Dissimilar material joining method and resistance welding device used therein
The method of forming a protrusion on a first member to be welded addresses the challenge of joining dissimilar materials by accurately positioning and melting the second member, achieving strong welds in mass-produced resistance welding.
Patent Information
- Application Number
- JP2021028824
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-02-25
- Publication Date
- 2024-10-07
- Estimated Expiration
- 2041-02-25
AI Technical Summary
Existing resistance welding methods struggle to reliably join dissimilar materials like aluminum and steel in mass production due to difficulties in accurately positioning interposed small pieces between the joining parts, especially in car body production, where processing accuracy is low and robots can only perform welding at taught positions.
A method involving a first member with a small protrusion formed by plastic deformation, allowing the protruding tip to contact and melt a second member with a lower melting point when sandwiched between electrodes, ensuring accurate positioning and strong welds by increasing temperature at the contact point.
Enables robust welding of dissimilar materials with different melting points, such as steel and aluminum, in mass-produced resistance welding equipment using robots, ensuring strong and accurately positioned joints.
Smart Images

Figure 0007562444000001 
Figure 0007562444000002 
Figure 0007562444000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for joining dissimilar materials and a resistance welding apparatus used therein, and more particularly to a method for joining dissimilar materials for joining a plate-shaped first joined member and a plate-shaped second joined member having a melting point lower than that of the first joined member. [Background technology]
[0002] Resistance welding, which is one of the joining methods, has advantages such as less distortion, good appearance, and short welding time, and is widely used in the automobile industry, especially in the manufacture of car bodies. As is well known, resistance welding, also known as spot welding, is performed by melting the joined members themselves with Joule heat caused by the contact resistance between the members to be joined. The most common joined members for car bodies in such resistance welding are steel plates, so-called steel plates. On the other hand, for example, aluminum (alloy) plates are being used to reduce the weight of car bodies. Although resistance welding technology between aluminum joined members is being established, dissimilar material resistance welding, especially mass-produced resistance welding, between aluminum joined members and iron-based material joined members, such as steel plates, is still under development because the melting points of the two materials are significantly different.
[0003] A method for joining dissimilar materials with different melting points by resistance welding is described in, for example, Patent Document 1 below. In this dissimilar material joining method, for example, a material with a melting point higher than aluminum but lower than steel, such as a small piece of iron, is sandwiched between the joining parts of an aluminum member to be joined and a steel member to be joined, and the aluminum member to be joined and the steel member to be joined are sandwiched between electrodes with the small piece sandwiched between them, and pressure and electricity are applied to weld the two members to be joined. At this time, by making the number of contact points between the steel member to be joined and the small piece smaller than the number of contact points between the aluminum member to be joined and the small piece, the steel member to be joined, which has a higher melting point, and the small piece melt first, and then the aluminum member to be joined and the small piece melt. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Japanese Patent Application Publication No. 6-7958 Summary of the Invention [Problem to be solved by the invention]
[0005] However, when the dissimilar material joining method described in the above Patent Document 1 is used for mass-production resistance welding of plate members for vehicle bodies, particularly mass-production resistance welding using a robot, it is difficult to hold a small piece separate from the members to be joined that are transported along a line between the joining portions of the members to be joined, and to properly abut an electrode against the portion where the small piece is sandwiched. Even if it is possible to hold a small piece separate from the members to be joined, it is difficult to find the portion where the small piece is sandwiched from the outside of the members to be joined. In particular, the plate members for vehicle bodies are formed by press working before joining the plate members, and the processing accuracy is not very high, whereas a robot can only perform resistance welding at a taught position, so that resistance welding is not necessarily performed properly at the portion where the small piece is sandwiched.
[0006] The present invention has been made in consideration of the above-mentioned problems, and an object of the present invention is to provide a dissimilar material joining method and resistance welding apparatus that are capable of welding plate-shaped joined members having different melting points, even in mass-production resistance welding equipment using, for example, a robot. [Means for solving the problem]
[0007] A dissimilar material joining method for achieving the above object includes the steps of: A method for joining dissimilar materials, comprising: sandwiching a plate-like second member to be joined, the second member having a melting point lower than that of the first member to be joined, sandwiching the second member between opposing electrodes at a portion where the second member is sandwiched between the first member to be joined as a joining portion, applying pressure and electricity to the electrodes, and joining the first member to the second member at the joining portion, The joining portion of the first joined member is plastically deformed to form a small protrusion having a predetermined protrusion dimension and tip cross-sectional area in advance, and with the protruding tip of the small protrusion abutting the second joined member, the joining portion is clamped between the electrodes and pressure and electricity are applied thereto to melt the second joined member, and the first joined members are welded together at the molten portion of the second joined member.
[0008] According to this configuration, for example, a plate-like second member to be joined, such as an aluminum plate member, having a low melting point is sandwiched between a first member to be joined, such as a steel plate, and the portion where the second member to be joined is sandwiched between the first member to be joined, and the joining portion is sandwiched between opposing electrodes and pressure and current are applied to join the two members to be joined. At this time, a small protrusion is formed in advance at the joining portion of the first member to be joined by plastically deforming the first member itself. When the protruding tip of the small protrusion is in contact with the second member to be joined, and the joining portion including the small protrusion is sandwiched between opposing electrodes and pressure and current are applied, a large current flows through the protruding tip of the small protrusion, which has a small contact area, and the temperature rises significantly. The heat generated by this temperature rise melts the second member to be joined, which has a low melting point, and the first members to be joined come into contact with each other through the melted portion, and the contact portion melts, solidifies, and is welded. That is, the first member to be joined penetrates into the molten portion of the second member to be joined, and the first members to be joined are welded together. Therefore, unlike a welding state in which the molten second member to be joined is joined to the first member to be joined at an interface, the first members to be joined are welded together inside the plate of the second member to be joined, and sufficient welding (joining) strength is ensured. In addition, since the protruding tip of the small protrusion is abutted against the second member to be joined, the outer surface of the first member to be joined is recessed at the joining portion where the small protrusion is located, and therefore the position of the small protrusion can be accurately detected, and therefore, for example, even with mass production resistance welding equipment using a robot, both joining members can be reliably joined at the position of the small protrusion, i.e., at the joining portion.
[0009] Another configuration of the present invention is characterized in that the small protrusion is formed on a folded portion provided on the first joined member, and the folded portion is folded back to sandwich the second joined member between the folded portion and the plate-shaped portion of the first joined member.
[0010] According to this configuration, the second member to be joined is sandwiched between the folded portion and the plate-shaped portion of the first member to be joined simply by folding back the folded portion of the first member to be joined, whereby the protruding tip of the small protrusion comes into contact with the second member to be joined, and both members to be joined are welded (joined) simply by sandwiching a portion of the folded portion between opposing electrodes and applying pressure and electricity. Therefore, since there is no need to prepare a separate first member to be joined with a small protrusion formed at the joining portion or to sandwich the second member to be joined between the first member to be joined and the separate first member to be joined, joining of both members to be joined is simplified and it is also possible to join the two members at the position of the folded portion, i.e., a more accurate position.
[0011] A further configuration of the present invention is characterized in that a hole is formed in the folded portion when the folded portion is folded back.
[0012] According to this configuration, when the second member to be joined is sandwiched between the folded portion and the plate-like portion of the first member to be joined, and the sandwiched portion is sandwiched between opposing electrodes as a joining portion and electricity is passed through, current flows through the bent portion of the folded portion (current is shunted). Since the bent portion of the folded portion has a hole formed therein, when electricity is passed between the opposing electrodes, the amount of current flowing through the bent portion decreases, and the amount of current flowing through the protruding tip of the small protrusion can be increased by that amount, so that the temperature of the protruding tip of the small protrusion can be increased, and thus the second member to be joined can be reliably melted and the first members to be joined can be welded together.
[0013] Further, a resistance welding apparatus according to the present invention is a resistance welding apparatus used in the above-mentioned dissimilar material joining method, The present invention is characterized in that it comprises a mounting support portion that mounts the first joined member with the folded portion bent in a direction approximately perpendicular to the plate-shaped portion of the first joined member and the second joined member abutted on the plate-shaped portion of the first joined member; a bending electrode that constitutes one of the opposing electrodes and is pressed against the folded portion with the first and second joined members mounted on the mounting support portion to bend the folded portion toward the second joined member; a drive mechanism that drives the bending electrode to fold the folded portion; and a current control device that drives the bending electrode by the drive mechanism to fold the folded portion toward the second joined member and then passes current between the opposing electrodes including the bending electrode.
[0014] According to this configuration, the first member to be joined, whose folded portion is bent in the substantially orthogonal direction, is mounted on the mounting support with the second member in contact with the folded portion, and in this state, the bending electrode is driven by the drive mechanism to press the folded portion against the folded portion, and the folded portion is bent toward the second member to be joined, whereby the folded portion is folded back and the protruding tip of the small protrusion is brought into contact with the second member to be joined as described above. At this time, the bending electrode constituting one of the opposing electrodes is pressed against the folded portion of the first member to be joined, so that if the folded portion and the plate-shaped portion of the first member to be joined, which are sandwiching the second member to be joined, are pressed and current is applied between this bending electrode and the other electrode, the joining portions of both joining members can be joined by welding as is. Effect of the Invention
[0015] As described above, according to the present invention, plate-shaped joining members having different melting points can be firmly joined by welding even in mass-production resistance welding equipment using robots, making it possible to mass-produce steel plates and aluminum plate members used for plate members for vehicle bodies, for example. [Brief description of the drawings]
[0016] [Figure 1] 1 is a detailed explanatory diagram of one embodiment of a dissimilar material joining method of the present invention. FIG. [Diagram 2] 1 is a perspective view showing an embodiment of a resistance welding apparatus used in a dissimilar material joining method of the present invention. [Diagram 3] 3 is a perspective view of a joining portion of a first joined member used in a method for joining dissimilar materials by the resistance welding apparatus of FIG. 2. [Figure 4] 3 is an explanatory diagram of a dissimilar material joining method using the resistance welding apparatus of FIG. 2. [Diagram 5] 5 is a cross-sectional view of a state after joining by the method for joining dissimilar materials shown in FIG. 4. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] Hereinafter, the embodiment of the dissimilar material joining method and the resistance welding device used therein will be described in detail with reference to the drawings. FIG. 2 is a perspective view showing one embodiment of the resistance welding device used in the dissimilar material joining method of the present invention. For example, this resistance welding device is attached to a manipulator of an industrial robot arranged in a body manufacturing line of the automobile industry. Therefore, the orientation of this resistance welding device can be changed in any direction according to the rotation and movement of the manipulator of the robot, but here, the description will be made according to the state of FIG. 2. This resistance welding device has a substantially L-shaped arm member 10 in which an extension part 10b extending in the lateral direction of the figure is protruding from the lower end of a main body part 10a extending in the vertical direction of the figure, and a lower electrode 7 is protruding upward from the tip part of this extension part 10b. A substantially box-shaped frame member 11 penetrating in the vertical direction is fitted on the outside of the main body part 10a of this arm member 10, and both are connected to each other so as to be slidable in the vertical direction of the figure. An upper electrode support part 11a extends from the lower end of the frame member 11 above the extension part 10b of the arm member 10 and protrudes in the same direction as the extension part 10b, and a mounting support part 6 is provided on the upper electrode support part 11a for mounting the first joined member 1 and the second joined member 2 to be joined to each other. A coil spring 12 is interposed between the upper electrode support part 11a of the frame member 11 and the extension part 10b of the arm member 10 to bias the frame member 11 upward in the figure and the arm member 10 downward in the figure. The coil spring 12 is not shown in the following explanatory diagrams.
[0018] The mounting support portion 6 is provided on two mounting plate members 13 arranged on the upper electrode support portion 11a at a distance in the lateral direction perpendicular to the protruding direction of the upper electrode support portion 11a, and the lower electrode 7 passes between the two mounting plate members 13 as described later. The two mounting plate members 13 are cut out at the same height in the vertical direction in the figure, and the two joining members 1 and 2 are mounted on the upper surfaces of the cut-out portions (hereinafter, cut-out portions) in the figure with the second joining member 2 abutting on the first joining member 1. Therefore, the upper surface of the cut-out portion in the figure becomes the mounting surface 14 of the mounting support portion 6 on which the two joining members 1 and 2 are mounted. In addition, a rotating shaft support portion 13a that protrudes upward in the figure on the main body side of the frame member 11 is protruded from the cut-out portions of the two mounting plate members 13. Between the two mounting plate members 13, a folded electrode member 15 is attached so as to be rotatable in the vertical direction in the figure, which is obtained by folding back the folded portion 3 of the first joined member 1 described later and which constitutes the opposing electrode of the lower electrode 7, i.e., the upper electrode. As shown in FIG. 3, for example, the folded electrode member 15 is configured to include a folded electrode portion (folded electrode) 8 that protrudes obliquely upward in the figure toward the upper side of the lower electrode 7 between the two mounting plate members 13, a shaft support portion 15a that protrudes obliquely downward in the figure from the folded electrode portion 8 toward the lower electrode 7 side, and an arm portion 15b that extends in the opposite direction to the folded electrode portion 8, i.e., obliquely downward in the figure. A rotating shaft 16 that penetrates the two mounting plate members 13 is inserted into the shaft support portion 15a, whereby the folded electrode member 15 is supported so as to be rotatable in the vertical direction in the figure.
[0019] Meanwhile, a connecting member 17 extending in approximately the same direction as the extending direction of the folded electrode member 15 is supported between the two mounting plate members 13 on the rotating shaft supporting portion 13a of the mounting plate member 13 above the folded electrode member 15 in the figure so as to be rotatable in the vertical direction in the figure. This connecting member 17 is configured to include a connecting portion 17a extending obliquely upward in the figure above the folded electrode member 15 toward the upper side of the lower electrode 7 in the same manner as the folded electrode member 15, and a link portion 17b extending obliquely downward in the figure substantially parallel to the arm portion 15b of the folded electrode member 15, and a rotating shaft 18 penetrating the rotating shaft supporting portions 13a of the two mounting plate members 13 is inserted into the intermediate portion of the connecting member 17, whereby the connecting member 17 is supported so as to be rotatable in the vertical direction in the figure. The tip end in the extension direction of the arm portion 15b of the bent electrode member 15 and the tip end in the extension direction of the link portion 17b of the connecting member 17 are rotatably connected to two link members 19 that sandwich the bent electrode member 15 and the connecting member 17, and the tip end in the extension direction of the connecting portion 17a of the connecting member 17 is rotatably connected to the lower end of a cylinder rod 20a of an air cylinder 20 shown in Figure 2, which faces downward. Also, the cylinder body 20b of this air cylinder 20 is rotatably connected to the main body portion 10a of the arm member 10. Therefore, the link mechanism including the bent electrode member 15 is driven by the air cylinder 20.
[0020] 2, when the cylinder rod 20a of the air cylinder 20 is extended from a state in which the bent electrode portion 8 of the bent electrode member 15 is extended obliquely upward in the figure, the connecting portion 17a of the connecting member 17 is moved downward in the figure, and the link portion 17b is relatively rotated upward in the figure. Accordingly, the arm portion 15b of the bent electrode member 15 is pulled upward by the link member 19, and the bent electrode portion 8 is relatively rotated downward toward the mounting surface 14 of the two mounting plate members 13. Therefore, as shown by the two-dot chain line in FIG. 2, when the portions of both the joining members 1 and 2 mounted on the mounting surface 14 of the mounting support portion 6 that are bent upward in the figure are pressed by the bent electrode portion 8, the movement of the bent electrode portion 8 causes the bent portion to be folded back onto the mounting surface 14 of the mounting plate member 13. That is, the bent portion corresponds to the folded portion 3 of the present invention, and the link mechanism constituted by the air cylinder 20 and each link member constitutes the drive mechanism of the present invention. The drive of the air cylinder 20 and the pressure and current control of the counter electrodes 7, 8 are performed by a separate welding control device 9. The welding control device 9 is configured to include an arithmetic processing device, a storage device, and an input / output device, such as a programmable control unit. That is, the welding control device 9 controls the expansion and contraction of the air cylinder 20, and controls the pressure and current control (current control device) of the counter electrodes 7, 8 according to a program stored in advance while inputting various sensor signals (not shown). The corners where the folded electrode portion 8 abuts against the folded portion 3 are rounded. The drive source of the drive mechanism can be a servo motor instead of the air cylinder 20.
[0021] In this embodiment, the first member 1 of the members to be joined is the steel plate, and the second member 2, which has a lower melting point than the first member 1, is an aluminum plate member (hereinafter also referred to as an aluminum plate). FIG. 3 shows a folded portion 3 formed on the steel plate, which is the first member 1, and the aluminum plate, which is the second member 2, is abutted on the plate-shaped portion 1a of the first member 1. In this embodiment, a part of the end of the plate-shaped first member 1 is extended in a tongue shape (tab shape) to form the folded portion 3, and this extended folded portion 3 is previously folded in a direction approximately perpendicular to the plate-shaped portion 1a, as shown in FIG. 3. This folded portion 3 is folded back onto the aluminum plate, which is the second member 2, by the movement of the bending electrode portion 8, and the portion where the second member 2 is sandwiched between the folded portion 3 and the plate-shaped portion 1a of the first member 1 is used as a joining portion and is joined by the resistance welding device. It should be noted that this folded portion 3 is merely an example, and can be set arbitrarily according to the shape and specifications of the actual vehicle body panel member.
[0022] As shown in FIG. 3, small protrusions 4 are formed at the folded portion 3, i.e., the joining portion of the first joined member 1. The small protrusions 4 are formed by plastically deforming the plate material of the folded portion 3 in advance, and have a predetermined protruding dimension and a cross-sectional area at the tip. The protruding dimension of the small protrusions 4 is relatively small, and it is particularly important that the cross-sectional area at the tip is small. When the folded portion 3 is folded back toward the second joined member 2, the protruding tip of the small protrusion 4 abuts against the second joined member 2. The small protrusions 4 in this embodiment are conical, but for example, circular burring, i.e., a truncated cone shape (annular shape) with a hole, can also be applied. These small protrusions 4 are formed by plastically deforming the first joined member 1, so the plate surface opposite to the protruding direction of the small protrusions 4 is recessed.
[0023] In this embodiment, a rectangular slit-shaped hole 5 is formed in the bent portion of the folded portion 3 of the first member 1 along the extension direction of the folded portion. This is for reducing current shunting during current flow. When the second member 2 is sandwiched between the folded portion 3 and the plate-shaped portion 1a of the first member 1 and the folded portion 3 and the plate-shaped portion 1a are sandwiched between the opposing electrodes 7 and 8 and a current is applied, as in this embodiment, current also flows through the folded portion of the folded portion 3 into the inside of the plate of the first member 1 (current shunting occurs). In this embodiment, the folded portion 3 is provided with a small protrusion 4, and the largest current flows in the contact area of the small protrusion 4 with the second member 2, but if current shunting occurs in the folded portion of the folded portion 3, the amount of current flowing in the contact area of the small protrusion 4 with the second member 2 becomes smaller, and the temperature rise in this contact area becomes smaller. Therefore, holes 5 are formed in the bent portion of the folded-back portion 3 to reduce the cross-sectional area through which the current flows and reduce the shunting, thereby ensuring the amount of current flowing to the contact portion of the small protrusion 4. Therefore, holes 5 in the bent portion should ideally be provided on the shortest line connecting the portion of the plate-like portion 1a of the first joined member 1 with which the lower electrode 7 contacts and the small protrusion 4 (on the straight line connecting the two before the folded-back portion 3 is bent or folded back). However, even if holes 5 are formed at a position shifted from this shortest line, the shunting reduction effect can still be achieved.
[0024] Next, an outline of a method for joining a first member 1 having a folded portion 3 on which the small protrusion 4 is formed and a second member 2 having a lower melting point than the first member 1 using the resistance welding device will be described. FIG. 4(a) shows a state in which the folded electrode portion 8 of the folded electrode member 15 starts to contact the folded portion 3 of the first member 1. When the cylinder rod 20a of the air cylinder 20 is extended from this state as described above, the folded electrode portion 8 of the folded electrode member 15 is rotated downward, counterclockwise in FIG. 4, so that the folded portion 3 of the first member 1 is pressed by the folded electrode portion 8 and folded toward the second member 2, and finally, as shown in FIG. 4(b), the folded portion 3 is folded back onto the plate-shaped portion 2a of the second member 2. Once the folded portion 3 has been folded back onto the second joined member 2 in this manner, the joining area is sandwiched between the folded electrode portion 8 in contact with the folded portion 3 and the lower electrode 7 in contact with the plate-shaped portion 1a of the first joined member 1, and pressure is applied to both joining members 1, 2 with the opposing electrodes 7, 8, and electricity is passed between the electrodes 7, 8. As will be described later, the aluminum plate, which is the second joined member 2, is melted and the first joined members 1 are welded together at the molten portion.
[0025] In FIG. 4(a), the lower electrode 7 is already in contact with the lower surface of the plate-like portion 1a of the first member 1. However, at this stage, as shown in FIG. 3, the upper end surface of the actual lower electrode 7 is considerably lower than the mounting surface 14 of the mounting plate member 13. As shown in FIG. 4(b), if the cylinder rod 20a of the air cylinder 20 continues to be extended after the folded electrode portion 8 of the folded electrode member 15 folds back the folded portion 3 of the first member 1 toward the second member 2, the folded electrode member 15 will not rotate downward any further. Therefore, the cylinder body 20b of the air cylinder 20 is moved relatively upward in FIG. 2, and the arm member 10 connected to this cylinder body 20b is moved upward. As a result, the lower electrode 7 rises and passes between the two mounting plate members 13 to come into contact with the lower surface of the plate-like portion 1a of the first member 1. Furthermore, when the cylinder rod 20a of the air cylinder 20 is contracted, the arm member 10 and the frame member 11 are restored to the state shown in Fig. 2 by the biasing force of the coil spring 12. Note that, instead of the coil spring 12 as the return spring, it is also possible to apply an air spring or a floating mechanism using a servo motor.
[0026] FIG. 1 shows the details of the bending (folding) process of the folded portion 3 by the folded electrode portion 8 of the folded electrode member 15 and the subsequent welding process. When the folded electrode portion 8 of the folded electrode member 15 is rotated downward as shown in FIG. 1(a), the folded portion 3 in contact with the folded electrode portion 8 is pressed in the lower left direction of the figure and folded toward the second joined member 2. Furthermore, when the folded portion 3 of the first joined member 1 is folded toward the second joined member 2, the protruding tip of the small protrusion 4 protruding toward the second joined member 2 is brought into contact with the second joined member 2 as shown in FIG. 1(b). At this time, the contact area between the small protrusion 4 and the second joined member 2 is small, so if electricity is applied between the folded electrode portion 8 and the lower electrode 7 in this state, a large current flows to the protruding tip of the small protrusion 4, and the contact portion of the small protrusion 4 of the first joined member 1, which has a large electrical resistivity, with the second joined member 2 is significantly heated. The heat generated by this temperature rise melts the contact area with the small protrusion 4 of the second member to be joined, which is made of an aluminum plate with a low melting point. When the second member to be joined 2 melts in this manner and the folded-back portion 3 and plate-like portion 1a of the first member to be joined 1 are pressed by the folding electrode portion 8 and the lower electrode 7, the folded-back portion 3 and plate-like portion 1a of the first member to be joined 1 penetrate into the molten portion of the second member to be joined 2, and the first members to be joined 1 melt and solidify in the molten portion of the second member to be joined 2, as shown in Fig. 1(c), and are welded together.
[0027] FIG. 5 is a detailed cross-sectional view of the welded portion between the first joined members 1 in FIG. 1(c). As is clear from the figure, the aluminum plate, which is the second joined member 2, is completely melted at the welded (joined) portion between the steel plates, which are the first joined members 1, and the first joined members 1 enter this molten portion and are welded to each other. The resistance welded portion between the steel plates, which are the first joined members 1, has already proven to be strong enough, so this dissimilar material joint (welded) portion also has sufficient strength. In addition, as described above, by providing the slit-shaped hole portion 5 at the bent portion of the folded portion 3, the amount of current between the small protrusion 4 and the second joined member 2 can be secured, and the small protrusion 4 can be significantly heated during resistance welding to reliably melt the second joined member 2, and as a result, the first joined members 1 that have entered the molten portion can be welded to each other. The small depressions on the upper surface of the welded portion between the first joined members 1 in FIG. 5 are traces left when the small protrusion 4 is formed by plastic deformation.
[0028] In this manner, in the dissimilar material joining method of this embodiment, the second joined member 2, which is a plate-like member with a low melting point such as an aluminum plate, is sandwiched between the first joined member 1, which is a plate-like member with a high melting point such as a steel plate, and the portion where the second joined member 2 is sandwiched between the first joined member 1 is used as the joining portion, and the joining portion is sandwiched between the opposing electrodes 7, 8 and pressure and current are applied to join the two joining members 1, 2. At this time, the small protrusion 4 is formed in advance at the joining portion of the first joined member 1 by plastically deforming the first joined member 1 itself, so when the joining portion including the small protrusion 4 is sandwiched between the opposing electrodes 7, 8 and pressure and current are applied with the protruding tip of the small protrusion 4 in a state where it is in contact with the second joined member 2, a large current flows through the protruding tip of the small protrusion 4, which has a small contact area, and the temperature rises significantly. The heat generated by this temperature rise melts the second joined member 2, which has a low melting point, and the first joined members 1 come into contact with each other through the melted portion, and the contact portion melts, solidifies, and is welded. That is, the first joined member 1 penetrates into the molten portion of the second joined member 2, and the first joined members 1 are welded together. Therefore, unlike a welding state in which the molten second joined member 2 is joined to the first joined member 1 at an interface, the first joined members 1 are welded together inside the plate of the second joined member 2, ensuring sufficient welding (joining) strength. In addition, since the protruding tip of the small protrusion 4 is abutted against the second joined member 2, the outer surface of the first joined member 1 is recessed at the joining portion where the small protrusion 4 is located, so that the position of the small protrusion 4 can be accurately detected, and therefore, for example, even with mass production resistance welding equipment using a robot, both joining members 1 and 2 can be reliably joined at the position of the small protrusion 4, i.e., at the joining portion.
[0029] Also, a small protrusion 4 is formed on the folded portion 3 of the first member to be joined 1, and the folded portion 3 is folded back to sandwich the second member to be joined 2 between the folded portion 3 and the plate-like portion 1a of the first member to be joined 1. Therefore, simply by folding back the folded portion 3 of the first member to be joined 1, the second member to be joined 2 is sandwiched between the folded portion 3 and the plate-like portion 1a of the first member to be joined 1, whereby the protruding tip of the small protrusion 4 is brought into contact with the second member to be joined 2, and therefore both joining members 1 and 2 are welded (joined) by simply sandwiching a certain portion of the folded portion 3 between the opposing electrodes 7 and 8 and applying pressure and electricity thereto. As a result, there is no need to prepare a separate first joined member 1 having a small protrusion 4 formed at the joining site, or to sandwich the second joined member 2 between that first joined member 1 and the separate first joined member 1. This simplifies the joining of the two joining members 1, 2, and also makes it possible to join the two at the position where the folded-back portion 3 is located, i.e., at a more accurate position.
[0030] In addition, a hole 5 is formed in the bent portion when the folded portion 3 is folded. When the second joined member 2 is sandwiched between the folded portion 3 and the plate-like portion 1a of the first joined member 1, and the sandwiched portion is used as a joining portion and sandwiched between the opposing electrodes 7, 8 and electricity is passed through, a current flows through the folded portion of the folded portion 3 (a shunt current occurs). Since the hole 5 is formed in the folded portion of the folded portion 3, when electricity is passed between the opposing electrodes 7, 8, the amount of current flowing through the folded portion decreases, and the amount of current flowing through the protruding tip of the small protrusion 4 can be increased by that amount, so that the temperature rise of the protruding tip of the small protrusion 4 can be ensured, and the second joined member 2 can be reliably melted to weld the first joined members 1 together.
[0031] In the resistance welding device of the above embodiment, the first member 1, whose folded portion 3 is folded in a substantially perpendicular direction, is mounted on the mounting support 6 with the second member 2 abutting on the first member 1, and the folding electrode 8 is driven by a driving mechanism such as an air cylinder 20 or a link mechanism to press the folded portion 3 against the folded portion 3, and the folded portion 3 is folded toward the second member 2, so that the protruding tip of the small protrusion 4 abuts against the second member 2. At this time, the folding electrode 8, which constitutes one of the opposing electrodes, is pressed against the folded portion 3 of the first member 1, so that the folding electrode 8 and the lower electrode 7 press the folded portion 3 and the plate-shaped portion 1a of the first member 1, which sandwich the second member 2, and then the joining portions of both members 1 and 2 can be joined by welding.
[0032] Although the dissimilar material joining method according to the embodiment has been described above, the present invention is not limited to the configuration described in the above embodiment, and various modifications are possible within the scope of the gist of the present invention. For example, in the above embodiment, a steel plate and an aluminum plate are used for the first joined member 1 and the second joined member 2, which have different melting points, but these joined members are not limited to a steel plate and an aluminum plate. The gist of the present invention is that the second joined member 2, which has a low melting point, is locally melted and the first joined members 1 are welded together at the melted portion, thereby joining the two joined members. The present invention can be applied to any joined member as long as the plate-shaped joined member meets this technical feature.
[0033] Furthermore, the resistance welding device described in the above embodiment is one example, and for example, the mechanism for folding back the folded-back portion 3 of the first joined member 1 towards the second joined member 2 is not limited to the above. The resistance welding device in the above embodiment is characterized in that the member for folding back the folded-back portion 3 of the first joined member 1 towards the second joined member 2 also serves as an electrode. As long as the resistance welding device has such characteristics, various modifications can be made within the scope of the gist of the present invention. [Explanation of symbols]
[0034] 1 First member to be joined 2 Second member to be joined 3 Folded section 4 Small protrusion 5 Hole 6 Mounting support 7 Lower electrode (electrode) 8 Bent electrode part (bent electrode, electrode) 9 Welding control device (current control device) 20 Air cylinder (drive mechanism)
Claims
1. 1. A method for joining dissimilar materials, comprising: sandwiching a plate-shaped second joined member having a melting point lower than that of the first joined member between a plate-shaped first joined member; sandwiching the second joined member between opposing electrodes at a joining portion where the second joined member is sandwiched between the first joined member, applying pressure and electricity thereto, and joining the first joined member and the second joined member at the joining portion, The joining portion of the first workpiece is plastically deformed to form a small protrusion having a predetermined protrusion dimension and a tip cross-sectional area, With the protruding tip of the small protrusion in contact with the second workpiece, the joining portion is sandwiched between the electrodes, and pressure is applied thereto to melt the second workpiece; A method for joining dissimilar materials, comprising welding the first members to each other at a molten portion of the second member.
2. The method for joining dissimilar materials according to claim 1, characterized in that the small protrusion is formed on a folded portion provided on the first member to be joined, and the folded portion is folded back to sandwich the second member to be joined between the folded portion and a plate-shaped portion of the first member to be joined.
3. The method for joining dissimilar materials according to claim 2, wherein a hole is formed in the folded portion when the folded portion is folded back.
4. A resistance welding apparatus used in the dissimilar material joining method according to claim 2 or 3, a mounting support portion on which the first joined member is mounted in a state in which the folded-back portion is folded in a direction substantially perpendicular to the plate-like portion of the first joined member and the second joined member is in contact with the plate-like portion of the first joined member; a bending electrode that constitutes one of the opposing electrodes and is pressed against the folded portion while the first and second workpieces are mounted on the mounting support portion, thereby bending the folded portion toward the second workpiece; a driving mechanism that drives the bending electrode to perform bending processing on the folded portion; a current control device that drives the bending electrode using the drive mechanism so that the folded portion is folded toward the second workpiece side, and then passes current between opposing electrodes including the bending electrode.
Citation Information
Patent Citations
Resistance welding method
JP1989154879A
Welding method for aluminum alloy material and different material
JP1994007958A
Overlapping / Joining method for two kind metal members having different melting point
JP1997085454A
Fastener, apparatus and method for resistance welding
JP2016528044A