tunnel junction formed by a three-layer stack of cadmium tin oxide, cadmium oxide, and cadmium tin oxide. Thus, the conductive layer 180 may be formed as a stack of conformal layers of transparent conductive oxides. As mentioned above, such transparent conductive oxides may have a refractive index mismatch of at least 0.75 with the absorber layer 160, the back contact layer 170, or both.
[0089]
[0105] Materials such as semiconductors and transparent conducting oxides may be doped with impurities to alter their electrical and optical properties. Dopants may be incorporated into functional layers to modify the n-type or p-type charge carrier concentration. Charge densities of around 1×10 16 cm -3 If the electron donor carrier is greater than about 1×10, it may be considered to be of the "+" type. The boundary is not strict, but it is 11 cm -3 ~Approx. 1×10 16 cm -3 in the range, the material may be considered n-type, with a donor carrier density of approximately 1×10 16 cm -3 Similarly, if the electron acceptor carriers (i.e., "holes") are greater than about 1×10 11 cm -3 ~Approx. 1×10 16 cm -3 in the range, the material is generally considered p-type, with an acceptor carrier density of approximately 1 × 10 16 cm -3If the carrier concentration is greater than 100 times higher, it is considered p+ type. Regardless of the absolute carrier density, the boundary is not exact and may overlap, since a layer can be p+ for a layer that is p-type (or n+ for a layer that is n-type) if the carrier concentration is at least two orders of magnitude (i.e., 100 times) higher. Furthermore, the boundary is not exact and may overlap, since a layer can be p+ for a layer that is p-type (or n+ for a layer that is n-type) if the carrier concentration is at least two orders of magnitude (i.e., 100 times) higher. 18 cm -3 The greater charge density may be considered to be of the "++" type. Thus, a layer of either n-type or p-type may be "++" relative to a layer of the same type which is itself "+" relative to a third layer if the ++ layer has more than 100 times the carrier density of the same type as the + layer.
[0090]
[0106] 2 and 6, the tandem photovoltaic device 300 includes a second sub-module 500. The second sub-module 500 may be disposed below or below the first sub-module 100, with the front side 302 of the tandem photovoltaic device 300 as the top surface facing the primary light. The photovoltaic device sub-module 500 may include multiple layers disposed between a first surface 502 of the front side of the second sub-module 500 and a second surface of the back side of the second sub-module 500. One or more of the multiple layers may include a photovoltaic absorber material. In some embodiments, the layers of the photovoltaic device sub-module 500 may be divided into multiple photovoltaic cells.
[0091]
[0107] The second sub-module 500 of the tandem photovoltaic device 300 may include one or more absorber materials in a layered structure. In one example, the second sub-module 500 may include a silicon absorber, which may include amorphous, polycrystalline, crystalline, or thin-film silicon. In another example, the second sub-module 500 may include a perovskite absorber material. In a further example, the second sub-module 500 may include a I-III-VI absorber material, such as, for example, copper indium gallium sulfide / selenide (CIGS), CuInSe2 (CIS), or GaAs, and may be provided as a thin film. In another example, the second sub-module 500 may include a II-VI absorber material, such as, for example, CdTe, CdZnTe, or CdSeTe.
[0092]
[0108] The second sub-module 500 may share various aspects with the first sub-module 100. The second sub-module 500 may have a front layer 501 on a front side 502 of the second sub-module 500. The front surface of the front layer 501 may define the front surface 502 of the second sub-module 500. In some embodiments, the front layer 501 is a buffer layer. In some embodiments, the front layer 501 is a conductive layer. In some embodiments, the front layer 501 includes a conductive metal grid. In some embodiments, the front layer 501 includes a transparent conductive oxide. In certain embodiments, the remainder or the entirety of the second sub-module 500 may be configured the same or substantially the same as the first sub-module 100. An embodiment of the second sub-module 500 may include portions that are the same or substantially the same in function and structure as portions of the first sub-module 100.
[0093]
[0109] 2 and 6, the tandem photovoltaic device 300 includes an interface 400 positioned between the first sub-module 100 and the second sub-module 500. However, it is understood that one or more additional interfaces 400 may be positioned between additional sub-modules of the tandem photovoltaic device 300 (e.g., the second sub-module and a third sub-module, the third sub-module and a fourth sub-module, etc.). It is further understood that the interface 400 may include portions of the first sub-module 100 and / or the second sub-module 500, including adjacent layers of the first sub-module 100 and / or the second sub-module 500, as well as layers of the first sub-module 100 and / or the second sub-module 500 that have been subjected to a particular process. Similarly, the interface 400 may include one or more layers or structures interposed between the first sub-module 100 and the second sub-module 500 that are not present in either the first sub-module 100 or the second sub-module 500. Examples include when one or more of the absorber layer 160, the back contact layer 170, the conductive layer 180, and / or the back layer 199 form part of the interface 400, where such layers may be subjected to specific treatments and / or may cooperate with additional layers, coatings and materials to reduce reflected light passing between the first sub-module 100 and the second sub-module 500.
[0094]
[0110] An example of the structure of the interface 400 is shown diagrammatically in the cross-sectional portion of FIG. 7A. The interface 400 includes a first layer 410 of the first submodule 100. The first layer 410 has a first surface 414. In some embodiments, the first surface 414 has a root-mean-square (RMS) roughness of less than 170 nanometers. In this example, the first layer 410 includes the absorber layer 160 of the first submodule 100. Optionally, the absorber layer 160 includes a II-VI semiconductor. Upon formation of the absorber layer 160, the first surface 414 may be initially rough due to the grain structure of such thin-film semiconductor material used for the absorber layer 160. Thus, the initially rough surface may be polished (e.g., mechanically and / or chemically polished) to form the first surface 414 having a root-mean-square roughness of less than 170 nanometers. Specifically, the second surface 164 of the absorber layer 160 may be polished to reduce roughness. As described above, the second surface 164 of the absorber layer 160 may be polished to a roughness that has an RMS average of less than 170 nanometers. Optionally, the second surface 164 of the absorber layer 160 may be polished to a roughness that has an RMS average of less than 160 nanometers. Optionally, the second surface 164 of the absorber layer 160 may be polished to a roughness that has an RMS average of less than 150 nanometers. Optionally, the second surface 164 of the absorber layer 160 may be polished to a roughness that has an RMS average of less than 120 nanometers. Optionally, the second surface 164 of the absorber layer 160 may be polished to a roughness that has an RMS average of less than 100 nanometers. According to embodiments provided herein, the back contact 170 and the conductive layer 180 may be substantially conformal to the absorber layer. Thus, polishing the second surface 164 of the absorber layer 160 can reduce the roughness of the first surface 172 and second surface 174 of the back contact layer 180. Additionally, polishing the second surface 164 of the absorber layer 160 can reduce the roughness of the first surface 182 and second surface 184 of the conductive layer 180.
[0095]
[0111] The example of the interface 400 shown in FIG. 7A includes a second layer 420, which is in contact with the first surface 414 of the first layer 410. The second layer 420 is positioned between the first layer 410 and the second submodule 500. The second layer 420 may include a transparent layer, such as the back contact layer 170 of the first submodule 100. The second layer 420 may also include a conductive layer, such as the conductive layer 180 of the first submodule 100. As a result of polishing the second surface 164 of the absorber layer 160 (e.g., as the first surface 414 of the first layer 410) to now have an RMS of less than 170 nanometers, the first layer 410 and the second layer 420 can have an index mismatch of at least 0.75 so that the polished surface minimizes the amount of reflected light 13 that is directed back toward the first submodule 100.
[0096]
[0112] The roughness of the pre-scribe or scribe-free first surface 414 may be consistent across the entire surface or span of the submodule. Submodules provided herein may have a surface area greater than 1 square meter. The span of the first submodule may be greater than 0.5 m, greater than 0.8 m, 1.0 m or more, 1.2 m or more, less than 2.5 m, in the range of 0.5 m to 2.5 m, or in the range of 1.0 m to 2.0 m. In some embodiments, the roughness of the first surface 414 across the span of the first submodule has an RMS surface roughness value in the range of 15 nm to 250 nm, in the range of 25 nm to 225 nm, in the range of 50 nm to 200 nm, in the range of 150 nm to 200 nm, in the range of 50 nm to 175 nm, in the range of 50 nm to 170 nm, in the range of 50 nm to 160 nm, in the range of 50 nm to 150 nm, in the range of 50 nm to 120 nm, or in the range of 50 nm to 100 nm.
[0097]
[0113] Another example of the interface 400' structure is shown diagrammatically in the cross-sectional portion of FIG. 7B. The interface 400' includes a first layer 410' of a first submodule 100, which is positioned adjacent to a second submodule 500. The first layer 410' has a first surface 414' having a roughness RMS of about 175 nanometers to about 200 nanometers. In this example, the first layer 410' includes an absorber layer 160 of the first submodule 100, which includes a II-VI semiconductor. The formation of the absorber layer 160 may result in a rough first surface 414' due to the grain structure of such material used for the absorber layer 160.
[0098]
[0114] The example of the interface 400' shown in FIG. 7B includes a second layer 420' of the first submodule 100, where the second layer 420' is in direct contact with the first surface 414' of the first layer 410'. The second layer 420' is positioned between the first layer 410' and the second submodule 500. The second layer 420' includes a first surface 422 and a second surface 424, where the first surface 422 of the second layer 420' is in contact with the first surface 414' of the first layer 410'. The second surface 424 of the second layer 420' has a roughness that is less than 170 nanometers RMS. The first layer 410' and the second layer 420' have a refractive index mismatch of less than 0.2. In this manner, the first layer 410' and the second layer 420' of the interface 400' can minimize the amount of reflected light 13 that is directed back toward the first sub-module 100. The second layer 420' can include a transparent layer, which can include titanium dioxide. For example, the second layer 420' can be formed by a coating composition including titanium dioxide that is coated on the first layer 410'. By drying and / or curing the coating composition, the second surface 424 can be made horizontal and smooth, and the second surface 424 can exhibit an RMS of 25 nm to 200 nm, 50 nm to 170 nm, or less than 25 nanometers.
[0099]
[0115] Interface 400 may have an average transmittance of greater than 20% for light having wavelengths between 800 nm and 1200 nm. Optionally, interface 400 may have an average transmittance of greater than about 25% for light having wavelengths between 800 nm and 1200 nm, such as, for example, greater than about 50% in one embodiment, or greater than about 60% in another embodiment, or greater than about 75% in a further embodiment.
[0100]
[0116] 8, one embodiment of a method of making a tandem photovoltaic device 300 is shown at 800. A first step at 805 may include providing a first sub-module 100 and a second sub-module 500. A second step at 810 may include forming an interface 400 between the first sub-module 100 and the second sub-module 500, the interface 400 including a first layer 410 of the first sub-module 100, the first layer 410 adjacent the second sub-module 500, the first layer 410 having a first surface 414. The step of forming the interface 400 in 810 may include a third step 815 of polishing the first surface to provide a roughness that is less than 25 nanometers root mean squared, and a fourth step 820 of applying a second layer 420 of the first submodule 100, the second layer 420 contacting the first surface 414 of the first layer 410, the second layer 420 being between the first layer 410 and the second submodule 500. The polishing of the first surface 414 in the third step 815 may include mechanical and / or chemical polishing techniques. In this way, the first layer 410 and the second layer 420 may have a refractive index mismatch of at least 0.75, while the polished first surface 414 minimizes the amount of reflected light 13 that is directed back towards the first submodule 100.
[0101]
[0117] 9, another embodiment of a method of making a tandem photovoltaic device 300 is shown at 900. A first step at 905 may include providing a first sub-module 100 and a second sub-module 500. A second step at 910 may include forming an interface 400' between the first sub-module 100 and the second sub-module 500. The step of forming the interface 400' at 910 may include a third step 915 of providing a first layer 410' of the first sub-module 100, the first layer 410' adjacent the second sub-module 500, the first layer 410' having a first surface 414', the first surface 414' having a root mean square average roughness of about 50 nanometers to about 200 nanometers. The step of forming the interface 400' in 910 may further include a fourth step 920 of forming a second layer 420' of the first submodule 100, the second layer 420' contacting the first surface 414' of the first layer 410', the second layer 420' being between the first layer 410' and the second submodule 500, the first layer 410' and the second layer 420' having a refractive index mismatch of less than 0.2, the second layer 420' may be formed by applying a coating composition by one of spray coating, roll coating, and slot die coating. The second layer 420' may include a transparent layer, and the coating composition used to form such layer may include titanium dioxide. Optionally, the coating composition may be dried to remove one or more solvents and may be heat cured.
[0102]
[0118] In the layer formation step of the exemplary method, the deposition assembly can simultaneously achieve a substantially uniform layer or coating along the width of the substrate. The deposition assemblies provided herein are scalable to coat large substrates, e.g., substrates having dimensions of about 1 m or more in length and / or width, in the range of 0.5-2.0 m in length and width, or up to about 2 m in length and / or width. The width may be measured across a dimension perpendicular to the edge and perpendicular to the direction of transport during the manufacturing process. The deposition assembly may be located above a conveyor to deposit material on the upwardly facing surface of the substrate, layer stack, or partially formed device. The conveyor may be of a roll type including rolls that support the downwardly facing surface of the substrate to transport the substrate during layer formation and processing. Processing may include transporting the substrate through multiple deposition and processing stations to form layers of the layer stack on the substrate. As an example, a transparent coating is applied over previously deposited layers as the substrate moves through the deposition assembly, and the transparent coating is dried and cured as it subsequently passes through the processing stations.
[0103]
[0119] Test Example
[0104] [Table 1]
[0105]
[0120] Table 1 shows a summary of various experimental embodiments according to the present disclosure. The Comparative Example and Examples 1-17 were all prepared from the same stack of materials. Specifically, a glass substrate was coated with a pre-contact material comprising a fluorine-doped tin oxide layer. The pre-contact material was coated with a CdSeTe absorber layer. The absorber layer was coated with a conductive layer from a tri-layer stack of cadmium tin oxide, cadmium oxide, and cadmium tin oxide. Each of the Comparative Example and Examples 1-17 was prepared as similarly as possible, except for the polishing applied to the backside of the absorber layer, i.e., the interface between the absorber layer and the conductive layer. The Comparative Example was not polished. The backside of the absorber layer for each of Examples 1-17 was mechanically polished to various levels of roughness. The RMS (Rq) values were determined using LCSM and are summarized in Table 1. The amount of light at a wavelength of 1,000 nanometers that was transmitted through each stack was determined for the Comparative Example and Examples 1-17. Table 1 summarizes the relative improvement in percentage of light transmitted for Examples 1-17 versus the Comparative Example.
[0106]
[0121] As shown in Table 1, a reduction in the RMS average strongly coincides with an increase in transmission. Specifically, a reduction in roughness to an RMS average of less than 160 nanometers resulted in an improvement in transmission of about 5% (see Examples 6, 11, and 12). A reduction in roughness to an RMS average of less than 120 nanometers resulted in an improvement in transmission of about 15% (see Examples 1 and 4). A reduction in roughness to an RMS average of less than 100 nanometers resulted in an improvement in transmission of about 19% (see Examples 15 and 16).
[0107]
[0122] It should be noted that certain layers were omitted from the stacks tested to facilitate the completion of the experiments. Specifically, the back contact layer was not disposed between the absorber layer and the conductive layer. Testing of the multi-layer back contact shows substantial match between the absorber surface and the compatibility of the back contact surface. In general, the back contact layer (e.g., ZnTe) may be substantially conformal with the absorber layer and may have a substantially similar refractive index as the absorber layer. Thus, the results in Table 1 show an improvement of the device having the back contact layer. It is expected that the performance of the device will remain consistent or may improve with the addition of an encapsulant. Specifically, the conductive layer and the transparent layer may be substantially conformal and may have improved roughness at the interface with the encapsulant. It is believed that most encapsulant materials are not refractive index matched with the conductive layer, resulting in improved transmission compared to the comparative example.
[0108]
[0123] The exemplary embodiments are provided so that the disclosure is thorough and fully conveys its scope to those skilled in the art. Numerous specific details are set forth, such as examples of specific components, devices and methods, to provide a thorough understanding of the embodiments of the present disclosure. It will be apparent to those skilled in the art that specific details need not be utilized, that the exemplary embodiments may be embodied in many different forms, and that none of these should be construed to limit the scope of the present disclosure. In some exemplary embodiments, well-known processes, well-known device structures, and well-known technologies are not described in detail. Equivalent changes, modifications and variations of some embodiments, materials, compositions and methods can be made within the scope of the present technology with substantially similar results.
Claims
1. A first submodule; and A second sub-module on the first sub-module, the first sub-module including an interface between the first sub-module and the second sub-module. Including, the interface transmits a portion of the light; the interface optically couples the first sub-module and the second sub-module; The interface, an absorber layer formed from a thin film semiconductor, the absorber layer having a surface with a root mean square roughness between 50 nanometers and 200 nanometers; and a conductive layer on a surface of said absorber layer, said conductive layer having a refractive index mismatch with said absorber layer of at least 0.75; A tandem photovoltaic device comprising:
2. The tandem photovoltaic device of claim 1 , wherein the thin film semiconductor is a II-VI material, a I-III-VI material, or a perovskite.
3. The tandem photovoltaic device of claim 1 or claim 2, wherein the conductive layer comprises a transparent conductive oxide.
4. The tandem photovoltaic device of claim 3 , wherein the transparent conductive oxide is cadmium tin oxide.
5. The tandem photovoltaic device of claim 3 , wherein the transparent conductive oxide is cadmium oxide.
6. The tandem photovoltaic device of claim 1 , wherein the conductive layer comprises a plurality of layers, the plurality of layers comprising a layer of cadmium tin oxide and a layer of cadmium oxide.
7. The tandem photovoltaic device of any one of claims 1 to 6, wherein the conductive layer comprises a transparent tunnel junction.
8. The tandem photovoltaic device of any one of claims 1 to 7, comprising a back contact layer on a surface of the absorber layer and between the absorber layer and the conductive layer.
9. The tandem photovoltaic device of claim 8 , wherein the back contact layer comprises ZnTe.
10. The tandem photovoltaic device of any one of claims 1 to 9, wherein the absorber layer has a surface roughness root mean square average of less than 170 nanometers.
11. The tandem photovoltaic device of any one of claims 1 to 9, wherein the absorber layer has an average root mean square surface roughness of less than 160 nanometers, less than 150 nanometers, or less than 120 nanometers.
12. The tandem photovoltaic device of any one of claims 1 to 9, wherein the absorber layer has a surface with an average root mean square dimension of less than 100 nanometers.
13. The tandem photovoltaic device of any one of claims 1 to 9, wherein the absorber layer has a surface roughness root mean square average of 175 nanometers to 200 nanometers.
14. The tandem photovoltaic device of any one of claims 1 to 13, comprising a transparent layer on said conductive layer, said transparent layer comprising titanium dioxide.
15. The tandem photovoltaic device of any of claims 1 to 13, comprising a transparent layer on said conductive layer, said transparent layer and said conductive layer having a refractive index mismatch of less than 0.
2.
16. The tandem photovoltaic device of any one of claims 1 to 15, wherein the transparent layer has a refractive index of 1.7 to 2.
3.
17. The tandem photovoltaic device of any one of claims 14 to 16, wherein the transparent layer has a gradient refractive index.
18. The tandem photovoltaic device according to any one of claims 14 to 17, wherein the transparent layer has a thickness in the range of 100 nm to 1000 nm.
19. The tandem photovoltaic device according to any one of claims 14 to 17, wherein the transparent layer has a thickness in the range of 150 nm to 800 nm.
20. A first submodule; and A second sub-module on the first sub-module, the first sub-module including an interface between the first sub-module and the second sub-module. Including, the interface transmits a portion of the light; the interface optically couples the first sub-module and the second sub-module; The interface, an absorber layer formed from a thin film semiconductor, the absorber layer having a surface with a root mean square average roughness of less than 170 nanometers; and a conductive layer on a surface of said absorber layer, said conductive layer having a refractive index mismatch with said absorber layer of at least 0.75; A tandem photovoltaic device comprising:
21. A first sub-module; A second sub-module; 11. A tandem photovoltaic device comprising an interface between the first sub-module and the second sub-module, the interface passing a portion of light, the interface optically coupling the first sub-module and the second sub-module, and optically coupling the first sub-module and the second sub-module comprising reducing reflection of the portion of light.
22. 22. The tandem photovoltaic device of claim 21 , wherein the interface comprises a first layer of the first submodule, the first layer adjacent to the second submodule, the first layer having a first surface, the first surface having a root mean square average roughness of less than 170 nanometers.
23. 23. The tandem photovoltaic device of claim 22, wherein the interface includes a second layer of the first submodule, the second layer contacting the first surface of the first layer, and the second layer being between the first layer and the second submodule.
24. 24. The tandem photovoltaic device of claim 23, wherein the first layer and the second layer have a refractive index mismatch of at least 0.
75.
25. 24. The tandem photovoltaic device of claim 23, wherein the first layer comprises an absorber layer having a II-VI semiconductor and the second layer comprises a transparent layer.
26. The tandem photovoltaic device of claim 25 , wherein the second layer comprises a conductive layer.
27. the interface includes a first layer of the first submodule, the first layer adjacent to the second submodule, the first layer having a first surface, the first surface having a root mean square average roughness of less than 170 nanometers; the interface includes a second layer of the first sub-module, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second sub-module; the first layer and the second layer have a refractive index mismatch of at least 0.75; the first layer comprises an absorber layer having a II-VI semiconductor and the second layer comprises a transparent layer; and The tandem photovoltaic device of claim 21 , wherein the second layer comprises a conductive layer.
28. The interface, a first layer of the first submodule, the first layer adjacent the second submodule, the first layer having a first surface, the first surface having a root mean square average roughness of about 175 nanometers to about 200 nanometers; and a second layer of the first submodule, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second submodule, the first layer and the second layer having a refractive index mismatch of less than 0.2; 22. The tandem photovoltaic device of claim 21 comprising:
29. 30. The tandem photovoltaic device of claim 28, wherein the second layer comprises a first surface and a second surface, the first surface of the second layer in contact with the first surface of the first layer, and the second surface of the second layer has a root-mean-square roughness of less than 170 nanometers.
30. 30. The tandem photovoltaic device of claim 28, wherein the first layer comprises an absorber layer having a II-VI semiconductor and the second layer comprises a transparent layer.
31. The tandem photovoltaic device of claim 30 , wherein the transparent layer comprises titanium dioxide.
32. The interface, a first layer of the first submodule, the first layer adjacent the second submodule, the first layer having a first surface, the first surface having a root mean square roughness of about 175 nanometers to about 200 nanometers; a second layer of the first submodule, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second submodule, the first layer and the second layer having a refractive index mismatch of less than 0.2; Including, the second layer comprises a first surface and a second surface, the first surface of the second layer contacting the first surface of the first layer, and the second surface of the second layer having a root mean square average roughness of less than 170 nanometers; the first layer comprises an absorber layer having a II-VI semiconductor and the second layer comprises a transparent layer; and The tandem photovoltaic device of claim 21 , wherein the transparent layer comprises titanium dioxide.
33. The tandem photovoltaic device of claim 21 , wherein the interface is configured to transmit at least 60% of the light having a wavelength between about 800 nm and about 1200 nm that passes therethrough.
34. 1. A method of making a tandem photovoltaic device, comprising: providing a first sub-module and a second sub-module; and forming an interface between the first sub-module and the second sub-module, the interface passing a portion of light, the interface optically coupling the first sub-module and the second sub-module, and optically coupling the first sub-module and the second sub-module includes reducing reflection of the portion of light. A method comprising:
35. the interface includes a first layer of the first submodule, the first layer adjacent to the second submodule, the first layer having a first surface; and 35. The method of claim 34, wherein forming the interface between the first sub-module and the second sub-module comprises polishing the first surface to provide a root mean square roughness of less than 170 nanometers.
36. 36. The method of claim 35, wherein polishing the first surface to provide a root mean square average roughness of less than 170 nanometers comprises a member selected from the group consisting of mechanically polishing the first surface, chemically polishing the first surface, and combinations thereof.
37. the interface includes a second layer of the first sub-module, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second sub-module; the first layer and the second layer have a refractive index mismatch of at least 0.75; the first layer comprises an absorber layer having a II-VI semiconductor and the second layer comprises a transparent layer; and 37. The method of claim 36, wherein the second layer comprises a conductive layer.
38. The interface, a first layer of the first submodule, the first layer adjacent the second submodule, the first layer having a first surface, the first surface having a root mean square roughness of about 175 nanometers to about 200 nanometers; 35. The method of claim 34, wherein forming the interface between the first sub-module and the second sub-module comprises forming a second layer of the first sub-module, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second sub-module, and the first layer and the second layer having a refractive index mismatch of less than 0.
2.
39. 40. The method of claim 38, wherein forming the second layer of the first module comprises applying a coating composition by one of spray coating, roll coating, and spin coating.
40. the second layer comprises a first surface and a second surface, the first surface of the second layer contacting the first surface of the first layer, and the second surface of the second layer having a root mean square average roughness of less than 170 nanometers; the first layer comprises an absorber layer having a II-VI semiconductor and the second layer comprises a transparent layer; and 40. The method of claim 39, wherein the transparent layer comprises titanium dioxide.
41. A first sub-module; A second sub-module; 11. A tandem photovoltaic device comprising an interface between the first sub-module and the second sub-module, the interface passing a portion of light, the interface optically coupling the first sub-module and the second sub-module, and optically coupling the first sub-module and the second sub-module comprising reducing reflection of the portion of light.
42. 42. The tandem photovoltaic device of claim 41 , wherein the interface comprises a first layer of the first submodule, the first layer adjacent to the second submodule, the first layer having a first surface, the first surface having a root mean square roughness of less than 170 nanometers.
43. 43. The tandem photovoltaic device of claim 42, wherein the interface includes a second layer of the first submodule, the second layer contacting the first surface of the first layer, and the second layer being between the first layer and the second submodule.
44. 44. The tandem photovoltaic device of claim 43, wherein the first layer and the second layer have a refractive index mismatch of at least 0.
75.
45. The tandem photovoltaic device of claim 43 or claim 44, wherein the first layer comprises an absorber layer having a II-VI semiconductor and the second layer comprises a transparent layer.
46. 46. The tandem photovoltaic device of claim 45, wherein the second layer comprises a conductive layer.
47. the interface includes a first layer of the first submodule, the first layer adjacent to the second submodule, the first layer having a first surface, the first surface having a root mean square average roughness of less than 170 nanometers; the interface includes a second layer of the first sub-module, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second sub-module; the first layer and the second layer have a refractive index mismatch of at least 0.75; the first layer comprises an absorber layer having a II-VI semiconductor and the second layer comprises a transparent layer; and 42. The tandem photovoltaic device of claim 41 , wherein the second layer comprises a conductive layer.
48. The interface, a first layer of the first submodule, the first layer adjacent the second submodule, the first layer having a first surface, the first surface having a root mean square average roughness of about 175 nanometers to about 200 nanometers; and a second layer of the first submodule, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second submodule, the first layer and the second layer having a refractive index mismatch of less than 0.2; 42. The tandem photovoltaic device of claim 41 , comprising:
49. 42. The tandem photovoltaic device of claim 41 , wherein the second layer comprises a first surface and a second surface, the first surface of the second layer in contact with the first surface of the first layer, and the second surface of the second layer having a root-mean-square roughness of less than 25 nanometers.
50. The tandem photovoltaic device of claim 48 or claim 49, wherein the first layer comprises an absorber layer having a II-VI semiconductor and the second layer comprises a transparent layer.
51. 51. The tandem photovoltaic device of claim 50, wherein the transparent layer comprises titanium dioxide.
52. The interface, a first layer of the first submodule, the first layer adjacent the second submodule, the first layer having a first surface, the first surface having a root mean square roughness of about 175 nanometers to about 200 nanometers; a second layer of the first submodule, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second submodule, the first layer and the second layer having a refractive index mismatch of less than 0.2; Including, the second layer comprises a first surface and a second surface, the first surface of the second layer contacting the first surface of the first layer, and the second surface of the second layer having a root mean square average roughness of less than 170 nanometers; the first layer comprises an absorber layer having a II-VI semiconductor and the second layer comprises a transparent layer; and 52. The tandem photovoltaic device of claim 51 , wherein the transparent layer comprises titanium dioxide.
53. The tandem photovoltaic device according to one of claims 41 to 52, wherein the interface is configured to transmit at least 60% of the light having a wavelength between about 800 nm and about 1200 nm that passes through it.
54. 1. A method of making a tandem photovoltaic device, comprising: providing a first sub-module and a second sub-module; and forming an interface between the first sub-module and the second sub-module, the interface passing a portion of light, the interface optically coupling the first sub-module and the second sub-module, and optically coupling the first sub-module and the second sub-module includes reducing reflection of the portion of light. A method comprising:
55. the interface includes a first layer of the first submodule, the first layer adjacent to the second submodule, the first layer having a first surface; and 55. The method of claim 54, wherein forming an interface between the first sub-module and the second sub-module comprises polishing the first surface to provide a root-mean-square roughness of less than 25 nanometers.
56. 56. The method of claim 55, wherein polishing the first surface to provide a root mean square average roughness of less than 25 nanometers comprises a member selected from the group consisting of mechanically polishing the first surface, chemically polishing the first surface, and combinations thereof.
57. the interface includes a second layer of the first sub-module, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second sub-module; the first layer and the second layer have a refractive index mismatch of at least 0.75; the first layer comprises an absorber layer having a II-VI semiconductor and the second layer comprises a transparent layer; and 57. The method of claim 56, wherein the second layer comprises a conductive layer.
58. The interface, a first layer of the first submodule, the first layer adjacent the second submodule, the first layer having a first surface, the first surface having a root mean square roughness of about 175 nanometers to about 200 nanometers; 55. The method of claim 54, wherein forming an interface between the first sub-module and the second sub-module comprises forming a second layer of the first sub-module, the second layer contacting the first surface of the first layer, the second layer being between the first layer and the second sub-module, and the first layer and the second layer having a refractive index mismatch of less than 0.
2.
59. 60. The method of claim 58, wherein forming the second layer of the first module comprises applying a coating composition by one of spray coating, roll coating, and spin coating.
60. the second layer comprises a first surface and a second surface, the first surface of the second layer contacting the first surface of the first layer, the second surface of the second layer having a root mean square average roughness of less than 170 nanometers; the first layer comprises an absorber layer having a II-VI semiconductor, and the second layer comprises a transparent layer; 60. The method of claim 59, wherein the transparent layer comprises titanium dioxide.
61. A method according to any one of claims 54 to 60, wherein the transparent layer has a refractive index in the range of 1.7 to 2.
3.
62. The method of any of claims 54 to 61, wherein the transparent layer has a gradient refractive index.
Citation Information
Patent Citations
Multijunction semiconductor element and solar cell element using it
JP2005057251A
Photoelectric conversion apparatus and method of manufacturing the same
JP2011086731A
Thin-film solar cell and method of manufacturing the same
JP2012114296A
Organic-inorganic hybrid perovskite nanocrystals and methods for making same
JP2019523740A
Photovoltaic devices with transparent tunnel junctions.
JP2019530984A