Method for processing a semiconductor wafer

The wafer processing system addresses wafer damage during thinning by profiling and modifying edge defects, improving yield and reducing costs through methods like stealth laser dicing and trench formation.

JP7566052B2Active Publication Date: 2024-10-11YANGTZE MEMORY TECH CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2022578917
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-11-19
Publication Date
2024-10-11
Estimated Expiration
2040-11-19

AI Technical Summary

Technical Problem

Current wafer processing techniques for semiconductor wafers, particularly during thinning processes, result in wafer damage due to defects that compromise structural integrity and reduce yield, leading to increased manufacturing costs.

Method used

A wafer processing system that determines a wafer profile before thinning and modifies the wafer accordingly by identifying and remediating edge defects through methods like stealth laser dicing or partial trench formation to prevent defect propagation during thinning.

Benefits of technology

Improves wafer processing yield by maintaining structural integrity and reducing debris, while ensuring the integrity of the wafer flat and minimizing equipment modifications, thus enhancing semiconductor performance and reducing manufacturing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007566052000001
    Figure 0007566052000001
  • Figure 0007566052000002
    Figure 0007566052000002
  • Figure 0007566052000003
    Figure 0007566052000003
Patent Text Reader

Abstract

The present disclosure describes a method and system for processing a semiconductor wafer. The wafer processing method includes measuring one or more wafer characteristics of the wafer using multiple detectors. The wafer includes a device region and a peripheral region. The method also includes determining a wafer correction profile for the wafer based on the measured one or more wafer characteristics. The method further includes correcting a ring-shaped portion of the wafer in the peripheral region using the wafer correction profile. The corrected ring-shaped portion has a penetration depth that is less than a thickness of the wafer. The method further includes performing a wafer thinning process on the wafer.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates generally to the field of semiconductor technology, and more particularly to systems and methods for improving yields in semiconductor wafer processing. [Background technology]

[0002] Semiconductor wafers undergo numerous processing operations during semiconductor wafer fabrication processing in integrated circuit (IC) fabrication facilities. To increase device density, semiconductor wafers can be bonded together, and often a wafer thinning process is performed on the bonded semiconductor wafers to reduce the thickness of the wafers. Current wafer processing techniques have shortcomings that must be addressed, such as wafer damage resulting from wafer thinning. Summary of the Invention [Means for solving the problem]

[0003] Aspects of the present disclosure are best understood from the following detailed description when read in conjunction with the accompanying drawings, in which: It should be noted that, according to common practice in the industry, various features have not been drawn to scale, and in fact, dimensions of various features may have been intentionally increased or decreased for clarity of illustration and discussion. [Brief description of the drawings]

[0004] [Figure 1A] FIG. 1 is a diagram of a semiconductor wafer according to some embodiments of the present disclosure. [Figure 1B] FIG. 1 is a diagram of a semiconductor wafer according to some embodiments of the present disclosure. [Figure 2A] 1 is a cross-sectional view of an edge portion of a semiconductor wafer according to some embodiments of the present disclosure. [Figure 2B] 1 is a cross-sectional view of an edge portion of a semiconductor wafer according to some embodiments of the present disclosure. [Figure 2C] 1 is a cross-sectional view of an edge portion of a semiconductor wafer according to some embodiments of the present disclosure. [Figure 2D] 1 is a cross-sectional view of an edge portion of a semiconductor wafer according to some embodiments of the present disclosure. [Diagram 3] 1 is a cross-sectional view of a wafer in a wafer thinning apparatus according to some embodiments of the present disclosure. [Figure 4A] FIG. 1 is a diagram of a semiconductor wafer incorporating wafer modification according to some embodiments of the present disclosure. [Figure 4B] FIG. 1 is a diagram of a semiconductor wafer incorporating wafer modification according to some embodiments of the present disclosure. [Diagram 5] 1A-1D are cross-sectional views of a semiconductor wafer incorporating wafer modification during a wafer thinning process according to some embodiments of the present disclosure. [Figure 6] 1A-1D are cross-sectional views of a semiconductor wafer incorporating wafer modification during a wafer thinning process according to some embodiments of the present disclosure. [Figure 7] FIG. 1 illustrates an exemplary apparatus for forming wafer modifications in a semiconductor wafer in accordance with some embodiments of the present disclosure. [Figure 8] FIG. 1 illustrates an exemplary apparatus for forming wafer modifications in a semiconductor wafer in accordance with some embodiments of the present disclosure. [Figure 9] 1A-1D illustrate an exemplary fabrication process for forming wafer modifications in a semiconductor wafer in accordance with some embodiments of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0005] While specific configurations and arrangements are discussed, it should be understood that this is done for illustrative purposes only. Those skilled in the art will recognize that other configurations and arrangements can be used without departing from the spirit and scope of the present disclosure. Those skilled in the art will recognize that the present disclosure can be used in a variety of other applications.

[0006] It should be noted that references herein to "one embodiment," "an embodiment," "an exemplary embodiment," "some embodiments," and the like, indicate that the described embodiment may include a particular feature, structure, or characteristic, but not all embodiments necessarily include that particular feature, structure, or characteristic. Moreover, such phrases do not necessarily refer to the same embodiment. Furthermore, when a particular feature, structure, or characteristic is described in connection with one embodiment, it is within the knowledge of one of ordinary skill in the art to implement such feature, structure, or characteristic in connection with other embodiments, whether or not explicitly described.

[0007] Generally, terms can be understood, at least in part, from contextual usage. For example, the term "one or more" as used herein may be used to describe any feature, structure, or characteristic in a singular sense or to describe a combination of features, structures, or characteristics in a plural sense, depending at least in part on the context. Similarly, terms such as "a," "an," or "the" may be understood to convey singular usage or to convey plural usage, again depending at least in part on the context.

[0008] It should be readily understood that the meanings of "on," "above," and "over" in this disclosure are to be interpreted in the broadest sense, such that "on" does not only mean "directly on" something, but also includes the meaning "on" something with an intermediate feature or layer between them, and that "above" or "over" does not only mean "above" or "over" something, but can also include the meaning "above" or "over" something (i.e., located directly above something) with no intermediate features or layers between them.

[0009] Additionally, spatially relative terms such as "beneath," "below," "lower," "above," "upper," and the like may be used herein to describe the relationship of one element or feature shown in the figures to another element or feature for ease of description. The spatially relative terms are intended to encompass different orientations of the device during use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations) and the spatially relative descriptors used herein may likewise be interpreted accordingly.

[0010] As used herein, the term "substrate" refers to a material on which a layer of material is subsequently added. The substrate includes a top surface and a bottom surface. The top surface of the substrate is where the semiconductor devices are formed, and thus the semiconductor devices are formed on the top side of the substrate. The bottom surface is opposite the top surface, and thus the bottom side of the substrate is opposite the top side of the substrate. The substrate itself can also be patterned. The material added on top of the substrate can be patterned or left unpatterned. Additionally, the substrate can include a wide range of semiconductor materials, such as silicon, germanium, gallium arsenide, indium phosphide, and the like. Alternatively, the substrate can be made of a non-conductive material, such as glass, plastic, or a sapphire wafer.

[0011] As used herein, the term "layer" refers to a portion of material that includes a region having a thickness. A layer may extend throughout an underlying or overlying structure, or may have an extent that is less than the extent of the underlying or overlying structure. Furthermore, a layer may be a region of a homogeneous or heterogeneous continuous structure that has a thickness that is less than the thickness of the continuous structure. For example, a layer may be located between the top and bottom surfaces of a continuous structure or between any pair of horizontal planes at the top and bottom surfaces. A layer may extend horizontally, vertically, and / or along a tapered surface. A substrate may be a layer, may include one or more layers within it, and / or may have one or more layers thereupon, thereabove, and / or therebelow. A layer may include multiple layers. For example, an interconnect layer may include one or more conductor and contact layers (where contacts, interconnect lines, and / or vias are formed) and one or more dielectric layers.

[0012] As used herein, the term "nominal" refers to a desired or target value of a characteristic or parameter for a component or process operation that is set during the design phase of a product or process, along with a range of values ​​above and / or below the desired value. The range of values ​​may be due to slight variations in the manufacturing process or tolerances. As used herein, the term "about" refers to the value of a given quantity that may vary based on a particular technology node associated with the semiconductor device of interest. Based on a particular technology node, the term "about" can refer to the value of a given quantity that varies within a range of, for example, 10-30% of the value (e.g., ±10%, ±20%, or ±30% of the value).

[0013] As used herein, the term "3D NAND memory device" (herein referred to as "memory device") refers to a semiconductor device in which a string of vertically oriented 3D NAND memory cell transistors (herein referred to as "memory strings", such as NAND strings or 3D NAND strings) is located on a horizontally oriented substrate such that the memory strings extend vertically relative to the substrate. As used herein, the term "vertical" nominally means perpendicular to the lateral plane of the substrate.

[0014] In this disclosure, the term "horizontal / horizontally" nominally means parallel to the lateral plane of the substrate.

[0015] Stacking semiconductor wafers to form three-dimensional integrated circuits is one of the approaches to meet the demand for increased device density. Generally, stacked wafers can provide benefits such as smaller die size, higher device density, and improved performance compared to monolithic integrated circuits. Stacking semiconductor wafers can include attaching one semiconductor wafer to another using various methods such as bonding or application of adhesives, and the stacked semiconductor wafers can be thinned to reduce their overall thickness to further minimize the device footprint and reduce device size. For example, the device density of three-dimensional ("3D") memory devices can be increased by stacking peripheral devices and back-end-of-line (BEOL) interconnects on top of array devices and performing a wafer thinning process on the stacked wafer structure to reduce its overall thickness. The wafer thinning process can be a backgrind process in which the semiconductor wafers undergo a grinding process using a grinding device. Specifically, the semiconductor wafer can be positioned on the chuck via adhesive and / or vacuum, and a grinding head is pressed against the surface of the semiconductor wafer, the grinding head configured to perform rotational and lateral motions to uniformly remove material from the semiconductor wafer. The wafer thinning process can also include a polishing process, such as a chemical mechanical polishing (CMP) process that utilizes a chemical slurry along with a polishing pad to remove material from the wafer until a nominal wafer thickness is achieved. During the CMP process, the wafer is positioned on the chuck via adhesive and / or vacuum, and the wafer is rotated at a preset rotational speed while a polishing pad held by a polishing head is pressed against a lateral surface of the rotating wafer. As the wafer thins during the grinding or CMP process, defects in the wafer can cause physical damage to the wafer, which can reduce device yields and increase manufacturing costs. For example, the wafer peripheral area can include irregularly shaped edges, which can propagate to the wafer and result in cracks or fissures when forces are applied to the wafer by the polishing head.Cracks or fissures can compromise the structural integrity of the wafer, rendering it unusable for further processing.

[0016] To address the above shortcomings, embodiments described herein are directed to providing systems and methods for improving wafer processing yields during a wafer thinning process. More particularly, the present disclosure is directed to a wafer processing system configured to determine a wafer profile prior to a wafer thinning process and modify the wafer accordingly, such that each wafer is customized according to the wafer profile. For example, the wafer processing system identifies wafer edge defects located in a peripheral region of the wafer and modifies a portion of the peripheral region to create a barrier that prevents the defects from propagating into a device region of the wafer during the wafer thinning process. In some embodiments, modifying the portion of the peripheral region can include partially cutting the wafer along the perimeter and forming a trench along the perimeter. In some embodiments, modifying the portion of the peripheral region can include modifying a physical attribute of a portion of the wafer by a non-invasive method, such as stealth laser dicing.

[0017] Various embodiments described in this disclosure can provide benefits such as improved wafer processing yields, maintenance or improvement of vacuum retention during the wafer thinning process, improved wafer edge profile after the wafer thinning process, among others. The improved wafer processing yields in turn ensure and improve the performance and yield of semiconductor wafers.

[0018] 1A and 1B are cross-sectional and plan views, respectively, of an exemplary semiconductor wafer according to some embodiments. The semiconductor wafer 100 includes a substrate 102 and an array of semiconductor dies 104 formed on the substrate 102. The semiconductor wafer 100 can include a top surface 102A and a bottom surface 102B. The semiconductor dies are areas of the top surface 102A of the semiconductor wafer 100 where integrated circuits are arranged together. One type of semiconductor wafer has a circular circumference and is truncated by a flat edge called the wafer flat. As shown in FIGS. 1A and 1B, the semiconductor wafer 100 includes a wafer flat 113 located within the perimeter region 108. During fabrication, the positions of the semiconductor dies are referenced with respect to the wafer flat and the wafer center. Thus, the wafer flat 113 is often a reference for the semiconductor wafer 100 and is used by equipment to precisely place the semiconductor wafer 100 in a desired location. In some embodiments, the semiconductor dies 104 extend into the body of the substrate 102. In some embodiments, the semiconductor die 104 is formed on the top surface of the substrate 102, as shown in FIG. 1A. The semiconductor wafer 100 includes a device region 106 in which the die 104 is positioned, and a ring-shaped peripheral region 108 surrounding the device region 106. In some embodiments, the peripheral region 108 does not include any semiconductor die. In some embodiments, the peripheral region 108 may include dummy dies to maintain processing uniformity and not include active devices. The peripheral region 108 may include a wafer edge 110 that physically connects the top and bottom surfaces of the semiconductor wafer 100, and the wafer edge 110 extends in a substantially vertical direction (e.g., z-direction). In some embodiments, the wafer edge 110 may be a smooth plane that is substantially perpendicular to the top or bottom surface of the wafer 100. In some embodiments, at least a portion of the wafer edge 110 may be a curved surface. However, the wafer edge 110 may also include various defects that may compromise the structural integrity of the semiconductor wafer during fabrication operations, such as a wafer thinning process.

[0019] 2A-2B are enlarged views of the wafer edge region 112 of FIG. 1, each showing various wafer edge profiles of the wafer edge 110 according to some embodiments. FIG. 2A shows a standard wafer edge without defects. As shown in FIG. 2A, the wafer edge 110 is a substantially smooth surface that continuously connects the top surface 102A and the bottom surface 102B of the wafer 100. In some embodiments, the wafer edge 110 can have a curved profile along the vertical direction (e.g., z-direction). In some embodiments, the wafer edge 110 can have a substantially straight profile along the vertical direction (not shown in FIG. 2A). FIGS. 2B-2D show an exemplary edge defect 203 that may occur on or near the wafer edge 110. The edge defect 203 shown in FIGS. 2B-2D may be caused by the accidental removal (e.g., chipping) of a portion of the wafer edge 110. In some embodiments, the edge defect 203 may result from the wafer fabrication process. 2B and 2C show edge defects 203, such as single-step and multi-step step defects, respectively. FIG. 2D shows an edge defect 203 having an irregularly shaped profile. Each edge defect 203 shown in FIGS. 2B-2D may have a defect depth t measured vertically from the wafer top surface 102A. The defect depth t may vary based on the type and severity of the edge defect 203. In some embodiments, the ratio A of the defect depth t to the substrate thickness T may be about 1% to about 80%. For example, the ratio A of t / T may be about 1% to about 20%, about 20% to about 50%, about 50% to about 80%, or any suitable ratio. In some embodiments, the ratio A may be less than about 1% or greater than about 80%. In some embodiments, the edge defect 203 may extend to near the wafer backside 102B, which is not shown in FIGS. 2A-2D for simplicity.

[0020] FIG. 3 illustrates a semiconductor wafer mounted in a wafer thinning apparatus during a wafer thinning process according to some embodiments. In some embodiments, the wafer thinning apparatus can be a rotary backgrinder or a CMP tool. The rotary backgrinder can include, for example, a chuck 306 and a vacuum channel 308 embedded in the chuck 306. The chuck 306 can be configured to rotate about an axis 307 at a preset rotational speed ω. The wafer 300 can include a substrate 302 and a semiconductor die 304 formed on a wafer front surface 302A. The wafer 300 can also include an edge defect 303 formed proximate to the periphery of the substrate 302. In some embodiments, the substrate 302, the edge defect 303, and the semiconductor die 304 are similar to the substrate 102, the edge defect 203, and the semiconductor die 104 shown in FIGS. 1 and 2A-2D, respectively, and will not be described in detail herein for simplicity. The front side 302A of the wafer 300 can be attached to a protective tape 314, which is mounted on the chuck 306 using negative pressure generated by a vacuum channel 308. The vacuum channel 308 can be coupled to one or more vacuum sources (e.g., rough pumps), but such vacuum sources are not shown for simplicity. In some embodiments, the protective tape 314 can be a backgrind (BG) tape used to protect the wafer surface during a backgrind process. The protective tape 314 can conform to the contours of the front side 302A, including the surface of the edge defects 303. A grinding process 310 can be applied to the back side 302B of the substrate 302 to reduce the thickness of the substrate 302. During the grinding process, a backgrinder cup wheel 330 is pressed against the back side 302B and rotated at a nominal rotational speed. The relative lateral motion between the back-grinder cup wheel 330 and the wafer 300 , as well as the downward pressure from the back-grinder cup wheel 330 , allows for uniform removal of material from the substrate 302 .However, the downward pressure from the backgrinder cup wheel 330 can exacerbate the edge defect 303, potentially resulting in a crack 312 that extends into the bulk body of the substrate 302. The crack 312 can compromise the structural integrity of the substrate 302, which can lead to wafer failure and reduced fabrication yields.

[0021] 4A and 4B show a partially repaired semiconductor wafer before a wafer thinning process. FIGS. 4A and 4B are cross-sectional and plan views, respectively, of a semiconductor wafer including a substrate 402, an edge defect 403, and a semiconductor die 404. Other suitable structures may be included on the semiconductor wafer 400, but are not shown for simplicity. The semiconductor wafer 400 may include a device region 406 and a ring-shaped peripheral region 408 surrounding the device region 406. The edge defect 403 is formed in the peripheral region of the wafer 400 located between the wafer edge and the semiconductor die 404. The above-mentioned structures of the semiconductor wafer 400 may be similar to those shown in FIGS. 1A-1B, 2A-2D, and 3, respectively, and will not be described in detail herein for simplicity. The semiconductor wafer 400 may also include a wafer repair region 420 formed in the peripheral region 408. The wafer repair region 420 is positioned in the peripheral region 408 between the edge defect 403 and the semiconductor die 404. The wafer repair region 420 can allow for mechanical separation between the edge defects 403 and the device region 406, so that the edge defects 403 do not propagate into the device region 406 during the wafer thinning process. In some embodiments, the wafer repair region 420 can be a trench formed by an invasive method, such as removing a portion of material from the substrate 402. For example, the trench can be formed by mechanical dicing techniques (e.g., with a dicing blade) and by partially dicing the wafer along the wafer circumference (e.g., not penetrating the entire thickness of the wafer). In some embodiments, the wafer repair region 420 can be formed by a patterning and etching process. In some embodiments, the wafer repair region 420 can also be formed by altering material properties through various non-invasive methods, such as stealth laser dicing, which forms a modified layer in the wafer by focusing a laser beam into the wafer.During the stealth laser dicing process, a focused infrared laser beam penetrates the backside of the semiconductor wafer, causing a very localized short-term melting, converting one type of material to another type of material, and surrounding it with an area of ​​concentrated stress and microcracks. For example, the infrared laser beam can locally convert a crystalline silicon material to a polysilicon material. The infrared laser can be sequentially focused at different depths in the substrate, thus forming vertical planes of stacked modified material. These subsurface modified layers result in a weak cleave plane that essentially runs along the wafer circumference, thereby enabling mechanical separation in the vertical direction (e.g., z-direction). During the wafer thinning process, a portion of the semiconductor wafer 400 containing edge defects 403 can be cut from another portion of the semiconductor wafer 400 containing the semiconductor die 404, either through a trench or by following an induced and controlled crack.

[0022] The wafer repair region 420 can be formed from the front surface 402A of the wafer 400 and has a repair depth d measured from the wafer front surface 402A. In some embodiments, the repair depth d is equal to or greater than the defect depth t, such that when the semiconductor wafer 400 is thinned from the wafer back surface 402B, the back grinder cup wheel of the wafer thinning apparatus contacts the wafer repair region 420 before making contact with the wafer defect 403. In some embodiments, the ratio B of the repair depth d to the substrate thickness T can be about 1% to about 80%. For example, the ratio B of d / T can be about 1% to about 20%, about 20% to about 50%, about 50% to about 80%, or any suitable ratio. In some embodiments, the ratio B can be less than about 1% or greater than about 80%. Lowering the ratio B can provide the benefit of greater mechanical strength of the wafer 400, especially in the peripheral region 408. In some embodiments, the ratio B of d / T can be greater than the ratio A of t / T described above with reference to FIGS. 2A-2D. In some embodiments, the repair depth d is greater than or equal to the defect depth t. For example, the ratio C of t / d (i.e., the defect depth t to the repair depth d) can be about 50% to about 100%. In some embodiments, the ratio C can be about 50% to about 70%, about 70% to about 85%, about 85% to about 100%. A lower value of the ratio C can ensure that the repair depth d exceeds the defect depth t, while a higher value of the ratio C can provide the benefit of a smaller penetration depth of the wafer repair region 420, thereby reducing fabrication costs. As discussed above, the wafer flat is used by various fabrication equipment to identify the wafer position and wafer orientation, and therefore maintaining the wafer flat is essential for wafer fabrication. Thus, having the wafer repair region 420 only partially penetrate the substrate 402 can provide the benefit of maintaining the wafer flat 413 intact prior to the wafer thinning process. In contrast, a ring-shaped trench that penetrates the entire thickness of the substrate 402 would potentially remove the wafer flat 413, resulting in expensive equipment modifications to accommodate the non-flat wafer.The wafer repair area 420 can have a width w that is less than or equal to the separation distance between the edge defect 403 and the active area 406. In some embodiments, the width w can be about 20% to about 80% of the repair depth d. For example, the ratio of the width w to the repair depth d can be about 20% to about 40%, about 40% to about 60%, about 60% to about 80%, or any suitable ratio.

[0023] FIG. 5 is a cross-sectional view of a repaired semiconductor wafer mounted in a wafer thinning apparatus at the beginning of a wafer thinning process according to some embodiments. Wafer 500 includes substrate 502, edge defect 503, semiconductor die 504, and wafer repair region 520. Each of the above-mentioned structures of wafer 500 can be similar to the structures of wafer 400 shown in FIGS. 4A-4B. Wafer repair region 520 shown in FIG. 5 can be a trench formed by removing a ring-shaped portion of material from substrate 502. In some embodiments, the removed portion can also be a variation of the ring-shaped structure. For example, the removed portion can be partially ring-shaped along the circumference of the ring shape (e.g., an area of ​​the wafer is not removed along the curvature of the ring-shaped removed portion). In some embodiments, one or more breaks can be located proximate to the wafer flat. In some embodiments, the removed portion can also be an elliptical structure. In some embodiments, wafer repair region 520 can also be any suitable repair that can provide a barrier that allows for physical separation between edge defect 503 and semiconductor die 504 during the wafer thinning process. The wafer 500 is flipped upside down and its front surface 502A is mounted on a protective tape 514. The wafer 500 is then positioned on a chuck 506 using negative pressure provided by a vacuum channel 508. A grinding process 510 can be applied to the back surface 502B to reduce the thickness of the wafer 500. During the grinding process 510, a back grinder cup wheel 530 is pressed against the substrate 502 and rotated at a nominal rotational speed. Similar to the grinding process shown in FIG. 3, the relative lateral movement between the back grinder cup wheel 530 and the wafer 500, as well as the downward pressure from the back grinder cup wheel 530, can remove material from the substrate 502.

[0024] FIG. 6 is a cross-sectional view of a repaired semiconductor wafer mounted in a wafer thinning apparatus during a wafer thinning process according to some embodiments. As the grinding process 510 of FIG. 5 progresses and the backgrinder cup wheel 530 moves further down (e.g., in the z-direction), the thickness of the substrate 502 is reduced and a wafer repair region 520 is exposed. The wafer repair region 520 is configured to allow for physical separation between the edge defect 503 and the semiconductor die 504 when the wafer repair region 520 is exposed during the grinding process 510. For example, when the wafer repair region 520 is exposed, the wafer portion 503A including the semiconductor die 504 is physically separated from the wafer portion 503B including the edge defect 503. Thus, even if the edge defect 503 may have caused a crack 612 during the grinding process 510, the crack 612 is not likely to propagate to the bulk of the substrate 502 on which the semiconductor die 504 is formed.

[0025] Wafer repair provides several benefits. First, the wafer fabrication yield is improved by limiting the propagation of defects. The structural integrity of the wafer active area can be maintained since defects generated by edge defects during grinding cannot propagate into the bulk substrate. Second, the amount of debris can be reduced during the wafer grinding process. Because the wafer portion 503B is removably attached to the wafer portion 503A before the grinding process and separated from the wafer portion 503A in a controlled manner via the wafer repair area 520, only a minimal amount of debris is generated compared to the debris or wafer chipping that may be generated during the grinding process 310 of FIG. 3 where the semiconductor wafer 300 is thinned. Third, the vacuum quality at the circumference of the wafer 500 during the grinding process can be improved. For example, because the shape of edge defect 503 is irregular, protective tape 514 attached to wafer portion 503B does not need to contact vacuum channels 508 before grinding process 510, but can contact vacuum channels 508 after wafer portion 503B is separated from wafer portion 503A.

[0026] 7 and 8 illustrate an exemplary wafer repair system according to some embodiments. FIG. 9 is a flow diagram of a method 900 illustrating an exemplary method of processing a semiconductor wafer according to some embodiments. By way of example and not limitation, the wafer repair process of the method 900 can be performed in the wafer repair station 700 and the wafer repair system 800 illustrated in FIG. 7 and FIG. 8, respectively. The present disclosure is not limited to this description of operations. Conversely, other operations are within the spirit and scope of the present disclosure. It should be understood that additional operations can also be performed. Moreover, not all operations are required to perform the disclosure provided herein. Moreover, some of the operations can be performed simultaneously or in a different order than illustrated in FIG. 9. In some implementations, one or more other operations can be performed in addition to or instead of the operations described herein. For illustrative purposes, the method 900 is described with reference to the embodiments of FIG. 1-8. However, the method 900 is not limited to these embodiments. For illustrative purposes, the method 900 is described with reference to a wafer repair station for a single wafer. Based on the disclosure herein, the method 900 can be equally applied to a batch wafer repair station capable of processing multiple wafers at one time. Both single wafer station and batch station configurations are within the spirit and scope of the present disclosure.

[0027] Method 900 begins with operation 910 according to some embodiments where a wafer is transferred to a wafer repair chamber of wafer repair station 700. For example, wafer 710 may be transferred to wafer repair chamber 702 via a transfer module having a robotic arm (not shown). Wafer repair chamber 702 may be a module within a wafer processing cluster tool and may further include additional wafer processing stations, modules, and equipment appropriate for its operation.

[0028] The wafer repair station 700 can be a component of a processing cluster tool (not shown in FIG. 7 for simplicity). The processing cluster tool can include additional components, such as modules (e.g., transfer modules and dicing stations), robotic arms, pumps, exhaust lines, heating elements, gas and chemical delivery lines, controllers, valves, and external and internal electrical connections to other components of the cluster tool (e.g., computer units, chemical analyzers, motor controllers, mass flow controllers, pressure controllers, valves, and pumps). Such additional components are not depicted in FIG. 7 but can be combined with the illustrated components without departing from the spirit and scope of the present disclosure.

[0029] The wafer repair station 700 may include a process chamber 702, a wafer holder 719, a spin base 725, a repair mechanism 730, an arm 735, and a motor 740. The repair mechanism 730 may be any suitable wafer repair device capable of repairing physical or chemical characteristics of a selected area of ​​a semiconductor wafer. The wafer repair station 700 may further include detectors 780a-780c positioned about the process chamber 702 to detect wafer characteristics, such as characteristics of wafer edge defects. The processing system 790 may receive the detected wafer characteristics via a communication channel 792 and generate a wafer profile. In some embodiments, the wafer profile may include metrology data for the wafer. For example, the wafer profile may include dimensions, material composition, types and locations of defects, and any other suitable information customized for each individual wafer. In some embodiments, the wafer profile may be selected from a database of wafer profiles based on characteristics of the individual wafer.

[0030] 9, the method 900 begins with operation 910 according to some embodiments, which includes transferring a wafer to a wafer repair chamber of a wafer repair station. As shown in FIG. 7, the wafer 710 is positioned in the processing chamber 702. The wafer 710 can be secured onto a wafer holder 719 using a clamp, a vacuum chuck, an adhesive tape, or the like. In some embodiments, the wafer 710 can include a semiconductor die 704 formed on a front side of the wafer 710. The wafer holder 719 is further attached to a spin base 725 of the wafer repair station 700. In some embodiments, the wafer holder 719 can rotate the semiconductor wafer 710 via the spin base 725 at different rotational speeds during the wafer repair process. In some embodiments, the semiconductor wafer 710 can be rotated at any suitable rotational speed. For example, the semiconductor wafer 710 can be rotated at about 300 rpm, 500 rpm, 1000 rpm, 2000 rpm, or any suitable rotational speed.

[0031] The method 900 proceeds to operation 920 according to some embodiments, which includes measuring wafer characteristics using one or more detectors. With reference to FIG. 7, one or more detectors 780a-780c may be positioned around the wafer repair chamber 702 to detect and measure wafer characteristics, such as characteristics of wafer edge defects. For example, the detectors 780a-780c may be configured to detect whether wafer edge defects are present around the circumference of the semiconductor wafer 710. In response to detecting the wafer edge defects, the detectors 780a-780c proceed to measure various characteristics of the wafer edge defects, such as location, defect depth, width, and type of the wafer edge defects. Examples of wafer edge defects may include wafer edge defects 203, 303, 403, and 503 shown in FIGS. 2A-2D and 3-5, respectively. In some embodiments, the detectors 780a-780c are positioned around the sidewalls and / or top / bottom walls of the wafer repair chamber 702. Data characteristic of the detected wafer edge defects can be transmitted to a processing system 790, which can determine whether the wafer edge defects are below a variation threshold, e.g., whether the detected wafer edge defects are excessive (e.g., extend into the semiconductor die 704). In response to the wafer edge defects not being excessive, the processing system 790 can proceed to create a wafer correction profile for forming a wafer correction region in the semiconductor wafer 710. In response to the wafer edge defects being excessive, the processing system 790 can proceed to alert a user or select a die to sacrifice. The detectors 780a-780c can also determine. For example, three detectors can be positioned around the wafer correction chamber 702, with the detectors facing the sidewall and top wall of the wafer correction chamber 702. In some embodiments, viewports can be installed on the sidewall and top wall of the wafer correction chamber 702 and aligned with the respective detectors such that the interior of the wafer correction chamber 702 is visible to the respective detectors. In some embodiments, the detectors 780a-780c can be located within the wafer modification chamber 702.In some embodiments, the detectors 780a-780c can be configured to detect wafer characteristics of the semiconductor wafer 710, such as, for example, thickness, width, and type of wafer edge defects on the semiconductor wafer 710. In some embodiments, the detectors 780a-780c can be located in a detector chamber configured to detect wafer characteristics before the semiconductor wafer 710 is transported into the wafer repair chamber 702. In some embodiments, the detectors 780a-780c can be laser thickness sensors, optical profilers, step profilers, multi-wavelength ellipsometers, ion beam analyzers, and / or any other suitable detectors, or combinations thereof. In some embodiments, the detectors 780a-780c can each be a charge-coupled device (CCD) camera, which is a component of a CCD-based image detection system. In some embodiments, photocells or other such automated detection devices that detect images of areas presented to the photocells can also be used. In some embodiments, the detectors 780a-780c can include at least one CCD monochrome or color camera, depending on the inspection process. Thus, detectors 780a-780c can each be configured to create one or more high resolution images of the wafer and provide the high resolution images to a user or processing system.

[0032] Referring to FIG. 9, the method 900 proceeds to operation 930 according to some embodiments, which includes determining a wafer profile based on the measured wafer characteristics. As shown in FIGS. 7 and 8, the processing system 790 can be electrically connected to the detectors 780a-780c and the wafer repair chamber 702 via a communication channel 792. The processing system 790 can include processing circuitry and software to analyze signals produced by the detectors 780a-780c and generate a wafer profile using those signals. The communication channel 792 can be any suitable wiring, fiber optic, or wireless technology for transmitting signals. The generated wafer profile can be suitable for viewing by a user. For example, the resulting wafer profile can be displayed on the processing system 790 or a display device, such as, for example, a computer monitor located at an operator workstation. The generated wafer profile can include information such as the location, depth, width, and type of wafer edge defects within the peripheral region of the semiconductor wafer.

[0033] Based on the wafer profile, the processing system 790 can determine a suitable wafer correction recipe or processing conditions for the wafer. For example, the wafer correction recipe can depend on the defect depth of the wafer edge defects. Specifically, the processing system 790 can set the wafer correction depth to be equal to or greater than the edge defect depth. Examples of the defect depth and correction depth can include the defect depth t and correction depth d shown in FIGS. 2A-2D and 3-5. The wafer correction recipe can also include information related to the location of the wafer correction. For example, the wafer correction can be positioned within a peripheral region along the circumference of the wafer. The detector can be operated by the processing system 790 to perform a one-time measurement of the wafer characteristics or can be operated to continuously measure the wafer characteristics at predetermined intervals during the wafer processing. Thus, the detector can provide continuous monitoring of the wafer processing and transmit the detected results to the processing system 790, so that the processing system 790 can adjust the processing recipe or conditions in real time during the wafer correction process.

[0034] In some embodiments, the processing system 790 can be configured to receive extremely large data sets (e.g., big data) and computationally analyze them to reveal patterns, trends, and associations related to wafer edge defects and the resulting processed wafers. In particular, the processing system 790 can receive collected data sets from a detector that represent the shape, thickness, composition, roughness, and any other suitable characteristics of the wafer edge of the wafer, and analyze the data sets with reference to a wafer rework process. The data sets can be used as feedback by the processing system 790 to fine-tune the wafer rework recipe in real-time or after processing so that the wafer rework process can be continuously improved, resulting in improved wafer processing uniformity and device yields.

[0035] The processing system 790 can be configured to perform various additional or alternative analytical tasks, such as analyzing any suitable signal, processing statistics, scheduling tasks, generating an alarm signal, generating further control signals, etc. For example, upon detecting excessive wafer edge defects, the processing system 790 can be configured to generate an alarm signal to alert a user. The processing system 790 can be further configured to perform a series of scheduled tasks within the wafer repair chamber to reduce wafer edge defects. In some embodiments, an example of excessive wafer edge defects can include wafer edge defects that extend into an active device area of ​​the wafer. In response to detecting excessive wafer edge defects, the processing system 790 can determine appropriate next steps, such as identifying semiconductor dies that may be affected by the wafer edge defects and adjusting the path of the wafer repair accordingly. Various other wafer repair parameters can include, for example, the travel speed, position, and angle of the corrector 730, the rotation speed of the semiconductor wafer 710, combinations thereof, and any other suitable processing parameters. The processing system 790 can be located adjacent to the wafer repair chamber 702 so that, for example, an operator can easily access both the processing system 790 and the wafer repair chamber 702 to determine wafer edge defects and the wafer repair process to correct any problems that may arise. Alternatively, in some embodiments, the processing system 790 can be located in a remote location, such as a process command center that can monitor various images from various processing stations or wet benches together.

[0036] 9, the method 900 proceeds to operation 940 according to some embodiments, which includes performing a wafer correction process on the semiconductor wafer based on the measured wafer characteristics. As shown in FIG. 7, a wafer correction 720 may be formed on a wafer 710 according to one or more wafer correction recipes.

[0037] The wafer repair station 700 includes a repairer 730 mounted on an arm 735. The processing system 790 can instruct the repairer 730 to perform a wafer repair process based on the wafer repair profile. In some embodiments, the repairer 730 can be a dicing blade configured to perform a partial dicing process, such as removing a portion of material from the wafer 710, rather than penetrating the entire thickness of the wafer. For example, the dicing blade can penetrate into the wafer 710 to a preset depth (e.g., repair depth d shown in FIGS. 4A and 4B) that is less than the wafer thickness, forming a ring-shaped trench that is substantially concentric with the ring-shaped peripheral region of the wafer 710. In some embodiments, the trench extends into the wafer 710 but does not completely penetrate the entire thickness of the wafer. In some embodiments, the repairer 730 can be a set of laser focusing lenses that focus an infrared laser beam to a focal point within the bulk substrate of the wafer 710. Various parameters of the modifier 730 can be adjusted to perform a partial stealth laser dicing process, such as penetrating a portion of the wafer 710 but not the entire thickness. For example, the power, frequency, depth of focus, number of passes, travel distance, and any suitable parameters can be adjusted based on the physical and chemical properties of the material forming the wafer 710. Increasing the laser frequency can provide the benefit of a smoother cleave plane. Additionally, increasing the laser power can provide the benefit of more microcracks being formed. In some embodiments, the modifier 730 can provide an infrared laser having a power of about 85 W and a frequency of about 60 kHz to form a modification layer in the semiconductor wafer 710 when the substrate is formed using single crystal silicon. The modifier 730 can be moved laterally along the x-direction (e.g., along direction 732) by a motor 740 via an arm 735, such that the modifier 730 can be positioned directly above any suitable area on the semiconductor wafer 710. For example, the modifier 730 can be positioned above the peripheral area of ​​the wafer 710.An example of a wafer peripheral region may include the peripheral region 408 shown in FIGS. 4A and 4B. In some embodiments, the modifier 730 may make two or more passes through the desired region. The modifier 730 may also move vertically in the y direction (e.g., along direction 734) so ​​that the height between the semiconductor wafer 710 and the modifier 730 may be adjusted before, during, or after the wafer correction process. For example, moving the modifier 730 vertically may adjust the laser focus or blade cutting depth of the modifier 730. In some embodiments, the modifier 730 may also rotate about the vertical axis 711 of the wafer 710 so that the modifier 730 may form a substantially concentric ring-like modified portion with the wafer 710. For example, the modifier 730 may be configured to rotate 90°, 180°, 360°, or any suitable range. In some embodiments, the modifier 730 may conform to the circumferential contour of the wafer 710. In some embodiments, other suitable parameters of the modifier 730 may also be adjusted over the duration of the process based on the detected wafer profile and processing conditions. In some embodiments, adjustable parameters include, but are not limited to, the height between the modifier 730 and the semiconductor wafer 710, the orientation of the modifier 730 relative to the top surface of the semiconductor wafer 710, the speed of movement of the modifier 730, the path of movement of the modifier 730, any suitable parameters, and / or combinations thereof.

[0038] FIG. 8 is a diagram of a wafer repair system 800 according to some embodiments. The wafer repair system 800 can include, among other components, a processing system 790, a repair controller 850, an arm controller 860, and a chamber controller 870. The wafer repair system 800 can further include other suitable components, such as additional detectors, sensors, pumps, valves, etc., but for simplicity, these structures are not shown in FIG. 8. In some embodiments, the repair controller 850, the arm controller 860, and the chamber controller 870 can include any suitable computer control modules, such as valves, motors, or wafer stages. In some embodiments, the controllers described above can control various process parameters based on the generated wafer profile and monitoring of the wafer repair process. In some embodiments, the repair controller 730 can be controlled by the repair controller 850 to provide an infrared laser for stealth dicing. In some embodiments, the repair controller 730 can be controlled by the repair controller 850 to form trenches in the wafer 710 using a rotating dicing blade. In some embodiments, the modifier controller 850 can control the orientation of the modifier 730 relative to the top surface of the semiconductor wafer 710, the rotational speed of the dicing blade, the laser power and frequency, and any suitable parameters. In some embodiments, the arm controller 860 can be operated to move the modifier 730 to be positioned over different areas of the wafer 710. In some embodiments, the arm controller 860 can also control the height between the modifier 730 and the semiconductor wafer 710, the lateral movement speed of the modifier 730, the movement path of the modifier 730, among other parameters. The chamber controller 870 can be used to control various parameters of the wafer modifier chamber 702, such as the chamber pressure, temperature, and / or any suitable parameters. The detector 780 and processing system 790 can determine a wafer profile for a wafer transported into the wafer modifier chamber 702.Detector 780 may be detectors 780a-780c of FIG. 7 that measure various characteristics of the wafer. For example, detector 780 may determine the characteristics of the wafer edge and detect the presence of a wafer edge defect. If a wafer edge defect is detected, detector 780 may further detect the location, depth, width, type, or any suitable characteristics of the wafer edge defect and transmit the data to processing system 790 for further processing, such as creating a wafer correction profile. Processing system 790 may receive the measured characteristics of the wafer to determine a wafer profile and use the wafer profile to correct the wafer accordingly. Specifically, processing system 790 may create a recipe to form a wafer correction region based on the wafer profile. For example, processing system 790 may be configured to create the cross-sectional views and measurements of the wafer edge defects shown in FIGS. 2B-2D. As a result, processing system 790 may control corrector 730 via arm controller 850 to form wafer correction region 720 in wafer 710.

[0039] 9, the method 900 proceeds to operation 950 according to some embodiments, which includes performing a wafer thinning process on the modified semiconductor wafer based on the measured wafer characteristics. One example of performing a wafer thinning process can include the grinding process 510 performed on the wafer 500 shown in FIGS. 5 and 6, which will not be described in detail herein for simplicity.

[0040] Various embodiments described herein are directed to systems and methods for improving wafer processing yields during a wafer thinning process. More particularly, the present disclosure is directed to a wafer processing system configured to determine a wafer profile prior to a wafer thinning process and modify the wafer accordingly, such that each wafer is customized according to the wafer profile. For example, the wafer processing system identifies defects located in a peripheral region of the wafer and modifies a portion of the peripheral region to create a barrier that prevents the defects from propagating into a device region of the wafer during the wafer thinning process. In some embodiments, modifying the portion of the peripheral region can include partially cutting the wafer along the perimeter and forming a trench along the perimeter. In some embodiments, modifying the portion of the peripheral region can include modifying a physical attribute of a portion of the wafer by a non-invasive method, such as stealth laser dicing.

[0041] In some embodiments, a method for processing a wafer includes measuring one or more wafer characteristics of a wafer using a plurality of detectors. The wafer includes a device region and a peripheral region. The method also includes determining a wafer correction profile for the wafer based on the measured one or more wafer characteristics. The method further includes correcting a ring-shaped portion of the wafer in the peripheral region using the wafer correction profile. The corrected ring-shaped portion has a penetration depth less than a thickness of the wafer. The method further includes performing a wafer thinning process on the wafer.

[0042] In some embodiments, a method for processing a wafer includes detecting wafer edge defects at a circumference of the wafer. The wafer has a front side and a back side and has an array of semiconductor dies on the front side. The method also includes measuring one or more characteristics of the wafer edge defects, the one or more characteristics including at least a defect depth. The method also includes modifying a portion of the wafer between the array of semiconductor dies and the wafer edge defects from the front side. The modified portion has a penetration depth measured from the front side, the penetration depth being less than the defect depth. The method further includes performing a wafer thinning process on the back side of the wafer.

[0043] In some embodiments, the wafer processing system includes one or more detectors configured to determine one or more characteristics of the wafer. The wafer has a device region and a perimeter region surrounding the device region. The wafer processing system further includes a wafer correction apparatus and a processing system. The processing system is configured to receive the one or more characteristics and determine a wafer correction profile based on the one or more wafer characteristics. The processing system is further configured to correct a ring-shaped portion of the wafer within the perimeter region using the wafer correction profile. The corrected ring-shaped portion has a penetration depth less than a thickness of the wafer.

[0044] Thus, the above description of the specific embodiments fully reveals the general nature of the present disclosure, which can be easily modified and / or adapted by others to various applications without undue experimentation by applying knowledge within the scope of the art without departing from the general concept of the present disclosure. Therefore, such adaptations and modifications are intended to be within the meaning and range of equivalents of the disclosed embodiments based on the teaching and guidance presented herein. It should be understood that the terms or phrases in this specification are for the purpose of description and not limitation, and thus the terms or phrases in this specification should be interpreted in light of the teaching and guidance by those skilled in the art.

[0045] The embodiments of the present disclosure have been described above with the help of functional building blocks illustrating examples of implementations of specified functions and relationships thereof. The boundaries of these functional building blocks have been arbitrarily defined herein for convenience of description. Alternative boundaries may be defined so long as the specified functions and relationships thereof are appropriately performed.

[0046] The Overview and Abstract sections describe one or more exemplary embodiments of the disclosure but not all of the disclosure contemplated by the inventors, and are thus not intended to be limiting of the scope of the disclosure and the appended claims in any way.

[0047] The breadth and scope of the present disclosure should not be limited by any of the above-described exemplary embodiments, but should be defined only in accordance with the following claims and their equivalents. [Explanation of symbols]

[0048] 100 Semiconductor Wafers 102 Substrate 102A Top 102B Bottom, Wafer Backside 104 Semiconductor Die 106 Device Area 108 Surrounding Area 110 Wafer Edge 112 Wafer edge area 113 Wafer flat part 203 Edge Defects 300 wafers 302 Substrate 302A Front 302B back side 303 Edge Defects 304 Semiconductor Die 306 Chuck 307 Axis 308 Vacuum Channel 310 Grinding Process 312 Crack 314 Protective Tape 330 Back Grinder Cup Wheel 400 Semiconductor Wafers 402 Substrate 402A Wafer Front 402B Wafer backside 403 Edge Defect 404 Semiconductor Die 406 Device Area 408 Surrounding Area 413 Wafer flat part 420 Wafer Repair Area 500 wafers 502 Substrate 502A front 502B back 503 Edge Defect 503A: Wafer portion including semiconductor die 504 503B Wafer portion including edge defect 503 504 Semiconductor Die 506 Chuck 508 Vacuum Channel 510 Grinding Process 514 Protective Tape 520 Wafer Repair Area 530 Back Grinder Cup Wheel 612 Crack 700 Wafer Repair Station 702 Wafer repair chamber, processing chamber 704 Semiconductor Die 710 Wafer 711 Vertical axis 719 Wafer Holder 720 Wafer Repair, Wafer Repair Area 725 Spinbase 730 Corrector 732 directions 734 directions 735 Arm 740 Motor 780a Detector 780b detector 780c detector 790 Processing System 792 Communication Channels 800 Wafer Repair System 850 Corrector Controller 860 Arm Controller 870 Chamber Controller A is the ratio of defect depth t to substrate thickness T B Ratio of correction depth d to substrate thickness T C t / d ratio d Correction depth T Board thickness t defect depth w width ω rotation speed

Claims

1. 1. A method for processing a wafer, comprising: measuring one or more wafer characteristics; determining a wafer modification profile for the wafer based on the one or more wafer characteristics; modifying a portion of the wafer from a first surface of the wafer using the wafer modification profile, the modified portion having a penetration depth less than a thickness of the wafer; performing a wafer thinning process on a second surface of the wafer, the second surface being opposite the first surface of the wafer; measuring the one or more wafer characteristics includes determining one or more characteristics of edge defects within a peripheral region of the wafer; wherein determining the one or more characteristics of the edge defect includes measuring a defect depth of the edge defect; the step of determining the wafer modification profile includes setting the penetration depth equal to or greater than the defect depth; the step of repairing the portion of the wafer includes forming a wafer repair area between a device area and an edge defect formed on a circumference of the wafer. method.

2. 2. The method of claim 1, wherein said forming said wafer repair region comprises forming a ring-shaped trench substantially concentric with said wafer.

3. 3. The method of claim 2, wherein the step of forming the ring-shaped trench comprises performing a dicing process that penetrates partially into the thickness of the wafer.

4. 2. The method of claim 1, wherein the forming the wafer repair area comprises performing a stealth laser dicing process on the wafer.

5. 2. The method of claim 1, wherein the step of performing the wafer thinning process comprises performing a back grind process on the second surface of the wafer.

6. said step of performing said background grinding process further comprising: pressing a backgrinder cup wheel against the second surface of the wafer; rotating the backgrinder cup wheel to remove material from the wafer such that the backgrinder cup wheel contacts the repaired portion before contacting a wafer edge defect; and mechanically isolating, in the repaired portion, a device area from a surrounding portion of the wafer that contains the wafer edge defect.

7. 1. A method for processing a wafer, comprising: detecting wafer edge defects around a circumference of the wafer, the wafer including a front side and a back side and comprising an array of semiconductor dies on the front side; measuring one or more characteristics of the wafer edge defects, the one or more characteristics including at least a defect depth; repairing a portion of the wafer between the array of semiconductor dies and the wafer edge defect from the front surface, the repaired portion comprising a penetration depth measured from the front surface, the penetration depth being less than the defect depth; performing a wafer thinning process on the backside of the wafer; the step of modifying the portion of the wafer from the front side comprises: forming a ring-shaped trench substantially concentric with the wafer, partially penetrating the wafer; or forming a ring-shaped modified layer using stealth laser dicing, the ring-shaped modified layer being substantially concentric with the wafer; method.

8. 8. The method of claim 7, wherein the step of performing the wafer thinning process comprises performing a back grind process on the back side of the wafer.

9. said step of performing said background grinding process further comprising: pressing a backgrinder cup wheel against the backside of the wafer; rotating the backgrinder cup wheel to remove material from the wafer such that the backgrinder cup wheel contacts the repaired portion before contacting the wafer edge defect; and c) mechanically isolating, in the repaired portion, the array of semiconductor dies from a peripheral portion of the wafer that contains the wafer edge defects.

10. one or more detectors configured to determine one or more characteristics of a wafer, the wafer including a device region and a surrounding region surrounding the device region; A wafer repair device; a processing system, the wafer includes an edge defect formed on a circumference of the wafer, and the one or more characteristics include at least a defect depth of the edge defect; the processing system comprising: receiving the one or more characteristics; determining a wafer correction profile based on the one or more wafer characteristics, and setting a penetration depth in determining the wafer correction profile to be equal to or greater than the defect depth; configured to instruct the wafer repair device to repair a ring-shaped portion of the wafer within the peripheral region using the wafer repair profile, the repaired ring-shaped portion having the penetration depth less than a thickness of the wafer; the ring-shaped portion of the wafer is substantially concentric with the wafer and is formed between the edge defect and the device region; modifying the ring-shaped portion of the wafer includes partially dicing the wafer along the ring-shaped portion substantially concentric with the wafer using a mechanical dicing technique or a stealth laser dicing technique. Wafer processing system.

Citation Information

Patent Citations

  • Method for manufacturing semiconductor wafer

    JP2004063883A

  • Manufacturing method of semiconductor device

    JP2007096115A

  • Processing method of wafer

    JP2020057709A