Connector Unit
The conductive particle arrangement film, embedded in an elastomer film with matching thickness and arranged in the plane direction, addresses the challenges of irregular semiconductor device test areas by ensuring stable insulation and ease of handling, achieving high-precision continuity testing with low resistance values.
Patent Information
- Application Number
- JP2022205255
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2016-11-30
- Filing Date
- 2022-12-22
- Publication Date
- 2024-10-09
- Estimated Expiration
- 2037-11-20
AI Technical Summary
Conventional test probe units struggle to accurately follow the irregularities of semiconductor device test areas, leading to poor continuity test results and appearance defects due to the curvature of conductive particles under magnetic fields, necessitating a sacrifice in fine-pitch formation and handling ease.
A conductive particle arrangement film is embedded in an elastomer film with thickness matching the average particle diameter, arranged in the plane direction, ensuring stable insulation and easy handling, allowing for accurate continuity testing on uneven or non-fine pitch targets.
The film enables high-precision continuity testing with low resistance values, avoiding appearance defects and accommodating various specifications by maintaining stable insulation and ease of use, even on fine-pitch and smooth test areas.
Smart Images

Figure 0007564462000001 
Figure 0007564462000002 
Figure 0007564462000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a conductive particle arranged film that is useful as an inspection probe material for an inspection probe unit used in continuity testing of semiconductor devices and the like, an anisotropic conductive connector, or an anisotropic conductive adapter. [Background technology]
[0002] When conducting a continuity test of a semiconductor device, a test probe unit is generally used in which a probe material having a plurality of fine rod-shaped electrodes arranged in a planar direction is connected to a test circuit board. However, since the test target area is not necessarily smooth and has irregularities, there is a concern that a conventional simple test probe unit cannot follow the irregularities of the test target area, and a highly accurate continuity test result cannot be obtained. In addition, there is a concern that the appearance of the test area may be deteriorated because the probe material is directly pressed against the terminal of the semiconductor device. For this reason, in order to prevent a decrease in test accuracy due to the irregularities of the test target area during a continuity test and to prevent the appearance of the semiconductor device from being deteriorated, it is considered to arrange an anisotropic conductive elastomer sheet (Patent Document 1) in which conductive particles are arranged in a planar direction and are continuous in the thickness direction by a parallel magnetic field, as an anisotropic conductive connector, between the probe material in the test probe unit and the test circuit board (Patent Document 2). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Japanese Patent Application Publication No. 10-188672 [Patent Document 2] JP 2009-98065 A Summary of the Invention [Problem to be solved by the invention]
[0004] However, in the anisotropically conductive elastomer sheet of Patent Document 1, there is a possibility that the conductive particle groups that are continuous in the thickness direction may be curved due to the influence of a magnetic field, and in order to stably ensure the insulation between the conductive particle groups that are separated in the planar direction, there is a problem that the fine pitch in the planar direction of the anisotropically conductive elastomer sheet must be sacrificed. In addition, since there are various specifications for performing inspections with such sheets, there is a demand for sheets that are easier to handle.
[0005] The object of the present invention is to obtain highly accurate continuity test results and avoid the occurrence of visual defects when a continuity test of a fine-pitch continuity test target such as a semiconductor device is performed using an inspection probe unit, even if the test target area is not smooth but uneven, and to provide a continuity test member that is easy to use and has excellent handleability even if the test target area is smooth and the continuity test target is not fine-pitch. [Means for solving the problem]
[0006] The inventors have discovered that the above-mentioned problems can be solved by using a conductive particle-disposed film, in which conductive particles are embedded in the middle of the depth direction of an elastomer film of a thickness approximately the same as the average particle diameter and disposed in the planar direction, as an inspection probe material, an anisotropic conductive connector, or an anisotropic conductive adapter, instead of the anisotropic conductive elastomer sheet of Patent Document 1, and have thus completed the present invention.
[0007] That is, the present invention provides a particle-disposed film in which conductive particles are disposed in a planar direction of an elastomer film, The thickness of the elastomer film is approximately equal to the average particle size of the conductive particles, A conductive particle-disposed film is provided in which ends of the conductive particles are located near the outermost surface of each of the two faces of the elastomer film.
[0008] The present invention also provides a method for producing the aforementioned conductive particle-disposed film, comprising the steps of: The method includes arranging conductive particles in the recesses of a transfer mold having a plurality of recesses formed in a planar direction, pressing an elastomer film against the recess-formed surface of the transfer mold to transfer the conductive particles, and sandwiching the elastomer film to which the conductive particles have been transferred between a pair of platens, and applying heat and pressure to press the conductive particles into the elastomer film.
[0009] Furthermore, the present invention provides an inspection probe unit in which the above-mentioned conductive particle arranged film is installed as an inspection probe material on an electronic circuit board for continuity inspection.
[0010] In addition, the present invention provides an inspection probe unit having an electronic circuit board for continuity inspection and a probe material having an electrode structure electrically connected thereto, The present invention provides an inspection probe unit in which the above-mentioned conductive particle-disposed film is disposed as an anisotropic conductive connector between an electronic circuit board for continuity inspection and a probe material.
[0011] Furthermore, the present invention provides an inspection probe unit having an electronic circuit board for continuity inspection and a probe material having an electrode structure electrically connected thereto, An inspection probe unit is provided in which the above-mentioned conductive particle-disposed film is disposed as an anisotropic conductive adapter on the tip of the probe material on the side opposite to the electronic circuit board for continuity inspection.
[0012] The present invention also provides an inspection probe unit having an electronic circuit board for continuity testing and a probe material having an electrode structure electrically connected thereto, An inspection probe unit is provided in which the above-mentioned conductive particle arrangement film is arranged as an anisotropic conductive adapter on the tip of the probe material opposite the electronic circuit board for continuity inspection and on the tip of the probe material opposite the electronic circuit board for continuity inspection.
[0013] The present invention also provides a continuity inspection method in which the above-mentioned inspection probe unit is applied to an object to be inspected for continuity. Effect of the Invention
[0014] In the conductive particle-disposed film of the present invention, the conductive particles are embedded in the middle of the depth direction of an elastomer film having a thickness substantially equal to the average particle diameter and are disposed in the surface direction. Therefore, it is not essential to connect the conductive particles in the film thickness direction, so that a continuity test of a fine pitch continuity test target such as a semiconductor device (for example, a rectangular terminal having a width of 2 to 15 μm or a terminal having a distance between terminals of 3 to 25 μm) is possible. In addition, in order to improve the accuracy of the continuity test, when a continuity test is performed at a low resistance value of, for example, less than 1000 mΩ, a plurality of conductive particles can be brought into contact with the terminals, so that even if the distance between the terminals of the continuity test target becomes wider than the above-mentioned range, a continuity test can be performed with low resistance and high accuracy. Moreover, since the continuity test target is pressed against the continuity test target in a substantially flat surface, it is possible to avoid the occurrence of visual defects in the continuity test target. It is also possible to perform a high-accuracy continuity test of a continuity test target having a smooth test target area or a continuity test target having a non-fine pitch. In other words, the appropriateness of the continuity of the continuity test target can be easily and non-destructively determined.
[0015] Furthermore, an inspection probe unit equipped with the conductive particle arrangement film of the present invention can achieve the effects of the invention derived from the conductive particle arrangement film of the present invention, and if the conductive particle arrangement film is compatible with fine pitches, it can be used for continuity inspection targets with wide pitches without changing the design of the conductive particle arrangement film. [Brief description of the drawings]
[0016] [Figure 1] FIG. 1 is a cross-sectional view of a conductive particle-disposed film of the present invention. [Diagram 2] FIG. 2 is a cross-sectional view of the conductive particle arranged film of the present invention. [Figure 3A] FIG. 3A is an explanatory diagram of the positional relationship between the outermost surface of the elastomer film and the conductive particles. [Figure 3B] FIG. 3B is an explanatory diagram of the positional relationship between the outermost surface of the elastomer film and the conductive particles. [Figure 3C] FIG. 3C is an explanatory diagram of the positional relationship between the outermost surface of the elastomer film and the conductive particles. [Figure 4A] FIG. 4A is a cross-sectional view of a laminate-type conductive particle-disposed film of the present invention. [Figure 4B] FIG. 4B is a cross-sectional view of a laminate-type conductive particle-disposed film of the present invention. [Figure 5A] FIG. 5A is a cross-sectional view of a laminate-type conductive particle-arranged film of the present invention that uses a flexible connector sheet. [Figure 5B] FIG. 5B is a cross-sectional view of a laminate-type conductive particle-arranged film of the present invention that uses a flexible connector sheet. [Figure 5C] FIG. 5C is a top view of the conductive particle distribution film of FIG. 5B. [Figure 5D] FIG. 5D is a cross-sectional view of a laminate-type conductive particle-arranged film of the present invention that uses a flexible connector sheet. [Figure 6A] FIG. 6A is a schematic cross-sectional view of an inspection probe unit that uses the conductive particle arranged film of the present invention as an inspection probe. [Figure 6B] FIG. 6B is a schematic cross-sectional view of an inspection probe unit that utilizes the conductive particle arranged film of the present invention as an anisotropic conductive connector. [Figure 6C] FIG. 6C is a schematic cross-sectional view of an inspection probe unit that utilizes the conductive particle arranged film of the present invention as an anisotropic conductive adapter. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] An example of the conductive particle-disposed film of the present invention will now be described in detail with reference to the drawings, in which the same reference numerals denote the same or equivalent components.
[0018] <Overall structure of conductive particle-arranged film> FIG. 1 is a cross-sectional view of a conductive particle-arranged film 10 of the present invention. In this conductive particle-arranged film 10, conductive particles 1 are arranged in the planar direction of an elastomer film 2. Here, "arranged in the planar direction" means that, when the conductive particle-arranged film 10 is viewed in plan, the conductive particles 1 are arranged at a distance from one another (preferably arranged in a regular pattern (e.g., a square lattice pattern, a rectangular lattice pattern, a diagonal lattice pattern, a hexagonal lattice pattern)). In this case, as shown in FIG. 2, a plurality of conductive particles 1 may be gathered or connected in a planar manner to form one unit and spaced apart from one another. For example, the minimum distance of separation (the shortest distance between conductive particles) is preferably 0.5 times or more the conductive particle diameter, and more preferably 0.7 times or more, in order to avoid unnecessary contact between conductive particles. There is no particular upper limit, and it can be set appropriately depending on the object, but as an example for fine pitch, it is preferably 10 times or less the conductive particle diameter, more preferably 5 times or less, and even more preferably 2 times or less. Here, the conductive particles 1 being arranged apart from one another means that preferably 95% or more, more preferably 98% or more, and even more preferably 99.5% or more of the total number of conductive particles within a rectangular or square area in which the number of conductive particles is 1000 or more, preferably 2000 or more, are independent. When conductive particles are intentionally connected, the connected particles are counted as one conductive particle (conductive particle diameter refers to the size of each individual conductive particle).
[0019] In addition, the distance between the conductive particles does not necessarily have to be equal to the distance between the terminals of the continuity test object, and it is preferable that the distance between the conductive particles is smaller than the distance between the terminals of the continuity test object. This is because the conductive resistance value can be reduced by contacting a plurality of conductive particles with the terminal of the continuity test object. Therefore, the number of conductive particles contacting the terminal may be one, but three or more are preferable, and eleven or more are more preferable.
[0020] In conductive particle arrangement film 10 of the present invention, as shown in Figure 1, the thickness t of elastomer film 2 is approximately equal to the average particle diameter d of conductive particles 1. The reason for making it "approximately equal" is to enable electrical continuity on both sides of the conductive particle arrangement film and to enable it to be pressed against an object to be tested for electrical continuity on a substantially flat surface. Usually, there is a relationship of 0.70d≦t≦1.10d.
[0021] Regarding the positional relationship between the elastomer film 2 and the conductive particles 1, in the present invention, it is necessary that the ends of the conductive particles 1 are located near the outermost surface of each of both sides of the elastomer film 2. This "nearby" state is shown in Figs. 3A to 3C, which are partial views of one surface of the elastomer film 2. That is, Fig. 3A shows a state in which the ends of the conductive particles 1 are in contact with the surface of the elastomer film 2. Fig. 3B shows a state in which the ends of the conductive particles 1 are embedded in the elastomer film 2 from the surface. The embedded depth (elastomer coating thickness) a is usually within 10% of the thickness from one side of the surface of the elastomer film 2, preferably within 5%. Fig. 3C shows a state in which the ends of the conductive particles 1 are exposed from the surface of the elastomer film 2. The exposed height b is preferably within 30% of the thickness from one side of the surface of the elastomer film 2. Therefore, six types of "vicinity" patterns are envisioned on both sides of elastomer film 2: both sides in the form of Figure 3A, Figure 3B, or Figure 3C, one side in the form of Figure 3A and the other side in Figure 3B, one side in the form of Figure 3A and the other side in Figure 3C, and one side in the form of Figure 3B and the other side in Figure 3C. In addition, the degree of exposure of the conductive particles from the elastomer film and the degree of coverage by the elastomer may be the same or different on one side and the other side of the conductive particle-arranged film.
[0022] (Elastomer film 2) The thickness t of the elastomer film 2 is determined mainly according to the surface irregularities of the object of the continuity test and the handleability of the conductive particle-arranged film, but as described below, it can be appropriately adjusted according to the lamination mode of the conductive particle-arranged film. When applied to a semiconductor device, taking into consideration the bump height and its variation, it is preferably 3 μm or more, more preferably 10 μm or more, and particularly preferably 30 μm or more. The upper limit of the thickness is not particularly limited, but taking into consideration the handleability of the conductive particle-arranged film and fine pitch compatibility, it is usually 200 μm or less, preferably 100 μm or less, and more preferably 50 μm or less. The thickness t of the elastomer film 2 can be measured using a known film thickness meter (for example, Fujiwork Co., Ltd., Film Tester Thickness Measuring Instrument, HKT Handy Series).
[0023] Examples of the elastomer film 2 described above include elastomer films such as polybutadiene, natural rubber, polyisoprene, conjugated diene rubber such as SBR and NBR and their hydrogenated products, block copolymers such as styrene butadiene diene block copolymer and styrene isoprene block copolymer and their hydrogenated products, chloroprene, urethane rubber, polyester rubber, epichlorohydrin rubber, silicone rubber, ethylene propylene copolymer, ethylene propylene diene copolymer, silicone rubber, and the like. When weather resistance is required for the elastomer film 2, elastomer films other than conjugated diene rubber are preferred, and silicone rubber films are particularly preferred from the viewpoints of moldability and electrical properties. In addition, the elastomer film 2 may contain a resin used in an anisotropic conductive connection material such as a thermosetting anisotropic conductive film, a thermosetting connection material for electronic components that does not contain conductive particles, a pressure sensitive adhesive composition or adhesive composition for electronic components, or a resin composition for underfill. In addition, the same or different films may be laminated to form a laminated type elastomer film 2. From the viewpoint of convenience, it is desirable for this elastomer film 2 to have a property that it can be detached from the object of continuity inspection during inspection. This can be one of the major differences from known curable adhesive films for electronic components (for example, thermosetting anisotropic conductive films).
[0024] In addition, when a heat-cured elastomer film 2 is used, the laminated type has the effect of expanding the options for manufacturing conditions. Furthermore, it is possible to fine-tune the inspection conditions by laminating various films before the inspection process, or to make the inspection process itself a black box. In addition, when the elastomer film 2 does not contain a heat-cured film and has a composition similar to that of a slightly adhesive adhesive film, the options for handling in the inspection process are expanded, such as by replacing the film for each continuity inspection target. In the case of the laminated type, the required characteristics can be adjusted by combining them in this way.
[0025] (Conductive Particles 1) On the other hand, the average particle diameter of the conductive particles 1 is approximately the same as that of the elastomer film, and is usually 200 μm or less, preferably 2 μm to 50 μm, more preferably 2.5 μm to 30 μm, and particularly preferably 2.8 μm to 20 μm. In addition, in order to improve the accuracy of the continuity test, it is desirable that the conductive particle diameter is uniform. Specifically, the CV value (conductive particle diameter standard deviation / conductive particle average particle diameter) is preferably 20% or less, more preferably 10% or less, and even more preferably 5% or less. There is no particular restriction on the lower limit of the CV value, since the smaller the CV value, the more uniform the particle diameter becomes, which is preferable.
[0026] Examples of the conductive particles 1 include magnetic metal particles such as nickel, iron, and cobalt, or alloy particles thereof, and nonmagnetic solder particles. These particles may contain precious metals such as gold, silver, palladium, and rhodium, preferably gold or silver. These metal particles or alloy particles may be used as the core, and the surface of the core may be coated with a precious metal by electrolytic plating, electroless plating, sputtering, vacuum deposition, or the like. Alternatively, nonmagnetic metal particles or inorganic particles such as glass beads or organic polymer particles may be used as the core, and these may be coated with a conductive magnetic material such as nickel or cobalt, and further coated with a precious metal. The conductive particles 1 may be made of metal-coated resin particles in which organic polymer particles are used as the core and coated with a metal or the like. In the case where metal-coated resin particles are used in which the conductive particles are coated with a metal or the like, it is preferable in that the conductive state is easily adjusted due to deformation of the conductive particles when pressure is applied and repulsion of the organic polymer particles. In addition, conductive fine particles-containing metal-coated resin particles in which conductive fine particles are contained in organic polymer particles and further coated with a metal or the like may be used. The effect of lowering the conductive resistance value can be expected. In the present invention, two or more kinds of the conductive particles 1 described above may be used in combination.
[0027] (Lamination of conductive particle-arranged films) In order to increase the overall thickness of conductive particle-arranged film 10 of the present invention, a plurality of identical conductive particle-arranged films 10 can be laminated (FIG. 4A). Furthermore, when laminating, a plurality of different conductive particle-arranged films 10, 11 can also be laminated (FIG. 4B). In the latter case, conductive particles with relatively different particle sizes are used in conductive particle-arranged film 10 and conductive particle-arranged film 11, which is preferable as it makes it easier to maintain the connection of the conductive particles in the thickness direction of the conductive particle-arranged film.
[0028] In addition, when stacking conductive particle-arranged films 10, conductive particle-arranged films 10 and a flexible connector sheet having a through electrode provided on an insulating flexible sheet may be stacked to form a unit, and as shown in FIG. 5A, a flexible connector sheet 32 having a through electrode 31 provided on an insulating flexible sheet 30 may be sandwiched between two conductive particle-arranged films 10 (see Japanese Patent No. 3951333). In this case, as shown in FIG. 5B, in conductive particle-arranged film 10, one or two conductive particles may be arranged corresponding to through electrode 31, but it is preferable to arrange more than one conductive particle 1 (preferably three or more, more preferably ten or more). A plurality of conductive particles 1 arranged corresponding to one through electrode 31 may be connected to each other, but as shown in FIG. 5C, a plurality of conductive particles 1 (upper) corresponding to one through electrode 31 may be arranged independently and separately from each other without being connected to each other when viewed in a plane. At this time, it is preferable that the conductive particles 1 (lower) of the conductive particle-arranged film arranged under the flexible connector sheet do not overlap with the conductive particles 1 (upper) of the conductive particle-arranged film arranged on the flexible connector sheet. The conductive particle arrangement state as shown in FIG. 5C can be created, for example, by changing the distance between the conductive particles or the number of conductive particles, by making the arrangement pattern itself different, or by changing the angle with respect to the reference line even if the arrangement pattern is the same. For example, one side of the conductive particle-arranged film or one side of the terminal can be used as the reference line. This makes it possible to prevent bias in the pressing force during the continuity test. Furthermore, as shown in FIG. 5D, the conductive particles 1 may be present in an area S of the conductive particle-arranged film 10 that does not face the through electrode 31.
[0029] The insulating flexible sheet may be, for example, an FPC using a known polyimide, or may be a material used as a buffer material such as a silicone rubber sheet with through holes and electrodes provided therein. The thickness of these sheets may be set appropriately in accordance with the purpose of the inspection, similar to that of the conductive particle-arranged film 10. There is no particular limit to the number of sheets to be stacked, and it may be set appropriately in accordance with the purpose of stacking. The total thickness, including the insulating flexible sheet, is the same as the total thickness of the laminate-type conductive particle-arranged film 10 described below.
[0030] The film thickness t and the average particle diameter d of the conductive particles in the conductive particle-arranged film arranged inside the laminated type conductive particle-arranged film do not have to satisfy the relationship of 0.70d≦t≦1.10d. As described above, when a through electrode is provided in an insulating flexible sheet, if this through electrode protrudes from the surface of the insulating flexible sheet, the conductive particles present in the conductive particle-arranged film on the inside of the laminate are pressed by the protruding through electrode. In addition, a case where an elastomer film 2 (a conductive particle-arranged film without conductive particles) is laminated on at least one side of the conductive particle-arranged film is also assumed. If the through electrode protrudes from the surface of the insulating flexible sheet, a resin is required to fill the space around the protruding through electrode. The laminate may be a laminate of a conductive particle-arranged film in which conductive particles with a relatively small particle diameter are densely spread and a conductive particle-arranged film made of conductive particles with a relatively large particle diameter (for example, 10 to 50 μm, preferably 10 to 30 μm). A conductive particle-arranged film in which conductive particles of relatively small particle diameters (for example, 2 to 9 μm) are densely packed can have conductive particles of 2 to 9 μm arranged in a hexagonal lattice or a similar arrangement (such as a lattice slightly distorted or stretched from a hexagonal lattice, a square lattice, or a lattice with a conductive particle at the center point of a square lattice). Conductive particles of relatively large particle diameters can be arranged via conductive particles of small particle diameters to form a desired conductive path. Since there is a risk that contact between particles will be insufficient with only large particle diameters, it is preferable that the small particle diameter plays a supporting role. It is preferable that the large particle diameter is at least twice, preferably at least 2.5 times, and more preferably at least 3 times larger than the small particle diameter. The arrangement of small particle diameters and large particle diameters is preferably the same so that they have similarity in order to facilitate the design of the conductive path. In addition, it is preferable that the arrangements are different in order to avoid the formation of irregular conductive paths in the film surface direction.
[0031] In addition, when a plurality of conductive particles are arranged corresponding to the through electrodes 31, the diameter of the conductive particles is relatively smaller than when one conductive particle is arranged, and the thickness of one laminated conductive particle-arranged film 10 is accordingly thinner. Therefore, by laminating two or more sets, preferably four or more sets, of units each consisting of the conductive particle-arranged film 10 and the flexible connector sheet 32, the overall thickness can be easily increased to, for example, 30 μm or more, making it easier to adapt to the inspection of various continuity inspection objects including semiconductor devices. In a typical semiconductor package, the height of the solder electrode is about 100 μm, so it is desirable to make the thickness about 400 μm in consideration of this (in this case, a laminated type is preferable due to the relationship between the thickness and the size of the conductive particles). In addition, in recent years, when the terminal of the semiconductor device contains Au, there is a high demand for a low height in order to reduce material costs. For example, it is 8 μm or less, preferably 6 μm or less, and more preferably 3 μm or less. In such cases or when inspecting before the terminal is provided (an example of a continuity inspection object in a substantially smooth state), the conductive particle-arranged film 10 may be 30 μm or less.
[0032] When considering practical application to continuity testing, the total thickness of the laminated type conductive particle arrangement film 10 (if an insulating flexible sheet is present as described above, this will be the total thickness including this) is set according to the bump height of the continuity test target such as a semiconductor device, semiconductor package, or wiring board with electrodes, and is preferably 20 μm or more, more preferably 30 μm or more, and even more preferably 50 μm or more in the lower limit direction, and is preferably 400 μm or less, more preferably 200 μm or less, and even more preferably 150 μm or less in the upper limit direction. Note that when the electrodes formed in a circuit on the board to be tested for continuity are protected by a passivation film about several μm thick, a total thickness thinner than the above range may be applicable.
[0033] In the case of a laminated type conductive particle-disposed film, the conductive particles in the outermost elastomer film may be arranged on one surface in a hexagonal lattice pattern or a distorted lattice pattern. This is because the number density of the conductive particles can be increased. In order to make the pattern shape easier to recognize, the conductive particles may be arranged on one surface in a square lattice, rectangular lattice, or a distorted lattice pattern. Also, a regular arrangement may be provided in correspondence with the terminal arrangement. For example, since terminals are generally rectangular or circular, the appropriateness of continuity during testing can be determined by arranging the conductive particles in a manner similar to the external shapes of these terminals.
[0034] Regardless of whether the film is a laminated type or not, two or more types of conductive particle-arranged films having different conduction paths for the terminals of the continuity test target can be prepared and each of them can be applied to the continuity test of the same semiconductor device or other continuity test target, thereby enabling precise judgment of the conduction failure of the terminals of the continuity test target. Here, different conduction paths means that the conductive particles, through-hole electrodes, and other conductive members are different in the cross-sectional view of the film in the path from the conductive particles that contact the terminals of the continuity test target to the receiving unit (such as the conductive unit of the test probe unit described later) that detects the conduction. Two or more types of conductive particle-arranged films having different conduction paths can be obtained by designing the arrangement of conductive particles for each conductive particle-arranged film according to the terminal shape and terminal arrangement state of the continuity test target of the semiconductor device or other continuity test target. Alternatively, a continuity test can be realized with a conductive particle-arranged film having two substantially different conduction paths by contacting one type of conductive particle-arranged film with the continuity test target of the semiconductor device or other continuity test target at a different angle in the planar direction (for example, by changing the angle and pasting the conductive particle-arranged film). By collating the inspection results thus obtained, fine pitch can be accommodated and the range that can be inspected can be expanded using one or a minimum number of substrates.
[0035] The conductive particle-arranged film 10 of the present invention may further have an adhesive layer formed on at least one side thereof. By providing an adhesive layer, the conductive particle-arranged film 10 can be attached to and detached from the continuity test target, etc. In addition, since such an adhesive layer is a component separate from the elastomer film, the adhesive layer covers the ends of the conductive particles and functions as a protective material for the conductive particles. Therefore, by providing such an adhesive layer, it becomes possible to stably perform a continuity test using the conductive particle-arranged film 10 multiple times. In addition, when an adhesive layer is provided, it may be provided on only one side of the conductive particle-arranged film 10, or on both sides. For example, if the conductive particles are metal-coated resin particles described later, they may not be able to withstand multiple uses depending on the test conditions. For this reason, it is desirable that the conductive particle-arranged film 10 is detachable, and it may be preferable to provide a weak adhesive layer. This thickness can be made thicker than the height at which the conductive particles are exposed from the elastomer film, since a slightly adhesive layer may be provided to protect the conductive particles; specifically, it can be made 25 μm or less, which is 10% of the conductive particle diameter of 200 μm plus a margin; in order to obtain sufficient adhesion, a thickness of 1 μm or more is preferable, and a thickness of 2 μm or more is more preferable.
[0036] The area of conductive particle-arranged film 10 can be determined according to the purpose of the inspection, and can be selected from the following combinations. As an example, the lower limit of one side is preferably 0.5 mm or more, more preferably 0.8 mm or more, and even more preferably 2 mm or more. This is based on the film width of a typical anisotropic conductive film connection body (i.e., the length of the short side of a driver IC or the width of a tool that is actually pressed on an electrode of an FPC). The larger the upper limit of one side, the more preferable, but taking into account practical handling, as an example, it is preferably 600 mm or less, more preferably 450 mm or less, and even more preferably 300 mm or less. In addition, as the product form of conductive particle-arranged film 10, a roll is preferable, especially considering transportability. In addition, a sheet is preferable, especially considering workability.
[0037] <Method of manufacturing conductive particle-arranged film> The conductive particle-disposed film of the present invention described above can be manufactured in the same manner as in the conventional manufacturing method of anisotropic conductive films in which conductive particles are regularly arranged. For example, the conductive particles can be disposed in the recesses of a transfer mold in which a plurality of recesses are formed in a planar direction, an elastomer film is pressed against the recess-formed surface of the transfer mold to transfer the conductive particles, and the elastomer film to which the conductive particles have been transferred is sandwiched between a pair of platens and heated and pressurized to press the conductive particles into the elastomer film (see, for example, Japanese Patent No. 6187665).
[0038] <Inspection probe unit> The conductive particle-disposed film of the present invention can be preferably used as an inspection probe material for an inspection probe unit, as an anisotropic conductive connector, or as an anisotropic conductive adapter.
[0039] One example of the inspection probe unit of the present invention is inspection probe unit 100, in which conductive particle arranged film 10 of the present invention (see FIG. 1) is installed as an inspection probe material on electronic circuit board 50 for continuity testing, as shown in FIG. 6A. In this case, the conductive particle arranged films of FIGS. 2, 4A, 4B, and 5A-5D can be diverted in place of conductive particle arranged film 10. Note that a conventionally known electronic circuit board for continuity testing can be used as electronic circuit board 50 for continuity testing.
[0040] Another example of the inspection probe unit of the present invention is an inspection probe unit 200 having an electronic circuit board 50 for continuity testing and a probe material 60 having an electrode structure 61 that is electrically connected thereto, as shown in Fig. 6B, in which the conductive particle-arranged film 10 of the present invention is disposed as an anisotropic conductive connector between the electronic circuit board 50 for continuity testing and the probe material 60. In this case, the electrode structure 61 and the probe material 60 may be conventionally known.
[0041] 6C , there is an inspection probe unit 300 having an electronic circuit board 50 for continuity testing and a probe material 60 equipped with an electrode structure 61 that is in electrical conduction with the electronic circuit board 50, in which the conductive particle arrangement film 10 of the present invention is arranged as an anisotropic conductive adapter on the tip of the probe material 60 opposite the electronic circuit board 50 for continuity testing. In this case, the conductive particle arrangement film 10 of the present invention may be additionally arranged between the electronic circuit board 50 for continuity testing and the probe material 60.
[0042] In addition, although the specifications of the inspection probe unit described above may need to be changed each time depending on the bump layout, if the conductive particle arrangement film used as the probe material is compatible with fine pitch, it can be applied to wider pitches without changing the design of the conductive particle arrangement film, making it economical.
[0043] <Continuity test method> The inspection probe unit of the present invention can be preferably applied to the continuity test of various electronic components such as semiconductor devices. Specifically, the continuity test can be realized by pressing the probe material of the inspection probe unit against the electrode of the electronic component to be tested for continuity, and measuring the electrical resistance between the electrode of the electronic component and the electronic circuit board for continuity test constituting the inspection probe unit by a known method via a conductive particle arrangement film.
[0044] In such a continuity test, in order to realize a highly accurate test, it is preferable that the resistance value of each terminal to be measured is as low as possible. As an example, if it is less than 1000 mΩ, there is no practical problem, if it is 200 mΩ or less, it is preferable, if it is 100 mΩ or less, it is more preferable, if it is 50 mΩ or less, it is even more preferable. This can be appropriately selected depending on the object to be tested and the conditions of the test. In this case, the continuity resistance value preferably refers to a state in which a sufficient pressure is applied to the object to be tested and a stable resistance value is shown.
[0045] The temperature conditions for the continuity test include room temperature conditions (20°C±15°C), low temperature conditions (e.g., -40°C), and high temperature conditions (e.g., 100°C).Furthermore, heat cycle temperature conditions (-40°C / 100°C / 1000 cycles) are also included.
[0046] The terminal pitch (minimum terminal length + space between terminals) of a continuity test target such as a semiconductor device is generally about 200 μm, but the test probe unit of the present invention can accommodate a narrower terminal pitch. This is because conductive particles with a particle diameter of, for example, about 2.5 μm to 30 μm can be arranged on the outermost surface of the test probe unit. Specifically, if only one conductive particle is required to act as a probe, a test terminal of about 10×10 μm can be obtained by arranging conductive particles with a particle diameter of 3 μm in a hexagonal lattice shape with a center-to-center distance of 6 μm. Therefore, the terminal pitch of the continuity test target depends on the size of the electrodes in contact with the conductive particles, but if the length of the electrodes is set to about 10 μm at the minimum and the distance between the electrodes is set to about 10 μm at the minimum, the terminal pitch can be set to about 20 μm.
[0047] In addition, since the conductive resistance value measured in the continuity test is considered to depend on the material and size of the conductive particles, and further on the number of conductive particles in contact with the electrode, it may be required to make the terminal pitch larger depending on the conductive resistance value to be measured. Therefore, the terminal pitch applicable to the continuity test is preferably 20 μm or more, more preferably 30 μm or more, and even more preferably 50 μm or more in the lower limit direction, and is preferably 400 μm or less, more preferably 200 μm or less, and even more preferably 150 μm or less in the upper limit direction. [Industrial Applicability]
[0048] In the conductive particle-disposed film of the present invention, the conductive particles are embedded in the middle of the depth direction of an elastomer film having a thickness approximately equal to the average particle diameter of the conductive particles and are disposed in the planar direction. Therefore, the conductive particle-disposed film of the present invention is useful for high-precision continuity testing of fine-pitch continuity test objects such as semiconductor devices. It is also useful for high-precision continuity testing of continuity test objects with smooth test target areas and non-fine-pitch continuity test objects. [Explanation of symbols]
[0049] 1. Conductive particles 2 Elastomer film 10, 11 Conductive particle arrangement film 30 Insulating flexible sheet 31 Through electrode 32 Flexible connector sheet 50 Electronic circuit board for continuity testing 60 Probe material 61 Electrode structure 100, 200, 300 Inspection probe unit t Elastomer film thickness d Average particle size of conductive particles
Claims
1. A laminated connector unit having a flexible connector sheet in which a through electrode is provided on an insulating flexible sheet, and a pair of conductive particle-disposed films sandwiching the flexible connector sheet, The conductive particle-arranged film is a conductive particle-arranged film in which conductive particles are arranged in the planar direction of an elastomer film made of a cured resin, and the average particle diameter d of the conductive particles and the thickness t of the elastomer film are expressed by the following formula: 0.70d≦t≦1.10d Fulfilling The conductive particles are arranged independently without being connected in the thickness direction of the elastomer film, Each conductive particle-disposed film has a plurality of conductive particles disposed locally and independently and spaced apart from each other in correspondence with the through electrodes, without being connected to each other; A connector unit in which the interparticle distance between conductive particles locally arranged on one of a pair of conductive particle arrangement films is different from the interparticle distance between conductive particles locally arranged on the other of the pair of conductive particle arrangement films so that the conductive particles do not overlap when viewed in a plane.
2. 2. The connector unit according to claim 1, wherein the conductive particles are exposed such that ends of the conductive particles are located within 30% of the thickness of one surface of the elastomer film.
3. A connector unit as described in claim 1, wherein the number of conductive particles locally arranged on one of a pair of conductive particle arranged films is different from the number of conductive particles locally arranged on the other of the pair of conductive particle arranged films so that the conductive particles do not overlap in a planar view.
4. A connector unit as described in claim 1, wherein the arrangement pattern of the conductive particles locally arranged on one of the pair of conductive particle arrangement films and the arrangement pattern of the conductive particles locally arranged on the other are different from each other so that the conductive particles do not overlap in a planar view.
5. 5. The connector unit according to claim 1, wherein the conductive particles have a uniform particle size.
6. 6. The connector unit according to claim 1, wherein the CV value of the average particle size of the conductive particles is 20% or less.
7. A connector unit described in any one of claims 1 to 6, wherein an adhesive layer is formed on at least one side of the conductive particle arrangement film.
8. A method for producing a conductive particle-disposed film, in which conductive particles are arranged in the plane direction of an elastomer film made of a cured resin, an average particle diameter d of the conductive particles and a thickness t of the elastomer film satisfy the formula "0.70d≦t≦1.10d", and the conductive particles are exposed such that ends of the conductive particles are located within 30% of the thickness of one surface of the elastomer film, the conductive particle-arranged film is a conductive particle-arranged laminate film in which a plurality of conductive particle-arranged films are laminated together, A manufacturing method in which conductive particles are placed in the recesses of a transfer mold which has multiple recesses formed in a planar direction, an elastomer film is pressed against the recessed surface of the transfer mold to transfer the conductive particles, and the elastomer film to which the conductive particles have been transferred is sandwiched between a pair of base plates and heated and pressurized to force the conductive particles into the elastomer film.
9. 9. The method according to claim 8, further comprising forming an adhesive layer on at least one surface of the conductive particle-disposed film.
10. A conductive particle-arranged laminate film in which a plurality of conductive particle-arranged films are laminated, in which conductive particles are arranged in a planar direction of an elastomer film made of a cured resin, A conductive particle-disposed laminate film in which the thickness of the elastomer film in the conductive particle-disposed film is approximately equal to the average particle diameter of the conductive particles, and the ends of the conductive particles are located near the outermost surfaces of each of both sides of the elastomer film.
11. 11. The conductive particle-arranged laminate film according to claim 10, further comprising an adhesive layer formed on at least one surface of the conductive particle-arranged film.
12. 12. An inspection probe unit comprising the conductive particle-disposed laminate film according to claim 10 or 11, which is disposed as an inspection probe material on an electronic circuit board for continuity inspection.
13. An inspection probe unit having an electronic circuit board for continuity inspection and a probe material having an electrode structure electrically connected thereto, 12. An inspection probe unit, comprising: an electronic circuit board for continuity inspection; and a probe material and a conductive particle-disposed laminate film according to claim 10 or 11 disposed between the electronic circuit board and the probe material as an anisotropic conductive connector.
14. An inspection probe unit having an electronic circuit board for continuity inspection and a probe material having an electrode structure electrically connected thereto, 12. An inspection probe unit comprising the conductive particle-disposed laminate film according to claim 10 or 11 disposed as an anisotropic conductive adapter on the tip of a probe material on the side opposite to an electronic circuit board for continuity inspection.
15. An inspection probe unit having an electronic circuit board for continuity inspection and a probe material having an electrode structure electrically connected thereto, An inspection probe unit in which the conductive particle-disposed laminate film according to claim 10 or 11 is arranged as an anisotropic conductive adapter at the tip of the probe material opposite the electronic circuit board for continuity testing and at the tip of the probe material opposite the electronic circuit board for continuity testing.
16. A continuity inspection method comprising applying the inspection probe unit according to any one of claims 12 to 15 to an object to be inspected for continuity.
Citation Information
Patent Citations
Anisotropic conducting sheet
JP1986188818A
Connection member and structure and method for connecting electrode using the same
JP1996148213A
Conductive elastomer composition
JP1998188672A
Sheet-shaped connector, its method of manufacture and electrical inspection apparatus
JP2001351702A
Probe member and manufacturing method thereof, and application of probe member
JP2009098065A