How to inspect for welding defects

The method improves welding defect detection in secondary batteries by measuring multiple strengths and establishing reference values to identify all types of defects, including weak ones, through a combination of tensile, torsional, and peel strength measurements.

JP7551207B2Active Publication Date: 2024-09-17LG ENERGY SOLUTION LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2022552350
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-08-21
Filing Date
2021-06-16
Publication Date
2024-09-17
Estimated Expiration
2041-06-16

AI Technical Summary

Technical Problem

Existing welding defect inspection methods primarily rely on tensile strength measurements, which are inadequate for detecting all types of welding defects, particularly weak and intermittent ones in secondary battery production.

Method used

A method that includes measuring tensile, torsional, and peel strengths of the welded portions between electrode tabs and leads, deriving correlations between these strengths and welding defects, and establishing reference values to detect all types of defects, including weak ones, by using a combination of ultrasonic and laser welding methods.

Benefits of technology

Enhances the reliability and accuracy of welding defect detection by confirming the correlation between multiple strength types and standardizing the detection process, enabling the identification of all weak-level weld defects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007551207000005
    Figure 0007551207000005
  • Figure 0007551207000002
    Figure 0007551207000002
  • Figure 0007551207000001
    Figure 0007551207000001
Patent Text Reader

Abstract

The present invention relates to a method for inspecting weld defects, and includes the steps of manufacturing a sample electrode assembly by welding an electrode lead to an electrode tab formed on the electrode assembly; measuring the tensile strength, torsional strength, and peel strength of the weld between the electrode tab and the electrode lead for the sample electrode assembly; deriving correlations between the tensile strength, torsional strength, and peel strength and the presence or absence of weld defects; and deriving reference values ​​for the tensile strength, torsional strength, and peel strength to determine the presence or absence of weld defects.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] This application claims the benefit of priority based on Korean Patent Application No. 10-2020-0105340, filed on August 21, 2020, and all contents disclosed in the documents of said Korean patent application are incorporated herein by reference.

[0002] The present invention relates to an inspection method for defective welding and a manufacturing method for a secondary battery including the same. [Background technology]

[0003] Recently, rechargeable secondary batteries have been widely used as energy sources for wireless mobile devices. Secondary batteries are also attracting attention as energy sources for electric vehicles and hybrid electric vehicles, which have been presented as a solution to air pollution caused by existing gasoline and diesel vehicles that use fossil fuels. Therefore, the types of applications using secondary batteries are becoming very diverse due to the advantages of secondary batteries, and it is expected that secondary batteries will be applied to more fields and products in the future.

[0004] Such secondary batteries may be classified into lithium ion batteries, lithium ion polymer batteries, lithium polymer batteries, etc. according to the configuration of the electrodes and electrolyte, and among them, the use of lithium ion polymer batteries, which are less likely to leak electrolyte and are easy to manufacture, is increasing. In general, secondary batteries are classified into cylindrical batteries and prismatic batteries in which an electrode assembly is housed in a cylindrical or prismatic metal can, and pouch-type batteries in which an electrode assembly is housed in a pouch-type case of an aluminum laminate sheet, according to the shape of the battery case. The electrode assembly housed in the battery case is a chargeable and dischargeable power generating element having a positive electrode, a negative electrode, and a separator structure interposed between the positive electrode and the negative electrode, and is classified into a jelly roll type in which a separator is interposed between a long sheet-like positive electrode and a negative electrode coated with an active material and wound up, and a stack type in which a number of positive electrodes and negative electrodes of a predetermined size are stacked in sequence with a separator interposed between them.

[0005] The positive electrode and the negative electrode are formed by applying a positive electrode slurry containing a positive electrode active material and a negative electrode slurry containing a negative electrode active material to a positive electrode current collector and a negative electrode current collector, respectively, and then drying and rolling the resulting mixture. At this time, a small amount of binder is added to the positive electrode slurry and the negative electrode slurry to prevent the active material from being detached from the current collector.

[0006] Meanwhile, a positive electrode tab and a negative electrode tab are formed on the positive electrode and the negative electrode for electrical connection to the outside, and a positive electrode lead and a negative electrode lead are connected to the positive electrode tab and the negative electrode tab, respectively. At this time, the positive electrode tab and the positive electrode lead, and the negative electrode tab and the negative electrode lead may be joined by welding. At this time, since welding defects may occur between the tabs and the leads, a welding defect inspection is performed to detect welding defects.

[0007] Inspection of such weld defects generally involves measuring the weld strength of the welded portion between the tab and the lead, but mainly involves measuring the tensile strength of the welded portion between the tab and the lead, specifically, measuring the tensile strength generated when the tab and the lead are pulled in opposite directions.

[0008] However, it is difficult to detect all types of welding defects and weak welding defects that occur intermittently by using tensile strength alone.

[0009] Therefore, there is a need to develop a method for inspecting weld defects that can detect all of the above-mentioned weak level weld defects. Summary of the Invention [Problem to be solved by the invention]

[0010] The present invention has been devised to solve the above problems, and an object of the present invention is to provide a method for inspecting weld defects, which can improve the reliability and accuracy of welding by detecting all weak-level weld defects. [Means for solving the problem]

[0011] In one embodiment of the present invention, a method for inspecting for welding defects includes the steps of manufacturing a sample electrode assembly by welding an electrode lead to an electrode tab formed on the electrode assembly, measuring the tensile strength, torsional strength and peel strength of the welded portion between the electrode tab and the electrode lead for the sample electrode assembly, deriving correlations between the tensile strength, torsional strength and peel strength and the presence or absence of welding defects, and deriving reference values ​​for the tensile strength, torsional strength and peel strength for determining the presence or absence of welding defects.

[0012] In a specific example, the step of measuring the tensile strength, torsional strength, and peel strength includes the step of preparing three sets of electrode assembly samples and measuring any one of the tensile strength, torsional strength, and peel strength for each set.

[0013] The tensile strength, torsional strength and peel strength are measured by a measuring device that includes a first gripper that clamps an end of the electrode lead and a second gripper that clamps the electrode assembly.

[0014] At this time, the first gripper applies a force in a predetermined direction to the electrode lead to break the welded portion.

[0015] Meanwhile, in one embodiment of the present invention, the step of deriving the correlation between the tensile strength, torsional strength and peel strength and the presence or absence of welding defects includes a process of creating a database of the relationship between the tensile strength, torsional strength and peel strength of the welded portion between the electrode tab and the electrode lead and the presence or absence of welding defects.

[0016] In this case, the reference value is derived from a database.

[0017] In another embodiment of the present invention, the method for inspecting for weld defects further includes the steps of measuring the tensile strength, torsional strength and peel strength of the welded portion between the electrode tab and the electrode lead by varying a welding method of the welded portion between the electrode tab and the electrode lead, and deriving a correlation between the tensile strength, torsional strength and peel strength and the presence or absence of weld defects for each welding method.

[0018] In this case, the method for inspecting for welding defects according to the present invention further includes the step of deriving a reference value for determining the presence or absence of a welding defect for each welding method.

[0019] The welding method can be ultrasonic welding or laser welding.

[0020] The method for inspecting welding defects according to the present invention further includes a step of determining a cause of occurrence of the welding defect from the above correlation, and creating a database of the causes.

[0021] The method for inspecting welding defects according to the present invention further includes a step of determining welding defects of the electrode assembly.

[0022] In this case, the step of determining the welding defect includes a process of manufacturing three sets of electrode assemblies to be inspected by welding electrode leads to electrode tabs, measuring any one of tensile strength, torsional strength, and peel strength for each set, and comparing the measured value with a reference value to determine whether or not there is a defect.

[0023] At this time, the step of determining the presence or absence of defects includes a step of comparing the measured values ​​with reference values ​​for two of the tensile strength, torsional strength, and peel strength.

[0024] The step of determining the presence or absence of defects also includes a step of comparing the measured values ​​of tensile strength, torsional strength and peel strength with standard values.

[0025] The present invention also provides a method for manufacturing a secondary battery, including the above-mentioned method for inspecting for welding defects. Effect of the Invention

[0026] The method for inspecting weld defects according to the present invention has the advantage that it can be applied to all welding processes by confirming and standardizing the correlation between tensile strength, torsional strength, and peel strength and the presence or absence of weld defects.

[0027] Furthermore, by measuring different types of strength tests in parallel in addition to tensile strength and deriving a reference value for determining defects from the measured values, it is possible to detect all low-level welding defects, thereby improving the reliability and accuracy of welding. [Brief description of the drawings]

[0028] [Figure 1] 4 is a flowchart showing the procedure of a method for inspecting welding defects according to one embodiment of the present invention. [Diagram 2] 1 is a schematic diagram showing a method for measuring tensile strength in a method for inspecting welding defects according to the present invention; [Diagram 3] 1 is a schematic diagram showing a method for measuring torsional strength in a method for inspecting weld defects according to the present invention; [Figure 4] 1 is a schematic diagram showing a method for measuring peel strength in a method for inspecting welding defects according to the present invention; [Diagram 5] 6 is a flowchart showing the steps of a method for inspecting welding defects according to another embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0029] The present invention will be described in detail below. Before that, the terms and words used in the specification and claims should not be interpreted as being limited to their ordinary or dictionary meanings, but should be interpreted as meanings and concepts that are consistent with the technical idea of ​​the present invention, based on the principle that an inventor can appropriately define the concept of a term in order to best describe his own invention.

[0030] In this application, the terms "comprise" and "have" are intended to specify the presence of a feature, number, step, operation, component, part, or combination thereof described herein, and should be understood as not precluding the presence or addition of one or more other features, numbers, steps, operations, components, parts, or combinations thereof. In addition, when a part such as a layer, film, region, or plate is described as being "on" another part, this includes not only the case where it is "directly on" the other part, but also the case where there is another part in between. Conversely, when a part such as a layer, film, region, or plate is described as being "under" another part, this includes not only the case where it is "directly under" the other part, but also the case where there is another part in between. In addition, in this application, being "on" may include not only the case where it is located on the top, but also the case where it is located on the bottom.

[0031] The present invention will be described in detail below.

[0032] FIG. 1 is a flow chart showing the steps of a method for inspecting welding defects according to one embodiment of the present invention.

[0033] Referring to FIG. 1, in one embodiment of the present invention, a method for inspecting for welding defects includes a step (S10) of manufacturing a sample electrode assembly by welding an electrode lead to an electrode tab formed on the electrode assembly, a step (S20) of measuring the tensile strength, torsional strength and peel strength of a welded portion between the electrode tab and the electrode lead for the sample electrode assembly, a step (S30) of deriving correlations between the tensile strength, torsional strength and peel strength and the presence or absence of welding defects, and a step of deriving reference values ​​for the tensile strength, torsional strength and peel strength for determining the presence or absence of welding defects.

[0034] As described above, in general inspections for welding defects, the tensile strength of the welded portion between the tab and the lead is measured. However, such inspections of tensile strength can only grasp the welding strength in one direction, so there is a problem that it is difficult to detect all types of welding defects and weak welding defects that occur intermittently.

[0035] The method for inspecting weld defects according to the present invention has the advantage that it can be applied to all welding processes by confirming the correlation between the tensile strength, torsional strength, and peel strength for grasping the weld strength and the presence or absence of weld defects and standardizing based on the correlation.

[0036] Furthermore, with regard to weld strength, by measuring different types of strength tests in parallel in addition to tensile strength and deriving a reference value for defect judgment from the measurements, it is possible to detect all weak-level weld defects, thereby improving the reliability and accuracy of welding.

[0037] Each step of the method for inspecting welding defects according to the present invention will be described in detail below.

[0038] Meanwhile, in the specification of the present invention, the weld strength refers to the strength of the welded portion between the electrode tab and the electrode lead, and is a term generally referring to tensile strength, torsional strength and peel strength.

[0039] <Manufacturing of electrode assembly samples> In the method for inspecting weld defects according to the present invention, a sample electrode assembly is manufactured by welding an electrode lead to an electrode tab formed on the electrode assembly.

[0040] In this case, the electrode assembly may be formed by alternately stacking a positive electrode, a separator, and a negative electrode, and each of the positive electrode and the negative electrode may have a structure in which an active material layer is formed by applying an electrode slurry containing an electrode active material to a current collector and then performing a drying and rolling process.

[0041] The current collector may be a positive electrode current collector or a negative electrode current collector, the electrode active material may be a positive electrode active material or a negative electrode active material, and the electrode slurry may further include a conductive material and a binder in addition to the electrode active material.

[0042] In the present invention, the positive electrode current collector is generally made to a thickness of 3 to 500 μm. Such a positive electrode current collector is not particularly limited as long as it has high conductivity without inducing chemical changes in the battery. For example, stainless steel, aluminum, nickel, titanium, baked carbon, or aluminum or stainless steel surface-treated with carbon, nickel, titanium, silver, etc. may be used. The current collector may have fine irregularities on its surface to increase the adhesive force of the positive electrode active material, and may be in various forms such as a film, sheet, foil, net, porous body, foam, nonwoven fabric, etc.

[0043] In the case of a negative electrode current collector sheet, it is generally made to a thickness of 3 to 500 μm. Such a negative electrode current collector is not particularly limited as long as it has conductivity without inducing a chemical change in the battery. For example, copper, stainless steel, aluminum, nickel, titanium, baked carbon, copper or stainless steel surface treated with carbon, nickel, titanium, silver, etc., aluminum-cadmium alloy, etc. can be used. In addition, like the positive electrode current collector, it is also possible to form fine irregularities on the surface to strengthen the binding force of the negative electrode active material, and it can be used in various forms such as a film, sheet, foil, net, porous body, foam, nonwoven fabric, etc.

[0044] In the present invention, the positive electrode active material is a material capable of undergoing an electrochemical reaction, and contains two or more transition metals as a lithium transition metal oxide. For example, lithium cobalt oxide (LiCoO2) substituted with one or more transition metals, layered compounds such as lithium nickel oxide (LiNiO2), lithium manganese oxide substituted with one or more transition metals, and lithium manganese oxide having the chemical formula LiNi 1-y M y Lithium nickel oxide represented by the formula LiO2 (where M=Co, Mn, Al, Cu, Fe, Mg, B, Cr, Zn or Ga, containing at least one of the above elements, and 0.01≦y≦0.7), 1+z Ni 1 / 3 Co 1 / 3 Mn 1 / 3 O2, Li 1+z Ni0.4 Mn 0.4 Co 0.2 Like O2 and the like, Li 1+z Ni b Mn c Co 1-(b+c+d) M d O (2-e) A e (Here, -0.5 ≤ z ≤ 0.5, 0.1 ≤ b ≤ 0.8, 0.1 ≤ c ≤ 0.8, 0 ≤ d ≤ 0.2, 0 ≤ e ≤ 0.2, b + c + d < 1, M = Al, Mg, Cr, Ti, Si or Y, and A = F, P or Cl) lithium nickel cobalt manganese composite oxide represented by the chemical formula Li 1+x M 1-y M' y PO 4-z X z (Here, M = transition metal, preferably Fe, Mn, Co or Ni, M' = Al, Mg or Ti, X = F, S or N, 0.5 ≤ x ≤ +0.5, 0 ≤ y ≤ 0.5, 0 ≤ z ≤ 0.1) olivine-type lithium metal phosphate represented by the formula, etc. are mentioned, but it is not limited to these only.

[0045] The negative electrode active material is, for example, carbon such as graphitizable carbon and graphite-based carbon; Li x Fe2O3 (0 ≤ x ≤ 1), Li x WO2 (0 ≤ x ≤ 1), Sn x Me 1-x Me’ y O z (Me: Mn, Fe, Pb, Ge; Me’: Al, B, P, Si, Group 1, Group 2, Group 3 elements of the periodic table, halogen; 0 < x ≤ 1; 1 ≤ y ≤ 3; 1 ≤ z ≤ 8) metal composite oxides such as; lithium metal; lithium alloy; silicon-based alloy; tin-based alloy; metal oxides such as SnO, SnO2, PbO, PbO2, Pb2O3, Pb3O4, Sb2O3, Sb2O4, Sb2O5, GeO, GeO2, Bi2O3, Bi2O4, Bi2O5; conductive polymers such as polyacetylene; Li-Co-Ni-based materials and the like can be used.

[0046] The conductive material is usually added in an amount of 1 to 30% by weight based on the weight of the entire mixture including the positive electrode active material. Such a conductive material is not particularly limited as long as it has conductivity without inducing a chemical change in the battery. For example, graphite such as natural graphite or artificial graphite, carbon black such as carbon black, acetylene black, ketjen black, channel black, furnace black, lamp black, and thermal black, conductive fibers such as carbon fiber and metal fiber, metal powders such as carbon fluoride, aluminum, and nickel powder, conductive whiskers such as zinc oxide and potassium titanate, conductive metal oxides such as titanium oxide, and conductive materials such as polyphenylene derivatives can be used.

[0047] The binder is a component that aids in binding the active material and conductive material, etc., and binding to the current collector, and is usually added in an amount of 1 to 30% by weight based on the weight of the entire mixture including the positive electrode active material. Examples of such binders include polyvinylidene fluoride, polyvinyl alcohol, carboxymethyl cellulose (CMC), starch, hydroxypropyl cellulose, regenerated cellulose, polyvinylpyrrolidone, tetrafluoroethylene, polyethylene, polypropylene, ethylene-propylene-diene terpolymer (EPDM), sulfonated EPDM, styrene-butylene rubber, fluororubber, and various copolymers.

[0048] Meanwhile, the separator is an insulating thin film that is interposed between the positive and negative electrodes and has high ion permeability and mechanical strength. The pore diameter of the separator is generally 0.01 to 10 μm, and the thickness is generally 5 to 300 μm. As such a separator, for example, a sheet or nonwoven fabric made of an olefin polymer such as polypropylene, which is chemically resistant and hydrophobic, glass fiber, or polyethylene, etc. is used.

[0049] In the electrode assembly, an electrode tab is formed on one side of the electrode, and the electrode tab may be a positive electrode tab or a negative electrode tab. A positive electrode lead and a negative electrode lead are connected to the positive electrode tab and the negative electrode tab, respectively. The positive electrode lead and the negative electrode lead are drawn out to the outside of the battery case and serve as terminals electrically connected to the outside. In this case, the positive electrode lead and the negative electrode lead may be joined to the positive electrode tab and the negative electrode tab, respectively, by welding. As a welding method, a known method may be used, for example, ultrasonic welding or laser welding may be used.

[0050] <Weld strength measurement> When a sample of the electrode assembly is manufactured, the weld strength, i.e., tensile strength, torsional strength, and peel strength, of the welded portion between the electrode tab and the electrode lead of the sample electrode assembly is measured. In the method for inspecting weld defects according to the present invention, two or more types of weld strength can be measured depending on the direction of the external force.

[0051] That is, the method for inspecting weld defects according to the present invention can detect all low-level weld defects by adding torsion strength and peel strength, which are measured while applying an external force in a direction different from that of the tensile strength, to the tensile strength as a criterion for judging weld defects, and can improve the reliability and accuracy of welding.

[0052] The step of measuring the tensile strength, torsional strength and peel strength includes the steps of preparing three sets of electrode assembly samples and measuring any one of the tensile strength, torsional strength and peel strength for each set.

[0053] As described below, the tensile strength, torsional strength, and peel strength are measured by applying an external force to the electrode tab in a certain direction to break the welded portion between the electrode tab and the electrode lead, and it is difficult to measure a different type of weld strength for an electrode assembly sample that has completed measurement for one type of weld strength. Therefore, after preparing three sets of electrode assembly samples, one of the tensile strength, torsional strength, and peel strength is measured for each set. At this time, one set includes at least one electrode assembly sample, and one set may include two or more electrode assembly samples. At this time, when one set includes two or more electrode assembly samples, the average of the weld strengths of the two electrode assembly samples may be determined as the weld strength of the set.

[0054] On the other hand, the tensile strength, torsional strength and peel strength can be measured using the same type of measuring device.

[0055] Fig. 2 is a schematic diagram showing a method for measuring tensile strength in the method for inspecting weld defects according to the present invention, Fig. 3 is a schematic diagram showing a method for measuring torsional strength in the method for inspecting weld defects according to the present invention, and Fig. 4 is a schematic diagram showing a method for measuring peel strength in the method for inspecting weld defects according to the present invention.

[0056] 2 to 4, the electrode assembly 100 has a structure in which the positive electrode 111, the negative electrode 112, and the separator 113 are alternately stacked as described above, and has an electrode tab 120, which is either a positive electrode tab or a negative electrode tab, formed on one side, and an electrode lead 130 joined to the electrode tab by welding.

[0057] Meanwhile, the measuring device 200 includes a first gripper 210 for holding the end of the electrode lead, and a second gripper 220 for holding the electrode assembly.

[0058] Specifically, the second gripper 220 fixes the electrode assembly 100. The second gripper 220 may have a structure in which a pair of pressure plates are formed on a surface in contact with the electrode assembly 100 so as to pressurize the electrode assembly 100 from both sides. The pair of pressure plates can appropriately pressurize and fix the electrode assembly by adjusting the gap between them.

[0059] The first gripper 210 may have a structure in which a space is formed in which the electrode lead 130 can be accommodated so that the end of the electrode lead 130 can be fixed. For example, the first gripper 210 may have a structure in which a pair of pressure plates are formed on a surface that contacts the electrode lead. In this case, the pressure plates can fix the electrode lead by appropriately adjusting the gap therebetween. In the present invention, there is no specific limitation on the shape of the first gripper 210 and the second gripper 220 as long as they can fix the electrode assembly and the electrode lead.

[0060] At this time, the first gripper 210 applies force to the electrode lead in a predetermined direction to break the welded portion.

[0061] 2, the first gripper 210 can apply a tensile force to the welded portion between the electrode lead 130 and the electrode tab 120 by pulling the electrode lead 130 in a direction parallel to the direction in which the electrode lead 130 is pulled out. The first gripper 210 can pull the electrode lead 130 until the welded portion breaks, and the force that the welded portion receives when it breaks can be defined as the tensile strength of the welded portion. The force that the welded portion receives when it breaks can be measured using a known measuring device or the like.

[0062] 3, the first gripper 210 may apply a twisting force to the welded portion between the electrode lead 130 and the electrode tab 120 by rotating about a central portion of the electrode lead in the width direction as a rotation axis. The first gripper 210 rotates until the welded portion breaks, and the force that the welded portion receives when it breaks may be defined as the torsional strength of the welded portion. Similarly, the force that the welded portion receives when it breaks may be measured using a known measuring device or the like.

[0063] 4, the first gripper 210 can apply force from a perpendicular direction that is 90 degrees to the direction in which the electrode tab 120 or the electrode lead 130 is pulled out, so as to peel off the electrode lead 130 from the electrode tab 120. The first gripper 210 can apply force until the welded portion breaks, and the force that the welded portion receives when it breaks can be defined as the peel strength of the welded portion. Similarly, the force that the welded portion receives when it breaks can be measured using a known measuring device or the like.

[0064] The above-mentioned welding strength can be measured for a plurality of electrode assembly samples, and can also be measured for electrode assembly samples that have been welded using different welding methods, as described below.

[0065] <Derive correlation with the presence or absence of welding defects> When the tensile strength, torsional strength and peel strength of the electrode assembly sample are measured, a correlation between the tensile strength, torsional strength and peel strength and the presence or absence of welding defects is derived. Here, the correlation means a tendency that the presence or absence of welding defects is indicated according to the values ​​of the tensile strength, torsional strength and peel strength.

[0066] Specifically, the step of deriving the correlation with the presence or absence of welding defects includes a process of creating a database of the relationship between the tensile strength, torsional strength, and peel strength of the welded portion between the electrode tab and the electrode lead and the presence or absence of welding defects. This is to grasp the tendency of the presence or absence of welding defects with respect to the tensile strength, torsional strength, and peel strength as described above. To this end, after manufacturing a plurality of electrode assembly samples, the tensile strength, torsional strength, and peel strength of each can be measured and stored in a storage system such as a memory, and such a database can be recorded as visual data such as a table or graph. At this time, for the sake of measurement accuracy, it is preferable to measure the tensile strength, torsional strength, and peel strength of as many electrode assembly samples as possible.

[0067] On the other hand, the presence or absence of a weld defect means whether or not an actual defect has occurred in the welded portion between the electrode lead and the electrode tab, and can be determined, for example, by observing the appearance or surface condition of the welded portion.

[0068] <Derivation of standard values> The correlation between the tensile strength, torsional strength, and peel strength and the presence or absence of a welding defect is derived, and a reference value for determining the presence or absence of the welding defect is derived therefrom. The reference value is derived from the database. In addition, all reference values ​​for each of the tensile strength, torsional strength, and peel strength are derived.

[0069] Specifically, the database stores the measured values ​​of the tensile strength, torsional strength, and peel strength of the electrode assembly samples whose welding state has been determined to be poor, and the tensile strength, torsional strength, and peel strength of the electrode assembly samples whose welding state has been determined to be good. Here, for example, the minimum value of the measured values ​​of the tensile strength, torsional strength, and peel strength of the electrode assembly samples whose welding state has been determined to be good may be set as the reference value.

[0070] In other words, the method for inspecting weld defects according to the present invention has the advantage that it can be applied to all welding processes by confirming and standardizing the correlation between the tensile strength, torsional strength, and peel strength and the presence or absence of weld defects.

[0071] Furthermore, with regard to weld strength, by measuring different types of strength tests in parallel in addition to tensile strength and deriving a reference value for determining defects therefrom, it is possible to detect all weak-level weld defects, thereby improving the reliability and accuracy of welding.

[0072] Meanwhile, in another embodiment of the present invention, a method for inspecting a weld defect includes measuring a tensile strength, a torsional strength and a peel strength of a welded portion between an electrode tab and an electrode lead by changing a welding method of the welded portion between the electrode tab and the electrode lead, and deriving a correlation between the tensile strength, the torsional strength and the peel strength and the presence or absence of a weld defect for each welding method. The method for inspecting a weld defect further includes a step of deriving a reference value for the presence or absence of a weld defect for each welding method.

[0073] FIG. 5 is a flowchart showing the procedure of a method for inspecting welding defects according to another embodiment of the present invention.

[0074] That is, referring to FIG. 5, the method for inspecting for welding defects includes a step (S20) of manufacturing a sample electrode assembly by welding an electrode lead to an electrode tab formed on the electrode assembly, a step (S21) of measuring the tensile strength, torsional strength and peel strength of a welded portion between the electrode tab and the electrode lead using different welding methods for the sample electrode assembly, a step (S22) of deriving a correlation between the tensile strength, torsional strength and peel strength and the presence or absence of welding defects, and a step (S23) of deriving a reference value for determining the presence or absence of welding defects for each welding method.

[0075] On the other hand, examples of the welding method include laser welding and ultrasonic welding.

[0076] That is, in the process of deriving a reference value for determining whether or not there is a welding defect, the present invention can reflect variations in weld strength that may vary depending on the welding method by dividing the reference value into specific values ​​according to the welding method.

[0077] Here, each step in the method for inspecting for welding defects is the same as that described above. Specifically, after preparing three sets of electrode assembly samples using one type of welding method, one of the tensile strength, torsional strength, or peel strength is measured for each set. The same process is repeated by changing the welding method.

[0078] In this case, the measurement device may include a first gripper that secures an end of the electrode lead, and a second gripper that secures the electrode assembly.

[0079] Meanwhile, when the weld strength is measured, correlations between the tensile strength, torsional strength, and peel strength for each welding method and the presence or absence of a weld defect are derived therefrom. At this time, the method may further include determining the cause of the weld defect from the tensile strength, torsional strength, and peel strength for the welding method, and creating a database of the cause. To this end, a plurality of electrode assembly samples may be manufactured using different welding methods, and the tensile strength, torsional strength, and peel strength of each sample may be measured, and the measured values ​​may be stored in a storage system such as a memory. Such a database may be recorded as visual data such as a table or a graph. Also, the reference value may be derived from such a database. A specific process for deriving the reference value may be the same as that described above, for example.

[0080] In addition, the method for inspecting weld defects according to the present invention further includes a step of determining the cause of the weld defects from the correlation and creating a database of the causes. When the welding method is different, the cause of the weld defects is also different. Therefore, the present invention creates a database of tensile strength, torsional strength, and peel strength according to the welding method and the cause of the weld defects, and can be used as a reference sample for finding the cause of the weld defects when the weld defects occur.

[0081] Once a reference value for the presence or absence of a welding defect is thus obtained, a step of determining whether or not there is a welding defect in an actual electrode assembly is performed based on the reference value.

[0082] The step of determining the welding defects includes a process of manufacturing three sets of electrode assemblies to be inspected by welding electrode leads to electrode tabs, measuring any one of tensile strength, torsional strength, and peel strength for each set, and comparing the measured values ​​with a reference value to determine whether or not there is a defect.

[0083] Specifically, the manufacturing method of the electrode assembly and the method of measuring the tensile strength, torsional strength and peel strength are the same as those described above. The tensile strength, torsional strength and peel strength can be measured by the measuring device described above. Also, different types of weld strength can be measured for each set.

[0084] When the tensile strength, torsional strength, and peel strength are measured, they are compared with a reference value to determine whether or not there is a defect. In this case, the process of determining whether or not there is a defect includes a process of comparing the measured values ​​of two of the tensile strength, torsional strength, and peel strength with the reference value. In this case, for example, the measured values ​​of any two of the tensile strength, torsional strength, and peel strength are compared with the reference value, and if both of the two measured values ​​meet the reference value, the electrode assembly may be determined as a good product. In this case, the electrode assembly determined as a good product may be an electrode assembly manufactured on the same process line.

[0085] In another example, the step of determining the presence or absence of defects includes a step of comparing the measured values ​​with reference values ​​for tensile strength, torsional strength, and peel strength. In this case, for example, the measured values ​​for all of the tensile strength, torsional strength, and peel strength are compared with the reference values, and the electrode assembly may be determined as a non-defective product if the measured values ​​for all of the tensile strength, torsional strength, and peel strength satisfy the reference values. As described above, the electrode assemblies determined as non-defective products may be electrode assemblies manufactured in the same process line.

[0086] The present invention also provides a method for manufacturing a secondary battery, including the above-mentioned method for inspecting for welding defects.

[0087] Specifically, the secondary battery is manufactured by housing an electrode assembly having a structure in which a positive electrode, a separator, and a negative electrode are alternately stacked in a battery case. In this case, the positive electrode, the negative electrode, and the separator may be the same as those in the above-mentioned electrode assembly sample. In addition, the electrode assembly may be one that is determined to be a non-defective product when inspected according to the above-mentioned inspection method for welding defects.

[0088] Meanwhile, the battery case is not particularly limited as long as it is used as an exterior material for packaging a battery. A cylindrical, rectangular or pouch-shaped battery case may be used, and more specifically, a pouch-shaped battery case may be used. Similarly, details regarding the battery case are well known to ordinary engineers, so a detailed description will be omitted.

[0089] When the electrode assembly is housed in the battery case, an electrolyte is injected, the battery case is sealed, and an activation process is performed to manufacture a secondary battery.

[0090] The above description is merely illustrative of the technical idea of ​​the present invention, and various modifications and variations are possible within the scope of the essential characteristics of the present invention if one has ordinary knowledge in the technical field to which the present invention belongs. Therefore, the drawings disclosed in the present invention are for the purpose of explaining the technical idea of ​​the present invention, rather than for the purpose of limiting the technical idea of ​​the present invention, and the scope of the technical idea of ​​the present invention is not limited by such drawings. The scope of protection of the present invention should be interpreted by the claims, and all technical ideas within the scope equivalent thereto should be interpreted as being included in the scope of the present invention.

[0091] In this specification, terms indicating directions such as up, down, left, right, front, and back are used for the convenience of explanation, but it is self-evident that such terms may change depending on the position of the object in question, the position of the observer, etc. [Explanation of symbols]

[0092] 100: Electrode assembly 111: Positive electrode 112: Negative electrode 113: Separation membrane 120: Electrode tab 130: Electrode lead 200: Measuring equipment 210: First gripper 220: Second gripper

Claims

1. manufacturing a sample of the electrode assembly by welding an electrode lead to an electrode tab formed on the electrode assembly; measuring the tensile strength, torsional strength and peel strength of a weld between the electrode tab and the electrode lead for a sample of the electrode assembly; Deriving a correlation between the tensile strength, the torsional strength, and the peel strength and the presence or absence of a welding defect; Deriving reference values ​​for tensile strength, torsional strength, and peel strength for determining whether or not there is a welding defect; a step of measuring a tensile strength, a torsional strength and a peel strength of the welded portion between the electrode tab and the electrode lead by changing a welding method of the welded portion between the electrode tab and the electrode lead, and deriving a correlation between the tensile strength, the torsional strength and the peel strength and the presence or absence of a weld defect for each welding method.

2. The step of measuring the tensile strength, torsional strength, and peel strength includes: Three sets of samples of the electrode assembly were prepared, 2. The method of claim 1, further comprising the step of measuring any one of tensile strength, torsional strength and peel strength for each set.

3. The tensile strength, torsional strength and peel strength are a first gripper for clamping an end of the electrode lead; and The method for inspecting welding defects according to claim 1 or 2, wherein the measurement is performed by a measuring device including a second gripper that fixes the electrode assembly.

4. The method for inspecting for defective welding according to claim 3 , wherein the first gripper applies a force in a predetermined direction to the electrode lead to break the welded portion.

5. The method for inspecting a welding defect according to claim 1 , further comprising the step of deriving the reference value for determining the presence or absence of a welding defect for each welding method.

6. The method for inspecting a weld defect according to claim 1 or 5, wherein the welding method is ultrasonic welding and laser welding.

7. The method for inspecting welding defects according to claim 1 , further comprising the steps of determining a cause of occurrence of welding defects from the correlation, and creating a database of the cause of occurrence.

8. The method for inspecting weld defects according to claim 1 , further comprising the step of determining weld defects of the electrode assembly.

9. The step of determining a welding defect includes: The electrode leads are welded to the electrode tabs to manufacture three sets of the electrode assemblies to be tested; Measure any one of the tensile strength, torsional strength, and peel strength for each set, The method for inspecting weld defects according to claim 8 , further comprising the step of comparing the measured value with the reference value to determine the presence or absence of a defect.

10. The process of determining whether or not there is a defect comprises:

10. The method for inspecting weld defects according to claim 9, further comprising the step of comparing the measured values ​​with the reference values ​​for two of tensile strength, torsional strength, and peel strength.

11. The process of determining whether or not there is a defect comprises:

10. The method for inspecting weld defects according to claim 9, further comprising the step of comparing the measured values ​​with the reference values ​​for tensile strength, torsional strength and peel strength.

12. A method for manufacturing a secondary battery, comprising the method for inspecting for welding defects according to claim 1 .

Citation Information

Patent Citations

  • Method of joining two or more electrode plate forming members

    JP2013084448A

  • Success / failure determination method of laser welding

    JP2018111120A

  • Weld zone resistance measuring method and weld zone resistance measuring device

    JP2019060769A

  • Electrode with improved electrode tab welding characteristics and secondary battery including the same