Copper foil, electrodes containing the same, a secondary battery containing the same, and a method for manufacturing the same.

Copper foil with a controlled GOS value is manufactured using a specific electrolytic process, addressing curling and tearing issues, thereby improving the production of high-capacity secondary batteries and related components.

JP2026116701APending Publication Date: 2026-07-10SK NEXILIS CO LTD

Patent Information

Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
SK NEXILIS CO LTD
Filing Date
2025-12-04
Publication Date
2026-07-10

AI Technical Summary

Technical Problem

The challenge of manufacturing thin copper foil for secondary batteries is the occurrence of curling, wrinkling, or tearing during the manufacturing process, which affects the production of high-capacity and high-quality batteries.

Method used

Copper foil with a room temperature GOS value between 4° to 12° is produced using a specific electrolytic process involving copper ions, sulfuric acid, chlorine, and organic additives, including a brightener, moderator, and roughness modifier, with a protective layer to prevent curling, wrinkling, or cracking.

Benefits of technology

The solution prevents defects during manufacturing, enhancing the productivity of intermediate components and final products like flexible printed circuit boards and secondary batteries by ensuring the copper foil's flexibility and stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2026116701000001_ABST
    Figure 2026116701000001_ABST
Patent Text Reader

Abstract

The present invention provides copper foil, an electrode containing the same, a secondary battery containing the same, and a method for manufacturing the same. [Solution] One embodiment of the present invention provides a copper foil comprising a copper film having a matte surface and a shiny surface, and a protective layer on the copper film, wherein the room temperature GOS value is in the range of 4° to 12°. The room temperature GOS value is measured at room temperature using an electron backscatter diffraction pattern analyzer (EBSD) on the cross-section of the copper foil.
Need to check novelty before this filing date? Find Prior Art