Aspect structure

JP7558580B2Active Publication Date: 2024-10-01YAMATO ENG SHOP CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2022206536
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-12-23
Publication Date
2024-10-01
Estimated Expiration
2042-12-23

AI Technical Summary

Benefits of technology

【0023】 以上のように、本発明によれば、木造建築物の床構面、屋根構面、或いは壁構面の構造として、簡易な構成で、手間、時間、コストを低減して構築することができる剛性の高い構面構造を、提供することができる。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007558580000002
    Figure 0007558580000002
  • Figure 0007558580000003
    Figure 0007558580000003
  • Figure 0007558580000004
    Figure 0007558580000004
Patent Text Reader

Abstract

To provide a structural surface structure with high rigidity allowed to be constructed as a structure of a floor structural surface, a roof structural surface, or a wall structural surface of a wooden building in a simple constitution as well as with reduced labor work, time, and cost.SOLUTION: A structural surface structure is configured to array a plurality of wooden thick plates 10 in a flat rectangular parallelepiped shape in a width direction orthogonal to a longitudinal direction, wherein the thick plates 10 adjacent to each other are connected with U-shaped nails 30 provided with an intermediate shaft part 31 and a pair of nail parts 32 extending in the same direction from each of both ends of the intermediate shaft part 31, the thick plates 10 have fitting parts 20 between the adjacent thick plates 10 through a mortise joint or a tenon joint formed in side surfaces facing the adjacent thick plates 10, and the pair of nail parts 32 are hammered in the fitting parts 20 such that the intermediate shaft part 31 of the U-shaped nail 30 is parallel to the longitudinal direction.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a structural surface structure, which is a floor structural surface, a roof structural surface, or a wall structural surface structure of a wooden building. [Background technology]

[0002] The current Building Standards Act requires structural calculations for wooden buildings with three or more stories, whereas wooden buildings with two or less stories and an area that does not exceed a certain value do not require structural calculations. Instead, they require that the amount of walls required be calculated according to the floor area, and that load-bearing walls be arranged so that the amount of walls present is equal to or greater than the required amount. The Building Standards Act Enforcement Order specifies multiple structural specifications and the wall factor for each specification, so that load-bearing walls are selected by referring to these wall factors when designing buildings. Here, the wall factor is a numerical value that indicates the rigidity of the wall structure, and a wall factor of 1 indicates a load-bearing strength of 1.96 kN per 1 meter of length.

[0003] However, in recent years, there have been a series of large-scale earthquakes that have caused great damage, and an increasing number of building owners are requesting that new buildings, even wooden buildings of two stories or less, have a seismic resistance class of class 3. Seismic resistance classes are stipulated as housing performance indications in the Act on Promotion of Housing Quality Assurance (hereinafter referred to as the "Housing Quality Assurance Act"), with seismic performance equivalent to that stipulated by the Building Standards Act being seismic resistance class 1, and seismic performance that is 1.25 times and 1.5 times that being seismic resistance class 2 and seismic resistance class 3, respectively.

[0004] In order to indicate housing performance under this Quality Assurance Act, in addition to evaluating the strength of the wall structural members, it is also necessary to evaluate the strength of the horizontal structural members (floor structural members, roof structural members). Horizontal structural members have the function of transmitting horizontal forces such as loads from earthquakes and wind pressure from strong winds to bearing walls, and in order to transmit large horizontal forces to bearing walls, the horizontal structural members also need to have a corresponding level of rigidity. The floor magnification is a numerical value that serves as an index of the rigidity of the horizontal structural members, just like the wall magnification, which is an index of the rigidity of the wall structural members.

[0005] Furthermore, the Act on Long-Term Quality Housing was enacted with the aim of promoting the spread of high-performance housing that can be passed down from generation to generation, and with the special tax treatment available, the number of builders seeking long-term quality housing is increasing. In order to be certified as a long-term quality housing, there are certain performance conditions, and in terms of earthquake resistance, it is required to have a seismic resistance grade of Class 2 or higher. Therefore, the floor and wall magnification factors are required as mentioned above.

[0006] In addition, the so-called Exception No. 4 of Article 6 of the Building Standards Act is scheduled to be abolished in 2025, and structural calculations will be required for new construction of two-story wooden buildings (excluding single-story buildings). For these calculations, floor and wall multipliers are necessary. Using horizontal structural members with a high floor multiplier and wall structural members with a high wall multiplier allows greater freedom in the design of buildings.

[0007] Conventionally, wide structural plywood panels have been used to construct horizontal structural surfaces with high floor ratios and wall structural surfaces with high wall ratios. In response to this, the applicant of the present invention has considered whether it would be possible to construct horizontal structural surfaces and wall structural surfaces with high rigidity using board materials (thick boards) cut from wooden logs. Since the width and length of thick boards are limited by the diameter of the logs, they cannot be made as wide as plywood panel materials, and their strength remains correspondingly low, so that currently they are hardly used as a construction material for structural surfaces.

[0008] In recent years, Japan's timber resources have not been fully utilized, which has led to forest degradation, and this has become a problem. In particular, cedar trees have not been utilized much, even though the trees planted after the war are now due for felling. Although cedar trees are found all over Japan and are inexpensive, the demand for them is low. Therefore, if we could build highly rigid structural structures using planks taken from Japanese timber logs, including cedar, we would be able to effectively utilize Japan's timber resources, and provide buildings with highly rigid structural structures at low cost.

[0009] However, the Building Standards Act and related laws and regulations stipulate that the wall factor for structural plywood is 2.5, while for boards, the value varies depending on the type of wood and the presence of knots, and so the wall factor is set at a uniform 0.5 regardless of the type or thickness of the wood. Regarding the floor factor, the evaluation method standard based on the Quality Assurance Act stipulates that the floor factor is 0.7 to 3.0 when structural plywood is used, but 0.2 to 0.3 when thick boards are used and joists are placed at a specified interval. With such low wall and floor factors, it is not possible to design wooden buildings with earthquake resistance grade 3 or long-lasting excellent houses. If a reinforcing structure such as firestop is used to compensate for the strength, not only will the amount of wood required and the amount of work required increase, but the interior appearance will also be poor.

[0010] In addition, for specifications that do not use joists, no statutes prescribe the floor ratio. In light of this, the applicant came up with the idea of ​​constructing a highly rigid structural surface structure using thick planks taken from wood logs, obtaining strength characteristic values ​​through testing at a designated evaluation agency and receiving building confirmation that the structure satisfies building standards set forth in statutes, etc., by considering that for structural specifications not prescribed by statutes, etc., a designated evaluation agency can conduct evaluation tests and perform calculations based on the strength characteristic values ​​obtained from the test results, together with the certification of the test results. In this way, the applicant came up with the idea of ​​constructing a highly rigid structural surface structure using thick planks taken from wood logs, obtaining strength characteristic values ​​through testing at a designated evaluation agency, and receiving building confirmation that the structure satisfies building standards, such as seismic resistance grades.

[0011] There have been several reports on attempts to construct floor or wall structural surfaces using cedar planks and measure their floor or wall magnification (see, for example, Non-Patent Documents 1 to 3). Non-Patent Document 1 reports that a maximum floor magnification of approximately 3.0 was obtained by lining up cedar planks that had been subjected to this groove processing in the width direction, but grooves were made on the back side of the planks and back battens called "wood dowels" were inserted so as to be embedded in the direction perpendicular to the planks. Non-Patent Document 2 reports that a floor magnification of 2.7 was obtained by lining up cedar planks that had been subjected to this groove processing in the width direction, but cross battens were placed in the direction perpendicular to the planks and then nailed to the planks.

[0012] In other words, in both Non-Patent Documents 1 and 2, components arranged in a direction perpendicular to the cedar thick board are fixed to the thick board, which results in a complex configuration and the problem of increased effort, time, and cost.

[0013] Non-Patent Document 3 reports that thick cedar boards that have been processed with this method are lined up in the width direction and a wall ratio of 3.0 or more is obtained, but in addition to placing multiple reinforcing plates perpendicular to the thick boards and screwing them to the thick boards, two reinforcing plates that have been processed with a diagonal cut so that they cross in the center are arranged like diagonal braces and screwed in. Therefore, the structure is complicated, and there are problems in that it takes time, effort, and cost.

[0014] Therefore, there is a demand for a highly rigid structural panel structure that can be constructed with a simple configuration and with reduced effort, time, and cost. [Prior art documents] [Non-patent literature]

[0015] [Non-Patent Document 1] Kinsaku Nakata, "In-plane shear test of cedar plank floor structure using wooden dowels and wood screws", Nara Prefectural Forest Technology Center Research Report, Nara Prefectural Forest Technology Center, April 2016, No. 45, p.7-19 [Non-Patent Document 2] Shingo Nakayama, "Development of high-strength floor structure using cedar planks", [online], Mie Prefecture, [Retrieved December 19, 2022], Internet<URL:https: / / www.pref.mie.lg.jp / ringi / hp / 000250604.htm> [Non-Patent Document 3] Kinsaku Nakata, "Horizontal Load Test of Sugi Plank Shear Wall with Screwed Reinforcement Plates," Nara Prefectural Forest Technology Center Research Report, Nara Prefectural Forest Technology Center, April 2015, No. 44, pp. 49-58 Summary of the Invention [Problem to be solved by the invention]

[0016] In view of the above-mentioned circumstances, the present invention aims to provide a highly rigid structural structure that can be constructed with a simple configuration and reduced effort, time, and cost as the floor structural surface, roof structural surface, or wall structural surface structure of a wooden building. [Means for solving the problem]

[0017] In order to solve the above problems, the structural structure according to the present invention comprises: "It is a structural structure in which several wooden flat rectangular planks are arranged in a row in the width direction perpendicular to the length direction. The adjacent planks are joined by a nail having an intermediate shaft portion and a pair of nail portions extending in the same direction from both ends of the intermediate shaft portion, The thick plate has a side surface facing an adjacent thick plate that is subjected to a groove processing or a scoop processing, so that the adjacent thick plates have a fitting portion therebetween, Furthermore, a pair of the nail portions are driven into the mating portions so that the intermediate shaft portions of the nails are parallel to the longitudinal direction.

[0018] The term "structural plane structure" refers collectively to the structures of floor, roof, and wall. Note that the horizontal plane is a concept that includes the floor and roof planes, and the wall planes are sometimes called the vertical planes.

[0019] When wooden planks are lined up in a row in the width direction to construct a structural surface, the structural specification of joining adjacent planks together with a nail is a new and unprecedented one. Even if one were to conceive of joining adjacent planks together with a nail, it would be a normal idea for a person skilled in the art to use a pair of nails so that one of the nails is driven into one of the adjacent planks and the other of the pair of nails is driven into the other of the adjacent planks, that is, so that the intermediate shaft is perpendicular to the longitudinal direction of the planks and straddles the boundary between the adjacent planks.

[0020] In contrast, in the present invention, by applying a grooved or scooped finish to the side of the thick boards, a fitting portion is provided between adjacent thick boards, and then a pair of nail portions is hammered into the fitting portion so that the intermediate shaft portion of the nail is parallel to the longitudinal direction of the board material to construct a structural surface. In other words, from the outside of the constructed structural surface, it does not look like the nails are joining adjacent thick boards together.

[0021] This method of using nails is extremely novel and, as will be described in detail later, is extremely groundbreaking in that it makes it possible to construct a highly rigid structural structure simply by using nails in a creative way.

[0022] According to the present invention, unlike the conventional technology, no wood is used to join the thick boards, such as back rails, cross rails, or reinforcing boards, and the thick boards are joined only with nails, so the structural structure is very simple. Furthermore, since wood is not required to join the thick boards and nails are inexpensive, the structural structure can be constructed at low cost. Furthermore, since the nails can be driven into the wood at high speed with simple work by using a general stapler (tacker), the structural structure can be constructed easily and in a short time. Effect of the Invention

[0023] As described above, according to the present invention, it is possible to provide a highly rigid structural surface structure that can be constructed with a simple configuration and reduced effort, time, and cost as a floor structural surface, roof structural surface, or wall structural surface structure of a wooden building. [Brief description of the drawings]

[0024] [Figure 1] FIG. 1A is a perspective view of a thick plate that has been subjected to the main groove processing, and FIG. 1B is a perspective view of a thick plate that has been subjected to the double scoop processing. [Diagram 2] FIG. 1(a) is an explanatory diagram of a joint using a nail for joining thick boards that have been subjected to this groove processing, and FIG. 1(b) is an explanatory diagram of a joint using a nail for joining thick boards that have been subjected to a scoop processing. [Diagram 3] This is a plan view of specimen E1. [Figure 4] FIG. 4 is an enlarged view of range A in FIG. [Diagram 5] 5A is a cross-sectional view taken along line BB in FIG. 4, and FIG. 5B is a cross-sectional view taken along line CC in FIG. [Figure 6] This is a plan view of test specimen R1. [Figure 7] FIG. 7 is an enlarged view of range D in FIG. [Figure 8] 8A is a cross-sectional view taken along line EE in FIG. 7, and FIG. 8B is a cross-sectional view taken along line FF in FIG. [Figure 9] This is a plan view of test specimen R2. [Figure 10] FIG. 10 is an enlarged view of the G range in FIG. [Figure 11] 11 is a cross-sectional view taken along line HH in FIG. 10. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0025] The structural surface structure according to one embodiment of the present invention will be described below with reference to the drawings. The structural surface structure according to this embodiment is a floor structural surface, roof structural surface, or wall structural surface structure of a wooden building, in which a plurality of thick planks, which are board materials cut from logs of wood, are arranged in a row in the width direction.

[0026] 1(a) and 1(b), the thick board will be described. The thick board 10 is a flat rectangular wooden board having a length of 90 mm to 185 mm in a width direction (X direction in the figure) perpendicular to the longitudinal direction (Y direction in the figure) and a length of 21 mm to 40 mm in a thickness direction (Z direction in the figure) perpendicular to the longitudinal and width directions.

[0027] In this embodiment, the thick plate 10 is a thick plate 10a having a pair of side surfaces, i.e., a surface facing an adjacent thick plate 10, which is subjected to the present groove processing, or a thick plate 10b having a pair of side surfaces subjected to the ladle processing. When there is no need to distinguish between the thick plate 10a and the thick plate 10b, they are collectively referred to as the thick plate 10.

[0028] In the thick plate 10a subjected to this groove processing, as shown in Fig. 1(a), a convex portion 11a is formed on one of a pair of side surfaces, and a concave portion 12a is formed on the other of the pair of side surfaces. The size and position of the convex portion 11a and the concave portion 12a are set so that the convex portion 11a of one of the adjacent thick plates 10a is fitted into the concave portion 12a of the other, and the front and back surfaces of both plate materials 10a are on the same plane. By fitting the convex portion 11a and the concave portion 12a in this way, a fitting portion 20 is formed between the adjacent thick plates 10a.

[0029] The ladle cutting is a process in which half of the plate thickness is cut out alternately. That is, in the thick plate 10b that has been ladle cut, a notch 12b is formed on the front side of one of the pair of side surfaces, resulting in a protrusion 11b on the back side, and a notch 12b is formed on the back side of the other of the pair of side surfaces, resulting in a protrusion 11b on the front side. By overlapping such protrusion 11b and notch 12b, a fitting portion 20 is formed between the adjacent thick plates 10b, and the front and back surfaces of both plates 10b are on the same plane.

[0030] The nail 30 is a nail comprising an intermediate shaft portion 31 and a pair of nail portions 32 extending in the same direction from both ends of the intermediate shaft portion 31 (see Figs. 2(a) and (b)). That is, the nail 30 is U-shaped. The intermediate shaft portion 31 used for the nail 30 has a length of 12 mm to 36 mm. The length of the nail portion 32 in the nail 30 is set according to the thickness of the thick board 10, and is set to 16 mm to 34 mm, which is slightly shorter than the thickness.

[0031] When joining thick boards 10a that have been subjected to this groove processing with a nail 30, as shown in Fig. 2(a), the convex portion 11a of one of the adjacent thick boards 10a is fitted with the concave portion 12a of the other to form the fitting portion 20. Then, the nail 30 is oriented so that the intermediate shaft portion 31 is parallel to the longitudinal direction of the thick boards 10a, and the pair of nail portions 32 of the nail 30 are driven into the fitting portion 20.

[0032] When joining the planks 10b that have been subjected to the ladle processing with the nail 30, as shown in Fig. 2(b), the extension portion 11b of one of the adjacent planks 10b and the notch portion 12b of the other are overlapped to form the mating portion 20. Then, in the same manner as above, the nail 30 is oriented so that the intermediate shaft portion 31 is parallel to the longitudinal direction of the planks 10b, and the pair of nail portions 32 of the nail 30 are driven into the mating portion 20.

[0033] Here, no adhesive is used to join adjacent planks 10. This is because, unlike in the case of manufacturing building components in a factory, the use of adhesives is prohibited during construction at a building site.

[0034] Next, the structural surface structure of this embodiment is actually constructed, and the strength characteristic values ​​obtained by an evaluation test are compared with those of a structural surface structure of a comparative example.

[0035] 3 to 5, the test structural surface E1, which is the structural surface structure of this embodiment, was constructed by preparing a frame formed of a pair of first long members 51 and a pair of second long members 52 perpendicular to the first long members 51, and then arranging a plurality of thick boards 10 in a row in the width direction while spanning the pair of second long members 52. Within the frame, two third long members 53 parallel to the second long members 52 were spanned between the pair of first long members 51.

[0036] The size of the frame was 2730mm x 2730mm, and 105mm x 105mm square cedar timbers were used for the first long material 51, the second long material 52, and the third long material 53. The distance between adjacent third long materials 53, and the distance between the second long material 52 and the adjacent third long material 53, were each 910mm. Both ends of the second long material 52 and the first long material 51, and both ends of the third long material 53 and the first long material 51 were each joined by dovetailing.

[0037] The thick boards were made of cedar boards 10a with a width and length of 135 mm and a thickness of 30 mm, which were processed with the original groove. In addition, it was assumed that the thick boards would be joined in the longitudinal direction at the actual construction site, so the thick boards 10a were made of a thick board 10aL with a longitudinal length of 1820 mm and a thick board 10aS with a longitudinal length of 910 mm, and one of the two third long members 53, a third long member 53b, was used as the joint between the thick boards 10aL and 10aS. The joint between the thick boards 10aL and 10aS was made with a pot joint. Twenty pieces each of the thick boards 10aL and 10aS were used.

[0038] When the thick boards 10aL and 10aS are arranged in a row in the width direction, the convex portion 11a of one of the adjacent thick boards 10aL is fitted into the concave portion 12a of the other, and the convex portion 11a of one of the adjacent thick boards 10aS is fitted into the concave portion 12a of the other, to form the fitting portion 20. Then, both ends of each of the thick boards 10aL are fastened to one of the pair of second elongated members 52 and the third elongated member 53b with three nails 40, and the thick board 10aL is fastened to the third elongated member 53 at the center in the longitudinal direction with three nails 40. Also, both ends of each of the thick boards 10aS are fastened to the other of the pair of second elongated members 52 and the third elongated member 53b with three nails 40. As the nails 40, CN nails having a length of 90 mm were used.

[0039] Furthermore, at the boundary between adjacent planks 10aL and at the boundary between adjacent planks 10aS, a pair of nail portions 32 of the nail 30 were driven into the fitting portion 20 with the intermediate shaft portion 31 parallel to the longitudinal direction of the planks 10aL and 10aS. This method of driving the nail 30 with the intermediate shaft portion 31 parallel to the longitudinal direction of the planks is hereinafter referred to as "parallel driving of nails". The nail 30 used had an intermediate shaft portion 31 length of 22 mm and a pair of nail portions 32 length of 28 mm, and the pitch (the distance between the nail and the adjacent nail) of the nail 30 in each plank 10aL and 10aS was 150 mm.

[0040] In addition, a structural structure constructed in the same manner as the structural structure E1, except that the pitch of the nails 30 in each of the thick boards 10aL and 10aS was 300 mm, was used as a test structural structure E2.

[0041] For comparison, a structural structure constructed identically to the test structural face E1 except for the direction of the nail 30 was used as the test structural face R1. In the test structural face R1, as shown in Figs. 6-8, one of the pair of nail parts 32 of the nail 30 was driven into one of the mating parts 20 of the adjacent thick boards 10aL and 10aS with the intermediate shaft part 31 perpendicular to the longitudinal direction of the thick boards 10aL and 10aS at the boundary part between the adjacent thick boards 10aL and 10aS, and the other of the pair of nail parts 32 of the nail 30 was driven into the mating part 20 of the other adjacent thick boards 10aL and 10aS. The method of driving the nail 30 with the intermediate shaft part 31 perpendicular to the longitudinal direction of the thick boards in this way is hereinafter referred to as "perpendicular nail driving". The pitch of the nail 30 was 150 mm.

[0042] Furthermore, another test structural member R2 was constructed as a structural member for comparison. As shown in Figs. 9 to 11, the test structural member R2 had the same structure as the test structural members E1, E2, and R1, except that the nails 30 were not used.

[0043] In-plane shear tests were conducted on the test structural surfaces E1, E2, R1, and R2. The tests were conducted at the Gifu Prefectural Academy of Forest Culture, which is designated as an evaluation institution for strength tests of wooden structures. The in-plane shear tests were conducted in accordance with the test method for allowable stress design of wooden frame construction houses by the Japan Housing and Wood Technology Center (public foundation). Specifically, the axial direction of a pair of second long members 52 was set to the up-down direction, and the lower end was fixed to the testing device, and forces in positive and negative directions (axial direction of the first long member 51) were repeatedly applied to the upper end. The repeated loads were set to apparent shear deformation angles of 1 / 450, 1 / 300, 1 / 200, 1 / 150, 1 / 100, 1 / 75, 1 / 50, and 1 / 30 rad, and finally a large deformation was applied in the positive direction.

[0044] Tests were conducted on multiple specimens for each of the test structural surfaces E1, E2, R1, and R2, and the strength characteristic values ​​obtained from the load-shear deformation angle curves for each were averaged and are shown in Table 1. Table 1 shows the "floor ratio" as the stiffness index value for the structural surfaces, but this is when the second long member 52 is considered to be a beam and the test structural surfaces E1, E2, R1, and R2 are considered to be floor structural surfaces. If the second long member 52 is considered to be a column, the test structural surfaces E1, E2, R1, and R2 can be considered to be wall structural surfaces, and the "wall ratio" is obtained as the stiffness index value.

[0045] [Table 1]

[0046] As shown in Table 1, the floor factor of the test structural surface R2, which was made by simply nailing the thick board 10 to the second long member 52 and the third long member 53 without using the nails 30, was a low value of 0.9. With such a low floor factor, it is not possible to design a wooden building with excellent earthquake resistance and durability.

[0047] The test structural plane R1 corresponds to a structure in which the nails 30 are driven perpendicularly into the test structural plane R2. The floor ratio of the test structural plane R2 is 1.3, which is larger than that of the test structural plane R1, but is still low. The perpendicular driving of the nails is a method that a person skilled in the art would come up with using ordinary creativity when thinking of joining thick boards arranged in a row in the width direction with nails. In the case of perpendicular driving, it is clear from the outside that the nails are joining adjacent thick boards. However, this test revealed that a structural plane structure with high rigidity cannot be obtained by driving the nails perpendicularly. This is thought to be because the nails cannot resist the external force acting in the longitudinal direction of the thick board and the component force of the external force, and the thick boards are shifted in the longitudinal direction while the nails are rotated.

[0048] In contrast, the test structural plane E1, which corresponds to a structure in which the nails 30 are driven in parallel to the test structural plane R2 and the pitch of the nails 30 is 150 mm, had a floor ratio of 2.6. This is a high value comparable to the floor ratio of structural plywood. Two nail parts 32 per nail 30 are driven into the mating parts 20 on the same line in the longitudinal direction of the thick boards 10aL, 10aS, and the intermediate shaft part 31 connects these two joints, so it is considered that the nails 30 effectively suppress the longitudinal displacement of the adjacent thick boards 10aL, 10aS.

[0049] It is not obvious from the outside that the parallel nails 30 are joining the adjacent planks 10aL and 10aS. This method of using the nails 30 is very novel and groundbreaking, something that has not been thought of by those skilled in the art before.

[0050] In this way, a structural structure that exhibits a floor multiplier comparable to that of structural plywood makes it possible to design wooden buildings that are highly earthquake-resistant and durable, and also allows for a high degree of freedom in design.

[0051] Test structural face E2, which is similar to test structural face E1 in that the nails 30 are driven in parallel, but has a larger nail pitch of 300 mm, had a floor ratio of 1.9, which was significantly lower than the floor ratio of test structural face E1. This shows that the effect of parallel nails, that is, the effect of preventing the thick boards lined up in the width direction from shifting in the longitudinal direction, is very large.

[0052] As described above, by driving the nails 30 in parallel into the fitting parts 20 of the thick boards 10aL, 10aS arranged in a row in the width direction, a structural structure with high floor and wall ratios can be obtained, and wooden buildings with high earthquake resistance and durability can be designed with a high degree of freedom. The structural structure of this embodiment is an opportunity to break away from conventional wooden buildings that have relied on structural plywood to increase strength, and to switch to wooden buildings that use thick boards of natural wood as they are, which are suited to the Japanese climate, but also have excellent earthquake resistance and durability.

[0053] In addition, in this embodiment, cedar is used as the thick boards, so that Japanese cedar wood, which is currently in its harvesting period but is not being used due to lack of demand, can be effectively utilized as a resource. Furthermore, by using cedar wood, which is abundant in various parts of Japan and is inexpensive, it is possible to provide wooden buildings with high earthquake resistance and durability at low cost. Although it is possible to use cedar as a material for plywood, in that case, many steps are required, such as pre-treating with steam, slicing it thinly to make veneers, drying, laminating and gluing a large number of veneers, and compressing them with heat, which is both time-consuming and costly. In contrast, the structural structure of this embodiment uses the thick boards taken from cedar logs as they are, and can create new demand for cedar without incurring extra time or cost.

[0054] Furthermore, the structural surface structure of this embodiment does not use adhesives. In the case of structural plywood, the adhesive layer prevents moisture from penetrating, and as wooden buildings become more airtight, condensation is more likely to occur, which is a problem. In contrast, this embodiment does not use adhesives to join the thick boards, so there is no adhesive layer to prevent moisture from penetrating, making condensation less likely to occur, and it has the advantage of not having the problem of pollution of the living environment due to volatile components contained in the adhesive.

[0055] The present invention has been described above with reference to preferred embodiments, but the present invention is not limited to the above embodiments, and various improvements and design changes are possible without departing from the spirit of the present invention, as described below.

[0056] For example, in the above embodiment, the structural structure is a floor structural structure or a wall structural structure, but the present invention can also be applied to a roof structural structure, which is a horizontal structural structure. In the case of a sloping roof, it is necessary to multiply the coefficient taking into account the sloping of the roof, but the rigidity index value can be calculated based on the floor magnification factor obtained as a result of the above test.

[0057] In addition, although the above example shows the use of cedar as the material for the thick boards, the material for the thick boards is not limited to cedar. Cedar is the wood with the lowest strength among the woods that are generally available. Therefore, when other woods are used, a value higher than the index value of rigidity obtained by the above test can be obtained. [Explanation of symbols]

[0058] 10 Planks 10a, 10aL, 10aS thick plate (thick plate with genuine groove processing) 10b Thick plate (thick plate with ladle processing) 11a Convex part 11b Extension part 12a Recess 12b Notch 20 Fitting part 30 Matakugi 31 Intermediate shaft 32 Nail part 40 nails 51 First long material 52 Second long material 53,53b Third long piece

Claims

[Claim 1] This is a structural structure in which multiple wooden flat rectangular planks are arranged in a row in the width direction perpendicular to the longitudinal direction. The adjacent planks are joined by a nail having an intermediate shaft portion and a pair of nail portions extending in the same direction from both ends of the intermediate shaft portion, The thick plate has a side surface facing an adjacent thick plate that is subjected to a groove processing or a scoop processing, so that the adjacent thick plates have a fitting portion therebetween, A pair of the nail portions are driven into the fitting portions so that the intermediate shaft portions of the nails are parallel to the longitudinal direction. A structural surface structure characterized by:

Citation Information

Patent Citations

  • JP1989068461U

  • Production of floor member and sound-insulating floor member for direct application obtained thereby

    JP1992068160A

  • Temporary wooden floor

    JP1994028073U

  • Floor material and manufacture thereof

    JP1998121698A

  • Wooden floor material

    JP2004293052A