Shielding film and circuit board

The shielding film with a higher grayscale contrast structure layer and electromagnetic shielding layer addresses the issue of unclear identification codes on small substrates by enhancing clarity and resolution through a clear contrast mechanism.

JP7557609B2Active Publication Date: 2024-09-27GUANGZHOU FANGBANG ELECTRONICS
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023504656
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-07-24
Filing Date
2020-09-10
Publication Date
2024-09-27
Estimated Expiration
2040-09-10

AI Technical Summary

Technical Problem

The challenge of printing clear identification codes on small, flexible substrates in electronic products is exacerbated by miniaturization, leading to unclear and inaccurate identification due to size constraints.

Method used

A shielding film comprising a first film layer, a contrast structure layer, and an electromagnetic shielding layer, where the contrast structure layer has a higher grayscale value than the first film layer, allowing for a clear contrast and formation of a hollow pattern for the identification code, enhancing clarity and resolution.

Benefits of technology

The solution provides high clarity and accuracy for identification codes, enabling easier tracking of electronic components by forming a strong contrast between the contrast structure layer and the first film layer, improving identification precision.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007557609000008
    Figure 0007557609000008
  • Figure 0007557609000002
    Figure 0007557609000002
  • Figure 0007557609000007
    Figure 0007557609000007
Patent Text Reader

Abstract

Shielding film and circuit board. The shielding film includes a first film layer (11), a contrast structure layer (12), and an electromagnetic shielding layer (13), the first film layer (11) is disposed on a first side of the electromagnetic shielding layer (13), the contrast structure layer (12) is disposed on the first side of the electromagnetic shielding layer (13), the color grayscale value of the contrast structure layer (12) is greater than the color grayscale value of the first film layer (11), and a hollow pattern of an identification code is formed on the layer of the contrast structure layer (12) and the first film layer (11) that is farther from the electromagnetic shielding layer (13). The strong light-dark or color contrast between the contrast structure layer (12) and the first film layer (11) of the shielding film allows users to obtain a clear identification code, improving the accuracy and precision of the identification code, and thereby facilitating tracking of components or electronic products identified by the identification code.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD OF THE DISCLOSURE This application relates to the electronics field, for example, to shielding films and circuit boards. [Background technology]

[0002] With the rapid development of the electronics industry, electronic products are further developed toward miniaturization, light weight and high density packaging, which has greatly promoted the development of flexible circuit boards, and the connection and integration of element devices and conductors is gradually realized. Flexible circuit boards can be widely used in industries such as mobile phones, liquid crystal displays, communications, and aerospace.

[0003] With the integration of various functions in electronic products such as smartphones, the internal components are gradually becoming higher in frequency and speed. For example, among the various functions of a mobile phone, in addition to the existing voice transmission function, the camera function has become an essential function, and wireless local area networks (WLANs), global positioning systems (GPSs) and Internet access functions have also become widespread. In addition, future sensing components will be gradually integrated, and the trend of higher frequency and higher speed for the internal components of smartphones is inevitable.

[0004] In conventional electronic products, various components are integrated inside the electronic product, and in order to better track the electronic product or a component inside the electronic product, an identification code is often provided inside the electronic product, and the identification code can be scanned to track the information of the electronic product or a component inside the electronic product. In the conventional technology, an identification code (such as a two-dimensional code) is printed on a steel plate, but the size of the steel plate is limited due to the thinning of electronic products, so that it is difficult to print a two-dimensional code on the steel plate. In the conventional technology, an identification code can be printed on a flexible substrate of an electronic product by a printing method, but due to the small size of the flexible substrate, the printed identification code is not clear, the accuracy cannot meet the identification requirements, and there are also situations where the identification code cannot be printed on a small-sized flexible substrate. Summary of the Invention [Means for solving the problem]

[0005] An embodiment of the present application provides a shielding film and a circuit board to provide an identification code on the shielding film, thereby achieving improved clarity and resolution of the identification code.

[0006] In a first aspect, embodiments of the present application provide a shielding film including a first film layer, a contrast structure layer, and an electromagnetic shielding layer; the first film layer is disposed on a first side of the electromagnetic shielding layer; the contrast structure layer is disposed on a first side of the electromagnetic shielding layer; The grayscale value of the color of the contrast structure layer is greater than the grayscale value of the color of the first film layer.

[0007] In a second aspect, the present embodiment provides a shielding film comprising a first film layer, a contrast structure layer, and an electromagnetic shielding layer; the first film layer is disposed on a first side of the electromagnetic shielding layer; the contrast structure layer is disposed on a first side of the electromagnetic shielding layer; The contrast structure layer has a color grayscale value greater than the color grayscale value of the first film layer, and a hollow pattern of an identification code is formed in the layer farther from the electromagnetic shielding layer among the contrast structure layer and the first film layer.

[0008] In a third aspect, an embodiment of the present application provides a circuit board, the circuit board including a printed circuit board and a shielding film according to any embodiment of the present application, the shielding film having an adhesive film layer disposed on a side of the electromagnetic shielding layer away from the first film layer; The printed circuit board is attached to one side of the adhesive film layer of the shielding film.

[0009] In the present application, the shielding film includes an electromagnetic shielding layer for shielding electromagnetic interference, and a first film layer and a contrast structure layer are disposed on a first side of the electromagnetic shielding layer, and the first film layer may be disposed between the electromagnetic shielding layer and the contrast structure layer, and the contrast structure layer may be disposed between the electromagnetic shielding layer and the first film layer, and the color grayscale value of the contrast structure layer needs to be greater than the color grayscale value of the first film layer, so that a clear contrast in brightness between the contrast structure layer and the first film layer can be formed. In this embodiment, a hollow pattern of an identification code is formed on the layer farther from the electromagnetic shielding layer among the contrast structure layer and the first film layer, so that the user can obtain a highly clear identification code with a strong brightness or color contrast between the contrast structure layer and the first film layer, thereby improving the identification accuracy and precision of the identification code, and easily tracing the parts or electronic products identified by the identification code. [Brief description of the drawings]

[0010] [Figure 1] FIG. 1 is a schematic diagram of the structure of a shielding film according to an embodiment of the present application. [Diagram 2] FIG. 2 is a schematic diagram of the structure of another shielding film according to an embodiment of the present application. [Diagram 3]FIG. 3 is a structural schematic diagram of another shielding film according to an embodiment of the present application. [Figure 4] FIG. 4 is a structural schematic diagram of another shielding film according to an embodiment of the present application. [Diagram 5] FIG. 5 is a schematic diagram of the structure of another shielding film according to an embodiment of the present application. [Figure 6] FIG. 6 is a structural schematic diagram of another shielding film according to an embodiment of the present application. [Figure 7] FIG. 7 is a schematic plan view of the electromagnetic shielding layer according to an embodiment of the present invention. [Figure 8] FIG. 8 is a structural schematic diagram of another shielding film according to an embodiment of the present application. [Figure 9] FIG. 9 is a schematic diagram of the structure of another shielding film according to an embodiment of the present application. [Figure 10] FIG. 10 is a schematic diagram of the structure of another shielding film according to an embodiment of the present application. [Figure 11] FIG. 11 is a schematic diagram showing the structure of a circuit board according to an embodiment of the present invention. [Figure 12] FIG. 12 is a structural schematic diagram of an electronic device according to an embodiment of the present application. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] The present application will be described in more detail below with reference to the drawings and examples. It is to be understood that the specific examples described herein are merely for the purpose of interpreting the present application, and are not intended to limit the present application. In addition, it is necessary to further explain that, for the convenience of description, the drawings show only parts related to the present application, rather than all structures.

[0012] With the development of flexible circuit boards, electromagnetic interference shielding (EMI shielding) is an important index for evaluating the performance of flexible circuit boards. Under high frequency and high speed driving, the internal and external electromagnetic interference of components, as well as the attenuation, insertion loss and jitter of signals during transmission, are gradually becoming more serious, and general electronic products need to attach a shielding film to a printed circuit board to achieve electromagnetic interference shielding. Combined with the traditional situation that it is difficult to provide an identification code due to the size specifications of electronic products, the embodiment of the present application creatively provides an identification code on a shielding film, thereby improving the clarity and resolution of the identification code.

[0013] Specifically, an embodiment of the present application provides a shielding film including a first film layer, a contrast structure layer, and an electromagnetic shielding layer, a first film layer disposed on a first side of the electromagnetic shielding layer; a contrast structure layer disposed on a first side of the electromagnetic shielding layer; The grayscale value of the color of the contrast structure layer is greater than the grayscale value of the color of the first film layer.

[0014] In the embodiment of the present application, the grayscale value of the color of the contrast structure layer is greater than the grayscale value of the color of the first film layer, but after the identification code is formed, the device can distinguish between the two colors and further process them to form a clear and identifiable identification code, and there is no limitation on how much the grayscale value of the color of the contrast structure layer is greater than the grayscale value of the color of the first film layer.

[0015] In an embodiment of the present application, the shielding film includes an electromagnetic shielding layer for shielding electromagnetic interference, and a first film layer and a contrast structure layer are disposed on a first side of the electromagnetic shielding layer, and the first film layer may be disposed between the electromagnetic shielding layer and the contrast structure layer, and the contrast structure layer may be disposed between the electromagnetic shielding layer and the first film layer, and the color grayscale value of the contrast structure layer needs to be greater than the color grayscale value of the first film layer, so that a clear contrast in brightness between the contrast structure layer and the first film layer can be formed. In this embodiment, a hollow pattern of an identification code is formed on the layer farther from the electromagnetic shielding layer among the contrast structure layer and the first film layer, so that the user can obtain a highly clear identification code with a strong brightness or color contrast between the contrast structure layer and the first film layer, thereby improving the identification precision and accuracy of the identification code, and easily tracing the parts or electronic products identified by the identification code.

[0016] The above is the gist of the present application, and the technical solutions of the embodiments of the present application will be described clearly and completely below with reference to the drawings of the embodiments of the present application. Based on the embodiments of the present application, under the premise that no creative work is required by those skilled in the art, all other embodiments obtained fall within the protection scope of the present application.

[0017] FIG. 1 is a structural schematic diagram of a shielding film according to an embodiment of the present application. As shown in FIG. 1, the shielding film includes a first film layer 11, a contrast structure layer 12, and an electromagnetic shielding layer 13. The material of the electromagnetic shielding layer 13 is a conductive material with excellent shielding performance, which can realize effective electromagnetic interference shielding. Preferably, the material of the electromagnetic shielding layer 13 can be copper, which ensures low cost and has good electrical properties, high shielding performance, high transmission quality, excellent reliability, etc. Of course, the material of the electromagnetic shielding layer 13 can also be a metal material such as aluminum, silver, etc., and this embodiment is not limited thereto. Preferably, as shown in FIG. 2, which is a structural schematic diagram of another shielding film according to an embodiment of the present application. The shielding film can further include an adhesive film layer 14, which is disposed on the side of the electromagnetic shielding layer 13 away from the first film layer 11, and is used to realize the connection between the electromagnetic shielding layer 13 and the circuit board.

[0018] The first film layer 11 is used to insulate and support the electromagnetic shielding layer 13, and prevents moisture and oxygen from penetrating into the electromagnetic shielding layer 13 to a certain extent. The first film layer 11 is preferably a color having a grayscale value closer to black, such as black or dark blue, and this embodiment does not limit the specific color of the first film layer 11. Preferably, the first film layer 11 may include at least one of epoxy resin, rubber, modified epoxy resin, polyimide, polyurethane resin, acrylic resin, modified acrylic resin, polyester, polyphenylene sulfide, polyethylene terephthalate, liquid crystal polymer, and ink, and in this embodiment, at least one of the above materials is mixed with other materials to form a dark color with a lower grayscale value.

[0019] Preferably, the color of the first film layer 11 may be black, and the first film layer 11 may include at least one of black polyimide and black ink, where black polyimide has a good water vapor barrier effect and black ink has a good flame retardant effect, and the first film layer 11 may be made of black polyimide material or black ink material, and the first film layer 11 may include black polyimide and black ink at the same time, so as to enhance the protective effect on the electromagnetic shielding layer 13. Preferably, in order to adapt to the trend of thinning of electronic products, the thickness range of the first film layer 11 is 0.5 μm to 40 μm, thereby reducing the thickness of the first film layer 11 as much as possible, and preferably, the thickness of the first film layer 11 may be 4 μm, and the thinning of the first film layer 11 is realized under the premise of having good insulation and protection performance.

[0020] The contrast structure layer 12 is used to form a clear color or brightness difference with the first film layer 11, and the grayscale value of the color of the contrast structure layer 12 is greater than the grayscale value of the color of the first film layer 11. In this embodiment, the grayscale parameter is used to convert the color into a high-quality grayscale gradation color to detect the brightness contrast between the contrast structure layer 12 and the first film layer 11. The grayscale represents various colors with black tones, that is, black is taken as the reference color, and different colors are represented by black with different saturation rates. Black and white are divided into 0 to 255 kinds of grayscale. The grayscale value of white is 255, and the grayscale value of black is 0. In this embodiment, the grayscale value of the color of the contrast structure layer 12 is limited to be greater than the grayscale value of the color of the first film layer 11, and preferably the difference between the grayscale value of the color of the contrast structure layer 12 and the grayscale value of the color of the first film layer 11 can be limited to be greater. For example, the color of the contrast structure layer 12 is silver, and the gray scale value of silver is larger, so that it forms a clear contrast between the silver color of the contrast structure layer 12 and the dark color of the first film layer 11 .

[0021] The contrast structure layer 12 and the first film layer 11 are located on the same side of the electromagnetic shielding layer 13, and the installation sequence of the contrast structure layer 12 and the first film layer 11 can be changed, for example, as shown in FIG. 2, the contrast structure layer 12 can be installed between the first film layer 11 and the electromagnetic shielding layer 13, or as shown in FIG. 3, which is a structural schematic diagram of another shielding film according to an embodiment of the present application. The first film layer 11 can be installed between the contrast structure layer 12 and the electromagnetic shielding layer 13. As long as the contrast structure layer 12 and the first film layer 11 overlap each other to form a clear contrast. Whether the installation sequence of the contrast structure layer 12 and the first film layer 11 is the installation sequence of FIG. 1 or the installation sequence of FIG. 3, the layer located at the outermost position is used to form the hollow pattern of the identification code, and the color of the other layers exposed from the hollow pattern can form a large brightness difference with the outermost layer, so that the identification code is more clear and users can identify it accurately. Specifically, as shown in Fig. 2, when the first film layer 11 is placed on the outermost side, it is necessary to form a hollow pattern of the identification code in the first film layer 11, and the light-colored (high brightness) contrast structure layer 12 is exposed from the hollow pattern in the first film layer 11 to form a clearer identification code. As shown in Fig. 3, when the contrast structure layer 12 is placed on the outermost side, it is necessary to form a hollow pattern of the identification code in the contrast structure layer 12, and the dark-colored first film layer 11 is exposed from the hollow pattern in the contrast structure layer 12 to form a clearer identification code. Preferably, the hollow pattern can be formed by laser ablation, and for example, the hollow pattern can be ablated by an ultraviolet laser and a carbon dioxide laser.

[0022] Preferably, the difference between the color grayscale value of the contrast structure layer 12 and the color grayscale value of the first film layer 11 is equal to or greater than a first grayscale threshold, and when the first grayscale threshold is equal to or greater than 10, the difference between the color grayscale value of the contrast structure layer 12 and the color grayscale value of the first film layer 11 is at least 10, thereby forming a clear light-dark difference between the contrast structure layer 12 and the first film layer 11, and improving the identification accuracy of the identification code identification device for the identification code formed on the contrast structure layer 12 and the first film layer 11.

[0023] In order to further increase the brightness difference between the contrast structure layer 12 and the first film layer 11, the above-mentioned first grayscale threshold can be limited to 50, so that the difference between the color grayscale value of the contrast structure layer 12 and the color grayscale value of the first film layer 11 is at least 50, the color brightness of the contrast structure layer 12 is larger and the color brightness of the first film layer 11 is smaller, so that the light-dark contrast between the contrast structure layer 12 and the first film layer 11 is larger, and the identification precision and accuracy of the identification code are improved.

[0024] On the basis of the above embodiment, in this embodiment, the first grayscale threshold value can be further limited to 100, so that the difference between the grayscale value of the color of the contrast structure layer 12 and the grayscale value of the color of the first film layer 11 is at least 100, for example, if the grayscale value of the color of the first film layer 11 is 0, the difference between the grayscale value of the color of the contrast structure layer 12 and the grayscale value of the color of the first film layer 11 is at least 100, even 255, and the grayscale value of the contrast structure layer 12 can be more than 100. When the difference in grayscale value is 255, one of the contrast structure layer 12 and the first film layer 11 is pure black, and the other is pure white, that is, the grayscale value of one of them is 255, and the grayscale value of the other is 0, the difference in brightness or color is large, and the visibility of the identification code is further increased.

[0025] It should be noted that in this embodiment, the shielding film is attached to the printed circuit board through the side where the adhesive film layer 14 is installed, and is used to quickly guide interference signals generated by electronic devices to the ground plate or ground line of the printed circuit board through the electromagnetic shielding layer 13. FIG. 4 is a structural schematic diagram of another shielding film according to an embodiment of the present application. Preferably, the side of the electromagnetic shielding layer 13 close to the adhesive film layer 14 can be roughened to form a number of protrusion structures 131, which are used to penetrate the adhesive film layer 14 and connect to the ground end of the printed circuit board, the protrusion structures 131 can realize the connection between the electromagnetic shielding layer 13 and the ground end, and the protrusion structures 131 can tightly adhere between the electromagnetic shielding layer 13 and the adhesive film layer 14 to avoid separation between the electromagnetic shielding layer 13 and the adhesive film layer 14, and when the adhesive amount of the adhesive film layer 14 is insufficient, the shielding film can be easily cut off. If the amount of adhesive in the adhesive film layer 14 is too large, separation will occur between the shielding film and the printed circuit board, and the adhesive is likely to overflow onto the edge of the printed circuit board. In this embodiment, by installing the protrusion structure 131, when the shielding film and the printed circuit board are pressed together, the protrusion structure 131 can push the overflowing adhesive into the recess of the adhesive film layer 14, thereby increasing the amount of adhesive that can be accommodated between the electromagnetic shielding layer 13 and the printed circuit board, and avoiding peeling between the shielding film and the printed circuit board.

[0026] It should be noted that in the production process of the above shielding film, the above first film layer 11, the contrast structure layer 12, the electromagnetic shielding layer 13 and the adhesive film layer 14 are all placed on a carrier film, which supports the above film layers, and after the first film layer 11, the contrast structure layer 12 and the electromagnetic shielding layer 13 are formed on the carrier film, the electromagnetic shielding layer 13 is roughened to form a protrusion structure 131, and the adhesive film layer 14 is pressed onto the protrusion structure 131 of the electromagnetic shielding layer 13 to form a base film material of the shielding film. Then, the base film material of the shielding film needs to be peeled off from the carrier film, and a hollow pattern of the identification code needs to be formed on the side of the shielding film away from the adhesive film layer 14 by ablation.

[0027] 5 is a structural schematic diagram of another shielding film according to an embodiment of the present application. In this embodiment, the side of the electromagnetic shielding layer 13 close to the adhesive film layer 14 may not be roughened, and preferably, a plurality of conductive particles 141 may be disposed in the adhesive film layer 14, and the conductive particles 141 are used to penetrate the adhesive film layer 14 and connect the ground end of the printed circuit board to the electromagnetic shielding layer 13. Compared with FIG. 4, the adhesive film layer 14 shown in FIG. 5 contains a plurality of conductive particles 141, and the conductive particles 141 aggregate to form larger particles, and the larger particles penetrate the adhesive film layer 14, thereby establishing a connection between the ground end of the printed circuit board and the electromagnetic shielding layer 13. In this case, the present embodiment does not roughen the electromagnetic shielding layer 13 during the manufacturing process, and the adhesive film layer 14 and the electromagnetic shielding layer 13 can be tightly adhered to each other, thereby forming the base film material of the shielding film.

[0028] Alternatively, the side of the electromagnetic shielding layer 13 close to the adhesive film layer 14 may be roughened to form a protrusion structure, and then the adhesive film layer 14 having conductive particles 141 may be coated, as shown in Fig. 6, which is a structural schematic diagram of another shielding film according to an embodiment of the present application. In this embodiment, the electromagnetic shielding layer 13 is roughened to form the protrusion structure 131, and at the same time, a plurality of conductive particles 141 can be disposed in the adhesive film layer 14, and the conductive particles 141 can penetrate the adhesive film layer 14 and electrically connect to the protrusion structure 131, thereby further improving the conductivity between the electromagnetic shielding layer 14 and the ground layer of the circuit board, and solving the existing problem of peeling between the shielding film and the circuit board layer due to insufficient adhesive capacity.

[0029] Preferably, as shown in Fig. 7, which is a schematic planar structure diagram of an electromagnetic shielding layer according to an embodiment of the present application. The electromagnetic shielding layer 13 is provided with a number of through holes 132, which is advantageous for the volatile substances in the adhesive film layer at high temperatures to be exhausted through the through holes 132 of the electromagnetic shielding layer 13, thereby avoiding the volatile substances in the adhesive film layer being difficult to be exhausted at high temperatures, thereby avoiding the peeling between the electromagnetic shielding film and the ground layer of the circuit board caused by foaming or delamination of the electromagnetic shielding layer 13, and further ensuring that the electromagnetic shielding film is grounded and discharging interference charges.

[0030] Preferably, the through holes 132 can be distributed regularly or irregularly in the electromagnetic shielding layer 13. As shown in FIG. 7, the regular distribution of the through holes 132 in the electromagnetic shielding layer 13 means that the shapes of the through holes 132 are the same and uniformly distributed in the electromagnetic shielding layer 13, and the irregular distribution of the through holes 132 in the electromagnetic shielding layer 13 means that the shapes of the through holes 132 are different and irregularly distributed in the electromagnetic shielding layer 13. Preferably, as shown in FIG. 7, the shapes of the through holes 132 are the same and the through holes 132 are uniformly distributed in the electromagnetic shielding layer 13. In addition, the through holes 132 may be circular or may have any other shape. FIG. 7 only takes the through holes 132 as an example, but any other shape of the through holes 132 falls within the scope of protection of the embodiments of the present application.

[0031] The shielding film is divided into two types based on the arrangement order of the first film layer 11 and the contrast structure layer 12 and will be described in detail below. For the first type, still refer to FIG. 3, preferably, in this embodiment, the contrast structure layer 12 may be disposed on the side of the first film layer 11 away from the electromagnetic shielding layer 13, and the contrast structure layer 12 forms a hollow pattern of an identification code. As shown in FIG. 3, in this embodiment, the material of the contrast structure layer 12 may be a metal, and the gray scale value of the color of the metal is preferably greater than the gray scale value of the color of the first film layer 11, and the difference is preferably 10 or more. It should be noted that the metal layer may include at least one of a metal element and a metal alloy, and this embodiment is not limited thereto. If the contrast structure layer 12 is a metal layer, after the user forms a hollow pattern on the metal layer, preferably, an insulating film is disposed on the side of the metal layer away from the electromagnetic shielding layer 13, and an opening is formed at the position of the insulating film corresponding to the hollow pattern of the identification code, so that the identification code can be exposed for the user to identify, thereby preventing the metal layer from contacting with external electronic components and causing a short circuit. In addition, if the insulating film is a colorless and transparent insulating film, the insulating film does not have the opening, but the identification code can still be exposed for the user to identify.

[0032] Also, preferably, the contrast structure layer 12 can be an adhesive layer or an ink layer with a gray scale value larger than that of the first film layer 11. In addition to providing protection to the electromagnetic shielding layer 13, the contrast structure layer 12 and the first film layer 11 exposed from the hollow pattern form a distinct identification code. In this embodiment, the adhesive layer can be a thermosetting adhesive.

[0033] Preferably, the contrast structure layer 12 can be a white adhesive layer or a white ink layer. In this embodiment, the contrast structure layer 12 is a white adhesive layer or a white ink layer, the grayscale value of the color of the contrast structure layer 12 is 255, the color of the first film layer 11 is preferably black, and the grayscale value of the color of the first film layer 11 is 0, so that the contrast between black and white is strong and it is easy to form a clearer identification code. In addition, the adhesive layer or the ink layer can also be other colors with high grayscale values, such as gray, yellow, etc., and this embodiment is not limited thereto.

[0034] For the second type, still referring to Fig. 2, preferably, the first film layer 11 can be disposed on the side of the contrast structure layer 12 away from the electromagnetic shielding layer 13, and a hollow pattern of an identification code is formed on the first film layer 11. Preferably, the contrast structure layer 12 can be an adhesive layer or an ink layer, and the color grayscale value of the adhesive layer or the ink layer is greater than the color grayscale value of the first film layer 11, and the color grayscale value of the adhesive layer or the ink layer is preferably 160 or more.

[0035] Preferably, the contrast structure layer 12 is a white or colorless adhesive layer, or the contrast structure layer 12 is a white ink layer. The material of the contrast structure layer 12 can be selected from at least one of modified epoxy resins, modified acrylic acids, modified rubbers, modified thermoplastic polyimides, modified polyesters, thermoplastic resins, thermosetting resins, and pressure-sensitive adhesives. In this embodiment, the contrast structure layer 12 is a white adhesive layer or a white ink layer, and the grayscale value of the color of the contrast structure layer 12 is preferably 255, and the grayscale value of the color of the first film layer 11 is preferably 0, so that the contrast between black and white is strong and it is easy to form a clearer identification code. In addition, the adhesive layer or ink layer can also be other colors with high grayscale values, such as gray, yellow, etc., and this embodiment is not limited thereto. It should be noted that when the contrast structure layer 12 is installed between the first film layer 11 and the electromagnetic shielding layer 13, the contrast structure layer 12 can select a colorless adhesive layer, which can effectively protect the electromagnetic shielding layer 13 and prevent the electromagnetic shielding layer 13 from being exposed to the hollow pattern. Because the contrast structure layer 12 is colorless, the electromagnetic shielding layer 13 is exposed through the hollow pattern, so that the black color of the first film layer 11 also forms a contrast with the color of the electromagnetic shielding layer 13, forming a clearer identification code; when copper is selected as the material of the electromagnetic shielding layer 13, the color of the electromagnetic shielding layer 13 is copper red, which can be easily distinguished from the copper red color and the black color, so that the colorless contrast structure layer 12 can effectively protect the copper and prevent the subsequent color from being easily distinguished from the first film layer 11 due to exposure to air and oxidation.

[0036] Preferably, the contrast structure layer 12 can further be a metal layer, the grayscale value of the metal color is greater than the grayscale value of the color of the first film layer 11, and the grayscale value of the metal color is preferably 10 or more.

[0037] Preferably, the material of the contrast structure layer 12 is at least one of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium, or the material of the contrast structure layer is an alloy formed of at least two of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium, or the material of the contrast structure layer is a combination between alloys formed of at least two of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium. As can be easily understood, it is better for the identification code to be clearly white and black, so the color of the metal material of the contrast structure layer 12 needs to be sufficiently bright, and it is preferable to use a silver or silver-white metal material. In this embodiment, the contrast structure layer 12 is formed by selecting at least one of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium, or an alloy formed of at least two of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium, or the material of the contrast structure layer is a combination between alloys formed of at least two of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium. The above materials are all white, silver or near silver, and for example, in this embodiment, nickel may be selected as the material of the contrast structure layer 12, or nickel-chromium alloy may be selected as the material of the contrast structure layer 12. In addition, the contrast structure layer 12 may also be other light-colored metals with lower gray scale value, and this embodiment is not limited thereto.

[0038] 8 is a structural schematic diagram of another shielding film according to an embodiment of the present application. Preferably, the contrast structure layer 12 may include a first metal layer 121 and a second metal layer 122, the first metal layer 121 being formed on the side of the first film layer 11 close to the electromagnetic shielding layer 13 by a sputtering process, and the second metal layer 122 being formed on the side of the first metal layer 121 away from the first film layer 11 by a plating process.

[0039] Besides the limitation on the gray scale value, this embodiment has certain requirements for the flatness of the contrast structure layer 12. The rougher the surface of the contrast structure layer 12, the darker the light on the surface of the contrast structure layer 12, and the lower the resolution between the first film layer 11. Therefore, in this embodiment, the contrast structure layer 12 can be divided into two layers, that is, first, a first metal layer 121 is formed on the first film layer 11 by a sputtering process so as to easily form a contrast with the first film layer 11, and a dense and flat metal surface is formed by the sputtering process, and then a second metal layer 122 is formed on the flat first metal layer 121 by a plating process. Preferably, the thickness range of the first metal layer 121 can be 10 Å to 2 μm, and the thickness range of the second metal layer 122 can be 0.1 μm to 10 μm. Preferably, when the thickness range of the second metal layer 122 is 0.2 μm to 0.4 μm, the resistance value of the second metal layer 122 per unit area (1 cm×1 cm) may be set to a range of 15 mΩ to 200 mΩ, and is preferably set to 30 mΩ.

[0040] In addition to the sputtering process, the first metal layer 121 may also be manufactured and formed by one or more of other processes, such as chemical plating, physical vapor deposition, chemical vapor deposition, evaporation plating, sputtering plating, electroplating and hybrid plating, and this embodiment does not limit the manufacturing process of the first metal layer 121, and it is preferable that the first metal layer 121 uses a sputtering process.

[0041] In the embodiment shown in FIG. 8, when forming the identification code by ablation, the laser energy forms a hollow pattern in the first film layer, thereby exposing the color of the first metal layer 121, and therefore, it is preferable that the grayscale value corresponding to the color of the first metal layer 121 is less than the grayscale value corresponding to the color of the second metal layer 122, for example, the first metal layer 121 can be selected to be Ag, and the second metal layer 122 can be selected to be Ni.

[0042] 9 is a structural schematic diagram of another shielding film according to an embodiment of the present application. Preferably, the first metal layer may include a first sputtered metal layer 1211 and a second sputtered metal layer 1212, the first sputtered metal layer 1211 is disposed between the first film layer 11 and the second sputtered metal layer 1212, and the color grayscale value of the first sputtered metal layer 1211 is greater than the color grayscale value of the second sputtered metal layer 1212.

[0043] In this embodiment, two sputtered metal layers can be provided because when the hollow pattern of the identification code is formed by actually ablating the first film layer 11, the laser energy may penetrate the first sputtered metal layer 1211, and the second sputtered metal layer 1212 is used to strengthen the guarantee and maintain the sputtered metal layer with high flatness exposed from the hollow pattern. In addition, the color grayscale value of the first sputtered metal layer 1211 can be greater than the color grayscale value of the second sputtered metal layer 1212, for example, the first sputtered metal layer 1211 can be silver and the second sputtered metal layer 1212 can be nickel, and the silver metal surface can form a clear color contrast with the dark first film layer 11, improving the clarity of the identification code.

[0044] Fig. 10 is a structural schematic diagram of another shielding film according to an embodiment of the present application. Preferably, the contrast structure layer 12 may further include a second film layer 15, the second film layer 15 is disposed between the first film layer 11 and the first metal layer 121, and the difference between the color grayscale value of the second film layer 15 and the color grayscale value of the first film layer 11 is equal to or greater than a first grayscale threshold, and the first grayscale threshold is equal to or greater than 10. The second film layer 15 is disposed between the first film layer 11 and the first metal layer 121, and when the first metal layer 121 includes a first sputtering metal layer and a second sputtering metal layer, the second film layer 15 is disposed between the first film layer 11 and the first sputtering metal layer, thereby further enhancing the protection of the first metal layer 121, for example, because the second film layer 15 is disposed, the situation that the laser energy may penetrate the first sputtering metal layer is completely avoided, and the first sputtering metal layer is protected. The grayscale value of the color of the second film layer 15 should be larger than that of the first film layer 11 as well, and the difference between the grayscale value of the color of the second film layer 15 and the grayscale value of the color of the first film layer 11 is preferably equal to or larger than a first grayscale threshold, and the first grayscale threshold is equal to or larger than 10. The difference between the grayscale value of the color of the second film layer 15 and the grayscale value of the color of the first film layer 11 is at least 10, so as to form a clear difference in brightness between the second film layer 15 and the first film layer 11, and to improve the identification accuracy of the identification code identification device for the identification code formed on the second film layer 15 and the first film layer 11. Preferably, the first grayscale threshold may be 50 or 100, and thus the brightness contrast between the second film layer 15 and the first film layer 11 can be increased, and the identification precision and accuracy for the identification code can be improved. Preferably, the second film layer 15 may be white or colorless, and the thickness range of the second film layer 15 may be 0.5 μm to 30 μm. The strong contrast between the white second film layer 15 and the dark first film layer 11 facilitates the formation of a clearer identification code.Moreover, the second film layer 15 may be colorless, so that the color of the first metal layer 121 can be transmitted through the second film layer 15 and exposed through the hollow pattern.

[0045] Based on the above embodiment, the embodiment of the present application further provides a shielding film, referring to FIG. 1, comprising a first film layer 11, a contrast structure layer 12 and an electromagnetic shielding layer 13; The first film layer 11 is disposed on a first side of the electromagnetic shielding layer 13; The contrast structure layer 12 is disposed on a first side of the electromagnetic shielding layer 13; The grayscale value of the color of the contrast structure layer 12 is greater than the grayscale value of the color of the first film layer 11, and a hollow pattern of the identification code is formed in the layer farther from the electromagnetic shielding layer 13 among the contrast structure layer 12 and the first film layer 11.

[0046] In an embodiment of the present application, the shielding film includes an electromagnetic shielding layer for shielding electromagnetic interference, and a first film layer and a contrast structure layer are disposed on a first side of the electromagnetic shielding layer, and the first film layer may be disposed between the electromagnetic shielding layer and the contrast structure layer, and the contrast structure layer may be disposed between the electromagnetic shielding layer and the first film layer, and the color grayscale value of the contrast structure layer needs to be greater than the color grayscale value of the first film layer, so that a clear contrast in brightness between the contrast structure layer and the first film layer can be formed. In this embodiment, a hollow pattern of an identification code is formed on the layer farther from the electromagnetic shielding layer among the contrast structure layer and the first film layer, so that the user can obtain a highly clear identification code with a strong brightness or color contrast between the contrast structure layer and the first film layer, thereby improving the identification precision and accuracy of the identification code, and easily tracing the parts or electronic products identified by the identification code.

[0047] Preferably, the identification code may include at least one of a bar code, a two-dimensional code, and a character. The identification code is a unique corresponding identification mark for identifying a part or an electronic product. The identification code may include a character pattern such as a number or an alphabet, and may be a bar code or a two-dimensional code, and the shielding film of this embodiment may include at least one of the bar code, the two-dimensional code, and the character, thereby identifying the corresponding part or electronic product. For example, the shielding film needs to be attached to the printed circuit board of the electronic device, and the identification code of the part can be provided at a position corresponding to the part on the shielding film. A plurality of identification codes can be provided on the shielding film in one-to-one correspondence with a plurality of parts, thereby solving the problem that the printed identification code is not clear due to the lack of a steel plate of a size sufficient to provide the identification code of the electronic product, and effectively improving the resolution and identification accuracy of the identification code. Preferably, the hollow pattern is formed by laser ablation. For example, the ablation of the hollow pattern can be performed by an ultraviolet laser and a carbon dioxide laser.

[0048] It should be noted that when ablating the above hollow pattern, there may be two cases: For the first type, only the layer farther from the electromagnetic shielding layer 13 among the contrast structure layer 12 and the first film layer 11 is completely ablated to form a hollow pattern of the identification code, but the layer closer to the electromagnetic shielding layer 13 is not ablated, that is, the ablation depth of the hollow pattern is the thickness of the layer farther from the electromagnetic shielding layer 13 among the contrast structure layer 12 and the first film layer 11. The structure of the layer closer to the electromagnetic shielding layer 13 that is not etched is exposed from the hollow pattern, and the identification code is formed in the contrast structure layer 12 and the first film layer 11.

[0049] For the second type, the layer of the contrast structure layer 12 and the first film layer 11 that is farther from the electromagnetic shielding layer 13 may be completely ablated to form a hollow pattern of the identification code, and at the same time, the layer closer to the electromagnetic shielding layer 13 may be partially ablated. In this embodiment, the layer closer to the electromagnetic shielding layer 13 is partially ablated but not completely ablated, and after the ablation of the identification code is completed, the hollow pattern can also expose the layer of the contrast structure layer 12 and the first film layer 11 that is closer to the electromagnetic shielding layer 13, thereby forming the identification code on the contrast structure layer 12 and the first film layer 11. Specifically, a groove pattern is formed on the layer of the contrast structure layer 12 and the first film layer 11 that is closer to the electromagnetic shielding layer 13, and the vertical projection of the hollow pattern onto the plane where the electromagnetic shielding layer is located completely overlaps with the groove pattern. The groove pattern is formed by partially ablating one of the contrast structure layer 12 and the first film layer 11, whichever is closer to the electromagnetic shielding layer 13, and the groove pattern and the hollow pattern are formed in the same process, so that the vertical projection of the hollow pattern onto the plane on which the electromagnetic shielding layer is located completely overlaps with the groove pattern.

[0050] 3, preferably, the contrast structure layer 12 may be disposed on the side of the first film layer 11 away from the electromagnetic shielding layer 13, and a hollow pattern of the identification code may be formed in the contrast structure layer 12. In this embodiment, when the hollow pattern of the identification code is formed by ablating the contrast structure layer 12, the first film layer 11 may not be ablated, and only the contrast structure layer 12 may be ablated; alternatively, the contrast structure layer 12 may be ablated to form the hollow pattern of the identification code, and at the same time, the first film layer 11 may be ablated partially to form a groove pattern, and the vertical projection of the hollow pattern onto the plane where the electromagnetic shielding layer is located completely overlaps with the groove pattern.

[0051] As shown in FIG. 3, in this embodiment, the material of the contrast structure layer 12 can be metal, and the grayscale value of the color of the metal is greater than the grayscale value of the color of the first film layer 11, and it is preferable that the difference between the grayscale value of the color of the metal and the grayscale value of the color of the first film layer 11 is 10 or more.

[0052] Preferably, the contrast structure layer 12 can be an adhesive layer or an ink layer, which has a gray scale value larger than that of the first film layer 11. The contrast structure layer 12 provides protection to the electromagnetic shielding layer 13, and forms a distinct identification code with the first film layer 11 exposed from the hollow pattern. In this embodiment, the adhesive layer can be a thermosetting adhesive.

[0053] Preferably, the contrast structure layer 12 can be a white adhesive layer or a white ink layer. In this embodiment, when the contrast structure layer 12 is a white adhesive layer or a white ink layer, the grayscale value of the color of the contrast structure layer 12 is 255, and the color of the first film layer 11 is preferably black, and the grayscale value of the color of the first film layer 11 is 0, so that the contrast between black and white is strong and it is easy to form a clearer identification code. In addition, the adhesive layer or ink layer can also be other colors with higher grayscale values, such as gray, yellow, etc., and this embodiment is not limited thereto.

[0054] Preferably, still referring to FIG. 1, the first film layer 11 may further be disposed on the side of the contrast structure layer 12 away from the electromagnetic shielding layer 13, and the first film layer 11 may form a hollow pattern of the identification code. In this embodiment, when the hollow pattern of the identification code is formed by ablating the first film layer 11, the contrast structure layer 12 may not be ablated, and only the first film layer 11 may be ablated; or, at the same time, the hollow pattern of the identification code is formed by ablating the first film layer 11, the contrast structure layer 12 may be partially ablated to form a groove pattern, and the vertical projection of the hollow pattern on the plane where the electromagnetic shielding layer is located is completely overlapped with the groove pattern. Preferably, the contrast structure layer 12 is one of an adhesive layer, an ink layer and a metal layer, or a combination of two or more of them.

[0055] Preferably, the contrast structure layer 12 can be an adhesive layer or an ink layer, and the color grayscale value of the adhesive layer or ink layer is greater than the color grayscale value of the first film layer 11, and the difference between the color grayscale value of the adhesive layer or ink layer and the color grayscale value of the first film layer 11 is preferably 10 or more. Preferably, the contrast structure layer 12 can be a white or colorless adhesive layer, or the contrast structure layer 12 is a white ink layer. The material of the contrast structure layer 12 can be selected from at least one of modified epoxy resins, modified acrylic acids, modified rubbers, modified thermoplastic polyimides, modified polyesters, thermoplastic resins, thermosetting resins, and pressure-sensitive adhesives. In this embodiment, when the contrast structure layer 12 is a white adhesive layer or a white ink layer, the color grayscale value of the contrast structure layer 12 is preferably 255, and the color grayscale value of the first film layer 11 is preferably 0, which has a strong contrast between black and white and easily forms a clearer identification code. In addition, the adhesive layer or ink layer may be other colors with low grayscale value, such as gray, yellow, etc., and this embodiment is not limited thereto. It should be noted that when the contrast structure layer 12 is installed between the first film layer 11 and the electromagnetic shielding layer 13, the contrast structure layer 12 can select a colorless adhesive layer, which can effectively protect the electromagnetic shielding layer 13 and prevent the electromagnetic shielding layer 13 from being exposed in the hollow pattern. And since the contrast structure layer 12 is colorless, the electromagnetic shielding layer 13 is exposed through the hollow pattern, and the black color of the first film layer 11 also forms a contrast with the color of the electromagnetic shielding layer 13, forming a more clear identification code; when copper is selected as the material of the electromagnetic shielding layer 13, the color of the electromagnetic shielding layer 13 is copper red, and the copper red color and black color can be easily distinguished, so the colorless contrast structure layer 12 can effectively protect the copper and prevent it from being easily distinguished from the color between the first film layer 11 in the subsequent process due to exposure to air and oxidation.

[0056] Preferably, the contrast structure layer 12 can also be a metal layer. The grayscale value of the color of the metal is greater than the grayscale value of the color of the first film layer 11, and the difference is preferably 10 or more. Preferably, the material of the contrast structure layer 12 is at least one of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium, or the material of the contrast structure layer is an alloy formed of at least two of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium, or the material of the contrast structure layer is a combination between alloys formed of at least two of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium. As can be easily understood, it is better for the identification code to be clearly black and white, so the color of the metal material of the contrast structure layer 12 needs to be sufficiently bright, and it is preferable to use a silver or silver-white metal material. In this embodiment, at least one of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium is selected as the contrast structure layer 12, or an alloy formed of at least two of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium is selected as the contrast structure layer 12, or the material of the contrast structure layer is a combination between the alloy formed of at least two of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium. All of the above materials are white, silver, or close to silver, and for example, in this embodiment, nickel can be selected as the material of the contrast structure layer 12, or a nickel-chromium alloy can be selected as the material of the contrast structure layer 12. In addition, the contrast structure layer 12 can also be other light-colored metals with lower grayscale values, and this embodiment is not limited thereto.

[0057] Preferably, the contrast structure layer 12 may include a first metal layer 121 and a second metal layer 122, where the first metal layer 121 is formed on the side of the first film layer 11 closer to the electromagnetic shielding layer 13 by a sputtering process, and the second metal layer 122 is formed on the side of the first metal layer 121 away from the first film layer 11 by a plating process.

[0058] Besides the limitation on the gray scale value, this embodiment has certain requirements for the flatness of the contrast structure layer 12. The rougher the surface of the contrast structure layer 12, the darker the light on the surface of the contrast structure layer 12, and the lower the resolution between the first film layer 11. Therefore, in this embodiment, the contrast structure layer 12 can be divided into two layers, that is, first, a first metal layer 121 is formed on the first film layer 11 by a sputtering process so as to easily form a contrast with the first film layer 11, and a dense and flat metal surface is formed by the sputtering process, and then a second metal layer 122 is formed on the flat first metal layer 121 by a plating process. Preferably, the thickness range of the first metal layer 121 is 10 Å to 2 μm, and the thickness range of the second metal layer 122 is 0.1 μm to 10 μm. Preferably, when the thickness range of the second metal layer 122 is 0.2 μm to 0.4 μm, the resistance value of the second metal layer 122 per unit area (1 cm×1 cm) may be set to a range of 15 mΩ to 200 mΩ, and is preferably set to 30 mΩ.

[0059] In the embodiment shown in FIG. 7, when the identification code is formed by ablation, the laser energy forms a hollow pattern in the first film layer, thereby exposing the color of the first metal layer, and therefore, it is preferable that the grayscale value corresponding to the color of the first metal layer is less than the grayscale value corresponding to the color of the second metal layer, for example, the first metal layer can be selected to be Ag, and the second metal layer can be selected to be Ni.

[0060] As shown in FIG. 9, preferably, the first metal layer may include a first sputtered metal layer 1211 and a second sputtered metal layer 1212, where the first sputtered metal layer 1211 is disposed between the first film layer 11 and the second sputtered metal layer 1212, and the color grayscale value of the first sputtered metal layer 1211 is greater than the color grayscale value of the second sputtered metal layer 1212.

[0061] In this embodiment, two sputtered metal layers can be provided because when forming the hollow pattern of the identification code by actually ablating the first film layer 11, the laser energy may penetrate the first sputtered metal layer 1211, and the second sputtered metal layer 1212 is used to strengthen the guarantee and maintain the sputtered metal layer with high flatness exposed from the hollow pattern. Also, the color grayscale value of the first sputtered metal layer 1211 can be made larger than the color grayscale value of the second sputtered metal layer 1212, for example, the first sputtered metal layer 1211 can be made silver, and thus the second sputtered metal layer 1212 can be made nickel, and the silver metal surface can form a clear color contrast with the dark first film layer 11, improving the clarity of the identification code.

[0062] Based on the same idea, an embodiment of the present application further provides a circuit board, as shown in Fig. 11, which is a structural schematic diagram of a circuit board according to an embodiment of the present application. The circuit board includes a printed circuit board 2 and a shielding film 1 according to any embodiment of the present application, and an adhesive film layer is provided on the side of the shielding film 1 away from the first film layer of the electromagnetic shielding layer, and the printed circuit board 2 is attached and installed on one side of the adhesive film layer of the shielding film 1. The circuit board of this embodiment includes the technical features of the shielding film according to any embodiment of the present application and has the beneficial effects of the shielding film according to any embodiment of the present application.

[0063] Many components with different functions are integrated on the printed circuit board 2, and in this embodiment, the identification code of the components can be provided at the position on the shielding film 1 corresponding to the components. The shielding film 1 may cover the entire printed circuit board to achieve full-layer electromagnetic shielding, or the shielding film 1 may include multiple sub-shielding films of small size, each sub-shielding film is used to cover a corresponding area of ​​the printed circuit board, and this embodiment is not limited thereto. In addition, the identification code of the electronic device on which the circuit board is located may be provided on the shielding film 1, and for example, the identification code of the electronic device may be provided on the edge area of ​​the shielding film 1.

[0064] An embodiment of the present application further provides an electronic device. FIG. 12 is a structural schematic diagram of an electronic device according to an embodiment of the present application. As shown in FIG. 12, the electronic device according to an embodiment of the present application includes a circuit board 3 according to any embodiment of the present application. The electronic device may be a mobile phone as shown in FIG. 12, or may be a computer, a television, a smart wearable terminal, etc., and the present embodiment is not particularly limited thereto.

[0065] It should be noted that the above is merely a preferred embodiment of the present application and the technical principles used. As can be understood by those skilled in the art, the present application is not limited to the specific embodiments described herein, and various obvious modifications, adjustments, and substitutions can be made by those skilled in the art without departing from the scope of protection of the present application. Therefore, although the present application has been described in detail by the above embodiments, the present application is not limited to the above embodiments, and may include many other equivalent embodiments without departing from the idea of ​​the present application, and the scope of the present application is determined by the appended claims.

Claims

1. A shielding film comprising a first film layer, a contrast structure layer, and an electromagnetic shielding layer, the first film layer is disposed on a first side of the electromagnetic shielding layer; the contrast structure layer is disposed on a first side of the electromagnetic shielding layer; the grayscale value of the color of the contrast structure layer is greater than the grayscale value of the color of the first film layer; further comprising an adhesive film layer; the adhesive film layer is disposed on a side of the electromagnetic shielding layer away from the first film layer; a plurality of protrusion structures are formed on the side of the electromagnetic shielding layer close to the adhesive film layer by a roughening treatment; The protrusion structure is used to penetrate the adhesive film layer and connect to the ground end of a printed circuit board.

2. the first film layer includes at least one of an epoxy resin, a rubber, a modified epoxy resin, a polyimide, a polyurethane resin, an acrylic resin, a modified acrylic resin, a polyester, a polyphenylene sulfide, a polyethylene terephthalate, a liquid crystal polymer, and an ink; The shielding film of claim 1 , wherein the first film layer has a thickness range of 0.5 μm to 40 μm.

3. 2. The shielding film of claim 1, wherein a difference between the grayscale value of the color of the contrast structure layer and the grayscale value of the color of the first film layer is greater than or equal to a first grayscale threshold, and the first grayscale threshold is greater than or equal to 10.

4. The shielding film of claim 3 , wherein the first grayscale threshold is 50.

5. The shielding film of claim 3 , wherein the first grayscale threshold is 100.

6. The shielding film of claim 1 , wherein the contrast structure layer is disposed on the side of the first film layer away from the electromagnetic shielding layer.

7. The shielding film of claim 6 , wherein the contrast structure layer is an adhesive layer or an ink layer.

8. The shielding film of claim 7, wherein the contrast structure layer is a white adhesive layer or a white ink layer.

9. The shielding film of claim 1 , wherein the first film layer is disposed on a side of the contrast structure layer away from the electromagnetic shielding layer.

10. 10. The shielding film of claim 9, wherein the contrast structure layer is an adhesive layer or an ink layer.

11. The shielding film of claim 10, wherein the contrast structure layer is a white adhesive layer or the contrast structure layer is a white ink layer.

12. Shielding film according to claim 6 or 9, wherein the contrast structure layer is a metal layer.

13. Shielding film according to claim 12, wherein the material of the contrast structure layer is at least one of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium, or the material of the contrast structure layer is an alloy formed from at least two of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium, or the material of the contrast structure layer is a combination between alloys formed from at least two of nickel, silver, platinum, titanium, aluminum, cobalt, and chromium.

14. The shielding film of claim 12 , wherein the contrast structure layer comprises at least two metal layers.

15. The contrast structure layer further includes a second film layer disposed between the first film layer and the metal layer; 13. The shielding film of claim 12, wherein a difference between the grayscale value of the color of the second film layer and the grayscale value of the color of the first film layer is greater than or equal to a first grayscale threshold, and the first grayscale threshold is greater than or equal to 10.

16. 16. The shielding film of claim 15, wherein the second film layer is white and the thickness range of the second film layer is 0.5 μm to 30 μm.

17. A plurality of conductive particles are disposed within the adhesive film layer; The shielding film of claim 1 , wherein the conductive particles are used to penetrate the adhesive film layer to connect a ground end of a printed circuit board to the electromagnetic shielding layer.

18. The shielding film of claim 1 , wherein the electromagnetic shielding layer is provided with a plurality of through holes.

19. A shielding film comprising a first film layer, a contrast structure layer, and an electromagnetic shielding layer, the first film layer is disposed on a first side of the electromagnetic shielding layer; the contrast structure layer is disposed on a first side of the electromagnetic shielding layer; the contrast structure layer has a greater grayscale value than the first film layer, and a hollow pattern of an identification code is formed on the contrast structure layer or the first film layer, the layer farther from the electromagnetic shielding layer; further comprising an adhesive film layer; the adhesive film layer is disposed on a side of the electromagnetic shielding layer away from the first film layer; a plurality of protrusion structures are formed on the side of the electromagnetic shielding layer close to the adhesive film layer by a roughening treatment; The protrusion structure is used to penetrate the adhesive film layer and connect to the ground end of a printed circuit board.

20. The shielding film of claim 19, wherein a groove pattern is formed in the contrast structure layer or the first film layer, whichever is closer to the electromagnetic shielding layer, and the vertical projection of the hollow pattern onto a plane on which the electromagnetic shielding layer is located completely overlaps with the groove pattern.

21. 21. The shielding film according to claim 19 or 20, wherein the contrast structure layer is disposed on the side of the first film layer away from the electromagnetic shielding layer, and the contrast structure layer is formed with a hollow pattern of the identification code.

22. 22. The shielding film of claim 21, wherein the contrast structure layer is an adhesive layer or an ink layer.

23. 21. The shielding film of claim 19 or 20, wherein the first film layer is disposed on the side of the contrast structure layer away from the electromagnetic shielding layer, and the first film layer is formed with a hollow pattern of the identification code.

24. 24. The shielding film of claim 23, wherein the contrast structure layer is one or a combination of two or more of an adhesive layer, an ink layer, and a metal layer.

25. A circuit board comprising a printed circuit board and the shielding film according to any one of claims 1 to 24, wherein an adhesive film layer is provided on a side of the electromagnetic shielding layer of the shielding film that is away from the first film layer; The printed circuit board is attached to one side of the adhesive film layer of the shielding film.

Citation Information

Patent Citations

  • Laminate for laser printing and print thereof

    JP1997123606A

  • Wiring circuit board assembly sheet

    JP2010161302A

  • Film for flip-chip type semiconductor rear surface, dicing tape integrated type film for semiconductor rear surface, manufacturing method of the film for flip-chip type semiconductor rear surface, and semiconductor device

    JP2012124465A

  • Surface treated copper foil, laminate using the same, printed wiring board, electronic apparatus and method for manufacturing printed wiring board

    JP2015148011A

  • Electromagnetic wave shield sheet and semiconductor device

    JP2016039160A