Method for determining quality of coating, method for determining quality of insulating layer, method for manufacturing substrate having coating, and method for manufacturing solar cell having insulating layer

The method of discoloration and image processing for insulating layers in solar cells addresses non-uniformity and defect detection, improving manufacturing efficiency and yield by enabling precise defect location and correction.

JP7560259B2Active Publication Date: 2024-10-02KANEKA CORP
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
JP2020037107
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-03-04
Publication Date
2024-10-02
Estimated Expiration
2040-03-04

AI Technical Summary

Technical Problem

Existing methods for forming insulating layers in solar cells using printing techniques often result in non-uniform films with defects like holes, leading to undesired short circuits and difficulty in confirming defect locations, which are time-consuming to detect and rectify.

Method used

A method involving discoloration steps under oxidizing or sulfiding conditions, followed by image processing, to identify and locate defects in insulating layers, and a recoloration step to restore the layers for reprinting, enhancing manufacturing efficiency.

Benefits of technology

Enables rapid confirmation of defect locations in insulating layers during manufacturing, improving yield by allowing for precise correction and preventing short circuits, thus enhancing the production process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007560259000001
    Figure 0007560259000001
  • Figure 0007560259000002
    Figure 0007560259000002
  • Figure 0007560259000003
    Figure 0007560259000003
Patent Text Reader

Abstract

To provide a method for determining the quality of a coating film capable of confirming the location of a coating defect of the coating film during a manufacturing process.SOLUTION: Disclosed is a coating quality determination method which determines the quality of a coating film formed on a base material. The coating film is formed in at least a part of the base material. This device includes: a color change step S1 of discoloring the exposed portion of the base material by exposing the base material under an oxidation condition or sulfurization condition; an image processing step S2 of photographing the surface of the base material to perform image processing; and a determination step S3 of determining the quality of the coating film based on the result of the image processing.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for determining the quality of a coating, a method for determining the quality of an insulating layer, a method for manufacturing a substrate having a coating, and a method for manufacturing a solar cell having an insulating layer. [Background technology]

[0002] Patent Documents 1 and 2 disclose techniques relating to the connection of electrodes of two polarities and wiring members in a back-contact type solar cell. The first wiring and the second wiring cross the first electrode and the second electrode, the first wiring is connected to the first electrode at a point where it intersects with the first electrode, and is insulated from the second electrode by an insulating layer at a point where it intersects with the second electrode; The second wiring is connected to the second electrode at a point where it intersects with the second electrode, and is insulated from the first electrode by an insulating layer at a point where it intersects with the first electrode; It is stated that: [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2018-133567 A [Patent Document 2] JP 2015-159286 A Summary of the Invention [Problem to be solved by the invention]

[0004] From the viewpoint of ease of manufacturing, a printing method is sometimes used as a method for forming an insulating layer. In this case, the insulating layer may not be formed as a uniform film. For example, holes may be generated in the insulating layer. This may result in an undesired short circuit between the electrode layer and the wiring member.

[0005] Therefore, during the manufacturing process, it is desirable to check whether the insulating layer is formed as a uniform film, for example, whether holes have occurred in the insulating layer (hereinafter also referred to as coating defects of the insulating layer).

[0006] In this regard, it is conceivable to use a probe to check for coating defects in the insulating layers one by one and at multiple locations on each insulating layer. However, this method takes time. Furthermore, although this method can check for the presence or absence of coating defects in the insulating layers, it is difficult to check the locations of the coating defects in the insulating layers.

[0007] Such problems also arise in various technical fields in which various coatings are formed on various substrates.

[0008] The present invention aims to provide a method for determining whether an insulating layer is defective, which can identify areas of coating defects in an insulating layer during the manufacturing process, and a method for manufacturing a solar cell having an insulating layer. The present invention also aims to provide a method for determining whether a coating is defective, which can identify areas of coating defects in a coating during the manufacturing process, and a method for manufacturing a substrate having a coating. [Means for solving the problem]

[0009] The coating quality determination method of the present invention is a method for determining the quality of a coating formed on a substrate, the coating being formed on at least a portion of the substrate, and includes a discoloration process for exposing the substrate to oxidizing conditions or sulfiding conditions to discolor the exposed portion of the substrate, an image processing process for photographing the surface of the substrate and performing image processing, and a determination process for determining the quality of the coating based on the results of the image processing.

[0010] The insulating layer quality determination method of the present invention is a method for determining the quality of an insulating layer formed between the first metal electrode layer or the second metal electrode layer and a wiring member in a back electrode type solar cell comprising a semiconductor substrate, a first semiconductor layer and a first metal electrode layer stacked in sequence on a portion of one main surface side of the semiconductor substrate, and a second semiconductor layer and a second metal electrode layer stacked in sequence on another portion of the one main surface side of the semiconductor substrate, wherein the insulating layer is formed on at least a portion of the semiconductor substrate corresponding to the wiring member on the first metal electrode layer or the second metal electrode layer, and the method includes a discoloration process of exposing the semiconductor substrate under oxidation conditions or sulfurization conditions to discolor the exposed portion of the first metal electrode layer or the second metal electrode layer, an image processing process of photographing the one main surface side of the semiconductor substrate and processing the image, and a determination process of determining the quality of the insulating layer based on the results of the image processing.

[0011] Another coating quality determination method according to the present invention is a method for determining the quality of a coating formed on a substrate, the coating being formed on at least a portion of the substrate, and the method includes a discoloration step of exposing the substrate to magnetization conditions and adhering iron sand to discolor exposed portions of the substrate, an image processing step of photographing the surface of the substrate and processing the images, and a determination step of determining the quality of the coating based on the results of the image processing.

[0012] Another insulating layer quality determination method according to the present invention is a method for determining the quality of an insulating layer formed between the first metal electrode layer or the second metal electrode layer and a wiring member in a back electrode type solar cell comprising a semiconductor substrate, a first semiconductor layer and a first metal electrode layer stacked in sequence on a portion of one main surface side of the semiconductor substrate, and a second semiconductor layer and a second metal electrode layer stacked in sequence on another portion of the one main surface side of the semiconductor substrate, wherein the insulating layer is formed on at least a portion of the semiconductor substrate on the first metal electrode layer or the second metal electrode layer that corresponds to the wiring member, and the method includes a discoloration step of exposing the semiconductor substrate under magnetization conditions and adhering iron sand to discolor the exposed portion of the first metal electrode layer or the second metal electrode layer, an image processing step of photographing the one main surface side of the semiconductor substrate and processing the image, and a determination step of determining the quality of the insulating layer based on the results of the image processing.

[0013] The method for producing a substrate having a coating according to the present invention includes forming the coating on at least a part of the substrate, and carrying out the discoloration step, the image processing step, and the determination step using the above-mentioned method for determining whether or not the coating is good.

[0014] Another method for manufacturing a substrate having a coating according to the present invention includes forming the coating on at least a portion of the substrate, and using the coating quality determination method described above, carrying out the discoloration step, the image processing step, the determination step, and the color restoration step, and if the coating is determined to be defective in the determination step, forming the coating again.

[0015] The manufacturing method of a solar cell having an insulating layer of the present invention is a back electrode type solar cell comprising a semiconductor substrate, a first semiconductor layer and a first metal electrode layer stacked in sequence on a portion of one main surface side of the semiconductor substrate, and a second semiconductor layer and a second metal electrode layer stacked in sequence on another portion of the one main surface side of the semiconductor substrate, the solar cell having an insulating layer formed between the first metal electrode layer or the second metal electrode layer and a wiring member, the insulating layer being formed on at least a portion of the semiconductor substrate that corresponds to the wiring member on the first metal electrode layer or the second metal electrode layer, and the discoloration process, the image processing process and the judgment process are carried out using the above-mentioned insulating layer quality judgment method.

[0016] Another method for manufacturing a solar cell having an insulating layer according to the present invention is a back electrode type solar cell comprising a semiconductor substrate, a first semiconductor layer and a first metal electrode layer stacked in sequence on a portion of one main surface side of the semiconductor substrate, and a second semiconductor layer and a second metal electrode layer stacked in sequence on another portion of the one main surface side of the semiconductor substrate, the method for manufacturing the solar cell having an insulating layer formed between the first metal electrode layer or the second metal electrode layer and a wiring member, the insulating layer being formed on at least a portion of the semiconductor substrate that corresponds to the wiring member on the first metal electrode layer or the second metal electrode layer, and the discoloration process, the image processing process, the judgment process and the color restoration process being carried out using the above-mentioned insulating layer quality judgment method, and if the insulating layer is judged to be defective in the judgment process, the insulating layer is formed again. Effect of the Invention

[0017] According to the present invention, it is possible to check for a defective coating portion of an insulating layer during the manufacturing process. Also, according to the present invention, it is possible to check for a defective coating portion of a coating during the manufacturing process. [Brief description of the drawings]

[0018] [Figure 1] FIG. 2 is a diagram showing the solar cell according to the embodiment as viewed from the back surface side. [Figure 2A]2 is a cross-sectional view taken along line IIA-IIA of the solar cell of FIG. 1. [Figure 2B] 2 is a cross-sectional view of the solar cell shown in FIG. 1 taken along line IIB-IIB. [Diagram 3] 1A and 1B are diagrams for explaining coating defects of an insulating layer in a solar cell according to an embodiment of the present invention. [Figure 4] 3 is a flowchart of a method for determining the quality of an insulating layer according to the present embodiment. [Diagram 5] 5 is a diagram for explaining a discoloration step in the insulating layer quality determining method shown in FIG. 4. [Figure 6] 5 is a diagram for explaining a discoloration step in the insulating layer quality determining method shown in FIG. 4. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] Hereinafter, an embodiment of the present invention will be described with reference to the accompanying drawings. In each drawing, the same or corresponding parts are denoted by the same reference numerals. For convenience, hatching and reference numerals may be omitted, in which case other drawings shall be referred to.

[0020] (Solar Cell) Fig. 1 is a view of the solar cell according to this embodiment as viewed from the back surface side. Fig. 2A is a cross-sectional view of the solar cell in Fig. 1 taken along line IIA-IIA, and Fig. 2B is a cross-sectional view of the solar cell in Fig. 1 taken along line IIB-IIB. The solar cell 1 shown in Figs. 1, 2A, and 2B is a back electrode type (also called a back contact type or back junction type) solar cell.

[0021] Solar cell 1 includes a semiconductor substrate 11 with two main surfaces, and the main surface of semiconductor substrate 11 has a first region 7 and a second region 8. In the following, the main surface of semiconductor substrate 11 that receives light is referred to as the light-receiving surface, and the main surface of semiconductor substrate 11 opposite the light-receiving surface (one main surface) is referred to as the back surface.

[0022] The first regions 7 are strip-shaped and extend in the Y direction (second direction). Similarly, the second regions 8 are strip-shaped and extend in the Y direction. The first regions 7 and the second regions 8 are alternately provided in the X direction (first direction) that intersects with the Y direction.

[0023] The solar cell 1 includes a passivation layer 13 and an optical adjustment layer 15, which are laminated in this order on the light-receiving surface side of the semiconductor substrate 11. The solar cell 1 also includes a passivation layer 23, a first conductive type semiconductor layer 25, and a first electrode layer 27, which are laminated in this order on a portion (first region 7) of the back surface side of the semiconductor substrate 11. The solar cell 1 also includes a passivation layer 33, a second conductive type semiconductor layer 35, and a second electrode layer 37, which are laminated in this order on another portion (second region 8) of the back surface side of the semiconductor substrate 11. The solar cell 1 also includes a first contact 41 and a first insulating layer 51 corresponding to the first electrode layer 27, and a second contact 42 and a second insulating layer 52 corresponding to the second electrode layer 37.

[0024] The semiconductor substrate 11 is formed of a crystalline silicon material such as single crystal silicon or polycrystalline silicon. The semiconductor substrate 11 is, for example, an n-type semiconductor substrate in which a crystalline silicon material is doped with an n-type dopant. The semiconductor substrate 11 may be, for example, a p-type semiconductor substrate in which a crystalline silicon material is doped with a p-type dopant. An example of the n-type dopant is phosphorus (P). An example of the p-type dopant is boron (B). The semiconductor substrate 11 functions as a photoelectric conversion substrate that absorbs incident light from the light-receiving surface side and generates photocarriers (electrons and holes).

[0025] By using crystalline silicon as the material for the semiconductor substrate 11, the dark current is relatively small, and a relatively high output (stable output regardless of illuminance) can be obtained even when the intensity of incident light is low.

[0026] The passivation layer 13 is formed on the light-receiving surface side of the semiconductor substrate 11. The passivation layer 23 is formed in a first region 7 on the back surface side of the semiconductor substrate 11. The passivation layer 33 is formed in a second region 8 on the back surface side of the semiconductor substrate 11. The passivation layers 13, 23, and 33 are formed of a material containing, for example, an intrinsic (i-type) amorphous silicon material as a main component. The passivation layers 13, 23, and 33 suppress recombination of carriers generated in the semiconductor substrate 11 and increase the carrier collection efficiency.

[0027] The optical adjustment layer 15 is formed on the passivation layer 13 on the light-receiving surface side of the semiconductor substrate 11. The optical adjustment layer 15 functions as an anti-reflection layer that prevents reflection of incident light, and also functions as a protective layer that protects the light-receiving surface side of the semiconductor substrate 11 and the passivation layer 13. The optical adjustment layer 15 is formed of an insulating material, for example, silicon oxide (SiO), silicon nitride (SiN), or a composite thereof such as silicon oxynitride (SiON).

[0028] The first conductive type semiconductor layer 25 is formed on the passivation layer 23, that is, in a first region 7 on the back surface side of the semiconductor substrate 11. On the other hand, the second conductive type semiconductor layer 35 is formed on the passivation layer 33, that is, in a second region 8 on the back surface side of the semiconductor substrate 11. That is, the first conductive type semiconductor layer 25 and the second conductive type semiconductor layer 35 have a strip shape and extend in the Y direction. The first conductive type semiconductor layer 25 and the second conductive type semiconductor layer 35 are alternately arranged in the X direction. A part of the second conductive type semiconductor layer 35 may overlap a part of the adjacent first conductive type semiconductor layer 25 (not shown).

[0029] The first conductive type semiconductor layer 25 is formed of, for example, an amorphous silicon material. The first conductive type semiconductor layer 25 is, for example, a p-type semiconductor layer in which an amorphous silicon material is doped with a p-type dopant (for example, the above-mentioned boron (B)).

[0030] The second conductive type semiconductor layer 35 is formed of, for example, an amorphous silicon material. The second conductive type semiconductor layer 35 is, for example, an n-type semiconductor layer in which an amorphous silicon material is doped with an n-type dopant (for example, the above-mentioned phosphorus (P)). Note that the first conductive type semiconductor layer 25 may be an n-type semiconductor layer, and the second conductive type semiconductor layer 35 may be a p-type semiconductor layer.

[0031] The first electrode layer 27 is formed on the first conductive type semiconductor layer 25, that is, in the first region 7 on the back side of the semiconductor substrate 11. The first electrode layer 27 has a first transparent electrode layer 28 and a first metal electrode layer 29 stacked in order on the first conductive type semiconductor layer 25. The second electrode layer 37 is formed on the second conductive type semiconductor layer 35, that is, in the second region 8 on the back side of the semiconductor substrate 11. The second electrode layer 37 has a second transparent electrode layer 38 and a second metal electrode layer 39 stacked in order on the second conductive type semiconductor layer 35. That is, the first metal electrode layer 29 and the second metal electrode layer 39 have a strip-like shape and extend in the Y direction. The first metal electrode layer 29 and the second metal electrode layer 39 are alternately provided in the X direction.

[0032] The first transparent electrode layer 28 and the second transparent electrode layer 38 are formed of a transparent conductive material. Examples of the transparent conductive material include ITO (Indium Tin Oxide: a composite oxide of indium oxide and tin oxide), ZnO (Zinc Oxide: zinc oxide), etc.

[0033] The first metal electrode layer 29 and the second metal electrode layer 39 are formed of a metallic material or a magnetizable material. Examples of metallic materials that can be used include Ag, Cu, Al, and alloys thereof. The first metal electrode layer 29 and the second metal electrode layer 39 may be formed of a conductive paste material that contains a metallic powder such as silver. Examples of magnetizable materials that can be used include soft magnetic materials such as iron, silicon iron, and permalloy.

[0034] The first contact 41 and the first insulating layer 51 are formed on the first metal electrode layer 29, i.e., in a first region 7 on the back side of the semiconductor substrate 11. The second contact 42 and the second insulating layer 52 are formed on the second metal electrode layer 39, i.e., in a second region 8 on the back side of the semiconductor substrate 11.

[0035] The first insulating layer 51 and the second contact 42 are arranged on a first straight line X1 extending in the X direction (first direction). The second insulating layer 52 and the first contact 41 are arranged on a second straight line X2 different from the first straight line X1 extending in the X direction (first direction). The first straight line X1 and the second straight line X2 intersect the first metal electrode layer 29 and the second metal electrode layer 39, and are arranged alternately in the Y direction (second direction).

[0036] The first insulating layer 51 covers the surface and side surfaces of the first metal electrode layer 29 and the side surfaces of the first transparent electrode layer 28. Similarly, the second insulating layer 52 covers the surface and side surfaces of the second metal electrode layer 39 and the side surfaces of the second transparent electrode layer 38.

[0037] The width of the first insulating layer 51 in the Y direction (second direction) and the width of the second contact 42 in the Y direction are greater than the width of the first wiring member 91. Similarly, the width of the second insulating layer 52 in the Y direction (second direction) and the width of the first contact 41 in the Y direction are greater than the width of the second wiring member 92. For example, the widths of the first insulating layer 51 and the second insulating layer 52 and the widths of the first contact 41 and the second contact 42 are not less than 1 mm and not more than 50 mm. This makes it possible to ensure alignment clearance when connecting the wiring members.

[0038] Examples of materials for the first insulating layer 51 and the second insulating layer 52 include silicon oxide (SiO), silicon nitride (SiN), and compounds thereof such as silicon oxynitride (SiON). Thermosetting resins such as epoxy resins or resin esters that can be applied by screen printing and baked can also be used. Inorganic particles such as silica or talc may be mixed into these resins to improve printability or chemical resistance.

[0039] Cu, Ag, Al, alloys thereof, etc. are used as the material of the first contact 41 and the second contact 42. The first metal electrode layer 29 and the second metal electrode layer 39 may be formed of, for example, a conductive paste material containing a metal powder such as silver.

[0040] 1, the first wiring member 91 extends in the X direction (first direction) along a first straight line X1. Similarly, the second wiring member 92 extends in the X direction (first direction) along a second straight line X2. That is, the first wiring member 91 and the second wiring member 92 intersect the first metal electrode layer 29 and the second metal electrode layer 39, and are alternately arranged in the Y direction (second direction).

[0041] The first wiring member 91 is electrically connected to the second metal electrode layer 39 by the second contact 42, and is electrically insulated from the first metal electrode layer 29 by the first insulating layer 51. Similarly, the second wiring member 92 is electrically connected to the first metal electrode layer 29 by the first contact 41, and is electrically insulated from the second metal electrode layer 39 by the second insulating layer 52.

[0042] The center-to-center distance (pitch) in the Y direction between the first wiring member 91 and the second wiring member 92 is larger than the center-to-center distance (pitch) in the X direction between the first metal electrode layer 29 and the second metal electrode layer 39. For example, the center-to-center distance (pitch) between the first wiring member 91 and the second wiring member 92 is 5 mm or more and 50 mm or less. This makes it possible to shorten the current path flowing through the metal electrode layer, reduce output loss caused by electrode resistance, and improve the power generation efficiency of the solar cell.

[0043] The first wiring member 91 and the second wiring member 92 may be a known tab wire or the like.

[0044] Here, from the viewpoint of ease of manufacturing, a printing method may be used as a method for forming the first insulating layer 51 and the second insulating layer 52, and the first contact 41 and the second contact 42. In this case, as shown in FIG. 3, the first insulating layer 51 or the second insulating layer 52 may not be formed as a uniform film. For example, a hole 55 may be generated in the first insulating layer 51 or the second insulating layer 52. Then, an undesired short circuit occurs between the first metal electrode layer 29 and the first wiring member 91, or between the second metal electrode layer 39 and the second wiring member 92, which may cause a leak when modularized.

[0045] In addition, the printing of the insulating layer is performed in that order, followed by printing of the contacts, but it is difficult to reprint the insulating layer after printing of the contacts. Therefore, after printing of the insulating layer and before printing of the contacts (during the manufacturing process), it is necessary to check whether the insulating layer is formed as a uniform film, for example, whether holes have occurred in the insulating layer (hereinafter also referred to as coating defects of the insulating layer).

[0046] In this regard, it is conceivable to use a probe to check for coating defects in the insulating layers one by one and at multiple locations on each insulating layer before printing the contacts. However, this method is time-consuming. Furthermore, although this method can check for the presence or absence of coating defects in the insulating layers, it is difficult to check the locations of the coating defects in the insulating layers.

[0047] In view of this, the present embodiment provides a method for determining whether an insulating layer is good or bad, which can check for defective coating locations in the insulating layer during the manufacturing process, and can restore the insulating layer to a state in which it can be reprinted and returned to the manufacturing process after checking for defective coating locations in the insulating layer.

[0048] (First embodiment) Next, a method for determining whether an insulating layer is good or bad in a solar cell according to the first embodiment and a method for manufacturing a solar cell using the method for determining whether an insulating layer is good or bad will be described with reference to Figures 4 and 5. Figure 4 is a flow chart of the method for determining whether an insulating layer is good or bad according to the present embodiment, and Figure 5 is a diagram for explaining the discoloration step in the method for determining whether an insulating layer is good or bad shown in Figure 4.

[0049] First, a semiconductor substrate 11 is prepared, in which a first insulating layer 51 is formed on a first straight line X1 on the first metal electrode layer 29, i.e., in a portion corresponding to a first wiring member 91 on the first metal electrode layer 29, and a second insulating layer 52 is formed on a second straight line X2 on the second metal electrode layer 39, i.e., in a portion corresponding to a second wiring member 92 on the second metal electrode layer 39.

[0050] Next, the semiconductor substrate 11 is exposed to an oxidation condition or a sulfurization condition. As a result, the exposed portion 29A of the first metal electrode layer 29 or the exposed portion 39A of the second metal electrode layer 39 is discolored (discoloration step S1) as shown in Fig. 5. This makes the exposed portion of the metal electrode layer visually distinguishable from the insulating layer.

[0051] As described above, examples of the material for the first metal electrode layer 29 and the second metal electrode layer 39 include Ag, Cu, etc. As described above, examples of the material for the first insulating layer 51 and the second insulating layer 52 include inorganic materials such as SiO, and organic materials such as epoxy.

[0052] "Exposing to oxidizing conditions" includes exposing to an oxidizing atmosphere such as immersion in an ozone (O3) aqueous solution, immersion in ozone gas, etc. "Exposing to oxidizing conditions" also includes heating in air.

[0053] "Exposing to sulfurizing conditions" includes exposing to a sulfurizing atmosphere such as H2S gas or aqueous solution, or S (sulfur) vapor.

[0054] For example, when the material of the first metal electrode layer 29 and the second metal electrode layer 39 is Ag, the exposed Ag at the coating defect portion of the first insulating layer 51 or the second insulating layer 52 is blackened by an oxidation reaction (4Ag+O2→2Ag2O). On the other hand, the first insulating layer 51 and the second insulating layer 52 made of SiO or the like are not discolored.

[0055] Furthermore, for example, when the material of the first metal electrode layer 29 and the second metal electrode layer 39 is Ag, the exposed Ag at the coating defect portion of the first insulating layer 51 or the second insulating layer 52 is blackened by the sulfurization reaction (2Ag+S→Ag2S). On the other hand, the first insulating layer 51 and the second insulating layer 52 made of SiO or the like are not discolored.

[0056] Next, the back surface of the semiconductor substrate 11 is photographed using a known imaging device such as a camera. At this time, the photographing direction may be only the front of the back surface, or may be two or more different directions with respect to the back surface. By photographing the back surface from two different directions tilted at 45 degrees in the X direction, for example, the information on the side surface of the electrode can be confirmed in more detail. Then, the photographed image is processed using a known image processing device composed of an arithmetic processor such as a DSP (Digital Signal Processor) or an FPGA (Field-Programmable Gate Array) (image processing step S2).

[0057] Next, based on the result of the image processing, the quality of the first insulating layer 51 or the second insulating layer 52 is judged (judgment step S3). For example, based on the discolored (for example, blackened as described above) portions 29A, 39A, the portions of the first insulating layer 51 or the second insulating layer 52 where the coating is defective are confirmed.

[0058] The location of the coating defect in the first insulating layer 51 or the second insulating layer 52 may be confirmed by visually inspecting the results of image processing displayed on a display device such as a display, etc. Alternatively, the location of the coating defect in the first insulating layer 51 or the second insulating layer 52 may be confirmed automatically using a device configured with an arithmetic processor such as a DSP (Digital Signal Processor) or an FPGA (Field-Programmable Gate Array).

[0059] Next, the semiconductor substrate 11 is exposed to reducing conditions, whereby the discoloration of the exposed portion 29A of the first metal electrode layer 29 or the exposed portion 39A of the second metal electrode layer 39 is reversed (color restoration step S4).

[0060] As described above, when the discoloration process is oxidation, "exposing to reducing conditions" includes exposing to a reducing atmosphere such as introduction into hydrogen (H2) gas, carbon monoxide (CO) gas, or hydrocarbon (CH4, C3H8, etc.) gas. In this case, the semiconductor substrate may be exposed to the reducing atmosphere while being heated. "Exposing to reducing conditions" also includes heating in air (e.g., 200 degrees).

[0061] In addition, when the discoloration process is sulfurization, "exposing to reducing conditions" may be exposing to a reducing atmosphere such as introducing into hydrogen (H2) gas, carbon monoxide (CO) gas, etc. In this case, the semiconductor substrate may be exposed to the reducing atmosphere while being heated.

[0062] Once this color restoration step has been performed, the semiconductor substrate can be returned to the manufacturing process. For example, a non-defective product in which no defective insulating layer coating locations are found in the determination process is advanced to the next contact formation process.

[0063] On the other hand, for example, defective products in which defective insulating layer coating parts are confirmed in the judgment process are returned to the insulating layer formation process. In this way, the defective insulating layer coating parts are improved and then the next contact formation process is started. In addition, when a printing plate such as screen printing is used in insulating film formation, if multiple samples are measured and the defective insulating layer coating parts are common to multiple samples, it is expected that the printing plate is defective. In addition to printing plates, it is also possible to expect that the mask is defective in a similar manner in processes that use masks such as photomasks for lithography. In this way, being able to quickly identify defects in printing plates or masks leads to an improvement in the yield of the manufacturing process.

[0064] As described above, according to the insulating layer quality determination method of the first embodiment and the solar cell manufacturing method using the insulating layer quality determination method, semiconductor substrate 11 is exposed under oxidation conditions or sulfurization conditions to discolor the exposed portion of first metal electrode layer 29 or second metal electrode layer 39 (discoloration step S1), the back surface of semiconductor substrate 11 is photographed and image processing is performed (image processing step S2), and the quality of first insulating layer 51 or second insulating layer 52 is determined based on the result of image processing (determination step S3). This makes it possible to check for defective coating locations of first insulating layer 51 or second insulating layer 52 during the manufacturing process.

[0065] Moreover, according to the insulating layer quality determination method of the first embodiment and the solar cell manufacturing method using the insulating layer quality determination method, after the determination step, the semiconductor substrate 11 is exposed to reducing conditions to reverse the discoloration of the exposed portion of the first metal electrode layer 29 or the second metal electrode layer 39 (recoloring step S4). As a result, after checking the location of the coating defect of the first insulating layer 51 or the second insulating layer 52, the first insulating layer 51 or the second insulating layer 52 can be restored to a state where it can be reprinted, and can be returned to the manufacturing process. This can improve the yield.

[0066] Second embodiment Next, a method for judging the quality of an insulating layer in a solar cell according to a second embodiment and a method for manufacturing a solar cell using the method for judging the quality of an insulating layer will be described with reference to FIGS.

[0067] First, as described above, a semiconductor substrate 11 is prepared in which a first insulating layer 51 is formed on a first straight line X1 on the first metal electrode layer 29, i.e., in a portion corresponding to the first wiring member 91 on the first metal electrode layer 29, and a second insulating layer 52 is formed on a second straight line X2 on the second metal electrode layer 39, i.e., in a portion corresponding to the second wiring member 92 on the second metal electrode layer 39.

[0068] Next, the semiconductor substrate 11 is exposed under magnetization conditions. As a result, the exposed portion 29A of the first metal electrode layer 29 or the exposed portion 39A of the second metal electrode layer 39 is magnetized as shown in FIG. 6. Then, by attaching iron sand to the exposed portion 29A of the first metal electrode layer 29 or the exposed portion 39A of the second metal electrode layer 39, the exposed portion 29A of the first metal electrode layer 29 or the exposed portion 39A of the second metal electrode layer 39 is discolored (for example, the iron sand is blackened) (discoloration step S1). This makes the exposed portion of the metal electrode layer visually distinguishable from the insulating layer. If it is difficult to distinguish the colors of the insulating layer and the iron sand, the iron sand may be painted in advance with a paint of a color different from that of the insulating layer.

[0069] As described above, examples of materials for the first metal electrode layer 29 and the second metal electrode layer 39 include magnetizable materials, specifically soft magnetic materials such as iron, iron silicon, permalloy, etc. As described above, examples of materials for the first insulating layer 51 and the second insulating layer 52 include SiO, etc.

[0070] "Exposing to magnetizing conditions" includes exposing to a magnetic field (magnetic field) atmosphere.

[0071] Next, in the same manner as described above, a known imaging device such as a camera is used to capture an image of the back surface of the semiconductor substrate 11. As described above, the image may be captured only from the front of the back surface, or from two or more different directions relative to the back surface. Then, the captured image is processed using a known image processing device constituted by an arithmetic processor such as a DSP or FPGA (image processing step S2).

[0072] Next, similarly to the above, the quality of the first insulating layer 51 or the second insulating layer 52 is judged based on the result of the image processing (judging step S3). For example, based on the discolored (for example, blackened as described above) portions 29A, 39A, the portions of the first insulating layer 51 or the second insulating layer 52 that have a coating defect are confirmed.

[0073] Next, the semiconductor substrate 11 is exposed to demagnetization conditions, which causes the magnetization of the exposed portion 29A of the first metal electrode layer 29 or the exposed portion 39A of the second metal electrode layer 39 to be demagnetized. Then, the iron sand in the exposed portion 29A of the first metal electrode layer 29 or the exposed portion 39A of the second metal electrode layer 39 is removed, for example, by air blowing, thereby returning the discoloration of the exposed portion 29A of the first metal electrode layer 29 or the exposed portion 39A of the second metal electrode layer 39 to its original state (color restoration step S4).

[0074] Examples of "exposing to demagnetizing conditions" include exposing the semiconductor substrate to a demagnetizing atmosphere such as thermal demagnetization by heating the semiconductor substrate or AC demagnetization using a coil and an AC power source.

[0075] Once this color restoration step has been performed, the semiconductor substrate can be returned to the manufacturing process. For example, a non-defective product in which no defective insulating layer coating locations are found in the determination process is advanced to the next contact formation process.

[0076] On the other hand, for example, defective products in which defective insulating layer coating parts are confirmed in the judgment process are returned to the insulating layer formation process. In this way, the defective insulating layer coating parts are improved and then the next contact formation process is carried out. As described above, when a printing plate such as screen printing is used in insulating film formation, if multiple samples are measured and the defective insulating layer coating parts are common to multiple samples, it is expected that the printing plate is defective. In addition to the printing plate, it is also expected that the mask is defective in a process that uses a mask such as a photomask for lithography. In this way, being able to quickly identify defects in the printing plate or mask leads to an improvement in the yield of the manufacturing process.

[0077] As described above, according to the insulating layer quality determination method of the second embodiment and the solar cell manufacturing method using the insulating layer quality determination method, the semiconductor substrate 11 is exposed under magnetization conditions, and iron sand is attached to the exposed portion of the first metal electrode layer 29 or the second metal electrode layer 39 to discolor the exposed portion (discoloration step S1), the back surface of the semiconductor substrate 11 is photographed and image processing is performed (image processing step S2), and the quality of the first insulating layer 51 or the second insulating layer 52 is determined based on the result of the image processing (determination step S3). This makes it possible to check the location of coating defects in the first insulating layer 51 or the second insulating layer 52 during the manufacturing process.

[0078] Moreover, according to the insulating layer quality determination method of the second embodiment and the solar cell manufacturing method using the insulating layer quality determination method, after the determination step, the semiconductor substrate 11 is exposed under demagnetization conditions to remove the iron sand, thereby returning the discoloration of the exposed portion of the first metal electrode layer 29 or the second metal electrode layer 39 to normal (color restoration step S4). As a result, after checking for defective coating locations of the first insulating layer 51 or the second insulating layer 52, the first insulating layer 51 or the second insulating layer 52 can be restored to a state where it can be reprinted, and can be returned to the manufacturing process. This can improve the yield.

[0079] The method for determining the quality of an insulating layer according to the second embodiment is suitable for an element that has resistance to a magnetic field (magnetic field).

[0080] Although the embodiments of the present invention have been described above, the present invention is not limited to the above-described embodiments and various changes and modifications are possible. For example, in the above-described embodiments, a method for determining the quality of an insulating layer in a solar cell and a method for manufacturing a solar cell using the method for determining the quality of an insulating layer have been described. However, the present invention is not limited to this and can also be applied to determining the quality of various coatings formed on various substrates and manufacturing substrates using the quality determination of the coatings. For example, In the manufacture of semiconductor devices, to determine the quality of protective films (insulating coatings) before metal plating of the base material (because it is too late to do so after plating), - In the manufacture of dissimilar metal-coated tab wires (wiring components) (such as Ag-coated Cu cores or Cu-coated Ag cores), to determine the quality of the metal coating (metal covering) on ​​the metal core (base material) (as the coverage rate cannot be determined from the resistance value of the wiring components alone), It is also applicable to

[0081] For example, in a method for determining the quality of a coating formed on at least a part of a substrate, the substrate may be exposed to oxidizing or sulfiding conditions to discolor the exposed part of the substrate (discoloration step), the surface of the substrate may be photographed and image-processed (image processing step), and the coating may be determined based on the result of the image processing (determination step). In a method for manufacturing a substrate having a coating, after forming a coating on at least a part of the substrate, the discoloration step, image processing step, and determination step may be performed using the above-mentioned coating quality determination method. This makes it possible to check the location of a coating defect during the manufacturing process.

[0082] In addition, in this method for determining the quality of a coating, the substrate may be exposed to reducing conditions after the determination step to reverse the discoloration of the exposed portion of the substrate (recoloring step). This allows the substrate to be restored to a state in which the coating can be reprinted after checking for defective coating areas, and returned to the manufacturing process. This can improve yields. That is, in the method for manufacturing a substrate having a coating, the above-mentioned recoloring step may be carried out after the determination step, and if the coating is determined to be defective in the determination step, the coating may be formed again.

[0083] Also, for example, in a method for determining the quality of a coating formed on at least a portion of a substrate, the substrate is exposed under magnetizing conditions, and iron sand is attached to the exposed portion of the substrate to discolor the exposed portion of the substrate (discoloration step), and the surface of the substrate is photographed and image processed (image processing step), The quality of the coating may be judged based on the result of the image processing (judging step). In addition, in the method for manufacturing a substrate having a coating, after forming a coating on at least a part of the substrate, the discoloration step, image processing step and judging step may be carried out using the above-mentioned coating quality judging method. This makes it possible to check for defective coating locations during the manufacturing process.

[0084] Furthermore, in this method for determining the quality of a coating, after the determination step, the substrate may be exposed to demagnetizing conditions and the iron sand removed to reverse the discoloration of the exposed portion of the substrate (recoloring step). This allows the substrate to be restored to a state in which reprinting of the coating is possible after checking for defective coating areas, and returned to the manufacturing process. This can improve the yield. That is, in the method for manufacturing a substrate having a coating, the above-mentioned recoloring step may be carried out after the determination step, and if the coating is determined to be defective in the determination step, the coating may be formed again. [Explanation of symbols]

[0085] 1. Solar Cell 7 First area 8 Second area 11 Semiconductor substrate 13,23,33 Passivation layer 15 Optical adjustment layer 25 First conductive type semiconductor layer 27 1st electrode layer 28 First transparent electrode layer 29 First metal electrode layer 29A Exposed part 35 Second conductive type semiconductor layer 37 Second electrode layer 38 Second transparent electrode layer 39 Second metal electrode layer 39A Exposed part 41 First Contact 42 Second Contact 51 First insulating layer 52 Second insulating layer 55 holes 91 First wiring member 92 Second wiring member X1 First straight line X2 Second straight line

Claims

1. A method for determining whether a coating formed on a surface of a substrate is good or bad, comprising the steps of: The coating is formed on at least a portion of the surface of the substrate, a discoloring step of exposing the substrate to oxidizing or sulfiding conditions to discolor exposed portions of a surface of the substrate; an image processing step of photographing and processing the surface of the base material; a determining step of determining whether the coating is good or bad based on a result of the image processing; a color restoration step of exposing the substrate to reducing conditions after the determination step to restore the discoloration of the exposed portion of the surface of the substrate; A coating quality determination method comprising the steps of:

2. A method for determining quality of an insulating layer formed between a wiring member and the first metal electrode layer or the second metal electrode layer in a back electrode type solar cell including a semiconductor substrate, a first semiconductor layer and a first metal electrode layer stacked in that order on a portion of one main surface side of the semiconductor substrate, and a second semiconductor layer and a second metal electrode layer stacked in that order on another portion of the one main surface side of the semiconductor substrate, the method comprising: the insulating layer is formed on at least a portion of the semiconductor substrate that corresponds to the wiring member on the first metal electrode layer or the second metal electrode layer; a discoloring step of exposing the semiconductor substrate to an oxidizing or sulfiding condition to discolor an exposed portion of the first metal electrode layer or the second metal electrode layer; an image processing step of photographing the one main surface side of the semiconductor substrate and processing the image; a determining step of determining whether the insulating layer is good or bad based on a result of the image processing; a color restoration step of exposing the semiconductor substrate to a reducing condition after the determination step, thereby removing the discoloration of the exposed portion of the first metal electrode layer or the second metal electrode layer; The method for determining whether an insulating layer is good or bad comprises the steps of:

3. A method for producing a substrate having a coating, comprising the steps of: forming the coating on at least a portion of the substrate; The color changing step, the image processing step, the determination step, and the color restoration step are carried out using the coating quality determination method according to claim 1, If the coating is determined to be defective in the determination step, the coating is formed again. A method for producing a substrate having a coating.

4. A method for manufacturing a back electrode type solar cell comprising: a semiconductor substrate; a first semiconductor layer and a first metal electrode layer laminated in sequence on a portion of one main surface side of the semiconductor substrate; and a second semiconductor layer and a second metal electrode layer laminated in sequence on another portion of the one main surface side of the semiconductor substrate, the solar cell having an insulating layer formed between the first metal electrode layer or the second metal electrode layer and a wiring member, forming the insulating layer on at least a portion of the semiconductor substrate corresponding to the wiring member on the first metal electrode layer or the second metal electrode layer; The method for determining whether an insulating layer is defective or not according to claim 2 is used to carry out the discoloration step, the image processing step, the determination step, and the restoration step, If the insulating layer is determined to be defective in the determination step, the insulating layer is formed again. A method for manufacturing a solar cell having an insulating layer.

Citation Information

Patent Citations

  • Thin film packaging method and device, thin film packaging system and solar cell

    CN108807579A

  • Selection method of semiiconductor pellet

    JP1977012566A

  • Pinhole detection method for dielectric film on semiconductors

    JP1977087367A

  • Method for detecting small hole

    JP1992016756A

  • Defect detecting method of insulating film or semiconductor film

    JP2005166705A