Bridging frustrated Lewis pairs as thermal triggers for the reaction of Si-H with alpha-beta unsaturated esters
Patent Information
- Application Number
- JP2021571823
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-06-04
- Filing Date
- 2020-06-02
- Publication Date
- 2024-10-02
- Estimated Expiration
- 2040-06-02
AI Technical Summary
Existing chemical reactions between silyl hydrides and alpha-beta unsaturated esters require transition metal catalysts, leading to undesired by-products and complex handling requirements, and there is a need for a catalyst that allows for storage stability without rapid reaction until triggered.
Utilizing bridged frustrated Lewis pairs (B-FLPs) as thermal triggers to catalyze the reaction between silyl hydrides and alpha-beta unsaturated esters, which dissociate upon heating to release a Lewis acid, initiating the reaction without the need for transition metal catalysts and allowing for storage stability.
The B-FLP system enables a one-component, storage-stable reaction that rapidly initiates upon heating, avoiding by-products and simplifying handling by eliminating the need for separate catalysts, while providing a gentle and efficient addition reaction.
Smart Images

Figure 0007560489000001 
Figure 0007560489000002 
Figure 0007560489000003
Abstract
Description
[Background technology]
[0001] FIELD OF THEINVENTION The present invention relates to the use of a bridged frustrated Lewis pair as a thermal trigger for the chemical reaction of silyl hydrides with alpha-beta unsaturated esters. The bridged frustrated Lewis pair dissociates upon heating to release a Lewis acid. The Lewis acid acts as a catalyst for the chemical reaction of silyl hydrides with alpha-beta unsaturated esters.
[0002] Introduction Frustrated Lewis pair ("FLP") is a term that refers to a pair of Lewis acids and Lewis bases in which the Lewis acid and Lewis base cannot complex and neutralize each other due to steric congestion. When the Lewis acid and Lewis base of an FLP are mixed, they remain independent of each other rather than mixing and neutralizing each other. In addition, FLPs have been found to indirectly bind to each other in the form of bridged frustrated Lewis pairs ("B-FLP"), in which a bridge molecule binds to both the acid and base of the FLP, forming a complex with the bridge molecule between the Lewis acid and the Lewis base. In some cases, the bridge molecule cleaves to produce a blocked Lewis acid and a blocked Lewis base, and a portion of the bridge molecule can complex with each of the Lewis acid and Lewis base, blocking further complexation or reaction. Hydrogen (H2) is an example of a bridge molecule that cleaves in this manner upon forming a B-FLP.
[0003] B-FLP has been used to activate bridge molecules for use in chemical reactions. For example, hydrogen (H2) has been used as a bridge molecule in B-FLP to activate hydrogen for use in hydrogenation reactions (see, e.g., JACS 2015, 137, 10018-10032), and carbon dioxide has been used as a bridge molecule in B-FLP to activate carbon dioxide for deoxyhydrosilylation (see, e.g., JACS 2010, 132, 10660-10661). Other molecules used as bridge molecules in B-FLP for use in activation for chemical reactions include nitrous oxide (N2O), sulfur dioxide (SO2), alkenes, and alkynes. See, for example, Angew. Chem. Int. Ed. 2009, 48, 6643-6646; Angew. Chem. Int. Ed. 2015, 54, 6400-6441 and JACS 2015, 137, 10018-10032. Summary of the Invention [Problem to be solved by the invention]
[0004] It would be surprising and useful to discover additional uses for B-FLP, especially if such uses allow for the control of chemical reactions other than those involving cross-linking molecules.
[0005] The present invention provides the surprising and unexpected use of B-FLP as a thermal trigger for the reductive curing reaction of silyl hydrides (Si-H) with alpha-beta unsaturated esters in reactions that do not require transition metal catalysis, such as hydrosilylation.
[0006] Hydrosilylation reaction is one way to react silyl hydrides with unsaturated bonds in a curing reaction. Hydrosilylation typically requires the presence of a transition metal catalyst, which tends to remain undesirably in the reaction product. However, it has been discovered that silyl hydrides and alpha-beta unsaturated esters undergo reductive curing reactions in the presence of Lewis acid catalysts without the need for transition metal catalysts. The reductive curing reaction between silyl hydrides and alpha-beta unsaturated esters is an addition reaction that either adds silicon to the carbonyl oxygen of the alpha-beta unsaturated ester to create a new silyl ether bond, or adds silicon to the alpha-carbon of the alpha-beta unsaturated ester to form a new silicon-carbon bond. The reaction produces these addition products without producing any by-products other than new addition products, especially gaseous materials. It also offers the advantage of not requiring expensive platinum catalysts and providing a milder and faster addition reaction than platinum-catalyzed hydrosilylation.
[0007] Lewis acid catalyzed reductive cure of silyl hydrides and alpha-beta unsaturated esters may be desired for curing siloxanes in coating, adhesive, and sealant applications. However, the reductive cure reaction tends to be rapid, which requires that the reaction system be provided and stored as a two-part system in which the catalyst is kept away from the Si-H and / or alpha-beta unsaturated ester until the reaction is desired. One-part systems are more easily handled and more desirable than two-part systems because they provide shelf stability for storage, but it is desirable to be able to store the reaction components together in a one-part system in such a way that they have a way to trigger the reductive cure reaction when desired to cure the system.
[0008] The present invention is a result of the discovery that B-FLP can be used in a silyl hydride / alpha-beta unsaturated ester reductive cure reaction system as a latent thermally triggered Lewis acid catalyst. That is, B-FLP containing a Lewis acid catalyst can be combined with a silyl hydride and an alpha-beta unsaturated ester to form a one-part reaction system that is storage stable at 23° C., but reacts rapidly upon heating to release the Lewis acid from the B-FLP. Upon heating, the Lewis acid dissociates from the B-FLP, allowing the Lewis acid to function as a reaction catalyst to initiate the addition reaction of the silyl hydride with the alpha-beta unsaturated ester. Desirably, the compositions of the present invention can be exposed to UV light without triggering the reaction by unblocking the Lewis acid.
[0009] B-FLP was found to be a particularly efficient triggering agent because it is resistant to remixing once decomposed. This means that once the Lewis acid is liberated, it continues to catalyze the reaction without being inhibited by the reformation of B-FLP. That is, it has an advantage over Lewis acids directly inhibited with a Lewis base, since the Lewis base remains in solution and can remix with the free Lewis acid to neutralize it. B-FLP requires the reformation of a bridge complex between the Lewis acid and the base, and this reformation is much less likely to occur randomly. This is especially true for escape-prone bridge molecules, such as those that are gaseous and escape the reaction system once B-FLP is decomposed. As a result, the use of B-FLP offers unprecedented control over essentially irreversibly triggering the reaction without the formation of interfering catalyst inhibitors, since once heated sufficiently to dissociate B-FLP, the acid catalyst is expected to be irreversibly released to catalyze the rapid reaction.
[0010] In a first aspect, the invention is a composition comprising a mixture of a silyl hydride, an alpha-beta unsaturated ester, and a bridged frustrated Lewis pair.
[0011] In a second aspect, the invention is a chemical reaction process comprising the steps of: (a) providing a composition of the first aspect; and (b) heating the composition to a temperature sufficient to dissociate a Lewis acid from a bridged frustrated Lewis pair.
[0012] The present invention is useful for preparing coatings, adhesives, and elastomers. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] Test methods refer to the most recent test method as of the priority date of this document unless a date is given with the test method number. Reference to a test method includes both a reference to the testing society and the test method number. The following test method abbreviations and identifiers apply herein: ASTM refers to ASTM International, EN refers to European Norm, DIN refers to Deutsches Institut fuer Normung, and ISO refers to the International Organization for Standardization.
[0014] Products identified by trade names refer to compositions available under those trade names from suppliers as of the priority date of this application.
[0015] "Plurality" means two or more. "And / or" means "and, or alternatively." All ranges are inclusive of endpoints unless otherwise indicated. Products identified by trade names refer to compositions available from suppliers under those trade names as of the priority date of this document, unless otherwise indicated herein.
[0016] The compositions of the present invention comprise a mixture of a silyl hydride, an alpha-beta unsaturated ester, and a bridged frustrated Lewis pair.
[0017] "Alpha-beta unsaturated ester" refers to a molecule containing an ester group and a double bond between the alpha and beta carbons in the chain, the carbon atoms being named based on their proximity to the carbonyl group of the ester. Acrylates and methacrylates are examples of alpha-beta unsaturated esters. Alpha-beta unsaturated esters can include silicon, such as polysiloxanes containing alpha-beta unsaturated esters.
[0018] "(Meth)acrylate" refers to the group consisting of methacrylates and acrylates, including silicon-containing molecules that contain acrylate or methacrylate functional groups.
[0019] An "alkyl" is a hydrocarbon group derived from an alkane by removing a hydrogen atom. A "substituted alkyl" is an alkyl having an atom or chemical moiety other than carbon and hydrogen in place of at least one carbon or hydrogen.
[0020] An "aryl" is a group derived from an aromatic hydrocarbon by removing a hydrogen atom. A "substituted aryl" is an aryl that has an atom or chemical moiety other than carbon and hydrogen in place of at least one carbon or hydrogen.
[0021] "Siloxane" refers to a molecule that contains at least one siloxane (Si-O-Si) bond. "Polysiloxane" is a molecule that contains multiple Si-O-Si bonds. Polysiloxanes typically contain siloxane units, referred to as M, D, T, or Q units. A standard M unit has the formula (CH3)3SiO 1 / 2 A standard D unit has the formula (CH3)2SiO 2 / 2 A standard T unit has the formula (CH3)SiO 3 / 2 A standard Q unit has the formula SiO 4 / 2 The M, D, and T units can have one or more methyl groups replaced with hydrogen or some other moiety.
[0022] A "silyl hydride" is a molecule that contains a silicon-hydrogen (Si-H) bond and can contain multiple Si-H bonds.
[0023] A "frustrated Lewis pair," or "FLP," is a system of Lewis acids and Lewis bases in which the Lewis acid and Lewis base are unable to complex and completely neutralize ("block") each other due to steric congestion. FLPs are known in the art and have been characterized in papers such as JACS 2015, 137, 10018-10032 and papers identified therein. Desirably, an FLP is a system of Lewis acids and Lewis bases in which congestion makes complexation and neutralization impossible at 20 degrees Celsius (°C). Although FLPs are known in the art, it can be determined whether any Lewis pair is an FLP by mixing equimolar amounts of a Lewis acid and a Lewis base at 20°C in a solvent that dissolves both. A Lewis acid and a Lewis base can be considered an FLP if more than 10 mole percent of the Lewis acid and Lewis base remain dissociated. The extent of dissociation is determined by any reasonable means, such as nuclear magnetic resonance spectroscopy or, preferably, ion chromatography using a conductivity or photometric detector.
[0024] Upon heating of the compositions of the present invention, the B-FLP releases a Lewis acid that catalyzes the reaction of the alpha-beta unsaturated ester with the silyl hydride. Heating the composition to a temperature of 80° C. or more, 90° C. or more, 100° C. or more, 110° C. or more, 120° C. or more, 130° C. or more, 140° C. or more, 150° C. or more, 160° C. or more, 170° C. or more, 180° C. or more, 190° C. or more, 200° C. or more, 210° C. or more, while generally not exceeding 300° C., not exceeding 250° C., not exceeding 240° C., not exceeding 230° C., not exceeding 220° C., not exceeding 210° C., not exceeding 200° C., not exceeding 175° C., not exceeding 150° C., not exceeding 140° C., not exceeding 130° C., not exceeding 120° C., not exceeding 110° C., or even not exceeding 100° C., causes the components in the composition to react and cure in 1 hour or less, preferably in 30 minutes or less, more preferably in 10 minutes or less, even more preferably in 5 minutes or less, and even more preferably in 2 minutes or less, 1 minute or less, or even 30 seconds or less.
[0025] The reaction of siloxanes with silyl hydrides is a rearrangement reaction that is generally represented by the following reaction: [ka] (wherein two optional reaction products are shown.) This reaction forms new siloxane bonds and is useful for forming crosslinked polysiloxane systems.
[0026] The compositions of the present invention are storage stable. By "storage stable" is meant that the composition does not form a gel at 23° C. in 10 hours or less, preferably 15 hours or less, even more preferably 24 hours or less, and even more preferably 5 days or less.
[0027] Alpha-Beta Unsaturated Esters The alpha-beta unsaturated ester has the following composition structure (alpha-beta unsaturated ester group) at one or more positions in the molecule: [ka] (wherein R contains the carbon bonded to the oxygen shown and can contain any other atoms.) By way of example, R can be an alkyl, substituted alkyl, benzyl, or a polymeric group having a carbon bonded to it to an oxygen.
[0028] Desirably, the alpha-beta unsaturated ester group may be part of a polymer. Such a polymer may contain one alpha-beta unsaturated ester group or two or more alpha-beta unsaturated ester groups. The alpha-beta unsaturated ester is selected from (meth)acrylates, i.e., compounds having acrylate and / or methacrylate groups, as shown below: [ka] [ka]
[0029] The alpha-beta unsaturated ester group can be bonded to a silicon atom that is typically part of a siloxane group (Si-O-Si) or a polysilane group (Si-Si), which itself is typically part of a polysiloxane chain. When the alpha-beta unsaturated ester group is bonded to a silicon atom, the bond between the oxygen and the silicon is through one or more (generally 2 or more, 3 or more, but not more than 6, 5 or even 4) carbon atoms through a single-bonded oxygen atom in the alpha-beta unsaturated ester group.
[0030] Examples of suitable alpha-beta unsaturated esters include those of the formula MD x D MA y M, wherein D MA is a standard D siloxane unit in which one of the methyl groups is methacryloxypropyl: [ka] where the subscript x is the average number of D units per molecule and is 10 or more, 20 or more, 30 or more, 40 or more, 50 or more, 60 or more, 70 or more, 80 or more, 90 or more, 100 or more, 110 or more, 120 or more, 130 or more, 140 or more, 150 or more, 160 or more, 170 or more, 180 or more, 190 or more, or even 200 or more, while generally being 1000 or less, 800 or less, 600 or less, 400 or less, or even 200 or less, and the subscript y is the average number of D units per molecule and is 10 or more, 20 or more, 30 or more, 40 or more, 50 or more, 60 or more, 70 or more, 80 or more, 90 or more, 100 or more, 110 or more, 120 or more, 130 or more, 140 or more, 150 or more, 160 or more, 170 or more, 180 or more, 190 or more, or even 200 or more. MA The average number of siloxane units is 1 or more, 2 or more, 3 or more, 4 or more, 5 or more, 6 or more, 7 or more, 8 or more, 9 or more, 10 or more, 12 or more, 14 or more, 16 or more, 18 or more, or even 20 or more, while generally being 50 or less, 40 or less, 30 or less, 20 or less, or even 10 or less. 29 Subscript values are determined by Si nuclear magnetic resonance spectroscopy.
[0031] Examples of suitable alpha-beta unsaturated esters that are methacryloxypropyl-terminated polydimethylsiloxanes include those available from Gelest under the trade names DMS-R11 (125-250 cSt), DMS-R18 (50-90 cSt), DMS-R11 (8-14 cSt), and DMS-R31 (1,000 cSt), as well as an acrylate-functional silane available from Gelest under the designation SIVATE™ A200.
[0032] Typically, the concentration of the alpha-beta unsaturated ester in the composition is 70 weight percent (wt%) or more, 75 wt% or more, 80 wt% or more, 85 wt% or more, or even 90 wt% or more, while typically 90 wt% or less, 85 wt% or less, 80 wt% or less, or even 75 wt% or less, based on the total weight of the silyl hydride, the alpha-beta unsaturated ester, and the B-FLP.
[0033] Silyl hydride Silyl hydrides contain one, preferably two or more Si-H bonds. The Si-H bonds are typically part of polysilanes (molecules containing multiple Si-H bonds) or polysiloxanes. Silyl hydrides containing multiple Si-H bonds are desirable as crosslinkers in the compositions of the present invention because they can react with multiple alpha-beta unsaturated ester bonds.
[0034] The silyl hydrides of the present invention may be polymeric. The silyl hydrides may be linear, branched, or contain a combination of linear and branched silyl hydrides. The silyl hydrides may be polysilanes, polysiloxanes, or combinations of polysilanes and polysiloxanes.
[0035] Desirably, the silyl hydride is a polysiloxane molecule having one Si-H bond or two or more Si-H bonds. When the silyl hydride is a polysiloxane, the Si-H bond is on a silicon atom of an M-type or D-type siloxane unit. The polysiloxane may be linear, M(≡SiO 1 / 2) type and D(=SiO 2 / 2 ) type units. Alternatively, the polysiloxane may be branched and contain only T(-SiO 3 / 2 ) type and / or Q(SiO 4 / 2 ) type units.
[0036] Examples of suitable silyl hydrides include pentamethyldisiloxane, bis(trimethylsiloxy)methyl-silane, tetramethyldisiloxane, tetramethylcyclotetrasiloxane, and hydride-terminated poly(dimethylsiloxane), such as those available from Gelest under the trade names DMS-H03, DMS-H25, DMS-H31, and DMS-H41.
[0037] The concentration of silyl hydride is sufficient to provide a molar ratio of Si-H groups to alpha-beta unsaturated ester groups that is typically 0.2 or more, 0.5 or more, 0.7 or more, 0.8 or more, 0.9 or more, 1.0 or more, 1.2 or more, 1.4 or more, 1.6 or more, 1.8 or more, 2.0 or more, 2.2 or more, or even 2.5 or more, while typically 5.0 or less, 4.5 or less, 4.0 or less, 3.5 or less, 3.0 or less, 2.8 or less, 2.5 or less, 2.3 or less, 2.0 or less, 1.8 or less, 1.6 or less, 1.4 or less, 1.2 or less, or even 1.0 or less.
[0038] Either the alpha-beta unsaturated ester or the silyl hydride (or both) can function as a crosslinker in the reaction. The crosslinker has at least two reactive groups per molecule and reacts with two different molecules through these reactive groups to crosslink them together. Increasing the length of the linear chain between the reactive groups in the crosslinker tends to increase the flexibility of the resulting crosslinked product. In contrast, shortening the length of the linear chain between the reactive groups in the crosslinker tends to reduce the flexibility of the resulting crosslinked product. In general, to obtain a more flexible crosslinked product, a linear crosslinker is desired, and the length between the reactive sites is selected to obtain the desired flexibility. To obtain a less flexible crosslinked product, a shorter linear crosslinker or even a branched crosslinker is desired to reduce the flexibility between the crosslinked molecules.
[0039] The silyl hydride may be the same molecule as the alpha-beta unsaturated ester, i.e., a single molecule containing both an alpha-beta unsaturated ester and a silyl hydride functional group may function as both a silyl hydride and an alpha-beta unsaturated ester. Alternatively, the silyl hydride may be a different molecule from the alpha-beta unsaturated ester. The silyl hydride may not include an alpha-beta unsaturated ester. The alpha-beta unsaturated ester may not include a silyl hydride group.
[0040] The compositions (and reaction processes) of the present invention can include two or more silyl hydrides, two or more alpha-beta unsaturated esters, and / or two or more components that function as both silyl hydrides and alpha-beta unsaturated esters.
[0041] Typically, the concentration of the silyl hydride in the composition is 5% by weight or more, 10% by weight or more, 15% by weight or more, 20% by weight or more, or even 25% by weight or more, while typically 30% by weight or less, 25% by weight or less, 20% by weight or less, 15% by weight or less, or even 5% by weight or less, based on the total weight of the silyl hydride, alpha-beta unsaturated ester, and B-FLP.
[0042] Bridged frustrated Lewis pair A bridged frustrated Lewis pair ("B-FLP") is a complex that includes an FLP, where the Lewis acid and Lewis base of the FLP are both bound to a bridge molecule to form a neutralized complex with the bridge molecule that is between the Lewis acid and the Lewis base (i.e., "bridged"). The bridge molecule can be cleaved, such as in the case of H2, such that one portion of the bridge molecule blocks the Lewis acid and another portion of the bridge molecule blocks the Lewis base. Alternatively, and preferably, the bridge molecule remains intact, and the B-FLP becomes a stable complex (at least at 23°C) with the bridge molecule simultaneously bound to the Lewis acid and Lewis base of the FLP.
[0043] The Lewis acid is selected from the group consisting of aluminum alkyls, aluminum aryls, arylboranes including triarylboranes (including substituted aryl and triarylboranes such as fluorinated arylboranes including tris(pentafluorophenyl)borane), boron halides, aluminum halides, gallium alkyls, gallium aryls, gallium halides, silylium cations, and phosphonium cations. Examples of suitable aluminum alkyls include trimethylaluminum and triethylaluminum. Examples of suitable aluminum aryls include triphenylaluminum and tris-pentafluorophenylaluminum. Examples of triarylboranes include the following formula: [ka] where R is independently selected at each occurrence from H, F, Cl, and CF3. Examples of suitable boron halides include (CH3CH2)2BCl and boron trifluoride. Examples of suitable aluminum halides include aluminum trichloride. Examples of suitable gallium alkyls include trimethylgallium. Examples of suitable gallium aryls include triphenylgallium. Examples of suitable gallium halides include trichlorogallium. Examples of suitable silylium cations include (CH3CH2)3Si + X - and Ph3Si + X - Examples of suitable phosphonium cations include FP(C6F5)3 + X - Examples include:
[0044] Lewis bases are the following bases: PR3, P(NR2)3, NR3, N(SiR3) x R 3-x , RC(NR)N, P(NR)R3, guanidine (C(=NR)(NR2)2), amidine (RC(=NR)NR2), phosphazene, and [ka] , where R is independently selected at each occurrence from the group consisting of hydrogen, alkyl, substituted alkyl, aryl, and substituted aryl. Examples of suitable Lewis bases for structure PR3 include tri(t-butyl)phosphine, tri(cyclohexyl)phosphine, PhP(tBu), (cyclohexyl)P(tBu), nBuP(tBu), Me(tBu), tBuP(i-Pr), P(CH 11)3, P(iBu)3, and P(n-Bu)3. Examples of suitable Lewis bases of the structure RC(NR)N include 1,5,7-triazabicyclo[4.4.0]dec-5-ene, 7-methyl-1,5,7-triazabicyclo4.4.0dec-5-ene, and 2,3,4,6,7,8,9,10-octahydropyrimidol[1,2-a]azepine (DBU). Examples of suitable guanidines include guanidine, biguanidine, and 1,1-dimethylguanidine. Examples of suitable amidines include diethylamide and diisopropylamide. Examples of suitable phosphazenes include tert-butylimino-tri(pyrrolidino)phosphorene, tert-octylimino-tris(dimethylamino)phosphorene, and 2-tert-butylimino-2-diethylamino-1,3-dimethylperhydro-1,3,2-diazaphosphorine. Examples of suitable Lewis bases of the following structure are: [ka] Examples include 1,3-dimesityl-imidazol-4,5-dihydro-2-ylidene, 1,3-bis(2,6-diisopropylphenyl)imidazol-2-ylidene, and 1,3-bis(2,4,6-trimethylphenyl)-4,5-dihydroimidazol-2-ylidene.
[0045] A crosslinking molecule within the broadest scope of the present invention includes any molecule that simultaneously binds and blocks the Lewis acid and Lewis base of the FLP to form a B-FLP. The interaction of the crosslinking molecule with the Lewis acid and Lewis base is such that the Lewis acid and Lewis base are blocked by the crosslinking molecule (or a portion thereof) at 23°C, but at least the Lewis acid is desirably unblocked at a temperature of 120°C or higher, preferably 110°C or higher, more preferably 100°C or higher, even more preferably 90°C or higher, 80°C or higher, or even 70°C or higher, while at the same time being desirably 300°C or lower, 240°C or lower, 220°C or lower, 200°C or lower, 180°C or lower, 160°C or lower, 150°C or lower, 125°C or lower, or even 100°C or lower. Unblocking the Lewis acid of the B-FLP can be evidenced by a composition of the present invention containing a B-FLP that cures in less than one-tenth the time required to gel at 23°C.
[0046] Examples of suitable cross-linking molecules include carbon dioxide, hydrogen molecules (H2), nitriles, alkenes, alkynes, ketones, esters, and aldehydes. Desirably, the cross-linking molecules contain 10 or less, preferably 9 or less, carbon atoms, and may contain 8 or less, 7 or less, 6 or less, 5 or less, 4 or less, 3 or less, 2 or less, and even 1 or less or 0 carbon atoms, while the cross-linking molecules may contain 1 or more, 2 or more, 3 or more, 4 or more, 5 or more, and even 6 or more carbon atoms. As mentioned earlier in this specification, in B-FLP, some cross-linking molecules can be cleaved, with a portion of the cross-linking molecules blocking Lewis acids and a portion of the cross-linking molecules blocking Lewis bases. It is preferred that the cross-linking molecules remain uncleaved while bridging the Lewis acids and Lewis bases of the FLP. In that respect, the cross-linking molecules are preferably not hydrogen (H2). More preferably, the cross-linking molecule does not include any molecule that cleaves while cross-linking the Lewis acids and Lewis bases of the FLP.
[0047] B-FLP is desirably "stable" in the compositions of the present invention, meaning that it does not dissociate and release a Lewis acid at temperatures below 23° C. B-FLP can be stable at temperatures below 30° C., below 50° C., below 70° C., and even below 80° C. At the same time, B-FLP dissociates at temperatures above 120° C., preferably above 110° C., more preferably above 110° C., above 100° C., above 90° C., and even above 80° C. B-FLP can be stable at temperatures below ... 1 H and 31 P, 11 B and / or 27 Dissociation of B-FLP is determined by examining for evidence of free Lewis acid by HCl (Al). Alternatively, dissociation of B-FLP can be detected by a composition that cures faster at a given temperature than the same composition without B-FLP.
[0048] One method for preparing B-FLP is by mixing the Lewis acid and Lewis base of the FLP together with the crosslinking molecule in a solvent at 23° C. The mixing promotes the formation of the B-FLP. The B-FLP can be isolated from the solvent, typically by evaporating the solvent or by filtering if the B-FLP precipitates from the solvent. The B-FLP can be stored for long periods at or below 23° C. The B-FLP can be mixed with a silyl hydride and a siloxane to form the composition of the present invention.
[0049] The compositions of the present invention typically contain sufficient B-FLP to provide a Lewis acid concentration of 0.1 parts per million (ppm) or more, 1 ppm or more, 10 ppm or more, 50 ppm or more, 100 ppm or more, 200 ppm or more, 300 ppm or more, 400 ppm or more, 500 ppm or more, 600 ppm or more, 700 ppm or more, 800 ppm or more, 900 ppm or more, 1000 ppm or more, while typically 10,000 ppm or less, 5,000 ppm or less, 1,000 ppm or less, based on the total weight of silyl hydride and alpha-beta unsaturated ester in the composition.
[0050] In contrast to typical blocked Lewis acid systems, the Lewis acid of the B-FLP of the present invention is complexed with a Lewis base via a bridging molecule, thus resulting in bimolecular complexation. Prior art suggests directly complexing the Lewis acid with a blocking agent that is sensitive to ultraviolet (UV) light, so that upon irradiation with UV light, the blocking agent dissociates from the Lewis acid. The B-FLP of the present invention does not require a UV-sensitive blocking agent and may not include any component that liberates the Lewis acid from the B-FLP upon irradiation with UV light. The B-FLP and compositions of the present invention may not include a photoacid generator or any other component that generates a Lewis acid upon exposure to UV radiation.
[0051] The composition of the present invention offers the advantage of a one-component reactive system that is storage stable even when exposed to UV light.Unlike the prior art, the composition does not require UV light for reaction, and does not need to be blocked from exposure to UV light to maintain storage stability.Desirably, the stability of the B-FLP of the present invention is not dependent on (i.e., independent of) exposure to UV light.
[0052] The compositions of the present invention may be free of water, or may contain water, preferably at a concentration of 1 weight percent (wt%) or less, 0.75 wt% or less, 0.5 wt% or less, 0.25 wt% or less, 0.1 wt% or less, 0.05 wt% or less, or even 0.01 wt% or less, based on the weight of the composition.
[0053] Optional Ingredients The compositions of the present invention may consist of a silyl hydride, an alpha-beta unsaturated ester, and a bridged frustrated Lewis pair. Alternatively, the compositions of the present invention may further comprise one optional ingredient or a combination of two or more optional ingredients. The optional ingredients are desirably present in a concentration of 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, 5% or less, or even 1% or less by weight based on the weight of the composition.
[0054] Examples of possible optional components include one or a combination of two or more components selected from the group consisting of hydrocarbyl solvents (typically at a concentration of 10% by weight or less, 5% by weight or less, or even 1% by weight or less based on the weight of the composition), pigments such as carbon black or titanium dioxide, fillers such as metal oxides including SiO2 (typically at a concentration of 50% by weight or less based on the weight of the composition), moisture scavengers, optical brighteners, stabilizers (such as antioxidants and UV stabilizers), and corrosion inhibitors. The composition of the present invention may also be free of any one of such additional components or any combination of two or more of such additional components.
[0055] In particular, the composition of the invention may contain up to 1% by weight of water, up to 0.5% by weight of water relative to the weight of the composition. Desirably, the composition is free of water.
[0056] Chemical Reaction Process The present invention includes a chemical reaction process comprising the steps of (a) providing a composition of the present invention and (b) heating the composition to a temperature sufficient to dissociate a Lewis acid from B-FLP. Upon heating the composition of the present invention, the Lewis acid is released from B-FLP and catalyzes the reaction of the silyl hydride with the alpha-beta unsaturated ester as described above. The composition of the present invention can be provided in step (a) by mixing together B-FLP, the silyl hydride, and the alpha-beta unsaturated ester. As described above, the silyl hydride and the alpha-beta unsaturated ester can be the same molecule.
[0057] The chemical reaction process can be carried out in the absence of water or with a concentration of water that is 1 weight percent (wt%) or less, 0.75 wt% or less, 0.5 wt% or less, 0.25 wt% or less, 0.1 wt% or less, 0.05 wt% or less, or even 0.01 wt% or less, based on the weight of the composition provided in step (a).
[0058] The composition has application, for example, as a coating that undergoes a thermally triggered curing reaction, or as a reactive composition for molding applications where the fluid is disposed within gold and heated to trigger curing to form a molded article. In such applications, the process of the present invention further comprises the step after step (a) and prior to step (b) where the composition is applied to a substrate or disposed within gold. EXAMPLES
[0059] material MD 50 D MA 2.6 M has the following structure: (CH3)3SiO 1 / 2 ((CH3)2SiO 2 / 2 ) 50 ((CH3)(CH2CH2CH2OC(O)C(CH2)CH3)SiO 2 / 2 ) 2.6 O 1 / 2 Si(CH3)3 MD in the following way 50 D MA 2.6Prepare M: Prepare a 1-liter, four-neck flask equipped with a thermocouple, mechanical stirrer, Dean Stark trap-adapted water-cooled condenser, and nitrogen bubbler. Charge the flask with 466.6 g of silanol-terminated polydimethylsiloxane (XIAMETER™ PMX-0930 available from Dow Chemical Company), 75.8 g of 3-methacryloxypropylmethyldimethoxysilane (Gelest), 21.4 g of Dow Corning 200 fluid (0.65 cSt), and 124 g of heptane. Add 0.40 milliliters (mL) of triflic acid to the flask with vigorous stirring. Heat to 76° C. Collect water, methanol, and heptane in the Dean Stark trap. After approximately 4 hours, the reflux temperature rises to 117° C. Remove the heat source and add 15.6 g of calcium carbonate and 32 g of sodium sulfate to the flask at a solution temperature of 101° C. Cool the pot temperature to 23° C. Stir the flask contents for 2 hours and then filter the flask contents through a 0.45 micrometer filter membrane. Rotary evaporate (Rotovap) the filtrate at 80° C. and less than 1 torr pressure for 30 minutes to obtain 456.7 g of MD as a clear, colorless liquid. 50 D MA 2.6 Get M.
[0060] MD 166 D MA 14 M has the following structure: (CH3)3SiO 1 / 2 ((CH3)2SiO 2 / 2 ) 166 ((CH3)(CH2CH2CH2OC(O)C(CH2)CH3)SiO 2 / 2 ) 14 O 1 / 2 Si(CH3)3 MD in the following way 166 D MA 14Prepare M: Prepare a 1-liter, four-neck flask equipped with a thermocouple, mechanical stirrer, Dean Stark trap-adapted water-cooled condenser, and nitrogen bubbler. Charge the flask with 558.9 g of silanol-terminated polydimethylsiloxane (XIAMETER™ PMX-0930 available from Dow Chemical Company), 18.5 g of 3-methacryloxypropylmethyldimethoxysilane (Gelest), 6.1 g of Dow Corning 200 fluid (0.65 cSt), and 121 g of heptane. Add 0.35 milliliters (mL) of triflic acid to the flask with vigorous stirring. Heat to 73° C. Collect water, methanol, and heptane in the Dean Stark trap. After approximately 1 hour, the reflux temperature rises to 90° C. Add 11.0 g of water to the flask and continue the azeotropic distillation process. After about 2 hours, the reflux temperature rises to 96° C. Remove the heat source and add 22.8 g of calcium carbonate and 50 g of sodium sulfate to the flask. Cool the pot temperature to 23° C. Stir the flask contents for 3 hours, then filter the flask contents through a 0.45 micrometer filter membrane. Rotary evaporate the filtrate at 80° C. and less than 1 torr pressure for 1 hour to obtain 586.9 g of MD as a clear, colorless liquid. 166 D MA 14 Get M.
[0061] MD H 65 M has the structure: (CH3)3SiO 1 / 2 (CH3HSiO 2 / 2 ) 65 O 1 / 2 Si(CH3)3 It can be obtained by the following process: A mechanical stirrer is fixed to a three-neck flask and 40 grams (g) of deionized water, 10 g of heptane, and 0.05 g of tosylic acid are added. A mixture of 200 g of methyldichlorosilane and 10 g of trimethylchlorosilane is added dropwise to it over 30 minutes while stirring. Stir for another 60 minutes at 23°C. Wash the reaction solution three times with 50 milliliters (mL) of deionized water each time. Dry the solution with anhydrous sodium sulfate and filter through activated charcoal. Remove the volatiles by rotary evaporation to obtain MD H 65 Obtain M silyl hydride.
[0062] B-FLP (1). In a glovebox, a Schlenk flask equipped with a magnetic stir bar is charged with tri(t-butyl)phosphine (200 milligrams (mg), 1.0 millimole (mmol), 1 equivalent (equiv)) and tris-pentafluorophenylborane (500 mg, 1 mmol, 1 equiv) and the components are dissolved in 10 milliliters (mL) of toluene. The Schlenk flask is sealed and removed from the glovebox. The Schlenk flask is connected to a Schlenk line. The contents of the Schlenk flask are stirred throughout the next step. The Schlenk line is purged with nitrogen and then carbon dioxide is bubbled through the line for 2 minutes. The Schlenk flask is exposed to a carbon dioxide atmosphere and then the flask cap is replaced with a septum. A needle is inserted through the septum to create an outlet for carbon dioxide gas and improve carbon dioxide circulation. After 5 minutes, a white solid precipitates from the reaction mixture. The flask is sealed and stirred at room temperature for an additional hour. Move the flask to a glove box. Add 20 mL of hexane and isolate the white solid by filtration through a glass frit. Wash the white solid with hexane three times (10 mL each time). The white solid is B-FLP(1) (540 mg, 71% yield). B-FLP(1) can be stored without decomposition even when exposed to UV light. 1 H, 31 P, and 11The solid is characterized by B nuclear magnetic resonance spectroscopy (NMR) to confirm the absence of impurities and starting materials. The predicted reaction and structure of B-FLP (1) is as follows: [ka]
[0063] Curing time method To determine the setting (gel) time at 23°C, monitor the reaction composition prepared and stored at 23°C until the composition gels. Setting time is the time required to form a gel. Determine when the sample gels by monitoring the flowability of the sample gel. Check the flowability of the vial contents by inverting the vial and looking at the contents to determine if it flows. Check flowability at 8 hour time intervals and after 24 hour intervals. Record the time at which gelation occurs as evidenced by the inability of the vial contents to flow in 1-2 seconds upon inversion. The composition is exposed to ambient (including ultraviolet) light during the test.
[0064] To determine cure time at 90° C., a 125 micrometer film of the reactant composition is stretched onto a glassine release film substrate and placed in an oven at 90° C. The time it takes for the film to gel at 90° C.
[0065] Comparative Example (Comp Ex) A: Reactant without Lewis Acid 1.68g MD H 65 M and MD of 10g 50 D MA 2.6 M is mixed in a dental cup to form a mixture having a molar ratio of Si-H to alpha-beta unsaturated ester groups of 3. The resulting mixture takes more than 5 days to harden at 23° C. and does not harden in 1 hour at 90° C.
[0066] Comparative Example A shows that a silyl hydride and an alpha-beta unsaturated ester do not cure by themselves at 23°C or 90°C.
[0067] Comparative Example B: Reactant with tris-pentafluorophenylborane 1.68g MD H 65 M and MD of 10g 50 D MA 2.6 M are mixed in a dental cup to form a mixture having a molar ratio of Si-H to alpha-beta unsaturated ester groups of 3. 500 parts by weight of tris-pentafluorophenylborane dissolved in toluene per 1 million parts by weight of the mixture is added to form a reactive composition. The resulting reactive composition cures at 23° C. for 4-5 hours and at 90° C. for 5 minutes.
[0068] Comparative Example B shows that a silyl hydride and an alpha-beta unsaturated ester are not storage stable at 23° C. in the presence of 500 ppm Lewis acid catalyst.
[0069] Example 1 1.68g MD H 65 M and MD of 10g 50 D MA 2.6 M are mixed in a dental cup to form a mixture. Sufficient B-FLP (1) (dissolved in toluene) is added to provide 500 parts by weight of tris-pentafluorophenylborane per 1 million parts by weight of the mixture to form a reaction composition with a molar ratio of Si-H to alpha-beta unsaturated ester groups of 3. The resulting reaction composition cures at 23°C for more than 5 days and at 90°C for 20 minutes. Example 1 shows that by introducing a Lewis acid as B-FLP, the reaction mixture is storage stable at 23°C but still reacts rapidly at 90°C.
[0070] Example 2 1.68g MD H 65 M and MD of 10g 166 D MA 14M are mixed in a dental cup to form a mixture with a molar ratio of Si-H to alpha-beta unsaturated ester groups of 3. Sufficient B-FLP (1) (dissolved in toluene) is added to provide 500 parts by weight of tris-pentafluorophenylborane per 1 million parts by weight of the mixture to form a reaction composition. The resulting reaction composition cures at 23°C for more than 5 days and at 90°C for 20 minutes. Example 2 shows that by introducing a Lewis acid as B-FLP, the reaction mixture is storage stable at 23°C but still reacts rapidly at 90°C.
Claims
1. containing a mixture of silyl hydrides, alpha-beta unsaturated esters, and Bridged Frustrated Lewis Pairs; The composition, wherein the bridged frustrated Lewis pair comprises a Lewis acid of a fluorinated arylborane, a Lewis base selected from the group consisting of PR3 and NR3, where R is independently selected at each occurrence from the group consisting of hydrogen, alkyl, substituted alkyl, aryl, and substituted aryl, and a bridging molecule selected from the group consisting of carbon dioxide and a nitrile.
2. The composition of claim 1 , wherein the composition is free of transition metals.
3. The composition of claim 1 or 2, wherein the alpha-beta ester is a (meth)acrylate or a combination of two or more (meth)acrylates.
4. (a) providing a composition according to any one of claims 1 to 3; (b) heating said composition to a temperature sufficient to dissociate a Lewis acid from said bridged frustrated Lewis pair.
5. 5. The process of claim 4, wherein step (a) comprises mixing together a bridged frustrated Lewis pair, a silyl hydride and an alpha-beta ester.
6. 6. The process of claim 4 or 5, wherein after step (a) and before step (b), the composition is applied to a substrate or placed in a mold.
Citation Information
Patent Citations
Amine Organoborane Complex Initiated Polymerizable Composition Containing Siloxane Polymerizable Component
JP2006522206A
Method for dissociating organoborane-amine complexes
JP2012530601A