P-type laterally diffused metal oxide semiconductor device and method of manufacture thereof

A simplified method for manufacturing PLDMOS devices by forming specific doping regions and well structures addresses the complexity of PLDMOS manufacturing, enabling compatibility with NLDMOS processes and achieving high breakdown voltage for high-voltage integrated circuits.

JP2024544735AActive Publication Date: 2024-12-03SOUTHEAST UNIV +1
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024538146
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2022-02-25
Filing Date
2022-11-30
Publication Date
2024-12-03
Estimated Expiration
2042-11-30

AI Technical Summary

Technical Problem

The manufacturing process of P-type lateral diffusion metal oxide semiconductor (PLDMOS) devices is complex and not compatible with the standard N-type lateral diffusion metal oxide semiconductor (NLDMOS) process, complicating the production of high-voltage integrated circuits.

Method used

A method is developed to manufacture PLDMOS devices by forming an N-type buried layer, patterning a mask layer, implanting N-type and P-type ions through specific windows, and performing thermal annealing to create well regions and doping layers, simplifying the process and making it compatible with NLDMOS manufacturing.

Benefits of technology

The method simplifies the PLDMOS manufacturing process, reducing complexity and making it compatible with NLDMOS processes, while achieving high breakdown voltage suitable for high-voltage integrated circuits.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024544735000001_ABST
    Figure 2024544735000001_ABST
Patent Text Reader

Abstract

A method of manufacturing a P-type laterally diffused metal oxide semiconductor device includes the steps of forming an N-type buried layer (220) in a substrate (210), forming a P-type region (230) overlying the N-type buried layer (220), forming a mask layer (240) overlying the P-type region (230), patterning the mask layer (240) to form at least two implantation windows (241, 243, 245), performing N-type ion implantation through the at least two implantation windows (241, 243, 245) to form a high pressure N-well doped region (231) and a low pressure N-well doped region (233), forming an oxide layer (244), and at least one of the steps of: The method includes the steps of removing at least a portion of the mask layer (240), performing P-type ion implantation into the P-type region (230) to form a P-type doped region (234), diffusing the P-type doped region (234) by thermal annealing to form a drift region (236) and two P-type well regions (238), diffusing the high voltage N-well doped region (231) to form a high voltage N-type well region (235), diffusing the low voltage N-well doped region (233) to form a low voltage N-type well region (237), and forming a source doped region (252), a drain doped region (254), and a gate (260).
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to the technical field of semiconductor integrated circuits, in particular to P-type laterally diffused metal oxide semiconductor devices, and further to a method for fabricating P-type laterally diffused metal oxide semiconductor devices. [Background technology]

[0002] This application claims priority to a Chinese patent application bearing application number 2022101816543 and entitled "P-TYPE LATERAL DIFFUSED METAL OXIDE SEMICONDUCTOR DEVICE AND MANUFACTURING METHOD THEREOF," filed on February 25, 2022, the entire contents of which are hereby incorporated by reference into this application.

[0003] High-voltage integrated circuits are an important field of power electronics. They integrate high-voltage power devices, signal processing systems, peripheral interface circuits, protection circuits, detection circuits, etc. into one chip to not only improve the reliability and stability of the system, but also reduce the power consumption, volume, weight and cost of the system. In high-voltage integrated circuits, when the potential of the high-side circuit is high, a level shifting technology is required to transmit a low-voltage signal to the high-voltage part to drive the high-voltage side power device. The level shifting circuit is a bridge that connects high and low voltage circuits, and raises the low-voltage signal output by the dead zone generating circuit in the front stage to a high-voltage signal for use by the high-voltage circuit in the rear stage, preventing mutual crosstalk between the high and low voltage signals in the front and rear stages. The high-voltage power conversion device LDMOS is an important device in the level shifting circuit, and its gate terminal receives the signal of the low-side circuit and outputs the high-voltage signal through its drain terminal, so that the LDMOS needs to withstand the voltage of the high-side circuit. Breakdown voltage is one of the important parameters for evaluating LDMOS devices. Breakdown voltage is the maximum voltage that the drain end of an LDMOS can withstand when a high voltage is applied to the drain end and the gate and source are at zero potential. If the voltage at the drain end exceeds the breakdown voltage of the device, the device will experience avalanche breakdown, and if the device remains in avalanche breakdown for a long time, it will burn out. LDMOS has excellent switching characteristics and high breakdown voltage, so it is widely used in high voltage power integrated circuits.

[0004] PLDMOS is a kind of LDMOS, and has the excellent performance of LDMOS, while PLDMOS can simplify the complexity of power integrated circuits as a high-side driver and reduce the chip area. However, unlike the manufacturing process of normal NLDMOS, the manufacturing process flow of the exemplary PLDMOS is more complicated. Summary of the Invention [Problem to be solved by the invention]

[0005] According to some embodiments, a method for fabricating a P-type laterally diffused metal oxide semiconductor device is provided. [Means for solving the problem]

[0006] A method for manufacturing a P-type laterally diffused metal oxide semiconductor device includes: forming an N-type buried layer in a substrate, forming a P-type region overlying the N-type buried layer, and forming a mask layer overlying the P-type region; patterning the mask layer to form at least two implantation windows; performing N-type ion implantation through the at least two implantation windows to form a high-pressure N-well doped region and a low-pressure N-well doped region in the P-type region, the low-pressure N-well doped region having a doping concentration higher than a doping concentration of the high-pressure N-well doped region; forming an oxide layer on a surface of the P-type region at each implantation window; removing at least a portion of the mask layer; performing P-type ion implantation into the P-type region to form a P-type doped region; Diffusing the P-type doping region to form a drift region and two P-type well regions, diffusing the high-pressure N-well doping region to form a high-pressure N-type well region, and diffusing the low-pressure N-well doping region to form a low-pressure N-type well region by thermal annealing, wherein the drift region is located between the high-pressure N-type well region and the low-pressure N-type well region, the two P-type well regions are located on both sides of the high-pressure N-type well region, and one of the P-type well regions is located between the high-pressure N-type well region and the drift region; forming a source doped region, a drain doped region and a gate, the source doped region being located in the low voltage N-type well region, the drain doped region being located in the P-type well region and between the high voltage N-type well region and the drift region, the gate being located between the source doped region and the drain doped region, and the source doped region and the drain doped region having P-type doping.

[0007] A P-type laterally diffused metal oxide semiconductor device includes a substrate, an N-type buried layer, a P-type region, a high-voltage N-type well region, a low-voltage N-type well region, a drift region and two P-type well regions, a field effect oxide layer, a gate, a body region and a source doping region, a substrate pull-out region, and a drain doping region; the N-type buried layer is provided in the substrate, the P-type region is provided on the N-type buried layer and the substrate, the high-voltage N-type well region, the low-voltage N-type well region, the drift region, and the two P-type well regions are provided within the P-type region; the field effect oxide layer is disposed on the P-type region; the gate is located on the low voltage N-type well region and the field effect oxide layer; the body region and the source doping region are disposed within the low voltage N-type well region, the body region is connected to a body region metal electrode, the source doping region is located between the gate and the body region and is connected to a source metal electrode; the substrate pull-out region is provided in one of the P-type well regions and is connected to a metal electrode of the substrate pull-out region; The drain doping region is provided in the other of the P-type well regions, and is located between the high voltage N-type well region and the drift region, and is connected to a drain metal electrode.

[0008] The details of one or more embodiments of the application are set forth in the accompanying drawings and the description below. Other features, objects, and advantages of the application will become apparent from the description, drawings, and claims. [Brief description of the drawings]

[0009] To better describe and explain the embodiments and / or examples of the invention disclosed herein, reference may be made to one or more drawings. Additional details or examples used to illustrate the drawings should not be construed as limiting the scope of the disclosed invention, either of the currently described embodiments and / or examples, or the currently understood best mode of such invention. [Figure 1] 1 is a flow chart illustrating a method for manufacturing a P-type laterally diffused metal oxide semiconductor device in one embodiment. [Figure 2a] 11 is a schematic cross-sectional view showing the configuration of a device after completion of step S120 in one embodiment. FIG. [Figure 2b] FIG. 11 is a schematic cross-sectional view showing the configuration of a device after the first step of injection in step S130 in one embodiment is completed. [Figure 2c] FIG. 11 is a schematic cross-sectional view showing the configuration of a device after the second step of injection in step S130 is completed in one embodiment. [Figure 2d] FIG. 11 is a schematic cross-sectional view showing the configuration of the device after completion of step S140 in one embodiment. [Figure 2e] FIG. 11 is a schematic cross-sectional view showing the configuration of the device after completion of step S160 in one embodiment. [Figure 2f] FIG. 11 is a schematic diagram showing the configuration of a drift region, a P-type well region, a high-voltage N-type well region, and a low-voltage N-type well region after a second thermal annealing in one embodiment. [Diagram 3] FIG. 2 is a schematic cross-sectional view of a P-type laterally diffused metal oxide semiconductor device according to one embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] In order to facilitate an understanding of the present invention, the present invention will now be more fully described with reference to the accompanying drawings, in which preferred embodiments of the present invention are illustrated. However, the present invention may be embodied in many different forms and is not limited to the embodiments set forth herein. Rather, these embodiments are provided to provide a more thorough and complete understanding of the present invention.

[0011] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this invention belongs. The terms used herein are for the purpose of describing specific examples only and are not intended to limit the invention. The term "and / or" used herein includes any and all combinations of one or more of the associated listed items.

[0012] When an element or layer is referred to as being "located on," "adjacent to," "connected to," or "coupled" with another element or layer, it is understood that it may be directly located on, adjacent to, connected to, or coupled with the other element or layer, or that there may be intervening elements or layers. In contrast, when an element is referred to as being "located directly on," "directly adjacent to," "directly connected to," or "directly coupled" with another element or layer, there are no intervening elements or layers. Terms such as first, second, third, etc. may be used to describe various elements, members, regions, layers, and / or portions, but it is understood that these elements, members, regions, layers, and / or portions should not be limited by these terms. These terms are used only to distinguish one element, member, region, layer, or portion from another element, member, region, layer, or portion. Thus, a first element, member, region, layer, or portion described below may be referred to as a second element, member, region, layer, or portion without departing from the teachings of the present invention.

[0013] Spatial relationship terms such as "below," "downward," "below," "below," "above," "above" and the like may be used herein to describe the relationship of one element or feature to another element or feature shown in the figures for ease of description. It should be understood that the spatial relationship terms are intended to encompass different orientations of the device in use and operation in addition to the orientation shown in the figures. For example, if the device in the figures were turned over, an element or feature described as "below" or "downward" or "below" the other element would be oriented "above" the other element or feature. Thus, the exemplary terms "downward" and "below" can include both an above and below orientation. The device may be oriented differently (rotated 90 degrees or at other orientations) and the spatial descriptors used herein may be interpreted accordingly.

[0014] The terms used herein are for the purpose of describing particular embodiments only and are not intended to be limiting of the present invention. As used herein, the singular forms "a", "one", and "said" are intended to include the plural unless the context clearly indicates otherwise. It is further understood that the terms "comprising" and / or "including" as used herein specify the presence of stated features, integers, steps, operations, elements and / or components, but do not preclude the presence or addition of one or more other features, integers, steps, operations, elements, components and / or groups. As used herein, the term "and / or" includes any and all combinations of the associated listed items.

[0015] Embodiments of the present invention are described herein with reference to cross-sectional views that are schematic illustrations of idealized embodiments (and intermediate structures) of the present invention. Thus, variations from the shapes depicted due to, for example, manufacturing techniques and / or tolerances, can be expected. Thus, embodiments of the present invention should not be limited to the particular shapes of regions depicted herein, but should include, for example, deviations in shapes due to manufacturing. For example, an implanted region depicted as a rectangle typically has rounded or curved features and / or implant concentration gradients at its edges, rather than a binary change from implanted to non-implanted regions. Similarly, buried regions formed by implantation may result in some implantation in the region between the buried region and the surface where the implantation occurs. Thus, the regions depicted in the drawings are schematic in nature, and their shapes are not intended to represent the actual shape of a region of a device, and are not intended to limit the scope of the present invention.

[0016] The terms in the semiconductor field used in this specification are technical terms commonly used by those skilled in the art. For example, for P-type and N-type impurities, in order to distinguish the doping concentration, P+ type represents P-type with a high doping concentration, P-type represents P-type with a medium doping concentration, P-type represents P-type with a low doping concentration, N+ type represents N-type with a high doping concentration, N-type represents N-type with a medium doping concentration, and N-type represents N-type with a low doping concentration.

[0017] In order to simplify the manufacturing process of PLDMOS and make it compatible with the manufacturing process of NLDMOS, according to one embodiment, a method for manufacturing a P-type laterally diffused metal oxide semiconductor device is proposed. Referring to FIG. 1, the method includes the following steps:

[0018] In step S110, an N-type buried layer is formed in a substrate, a P-type region located in the N-type buried layer is formed, and a mask layer is formed in the P-type region.

[0019] Referring to FIG. 2a, in one embodiment of the present application, the substrate 210 is a semiconductor substrate, the material of which can be undoped single crystal silicon, impurity doped single crystal silicon, silicon-on-insulator (SOI), stacked silicon-on-insulator (SSOI), stacked silicon-germanium-on-insulator (S-SiGeOI), silicon-germanium-on-insulator (SiGeOI) and germanium-on-insulator (GeOI), etc. In the embodiment shown in FIG. 2a, the material of the substrate 210 is single crystal silicon, i.e., a P-type silicon substrate. An N-type buried layer 220 is provided in the substrate 210. A P-type region 230 is located on the N-type buried layer 220. The P-type region 230 can be formed in an epitaxial manner or a non-epitaxial manner (for one complete substrate, implant a buried layer DN and then implant P to form a P doping region). The mask layer 240 is located on the P-type region 230 and includes a silicon oxide layer 246 and a silicon nitride layer 248 on the silicon oxide layer 246. Specifically, the material of the silicon oxide layer 246 may be silicon dioxide, and the material of the silicon nitride layer 248 may be silicon nitride.

[0020] In one embodiment, an N-type buried layer 220 may first be formed in a substrate 210, a P-type region 230 may then be formed on the N-type buried layer 220, and a silicon oxide layer 246 and a silicon nitride layer 248 may be deposited on the P-type region 230 to form a mask layer 240.

[0021] In step S120, the mask layer is patterned to form at least two implantation windows.

[0022] In one embodiment, a photoresist is applied to the mask layer 240, and the photoresist is exposed and developed by an N-well photomask to obtain a photoresist layer 292 as shown in FIG. 2a. Then, the mask layer 240 is etched using the photoresist layer 292 as an etching barrier layer to remove excess mask layer 240 to form a plurality of implantation windows as shown in FIG. 2a. The plurality of implantation windows includes a high-pressure N-well implantation window 241 and a low-pressure N-well implantation window 243, and may further include a plurality of N-type ion implantation windows 245 located between the high-pressure N-well implantation window 241 and the low-pressure N-well implantation window 243. Referring to FIG. 2a, in one embodiment, the interval d between adjacent windows of the plurality of N-type ion implantation windows 245 is 1.0 to 2.0 μm, and the width w of each N-type ion implantation window 245 is 2.0 to 4.0 μm.

[0023] In one embodiment, a thin oxide layer 242 is further formed on the surface of P-type region 230 at each implantation window.

[0024] In step S130, N-type ion implantation is performed through the plurality of implantation windows to form a high-voltage N-well doped region and a low-voltage N-well doped region in the P-type region.

[0025] In one embodiment, the N-type ion implantation in step S130 is a two-step implantation. Referring to FIG. 2b, the first N-type ion implantation forms high-pressure N-well doping regions 231 in the P-type regions 230 below each implantation window. Then, the photoresist layer 292 is removed, photoresist is applied again, and the photoresist is exposed by a low-pressure N-well photomask. The exposed photoresist layer covers the high-pressure N-well implantation window 241 and each N-type ion implantation window, but exposes the low-pressure N-well implantation window 243. As shown in FIG. 2c, the second N-type ion implantation is performed in the lower P-type region 230 through the low-pressure N-well implantation window 243, and the N-type ions implanted in the first step are overlapped to form the low-pressure N-well doping region 233. In one embodiment, the dose of the N-type ion implantation of the second implantation is higher than the dose of the N-type ion implantation of the first implantation, so that the doping concentration of the low-pressure N-well doped region 233 is higher than the doping concentration of the high-pressure N-well doped region 231.

[0026] 2b, in this embodiment, a first implant forms drift region doping adjustment regions 232 beneath each N-type ion implantation window 245. The N-type doped drift region doping adjustment regions 232 can adjust the doping concentration of the drift region formed in a subsequent step.

[0027] In one embodiment, the ion source for the two N-type ion implants of step S130 is phosphorous.

[0028] In step S140, an oxide layer is formed on the surface of the P-type region in each implantation window.

[0029] 2d, in one embodiment, the thin oxide layer 242 on the surface of the P-type regions 230 located in each implantation window is thickened to form oxide layer 244 by high temperature oxidation. The high temperature oxidation can be an oxygen-permeable thermal anneal or other high temperature oxygen-permeable process. The N-type ions implanted in step S130 diffuse during the anneal.

[0030] In step S150, at least a portion of the mask layer is removed.

[0031] In this step, a portion of the mask layer 240 is removed because a subsequent P-type ion implantation will be performed through the location of the mask layer 240. In one embodiment, in step S150, the silicon nitride layer 248 in the mask layer 240 is removed, leaving the silicon oxide layer 246.

[0032] In step S160, P-type ion implantation is performed into the P-type region to form a P-type doped region.

[0033] 2e, when P-type ions are implanted into P-type region 230, oxide layer 244 blocks the implantation of the P-type ions from the locations covered by silicon oxide layer 246 in the previous step to form P-type doped region 234. When the P-type ions diffuse to the areas of P-type region 230 where N-type ions were implanted, they are neutralized by the N-type ions.

[0034] In one embodiment, the ion source for the P-type ion implantation in step S160 is boron.

[0035] In step S170, thermal annealing is performed.

[0036] Referring to FIG. 2f, thermal annealing is performed again to promote the diffusion of the high-pressure N-well doping region 231, the low-pressure N-well doping region 233 and the P-type doping region 234, so that their bottoms reach the N-type buried layer 220. The high-pressure N-well doping region 231 forms a high-pressure N-type well region 235 after thermal annealing, and the low-pressure N-well doping region 233 forms a low-pressure N-type well region 237 after thermal annealing. The high-pressure N-type well region 235 and the low-pressure N-type well region 233 both contact the N-type buried layer 220. The P-type doping region 234 forms a drift region 236 and two P-type well regions 238 after thermal annealing. The two P-type well regions 238 are formed on both sides of the high-pressure N-type well region 235, respectively, and the drift region 236 is formed between the P-type well region 238 adjacent to the low-pressure N-type well region 237 and the low-pressure N-type well region 237. Since the doping adjustment region 232 of the N-type drift region is formed in advance in the region where the drift region 236 is located, in the process of forming the drift region 236 after the P-type doping region 234 is thermally annealed in step S170, the doping adjustment region 232 of the N-type drift region neutralizes some of the P-type ions of the drift region 236, so that the doping concentration of the drift region 236 is lower than that of the P-type well region 238. Note that, by making the dose of the P-type ion implantation in step S160 larger than the dose of the first N-type ion implantation in step S130, it can be effectively ensured that the P-type doping region 234 forms the P-type drift region 236 after the thermal annealing in step S170.

[0037] In one embodiment, the doping concentration of the high voltage N-well region 235 is lower than the doping concentration of the low voltage N-well region 237. The doping concentrations of the high voltage N-well region 235 and the low voltage N-well region 237 range from 1e 11 cm -2 ~1e 13 cm -2 It is.

[0038] In one embodiment, the doping concentration of the drift region 236 and the P-well region 238 ranges from 1e11 cm -2 ~1e 13 cm -2 It is.

[0039] In step S180, a source doping region, a drain doping region and a gate are formed.

[0040] 3, in one embodiment, a source doping region 252 is formed in the low voltage N-type well region 237 by photolithography and ion implantation processes. A drain doping region 254 is formed in the P-type well region 238 between the high voltage N-type well region 235 and the drift region 236 by photolithography and ion implantation processes. The source doping region 252 and the drain doping region 254 have P-type doping. Specifically, the source doping region 252 and the drain doping region 254 are P+ regions. A gate 260 is formed between the source doping region 252 and the drain doping region 254 by deposition, photolithography and etching processes.

[0041] In one embodiment, prior to forming the gate 260, the method further includes forming a field effect oxide layer 250 in the drift region 236. The gate 260, formed of polysilicon, extends above the field effect oxide layer 250 from an edge of the source doping region 252 toward the drain doping region 254.

[0042] In one embodiment, after step S180, the method further includes forming a source metal electrode S, a drain metal electrode D, and a gate metal electrode G. The source metal electrode S is located in the source doping region 252 and is electrically connected to the source doping region 252. The drain metal electrode D is located in the drain doping region 254 and is electrically connected to the drain doping region 254. The gate metal electrode G is located in the gate 260 and is electrically connected to the gate 260. A portion of the drain metal electrode D located above the field effect oxide layer 250 is a drain metal field plate, and a portion of the gate metal electrode G located above the field effect oxide layer 250 is a gate metal field plate.

[0043] In one embodiment, the method further includes forming a substrate pull-out region 256 and a body region 258. The substrate pull-out region 256 is formed in the P-type well region 238 on a side of the high-voltage N-type well region 235 away from the drift region 236, the substrate pull-out region 256 having a P-type doping. The body region 258 is formed in the low-voltage N-type well region 237, the body region 258 having an N-type doping. The source doping region 252 is located between the body region 258 and the drift region 236. In one embodiment of the present application, the substrate pull-out region 256 is a P+ region and the body region 258 is an N+ region.

[0044] In one embodiment, simultaneously with the step of forming the field effect oxide layer 250 described above, a field effect oxide layer 250 is formed on the surface of the drift region 236 between the substrate pull-out region 256 and the drain doping region 254, and a field effect oxide layer 250 is formed on the surface of the drift region 236 on both sides of the body region 258.

[0045] According to the above-mentioned method for manufacturing a P-type laterally diffused metal oxide semiconductor device, the patterned mask layer forms segmented implantation windows 245, and after N-type ion implantation, the surface of the implantation window is covered with an oxide layer 244, so that the oxide layer 244 can serve as a barrier layer during subsequent P-type ion implantation, so that the P-type ion implantation does not require a separate photomask, and the manufacturing process of a PLDMOS device can be effectively simplified and made compatible with the manufacturing process of an NLDMOS.

[0046] According to an embodiment, a P-type laterally diffused metal oxide semiconductor device (PLDMOS) applicable to a high-voltage integrated circuit with a breakdown voltage of 600V is further provided. The PLDMOS can be manufactured by the manufacturing method of the P-type laterally diffused metal oxide semiconductor device according to any of the above embodiments. Referring to FIG. 3, the PLDMOS includes a P-type substrate 210, an N-type buried layer 220 is provided in the substrate 210, and a P-type region is provided on the N-type buried layer 220 and the substrate 210. A high-voltage N-type well region 235, a low-voltage N-type well region 237, a P-type doped drift region 236, and a P-type well region 238 are provided in the P-type region. A field effect oxide layer 250 is provided on the P-type region, and a gate 260, specifically a polysilicon gate, is provided on the field effect oxide layer 250, and the gate 260 is located above the low-voltage N-type well region 237 and the field effect oxide layer 250. The low-voltage N-type well region 237 is provided with a cathode N-type heavily doped region (referred to as the body region 258) and a cathode P-type heavily doped region (referred to as the source doped region 252), and the body region 258 is connected to the metal electrode bulk of the body region. The source doped region 252 is located between the gate 260 and the body region 258, and is connected to the source metal electrode S. The P-type well region 238 is provided with an anode P-type heavily doped region (referred to as the substrate pull-out region 256), and the substrate pull-out region 256 is connected to the metal electrode Sub of the substrate pull-out region. The P-type well region 238 is provided with an anode P-type heavily doped region (referred to as the drain doped region 254), and the drain doped region 254 is located between the high-voltage N-type well region 235 and the drift region 236, and is connected to the drain metal electrode D.

[0047] 3, a first side of the drain front metal layer (i.e., drain metal electrode D) is located above the field effect oxide layer 250 between the drain doping region 254 and the substrate pull-out region 256, and a second side is located above the field effect oxide layer 250 on the drift region 236 and extends toward the drift region 236 to form a drain metal field plate. A first side of the gate front metal layer (i.e., gate metal electrode G) is located above the field effect oxide layer 250 on the drift region 236, and a second side is located above the gate 260, and a first side is extended above the drift region 236 to form a gate metal field plate.

[0048] Although the various steps in the flow charts of the present application are shown sequentially as indicated by the arrows, it should be understood that the steps are not necessarily performed sequentially in the order indicated by the arrows. Unless expressly stated herein, the steps do not have a strict order of execution and may be performed in other orders. Furthermore, at least some of the steps in the flow charts of the present application may include multiple steps or multiple stages, which are not necessarily performed simultaneously but may be performed at different times, and which are not necessarily performed sequentially but may be performed in order or alternating with other steps or at least some of the steps or stages in other steps.

[0049] The technical features of the above embodiments can be arbitrarily combined. For the sake of brevity, all possible combinations of the technical features of the above embodiments are not described, but as long as there is no contradiction in the combination of these technical features, they should all be considered within the scope of the present specification.

[0050] The above examples only show some embodiments of the present application, and the description is more specific and detailed, but this should not be understood as limiting the scope of protection of the patent. However, a person skilled in the art can make several modifications and improvements without departing from the concept of the present application, all of which are within the scope of protection of the present application. Therefore, the scope of protection of the patent of the present application should be based on the scope of the attached claims.

Claims

1. forming an N-type buried layer in a substrate, forming a P-type region overlying the N-type buried layer, and forming a mask layer overlying the P-type region; patterning the mask layer to form at least two implantation windows; performing N-type ion implantation through the at least two implantation windows to form a high-voltage N-well doped region and a low-voltage N-well doped region in the P-type region, the low-voltage N-well doped region having a doping concentration higher than a doping concentration of the high-voltage N-well doped region; forming an oxide layer on a surface of the P-type region at each of the implantation windows; removing at least a portion of the mask layer; performing P-type ion implantation into the P-type region to form a P-type doped region; Diffusing the P-type doping region to form a drift region and two P-type well regions, diffusing the high-pressure N-well doping region to form a high-pressure N-type well region, and diffusing the low-pressure N-well doping region to form a low-pressure N-type well region by thermal annealing, wherein the drift region is located between the high-pressure N-type well region and the low-pressure N-type well region, the two P-type well regions are located on both sides of the high-pressure N-type well region, and one of the P-type well regions is located between the high-pressure N-type well region and the drift region; forming a source doped region, a drain doped region and a gate, the source doped region being located in the low voltage N well region, the drain doped region being located in the P well region and between the high voltage N well region and the drift region, the gate being located between the source doped region and the drain doped region, and the source doped region and the drain doped region having P type doping.

2. the at least two implant windows include a high-pressure N-well implant window and a low-pressure N-well implant window; performing N-type ion implantation through each of the implantation windows to form the high-voltage N-well doped region and the low-voltage N-well doped region in the P-type region; performing a first N-type ion implantation through the high-voltage N-well implantation window and the low-voltage N-well implantation window to form the high-voltage N-well doping region; forming a photoresist layer over the P-type region, covering the high voltage N-well implant window and exposing the low voltage N-well implant window; 2. The method of claim 1, further comprising: implanting a second N-type ion through said low-voltage N-well implant window to form said low-voltage N-well doping region in said P-type region.

3. the at least two implantation windows further include a plurality of N-type ion implantation windows located between the high-voltage N-well implantation window and the low-voltage N-well implantation window; the first N-type ion implantation includes forming a corresponding number of N-type drift region doping adjustment regions in the P-type region through the plurality of N-type ion implantation windows; 3. The method of claim 2, wherein said photoresist layer covers said plurality of N-type ion implantation windows.

4. 4. The method of claim 3, wherein the spacing between adjacent ones of the plurality of N-type ion implantation windows is 1.0 to 2.0 μm.

5. 4. The method of claim 3, wherein the width of each N-type ion implantation window is between 2.0 and 4.0 μm.

6. 4. The method of claim 3, wherein the dose of the P-type ion implant is greater than the dose of the first N-type ion implant.

7. 2. The method of claim 1 , wherein the mask layer comprises a silicon dioxide layer and a silicon nitride layer overlying the silicon dioxide layer, and wherein removing at least a portion of the mask layer comprises removing the silicon nitride layer.

8. Prior to forming the gate, further comprising:

2. The method of claim 1, comprising forming a field effect oxide layer on the drift region, the field effect oxide layer being located between the source doped region and the drain doped region, the gate being a polysilicon gate, the polysilicon gate extending onto the field effect oxide layer.

9. forming a source metal electrode, a drain metal electrode and a gate metal electrode; 9. The method of claim 8, wherein the source metal electrode is located on and electrically connected to the source doping region, the drain metal electrode is located on and electrically connected to the drain doping region, the gate metal electrode is located on and electrically connected to the gate, a portion of the drain metal electrode located above a field effect oxide layer is a drain metal field plate, and a portion of the gate metal electrode located above the field effect oxide layer is a gate metal field plate.

10. forming a substrate pull-out region, the substrate pull-out region being formed in a P-type well region on a side of the high voltage N-type well region away from the drift region, the substrate pull-out region having a P-type doping; 2. The method of claim 1, further comprising forming a body region, the body region being formed in the low-voltage N-type well region, the body region having an N-type doping, and the source doping region being located between the body region and the drift region.

11. The N-type ion source for the N-type ion implantation is phosphorus, and the doping concentration is 1e 11 cm -2 ~1e 13 cm -2 The P-type ion source for the P-type ion implantation is boron, and the doping concentration is 1e 11 cm -2 ~1e 13 cm -2 2. The method of claim 1, wherein:

12. 2. The method of claim 1, wherein the drift region has a doping concentration lower than a doping concentration of the P-type well region.

13. 2. The method of claim 1, wherein the high voltage N-well region and the low voltage N-well region both contact the N-type buried layer.

14. 1. A P-type laterally diffused metal oxide semiconductor device comprising: The semiconductor device includes a substrate, an N-type buried layer, a P-type region, a high-voltage N-type well region, a low-voltage N-type well region, a drift region and two P-type well regions, a field effect oxide layer, a gate, a body region and a source doping region, a substrate pull-out region, and a drain doping region; the N-type buried layer is provided in the substrate, the P-type region is provided on the N-type buried layer and the substrate, the high-voltage N-type well region, the low-voltage N-type well region, the drift region, and the two P-type well regions are provided within the P-type region; the field effect oxide layer is disposed on the P-type region; the gate is located on the low voltage N-type well region and the field effect oxide layer; the body region and the source doping region are disposed within the low voltage N-type well region, the body region is connected to a metal electrode of the body region, and the source doping region is located between the gate and the body region and is connected to a source metal electrode; the substrate lead-out region is provided in one of the P-type well regions and is connected to a metal electrode of the substrate lead-out region; a drain doping region provided in the other of the P-type well regions, the drain doping region being located between the high voltage N-type well region and the drift region and connected to a drain metal electrode.

15. 15. The P-type laterally diffused metal oxide semiconductor device of claim 14, wherein the doping concentration of the drift region is less than the doping concentration of the P-type well region.

Citation Information

Patent Citations

  • Lateral double-diffused metal oxide semiconductor device

    CN112768521A

  • High-voltage P-type metal oxide transistor and producing method thereof

    CN1976057A

  • Semiconductor device and manufacture of silicon wafer

    JP1997307110A

  • Semiconductor device and manufacturing method of semiconductor device

    JP2017045884A