Joint structure
The bonded structure design with protrusions, discharge ports, and escape spaces addresses the issue of intermetallic compound exposure, ensuring strong and effective bonding of dissimilar metals by expelling these compounds, thus maintaining structural integrity.
Patent Information
- Application Number
- JP2020170293
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-10-08
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2040-10-08
AI Technical Summary
The bonding strength of dissimilar metals, such as an iron-based and aluminum-based metal members, is compromised by the exposure of intermetallic compounds at the joint ends, necessitating an improvement in joint integrity.
A bonded structure design featuring a first metal member with a protrusion on its bonding surface, discharge ports, and escape spaces to expel intermetallic compounds generated during liquid phase bonding, reducing their exposed area and preventing strength degradation.
The design effectively discharges intermetallic compounds, maintaining the bonding strength and ensuring proper joining of dissimilar metals by minimizing the exposed area of these compounds, thereby enhancing the structural integrity.
Smart Images

Figure 0007563934000001 
Figure 0007563934000002 
Figure 0007563934000003
Abstract
Description
[Technical field]
[0001] The present invention relates to bonded structure Regarding. [Background technology]
[0002] As a conventional joint structure, for example, Patent Document 1 describes a welded joint in which an iron-based metal member and an aluminum-based metal member are joined via a molten layer. This welded joint suppresses a decrease in joint strength by specifying the volume fraction and size of the intermetallic compound contained in the molten layer. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2019-126824 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, the joint structure described in the above-mentioned Patent Document 1 may have a reduced joint strength in the intermetallic compound exposed from the end of the molten layer, for example, and there is room for further improvement in this regard.
[0005] In view of the above, the present invention has been made, and is capable of properly joining dissimilar metals. bonded structure The purpose is to provide. [Means for solving the problem]
[0006] In order to solve the above-mentioned problems and achieve the object, a joint structure according to the present invention includes a first metal member having a first joint surface, a second metal member which is a metal member having a higher melting point than the first metal member and has a second joint surface and a protrusion protruding from the second joint surface toward the first joint surface, a liquid-phase joint formed by liquid-phase joining of the first joint surface and the second joint surface which face each other along a facing direction, an outlet formed by a gap between the first joint surface and the second joint surface and which opens to the outside at an end side of the first joint surface and the second joint surface in a cross direction which crosses the facing direction and which is capable of discharging an intermetallic compound generated by the liquid-phase joining to the outside, a first escape space portion adjacent to an end of the first joint surface in the cross direction and continuous with the outlet, and a second escape space portion adjacent to an end of the second joint surface in the cross direction and continuous with the outlet, and which faces the first escape space portion in the facing direction. the first metal member has a first opening and a second opening that are spaced apart and penetrate through the first metal member in a thickness direction, and the first joining surface for joining the second metal member is provided between the first opening and the second opening, the first opening is adjacent to one of the exhaust outlets and has one of the first escape space portions on the inside that is continuous with the one of the exhaust outlets, and the second opening is adjacent to the other of the exhaust outlets and has the other of the first escape space portions on the inside that is continuous with the other of the exhaust outlets. It is characterized by: Effect of the Invention
[0008] The present invention bonded structure The bonding method includes the following steps: a discharge port capable of discharging the intermetallic compound generated by the liquid phase bonding to the outside, and a first escape space portion and a second escape space portion continuous with the discharge port; therefore, the area of the exposed end face of the intermetallic compound can be reduced, and as a result, dissimilar metals can be properly bonded. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a cross-sectional view showing an example of the configuration of a joint structure according to the first embodiment. [Diagram 2] FIG. 2 is a perspective view showing an example of the configuration of the aluminum plate and the copper plate according to the first embodiment. [Diagram 3] FIG. 3 is a schematic diagram showing an example of the configuration of the welding machine according to the first embodiment. [Figure 4] FIG. 4 is a cross-sectional view showing the aluminum plate and the copper plate before being joined together according to the first embodiment. [Diagram 5] FIG. 5 is a cross-sectional view showing an aluminum plate and a copper plate being joined together according to the first embodiment. [Figure 6]FIG. 6 is a plan view showing an example of discharging the intermetallic compound according to the first embodiment. [Figure 7] FIG. 7 is a diagram showing the bonding surfaces of an aluminum plate and a copper plate photographed by an electron microscope according to the first embodiment. [Figure 8] FIG. 8 is a flowchart showing steps of the bonding method according to the first embodiment. [Figure 9] FIG. 9 is a plan view showing an example of discharging the intermetallic compound according to a modified example of the first embodiment. [Figure 10] FIG. 10 is a cross-sectional view showing an example of the configuration of a joint structure according to the second embodiment. [Figure 11] FIG. 11 is a plan view showing an example of the configuration of an aluminum plate according to the second embodiment. [Figure 12] FIG. 12 is a cross-sectional view showing an aluminum plate and a copper plate before being joined together according to the second embodiment. [Figure 13] FIG. 13 is a cross-sectional view showing an aluminum plate and a copper plate being joined together according to the second embodiment. [Figure 14] FIG. 14 is a plan view showing an example of discharging the intermetallic compound according to the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] The form (embodiment) for carrying out the present invention will be described in detail with reference to the drawings. The present invention is not limited to the contents described in the following embodiment. Furthermore, the components described below include those that a person skilled in the art can easily imagine and those that are substantially the same. Furthermore, the configurations described below can be appropriately combined. Furthermore, various omissions, substitutions, or modifications of the configurations can be made without departing from the gist of the present invention.
[0011] [First embodiment] A bonded structure 1 and a bonding method according to the first embodiment will be described with reference to the drawings. The bonded structure 1 is formed by liquid-phase bonding of dissimilar metals using a bonding method. Here, liquid-phase bonding refers to bonding by applying a voltage to a bonding portion in a state where the metals to be bonded are combined with each other, and melting the metals at the bonding portion. As shown in Figs. 1 and 2, the bonded structure 1 includes an aluminum plate 10 as a first metal member, a copper plate 20 as a second metal member, a liquid-phase bonding portion 30, an exhaust port 40, an exhaust path 50, a first escape space portion 60, and a second escape space portion 70. In this example, the aluminum plate 10 and the copper plate 20 are each formed in a rectangular shape.
[0012] In the following description, the direction along the short sides of the aluminum plate 10 and the copper plate 20 is referred to as the short side direction (cross direction) X, the direction along the long sides of the aluminum plate 10 and the copper plate 20 is referred to as the long side direction (cross direction) Y, and the direction in which the aluminum plate 10 and the copper plate 20 face each other is referred to as the facing direction Z. The short side direction X, the long side direction Y, and the facing direction Z cross each other and are typically perpendicular to each other.
[0013] The aluminum plate 10 is made of aluminum and formed into a rectangular plate (see FIG. 2). The aluminum plate 10 has a first bonding surface 11. The first bonding surface 11 is formed in a planar shape and perpendicular to the facing direction Z. In other words, the first bonding surface 11 is parallel to the short side direction X and the long side direction Y. More specifically, when a virtual plane perpendicular to the facing direction Z is taken as a virtual plane, the first bonding surface 11 is parallel along the virtual plane. The first bonding surface 11 faces the copper plate 20 in the facing direction Z, and is a portion to be liquid-phase bonded to a second bonding surface 21 of the copper plate 20 described later. In this example, the first bonding surface 11 is provided within a predetermined range on one side of the long side direction Y of the aluminum plate 10.
[0014] The copper plate 20 is a metal member having a higher melting point than the aluminum plate 10, and is made of copper. The copper plate 20 is formed into a rectangular plate (see FIG. 2), and in this example, is formed into the same shape as the aluminum plate 10, but is not limited thereto. The copper plate 20 is plated with tin as a sacrificial material for promoting the discharge of the intermetallic compound C. The copper plate 20 has a second bonding surface 21. The second bonding surface 21 faces the aluminum plate 10 in the facing direction Z, and is a portion that is liquid-phase bonded to the first bonding surface 11 of the aluminum plate 10. In this example, the second bonding surface 21 is provided within a predetermined range on one side of the copper plate 20 in the long side direction Y. The second bonding surface 21 has a protruding portion 21a and a flat portion 21b.
[0015] The protruding portion 21a is a portion protruding from the second bonding surface 21 toward the first bonding surface 11 of the aluminum plate 10, and one protruding portion is provided. For example, the protruding portion 21a protrudes from the flat portion 21b of the second bonding surface 21 toward the first bonding surface 11 side from the flat portion 21b along the facing direction Z. The protruding portion 21a is formed, for example, by pressing using a mold, and in this example, as shown in FIG. 2, is formed into a curved surface shape (for example, a spherical shape). Since the protruding portion 21a is formed on the copper plate 20 having a higher melting point than the aluminum plate 10, when the aluminum plate 10 and the copper plate 20 are bonded together, the protruding portion 21a presses the first bonding surface 11 of the aluminum plate 10 and enters the first bonding surface 11 side. In other words, the protruding portion 21a enters the first bonding surface 11 side of the aluminum plate 10 while maintaining the protruding shape of the protruding portion 21a. In other words, a recess is formed in the first bonding surface 11 of the aluminum plate 10 by being pressed by the protruding portion 21a, and the protruding portion 21a is accommodated in the recess. The protruding portion 21a is liquid-phase bonded to the first bonding surface 11 of the aluminum plate 10.
[0016] The flat portion 21b is formed in a flat shape and is a portion surrounding the periphery of the protruding portion 21a. In other words, the flat portion 21b is a portion extending from the edge of the protruding portion 21a to the outside of the protruding portion 21a along the short side direction X and the long side direction Y. That is, the flat portion 21b extends from the edge of the protruding portion 21a to the outside along a virtual plane. The flat portion 21b faces the first bonding surface 11 of the aluminum plate 10 and is liquid-phase bonded to the first bonding surface 11.
[0017] The liquid phase bonding portion 30 is a portion where the first bonding surface 11 and the second bonding surface 21 are liquid-phase bonded. That is, the liquid phase bonding portion 30 is a portion between the first bonding surface 11 and the second bonding surface 21. In other words, the liquid phase bonding portion 30 is a portion between the protruding portion 21a and the first bonding surface 11, and a portion between the flat portion 21b and the first bonding surface 11. The liquid phase bonding portion 30 is configured to include an intermetallic compound C generated by liquid phase bonding. The liquid phase bonding portion 30 is formed so that the thickness of the exposed end surface 31 of the intermetallic compound C exposed to the outside in the facing direction Z is relatively thin. The liquid phase bonding portion 30 is formed so that the thickness of the exposed end surface 31 is, for example, 3 μm or less, and preferably, the thickness of the exposed end surface 31 is 1 μm or less. The intermetallic compound C is a compound of a relatively hard and brittle material.
[0018] The discharge port 40 is a portion for discharging the intermetallic compound C to the outside. The discharge port 40 is formed by a gap between the first bonding surface 11 and the second bonding surface 21, and is a portion that opens to the outside at the end side of the first bonding surface 11 and the second bonding surface 21 in the short side direction X and the long side direction Y. The discharge port 40 is preferably provided in the aluminum plate 10 and the copper plate 20 at a position close to the electrode abutment portion 12 (see FIG. 1 and FIG. 6) which is a portion to which the electrode 101 (102) of the welding machine 100 described later abuts. The electrode abutment portion 12 is formed, for example, in a circular shape. The discharge port 40 is preferably provided, for example, within a predetermined distance from the outer circumferential edge 12a of the electrode abutment portion 12. Specifically, as shown in FIG. 6, the distance D of the discharge port 40 from the outer circumferential edge 12a of the electrode abutment portion 12 is preferably within 20% of the diameter of the electrode 101 (102). For example, when the ends of one side of the long side direction Y of the aluminum plate 10 and the copper plate 20 are joined, the outlet 40 is provided at three locations. For example, the outlet 40 is provided at both ends of the short side direction X of the first joining surface 11 and the second joining surface 21 and at one end of the long side direction Y of the first joining surface 11 and the second joining surface 21 (see FIG. 6). It is preferable that the length of the outlet 40 in the short side direction X or the long side direction Y is a predetermined length or more. For example, when the outlet 40 is provided at the ends of the short side direction X of the first joining surface 11 and the second joining surface 21, it is preferable that the length L of the outlet 40 in the long side direction Y is 10% or more of the diameter of the electrode 101 (102) (see FIG. 6). The outlet 40 can discharge the intermetallic compound C generated by the liquid phase bonding of the aluminum plate 10 and the copper plate 20 to the outside.
[0019] The discharge path 50 is a path for causing the intermetallic compound C to flow to the discharge port 40. The discharge path 50 is formed by a gap between the first bonding surface 11 and the second bonding surface 21, and is a portion that communicates with the discharge port 40 (see Figs. 1 and 4). The discharge path 50 has a space between the first bonding surface 11 and the second bonding surface 21. This space is connected to the discharge port 40. The discharge path 50 is capable of causing the intermetallic compound C generated by the liquid phase bonding of the aluminum plate 10 and the copper plate 20 to flow to the discharge port 40 via the space.
[0020] As shown in Figs. 1 and 6, the first escape space 60 is a portion that allows the intermetallic compound C discharged from the discharge port 40 to escape to the outside. The first escape space 60 is provided adjacent to the discharge port 40, is continuous with the discharge port 40, and is a portion that allows the intermetallic compound C discharged from the discharge port 40 to escape to the aluminum plate 10 side. The first escape space 60 is a space portion adjacent to the ends in the short side direction X and the long side direction Y of the first joint surface 11 of the aluminum plate 10. In this example, the first escape space 60 is adjacent to both ends in the short side direction X and one end in the long side direction Y of the main body of the aluminum plate 10. For example, as shown in Fig. 6, the first escape space 60 faces the side walls 13c and 13d in the short side direction X and the side wall 13i in the long side direction Y of the aluminum plate 10. The side walls 13c, 13d, and 13i are provided adjacent to the discharge port 40 and extend from the discharge port 40 along the facing direction Z to the opposite side to the copper plate 20. The first escape spaces 60 adjacent to the side walls 13c, 13d, and 13i respectively allow the intermetallic compound C discharged from the discharge port 40 to escape to the aluminum plate 10 side.
[0021] As shown in FIG. 1, the second escape space 70 is a portion that allows the intermetallic compound C discharged from the discharge port 40 to escape to the outside. The second escape space 70 is provided adjacent to the discharge port 40, is continuous with the discharge port 40, and allows the intermetallic compound C discharged from the discharge port 40 to escape to the copper plate 20 side. The second escape space 70 is a space portion adjacent to the ends in the short side direction X and the long side direction Y of the second joining surface 21 of the copper plate 20. In this example, the second escape space 70 is adjacent to both ends in the short side direction X and one end in the long side direction Y of the main body of the copper plate 20. The second escape space 70 faces the first escape space 60 in the facing direction Z. The second escape space 70 faces the side walls 13e and 13f in the short side direction X and the side wall (not shown) in the long side direction Y of the copper plate 20. These side walls 13e, 13f are provided adjacent to the discharge port 40 and extend from the discharge port 40 along the facing direction Z to the opposite side to the aluminum plate 10. The second escape spaces 70 adjacent to the side walls 13e, 13f allow the intermetallic compound C discharged from the discharge port 40 to escape to the copper plate 20 side.
[0022] Next, a joining method for joining an aluminum plate 10 and a copper plate 20 by a resistance welding welder 100 will be described. The welder 100 includes a positive electrode 101, a negative electrode 102, and a power source 104 that is connected to the positive electrode 101 and the negative electrode 102 via an electric wire 103 and supplies power. As shown in Fig. 8, the joining method includes a condition setting step (step S1) and a joining step (step S2).
[0023] In the condition setting step (step S1), processing conditions such as the power supplied from the power source 104 and the time for supplying the power are set in the welding machine 100. The processing conditions are preferably conditions that do not allow the growth of intermetallic compound C generated by liquid phase bonding of the aluminum plate 10 and the copper plate 20. After the condition setting step (step S1), the process proceeds to the joining step (step S2).
[0024] In the joining process (step S2), a voltage is applied to the aluminum plate 10 and the copper plate 20 in a state where the first joining surface 11 of the aluminum plate 10 and the second joining surface 21 of the copper plate 20 are pressed against each other, thereby performing liquid phase joining. For example, in the joining process, the aluminum plate 10 and the copper plate 20 are set between the positive electrode 101 and the negative electrode 102 of the welding machine 100 in a state where the first joining surface 11 of the aluminum plate 10 and the second joining surface 21 of the copper plate 20 face each other along the facing direction Z (see FIG. 4). Then, in the joining process, a voltage is applied from the positive electrode 101 in a state where a pressing force F (see FIG. 3) is applied by the welding machine 100 along the facing direction Z. As a result, in the joining process, parts of the first joining surface 11 and the second joining surface 21 are melted by heat generated by resistance, thereby performing liquid phase joining. At this time, in the joining process, the tin plated on the copper plate 20 melts, and the oxide films on the surfaces of the copper plate 20 and the aluminum plate 10 melt, and the oxide films are diffused into the molten phase of tin, and an intermetallic compound C is generated between the first joining surface 11 and the second joining surface 21. In the joining process, as shown in Figs. 5 and 6, the protrusion 21a pushes the intermetallic compound C toward the discharge port 40 through the discharge path 50, and the intermetallic compound C discharged from the discharge port 40 escapes to the first escape space 60 and the second escape space 70. At this time, in the joining process, the first joining surface 11 of the aluminum plate 10 and the second joining surface 21 of the copper plate 20 are deformed in a direction away from each other at the discharge port 40 by the action of heat generated by resistance and the pressing force F. That is, the gap of the discharge port 40 becomes wider. Then, the discharge port 40 with the wider gap smoothly discharges the intermetallic compound C generated by the liquid phase bonding to the outside. At this time, in the joining process, the intermetallic compound C containing the aluminum plate 10 that has been preferentially melted is discharged to the outside, thereby suppressing the tin concentration in the liquid phase bonded portion 30 to 10% or less. In the joining process, the application of voltage from the positive electrode 101 is stopped to solidify the intermetallic compound C that has escaped to the first escape space portion 60 and the second escape space portion 70, and the first bonding surface 11 and the second bonding surface 21 are bonded to form the bonded structure 1. In this case, in the joining process, the application of voltage is stopped to cool the bonded structure 1, and therefore the aluminum plate 10 and the copper plate 20 contract at the discharge port 40, and as a result, the first bonding surface 11 of the aluminum plate 10 and the second bonding surface 21 of the copper plate 20 are deformed in a direction approaching each other.In other words, the gap of the exhaust port 40 becomes narrower.
[0025] As described above, the joint structure 1 according to the first embodiment includes the aluminum plate 10, the copper plate 20, the liquid phase bonding portion 30, the exhaust port 40, the first escape space portion 60, and the second escape space portion 70. The aluminum plate 10 has the first bonding surface 11. The copper plate 20 is a metal member having a higher melting point than the aluminum plate 10, and has a protruding portion 21a protruding from the second bonding surface 21 toward the first bonding surface 11. The liquid phase bonding portion 30 is a portion where the first bonding surface 11 and the second bonding surface 21 opposed to each other along the opposing direction Z are liquid phase bonded. The exhaust port 40 is formed by a gap between the first bonding surface 11 and the second bonding surface 21, and opens to the outside at the ends of the first bonding surface 11 and the second bonding surface 21 in the short side direction X and the long side direction Y, and is a portion where the intermetallic compound C generated by the liquid phase bonding can be discharged to the outside. The first escape space 60 is adjacent to the ends of the first joint surface 11 in the short side direction X and the long side direction Y, and is continuous with the discharge outlet 40. The second escape space 70 is adjacent to the ends of the second joint surface 21 in the short side direction X and the long side direction Y, and is continuous with the discharge outlet 40 and faces the first escape space 60 in the facing direction Z.
[0026] With this configuration, the joint structure 1 can push out the intermetallic compound C toward the discharge port 40 by the protrusion 21a, and the intermetallic compound C discharged from the discharge port 40 can escape to the first escape space 60 and the second escape space 70. As a result, the joint structure 1 can promote the discharge of the intermetallic compound C, and can discharge a large amount of the intermetallic compound C to the outside before the intermetallic compound C solidifies. As a result, the joint structure 1 can reduce the intermetallic compound C remaining between the first joint surface 11 and the second joint surface 21, and can reduce the area of the exposed end surface 31 of the intermetallic compound C exposed to the outside from between the first joint surface 11 of the aluminum plate 10 and the second joint surface 21 of the copper plate 20. Therefore, the joint structure 1 can reduce the intermetallic compound C, which is a hard and brittle material, and can suppress a decrease in the joint strength of the intermetallic compound C, and as a result, can properly join dissimilar metals (see FIG. 7).
[0027] In the above-mentioned joined structure 1, the aluminum plate 10 and the copper plate 20 are each formed in a plate shape. The first escape space 60 is adjacent to both ends in the short side direction X and one end in the long side direction Y of the main body of the aluminum plate 10. The second escape space 70 is adjacent to both ends in the short side direction X and one end in the long side direction Y of the main body of the copper plate 20. With this configuration, the joined structure 1 can properly discharge the intermetallic compound C to the outside of the aluminum plate 10 and the copper plate 20.
[0028] The bonding method according to the embodiment includes a bonding step of applying a voltage to the aluminum plate 10 and the copper plate 20 to perform liquid phase bonding while pressing the first bonding surface 11 of the aluminum plate 10 against the second bonding surface 21 of the copper plate 20. This makes it possible to form a bonded structure 1 in which the area of the exposed end surface 31 of the intermetallic compound C exposed to the outside is reduced, thereby making it possible to properly bond dissimilar metals.
[0029] [Modification of the first embodiment] Next, a modified example of the first embodiment will be described. In the modified example, the same reference numerals are used for components equivalent to those in the first embodiment, and detailed description thereof will be omitted. Although the example in which the exhaust outlet 40 is provided at three locations when joining the ends on one side of the long side direction Y of the aluminum plate 10 and the copper plate 20 has been described, the present invention is not limited thereto. For example, as shown in FIG. 9, when joining the centers of the aluminum plate 10 and the copper plate 20 in the long side direction Y, the exhaust outlet 40 is preferably provided at a position close to the electrode abutment portion 12, so that the exhaust outlet 40 is provided at two locations in total, one on each side of the short side direction X. In this way, the exhaust outlet 40 is appropriately provided according to the position of the electrode abutment portion 12.
[0030] Second Embodiment Next, a joint structure 1A according to a second embodiment will be described. The joint structure 1A according to the second embodiment differs from the joint structure 1 according to the first embodiment in that it has an opening 13 in which a first escape space portion 60A is provided. In the second embodiment, the same components as those in the first embodiment are given the same reference numerals, and detailed description thereof will be omitted. As shown in Figs. 10 and 11, the joint structure 1A includes an aluminum plate 10A, a copper plate 20, a liquid phase bonding portion 30, an exhaust port 40A, an exhaust path 50A, a first escape space portion 60A, and a second escape space portion 70A.
[0031] The aluminum plate 10A is formed in a plate shape and has a first bonding surface 11A, an opening 13, and an aluminum plate main body 14. The first bonding surface 11A is a surface that is liquid-phase bonded to a second bonding surface 21 of the copper plate 20, and is a surface of a partial region on the entire surface of the aluminum plate main body 14 on the copper plate 20 side.
[0032] The openings 13 are through holes drilled in the aluminum plate body 14 along the opposing direction Z, and are provided at two locations on the aluminum plate body 14 along the short side direction X, and have a first opening 13a and a second opening 13b.
[0033] The first opening 13a is provided at one end of the first joint surface 11A in the short side direction X, and is adjacent to the discharge outlet 40A. The first opening 13a has a sidewall 13g extending from the discharge outlet 40A along the facing direction Z to the side opposite the copper plate 20. The sidewall 13g is provided adjacent to a first escape space portion 60A.
[0034] The second opening 13b is provided on the other end side of the first joint surface 11A in the short side direction X, and is adjacent to the discharge outlet 40A. The second opening 13b has a sidewall 13h extending from the discharge outlet 40A along the facing direction Z to the side opposite the copper plate 20. The sidewall 13h is provided adjacent to the first escape space portion 60A.
[0035] The outlet 40A is formed by a gap between the first joint surface 11A and the second joint surface 21, and is a portion that opens to the outside on the end sides of the first joint surface 11A and the second joint surface 21 in the short side direction X.
[0036] The discharge path 50A is a portion that is formed by a gap between the first joint surface 11A and the second joint surface 21, and that communicates with the discharge port 40A.
[0037] The first escape space 60A of the opening 13 is a portion for allowing the intermetallic compounds C discharged from the discharge port 40A to escape to the outside. The first escape space 60A is provided in each of the first opening 13a and the second opening 13b, and allows the intermetallic compounds C discharged from the discharge port 40A to escape to the aluminum plate 10 side.
[0038] The second escape space 70A is a portion that allows the intermetallic compound C discharged from the discharge port 40A to escape to the outside. The second escape space 70A is adjacent to an end of the second joining surface 21 of the copper plate 20 in the short side direction X, and allows the intermetallic compound C discharged from the discharge port 40A to escape to the copper plate 20 side.
[0039] In this way, in the joining process of the aluminum plate 10A in which the first escape space portion 60A is provided in the opening 13, a voltage is applied to the aluminum plate 10A and the copper plate 20 while the first joining surface 11A of the aluminum plate 10A and the second joining surface 21 of the copper plate 20 are pressed against each other to perform liquid phase joining. For example, in the joining process, the aluminum plate 10A and the copper plate 20 are set between the positive electrode 101 and the negative electrode 102A of the welding machine 100 in a state in which the first joining surface 11A of the aluminum plate 10A and the second joining surface 21 of the copper plate 20 face each other along the facing direction Z (see FIG. 12). Then, in the joining process, a voltage is applied from the positive electrode 101 while a pressing force F is applied by the welding machine 100 along the facing direction Z. As a result, in the joining process, the first joining surface 11A and the second joining surface 21 are partially melted by heat generated by resistance to perform liquid phase joining. At this time, in the joining process, an intermetallic compound C is generated between the first joining surface 11A and the second joining surface 21. In the joining process, as shown in Fig. 13 and Fig. 14, the protrusion 21a pushes out the intermetallic compound C toward the discharge port 40A through the discharge path 50A, and the intermetallic compound C discharged from the discharge port 40A escapes to the first escape space 60A and the second escape space 70A. In the joining process, the application of the voltage from the positive electrode 101 is stopped to solidify the intermetallic compound C that has escaped to the first escape space 60A and the second escape space 70A, and the first joining surface 11A and the second joining surface 21 are joined to form the joined structure 1A.
[0040] As described above, in the joined structure 1A according to the second embodiment, the aluminum plate 10A is formed in a plate shape and has the opening 13 adjacent to the discharge port 40A and in which the first escape space 60A is provided. With this configuration, the joined structure 1A can allow the intermetallic compound C to escape to the first escape space 60A provided in the opening 13 when joining is performed near the center of the aluminum plate main body 14.
[0041] In the above description, the opening 13 is described as a through hole drilled in the aluminum plate body 14 along the opposing direction Z, but is not limited to this and may be, for example, a groove shape having a bottom formed and a certain depth.
[0042] Although the aluminum plate 10 has the opening 13 in which the first escape space 60A is provided, the present invention is not limited to this. For example, not only the aluminum plate 10 but also the copper plate 20 may have the opening 13 in which the second escape space 70A is provided depending on the shape of the copper plate 20.
[0043] Although the first metal member is made of aluminum in the above example, the present invention is not limited to this, and may be made of other metals as long as they have a lower melting point than the second metal member.
[0044] Although the second metal member is made of copper in the above example, the second metal member is not limited to copper, and may be made of other metals as long as the metal has a higher melting point than the first metal member.
[0045] Although the electrode contact portion 12 is formed in a circular shape in the above example, the present invention is not limited to this, and may be formed in other shapes such as a polygon. [Explanation of symbols]
[0046] 1, 1A bonded structure 10, 10A Aluminum plate (first metal member) 11, 11A 1st joint surface 20 Copper plate (second metal member) 21 Second joint surface 21a Projection 30 Liquid phase junction 40, 40A outlet 60, 60A First relief space 70, 70A Second relief space 13 Opening (first opening) X Short side direction (cross direction) Y Long side direction (cross direction) Z Opposite Direction
Claims
1. a first metal member having a first bonding surface; a second metal member having a melting point higher than that of the first metal member, the second metal member having a second bonding surface and a protruding portion protruding from the second bonding surface toward the first bonding surface; a liquid phase bonded portion formed by liquid phase bonding the first bonding surface and the second bonding surface opposed to each other along an opposing direction; a discharge port formed by a gap between the first bonding surface and the second bonding surface, the discharge port opening to the outside at an end side of the first bonding surface and the second bonding surface in a cross direction crossing the facing direction and capable of discharging to the outside an intermetallic compound generated by the liquid phase bonding; a first escape space portion adjacent to an end of the first joint surface in the cross direction and continuous with the exhaust port; a second escape space portion adjacent to an end of the second joint surface in the cross direction, continuous with the discharge port, and opposing the first escape space portion in the opposing direction, the first metal member has a first opening and a second opening that are spaced apart from each other and extend through the first metal member in a thickness direction, and the first joining surface for joining the second metal member is provided between the first opening and the second opening; The first opening is adjacent to one of the exhaust ports and has one of the first relief spaces inwardly, the one of the first relief spaces being continuous with the one of the exhaust ports; A joint structure, characterized in that the second opening is adjacent to the other of the exhaust outlets and has the other of the first escape space portions therein that are continuous with the other of the exhaust outlets.
2. The first metal member and the second metal member are each formed into a plate shape, The first escape space is adjacent to an end of the first metal member in the cross direction, The joint structure according to claim 1 , wherein the second escape space is adjacent to an end of the second metal member in the cross direction.
Citation Information
Patent Citations
Pressure welding method of base metal by using eutectic reaction
JP1981062685A
Method for joining different metals by resistance welding, and joined structure
JP2007105737A
Method for joining different metals by resistance welding and joining structure of metals
JP2007130686A
Weld joined body
JP2019126824A