Method for manufacturing a laminated core for an electrical machine - Patents.com
The method of alloying metal sheet lamellas with foil lamellas in laminated cores enhances electrical resistance and mechanical properties by diffusing aluminum and silicon, addressing inefficiencies in existing manufacturing methods and reducing magnetostriction.
Patent Information
- Application Number
- JP2024534282
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-12-08
- Filing Date
- 2022-11-14
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2042-11-14
AI Technical Summary
Existing methods for manufacturing laminated cores of electrical machines face challenges in achieving high aluminum and silicon contents while maintaining low costs and preserving soft magnetic properties, leading to inefficiencies and increased magnetostriction.
A method involving the alloying of metal sheet lamellas with foil lamellas, where an insulating layer is formed by diffusing aluminum and silicon from a foil coating into the metal sheets during heat treatment, allowing for increased silicon and aluminum content in the near-surface region without excessive thickness, thereby enhancing electrical resistance and reducing magnetostriction.
This approach improves the electrical resistance and mechanical properties of laminated cores, reducing remagnetization losses and maintaining high magnetic permeability, while using cost-effective materials and avoiding grain size changes.
Smart Images

Figure 2024543629000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a laminated core of an electrical machine. [Background technology]
[0002] From EP 3511429 A1 a method for producing laminated cores is known, in which the sheet metal laminations of the initial laminated core are coated with a foil coating having an aluminum and / or silicon mass fraction of at least 20%. This initial laminated core is heat treated to obtain a laminated core. This allows to obtain a laminated core having a silicon content corresponding to a mass fraction of at least 6.5%. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] European Patent Application Publication No. 3511429 Summary of the Invention [Means for solving the problem]
[0004] The method according to the invention for producing a laminated core with the features of claim 1 has the advantage that it allows a later alloying of the metal sheets of a laminated core of an electric machine and a later production of insulating layers on or between the metal sheets of the laminated core at low cost. In this way, inexpensive electrical sheets with low aluminum and silicon contents, for example less than 4.0% by weight, can be alloyed by heat treatment to higher aluminum and silicon contents, for example between 4.0 and 8.5% by weight, at least in the region near the surface.
[0005] Furthermore, it is advantageous to increase the electrical resistivity of the metal laminations of the laminated core without excessively impairing the soft magnetic properties, thereby improving the efficiency of the electric machine. According to the invention, in a first step, foil sheets are provided, each comprising an aluminum support foil and a natural or produced insulating layer, for example an aluminum oxide foil layer, formed on the support foil, each having a foil coating on at least one side of the foil sheet, the foil coating comprising an alloying material, an adhesive binder for adhering the alloying material to the foil sheet, and in particular further powdered aluminum oxide.
[0006] Furthermore, in a second step, the metal sheet laminates of the laminated core are provided, which are not particularly electrically insulated, as opposed to the conventional forms in which they are electrically insulated, and if the metal sheet laminates have a lacquer insulation, this must be removed, since this can hinder diffusion and can lead to undesirable penetration of carbon from the lacquer layer into the metal sheet.
[0007] In a third step, an alternating stack of metal sheet laminates and foil laminates is performed, with at least one foil laminate located between each adjacent metal sheet laminate. Furthermore, in a fourth step, the laminate of the metal sheet and the foil is heated, e.g., heat-treated, - with the melting of the support foil, aluminum from the support foil of the foil sheet diffuses to a certain depth into the metal of the respective adjacent metal sheet, and alloying material from the foil coating of the foil sheet diffuses to a certain depth into the metal of the respective adjacent metal sheet to form alloyed regions; - The aluminum oxide foil layer of the foil laminate or the aluminum oxide from the foil coating of the foil laminate remains and forms an insulating layer between the metal laminates.
[0008] It is advantageous if the shape and / or area of the foil sheets corresponds to the shape and / or area, respectively, of the metal sheet sheets, as a result of which a particularly advantageous construction is achieved with regard to the geometry of the individual layers.
[0009] It is advantageous if the aluminum-based foil sheet is cut or is cut from an aluminum foil, which is provided with at least one aluminum oxide foil layer on at least one side and / or which is at least partially coated with an alloy material on at least one side. In particular, such an aluminum foil can therefore already be coated in an upstream production process, for example, pre-wound. Here, it is also advantageous if the foil coating is not too thick. This can allow for advantageous adhesion and winding.
[0010] It is also advantageous if the alloying material is at least partially applied to at least one side of the foil sheet by means of an adhesive binder, in particular a paste, and / or by means of a polysaccharide, in particular xanthan. The alloying material is preferably in the form of a powder. This allows a reliable bonding of the powdered alloying material to the aluminum foil. Here, the silicon powder and, optionally, also the aluminum oxide powder can be mixed with water and, for example, xanthan. This mixture can be applied to at least one side of the aluminum foil, for example, by means of a compressed air spray gun. During subsequent drying, the water evaporates and the xanthan remaining in the mixture ensures good adhesion of the powder. This can be done on one or both sides of the aluminum foil.
[0011] It is advantageous if at least one foil sheet is at least partially arranged between adjacent metal sheets. In the case of alloying of the metal sheets, a substantial increase in the mass fraction of silicon is made, but it is advantageous that the mass fractions of silicon and aluminum are not too large. This basically means that it is advantageous that the amount of aluminum (in metallic form) is not too large compared to the amount of silicon contained in the foil coating. If a double-sided coated foil is inserted between adjacent metal sheets, on the one hand the amount of silicon can be easily increased without the thickness of the foil coating becoming too large. This makes it possible to ensure in particular a reliable adhesion of the foil coating to both sides of the aluminum foil. On the other hand, the advantage arises that the total layer thickness of the aluminum oxide foil layers can be easily doubled. It is thus possible, in particular, to achieve in the manufactured laminated core the formation of an insulating layer of aluminum oxide between the electrical sheets during the heat treatment. Furthermore, it is also possible to achieve a limit to the mass fraction of aluminum, in order to reduce or completely prevent the increase in magnetostriction, in particular with an increase in the aluminum fraction.
[0012] It is advantageous if at least two foil sheets are arranged at least partially between adjacent metal sheet sheets. In the case of alloying the metal sheet sheets, a substantial increase in the mass fraction of silicon is made, but it is advantageous that the mass fractions of silicon and aluminum are not too large. This basically means that it is advantageous that the amount of aluminum (in metallic form) is not too large compared to the amount of silicon contained in the foil coating. If several foil sheets are inserted between adjacent metal sheet sheets, on the one hand, the amount of silicon can be easily increased without the thickness of the foil coating becoming too large. This makes it possible to ensure a reliable adhesion of the foil coating to the target surface of the aluminum foil in particular. On the other hand, the advantage arises that the total layer thickness of the aluminum oxide foil layer can be easily increased. This prevents the aluminum oxide foil layer from being partially rubbed off or otherwise partially peeled off, for example during handling. It is thus possible to achieve, in particular, that an insulating layer of aluminum oxide is formed in the manufactured laminate core. Furthermore, it is also possible to achieve a limitation of the mass fraction of aluminum, in order to reduce or completely prevent an increase in magnetostriction, in particular with an increase in the aluminum fraction. This can be achieved, for example, when using two foil sheets instead of a single foil sheet, where the two foil sheets have, in total, the same thickness as the single foil sheet. For example, instead of one foil sheet having a thickness of 10 μm, two foil sheets, each 5 μm thick, each with an aluminum oxide foil layer, can be used, thereby doubling the total thickness of the aluminum oxide foil layer.
[0013] It is also advantageous if the thickness of the foil sheet and the alloying material and possibly the electrically insulating solid applied to the foil sheet are selected such that after the heat treatment, at least on a part of the surface of the metal sheet, at least near the surface, the mass fraction of silicon is at least about 6.5%, and the mass fraction of silicon and aluminum is not more than 8.5%. In particular, this allows the disappearance of magnetostriction to be achieved, which results in low pressure sensitivity and high magnetic permeability. The alloying near the surface can concern, for example, an edge region or edge area of about 500 μm. This is advantageous, since at high frequencies, eddy currents also occur near the surface as well. The core region can then be advantageously realized without silicon and / or aluminum or with a small mass fraction of silicon and / or aluminum, so that the material of the electrical sheet in the core region has toughness and therefore high mechanical load-bearing capacity. Preferably, the mass fraction of silicon and aluminum is not more than 8.5%. Here, the starting material of the metal sheet can be formed, for example, with a mass fraction of silicon of about 3%. The mass fraction of silicon is then further increased by heat treatment, preferably to a mass fraction of 6.5% with respect to silicon.
[0014] In a further possible embodiment, it is advantageous if the thickness of the foil sheet and the alloy material and possibly the electrically insulating solid applied to the foil sheet are selected such that after the heat treatment, at least on a part of the surface of the metal sheet, at least in the vicinity of the surface, the mass fraction of silicon is between about 4% and about 5%, and the mass fraction of silicon and aluminum is less than or equal to about 8.5%. This configuration allows the use of inexpensive materials for the metal sheet. In particular, metal sheets made of materials that are substantially free of silicon fractions can be used. The mass fraction of silicon can then be increased by heat treatment.
[0015] The increase in the mass fraction of silicon is preferably not carried out into the core region of the sheet metal, since the heat treatment required for this would normally also change the grain size, thus avoiding any change in grain size.
[0016] It is advantageous if the foil sheet has a thickness of about 5 μm to about 10 μm, preferably as thin as possible. Here, for example, an aluminum oxide foil layer of 1 μm can be provided. Here, between the metal sheet sheets, the desired number of foil sheets can be inserted. Advantageous handling is thus made possible, since in particular at least partial peeling of the aluminum oxide foil layer can be reliably avoided. The advantage of the aluminum oxide foil layer of the aluminum foil is that therefrom, during the heat treatment, the aluminum oxide foil layer is formed as an electrically insulating layer between the electrical sheets. In the case of powders, the risk is high at locations that are not sufficiently electrically insulated. Moreover, in this form, the foil coating can be made relatively thin without the mass fraction of aluminum in the metal sheet sheet being undesirably large after the heat treatment.
[0017] It is also advantageous that the heat treatment of the metal sheets between which the coated foil sheets are arranged, which is carried out before the heat treatment for alloying, is carried out in the range of about 150°C to 500°C for about 1 hour to about 2 hours. This ensures that the adhesive binder or polysaccharide is decomposed. Here, the heat treatment can be carried out in the presence of hydrogen. At, for example, 400°C, xanthan is decomposed, for example, into water, carbon monoxide, carbon dioxide, and methane and is thus removed. Then, the diffusion of silicon and aluminum into the metal sheets can be carried out by heat treatment, for example, at 1250°C. When silicon and aluminum are completely diffused, aluminum oxide remains between the metal sheets as an electrically insulating layer.
[0018] In laminated cores for rotors, it is advantageous for the foil sheets to be partially coated with alloying material, so that the radially outer portions of the foil sheets of the laminated core are provided with more alloying material than the radially inner portions of the foil sheets, in particular, this allows a reduced alloying to be achieved near the shaft, where the material remains tough, whereas at positions away from the shaft a higher alloying can be achieved, increasing the specific electrical resistivity and thus reducing remagnetization losses.
[0019] Similarly, in a laminated core for a stator, it is advantageous if the foil sheets are partially coated with an alloy material, the alloy material being provided closer to the radially inner portion of the foil sheets than to the radially outer portion of the foil sheets.
[0020] Preferred exemplary embodiments of the invention are described in more detail below with reference to the accompanying drawings, in which corresponding elements are provided with the same reference numerals, and in which: [Brief description of the drawings]
[0021] [Figure 1] FIG. 2 is a partial schematic cross-sectional view of an aluminum foil structure according to an exemplary embodiment. [Diagram 2] FIG. 2 illustrates the aluminum foil shown in FIG. 1 with a foil coating according to an exemplary embodiment. [Diagram 3] FIG. 3 is a schematic diagram showing the aluminum foil shown in FIG. 2 in a partially rolled up state. [Figure 4] FIG. 4B is a partial schematic cross-sectional view of the structure of a laminated core according to an exemplary embodiment during manufacture, the left part representing the cross-section of the laminated core before heat treatment and the right part representing the cross-section of the laminated core after heat treatment, the cross-section represented by IV in FIG. 4A being shown. [Figure 4A] FIG. 2 is a schematic diagram of an entire laminated core. [Diagram 5] FIG. 5 shows the structure shown in FIG. 1 during manufacture in a modified form, prior to heat treatment, in a cross section of the entire laminated core, similar to FIG. 4. [Figure 6] FIG. 3 is a plan view of a coated foil sheet for the laminated core shown in FIG. 1 or FIG. 2 according to a possible configuration. [Figure 7] 3 is a diagram showing the laminated core shown in FIG. 1 or 2 in a completed manufacturing state after heat treatment. FIG. [Figure 8A] FIG. 1 is a phase diagram for explaining the present invention, in which a diagram for an austenite stabilizer is shown. [Figure 8B] FIG. 1 is a phase diagram for explaining the present invention, in which a diagram for eutectic forming materials is shown. [Figure 8C]FIG. 1 is a phase diagram for explaining the present invention, in which a diagram regarding ferrite forming elements is shown. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0022] 1 shows in a partially schematic cross-sectional view the structure of an aluminum foil 11 according to an exemplary embodiment. The aluminum foil 11 has an aluminum oxide foil layer 8. Furthermore, the aluminum foil 11 has a support foil 10, which is not oxidized and therefore consists of pure aluminum.
[0023] Figure 2 shows the aluminum foil 11 shown in Figure 1 with a foil coating 17 according to an exemplary embodiment. The foil coating 17 is formed from an alloying material 16 and is applied to one of the faces 12, 13. The alloying material 16 comprises silicon, and preferably consists at least substantially of silicon. The foil coating 17 may comprise further components. A configuration of the aluminum foil 11 that is as thin as possible with a foil coating 17 that includes an alloying element such as silicon that is as thick as possible is advantageous.
[0024] Figure 3 is a schematic diagram of the aluminium foil 11 shown in Figure 2 in a partially rolled state, where the foil coating 17 is not shown for ease of illustration. The foil sheets 6, 7 are cut from the aluminium foil 11 and then each foil sheet 6, 7 is coated with a foil coating 17.
[0025] The aluminium foil 11 can then be fed such that one or both sides 12, 13 of the aluminium foil 11 are provided with an aluminium oxide foil layer 8. Thus, depending on the configuration, there may be an aluminium oxide foil layer 8, 9 on only one of the sides 12, 13 or alternatively on both sides 12, 13. The aluminium foil 11 may be present wound up in a roll 18, which is shown diagrammatically.
[0026] Preferably, the aluminum oxide foil layer 8 is on only one of the faces 12,13 and the silicon based foil coating 17 is on only one of the faces 12,13. FIG. 4 shows in a partially schematic cross-sectional view the structure of a laminated core 1 according to an exemplary embodiment during manufacture.
[0027] Here, reference number 4 indicates a cross section indicated by IV in FIG. 4A from the entire laminated core 1 . The laminated core 1 can in particular be used for a rotor 2 (FIG. 6) or a stator of an electric machine 3. Such a rotor 2 can then comprise a plurality of such laminated cores 1. The laminated core 1 is in particular suitable for an electric machine 3 serving as an electric drive motor 3 for an automotive vehicle.
[0028] To manufacture the laminated core 1, the following method steps are carried out according to the invention: In a first step, foil sheets 6, 7, 10, 11 are provided, each of which comprises an aluminium support foil 10, i.e. aluminium foil, and a natural or produced insulating layer 8, in particular an aluminium oxide foil layer 8, formed on the support foil 10, and which respectively have a foil coating 17 on at least one side 12, 13. The foil coating 17 comprises an alloying material 16, such as silicon, an adhesive binder and in particular further powdered aluminium oxide.
[0029] In a subsequent second step, the sheet metal laminates 4, 5 of the laminated core 1 are provided, which are in particular not electrically insulated. In a subsequent third step, an alternating stacking of the metal sheet laminates 4,5 and the foil laminates 6,7,11 is carried out, such that at least one foil laminate 6,7,11 is located between adjacent metal sheet laminates 4,5, respectively.
[0030] In a subsequent fourth step, the stack of metal sheets 4, 5 and foil sheets 6, 7, 11 is heated, in particular heat-treated, a) as the support foil 10 melts, aluminum from the support foil 10 of the foil sheets 6, 7, 10, 11 diffuses into the metal of the adjacent metal sheets 4, 5 at a certain depth, and alloying material 16 from the foil coating 17 of the foil sheets 6, 7, 11 diffuses into the metal of the adjacent metal sheets 4, 5 at a certain depth 25, 26 to form alloyed regions 23, 24; b) Aluminum oxide (Al2O3) from the aluminum oxide foil layer 8 of the foil laminae 6,7,11 or the foil coating 17 remains and forms an insulating layer 27 between the metal sheet laminae 4,5.
[0031] The heating in the fourth step can for example be performed by radiation and / or convection, by induction or by the flow of an electric current through the metal laminations 4, 5. The laminated core 1 comprises metal laminations 4, 5, 5' based on an iron-based material.
[0032] During manufacture, at least one foil sheet 6, 7 is arranged between adjacent metal sheet laminates 4, 5, 5', respectively. In the exemplary embodiment shown in Figure 1, a foil sheet 6 is arranged between metal sheet laminates 4, 5 and a foil sheet 7 is arranged between metal sheet laminates 4, 5'.
[0033] Preferably, the entire roll or coil of aluminum foil 11 is coated and rewound. During the manufacture of the laminated core 1, which is carried out by stacking alternately sheet metal laminations (electrical sheets) 4, 5 and aluminum foil, the foil laminations 6, 7 are cut or cut from the aluminum foil roll 11 and placed between the sheet metal laminations 4, 5, 5'.
[0034] In the illustrated form, the foil sheet 6 comprises one aluminium oxide foil layer 8 on each side 12, 13. In addition, a foil coating 17 is applied to both sides 12, 13 of the foil sheet 6.
[0035] After heat treatment, the state shown on the right side of Figure 4 is reached. Now, the volume of the metal sheets 4, 5, 5' has increased, since silicon and aluminum have been diffused into the alloyed areas or regions 23, 24 of the metal sheets 4, 5, respectively. Now, aluminum can form a eutectic with silicon, which facilitates the diffusion. Aluminum oxide 8 remains between the layers 4, 5, 5'.
[0036] FIG. 5 shows the structure shown in FIG. 1 as produced in a modified form, in which, like FIG. 4, a cross section of the entire laminated core is shown. In this form, the foil sheets 6, 7 can be cut out of the aluminum foil 11 and a plurality of, for example two, foil sheets 6, 7 can be placed between adjacent metal sheet sheets 4, 5, respectively. This has the advantage that, when the aluminum foil 11 used comprises a layer 10 of pure aluminum, for example half its thickness, a larger amount of aluminum oxide and / or alloy material 16 can be introduced between adjacent metal sheet sheets 4, 5. This therefore allows the introduction of a correspondingly larger amount of aluminum oxide and / or alloy material 16 to be achieved without too great a loss of handling. For the sake of simplicity of illustration, the layer structure of the foil sheets 6, 7 is not shown in FIG. 5. The layer structure of the foil sheets 6, 7 is obtained in the same way from the form described on the basis of FIG. 1. The foil sheets 6, 7 are preferably much thinner than the foil coating 17 with the alloy material 16.
[0037] The foil coating 17 may comprise adhesive binders and / or polysaccharides, in particular xanthan, by means of which the alloying material 16 is applied to the upper side 14 of the aluminum foil 11 and thus to the foil sheets 6, 7. In a modified form, however, the alloying material 16 can also be applied as an aqueous suspension. However, application by adhesive binders and / or polysaccharides has the advantage that a more uniform and constant application is possible even with complex geometric shapes on the metal sheet sheets 4, 5, which are usually already punched out. A further advantage is that the powdered alloying material 16 does not fall off the aluminum foil 11 and the foil sheets 6, 7 after drying.
[0038] The adhesive binder or polysaccharide can be removed by a heat treatment carried out prior to the heat treatment for alloying. This heat treatment can be carried out in a hydrogen atmosphere at a temperature in the range of about 150°C to 500°C for about 1 to about 2 hours.
[0039] Further modifications are also conceivable. For example, more than two foil sheets 6, 7 can be arranged between adjacent metal sheet laminations 4, 5. Furthermore, it is also conceivable to realize structural variations within the laminated core 1. For example, it is not always necessary to provide a foil sheet 6, 7 between adjacent metal sheet laminations, and it is not always necessary to provide the same number of foil sheets 6, 7 between adjacent metal sheet laminations. However, preferably, a uniform structure of the laminated core is realized during production.
[0040] The thickness of the aluminum foil 11, and thus of the foil sheets 6, 7, and the foil coating 17, in particular the form and composition of the alloying material 16, are selected so that after the heat treatment, at least in the vicinity of the surface, at least in a portion 20 of the surface 21 of the metal sheet 5, the mass fraction of silicon is at least about 6.5% and the mass fraction of silicon and aluminum is not more than 8.5%. This also applies to the metal sheet 4. In a modified form, a specification can be selected in which the mass fraction of silicon is between about 4% and about 5% and the mass fraction of silicon and aluminum is not more than about 8.5%. The alloying of the metal sheet 5 can be carried out over the entire surface 21 of the metal sheet 5. However, the alloying can also be carried out only in a portion 20 of the surface 21 of the metal sheet 5, as will be described below with reference to FIG. 6.
[0041] FIG. 6 shows a plan view of the coated foil sheet 6 arranged on the metal sheet 5 for the laminated core 1 shown in FIG. 1 or 2 according to a possible configuration for the rotor 2. Here, the portion 20 is the radially outer portion 20, in which eddy currents can occur at least approximately essentially possible during operation. A higher alloying is therefore beneficial here in order to prevent losses due to eddy currents. Another portion 22 is the radially inner portion 22 of the surface 21. The portions 20, 22 of the metal sheet 5 correspond to the portions 20', 22' of the foil sheet 6. Here, the foil sheet 6 can be provided with a foil coating 17 such that the foil coating 17 is only on the portion 20' of the foil sheet 6. This means that after production, a higher alloying is achieved on the portion 20 of the metal sheet 5 than on the other portion 22 of the metal sheet 5. In particular, the iron material in the portion 22, where the metal sheet 5 is pressed, for example, against a shaft, can thereby have a higher mechanical load-bearing capacity.
[0042] Here, the silicon in portion 20 does not lose its volume after diffusing into the iron of the electrical sheet 5, but rather the thickness of the electrical sheet 5 increases accordingly, ensuring that no gap formation occurs in portion 22. To compensate for this, for example in portion 21 an inert powder such as aluminum oxide powder can be used.
[0043] The configuration described with respect to the rotor 2 on the basis of FIG. 6 can be realised in a similar but reversed manner in the laminated core 1 acting as the stator. FIG. 7 shows the laminated core 1 shown in FIG. 5 in the completed manufacturing state. Similarly, the laminated core 1 shown on the right side of FIG. 4 is obtained. The heat treatment used for alloying, which can be carried out for example at temperatures in the range of 950° C. to 1250° C., preferably at 1000° C. to 1100° C., for example for 10 minutes to 30 minutes, achieves a diffusion of silicon and aluminum into the metal sheets 4, 5. Here, a diffusion is achieved, preferably near the surface, resulting in an average penetration depth 25, 26 for the metal sheets 4, 5 that is less than half the metal sheet thickness of the metal sheets 4, 5. Between the metal sheets 4, 5 an aluminum oxide layer 27 remains as an insulator 27, the thickness 28 of the aluminum oxide being predeterminable. The cores 29, 30 of the metal sheets 4, 5 are less or barely alloyed with respect to the alloy material 16.
[0044] In one possible form, the aluminum foil 11 can have a thickness of about 5 μm to about 10 μm. However, in a modified form, for example the aluminum foil 11, anodized on both sides, can also have a foil thickness of 0.03 mm and an oxide layer thickness of 5 to 6 μm. For example, an alloy material 16 in the form of silicon powder with an average grain size of 1 to 5 μm is particularly suitable for such a foil thickness of 0.03 mm. Similarly, for example with a foil thickness of 5 μm, silicon powder with an average grain size of 1 to 5 μm and optionally even aluminum oxide powder with an average grain size of 0.5 μm can be used. The aluminum foil 11 can, for example, comprise an aluminum oxide foil layer with a thickness of 1 μm and a metallic aluminum layer with a thickness of 4 to 5 μm.
[0045] In a modified form, the aluminium oxide foil layer of the aluminium foil 11 and thus of the foil sheets 6, 7 can also be omitted when, in addition to the alloy material 16, aluminium oxide is applied to the aluminium foil 11 by means of a foil coating 17. Here, the aluminium oxide can be aluminium oxide powder. In principle, it is also possible to use an aluminium foil 11 with at least one aluminium oxide foil layer 8, 9 and further with a foil coating 17 comprising aluminium oxide.
[0046] Other electrically insulating solids, preferably used as electrically insulating powders, can also be used as electrically insulating components of the foil coating 17, as long as they are stable and do not melt in the hydrogen atmosphere, especially up to 1250°C. In the hydrogen atmosphere, a significant reduction in aluminum oxide occurs above 1300°C, up to a mass fraction of 20%. At a heat treatment temperature of 1250°C, the aluminum oxide is reduced by up to 7%. Silicon oxide (SiO2) and mullite (Al (4+2x) S (2-2x) O (10-x) , where x=0.17-0.59), is also stable and does not melt in a strongly reducing hydrogen atmosphere up to 1250° C. Preferably, oxides of aluminum and silicon are used to form the insulator 27.
[0047] The foil sheets 6, 7 can be punched out of the aluminum foil 11 to the same shape as the metal sheets 4, 5 before stacking on the laminated core 1. However, it is also possible to stack the non-punched foil sheets 6, 7 between the metal sheets 4, 5. The protruding foil can then be removed after stacking. It is also possible that the protruding foil is not removed and melts off during the heat treatment.
[0048] In the completed manufacturing state, for example, the aluminum oxide layer 27, which functions as an insulator 27, at least partially has fine channels perpendicular to the layer plane, typical of an anodized aluminum oxide layer, where furthermore the layer structure of the aluminum oxide layer 27 may consist of a number of thin partial layers.
[0049] Based on Figures 8A, 8B and 8C, the effect of suitable alloying element X on the size of each austenite domain in each FeX phase diagram is shown, where the concentration (wt%) of each alloying element X is plotted on the x-axis and the temperature T is plotted on the y-axis.
[0050] Fig. 8A is a phase diagram for explaining the present invention, in which a diagram for an austenite stabilizer is shown. As shown in the schematic phase diagram, with manganese as an austenite stabilizer, the austenite phase (γ) is stabilized at a lower temperature as the concentration of manganese increases. In the diagram, room temperature is shown as the lower temperature limit.
[0051] In Fig. 8A an exemplary behavior according to the invention is shown according to line Y, illustrating the effect of austenite stabilization during the course of heat treatment. Due to the diffusion of the austenite stabilizer into the respective metal sheet 4, 5, the austenite of the heated metal sheet 4, 5 is stabilized, such that upon cooling of the metal sheet 4, 5, the austenite is not transformed back into ferrite according to the phase diagram.
[0052] FIG. 8B shows a phase diagram for explaining the present invention, in which a diagram for eutectic forming materials is shown. As shown in the schematic phase diagram, with copper as a eutectic former, the austenite phase becomes stable at lower temperatures as the concentration of copper increases. However, this does not allow stability down to room temperature. Rather, at a certain copper concentration, a minimum temperature value occurs at which the austenite phase is still stable. This region, where austenite is stable even at low temperatures clearly below A3, allows the austenite to be nearly frozen upon cooling and thus preserved upon further cooling to room temperature. Then, as the concentration of copper increases further, the temperature at which the austenite phase is stable also increases. This makes it increasingly difficult, and eventually impossible, to nearly freeze the austenite upon cooling. A further increase in the copper concentration leads to a concentration at which the formation of the austenite phase in iron is no longer possible.
[0053] FIG. 8C is a phase diagram for explaining the present invention, showing a diagram relating to ferrite forming elements. As shown in the schematic phase diagram, ferrite (α) is the stable phase at room temperature due to ferrite-forming elements such as silicon or aluminum. This means that austenite is stable only when low concentrations of ferrite-forming elements and high temperatures are simultaneously present. Therefore, austenite cannot freeze out on cooling, since it will transform to ferrite at higher temperatures.
[0054] The invention is not limited to the exemplary embodiments described above.
Claims
1. A method for manufacturing a laminated core, in particular for the subsequent alloying of the metal sheets (4, 5) of a laminated core (1) and for the subsequent production of insulating layers (8, 9) on or between the metal sheets (4, 5) of said laminated core (1) of an electric machine, in particular a stator or rotor, comprising: - providing foil sheets (6, 7, 10, 11) each comprising an aluminium support foil (10) and a natural or produced aluminium oxide foil layer (8), each having a foil coating (17) on at least one side (12, 13), said foil coating (17) comprising an alloying material (16), in particular silicon, an adhesive binder and in particular further aluminium oxide in powder form; - providing the metal sheets (4, 5) of said laminated core (1), in particular not electrically insulated; - stacking the metal sheet laminates (4, 5) and the foil sheets (6, 7, 11) alternately, such that at least one foil sheet (6, 7, 11) is located between each adjacent metal sheet laminate (4, 5); - heating, in particular heat treating, the laminate of metal sheets (4, 5) and foil sheets (6, 7, 11), a) aluminum from the support foil (10) of the foil laminae (6, 7, 10, 11) diffuses into the metal of the respective adjacent metal sheet laminae (4, 5) with the dissolution of the support foil (10), and the alloy material (16) from the foil coating (17) of the foil laminae (6, 7, 11) diffuses into the metal of the adjacent metal sheet laminae (4, 5) at a certain depth (25, 26) to form alloy regions (23, 24); b) the aluminium oxide from the aluminium oxide foil layer (8) of the foil laminations (6, 7, 11) or the foil coating (17) remains and forms an insulating layer (27) between the metal laminations (4, 5); method.
2. 2. The method according to claim 1, characterized in that the shape and / or area of the foil sheets (6, 7, 11) correspond to the shape and / or area of the metal sheets (4, 5).
3. 3. The method according to claim 1 or 2, characterized in that the aluminium-based foil sheets (6, 7, 10, 11) are cut or are cut from an aluminium foil (11), the aluminium foil (11) being provided with the at least one aluminium oxide foil layer (8, 9) on at least one side and / or the aluminium foil (11) is at least partially coated or is coated with the alloy material (16) on at least one top side (14, 15).
4. 4. The method according to claim 3, characterized in that the alloy material (16), preferably formed in powder form, is or is applied at least partially to the at least one upper surface (14, 15) of the foil sheet (6, 7, 10, 11) by means of an adhesive binder, in particular a paste, and / or by means of a polysaccharide, in particular xanthan.
5. 5. The method according to claim 1, wherein at least two of said foil sheets (6, 7, 10, 11) are at least partially arranged between adjacent sheet metal sheets (4, 5).
6. 6. The method according to claim 1, wherein the thickness of the foil (6, 7, 10, 11) and the alloy material (16) and possibly electrically insulating solids applied to the foil (6, 7, 10, 11) are selected such that, after the heat treatment, on at least a portion (20) of the surface (21) of the metal sheet (4, 5), at least in the vicinity of the surface, the mass fraction of silicon is at least about 6.5% and the mass fraction of silicon and aluminum is not more than about 8.5%, or at least in the vicinity of the surface, the mass fraction of silicon is between about 4% and about 5% and the mass fraction of silicon and aluminum is not more than about 8.5%.
7. 7. The method according to any one of the preceding claims, characterized in that the foil sheets (6, 7, 10, 11) have a thickness of about 5 μm to about 10 μm.
8. 8. The method according to claim 1, characterized in that the heat treatment of the metal sheets (4, 5) between which the coated foil sheets (6, 7, 10, 11) are arranged, which is carried out before the heat treatment for alloying, is carried out in the range of about 150°C to 500°C for 1 hour to about 2 hours.
9. 9. The method according to claim 1, characterized in that in a laminated core for a rotor, the foil sheets (6, 7, 10, 11) are partially coated with the alloy material (16), the alloy material being provided closer to a radially outer portion (20') of the foil sheets (6, 7, 10, 11) than to a radially inner portion (22') of the foil sheets (6, 7, 10, 11).
10. 9. The method according to claim 1, characterized in that in a laminated core for a stator, the foil sheets (6, 7, 10, 11) are partially coated with the alloy material (16), the alloy material being provided closer to the radially inner portion (20') of the foil sheets (6, 7, 10, 11) than to the radially outer portion (22') of the foil sheets (6, 7, 10, 11).
Citation Information
Patent Citations
Manufacture for magnetic core
JP1982147119A
Magnetic substance and its manufacture
JP1996222422A
Methods of manufacturing coil and coil device
JP2010199291A
A laminated core made of soft magnetic material, and a method for joining single-layer core plates by the adhesive force forming the laminated soft magnetic core.
JP2012521649A
Magnetic steel sheet laminate and method for manufacturing the same
JP2019134161A