Negative lift-off resist composition comprising an alkali-soluble resin and a photoacid generator, and method for producing a metal film pattern on a substrate
The combination of alkali-soluble resins and photoacid generators in the negative lift-off resist composition addresses coating and solubility issues, resulting in high-quality resist patterns with improved sensitivity and resolution for microfabrication.
Patent Information
- Application Number
- JP2021563363
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-05-20
- Filing Date
- 2020-05-18
- Publication Date
- 2024-09-18
- Estimated Expiration
- 2040-05-18
AI Technical Summary
Existing negative lift-off resist compositions face issues with insufficient coating properties, solubility, pattern shape, removability, and sensitivity, especially for small pattern sizes, leading to defects and poor yield in microfabrication processes.
A negative lift-off resist composition comprising a combination of alkali-soluble resins and photoacid generators, specifically formulated to enhance coating properties, solubility, and pattern shape, using a variety of alkali-soluble resins and photoacid generators to achieve improved sensitivity and resolution.
The composition enables the formation of high-quality resist patterns with good solubility, reduced defects, and high yield, allowing for the creation of finely designed metal film patterns with inverted tapered shapes.
Smart Images

Figure 0007553469000040 
Figure 0007553469000041 
Figure 0007553469000039
Abstract
Description
[Technical field]
[0001] The present invention relates to a negative lift-off resist composition comprising an alkali-soluble resin and a photoacid generator. The present invention also relates to a method for producing a metal film pattern on a substrate. The present invention also relates to a method for producing a device comprising a metal film pattern. [Background technology]
[0002] The trend toward ever-finer, high-performance devices has led to a demand for ever-finer patterning in elements (e.g., semiconductor elements and FPD elements). Lithography techniques using photoresist (hereinafter simply referred to as "resist") are generally employed for microfabrication. As illustrated in FIG. 1, a lift-off process for creating electrodes is known, which is characterized by peeling off unnecessary electrode portions on a patterned resist layer. In contrast, a typical electrode etching process uses the resist pattern as a mask to peel off the electrode under the resist pattern (typically by dry etching) to obtain a designed electrode pattern.
[0003] Under these circumstances, a specific negative photoresist composition for forming a lift-off pattern has been researched, which is coated on an underlayer film and developed together with the underlayer film (Patent Document 1).
[0004] In order to achieve good high sensitivity in a reverse taper shape, a negative photoresist composition containing an alkali-soluble binder resin, a first photoacid generator containing a halogen, a triazine-based second photoacid generator, a crosslinker having an alkoxy structure, and a solvent has been investigated (Patent Document 2).
[0005] In order to achieve storage stability, high sensitivity, and film retention (after development) of more than 95% and to form a lift-off resist pattern with a sufficient undercut shape, a lift-off resist composition containing an alkali-soluble cellulose resin, although it is a positive resist, has been investigated (Patent Document 3). [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2005-37414 A [Patent Document 2] U.S. Patent Application Publication No. 2011 / 0274853 [Patent Document 3] U.S. Patent Application Publication No. 2012 / 0129106 Summary of the Invention [Problem to be solved by the invention]
[0007] The present inventors have found that there are one or more problems that still require improvement, as listed below: insufficient coatability; insufficient solubility of solutes; when the pattern size is small, it is difficult to obtain a developed resist pattern having a good shape and / or defects are observed; when the pattern size is small, the strippability of the resist pattern is insufficient; the yield is insufficient; the sensitivity and / or resolution of the resist layer is insufficient; and it is difficult to obtain an inverse taper shape.
[0008] The present inventors have now discovered that the invention described below solves at least one of these problems. [Means for solving the problem]
[0009] The present invention provides a negative lift-off resist composition comprising one or more (A) alkali-soluble resins and one or more (B) photoacid generators; The (A) alkali-soluble resin comprises an (A1) resin and / or an (A2) resin; (B) the photoacid generator comprises (B1) an onium salt and / or (B2) a sulfonyl compound; However, (i) when a negative lift-off resist composition contains a single (A) alkali-soluble resin, the negative lift-off resist composition contains a plurality of (B) photoacid generators, and (ii) when a negative lift-off resist composition contains a single (B) photoacid generator, the negative lift-off resist composition contains a plurality of (A) alkali-soluble resins; The (A1) resin is represented by the following formula (A1): [ka] R 11 , R 12 , R 14 , R 15 , R 17 and R 18 are each independently hydrogen, C 1-6 alkyl, carboxyl, halogen or cyano; R 13 and R 16 are each independently 1-6 Alkyl, C 1-6 alkoxy, halogen or cyano; R 19 is C 1-15 Alkyl or C 1-15 Alkoxy, R 19 The alkyl moiety of may form a saturated and / or unsaturated ring; m 11 is a number between 0 and 4, and n 11 is a number between 1 and 3, and m 11 +n 11 ≦5, m 12 is a number between 0 and 5, p A1 , q A1 and r A1 is the number of iterations, [p A1 / (p A1 +q A1 +r A1 )] is 30-98%, and [q A1 / (p A1 +q A1 +r A1 )] is 0 to 70%, and [r A1 / (p A1 +qA1 +r A1 )] is 0–70%; The (A2) resin is represented by the following formula (A2): [ka] R 21 , R 22 , R 24 and R 25 are each independently hydrogen, C 1-6 alkyl, carboxyl, halogen or cyano; R 23 is C 1-6 Alkyl, C 1-6 alkoxy, halogen or cyano; R 26 is C 1-15 Alkyl or C 1-15 Alkoxy, R 26 The alkyl moiety of may form a saturated and / or unsaturated ring; m 21 is a number between 0 and 4, and n 21 is a number between 1 and 3, and m 21 +n 21 ≦5, p A2 and r A2 is the number of iterations, [p A2 / (p A2 +r A2 )] is 30-100%, and [r A2 / (p A2 +r A2 )] is 0–70%; (B1) The onium salt is represented by the following formula (B1): [B m+ Cation][B m- Anion] (B1) B m+ The cation is represented by the following formula (B1)-C1 and / or formula (B1)-C2, and has a valency of m as a whole, where m is 1 to 3: [ka] R 31 , R 32 , R33 , R 34 and R 35 are each independently 1-6 Alkyl, C 1-6 Alkoxy or C 6-12 is aryl, m 31 , m 32 , m 33 , m 34 and m 35 are each independently a number from 0 to 3; B m- The anion is represented by the following formula (B1)-A1, (B1)-A2 and / or (B1)-A3: [ka] R 41 , R 42 and R 43 are each independently unsubstituted or C 1-6 Alkyl-substituted C 6-12 Aryl, unsubstituted or substituted with halogen or carbonyl 1-12 is alkyl, m 41 = 1 or 2; (B2) The sulfonyl compound is represented by the following formula (B2)-1 or (B2-2): [ka] R 51 , R 52 and R 53 are each independently hydrogen, C 1-6 Alkyl, C 1-6 Alkoxy or C 6-12 aryl, R 51 , R 52 and R 53 The alkyl moieties of may be joined together to form a cycloalkyl or aryl; m 52 = 0 or 1, R 54 is unsubstituted or halogen-substituted C 1-6 is alkyl, R 55are each independently 5-12 Cycloalkyl or C 6-12 It is aryl.
[0010] The present invention provides a method for producing a resist pattern, comprising: forming a coating of a negative lift-off resist composition over a substrate; baking the resist composition to form a resist layer; exposing the resist layer to light; and developing the resist layer to form a resist pattern.
[0011] The present invention provides a method for producing a metal film pattern on a substrate, comprising: producing a resist pattern; forming a metal film on the resist pattern; and peeling off the remaining resist pattern and the metal film thereon.
[0012] The present invention provides a method for producing an element, comprising a method for producing a resist pattern or a metal film pattern on a substrate. Effect of the Invention
[0013] This negative lift-off resist composition can exhibit good coatability. The solute in the composition can exhibit good solubility in a solvent. Even if the pattern size is small, a good shape of the resist pattern formed and developed by the composition can be obtained, and / or defects (e.g., pattern collapse) can be reduced. In addition, even if the pattern size is small, a clear peelability of the resist pattern formed by this composition can be obtained. A high yield can be achieved. The resist layer obtained by the composition of the present invention can exhibit good sensitivity. The photoresist layer can have good resolution. A resist pattern with an inverse taper shape can be obtained by the composition of the present invention. These are advantageous for a lift-off process for forming a metal film pattern, due to a finer designed pattern. [Brief description of the drawings]
[0014] [Figure 1]FIG. 1 is a schematic cross-sectional view of a lift-off process. [Diagram 2] FIG. 2 is a schematic cross-sectional view of the etching step. [Diagram 3] FIG. 3 is an explanatory diagram of a mask design used for resist patterning. [Figure 4] FIG. 4 is an explanatory diagram of a mask design used for resist patterning. Detailed Description of the Invention
[0015] [Description of the embodiment] The above summary and the following details are provided to illustrate the invention and are not intended to limit the invention as claimed.
[0016] definition Throughout this specification, unless expressly limited or stated otherwise, the symbols, units, abbreviations and terms defined below have the meanings given in the following definitions, descriptions and examples. Use of the singular includes the plural, and the words "a," "an," and "the" mean "at least one." Furthermore, use of the term "including" as well as other forms such as "includes" and "included" is not limiting. Also, terms such as "element" or "component" include both an element or component comprising one unit and an element or component comprising more than one unit. The term "and / or" includes the use of any single element and means any combination of any of the preceding elements. When a numerical range is specified using "-", "to" or "~", the numerical range includes both the numerical values before and after the "-", "to" or "~", and the units are the same for both numerical values. For example, "5-25 mol%" means "5 mol% or more and 25 mol% or less". As used herein, "C x-y ", "C x -C y " and "C x" refers to the number of carbon atoms in a molecule or substituent. For example, "C 1-6 "Alkyl" means an alkyl chain having 1 to 6 carbon atoms (eg, methyl, ethyl, propyl, butyl, pentyl, hexyl, etc.). When the polymer described herein has multiple types of repeating units, these repeating units are copolymerized. This copolymerization may be any one selected from alternating copolymerization, random copolymerization, block copolymerization, graft copolymerization, and any combination thereof. When the polymer or resin is represented by a chemical structure, n, m, etc. in parentheses indicate the number of repeats. Temperatures shown in this specification are in degrees Celsius. For example, "20 degrees" means "20 degrees Celsius."
[0017] Negative lift-off resist composition The present invention provides a negative lift-off resist composition comprising one or more (A) alkali-soluble resins and one or more (B) photoacid generators. The negative resist composition of the present invention is useful for a lift-off process in which a metal film pattern is obtained by peeling off a metal film portion formed on a developed resist layer (resist pattern wall) in a subsequent process. Since the composition of the present invention is a negative resist, the resist layer formed by the composition has the property that the exposed portion of the layer shows increased resistance to dissolution by a developer, and the unexposed portion is dissolved by a developer.
[0018] The composition of the present invention satisfies the following conditions: (i) when the negative lift-off resist composition contains a single (A) alkali-soluble resin, the negative lift-off resist composition contains multiple (B) photoacid generators; and (ii) when the negative lift-off resist composition contains a single (B) photoacid generator, the negative lift-off resist composition contains multiple (A) alkali-soluble resins. It is permissible for the composition of the present invention to simultaneously contain multiple (A) alkali-soluble resins and multiple (B) photoacid generators. It can be said that a composition that simultaneously satisfies the following conditions is excluded from the scope of the present invention: (iii) the alkali-soluble resin in the composition is a single alkali-soluble resin, and (iv) the photoacid generator in the composition is a single photoacid generator.
[0019] Alkali-soluble resin The composition of the present invention comprises one or more alkali-soluble resins (A). The alkali-soluble resin (A) comprises an (A1) resin and / or an (A2) resin. The resin is preferably an alkali-soluble binder resin. The resin preferably comprises a novolac polymer or a polyhydroxystyrene polymer. The resin contained in the composition of the present invention is preferably a random copolymer or a block copolymer, more preferably a random copolymer.
[0020] For example, the (A) alkali-soluble resin may contain no (A2) resin and may contain a plurality of (A1) resins.
[0021] In one embodiment of the present invention, the mass ratio of the alkali-soluble resin (A) to the total mass of the negative lift-off resist composition is 5 to 50 mass% (preferably 10 to 30 mass%, more preferably 10 to 25 mass%). When the thickness of the coating film formed from the negative lift-off resist composition is 1.0 μm or more, the mass ratio is preferably 15 to 30 mass% (more preferably 15 to 25 mass%, even more preferably 18 to 22 mass%). When the thickness of the coating film formed from the composition of the present invention is less than 1.0 μm, the mass ratio is preferably 5 to 15 mass% (more preferably 5 to 14 mass%, even more preferably 10 to 14 mass%). The thickness of the formed resist coating film can be increased by adding a larger amount of solid components (which can be mainly occupied by the alkali-soluble resin (A)) to the composition.
[0022] As mentioned above, the composition of the present invention may contain a plurality of (A) alkali-soluble resins. Although not wishing to be bound by theory, it is considered that it is good to contain a plurality of (A) alkali-soluble resins in the composition, since the alkali dissolution rate of the resist layer can be appropriately set to show good sensitivity, good resolution and / or good pattern shape.
[0023] In the present application, the weight average molecular weight (Mw) can be measured by gel permeation chromatography (GPC). In a preferred example of this measurement, the GPC column is set at 40 degrees Celsius; 0.6 mL / min of tetrahydrofuran is used as the elution solvent; and monodisperse polystyrene is used as the standard.
[0024] In one embodiment of the present invention, the weight average molecular weight (Mw) of the alkali-soluble resin (A) in the composition of the present invention is preferably 2,000 to 100,000, more preferably 3,000 to 50,000, even more preferably 4,000 to 20,000, and still more preferably 5,000 to 15,000.
[0025] (A1) Resin The (A1) resin is represented by the following formula (A1). [ka] R 11 , R 12 , R 14 , R 15 , R 17 and R 18 are each independently hydrogen, C 1-6 R is alkyl, carboxyl, halogen or cyano; preferably hydrogen or methyl; more preferably hydrogen. 17 It is an aspect of the invention that is methyl. R 13 and R 16 are each independently 1-6 Alkyl, C 1-6 It is alkoxy, halogen or cyano; preferably it is methyl, ethyl, isopropyl, t-butyl or fluorine; more preferably it is methyl or t-butyl.
[0026] R 19 is C 1-15 Alkyl or C 1-15 Alkoxy. R 19 The alkyl portion of R may form a saturated and / or unsaturated ring. 19 C 1-15 It is an aspect of the present invention that R is an alkyl group. 19 The alkyl portion of R is preferably a branched or cyclic structure, more preferably a branched structure. 19 is preferably methyl, ethyl, isopropyl, t-butyl, cyclopentyl, methylcyclopentyl, ethylcyclopentyl, methylcyclohexyl, ethylcyclohexyl, methyladamantyl or ethyladamantyl; more preferably, t-butyl, ethylcyclopentyl, methylcyclohexyl or ethyladamantyl; and even more preferably, t-butyl.
[0027] m 11is a number from 0 to 4. The (A) alkali-soluble resin does not contain an (A2) resin, and contains two (A1) resins, each of which is 1 / 2; in one (A1) resin, p A1 =100%, m 11 = 1; and in another (A1) resin, p A1 =100%, m 11 It may be one aspect of the present invention that m = 2. In this case, 11 = 1.5. The same applies below unless otherwise specified. m 11 is preferably 0, 1, 2, 3 or 4; more preferably 0, 1 or 2; and even more preferably 0. n 11 is a number from 1 to 3; more preferably 1 or 2, and even more preferably 1. m 11 +n 11 <=5. m 12 is a number from 0 to 5; preferably 0, 1, 2, 3, or 4; more preferably 0, 1, or 2; and even more preferably 0.
[0028] p A1 , q A1 and r A1 is the number of repetitions. [p A1 / (p A1 +q A1 +r A1 )] is 30 to 98%; preferably 50 to 95%; more preferably 70 to 95%; and further preferably 70 to 90%. [q A1 / (p A1 +q A1 +r A1 )] is 0 to 70%; preferably 0 to 40%; more preferably 5 to 40%; and further preferably 10 to 40%. [r A1 / (p A1 +q A1 +r A1 )] is 0 to 70%, preferably 0 to 40%. qA1 andr A1 It is preferable that [r A1 / (p A1 +q A1 +r A1 )]=0% is one preferred embodiment of the present invention.
[0029] The (A1) resin of the present invention is represented by formula (A1) and may or may not contain repeating units other than the units defined above. In a preferred embodiment, the (A1) resin of the composition of the present invention is represented by formula (A1) and does not contain repeating units other than the units defined above.
[0030] Specific examples of (A1) resins are listed below, for illustrative purposes only. [ka]
[0031] In one embodiment of the present invention, the weight average molecular weight (Mw) of the (A1) resin in the composition of the present invention is preferably 5,000 to 100,000, more preferably 5,000 to 50,000, even more preferably 5,000 to 20,000, and still more preferably 8,000 to 15,000.
[0032] The mass ratio of the (A1) resin to the total of the (A) alkali-soluble resins is preferably 30 to 100 mass%, more preferably 40 to 100 mass%, and further preferably 40 to 80 mass%. In one embodiment of the present invention, the (A) alkali-soluble resin does not contain the (A2) resin but contains the (A1) resin.
[0033] (A2) Resin The (A2) resin is represented by the following formula (A2). [ka] R 21 , R 22 , R 24and R 25 are each independently hydrogen, C 1-6 R is alkyl, carboxyl, halogen or cyano; preferably hydrogen or methyl, more preferably hydrogen. 24 It is an aspect of the invention that is methyl. R 23 is C 1-6 Alkyl, C 1-6 Alkoxy, halogen or cyano, preferably methyl, ethyl, isopropyl, t-butyl or fluorine; more preferably methyl or t-butyl.
[0034] R 26 is C 1-15 Alkyl or C 1-15 Alkoxy. R 26 The alkyl portion of R may form a saturated and / or unsaturated ring. 26 C 1-15 It is an aspect of the present invention that R is an alkyl group. 26 The alkyl portion of R is preferably a branched or cyclic structure, more preferably a branched structure. 26 is preferably methyl, ethyl, isopropyl, t-butyl, cyclopentyl, methylcyclopentyl, ethylcyclopentyl, methylcyclohexyl, ethylcyclohexyl, methyladamantyl or ethyladamantyl; more preferably t-butyl, ethylcyclopentyl, methylcyclohexyl or ethyladamantyl; and even more preferably t-butyl.
[0035] m 21 is a number from 0 to 4; preferably 0, 1, 2, 3, or 4; more preferably 0, 1, or 2; and even more preferably 0. n 21 is a number from 1 to 3; more preferably 1 or 2; and even more preferably 1. m 21 +n 21 <=5.
[0036] p A2and r A2 is the number of repetitions. [p A2 / (p A2 +r A2 )] is 30 to 100%; preferably 50 to 100%, more preferably 60 to 100%; and even more preferably 100%. [r A2 / (p A2 +r A2 )] is 0 to 70%; more preferably 0 to 50%; more preferably 0 to 40%; and even more preferably 0%.
[0037] The (A2) resin of the present invention is represented by formula (A2) and may or may not contain repeating units other than the units defined above. In a preferred embodiment, the (A2) resin of the composition of the present invention is represented by formula (A2) and does not contain repeating units other than the units defined above.
[0038] Specific examples of (A2) resins are listed below, for illustrative purposes only. [ka]
[0039] In one embodiment of the present invention, the weight average molecular weight (Mw) of the (A2) resin in the composition of the present invention is preferably 2,000 to 20,000, more preferably 4,000 to 20,000, and even more preferably 5,000 to 10,000.
[0040] The mass ratio of the (A2) resin to the total of the (A) alkali-soluble resin is preferably 10 to 100 mass%, more preferably 20 to 100 mass%, and further preferably 20 to 50 mass%. In one embodiment of the present invention, the (A) alkali-soluble resin does not contain the (A1) resin but contains the (A2) resin.
[0041] (B) Photoacid generator The composition of the present invention comprises one or more (B) photoacid generators (hereinafter sometimes referred to as PAGs). In the radiation-exposed portion of the negative resist composition, the PAG is exposed to radiation and generates an acid, which catalyzes the crosslinking reaction of the resin and, if present, the crosslinker.
[0042] (B) The photoacid generator comprises (B1) an onium salt and / or (B2) a sulfonyl compound. For example, (B) PAG may contain a plurality of (B1) onium salts without containing (B2) a sulfonyl compound.
[0043] It is one aspect of the present invention that the mass ratio of the (B) photoacid generator to the mass of the (A) alkali-soluble resin is 1 to 20 mass%, preferably 1 to 15 mass%, and more preferably 1 to 10 mass%. For clarity, throughout this application, when the composition of the present invention comprises a plurality of (A) alkali-soluble resins, the mass ratio of the (A) alkali-soluble resins means the sum of the mass ratios of the plurality of (A) alkali-soluble resins.
[0044] As mentioned above, the composition of the present invention may contain multiple (B)PAGs. Without wishing to be bound by theory, it is believed that it is good to contain multiple (B)PAGs in the composition, since the resolution and / or pattern shape can be appropriately set.
[0045] (B1) Onium salt The onium salt (B1) is represented by the following formula (B1). [B m+ Cation][B m- Anion] (B1)
[0046] B m+ The cation is represented by the following formula (B1)-C1 and / or formula (B1)-C2. B m+ The cations as a whole have a valency of m. m=1 to 3; preferably 1, 2 or 3; more preferably 1 or 2; and even more preferably 1. [ka]
[0047] R 31 , R 32 , R 33 , R 34 and R 35 are each independently 1-6 Alkyl, C 1-6 Alkoxy or C 6-12 It is aryl; preferably it is methyl, ethyl, t-butyl, 1,1-dimethylpropyl, methoxy or ethoxy; more preferably it is methyl, t-butyl, 1,1-dimethylpropyl or methoxy; and even more preferably it is t-butyl.
[0048] m 31 , m 32 , m 33 , m 34 and m 35 are each independently a number from 0 to 3; preferably, each independently is 0 or 1; more preferably, 0. 31 , m 32 , m 33 , m 34 and m 35 is one aspect of the present invention, wherein each of
[0049] B m+ Specific examples of cations are listed below and are for illustrative purposes only. [ka]
[0050] B m- The anion is represented by the following formula (B1)-A1, (B1)-A2 and / or (B1)-A3. [ka]
[0051] R41 , R 42 and R 43 are each independently unsubstituted or C 1-6 Alkyl-substituted C 6-12 Aryl, unsubstituted or substituted with halogen or carbonyl 1-12 alkyl; preferably unsubstituted or halogen-substituted C 1-6 alkyl; more preferably halogen-substituted C 1-4 more preferably, C1 or C4 alkyl substituted with halogen, wherein the halogen is preferably fluorine. In one aspect of the invention, R 41 , R 42 or R 43 The alkyl moieties of R may be joined internally or to each other to form a saturated cyclic hydrocarbon ring. 41 , R 42 or R 43 The alkyl moieties of do not join internally or with each other to form a saturated cyclic hydrocarbon ring. 1-6 In a preferred embodiment, all hydrogen atoms in the alkyl group are replaced by halogen.
[0052] m 41 = 1 or 2; preferably 1. 41 If =2, R 41 is a divalent linker.
[0053] B m- Specific examples of anions are listed below and are for illustrative purposes only. [ka]
[0054] For example, the following onium salt is an example of formula (B1): m+ The cation is represented by (B1)-C1 and has an overall valence of m=2. m- The anion is represented by the formula (B1)-A1 and has an overall valence of m=2. 41 = 2. m41 is a C4 alkylene substituted with fluorine. [ka]
[0055] (B2) Sulfonyl compounds The sulfonyl compound (B2) is represented by the following formula (B2)-1 or (B2-2). [ka]
[0056] R 51 , R 52 and R 53 are each independently hydrogen, C 1-6 Alkyl, C 1-6 Alkoxy or C 6-12 aryl; preferably C 1-6 It is an alkyl group. 51 , R 52 and R 53 The alkyl moieties of may be joined together to form a cycloalkyl or aryl; m 52 = 0 or 1; preferably 0. 52 = 1 is a preferred embodiment of the present invention. R 54 is unsubstituted or halogen-substituted C 1-6 alkyl; preferably fluorine-substituted C 1-4 It is an alkyl. R 55 are each independently 5-12 Cycloalkyl or C 6-12 aryl; preferably C 5-12 It is cycloalkyl; more preferably it is C6 cycloalkyl.
[0057] Specific examples of (B2) sulfonyl compounds are listed below, but for illustrative purposes only. [ka]
[0058] (C) Solvent The composition of the present invention may contain a (C) solvent. In one embodiment of the present invention, the (C) solvent comprises, for example, water and an organic solvent. In a preferred embodiment of the present invention, the (C) solvent is selected from the group consisting of an aliphatic hydrocarbon solvent, an aromatic hydrocarbon solvent, a monoalcohol solvent, a polyol solvent, a ketone solvent, an ether solvent, an ester solvent, a nitrogen-containing solvent, a sulfur-containing solvent, and any combination thereof.
[0059] (C) Examples of the solvent include aliphatic hydrocarbon solvents such as n-pentane, i-pentane, n-hexane, i-hexane, n-heptane, i-heptane, cyclohexane, and methylcyclohexane; aromatic hydrocarbon solvents such as benzene, toluene, xylene, ethylbenzene, trimethylbenzene, methylethylbenzene, n-propylbenzene, i-propylbenzene, diethylbenzene, and i-butylbenzene; methanol, ethanol, n-propanol, i-propanol, n-butanol, i-butanol, sec-butanol, t-butanol, n-pentanol, i-pentanol, 2-methylbutanol, 2-ethylhexanol, n-nonyl alcohol, 2,6-dimethylheptanol, and the like. monoalcohol solvents such as n-decanol-4, n-decanol, cyclohexanol, benzyl alcohol, phenylmethylcarbinol, diacetone alcohol, and cresol; polyol solvents such as ethylene glycol, propylene glycol, 1,3-butylene glycol, diethylene glycol, dipropylene glycol, triethylene glycol, tripropylene glycol, and glycerin; ketone solvents such as acetone, methyl ethyl ketone, methyl n-propyl ketone, methyl n-butyl ketone, diethyl ketone, trimethylnonanone, cyclohexanone, cyclopentanone, methylcyclohexanone, 2,4-pentanedione, acetonylacetone, acetophenone, and fenchone;Ethyl ether, i-propyl ether, n-butyl ether, n-hexyl ether, 2-ethylhexyl ether, dimethyl dioxane, ethylene glycol monomethyl ether, ethylene glycol monoethyl ether, ethylene glycol diethyl ether, ethylene glycol mono-n-butyl ether, ethylene glycol mono-n-hexyl ether, ethylene glycol monophenyl ether, ethylene glycol mono-2-ethylbutyl ether, ethylene glycol dibutyl ether, diethylene glycol monomethyl ether, diethylene glycol monoethyl ether, diethylene glycol diethyl ether, diethylene glycol mono-n-butyl ether, diethylene glycol di-n-butyl ether, diethylene glycol mono-n-hexyl ether, propylene glycol monomethyl ether (PGME), propylene glycol monoethyl ether, propylene glycol monopropyl ether, propylene glycol monobutyl ether ether solvents such as propylene glycol monomethyl ether, dipropylene glycol monoethyl ether, dipropylene glycol monopropyl ether, dipropylene glycol monobutyl ether, tripropylene glycol monomethyl ether, tetrahydrofuran, and 2-methyltetrahydrofuran; ester solvents such as diethyl carbonate, methyl acetate, ethyl acetate, γ-butyrolactone, γ-valerolactone, n-propyl acetate, i-propyl acetate, n-butyl acetate, i-butyl acetate, n-butyl propionate, methyl lactate, ethyl lactate (EL), γ-butyrolactone, n-butyl lactate, n-amyl lactate, diethyl malonate, dimethyl phthalate, diethyl phthalate, propylene glycol 1-monomethyl ether 2-acetate (PGMEA), propylene glycol monoethyl ether acetate, and propylene glycol monopropyl ether acetate; nitrogen-containing solvents such as N-methylformamide; and sulfur-containing solvents such as dimethyl sulfide. Any mixture of any of these solvents may also be used.
[0060] In particular, cyclohexanone, cyclopentanone, propylene glycol monomethyl ether, propylene glycol monoethyl ether, propylene glycol monopropyl ether, propylene glycol monobutyl ether, propylene glycol dimethyl ether, propylene glycol diethyl ether, propylene glycol 1-monomethyl ether 2-acetate, propylene glycol monoethyl ether acetate, propylene glycol monopropyl ether acetate, γ-butyrolactone, ethyl lactate, and any mixture of any of these are preferred in terms of storage stability of the solution.
[0061] In terms of coatability and / or solubility of solutes, propylene glycol monomethyl ether, propylene glycol 1-monomethyl ether 2-acetate, ethyl lactate, and a mixture of any two solvents selected therefrom are preferred. For this purpose, propylene glycol 1-monomethyl ether 2-acetate is more preferred as the (C) solvent.
[0062] The (C) solvent preferably comprises an organic solvent, and the amount of water in the composition is preferably 0.1% by weight or less, more preferably 0.01% by weight or less. In relation to another layer or coating, it is preferred that the (C) solvent does not contain water. In one embodiment of the present invention, the amount of water in the composition is preferably 0.00% by weight.
[0063] In one embodiment of the present invention, the mass ratio of the solvent (C) to the total mass of the negative lift-off resist composition is 30 to 94 mass%, preferably 50 to 94 mass%, more preferably 70 to 94 mass%, and even more preferably 75 to 90 mass%.
[0064] (D) Crosslinking agent The composition of the present invention may contain (D) a crosslinking agent (hereinafter, sometimes referred to as X linker). In a negative resist, the resin and the crosslinking agent undergo a crosslinking reaction due to, for example, heat from post-exposure baking. Then, the solubility of the exposed portion of the resist layer changes.
[0065] In one embodiment of the invention, the (D) crosslinking agent comprises at least one selected from the group consisting of aryl compounds, melamine compounds, guanamine compounds, glycoluril compounds, urea compounds, epoxy compounds, thioepoxy compounds, isocyanate compounds, azide compounds, and alkenyl compounds; and each of the compounds is unsubstituted or substituted with at least one group selected from a hydroxyl group, a methylol group, an alkoxymethyl group, and an acyloxymethyl group.
[0066] In one form of the invention, the composition of the invention may comprise a single or multiple (D) crosslinkers. The composition comprises multiple (D) crosslinkers, for example, two (D) crosslinkers.
[0067] In one embodiment of the present invention, the mass ratio of the (D) crosslinking agent to the mass of the (A) alkali-soluble resin is 1 to 20 mass %, preferably 3 to 20 mass %, and more preferably 5 to 15 mass %.
[0068] The (D) crosslinking agent of the present invention may comprise a (D1) crosslinking agent represented by formula (D1) and / or a (D2) crosslinking agent represented by formula (D2). In one embodiment of the present invention, the composition of the present invention comprises a single (D2) crosslinking agent without containing any other crosslinking agent.
[0069] In addition to the specific examples of formula (D1) or (D2) described below, the compounds described below are other specific examples, but are for illustrative purposes only. [ka]
[0070] (D1) Crosslinking agent The crosslinking agent (D1) is represented by the formula (D1). [ka]
[0071] R 61 is C 2-8 Alkoxyalkyl; preferably C 2-4 It is methoxylalkyl; more preferably -CH2-O-CH3. R 62 is C 2-8 Alkoxyalkyl; preferably C 2-4 It is methoxylalkyl; more preferably -CH2-O-CH3. R 63 is unsubstituted or C 1-6 Alkyl-substituted C 6-10 Aryl, unsubstituted or C 1-6 Alkyl-substituted C 1-8 Alkyl, or -NR 61 R 62 R 63 C 6-10 Aryl is preferably phenyl or naphthyl, more preferably phenyl. R 63 C 1-8 Alkyl is preferably methyl, ethyl, propyl, butyl, pentyl or hexyl, more preferably methyl or butyl. 6-10 C to substitute aryl 1-8 Alkyl, or R 63 C 1-8 Alkyl is preferably methyl, ethyl, isopropyl or butyl, more preferably methyl. R 63 , unsubstituted C 6-10 Aryl and C 1-8 More preferably, R is alkyl. Even more preferably, R 63 Ha-NR 61 R 62 R 61 and R 62 The definitions and preferred forms thereof are each independently the same as above. R 64 is unsubstituted or C 1-6 Alkyl-substituted C 6-10 Aryl, unsubstituted or C 1-6 Alkyl-substituted C 1-8 Alkyl, or -NR61 R 62 R 64 C 6-10 Aryl is preferably phenyl or naphthyl, more preferably phenyl. R 64 C 1-8 Alkyl is preferably methyl, ethyl, propyl, butyl, pentyl or hexyl, more preferably methyl or butyl. 6-10 C to substitute aryl 1-8 Alkyl, or R 64 C 1-8 Alkyl is preferably methyl, ethyl, isopropyl or butyl, more preferably methyl. R 64 , unsubstituted C 6-10 Aryl and C 1-8 More preferably, R is alkyl. Even more preferably, R 64 -NR 61 R 62 R 61 and R 62 The definitions and preferred forms thereof are each independently the same as above.
[0072] Specific examples of (D1) crosslinkers represented by formula (D1) are listed below for illustrative purposes only. [ka]
[0073] In one embodiment of the present invention, the mass ratio of the (D1) crosslinking agent to the mass of the (A) alkali-soluble resin is preferably 0.10 to 8 mass %, more preferably 0.5 to 5 mass %, and even more preferably 0.5 to 3 mass %.
[0074] (D2) Crosslinking agent The crosslinking agent (D2) is represented by the formula (D2). [ka]
[0075] R65 is unsubstituted or C 1-6 Alkyl-substituted C 1-20 It is an alkyl group. 65 C 1-20 The alkyl may be a straight chain alkyl or a branched alkyl. R 65 C 1-20 The alkyl is preferably C 1-10 R is alkyl, more preferably methyl, ethyl, propyl, butyl, pentyl, hexyl, heptyl, octyl, or -C(CH)-CH-C(CH), and even more preferably -C(CH)-CH-C(CH). 65 C 1-20 C to substitute alkyl 1-6 Alkyl is preferably methyl, ethyl, isopropyl or butyl, more preferably methyl. R 65 , unsubstituted C 1-20 Alkyl is more preferred. I D2 is 1, 2, 3 or 4; preferably 2 or 3; and more preferably 2. m D2 is 0, 1 or 2; preferably 0 or 1; and more preferably 1. n D2 is 0, 1 or 2; preferably 1. I D2 +m D2 +n D2 <=6.
[0076] Specific examples of (D2) crosslinkers represented by formula (D2) are listed below for illustrative purposes only. [ka]
[0077] In one embodiment of the present invention, the mass ratio of the crosslinking agent (D2) to the mass of the alkali-soluble resin (A) is preferably 0.50 to 40 mass%, more preferably 1 to 20 mass%, and even more preferably 5 to 15 mass%.
[0078] In one embodiment of the present invention, a resist film formed from the composition of the present invention using any one of the above amounts of crosslinking agent can exhibit good pattern profile and strippability.
[0079] Additives The composition of the present invention may further comprise further additives, which may be selected from the group consisting of quenchers, surfactants, dyes, contrast enhancers, acids, radical generators, adhesion enhancers to the substrate, bases, surface levelling agents and antifoaming agents.
[0080] In one embodiment of the present invention, the mass ratio of the other additive to the mass of the alkali-soluble resin (A) is preferably 0.05 to 10 mass%, more preferably 0.10 to 5 mass%, and even more preferably 0.10 to 2 mass%. Unless specifically stated below, in one embodiment of the present invention, the composition of the present invention does not contain any of these additives (0 mass%).
[0081] As dyes, monomeric dyes and azo dyes may be in the form of the present invention. The dyes described in WO 2001 / 61410 are in other forms. As dyes, 9-anthracenemethanol is in the preferred form of the present invention.
[0082] Quencher In order to improve properties such as resist pattern shape and long-term stability (post-exposure stability of a latent image formed by patternwise exposure of a resist layer), a quencher may be added to the composition of the present invention. As the quencher, an amine is preferable, and more preferably, a secondary aliphatic amine or a tertiary aliphatic amine can be used. Here, the aliphatic amine is a C 2-9 Alkyl or C 2-9 C refers to an alkyl alcohol amine. The alkyl moiety may be substituted with one or more alkylenes by an ether linker. 3-6 Tertiary aliphatic amines with alkyl alcohols are more preferred.
[0083] Specific examples of the quencher include trimethylamine, diethylamine, triethylamine, di-n-propylamine, tri-n-propylamine, triisopropylamine, tributylamine, tripentylamine, trioctylamine, diethanolamine, N,N-dicyclohexylmethylamine, triethanolamine, and tris[2-(2-methoxyethoxy)ethyl]amine.Triethanolamine and tris[2-(2-methoxyethoxy)ethyl]amine are more preferred.
[0084] In one embodiment of the present invention, the mass ratio of the quencher to the mass of the alkali-soluble resin (A) is preferably 0.05 to 5 mass %, more preferably 0.10 to 2 mass %, and even more preferably 0.10 to 1 mass %.
[0085] Surfactants The compositions of the present invention may also contain surfactants, which are useful for reducing pinholes or streaks in the coating and for increasing the spreadability and / or solubility of the composition.
[0086] In one embodiment of the present invention, the mass ratio of the surfactant to the mass of the alkali-soluble resin (A) is preferably 0.01 to 10 mass %, more preferably 0.05 to 5 mass %, and even more preferably 0.05 to 2 mass %.
[0087] Examples of the surfactant include polyoxyethylene alkyl ether compounds such as polyoxyethylene lauryl ether, polyoxyethylene stearyl ether, and polyoxyethylene oleyl ether; polyoxyethylene alkylaryl ether compounds such as polyoxyethylene octylphenol ether and polyoxyethylene nonylphenol ether; polyoxyethylene-polyoxypropylene block copolymer compounds; sorbitan fatty acid ester compounds such as sorbitan monolaurate, sorbitan monopalmitate, sorbitan monostearate, sorbitan trioleate, and sorbitan tristearate; and polyoxyethylene sorbitan fatty acid ester compounds such as polyoxyethylene sorbitan monolaurate, polyoxyethylene sorbitan monopalmitate, polyoxyethylene sorbitan monostearate, and polyoxyethylene sorbitan tristearate. Other examples of surfactants include fluorosurfactants such as F-TOP (trade name) EF301, EF303, and EF352 (Tochem Products Co., Ltd.), Megaface (trade name) F171, F173, R-08, R-30, and R-2011 (DIC Corporation), Fluorad FC430 and FC431 (Sumitomo 3M Limited), Asahiguard (trade name) AG710 (Asahi Glass Co., Ltd.), Surflon S-382, SC101, SC102, SC103, SC104, SC105, and SC106 (Asahi Glass Co., Ltd.); and organosiloxane polymers such as KP341 (Shin-Etsu Chemical Co., Ltd.).
[0088] Lift-off process One exemplary step form of the lift-off patterning process is shown in the schematic cross-sectional view of Figure 1. As shown in (a), a substrate is prepared, and then a resist composition is coated on the substrate to obtain a resist layer (shown in (b)). Next, as shown in (c), it is exposed to actinic radiation through a designed mask. After that, the resist layer is developed to form a resist pattern as shown in (d). The resist pattern has walls and trenches.
[0089] For the subsequent peeling process, a resist pattern having an inverse tapered shape is preferable. For example, the resist pattern has a good inverse tapered shape in which the side surface of the substrate and the wall of the resist pattern preferably form an angle of less than 90 degrees (more preferably 55 degrees or more and less than 90 degrees, and even more preferably 55 to 80 degrees). The angle can be measured from a cross-sectional photograph using a SEM (scanning electron microscope).
[0090] Then, as shown in (e), a metal is applied (preferably evaporated) onto the resist pattern to form a metal film. The metal film is preferably an electrode. The metal film is formed on the walls and trenches of the resist pattern. It is preferable that the resist layer has a thickness sufficient to create a gap between the metal film on the walls and the trenches, so that the resist layer stripping solution can penetrate through the gap.
[0091] Then, as shown in (f), the resist pattern and the metal film thereon are peeled off (preferably with a resist layer stripping solution) to obtain a metal film pattern on the substrate. Here, the metal film formed on the walls of the resist pattern is peeled off, leaving the designed metal film pattern formed on the trenches of the resist pattern.
[0092] For comparison, the resist etching process shown in the schematic cross-sectional view of Figure 2 is briefly described below. (a') shows the preparation of a substrate. (b') shows the formation of a metal film (e.g., an electrode), and (c') shows the formation of a resist layer on the metal film. (d') shows exposure through a mask, and (e') shows development to form a resist pattern. (f') shows dry etching to peel off the exposed metal film portion, and (g') shows the peeling off of the resist pattern remaining on the remaining metal film portion.
[0093] Formation of resist layer The composition of the present invention is applied onto the substrate. Prior to this application, the substrate surface may be pretreated with, for example, a 1,1,1,3,3,3-hexamethyldisilazane solution. The composition of the present invention undergoes a reaction under irradiation, and the irradiated portion becomes more resistant to dissolution by a developer. For application, a known method, for example, a spin coating method, can be used. Then, the applied resist composition is baked to remove the solvent in the composition to form a resist layer. The baking temperature varies depending on the composition used, but is preferably 70 to 150°C (more preferably 90 to 150°C, and even more preferably 100 to 140°C). This can be performed for 10 to 180 seconds, preferably 30 to 90 seconds, on a hot plate, or for 1 to 30 minutes in a hot gas atmosphere (for example, in a clean oven). The thickness of the formed resist layer is preferably 0.40 to 5.00 μm (more preferably 0.40 to 3.00 μm, and even more preferably 0.50 to 2.00 μm).
[0094] In the method for producing a resist pattern of the present invention, an underlayer film may be interposed between the substrate and the resist film so that the substrate and the resist film do not directly contact each other. Examples of the underlayer film include an underlayer antireflective film (BARC layer), an inorganic hard mask underlayer film (e.g., silicon oxide film, silicon nitride film, silicon oxynitride film, etc.), and an adhesion film. The underlayer film may be composed of a single layer or multiple layers. Since the resist layer according to the present invention has good stripping properties, it is a preferred embodiment that the resist film is formed on a substrate without an underlayer film, and this can reduce the unintended risk of dissolving the underlayer film (e.g., BARC) during resist development, which can make process control difficult. Other layers (eg, top antireflective coating, TARC) may be formed over the resist film.
[0095] Resist patterning The resist film is exposed through a predetermined mask. The wavelength of light used for exposure is not particularly limited. Exposure is performed with light having a wavelength of 13.5 to 365 nm (preferably, 13.5 to 248 nm). KrF excimer laser (248 nm), ArF excimer laser (193 nm), or extreme ultraviolet light (13.5 nm) are preferred; KrF excimer laser is more preferred. These wavelengths are allowed to vary within ±1%. The resist pattern created by the composition according to the present invention can be formed into a good shape and exhibit good peelability, so that a mask designed more finely can be used. For example, a mask having a line-space width of preferably 1.0 μm or less can be used, and more preferably a mask having a line-space width of less than 1.0 μm can be used.
[0096] If necessary, post-exposure baking can be performed after the exposure. The temperature of the post-exposure baking is selected from the range of 80 to 150° C., preferably 90 to 140° C., and the heating time of the post-exposure baking is selected from the range of 0.3 to 5 minutes, preferably 0.5 to 2 minutes.
[0097] Next, development is performed using a developer. The unexposed portion of the resist layer of the present invention is peeled off by development to form a resist pattern. The developer used for development in resist pattern formation is preferably a 2.38 mass % (±1% concentration change allowed) TMAH aqueous solution. Additives such as surfactants may be added to the developer. The temperature of the developer is generally selected from the range of 5 to 50°C, preferably 25 to 40°C, and the development time is generally selected from the range of 10 to 300 seconds, preferably 30 to 90 seconds. As the development method, a known method such as paddle development can be used. It is preferable that the resist layer is effectively peeled off and does not remain in the trench portion of the resist pattern.
[0098] After development, the resist pattern can be washed with water or a cleaning solution so as to replace the developer with water and / or a cleaning solution. The substrate can then be dried, for example, by spin drying.
[0099] Fabrication of metal film patterns on substrates A metal is applied onto the resist pattern to form a metal film. Known methods can be used. Evaporation and coating are preferred (vapor phase deposition is more preferred). In this specification, metal includes metal oxide. The metal film preferably has good electrical conductivity. Single or mixed metals can be used. The thickness of the formed metal film is preferably effectively smaller than the thickness of the resist pattern wall (preferably -80 to -20% of the thickness, more preferably -70 to -30% of the thickness), in order to create a gap through which the resist layer stripping solution can penetrate and reach the resist pattern wall.
[0100] The resist pattern and the metal film thereon are peeled off to obtain a metal film pattern on the substrate (in a narrow sense, this process can be called "lift-off"). The metal film formed on the walls of the resist pattern is peeled off, leaving the designed metal film pattern formed on the trenches of the resist pattern. This peeling can be performed using a known method, for example, a resist layer stripping solution. One form of the resist layer stripping solution is AZ Remover 700 (Merck Performance Materials Co., Ltd.). The patterned metal film is preferably an electrode on the substrate, which can be used to create an element in a later process.
[0101] Element manufacturing Thereafter, if necessary, the substrate is further processed to form an element. Such further processing can be performed using known methods. After the formation of the element, if necessary, the substrate is cut into chips, which are connected to a lead frame and packaged with resin. Preferably, the element is a semiconductor element, a high-frequency module, a solar cell chip, an organic light-emitting diode, and an inorganic light-emitting diode. One preferred form of the element of the present invention is a semiconductor element. Another preferred form of the element of the present invention is a high-frequency module, which can be made of a transmitter (including an IC chip) and a receiver.
[0102] Working Example The present invention will be described below with reference to examples. These examples are for illustrative purposes only and are not intended to limit the scope of the present invention. In the following description, "parts" are based on mass unless otherwise specified.
[0103] Preparation Example 1 of Example Composition 1 Prepare each of the components described below. [ka] Surfactant: Megafac R2011, DIC Corporation As the solvent, PGMEA is used.
[0104] Each component is added to a solvent. The weight percentages of the crosslinker A1, PAG A, PAG B, quencher, and surfactant are 10.66, 3.37, 0.62, 0.39, and 0.10% by weight, respectively, of the single or multiple polymers taken as 100% by weight. This 100% weight of polymer is based on the solid content.
[0105] The solution is then stirred to ensure all components are dissolved. The solution is mixed and solvent is added until the total solids concentration is 23.0% by weight. The resulting solution is filtered through a 0.1 μm capsule filter.
[0106] The resulting working composition is designated as Composition 1 in Table 1-1 below.
[0107] Preparation Examples 2 to 15 of Compositions 2 to 15 The preparation is carried out in the same manner as Preparation Example 1, except that the ingredients and / or amounts are changed as described in Table 1-1 below. Example compositions 2 to 15 are obtained.
[0108] [Table 1-1] In Table 1-1, "composition" means "composition." The same applies to the following tables.
[0109] Example of preparing a substrate for evaluation of embodiment composition 1 The substrate used in the following evaluation is prepared as follows. The surface of a silicon substrate (SUMCO Corporation, 8 inches) is treated with a 1,1,1,3,3,3-hexamethyldisilazane solution at 90° C. for 60 seconds. Example composition 1 is spin-coated thereon, and soft-baked at 110° C. for 60 seconds to form a resist layer with a thickness of 1.30 μm on the substrate. This is exposed through a mask using an FPA-3000EX5 (Canon). The mask used has multiple 1.0 μm lines and a line:space=1:1 area. The mask also has gradually narrower line-and-space areas. The widths of these lines are 1.0 μm, 0.9 μm, 0.8 μm, 0.7 μm, 0.6 μm, 0.5 μm, 0.45 μm, 0.40 μm, 0.38 μm, 0.36 μm, 0.34 μm, 0.32 μm, 0.30 μm, 0.28 μm, 0.26 μm, 0.24 μm, 0.22 μm, 0.20 μm, 0.18 μm, 0.16 μm, 0.14 μm, 0.12 μm, and 0.10 μm. There are multiple lines of the same width on the mask, and each line:space ratio is 1:1. For better understanding, the mask design is depicted in FIG. 3, which is for illustrative purposes and not for limiting the scope of the present invention. In FIG. 3, an inaccurate scale is used for better understanding.
[0110] The mask used also has multiple 1.0 μm lines and regions (isolated regions) with a line:space ratio of 1:5. The mask also has regions with lines and spaces that gradually narrow. The widths of these lines are 1.0 μm, 0.9 μm, 0.8 μm, 0.7 μm, 0.6 μm, 0.5 μm, 0.45 μm, 0.40 μm, 0.38 μm, 0.36 μm, 0.34 μm, 0.32 μm, 0.30 μm, 0.28 μm, 0.26 μm, 0.24 μm, 0.22 μm, 0.20 μm, 0.18 μm, 0.16 μm, 0.14 μm, 0.12 μm, and 0.10 μm. The mask has multiple lines of the same width, with each line:space ratio being 1:5. For better understanding, the mask design is depicted in Figure 4, which is for illustrative purposes and not for the purpose of limiting the scope of the invention, and in Figure 4, an inaccurate scale is used for better understanding.
[0111] The substrate is post-exposure baked (PEB) at 110°C for 60 seconds. The resist layer is then paddle developed using a 2.38% tetramethylammonium hydroxide (TMAH) aqueous solution for 60 seconds. With the paddle developer in a mound on the substrate, pure water is started to flow onto the substrate. The paddle developer is then replaced with pure water while the substrate is rotated. The substrate is then rotated at 2,000 rpm and spin-dried.
[0112] Examples of preparing evaluation substrates for compositions 2 to 15 Except for changing Working Composition 1 to Working Compositions 2 to 15, each substrate is prepared in the same manner as above.
[0113] Example of evaluation of resist pattern shape The shape of the resist pattern exposed through a 0.5 μm space in a dense area (line:space=1:1) on each of the above substrates is evaluated using an SEM device SU8230 (Hitachi High-Technologies Corporation). The evaluation criteria are as follows: A: No resist pattern collapse is observed B: Resist pattern collapse is observed The evaluation results are shown in Table 1-2 below.
[0114] Resolution evaluation example The exposure is performed with an exposure dose that can reproduce a 400 nm pattern with a 400 nm slit (line). Cross-sectional SEM observation confirms that the pattern shape is continuous from the 400 nm pattern to a narrower pattern. Here, the resolution is the space width just before the space width at which the pattern collapses or the gap is filled.
[0115] The evaluation criteria are as follows: X: In dense areas, the resolution is 340 nm or less Y: In dense areas, the resolution is greater than 340 nm X: In isolated areas, the resolution is 300 nm or less. Y: Resolution is greater than 300 nm in isolated areas
[0116] The overall evaluation is categorized as follows: A: Both dense and isolated areas are rated X. B: At least one of the dense and isolated areas is rated Y.
[0117] The evaluation results are shown in Table 1-2 below. [Table 1-2]
[0118] Preparation Examples 16 to 20 of Working Compositions 16 to 20 and Reference Preparation Example 1 of Reference Composition 1 The preparation is carried out in the same manner as Preparation Example 1, except that the ingredients and / or amounts are changed as described in Table 2-1 below, resulting in a total solids concentration of 13.0% by weight.
[0119] Working compositions 16-20 and reference composition 1 are obtained. [ka] [Table 2-1] In Table 2-1, "ref." means "reference." The same applies to the following tables.
[0120] Example of preparing a substrate for evaluation of embodiment composition 16 The substrates used in the following evaluations are prepared as follows: A BARC (underlayer antireflective coating) composition AZ KrF-17B (Merck Performance Materials, hereafter referred to as MPM) is spin-coated onto the surface of a silicon substrate (SUMCO, 8 inches) and baked at 180° C. for 60 seconds to obtain a BARC coating with a thickness of 38 nm. Working composition 16 is spin-coated thereon and soft-baked at 110° C. for 60 seconds to form a resist layer having a thickness of 0.50 μm on the substrate.
[0121] Exposure and post-treatment are carried out in the same manner as described in Example 1 for preparing a substrate for evaluation of Working Composition 1, except that the mask is changed to one having only dense regions. Then, a substrate for evaluation of Working Composition 16 is obtained.
[0122] Examples of preparing substrates for evaluation of working compositions 17 to 20 and reference composition 1 Except for changing Working Composition 16 to Working Compositions 17 to 20 and Reference Composition 1, each substrate is prepared in the same manner as in the example for preparing a substrate for evaluation of Working Composition 16.
[0123] Example of evaluation of resist pattern shape The shapes of resist patterns exposed through a 0.25 μm space in a dense area (line:space=1:1) on each substrate of Working Compositions 17 to 20 and Reference Composition 1 are evaluated using an SEM apparatus SU8230.
[0124] The evaluation criteria are as follows: A: No resist pattern collapse is observed B: Resist pattern collapse is observed The evaluation results are shown in Table 2-2 below.
[0125] Resolution evaluation example The exposure is performed with an exposure dose that can reproduce a 300 nm pattern with a 300 nm slit (line). The cross-sectional SEM is observed to confirm that the pattern shape is continuous from the 400 nm pattern to the narrower pattern. Here, the resolution is the space width just before the space width at which the space collapses.
[0126] The evaluation criteria are as follows: A: Resolution is 260nm or less B: Resolution is greater than 260 nm
[0127] [Table 2-2] The resist layers prepared from the working compositions exhibit better resolution than those prepared from the reference compositions.
[0128] Preparation Examples 21 to 24 of Compositions 21 to 24 The preparation is carried out in the same manner as Preparation Example 1, except that the ingredients and / or amounts are changed as described in Table 3-1 below, resulting in a total solids concentration of 24.0% by weight. Example compositions 21 to 24 are obtained. [ka] [Table 3-1]
[0129] Examples of preparing evaluation substrates for compositions 21 to 24 Each substrate is procured in the same manner as in the example for preparing an evaluation substrate for Example Composition 1, except that Example Composition 1 is changed to Example Compositions 21 to 24, a mask having only dense regions is used, and a resist layer having a thickness of 1.50 μm is formed on the substrate.
[0130] Example of evaluation of resist pattern shape The shape of the resist pattern exposed through a 0.7 μm space in a dense region (line:space=1:1) on each substrate of the working compositions 21 to 24 is evaluated by an SEM device SU8230. The evaluation criteria are as follows. A: No resist pattern collapse is observed B: Resist pattern collapse is observed The evaluation results are shown in Table 3-2 below.
[0131] Peelability evaluation example 20 mm x 20 mm pieces are prepared by cutting out each substrate of Example Compositions 21 to 24. These pieces are baked at 110°C for 90 seconds. Each piece is placed on a petri dish, sufficiently away from the center of the dish. Resist layer stripping solution (AZ Remover 700, MPM Co., Ltd.) is slowly added to the petri dish. While mixing with a stirrer, the solution is heated to 70°C. After mixing the solution for 10 minutes, the pieces are removed. The resist layer stripping solution is then washed away with sufficient pure water. The pieces are then dried by N2 gas spray.
[0132] The positions of the resist patterns that were exposed before being peeled off are observed with an optical microscope, starting from 1.0 μm line-space exposure to increasingly narrower ones. The evaluation criteria are as follows: A: The exposed resist pattern with a line-space of 0.7 μm or less is clearly peeled off. B: Exposed resist patterns with lines and spaces larger than 0.7 μm are clearly peeled off.
[0133] The evaluation results are shown in Table 3-2 above. [Table 3-2]
[0134] The resist pattern produced from the embodiment composition can be clearly peeled off.
[0135] 1. Substrate 2. Resist layer 3. Mask 4. Radiation 5. Metal Film 6. Substrate 7. Metal Film 8. Resist layer 9. Mask 10. Radiation 11.1.0μm wide lines 12.1.0μm wide space 13. Area with 1.0 μm wide lines and line:space = 1:1 14.0.9μm wide lines 15. 0.9μm wide space 16. Area with 0.9 μm wide lines and line:space = 1:1 17.1.0μm wide lines 18.5.0μm wide space 19. Area with 1.0 μm wide lines and line:space ratio of 1:5 20.0.9μm wide line 21.4.5μm wide space 22. Area with 0.9μm wide lines and line:space=1:5
Claims
1. A negative lift-off resist composition comprising one or more (A) alkali-soluble resins and one or more (B) photoacid generators; Where: The alkali-soluble resin (A) comprises an (A1) resin and an (A2) resin; (B) the photoacid generator comprises only (B1) an onium salt or (B2) a sulfonyl compound; However, (i) when a negative lift-off resist composition contains a single (A) alkali-soluble resin, the negative lift-off resist composition contains a plurality of (B) photoacid generators, and (ii) when a negative lift-off resist composition contains a single (B) photoacid generator, the negative lift-off resist composition contains a plurality of (A) alkali-soluble resins; The (A1) resin is represented by the following formula (A1): 【Chemistry 1】 R 11 , R 12 , R 14 , R 15 , R 17 and R 18 are each independently hydrogen, C 1-6 alkyl, carboxyl, halogen or cyano; R 13 and R 16 are each independently 1-6 Alkyl, C 1-6 alkoxy, halogen or cyano; R 19 is C 1-15 Alkyl or C 1-15 Alkoxy, where R 19 The alkyl moiety of may form a saturated and / or unsaturated ring; m 11 is a number from 0 to 4, and n 11 is a number from 1 to 3, m 11 +n 11 ≦5, m 12 is a number between 0 and 5, p A1 , q A1 and r A1 is the number of repetitions, and [p A1 / (p A1 +q A1 +r A1 ) is 30-98%, and [q A1 / (p A1 +q A1 +r A1 ) is 5-40%, and [r A1 / (p A1 +q A1 +r A1 ) )] is 0-70%; (A1) the weight average molecular weight (Mw) of the resin is 5,000 to 100,000; The (A2) resin is represented by the following formula (A2): 【Chemistry 2】 R 21 , R 22 , R 24 and R 25 are each independently hydrogen, C 1-6 alkyl, carboxyl, halogen or cyano; R 23 is C 1-6 Alkyl, C 1-6 alkoxy, halogen or cyano; R 26 is C 1-15 Alkyl or C 1-15 Alkoxy, where R 26 The alkyl moiety of may form a saturated and / or unsaturated ring; m 21 is a number from 0 to 4, and n 21 is a number from 1 to 3, m 21 +n 21 ≦5, p A2 and r A2 is the number of repetitions, and [p A2 / (p A2 +r A2 ) is 30-100%, and [r A2 / (p A2 +r A2 ) )] is 0-70%; The onium salt (B1) is represented by the following formula (B1): [B m+ cation] [B m- Anion] (B1) B m+ The cation is represented by the following formula (B1)-C1 and / or formula (B1)-C2, and has a valency of m as a whole, where m is 1 to 3: 【Chemistry 3】 R 31 , R 32 , R 33 , R 34 and R 35 are each independently 1-6 Alkyl, C 1-6 Alkoxy or C 6-12 is aryl, m 31 , m 32 , m 33 , m 34 and m 35 are each independently a number from 0 to 3; B m- The anion is represented by the following formula (B1)-A1, (B1)-A2 and / or (B1)-A3: 【Chemistry 4】 R 41 , R 42 and R 43 are each independently unsubstituted or C 1-6 Alkyl-substituted C 6-12 Aryl, unsubstituted or substituted with halogen or carbonyl 1-12 is alkyl, m 41 = 1 or 2; The sulfonyl compound (B2) is represented by the following formula (B2)-1 or (B2-2): 【Chemistry 5】 R 51 , R 52 and R 53 are each independently hydrogen, C 1-6 Alkyl, C 1-6 Alkoxy or C 6-12 aryl, where R 51 , R 52 and R 53 The alkyl moieties of may be joined together to form a cycloalkyl or aryl; m 52 = 0 or 1, R 54 is unsubstituted or halogen-substituted C 1-6 is alkyl, R 55 are each independently 5-12 Cycloalkyl or C 6-12 is aryl, A negative lift-off resist composition.
2. 2. The negative lift-off resist composition according to claim 1, further comprising a solvent (C).
3. 3. The negative lift-off resist composition according to claim 1, wherein a mass ratio of the alkali-soluble resin (A) to the total mass of the negative lift-off resist composition is 5 to 50 mass %; and a mass ratio of the photoacid generator (B) to the mass of the alkali-soluble resin (A) is 1 to 20 mass %.
4. 4. The negative lift-off resist composition according to claim 1, further comprising a crosslinking agent (D); wherein the crosslinking agent (D) comprises at least one selected from the group consisting of aryl compounds, melamine compounds, guanamine compounds, glycoluril compounds, urea compounds, epoxy compounds, thioepoxy compounds, isocyanate compounds, azide compounds, and alkenyl compounds; and each of these compounds is unsubstituted or substituted with at least one group selected from a hydroxyl group, a methylol group, an alkoxymethyl group, and an acyloxymethyl group.
5. The negative lift-off resist composition according to any one of claims 1 to 4, further comprising a crosslinking agent (D), wherein the crosslinking agent (D) comprises a crosslinking agent (D1) represented by formula (D1) and / or a crosslinking agent (D2) represented by formula (D2); 【Chemistry 6】 R 61 is C 2-8 Alkoxyalkyl, R 62 is C 2-8 is an alkoxyalkyl; R 63 is unsubstituted or C 1-6 Alkyl-substituted C 6-10 Aryl, unsubstituted or C 1-6 Alkyl-substituted C 1-8 Alkyl, or -NR 61 R 62 and R 64 is unsubstituted or C 1-6 Alkyl-substituted C 6-10 Aryl, unsubstituted or C 1-6 Alkyl-substituted C 1-8 Alkyl, or -NR 61 R 62 and 【Chemistry 7】 R 65 is unsubstituted or C 1-6 Alkyl-substituted C 1-20 is alkyl, I D2 is 1, 2, 3 or 4; m D2 is 0, 1 or 2; n D2 is 0, 1 or 2, and I D2 +m D2 +n D2 A negative lift-off resist composition, wherein the resistivity is ≦6.
6. 6. The negative lift-off resist composition according to claim 5, wherein the crosslinking agent (D) comprises a crosslinking agent (D2) represented by formula (D2):
7. n D2 7. The negative lift-off resist composition according to claim 5, wherein R is 1 or 2.
8. (A2) The Mw of the resin is 2,000 to 20,000; 8. The negative lift-off resist composition according to claim 1.
9. The negative lift-off resist composition according to any one of claims 1 to 8, further comprising at least one additive selected from the group consisting of a quencher, a surfactant, a dye, a contrast enhancer, an acid, a radical generator, an agent for enhancing adhesion to a substrate, a base, a surface leveling agent, and an antifoaming agent.
10. forming a coating of the negative lift-off resist composition according to any one of claims 1 to 9 above a substrate; baking the resist composition to form a resist layer; exposing the resist layer; developing the resist layer to form a resist pattern; The method for producing a resist pattern comprising the steps of:
11. The method for producing a resist pattern according to claim 10, wherein the exposure is performed with light having a wavelength of 13.5 to 365 nm.
12. Producing a resist pattern according to claim 10 or 11; forming a metal film on the resist pattern; and Stripping off the remaining resist pattern and the metal film thereon; A method for producing a metal film pattern on a substrate, comprising:
13. A method for producing an element, comprising the method for producing a resist pattern or a metal film pattern on a substrate according to any one of claims 10 to 12.
Citation Information
Patent Citations
Sulfonyl oxime compound, radiation-sensitive acid generator using the same, positive-type radiation- sensitive resin composition, and negative-type radiation- sensitive resin composition
JP2003137860A
Resist material, resist pattern and its production method as well as semiconductor device and its production method
JP2003162060A
Photosensitive composition and acid generating agent
JP2004117688A
Negative photoresist composition
JP2005037414A
Photosensitive composition, compound for use in photosensitive composition, and pattern-forming method using photosensitive composition
JP2008100988A