Membrane-electrode assembly and fuel cell including same
The membrane-electrode assembly with uneven portions and a catalyst layer structure addresses the bonding issue, improving durability and performance of polymer electrolyte membrane fuel cells.
Patent Information
- Application Number
- JP2024530571
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-07-14
- Filing Date
- 2022-11-23
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2042-11-23
AI Technical Summary
Conventional membrane-electrode assemblies in polymer electrolyte membrane fuel cells suffer from insufficient interfacial bonding between the electrolyte membrane and the electrode, leading to reduced durability and performance.
A membrane-electrode assembly with a polymer electrolyte membrane featuring uneven portions and a catalyst layer that includes a first catalyst layer filling the concave portions and a second catalyst layer on the convex portions, where the first catalyst layer has a higher ionomer content than the second, enhancing interfacial bonding and durability.
The improved interfacial bonding and durability result in enhanced performance and extended lifespan of the fuel cell.
Smart Images

Figure 2024543884000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a membrane-electrode assembly and a fuel cell including the same, and more particularly to a membrane-electrode assembly having improved durability and a fuel cell including the same. [Background technology]
[0002] 2. Description of the Related Art Fuel cells are cells that directly convert chemical energy produced by the oxidation of fuel into electrical energy. Fuel cells have been attracting attention as a next-generation energy source due to their environmentally friendly features of high energy efficiency and low pollutant emissions. A fuel cell generally has a structure in which an anode and a cathode are formed on either side of a polymer electrolyte membrane, and such a structure is called a membrane electrode assembly (MEA). Fuel cells can be classified into alkaline electrolyte fuel cells, polymer electrolyte membrane fuel cells (PEMFCs), etc. depending on the type of electrolyte membrane. Among them, polymer electrolyte membrane fuel cells are attracting attention as portable, vehicular, and home power sources due to their advantages such as low operating temperature of less than 100°C, fast start-up and response characteristics, and excellent durability. A representative example of such a polymer electrolyte membrane fuel cell is a proton exchange membrane fuel cell (PEMFC), which uses hydrogen gas as fuel. To summarize the reactions that occur in a polymer electrolyte membrane fuel cell, first, when a fuel such as hydrogen gas is supplied to the oxidizing electrode (or anode), hydrogen ions and electrons are generated at the oxidizing electrode by an oxidation reaction of the hydrogen gas. The generated hydrogen ions are transferred to the reducing electrode (or cathode) through the polymer electrolyte membrane, and the generated electrons are transferred to the reducing electrode (or cathode) through an external circuit. Oxygen gas is supplied to the reducing electrode, and the oxygen gas combines with the hydrogen ions and electrons to generate water through a reduction reaction. Conventional membrane-electrode assemblies are manufactured using flat films to provide a polymer electrolyte membrane, which can lead to poor interfacial adhesion between the electrolyte membrane and the electrodes, resulting in poor performance or a shortened lifespan of the polymer electrolyte membrane fuel cell. Meanwhile, Korean Patent Publication KR10-1715447B1 (published on December 24, 2014) is an invention relating to a membrane electrode assembly including an electrolyte membrane with concave portions on its surface and an electrode with convex portions on its surface, a manufacturing method thereof, and a fuel cell including the same. However, the Korean Patent Publication only discloses a polymer electrolyte membrane with concave portions, and there is still a problem in that the interfacial adhesion between the electrode and the electrolyte membrane is insufficient, resulting in a decrease in the durability of the electrode. Summary of the Invention [Problem to be solved by the invention]
[0003] SUMMARY OF THE PRESENT EMBODIMENTS The present invention has been made to solve the above problems, and an object of the present invention is to provide a membrane-electrode assembly which improves the interfacial adhesion between a polymer electrolyte membrane and a catalyst layer. Another object of the present invention is to solve the above problems and to provide a membrane-electrode assembly having improved durability by improving the interfacial adhesion between catalyst layers. It is still another object of the present invention to provide a fuel cell comprising the membrane-electrode assembly. The object of the present invention is not limited to the object mentioned above, and other objects and advantages of the present invention not mentioned can be understood from the following description and will be more clearly understood from the embodiment of the present invention. In addition, it will be easily understood that the object and advantages of the present invention can be realized by the means and combinations thereof described in the claims. [Means for solving the problem]
[0004] One embodiment of the present invention to achieve the above object provides a membrane-electrode assembly including a polymer electrolyte membrane having a concave-convex portion on at least one surface thereof and a catalyst layer disposed on the polymer electrolyte membrane, the catalyst layer including a first catalyst layer filling the inside of the concave-convex portion and a second catalyst layer disposed on the polymer electrolyte membrane, the first catalyst layer being interposed between the polymer electrolyte membrane and the second catalyst layer. Specifically, the first catalyst layer may be different from the second catalyst layer. According to yet another embodiment of the present invention, the first catalyst layer comprises a first ionomer, and the second catalyst layer comprises a second ionomer, and the weight of the first ionomer relative to the total weight of the first catalyst layer may be the same as or different from the weight of the second ionomer relative to the total weight of the second catalyst layer. Specifically, the weight of the first ionomer relative to the total weight of the first catalyst layer may be greater than the weight of the second ionomer relative to the total weight of the second catalyst layer. More specifically, the weight of the first ionomer relative to the total weight of the first catalyst layer may be greater than 35 wt %, and the weight of the second ionomer relative to the total weight of the second catalyst layer may be less than 35 wt %. Specifically, the first ionomer and the second ionomer may each independently be any one selected from the group consisting of a hydrocarbon-based ionomer, a fluorine-based ionomer, and a mixture thereof. Specifically, the uneven portion may include first recesses and first protrusions arranged alternately with the first recesses. According to still another embodiment of the present invention, the first catalyst layer may be filled to 80% (v / v) or more of the total volume of the first recess. According to yet another embodiment of the present invention, the first catalyst layer can fill the entire volume of the first recess. According to one specific example, the first catalyst layer can include a sidewall portion including a first sidewall portion and a second sidewall portion disposed opposite each other across the first central portion, the first sidewall portion can include a first side surface and a first curved surface extending from the first side surface to the upper surface of the first central portion, and the second sidewall portion can include a second side surface and a second curved surface extending from the second side surface to the upper surface of the first central portion. According to one specific example, the thickness H of the first central portion can be greater than 0 μm and less than 1 μm. According to one specific example, the minimum thickness I of the first sidewall portion can be greater than 0 and less than 0.8 times the thickness H of the first central portion, and greater than 0 and less than 0.5 times the thickness H of the first central portion. According to one specific example, a maximum width B of the first sidewall portion can be less than 0.2 times a width A between the first side surface and the second side surface. According to one specific example, a curvature R of the first curved surface can be less than or equal to a difference HI between a thickness H of the first central portion and a minimum thickness I of the first sidewall portion. According to yet another embodiment of the present invention, the first catalyst layer may further include a functional additive. Yet another embodiment of the present invention provides a fuel cell comprising the membrane-electrode assembly. Effect of the Invention
[0005] According to the present invention, it is possible to provide a membrane-electrode assembly that can improve not only the interfacial adhesion between the polymer electrolyte membrane and the catalyst layer, but also the chemical and mechanical durability, thereby improving both the performance and life of the fuel cell. In addition to the above-mentioned effects, specific effects of the present invention will be described below while explaining specific contents for carrying out the invention. [Brief description of the drawings]
[0006] [Figure 1] FIG. 1 is a cross-sectional view showing a membrane-electrode assembly according to one embodiment of the present invention. [Diagram 2] FIG. 2 is an enlarged cross-sectional view of the uneven portion of FIG. [Diagram 3] FIG. 4 is a cross-sectional view showing a membrane-electrode assembly according to another embodiment of the present invention. [Figure 4] FIG. 4 is a cross-sectional view showing a membrane-electrode assembly according to yet another embodiment of the present invention. [Diagram 5] FIG. 13 is a schematic diagram illustrating a fuel cell according to still another embodiment of the present invention. [Figure 6] 1 shows a photograph of a membrane-electrode assembly according to Example 1-1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0007] Hereinafter, each component of the present invention will be described in more detail so that a person having ordinary skill in the art to which the present invention pertains can easily implement the present invention. However, this is merely an example, and the scope of the present invention is not limited to the following content. One embodiment of the present invention provides a membrane-electrode assembly including a polymer electrolyte membrane having an uneven portion on at least one surface and a catalyst layer disposed on the polymer electrolyte membrane, the catalyst layer including a first catalyst layer filling the inside of the uneven portion and a second catalyst layer disposed on the polymer electrolyte membrane, the first catalyst layer being interposed between the polymer electrolyte membrane and the second catalyst layer. Specifically, the first catalyst layer may be different from the second catalyst layer. According to one aspect of the present invention, the first catalyst layer is interposed between the polymer electrolyte membrane and the second catalyst layer, thereby improving the interfacial adhesion between the polymer electrolyte membrane and the catalyst layer, and providing a membrane-electrode assembly having improved chemical and mechanical durability. This can improve both the performance and life of a fuel cell. The configuration of the present invention will be described in more detail below with reference to the drawings. 1. Membrane-electrode Assembly FIG. 1 is a cross-sectional view showing a membrane-electrode assembly according to one embodiment of the present invention. As shown in FIG. 1, a membrane-electrode assembly 100 according to the present invention comprises a polymer electrolyte membrane 10 and a catalyst layer 20 . The polymer electrolyte membrane 10 according to the present invention may have at least one surface with the uneven portion 15. Therefore, the polymer electrolyte membrane 10 may have the uneven portion 15 on one or both surfaces. One surface of the polymer electrolyte membrane 10 may have a plurality of projections and recesses 15 . The concave-convex portion 15 according to the present invention can include first concave portions and first convex portions arranged alternately with the first concave portions. For example, the first concave portions can be individual concave portions forming the concave-convex portion, and the first convex portions can be individual convex portions forming the concave-convex portion. Although FIG. 1 shows that the first catalyst layer 20a fills the entire volume of the first recess, the first catalyst layer 20a according to an embodiment of the present invention may be filled with 80% (v / v) or more of the entire volume of the first recess, preferably 80 to 95% (v / v), and more preferably 85 to 95% (v / v). If the first catalyst layer 20a fills less than 80% (v / v) of the entire volume of the first recess, the interfacial adhesion between the polymer electrolyte membrane and the catalyst layer may not be sufficiently large, and as a result, the durability of the interface may not be significantly improved. For example, the volume ratio of the first catalyst layer 20a to the entire volume of the first recess may be calculated by measuring the entire volume of the first recess and the volume of the first catalyst layer using a scanning electron microscope (SEM). The casting method used to manufacture polymer electrolyte membranes in the past is a method of forming a film shape by casting a solution in which a solute is dissolved in a solvent into a mold of a certain shape and evaporating the solvent with heat. This casting and drying process takes some time, and when forming uneven parts, the drying state due to heat varies in each part, making it difficult to manufacture various shapes of uniform shape.
[0008] According to the present invention, protrusions are formed on the surface of a roll press, and a polymer electrolyte membrane that does not have a concave-convex portion is passed between upper and lower rolls, and the concave-convex portion is formed on one or both sides of the polymer electrolyte membrane by pressing the protrusions. The number of concave-convex portions of the polymer electrolyte membrane may vary depending on the type of roll press. The thickness of the polymer electrolyte membrane before the unevenness is formed may be, for example, 5 to 20 μm, although the thickness of the polymer electrolyte membrane may be varied depending on the purpose. The polymer electrolyte membrane 10 may include an ion conductor. The ion conductor may be one selected from the group consisting of a fluorine-based ionomer, a hydrocarbon-based ionomer, and a mixture thereof. A detailed description thereof will be given later since it overlaps with the first ionomer and the second ionomer described later. The catalyst layer 20 according to the present invention may be disposed on the polymer electrolyte membrane 10. Specifically, the catalyst layer 20 may include a first catalyst layer 20a filling the inside of the uneven portion 15 and a second catalyst layer 20b disposed on the polymer electrolyte membrane 10. The first catalyst layer 20a may be interposed between the polymer electrolyte membrane 10 and the second catalyst layer 20b. The first catalyst layer 20a may comprise a first ionomer acting as a binder, and the second catalyst layer 20b may comprise a second ionomer acting as a binder. Specifically, the first ionomer may be the same as or different from the second ionomer, for example, the weight of the first ionomer relative to the total weight of the first catalyst layer may be the same as or different from the weight of the second ionomer relative to the total weight of the second catalyst layer.
[0009] Preferably, the weight of the first ionomer relative to the total weight of the first catalyst layer can be greater than the weight of the second ionomer relative to the total weight of the second catalyst layer. For example, the weight of the first ionomer relative to the total weight of the first catalyst layer can be greater than 35 wt %, and the weight of the second ionomer relative to the total weight of the second catalyst layer can be less than 35 wt %. In the past, when a catalyst layer was formed by coating one type of catalyst slurry on both sides of a polymer electrolyte membrane having a concave-convex portion and then drying it, there was a problem that the adhesion at the interface between the polymer electrolyte membrane and the catalyst layer was low due to the adhesion between the flat surfaces, and the chemical and mechanical durability was not improved overall. According to the present invention, the chemical and mechanical durability of the interface can be improved by forming the concave-convex portion, forming a first catalyst layer having a high ionomer content on the concave-convex portion, and then forming a second catalyst layer. By increasing the weight of the first ionomer compared to the weight of the second ionomer, the interfacial adhesion between the polymer electrolyte membrane and the catalyst layer can be increased and the durability between the catalyst layers can be improved overall. In addition, by reducing the ionomer content of the second catalyst layer, a performance improvement effect can be obtained through smooth material transfer. The first ionomer and the second ionomer can each independently be any one selected from the group consisting of a hydrocarbon-based ionomer, a fluorine-based ionomer, and a mixture thereof. The fluorine-based ionomer may be a fluorine-based polymer containing fluorine in the main chain having a cation exchange group or an anion exchange group, or a partially fluorinated polymer such as polystyrene-graft-ethylene tetrafluoroethylene copolymer, polystyrene-graft-polytetrafluoroethylene copolymer, etc. The fluorine-based ionomer may be a fluorine-based polymer including, for example, poly(perfluorosulfonic acid), poly(purple sulfuric acid), a copolymer of tetrafluoroethylene and fluorovinyl ether containing a sulfonic acid group, and defluorinated sulfurized polyether ketone, or a mixture thereof.
[0010] The cation exchange group is a functional group capable of transferring cations such as hydrogen ions, and may be, for example, an acidic group such as a sulfonic acid group, a carboxyl group, a boronic acid group, a phosphate group, an imide group, a sulfonimide group, or a sulfonamide group, and may generally be a sulfonic acid group or a carboxyl group. The anion exchange group is a polymer capable of transporting anions such as hydroxide ions, carbonate ions, or bicarbonate ions. The anion exchange group is commercially available in the form of hydroxide or halide (generally chloride). The anion exchange group can be used in industrial water purification, metal separation, catalytic processes, and the like. The polymer containing the anion exchange group may generally be a polymer doped with a metal hydroxide. Specifically, poly(ether sulfone), polystyrene, vinyl polymer, poly(vinyl chloride), poly(vinylidene fluoride), poly(tetrafluoroethylene), poly(benzimidazole), or poly(ethylene glycol) doped with a metal hydroxide may be used. The hydrocarbon ionomer may be a hydrocarbon polymer having a cation exchange group or an anion exchange group. For example, the hydrocarbon polymer may be a hydrocarbon polymer having at least one selected from the group consisting of imidazole, benzimidazole, polyamide, polyamideimide, polyimide, polyacetal, polyethylene, polypropylene, acrylic resin, polyester, polysulfone, polyether, polyetherimide, polyester, polyethersulfone, polyetherimide, polycarbonate, polystyrene, polyphenylene sulfide, polyetheretherketone, polyetherketone, polyarylethersulfone, polyphosphazene, and polyphenylquinoxaline in the main chain. The hydrocarbon ionomer may be a sulfonated polyimide (S-PI), a sulfonated polyarylethersulfone (S-PAES), a sulfonated polyetheretherketone (S-PEEK), a sulfonated polybenzimidazole (S-PBI), a sulfonated polysulfone (S-PSU), a sulfonated polystyrene (S-PS), a sulfonated polyphosphazene, a sulfonated polyquinoxaline, a sulfonated polyketone, a sulfonated polyphenylene oxide, a sulfonated polyethersulfone ... sulfone, sulfonated polyether ketone, sulfonated polyphenylene sulfone, sulfonated polyphenylene sulfide, sulfonated polyphenylene sulfide sulfone, sulfonated polyphenylene sulfide sulfone nitrile, sulfonated polyarylene ether, sulfonated polyarylene ether nitrilenitrile, sulfonated polyarylene ether ether nitrile, sulfonated polyarylene ether sulfone ketone, and a hydrocarbon polymer including a mixture thereof, but the technical idea of the present invention is not limited thereto.
[0011] The catalyst layer 20 according to the present invention may be made of any material that can be used as a catalyst in the hydrogen gas oxidation reaction and / or the oxygen gas reduction reaction, and preferably, a platinum-based metal or a non-platinum-based metal can be used. The platinum-based metal may be platinum (Pt) and / or a Pt-M alloy, where M may be any one selected from the group consisting of palladium (Pd), ruthenium (Ru), iridium (Ir), osmium (Os), gallium (Ga), titanium (Ti), vanadium (V), chromium (Cr), manganese (Mn), iron (Fe), cobalt (Co), nickel (Ni), copper (Cu), silver (Ag), gold (Au), zinc (Zn), tin (Sn), molybdenum (Mo), tungsten (W), lanthanum (La), and rhodium (Rh). Specifically, the Pt-M alloy may be Pt-Pd, Pt-Sn, Pt-Mo, Pt-Cr, Pt-W, Pt-Ru, Pt-Ni, Pt-Co, Pt-Y, Pt-Ru-W, Pt-Ru-Ni, Pt-Ru-Mo, Pt-Ru-Rh-Ni, Pt-Ru-Sn-W, Pt-Ru-Ir-Ni, Pt-Co-Mn, Pt-Co-Ni, Pt-Co-Fe, Pt-Co-Ir, Pt-Co-S, Pt-Co-P, Pt-Fe, Pt-Fe-Ir, Pt-Fe-S, Pt-Fe-P, Pt-Au-Co, Pt-Au-Fe, Pt-Au-Ni, Pt-Ni, Pt-Ni-Ir, Pt-Cr, Pt-Cr-Ir, or a mixture of two or more of these. The non-platinum based metal may be one selected from the group consisting of palladium (Pd), ruthenium (Ru), iridium (Ir), osmium (Os), and non-platinum based alloys. The non-platinum alloy may be Ir-Fe, Ir-Ru, Ir-Os, Co-Fe, Co-Ru, Co-Os, Rh-Fe, Rh-Ru, Rh-Os, Ir-Ru-Fe, Ir-Ru-Os, Rh-Ru-Fe, Rh-Ru-Os, Fe-N, Fe-P, Co-N, or a mixture of two or more of these. Catalyst layer 20 according to yet another embodiment of the present invention may include a catalyst in which metal nanoparticles fill the surface or internal pores of the support. The support can be, for example, a carbon-based support, a porous inorganic oxide such as zirconia, alumina, titania, silica, ceria, or a zeolite.
[0012] The carbon-based support may be selected from graphite, Super P, carbon fiber, carbon sheet, carbon black, Ketjen black, Denka black, acetylene black, carbon nanotube (CNT), carbon sphere, carbon ribbon, fullerene, activated carbon, carbon nanofiber, carbon nanowire, carbon nanoball, carbon nanohorn, carbon nanocage, carbon nanoring, ordered nano / mesoporous carbon, carbon aerogel, mesoporous carbon, graphene, stabilized carbon, activated carbon, and combinations of one or more thereof, but is not limited thereto, and any support available in the art may be used without limitation. The surface area of the carrier is 50 m2 / g or more, and the average particle size is preferably 10 to 300 nm. If the surface area of the support is less than the above range, it is not possible to obtain a uniform distribution of metal particles. FIG. 2 is an enlarged cross-sectional view of the uneven portion of FIG. As shown in FIG. 2, the first catalyst layer 20a according to the present invention can completely fill the entire volume of the first recess. The first catalyst layer 20a may include a first center portion cp and a side wall portion swp. The side wall portion swp may refer to members on both sides of the first center portion cp. Specifically, the side wall portion swp may include a first side wall portion swp1 and a second side wall portion swp2 that are disposed opposite each other with the first center portion cp in between. The first side wall portion swp1 may have a first side surface ss1 and a first curved surface cs1 extending from the first side surface ss1 to an upper surface cpus of the first central portion cp. Since the catalyst layer disposed on the polymer electrolyte membrane in the process of forming the first catalyst layer has an overall concave shape due to the influence of surface tension, etc., the first curved surface cs1 may be necessarily formed. The upper surface cpus of the first central portion cp may be, for example, a flat surface. The second side wall portion swp2 may include a second side surface ss2 and a second curved surface cs2 extending from the second side surface ss2 to an upper surface cpus of the first central portion cp. Since the catalyst layer disposed on the polymer electrolyte membrane in the process of forming the first catalyst layer generally has a concave shape due to the influence of surface tension, etc., the second curved surface cs2 may be necessarily formed.
[0013] The first center portion cp and the side wall portion swp may be in contact with the polymer electrolyte membrane 10. Specifically, the first center portion cp and the side wall portion swp may be disposed directly on the polymer electrolyte membrane 10. The thickness H of the first central portion cp may be more than 0 μm and less than 1 μm, and preferably 0.1 to 0.9 μm. If the thickness H of the first central portion cp exceeds the above numerical range, problems may occur in that the interface durability and interface bonding performance are reduced. The minimum thickness I of the first side wall portion swp1 may be more than 0 and less than 0.8 times the thickness H of the first central portion, and preferably more than 0 and less than 0.5 times the thickness H of the first central portion. If the minimum thickness I of the first side wall portion swp1 is less than the above numerical range, problems may occur in that the bending of the unevenness is weak and the interfacial bonding force is reduced, resulting in reduced durability, and if it exceeds the above numerical range, problems may occur in that the thickness H exceeds 1 μm, resulting in reduced interfacial durability and interfacial bonding force performance. The maximum width B of the first side wall portion swp1 may be less than 0.2 times, and preferably 0.02 to 0.18 times, the width A between the first side surface ss1 and the second side surface ss2. If the maximum width B of the first side wall portion swp1 exceeds the above numerical range, problems may occur in that the curvature of the unevenness is weak, the interfacial bonding strength is reduced, and durability is reduced. The curvature R of the first curved surface cs1 may be equal to or less than the difference HI between the thickness H of the first central portion and the minimum thickness I of the first sidewall portion. If the curvature of the first curved surface cs1 exceeds the difference HI between the thickness H of the first central portion and the minimum thickness I of the first sidewall portion, the maximum width B of the first sidewall portion swp1 becomes large, the bending of the unevenness is weak, and the interface bonding strength decreases, resulting in a problem of reduced durability. The curvature of the first curved surface cs1 may be measured, for example, by a method of comparing a circle having a radius equal to the maximum width B of the first sidewall portion swp1 with a circle having a radius equal to the difference HI between the thickness H of the first central portion cp and the minimum thickness I of the first sidewall portion swp1. That is, the curvature can be calculated by calculating the inverse of the curvature radii defined by the two circles. For example, the thickness H of the first central portion cp, the minimum thickness I of the first side wall portion swp1, the maximum width B of the first side wall portion swp1, and the curvature R of the first curved surface cs1 can all be measured or calculated through cross-sectional analysis using a scanning electron microscope (SEM).
[0014] Unlike that shown in FIG. 1, according to another embodiment of the present invention, the first catalyst layer 20a may fill the entire volume of the first recess and may extend to a part of the upper surface of the first protrusion disposed on one side of the first recess. Therefore, the width A between the first side ss1 and the second side ss2 may be 90 to 110% based on the electrode active area of the individual unevenness portion, and preferably 95 to 105%. If the width A between the first side ss1 and the second side ss2 is out of the above numerical range, the first catalyst layer may not fill the unevenness by 80% or more, or may fill it by more than 120%, so that the interface durability may not be improved, and the specific gravity of the second catalyst layer may be reduced, resulting in a deterioration in performance. For example, the width A between the first side ss1 and the second side ss2 may be measured through a cross-sectional analysis using a scanning electron microscope (SEM). According to yet another embodiment of the present invention, the first catalyst layer 20a may further include a functional additive. The functional additive may include any one selected from the group consisting of a radical scavenger, a heat dissipating material, a chelating agent, a hygroscopic material, and combinations thereof, and preferably includes all of them. The content of the functional additive is preferably 5 to 67 wt % based on the total solid content of the first catalyst layer. If the content of the functional additive is less than the above range, the heat dissipation effect and the oxygen radical scavenging effect may not be sufficiently improved, and if it exceeds the above range, the coating operation of the catalyst slurry may not be easy. The radical scavenger may be, for example, any one selected from the group consisting of transition metals, transition metal ions, transition metal oxides, transition metal complexes, noble metals, noble metal ions, noble metal oxides, noble metal complexes, and combinations thereof. However, the technical idea of the present invention is not limited thereto, and any particulate form capable of capturing oxygen radicals may be applied. The transition metal may be any one selected from the group consisting of cerium (Ce), manganese (Mn), tungsten (W), cobalt (Co), vanadium (V), nickel (Ni), chromium (Cr), zirconium (Zr), yttrium (Y), iridium (Ir), iron (Fe), titanium (Ti), molybdenum (Mo), lanthanum (La), and neodymium (Nd). The noble metal may be any one selected from the group consisting of silver (Ag), platinum (Pt), ruthenium (Ru), palladium (Pd), and rhodium (Rh). The first catalyst layer according to the present invention includes a radical scavenger, which can effectively capture oxygen radicals generated during fuel cell operation, thereby effectively preventing the oxygen radicals from changing the structure of the ion conductor compound that corresponds to the hydrogen ion channel.
[0015] The heat dissipation material may be, for example, h-BN (hexagonal-Boron Nitride), AlN, Al2O3, TiO2, ZnO, ZrO, SiO2, etc. The heat dissipation material can improve the performance of the fuel cell by dissipating heat generated during operation of the fuel cell to the outside. The chelating agent can be, for example, citric acid, which has the purpose of capturing dissolved metal ions and can have the effect of improving durability. The hygroscopic material may be, for example, an acrylic resin having acrylic acid as a monomer or a silicate compound. The first catalyst layer according to the present invention may have an effect of improving low humidification performance by including the hygroscopic material. 3 is a cross-sectional view showing a membrane-electrode assembly according to another embodiment of the present invention. The repeated explanations of the above-mentioned parts will be briefly explained or omitted. 3, a first catalyst layer 20a according to the present invention can be disposed on the surface of the first convex portion while filling the inside of the concave-convex portion 15. The thickness of the first catalyst layer disposed on the surface of the first convex portion is preferably within 1 μm. The second catalyst layer 20b can be interposed between a part and a different part of the first catalyst layer 20a arranged on the surface of the first convex portion. In other words, the second catalyst layer 20b can be inserted between the storage spaces defined by the first catalyst layers. The storage spaces are defined as between a part and a different part of the first catalyst layer 20a arranged on the surface of the first convex portion. In the membrane-electrode assembly according to the present invention, the first catalyst layer 20a is disposed on the surface of the first protrusion, so that the interfacial adhesion between the polymer electrolyte membrane and the catalyst layer can be further improved, thereby improving the durability of the membrane-electrode assembly. 4 is a cross-sectional view showing a membrane-electrode assembly according to another embodiment of the present invention. The repeated explanations of the above-mentioned parts will be briefly explained or omitted. As shown in FIG. 4, the first catalyst layer 20a according to the present invention may be disposed directly above the polymer electrolyte membrane 10, and more specifically, may be disposed on both the surfaces of the first recess and the first protrusion. The maximum thickness of the first catalyst layer 20a is preferably within 2 μm. In this specification, the "maximum thickness of the first catalyst layer 20a" is defined as the height from the surface where the first catalyst layer 20a and the polymer electrolyte membrane 10 contact each other to the surface where the first catalyst layer 20a and the second catalyst layer 20b contact each other.
[0016] 2.Fuel cell Yet another embodiment of the present invention provides a fuel cell comprising the membrane-electrode assembly. FIG. 5 is a schematic diagram illustrating a fuel cell according to still another embodiment of the present invention. As shown in FIG. 5, a fuel cell 200 according to the present invention may include a fuel supply unit 210 for supplying a mixed fuel obtained by mixing fuel and water, a reforming unit 220 for reforming the mixed fuel to generate a reformed gas containing hydrogen gas, a stack 230 for generating electrical energy by electrochemically reacting the reformed gas containing hydrogen gas supplied from the reforming unit 220 with an oxidant, and an oxidant supply unit 240 for supplying an oxidant to the reforming unit 220 and the stack 230. The stack 230 may include a plurality of unit cells that generate electrical energy by conducting an oxidation / reduction reaction between the reformed gas including hydrogen gas supplied from the reformer 220 and an oxidant supplied from the oxidant supplying unit 240. Each unit cell means a unit cell that generates electricity, and may include the membrane-electrode assembly that oxidizes / reduces oxygen in a reformed gas containing hydrogen gas and an oxidant, and a separator plate (also called a bipolar plate, hereinafter referred to as "separator plate") for supplying the reformed gas containing hydrogen gas and the oxidant to the membrane-electrode assembly. The separator plates are disposed on both sides of the membrane-electrode assembly. In this case, the separator plates located at the outermost sides of the stack are also referred to as end plates. Of the separation plates, the end plate may be provided with a pipe-shaped first supply pipe 231 for injecting the reformed gas containing hydrogen gas supplied from the reforming section 220, and a pipe-shaped second supply pipe 232 for injecting oxygen gas, and the other end plate may be provided with a first exhaust pipe 233 for discharging the reformed gas containing hydrogen gas that is ultimately left unreacted in the multiple unit cells to the outside, and a second exhaust pipe 234 for discharging the oxidant that is ultimately left unreacted in the unit cells to the outside. In the fuel cell, the separator, the fuel supply section, and the oxidant supply section constituting the electricity generating section are the same as those used in ordinary fuel cells, and therefore detailed description thereof will be omitted in this specification. Hereinafter, the embodiments of the present invention will be described in detail so that a person having ordinary skill in the art to which the present invention pertains can easily carry out the embodiments. However, this is merely an example, and the scope of the present invention is not limited to the following contents.
[0017] [Production Preparation Example 1: Production of Polymer Electrolyte Membrane] <Comparative Preparation Example 1: Production of a polymer electrolyte membrane without unevenness> A polymer electrolyte membrane was prepared by applying a polymer solution, which was a mixture of a solvent, in which water and isopropanol were mixed in a weight ratio of 1:1, and perfluorosulfonic acid, to a glass substrate using a doctor blade, and gradually increasing the temperature of the applied solution to 80°C and drying it for 4 hours. <Preparation Example 1: Production of polymer electrolyte membrane with unevenness> A polymer electrolyte membrane was manufactured by applying a polymer solution, which was a mixture of a solvent, in which water and isopropanol were mixed in a weight ratio of 1:1, and perfluorosulfonic acid, to a glass substrate using a doctor blade, and gradually increasing the temperature of the applied polymer solution to 80° C. and drying it for 4 hours. Thereafter, the glass substrate was removed, and a roll press (roll temperature: 120 to 160° C.) with concave and convex portions was used to press both sides of the polymer electrolyte membrane, thereby manufacturing a polymer electrolyte membrane having a first concave portion with a depth of 2 μm. [Production Example 1: Production of membrane-electrode assembly] When manufacturing the membrane-electrode assembly according to the embodiment, the volume of the first recess formed in the polymer electrolyte membrane according to Preparation Example 1 was calculated in advance, and the content of the catalyst slurry was adjusted. <Comparative Example 1-1: Membrane-electrode assembly manufactured using a polymer electrolyte membrane without unevenness> A catalyst slurry (3.5 mL) in which a commercial Pt / C catalyst from Tanaka and a binder (Nafion D-521) were mixed in a weight ratio of 1:0.48 was directly coated on both sides of the polymer electrolyte membrane of Comparative Preparation Example 1, and then dried at 80° C. for 5 minutes to prepare a membrane-electrode assembly. <Comparative Example 1-2: Membrane-electrode assembly manufactured using a polymer electrolyte membrane having uneven portions, in which a catalyst layer is formed using only one type of catalyst slurry> A first catalyst layer was formed by coating both sides of the polymer electrolyte membrane of Preparation Example 1 with a first catalyst slurry (3.5 mL) in which a commercial Pt / C catalyst from Tanaka and a first ionomer (Nafion D-521) were mixed in a weight ratio of 1:0.48. <Example 1-1: Membrane-electrode assembly in which the first catalyst layer fills 80% or more of the total volume of the first recess> A first catalyst slurry (0.7 mL) in which Tanaka's commercial Pt / C catalyst and a first ionomer (Nafion D-521) were mixed in a weight ratio of 1:0.56 was coated on both sides of the polymer electrolyte membrane according to Preparation Example 1, and then dried at 80° C. for 2 minutes to adjust the first catalyst layer to be filled with 90% (v / v) of the total volume of the first recess. Then, a second catalyst slurry (3.0 mL) in which a commercial Pt / C catalyst and a second ionomer (Nafion D-521) were mixed in a weight ratio of 1:0.48 was directly coated on the remaining 10% (v / v) of the first recess and on the surface of the first protrusions alternately arranged with the first recesses by a slot-die method. Then, the coated second catalyst slurry was dried at 80° C. for 4 minutes to form a second catalyst layer. <Example 1-2: Different from Example 1-1, but with the same binder content> A membrane-electrode assembly was prepared in the same manner as in Example 1-1, except that the first catalyst slurry and the second catalyst slurry were prepared by mixing a commercial Pt / C catalyst and an ionomer (Nafion D-521) in a weight ratio of 1:3. <Example 1-3: Different from Example 1-1, in which the binder type is a hydrocarbon-based ionomer> A membrane-electrode assembly was manufactured in the same manner as in Example 1-1, but as the first catalyst slurry and the second catalyst slurry, sulfonated poly(arylene ether sulfone); sPAES; sulfonation degree 17%, which is a hydrocarbon-based ionomer, was used instead of the fluorine-based ionomer (Nafion D-521). <Example 1-4: When the first catalyst slurry contains a functional additive> A membrane-electrode assembly was prepared in the same manner as in Example 1-1, but a catalyst slurry was prepared in which 100 parts by weight of a first catalyst slurry in which a commercial Pt / C catalyst and a first ionomer (Nafion D-521) were mixed in a weight ratio of 1:3 based on the total weight of the first catalyst slurry, and 7 parts by weight of radical scavenger particles (CeO2) were mixed. <Example 2-1: Membrane-electrode assembly in which the first catalyst layer fills less than 80% of the total volume of the first recess> A membrane-electrode assembly was manufactured in the same manner as in Example 1-1, but the first catalyst slurry (0.59 mL) and the second catalyst slurry (3.11 mL) were used to adjust the first catalyst layer to be filled at 75% (v / v) based on the total volume of the first recess. <Example 3-1: Case where the first catalyst layer is completely filled based on the total volume of the first recess> A membrane-electrode assembly was manufactured in the same manner as in Example 1-1, but the first catalyst slurry (0.85 mL) was used and the first catalyst layer was adjusted to fill the entire volume of the first recess. Specifically, the thickness H of the first central portion constituting the first catalyst layer was 0.8 μm, the width A between the first side and the second side was 3 μm, the minimum value I of the thickness of the first sidewall was 0.3 μm, the maximum value B of the width of the first sidewall was 0.5 μm, and the curvature of the first curved surface was 0.4 μm. -1 It was adjusted so that Thereafter, the second catalyst slurry (2.85 mL) according to Example 1-1 was coated onto the first convex portion and the surface of the first catalyst layer to form a second catalyst layer having a thickness of 9 μm. <Example 4-1: Unlike Example 3-1, when parameters are not satisfied> A membrane-electrode assembly was produced in the same manner as in Example 3-1, but using the first catalyst slurry (1.0 mL) and the second catalyst slurry (2.7 mL), the thickness H of the first central portion constituting the first catalyst layer was 1.2 μm, the width A between the first side surface and the second side surface was 3 μm, the minimum value I of the thickness of the first side wall portion was 1.0 μm, the maximum value B of the width of the first side wall portion was 0.8 μm, and the curvature of the first curved surface was 0.3 μm. -1 It was adjusted so that
[0018] [Experimental Example 1: Evaluation of mechanical durability of membrane-electrode assembly] The chemical durability of the membrane-electrode assembly of Preparation Example 1 was evaluated according to the durability evaluation protocol of the U.S. Department of Energy (DOE). Specifically, to evaluate the chemical durability of the membrane-electrode assembly, wet-dry cycling was performed for 20,000 cycles under air / air conditions at 80° C. with repeated cycles of wet 2 minutes and dry 2 minutes, and then hydrogen gas crossover was measured. The measured values are shown in Table 1 below. [Table 1] Referring to Table 1, it can be seen that the amount of hydrogen gas permeating the polymer electrolyte membrane is significantly less in the Example than in the Comparative Example when the amount of hydrogen gas was measured at the cathode electrode. It can be inferred that the chemical durability of the membrane-electrode assembly is significantly improved according to an embodiment of the present invention, thereby extending the performance and lifespan of the fuel cell. Comparing Examples 1-1 and 1-2 in terms of the content of the ionomer acting as a binder, it can be seen that when the content of the ionomer in the first catalyst slurry is higher than the content of the ionomer in the second catalyst slurry, the amount of hydrogen gas permeating the polymer electrolyte membrane is significantly lower. Comparing Example 1-1 and Example 2-1 in terms of the amount of the first catalyst layer filled based on the total volume of the first recess, it can be inferred that when the first catalyst layer is filled to 80% (v / v) or more based on the total volume of the first recess, the amount of hydrogen gas permeating the polymer electrolyte membrane is significantly reduced, and chemical durability is significantly improved.
[0019] [Experimental Example 2: Photograph of the membrane-electrode assembly according to Example 1-1] FIG. 6 shows a photograph of the membrane-electrode assembly according to Example 1-1. As shown in FIG. 6, it can be inferred that the membrane-electrode assembly according to Example 1-1 was realized. Although the preferred embodiments of the present invention have been described in detail above, the scope of the present invention is not limited thereto, and various modifications and improvements made by those skilled in the art using the basic concept of the present invention defined in the following claims also fall within the scope of the present invention.
Claims
1. A polymer electrolyte membrane having an uneven portion on at least one surface; a catalyst layer disposed on the polymer electrolyte membrane; A membrane-electrode assembly comprising: The catalyst layer is A first catalyst layer filling the inside of the uneven portion; and a second catalyst layer disposed on the polymer electrolyte membrane; The first catalyst layer comprises: A membrane-electrode assembly interposed between the polymer electrolyte membrane and the second catalyst layer.
2. The first catalyst layer comprises: A first ionomer is provided, The second catalyst layer comprises: a second ionomer; The weight of the first ionomer relative to the total weight of the first catalyst layer is 2. The membrane-electrode assembly of claim 1, wherein the weight of the second ionomer relative to the total weight of the second catalyst layer is the same as or different from that of the first catalyst layer.
3. The weight of the first ionomer relative to the total weight of the first catalyst layer is 3. The membrane-electrode assembly according to claim 2, wherein the weight of said second ionomer is greater than the total weight of said second catalyst layer.
4. The weight of the first ionomer relative to the total weight of the first catalyst layer is more than 35 wt %; 4. The membrane-electrode assembly according to claim 3, wherein the weight of the second ionomer relative to the total weight of the second catalyst layer is less than 35% by weight.
5. The first ionomer and the second ionomer each independently comprise:
3. The membrane-electrode assembly according to claim 2, which is any one selected from the group consisting of a hydrocarbon-based ionomer, a fluorine-based ionomer, and a mixture thereof.
6. The uneven portion is A first recess; and a first protrusion arranged alternately with the first recess; The first catalyst layer comprises:
2. The membrane-electrode assembly according to claim 1, wherein the first recess is filled to 80% (v / v) or more based on the total volume of the first recess.
7. The first catalyst layer comprises: filling the entire volume of the first recess; The first catalyst layer comprises: A first central portion; and a sidewall portion including a first sidewall portion and a second sidewall portion disposed opposite each other across the first central portion; The first side wall portion is A first aspect and a first curved surface extending from the first side surface to a top surface of the first central portion; The second side wall portion is The second aspect; and 7. The membrane-electrode assembly of claim 6, further comprising a second curved surface extending from said second side surface to a top surface of said first central portion.
8. The thickness H of the first central portion is The membrane-electrode assembly according to claim 7, wherein the thickness is more than 0 μm and less than 1 μm.
9. The minimum value I of the thickness of the first side wall portion is 8. The membrane-electrode assembly according to claim 7, wherein the thickness H of the first central portion is greater than 0 and less than 0.8 times the thickness H of the first central portion.
10. The minimum value I of the thickness of the first side wall portion is 10. The membrane-electrode assembly according to claim 9, wherein the thickness H of the first central portion is greater than 0 and less than 0.5 times the thickness H of the first central portion.
11. The maximum width B of the first side wall portion is 8. The membrane-electrode assembly according to claim 7, wherein the width A between the first side and the second side is less than 0.2 times the width A.
12. The curvature R of the first curved surface is 8. The membrane-electrode assembly according to claim 7, wherein the difference between the thickness H of the first central portion and the minimum thickness I of the first sidewall portion is equal to or less than HI.
13. The first catalyst layer comprises: The membrane-electrode assembly of claim 2, further comprising a functional additive.
14. A fuel cell comprising the membrane-electrode assembly according to claim 1.
Citation Information
Patent Citations
Solid polymer electrolyte fuel cell and manufacturing method therefor
JP2008159426A
Membrane-electrode assembly for solid macromolecular fuel cells
JP2011228014A
Membrane-electrode assembly, solid polymer fuel cell, and fuel cell system
JP2012243442A