MULTI-SHOWERHEAD CHEMICAL VAPOR DEPOSITION REACTOR, METHODS AND PRODUCTS - Patent application
A multi-showerhead chemical vapor deposition reactor with optical excitation addresses the challenge of producing kilometer-long HTS tapes with uniform properties, enhancing reactor efficiency and cost-effectiveness.
Patent Information
- Application Number
- JP2021549499
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-02-25
- Filing Date
- 2020-02-25
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2040-02-25
AI Technical Summary
Existing manufacturing processes for high temperature superconductor (HTS) tapes or wires, such as those made from rare earth-barium-copper oxide (REBCO) layers, fail to produce kilometer-long tapes with uniform properties and high reactor efficiency, necessary for cost-effective commercial applications.
A chemical vapor deposition reactor with multiple showerheads and optical excitation sources is used to deposit REBCO layers on textured metal tapes, ensuring uniform deposition and high efficiency over large areas, allowing for kilometer-long HTS tapes.
The reactor enables the production of high-quality kilometer-long HTS tapes with consistent properties and efficient deposition, facilitating cost-effective commercial production.
Smart Images

Figure 0007565934000001 
Figure 0007565934000002 
Figure 0007565934000003
Abstract
Description
Description of Related Applications
[0001] This application claims the benefit of priority under 35 U.S.C. §119 of U.S. Provisional Patent Application No. 62 / 809986, filed February 25, 2019, the contents of which are incorporated herein by reference in their entirety. [Technical field]
[0002] The present disclosure relates to a multi-showerhead metal-organic chemical vapor deposition (MOCVD) reactor having multiple showerheads that is particularly useful for producing high temperature superconductor (HTS) tapes or wires, methods for producing HTS tapes or wires, and HTS tapes or wires that can be produced using the disclosed reactors and methods. [Background technology]
[0003] Second generation high temperature superconductor (HTS) tapes or wires consist of a rare earth-barium-copper oxide (REBCO) layer deposited on a textured metal tape (typically Hastelloy or stainless steel). These have been deposited by physical vapor deposition techniques such as pulsed laser deposition (PLD) and reactive co-evaporation (RCE), by solution techniques such as metal organic vapor deposition (MOD), and by metal organic chemical vapor deposition (MOCVD). For successful commercial applications, kilometer-scale lengths of HTS tape with uniform properties are needed - at a cost comparable to copper cables of similar current carrying capacity. To date, neither the manufacturing equipment nor the processes have been successful enough to meet this need.
[0004] The use of photoexcited MOCVD has been proposed to improve the crystalline quality of the REBCO layer and therefore the performance of the HTS tapes. In addition, it has been suggested that photoexcitation would allow for increased growth rates while maintaining good performance. However, no process or reactor design has been developed to date that can use photoexcitation to produce kilometer-long HTS tapes. Additionally or alternatively, no reactor has been demonstrated that uses photoexcitation to provide high growth rates, uniform deposition, and high reactor efficiency over large deposition areas, e.g., deposition areas of 10 cm x 100 cm. Summary of the Invention [Problem to be solved by the invention]
[0005] It would therefore be desirable to establish a process and / or reactor that can use optical excitation to produce kilometer-long HTS tapes and / or that provides uniform deposition over large deposition areas and high reactor efficiency. In particular, if these characteristics can be achieved together in a process and / or reactor, it is believed that successful commercial production of HTS tapes can be achieved in that kilometer-long HTS tapes can be produced with good quality at reasonable cost. [Means for solving the problem]
[0006] According to some aspects of the present disclosure, a chemical vapor deposition reactor having multiple showerheads is provided. The reactor comprises a reactor chamber surrounded by a chamber wall, the chamber having a length and a width, the length being greater than the width. The chamber wall has inlet and outlet seal ports at opposite ends of the chamber along its length for receiving and transferring a tape during deposition onto the tape. The chamber contains a support plate for supporting the tape. The support plate has a length and a width, the length being greater than the width.
[0007] A precursor showerhead is positioned within the vessel, the precursor showerhead having a length and a width, the length being greater than the width. The precursor showerhead is positioned above a support plate, the precursor showerhead having a length dimension parallel to the length dimension of the support plate. First and second gas curtain showerheads are positioned within the vessel on either side of the precursor showerhead. Each of the first and second gas curtain showerheads has a length and a width, the length being greater than the width. The gas curtain showerheads are positioned such that a length dimension of the gas curtain showerhead is aligned parallel to a length dimension of the precursor showerhead.
[0008] The reactor further comprises one or more first illumination sources positioned on a first side of the width of the vessel and one or more second illumination sources positioned on a second side of the width of the vessel, positioned and aligned such that the illumination sources can illuminate the top surface of the tape during deposition by shining beams of illumination on the top surface beneath the respective curtain showerheads and beneath the precursor showerheads.
[0009] According to another aspect of the disclosure, a method is provided for forming kilometer-long high temperature superconductor tape, the method comprising: feeding a textured tape from a supply roll through a reactor vessel having vessel walls to a take-up roll; flowing high temperature superconductor precursor from an elongated precursor showerhead positioned within the vessel facing an upper surface of the tape, the precursor showerhead elongated in a direction along a centerline of the tape; flowing gas from first and second elongated gas curtain showerheads positioned within the vessel on either side of the precursor showerhead, the first and second elongated gas curtain showerheads elongated in a direction parallel to the centerline of the tape; and illuminating the upper surface of the tape with illumination from one or more first and one or more second illumination sources at opposite ends of the reactor positioned to pass illumination through each of the curtain showerheads and through the precursor showerhead to the upper surface of the tape.
[0010] Additional features and advantages are set forth in, and will be readily apparent to, those skilled in the art from the following detailed description, or may be learned by practicing the embodiments described herein, including the following detailed description, the claims, and the accompanying drawings.
[0011] It is to be understood that both the foregoing general description and the following detailed description are merely exemplary and are intended to provide an overview or framework for understanding the nature and character of the present disclosure and claims.
[0012] The accompanying drawings are included to provide a further understanding of the principles of the present disclosure, and are incorporated in and constitute a part of this specification. The drawings illustrate one or more embodiments and, together with the description, serve to explain, by way of example, the principles and operation of the present disclosure. It will be understood that the various features of the present disclosure disclosed in this specification and in the drawings can be used in any and all combinations. As non-limiting examples, various features of the present disclosure may be combined with each other according to the following embodiments: [Brief description of the drawings]
[0013] The following is a brief description of the figures in the accompanying drawings, which are not necessarily drawn to scale, and certain features and certain views of the figures may be depicted exaggerated in scale or schematic for clarity and conciseness. [Figure 1] 1 is a cross-sectional plan view of a reactor according to at least one example of the present disclosure. [Diagram 2] FIG. 2 is a cross-sectional schematic diagram taken along line II-II shown in FIG. 1 illustrating one or more alternative embodiments, such as alternative or optional features, of the present disclosure. [Diagram 3] FIG. 2 is a cross-sectional schematic diagram taken along line III-III shown in FIG. 1, in accordance with one or more embodiments of the present disclosure. [Figure 4] FIG. 4 is a schematic cross-sectional view corresponding to that of FIG. 3, illustrating one or more further features of one or more alternative embodiments. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] Additional features and advantages are set forth in, and will become apparent to, those skilled in the art from, the following detailed description, or may be learned by practicing the embodiments as set forth in the following description, taken in conjunction with the claims and the accompanying drawings.
[0015] As used herein, the term "and / or," when used in a list of two or more items, means that any one of the listed items can be used by itself, or any combination of two or more of the listed items can be used. For example, if a composition is described as containing components A, B, and / or C, the composition can contain A only; B only; C only; A and B in combination; A and C in combination; B and C in combination; or A, B, and C in combination.
[0016] In this document, relational terms such as first and second, top and bottom, etc. are used only to distinguish one entity or action from another entity or action without necessarily requiring or implying any actual such relationship or order between such entities or actions.
[0017] Modifications of the disclosure will occur to those skilled in the art and to those who make or use the disclosure. Accordingly, it is understood that the embodiments shown in the drawings and described above are for illustrative purposes only and are not intended to limit the scope of the disclosure, which is defined by the following claims, as interpreted in accordance with the principles of patent law, including the doctrine of equivalents.
[0018] For purposes of this disclosure, the term "connected" (in all of its forms: connect, connect, coupled, etc.) broadly means the joining of two components to one another, directly or indirectly. Such a joining may be stationary in nature or mobile in nature. Such a joining may be achieved by an intermediate member integrally molded with the two components and one another as one unitary body, or by the two components themselves. Such a joining may be permanent in nature or removable or releasable in nature, unless otherwise specified.
[0019] As used herein, the term "about" means that amounts, sizes, formulations, parameters, and other quantities and characteristics are not and need not be exact, but may be approximate and / or larger or smaller, as appropriate, to reflect tolerances, conversion factors, rounding, measurement errors, and the like, as well as other factors known to those of skill in the art. When the term "about" is used in describing a value or endpoint of a range, the disclosure should be understood to include the specific value or endpoint referred to. Whether or not a range value or endpoint is referred to in the specification as "about," the range value or endpoint is intended to include two embodiments: those modified by "about" and those not modified by "about." It will be further understood that each endpoint of a range is significant both in relation to the other endpoint and independently of the other endpoint.
[0020] As used herein, the terms "substantially," "substantially," and variations thereof are intended to state that a described feature is equal or approximately equal to a value or description. For example, a "substantially flat" surface is intended to indicate a surface that is flat or nearly flat. Additionally, "substantially" is intended to indicate that two values are equal or approximately equal. In some embodiments, "substantially" can mean values within about 10% of each other, such as within about 5% of each other, or within about 2% of each other.
[0021] Any directional terms used herein - e.g., up, down, right, left, front, back, upper and bottom - are used only with reference to the drawings depicted and are not intended to imply absolute orientation.
[0022] As used herein, nouns refer to "at least one" of an object and should not be limited to "only one" unless clearly indicated otherwise. Thus, reference to an "element" includes embodiments having two or more such elements unless the context clearly indicates otherwise.
[0023] There are many deposition methods to deposit YBCO layers on metal tapes. These include pulsed laser deposition (PLD), reactive co-evaporation (RCE), metal organic deposition (MOD), and metal organic chemical vapor deposition (MOCVD). MOCVD has been used to deposit YBCO on metal tapes in a reel-to-reel process. These tapes are 12 mm wide and are passed through many times to obtain a sufficiently thick layer in a reasonable time. Multiple passes are used because the deposition rate is slow. At higher deposition rates, the crystal quality is degraded and the desired performance (critical current, critical temperature, magnetic field performance, etc.) cannot be obtained. Photoexcitation-assisted deposition has been used to obtain good quality layers at higher deposition rates, but poor utilization of the metal organic precursors and poor uniformity of the YBCO thickness have been encountered.
[0024] In general, the present disclosure relates to a multiple showerhead metal organic chemical vapor deposition (MOCVD) reactor particularly suited for producing high temperature superconductor (HTS) tapes or wires, and a method for producing HTS tapes or wires.
[0025] A reactor is disclosed that enables reel-to-reel deposition of high temperature superconductor layers such as YBCO onto kilometer-long textured metal tapes by photoinduced metal organic chemical vapor deposition of consistent high quality. The reactor can be operated for extended periods without appreciable decay of photoinduced excitation, enabling the production of kilometer-scale tapes or wires.
[0026] 1 and 3, the reactor 10 includes multiple showerheads 40, 50, 60, with the precursor showerhead 40 positioned relatively close to the location of the top surface 22 of the textured metal tape 20 as it is being processed providing a uniform flow of precursors over the top surface 22 of the metal tape 20, and first and second gas curtain showerheads 50, 60 providing a gas curtain (an inert or otherwise non-reactive gas curtain) on either side of the precursor showerhead 40 on either side of the tape 20. This gas curtain helps to prevent deposition on the light or radiation source 72, 82 or on the windows 71, 81 (through which the light source or radiation source provides light or radiation to the top surface of the textured metal tape 20). The light sources 72, 82 or windows 71, 81 can comprise, for example, quartz windows, or light emitting diodes (LEDs) with optical elements structured to allow all or much of the light from the LEDs to pass through the narrow gap between the showerhead 40, 50, 60 and the tape 20 (particularly between the precursor showerhead 40 and the tape 20).
[0027] According to one embodiment, the first set 72 of light emitting diodes illuminate one half of the tape 20 as shown in Figure 3, and the second set 82 of light emitting diodes illuminate the other half, where the radiation from the LEDs 76, 86 is reflected by mirrors 78, 88 to form respective beams 73, 83 (parallel or focused), each beam actually illuminating half of the top surface 22 of the tape 20. Alternatively, the reactor 10 and beams 73, 83 as shown in Figures 1 and 4 may be structured such that the beams 73, 83 illuminate all or most of the top surface 22 of the tape 20 from both sides.
[0028] Heating mechanisms, such as passageways (not shown), are provided in the reactor walls and other parts of the reactor to allow heating of the reactor parts and walls, such as by flow of a heat transfer fluid, to maintain the surfaces of all reactor walls and internal parts (except for LEDs or windows) at a temperature high enough to prevent condensation of the precursors or reaction by-products, but not so high as to decompose them (e.g., in the range of 300 to 400° C., or about 350° C.).
[0029] 2, the tape 20 can be heated to a deposition temperature by passing a current through the tape 20, such as passing a current through the tape 20 between two conductive rollers 90, 92 in contact with the tape 20 and connected to a constant current source 94. Alternatively, or in addition, a tungsten halogen lamp 120 positioned below the tape 20, facing the lower surface 21 of the tape 20, may be used to heat the tape 20. The reactor 10 may include an envelope 31. If present, the pressure within this envelope 31 is higher than in the reactor housing 30, and the pressure is maintained by differential pumping. The tape 20 enters and exits the reactor housing 30 through one or more differentially pumped inlet and outlet tubes 16, 18 (one of each is shown). (Similarly, the tape 20 enters and exits the envelope 31 through differentially pumped tubes, as shown in one or more of the figures).
[0030] Referring again to Figures 1-3, with particular emphasis on the features in Figure 3, a tape or wire 20, preferably sized to a width ranging from 0.1 to 20 cm, or 1 to 15 cm, or 5 to 15 cm, or 8 to 12 cm, moves to the right as indicated by arrow A in Figure 1, as it exits the page of Figure 3, or from a supply reel 12 to a take-up reel 14, as in Figure 2. The reels 12, 14 may be at atmospheric pressure or at a low vacuum (e.g., low vacuum). There may be several stages of differential pumping between the reactor 10 and the pressure at which the reels 12, 14 are maintained. For the embodiment of the reactor 10 shown in Figure 3, the tape 20 is heated by passing a current from a constant current source 94, as shown in Figure 2 (i.e., without the optional or alternative lamps 120, also shown in Figure 2).
[0031] Precursors in a carrier gas are delivered by a closely spaced (central) precursor showerhead 40 at multiple points 42 along the deposition zone having a length within the range of 25 to 1000 cm, or 50 to 500 cm, or 60 to 300 cm, or 70 to 250 cm, or 80 to 150 cm, or about 100 cm. The precursor showerhead 40 is positioned close (1-2 cm) to the textured tape 20. The precursor showerhead 40 has two perforated plates (placed in series in the gas flow and acting as a mixing plate and showerhead) to provide sufficient pressure differential and uniform distribution of precursors on the top surface of the tape 20. Two additional showerheads 50, 60 create an inert gas curtain that prevents precursors or reaction byproducts from reaching the LED or the window through which the LED light enters the reactor 10. In addition, the LED or window is placed in a purged recess 80 to further inhibit precursors or reaction byproducts from reaching the light source. Exhaust manifolds (shown in FIG. 3) on both sides are connected to a vacuum pump (not shown) that uses throttling valves to maintain the reactor at the desired pressure. All reactor wall and internal component surfaces (except the LEDs) are maintained at a temperature (e.g., 350° C.) high enough to prevent condensation of precursors or reaction by-products, but not so high as to decompose them. The temperature of the tape 20 is monitored and controlled by one or more pyrometers sensing the bottom or top surface of the tape (top surface monitoring is shown in FIG. 2).
[0032] The precursor showerhead 40 creates a stagnant point flow to obtain a uniform YBCO layer on a 10 cm wide metal ("Hastelloy", stainless steel, etc.) tape 20 while achieving high precursor utilization. The tape 20 can be narrower or wider, in which case a narrower or wider precursor showerhead 40 is required. The length of the precursor showerhead 40 is preferably 100 cm in this design, but can be shorter or longer depending on the desired length of the deposition zone. Optical excitation is preferably provided by light emitting diodes (LEDs) emitting at 385-405 nm (e.g., the wavelength can be adjusted shorter or longer). A beam of light from an LED on one side of the reactor is directed at one side of the tape. Heating of the tape can be achieved by passing an electric current through the tape or by a tungsten halogen lamp positioned below the tape. A schematic diagram of the reactor 10 in which the tape 20 is heated by passing an electric current through it is shown in FIG. 2.
[0033] As can be seen from Figures 1 and 3, by having two curtain showerheads 50, 60, located on either side of the precursor showerhead 40, provide a gas curtain of inert or otherwise non-reactive gas, deposition on the LEDs is minimized or even completely avoided. In addition, the window or LEDs and associated optical elements 72, 82 are placed in a gas-purged recess 80 to further prevent precursors or reaction by-products from depositing thereon. For example, as shown in Figure 2, according to one embodiment, the light sources 72, 82 can be an array of LEDs 76, 86, and parabolic reflectors 78, 88 direct collimated light beams 73, 83 to substantially half (respective halves) of the tape 20, all along the deposition area. All reactor walls and showerheads are heated to about 350°C to prevent precursors or reaction by-products from depositing thereon, thereby eliminating the need to clean the reactor after every run. This also significantly reduces the chances of particles falling onto the tape. It is desirable for the LEDs to be water-cooled. In embodiments where the light source 72, 82 is in the form of a window, it is also possible to have the LEDs and optics external to the reactor vessel, with the light being brought in through a UV transmissive window 71, 81. By using optics, the LED light beam can be brought up just high enough to illuminate half the tape, but can also be fanned out laterally to illuminate a 5-10cm length of tape if desired.
[0034] The temperature of the tape is monitored by an emissivity corrected pyrometer or by one or more such pyrometers P as shown in Figures 2 and 3, directed at the top (Figure 2) or bottom (Figure 3) of the tape. The pyrometer ports are purged with gas to prevent any deposition of precursors or reaction by-products on the pyrometer. An exhaust manifold EM is connected to the vessel 30 via exhaust ports 100, 110 on either side of the reactor 10, and to a suitable vacuum pump (flow direction and position shown by arrow VP), which maintains the reactor 10 at the desired pressure. The spacing between the main showerhead and the tape is desirably about 1-2 cm, preferably about 1 cm. This relatively small spacing ensures that the Grashof number is small, since the Grashof number is proportional to the cube of the spacing. A sufficiently low Grashof number avoids buoyancy-induced convection. The resulting stagnation-point flow geometry used ensures uniform deposition. This is because the boundary layer, and the concentration of precursor above the boundary layer, is constant across the width of the tape 20 .
[0035] The tape 20 is preferably fed into the reactor through a differentially pumped chamber / enclosure 31 (FIG. 2) so that the supply and take-up reels 12, 14 can be brought to atmospheric pressure. Current is supplied to and drawn from the tape through highly conductive cylindrical electrodes 90, 92, which are preferably water-cooled. In some embodiments, the electrodes 90, 92 are made electrically isolated from ground and / or the rest of the reactor components / parts. The surfaces of the electrodes are highly polished to ensure good contact. Current is supplied from a constant current source 94 so that variations in contact resistance are not an issue. The main or precursor showerhead 40 has two perforated plates 44, 46 to ensure uniform flow from the showerhead 40. The outermost showerhead plate 46 has pores with diameters of about 0.6-1 mm (preferably 0.8 mm) and their length is about 0.5 to 1 cm. The density of the pores is 15-20 per square cm. The inner showerhead plate 44 has pores with diameters of 1-2 mm, lengths of 0.5 to 1 cm, and a density of 4 to 20 per square cm. Gas is supplied to the main showerhead through a manifold (not shown) with multiple ports 42 along the showerhead 40 to distribute the gas as evenly as possible over the inner showerhead plate 44. Two outer or curtain showerheads 50, 60, which provide a gas curtain (preferably an inert gas or Ar gas curtain), have plates 54, 64 with pore size, length and density similar to that of the inner showerhead plate 46 in the precursor showerhead 40. Gas, preferably Ar, is supplied to these outer showerheads 50, 60 through a manifold (not shown) with multiple ports 52, 62 along each showerhead 50, 60 to distribute the gas evenly over the respective perforated plates 54, 64. A plate 32 (support plate) separates the reactor vessel 30 into two parts. The spacing between the tape and plate 32 (backing plate) is preferably about 1 mm at the bottom and edges of the tape 20. One or more slots or holes 33 in the backing plate 32 allow gas (an inert purge gas) to be uniformly distributed underneath the tape 20.This flow prevents any precursors or reaction by-products from depositing on the bottom surface of the tape 20 or entering the bottom of the reactor chamber 30. In some embodiments, the backing plate is made in a spaced relationship (e.g., not in contact) with the tape, and the backing plate is made to support one or more gas purge lines made through the backing plate and directed to the underside of the tape. In some embodiments, the tape is heated directly by electrical current (i.e., direct contact with the backing plate) or heated by halogen lamps (i.e., no direct contact with the backing plate). In configurations where there is no direct contact, the backing plate is made to direct the gas purge to the backside of the tape. For heating embodiments using a susceptor, the susceptor is also referred to as a backing plate therein, in which case there may be additional thermally isolated "backing plates" on either side of the susceptor / backing plate. In the case of electrical current heating, if the backing plate is used as a backing plate, there will be additional insulating material made / placed at regular intervals along the length of the tape. Modeling showed that the deposition uniformity was approximately 1.7% and the reactor efficiency was 40%.
[0036] The tape 20 may alternatively or additionally be heated using tungsten halogen lamps positioned below the tape 20, as also shown in Figure 2. A fused quartz window may be used in the center of the plate 32 (such as center 36 depicted by dotted lines 37, 38) to allow lamp radiation to illuminate the bottom side of the tape 20. One or more slots or holes 33 (if multiple, evenly spaced along the deposition area) allow purging of the space between the tape 20 and the quartz window. The inert purge gas prevents precursors and reaction by-products from entering the space between the tape 20 and the quartz window, thereby preventing deposition on the window.
[0037] A group of lamps 120 is preferably controlled by one PID controller that gets feedback from an emissivity corrected pyrometer P that monitors the top or bottom surface of the tape 20. The emissivity corrected optical pyrometer is placed along the length of the deposition zone to provide feedback to the particular group of lamps underneath. The multi-zone heating zone allows for tailoring of the temperature profile along the tape. The pyrometer P can be positioned to monitor the temperature of the top or bottom surface of the tape. If the pyrometer monitors the top surface, a narrow diameter purge port, sealed at one end by a fused quartz window, is fabricated in the showerhead as shown in FIG. 2. If the pyrometer is placed underneath the tape to monitor the back side of the tape (FIG. 3), the tip of the pyrometer tube should be spaced far enough away from the tape so that the lamp illumination is not blocked. Also, the inner surface of the pyrometer tube should be rough so that the reflected light cannot propagate all the way to the pyrometer due to multiple reflections along the inner wall.
[0038] The tape can also be heated with an electrically heated susceptor (heater) placed in contact with the tape. The path of the susceptor and tape does not need to be curved to maintain good contact between the susceptor and tape. In some embodiments, the radius of the curve is about 20 to 50 m, preferably 25 m. In some embodiments, the showerhead should also be curved to maintain a constant height between the tape and the showerhead.
[0039] The tape may be heated using a combination of methods, such as a tungsten halogen lamp that heats the tape from below, or it may be heated by the passage of an electric current, as shown in FIG.
[0040] Using either a linear array of transmissive glass cylindrical lenses or a linear reflective collimator such as those available from Chromasens (Konstanz, Germany), the light from the linear array of LEDs can therefore be collimated in one dimension to illuminate the entire length and width of the tape, as can be seen from the illustration of the beams 73, 83 in FIG. 4 (for width) and FIG. 1 (for length and width). This can be done by using LEDs on both sides of the chamber. The linear or (slightly) focused beams 73, 83 from both sides of the chamber can (and preferably do) completely overlap to promote good coverage and uniformity. The direct array of transmissive lenses is such that an array of lenses or a single long cylindrical glass lens could also replace the transparent windows 71, 81 on both sides of the deposition chamber as an additional alternative embodiment.
[0041] One embodiment of a functional cylindrical lens is a 100-200 cylindrical plano-convex lens made from N-BK7 by K&S Optics (Greene County, NY, USA) with a focal length of 10 mm and a diameter of 12.5 mm. This lens can be placed approximately 10 mm away from the LED to capture just over half the light from the LED and collimate it into a straight beam approximately 10 mm wide.
[0042] An alternative lens with similar focusing characteristics is the LJ1878L2-A available from Thorlabs (Newton, NJ, USA). The Thorlabs lens has one advantage: an anti-reflective coating for the wavelength range of 350 to 700 nm, which encompasses the wavelengths of most interest for deposition chambers.
[0043] In linear reflection embodiments, a reflector similar to, for example, Reflector Type C or Type D from Chromasens, Inc., can be used. The specific geometry details of the reflector can be tailored to the final geometry of the deposition chamber to provide the appropriate tradeoff between light distribution uniformity and efficiency.
[0044] The choice of metal coating is important for the reflective elements. For wavelengths shorter than 500 nm, aluminum is generally the low-loss choice. At longer wavelengths, silver and gold are preferred. If one material must be used over a wide wavelength range, including both longer and shorter wavelengths than 500 nm, aluminum is generally preferred due to its uniformly low loss.
[0045] LED Wavelength Selection: It is possible to construct an array of LEDs with a variety of wavelengths selected to optimize the reaction and deposition process. For this YCBO reactor, a range of wavelengths can be used from UV to visible. One embodiment has a group of three wavelength LEDs repeated along the length of the LED array, with 365, 385 and 405 nm LEDs in the group providing full spectral coverage in the near UV and deepest blue wavelength ranges. The same type of wavelength diversity scheme can be created for other types of light sources, such as lasers.
[0046] While exemplary embodiments and examples have been set forth for illustrative purposes, the foregoing is not intended to limit the scope of the present disclosure and the appended claims in any way. Thus, modifications and variations may be made to the above-described embodiments and examples without substantially departing from the spirit and various principles of the present disclosure. All such modifications and variations are intended to be included within the scope of this disclosure and protected by the following claims.
[0047] Preferred embodiments of the present invention will be described below in detail.
[0048] EMBODIMENT 1 In a chemical vapor deposition reactor having multiple showerheads, a reactor vessel surrounded by a vessel wall, the vessel having a length and a width, the length being greater than the width, the vessel wall having inlet and outlet seal ports at opposite ends of the vessel along its length for receiving and transferring a tape during deposition onto the tape; a support plate within the tank for supporting the tape, the support plate having a length and a width, the length being greater than the width; a precursor showerhead positioned within the vessel, the precursor showerhead having a length and a width, the length being greater than the width, the precursor showerhead positioned above the support plate, a length dimension of the precursor showerhead parallel to a length dimension of the support plate; first and second gas curtain showerheads positioned on either side of the precursor showerhead, each of the first and second gas curtain showerheads having a length and a width, the length being greater than the width, and a length dimension of the gas curtain showerheads aligned parallel to a length dimension of the precursor showerhead; one or more first illumination sources positioned on a first side of a width of the vessel and one or more second illumination sources positioned on a second side of a width of the vessel, the first and second illumination sources positioned and aligned such that they can illuminate an upper surface of the tape during deposition by shining a beam of illumination on the upper surface beneath the curtain showerhead and beneath the precursor showerhead, respectively; A reaction apparatus comprising:
[0049] EMBODIMENT 2 2. The reactor of embodiment 1, wherein the one or more first illumination sources are positioned within one or more first recesses on the first side of the vessel and the one or more second illumination sources are positioned within one or more second recesses on the second side of the vessel.
[0050] EMBODIMENT 3 3. The reactor of embodiment 2, wherein the one or more first recesses and the one or more second recesses are provided with respective gas ports in communication with the interior of the respective recesses.
[0051] EMBODIMENT 4 4. The reactor of any one of the preceding claims, wherein the support plate comprises one or more slots or ports positioned below the tape for providing a purge gas flow between the tape and the support plate.
[0052] EMBODIMENT 5 5. The reactor of any one of the preceding embodiments, wherein the precursor showerhead is wider than 10 mm.
[0053] EMBODIMENT 6 6. The reactor of any one of the previous embodiments, wherein the precursor showerhead is positioned closer to a plane coinciding with the top surface than the gas curtain showerhead.
[0054] EMBODIMENT 7 7. The reactor of any one of embodiments 1 to 6, wherein the precursor showerhead is positioned within 0.8-2 cm of the top surface.
[0055] EMBODIMENT 8 7. The reactor of any one of embodiments 1 to 6, wherein the precursor showerhead is positioned within 0.8 to 1.2 cm from the top surface.
[0056] EMBODIMENT 9 9. The reactor of any one of the previous embodiments, wherein the precursor showerhead comprises one or more porous mixer-distribution plates.
[0057] EMBODIMENT 10 10. The reactor of embodiment 9, wherein the precursor showerhead comprises at least two porous mixer-distribution plates, including a first mixer-distribution plate having a first pore size and a second mixer-distribution plate having a second pore size, the second mixer-distribution plate being positioned between the first mixer-distribution plate and the support plate, and the first pore size being larger than the second pore size.
[0058] EMBODIMENT 11 11. The reactor of any one of the preceding claims, further comprising first and second conductive platens or rollers positioned in contact with the tape to heat the tape by passing an electric current along the tape.
[0059] EMBODIMENT 12 12. The reactor of embodiment 11, further comprising a constant current source connected to the first and second conductive platens or rollers.
[0060] EMBODIMENT 13 13. The reactor of any one of the preceding claims, further comprising a radiation source positioned below the support plate to heat the tape.
[0061] EMBODIMENT 14 14. The reaction device of any one of the preceding embodiments, further comprising one or more temperature sensors positioned to sense a temperature of the tape.
[0062] EMBODIMENT 15 15. The reactor of embodiment 14, wherein the one or more temperature sensors comprise one or more pyrometers positioned facing the top surface.
[0063] EMBODIMENT 16 15. The reactor of embodiment 14, wherein the one or more temperature sensors comprise one or more pyrometers positioned facing a lower surface of the tape.
[0064] EMBODIMENT 17 1. A method of forming a kilometer long high temperature superconductor tape, comprising: feeding the textured tape from a supply roll through a reactor vessel having a vessel wall to a take-up roll; flowing a high temperature superconductor precursor from an elongated precursor showerhead positioned within the vessel facing an upper surface of the tape, the precursor showerhead being elongated in a direction along a centerline of the tape; flowing gases from first and second elongated gas curtain showerheads positioned within the vessel on either side of the precursor showerhead, the first and second elongated gas curtain showerheads being elongated in a direction parallel to a centerline of the tape; and illuminating an upper surface of the tape with illumination from one or more first illumination sources and one or more second illumination sources positioned to pass illumination onto the upper surface of the tape under each of the curtain showerheads and through under the precursor showerhead; The method comprising:
[0065] EMBODIMENT 18 18. The method of embodiment 17, wherein the step of supplying the tape comprises supplying the tape continuously. [Explanation of symbols]
[0066] 10. Reactor 16 Inlet pipe 18 Outlet pipe 20 Tape 30 Case 31 Envelope 32 Support plate 33 Slots, holes 40 Precursor Showerhead 50, 60 Gas curtain shower head 52, 62 ports 71, 81 Windows 72, 82 light source 73, 83 Beam 80 Recess 90, 92 Conductive roller 94 Constant current source 120 Halogen lamp
Claims
1. In a chemical vapor deposition reactor having multiple showerheads, a reactor vessel surrounded by a vessel wall, the vessel having a length and a width, the length being greater than the width, the vessel wall having inlet and outlet seal ports at opposite ends of the vessel along its length for receiving and transferring a tape during deposition onto the tape; a support plate in the tank for supporting the tape, the support plate having a length and a width, the length being greater than the width; a precursor showerhead positioned within the vessel, the precursor showerhead having a length and a width, the length being greater than the width, the precursor showerhead positioned above the support plate, a length dimension of the precursor showerhead parallel to a length dimension of the support plate; first and second gas curtain showerheads positioned on either side of the precursor showerhead, each of the first and second gas curtain showerheads having a length and a width, the length being greater than the width, and a length dimension of the gas curtain showerheads aligned parallel to a length dimension of the precursor showerhead; one or more first illumination sources positioned on a first side of a width of the vessel and one or more second illumination sources positioned on a second side of a width of the vessel, the first and second illumination sources positioned and aligned such that they can illuminate an upper surface of the tape during deposition by shining a beam of illumination on the upper surface beneath the respective curtain showerhead and precursor showerhead; Equipped with The one or more first illumination sources are positioned within one or more first recesses on the first side of the vessel, and the one or more second illumination sources are positioned within one or more second recesses on the second side of the vessel.
2. A reaction apparatus as described in claim 1, wherein the one or more first recesses and the one or more second recesses are provided with respective gas ports communicating with the interiors of the respective recesses.
3. A reaction apparatus as described in claim 1 or 2, wherein the support plate includes one or more slots or ports positioned below the tape for supplying a purge gas flow between the tape and the support plate.
4. The reactor of claim 1, wherein the precursor showerhead is wider than 10 mm.
5. A reaction apparatus as described in any one of claims 1 to 4, wherein the precursor showerhead is positioned closer to a plane coinciding with the upper surface than the gas curtain showerhead.
6. The reactor of claim 1, wherein the precursor showerhead is positioned within 0.8 to 2 cm of the upper surface.
7. The reactor of claim 1, wherein the precursor showerhead is positioned within 0.8 to 1.2 cm of the upper surface.
8. The reactor of claim 1, wherein the precursor showerhead comprises one or more porous mixer / distribution plates.
9. The reaction apparatus of claim 8, wherein the precursor showerhead comprises at least two porous mixer-distributor plates, including a first mixer-distributor plate having a first pore size and a second mixer-distributor plate having a second pore size, the second mixer-distributor plate being positioned between the first mixer-distributor plate and the support plate, and the first pore size being larger than the second pore size.
Citation Information
Patent Citations
Method and apparatus for superconducting materials on tape substrates
JP2005534157A
Method and apparatus for deposition on large area substrates having reduced gas usage
US20110033638A1
Static deposition profile modulation for linear plasma source
US20130273262A1