Process for manufacturing a semiconductor wafer having an epitaxial layer deposited from the vapor phase in a deposition chamber - Patents.com
By calculating corrective actions based on positional deviations of previously coated wafers, the process addresses misalignment issues in semiconductor wafer manufacturing, improving uniformity and reducing particle formation during epitaxial layer deposition.
Patent Information
- Application Number
- JP2023562281
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-04-13
- Filing Date
- 2022-03-28
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2042-03-28
AI Technical Summary
Existing methods for manufacturing semiconductor wafers with epitaxial layers suffer from non-uniform thickness in the edge region due to misalignment of the substrate wafer on the susceptor, leading to increased edge roll-off and particle formation during deposition.
A process that calculates corrective actions for substrate wafer placement on the susceptor by averaging positional deviations of previously coated wafers, particularly for the first wafer after chamber etching, to ensure precise alignment and reduce misalignment effects.
Improves epitaxial layer thickness uniformity and reduces particle formation by accurately positioning the substrate wafer on the susceptor, enhancing the edge shape and deposition quality of semiconductor wafers.
Smart Images

Figure 0007567067000001 
Figure 0007567067000002 
Figure 0007567067000003
Abstract
Description
[Technical field]
[0001] The invention relates to a process for manufacturing semiconductor wafers having epitaxial layers deposited from the gas phase in a deposition chamber. Semiconductor wafers having epitaxial layers are required for the manufacture of electronic components. The epitaxial layers are typically deposited in a deposition chamber in the form of a single wafer reactor. The substrate wafer to be coated is placed on a susceptor and deposition gases are passed through the deposition chamber at deposition temperatures over the substrate wafer which rotates together with the susceptor. [Background technology]
[0002] One quality criterion for semiconductor wafers having epitaxial layers is the uniformity of the thickness of the epitaxial layer, especially at the edge region of the semiconductor wafer.
[0003] Prior art / issue WO 2017 102 597 A1 deals in particular with the problem of improving the edge profile of a semiconductor wafer having an epitaxial layer: it has been discovered that after a typical etch (chamber etch) that is periodically performed in a deposition chamber to remove material deposited in the deposition chamber during a previous coating operation, successive subsequent coating operations result in an increased edge roll-off in a semiconductor wafer having an epitaxial layer that is subsequently produced in the deposition chamber.
[0004] JP 2016 213 218 A describes a process for manufacturing semiconductor wafers of monocrystalline silicon with an epitaxial layer made of monocrystalline silicon. It is recommended that the robot that places the substrate wafer on the susceptor of the deposition reactor is moved to a placement position where the center of the substrate wafer is not located above the center of the susceptor for corrective precept. It has been found that otherwise the substrate wafer is not located on average in the center of the susceptor during deposition of the epitaxial layer. If the substrate wafer is not located concentrically in the pocket of the susceptor during deposition of the epitaxial layer, there is a negative effect on the uniformity of the thickness of the epitaxial layer. Moreover, any such misalignment may result in the undesirable formation of particles, especially if it entails contact of the edge of the substrate wafer with the susceptor. The corrective action is derived from an average that indicates the average deviation of the position of the center of the substrate wafer from the center of the susceptor during the preceding coating operation. Linked to the corrective action is the expectation of achieving, during the coating operation, a position of the center of the substrate wafer that is closer to the center of the susceptor by the amount of the mean deviation than would be the case without the corrective action. Summary of the Invention [Problem to be solved by the invention]
[0005] The inventors of the present invention have determined that the specification of corrective actions induced solely by position deviations of the substrate wafer during a preceding coating operation should be improved. [Means for solving the problem]
[0006] The object of the invention is to provide a process for manufacturing semiconductor wafers having epitaxial layers deposited from the gas phase in a deposition chamber, comprising: removing from the deposition chamber material deposited therein during a previous coating operation by etching the deposition chamber; and coating operations carried out successively in the etched deposition chamber, the coating operations in each case comprising: The coating operation includes placing the substrate wafer on a susceptor having a circular periphery by a robot, the robot moving the substrate wafer to a placement position and placing the substrate wafer on the susceptor with corrective measures such that the center of the substrate wafer is not located above the center of the susceptor at the placement position, and the coating operation further includes: depositing an epitaxial layer on a substrate wafer to form a semiconductor wafer having an epitaxial layer; For each first substrate wafer moved by the robot to a placement position after a deposition chamber etch, an amount of corrective action is achieved by the process that corresponds to the average of the position deviations of the previously coated substrate wafers themselves, each of which is to be coated for the first time after the preceding chamber etch.
[0007] Prior to the first coating operation after the chamber etch, the conditions in the deposition chamber are such that the incident radiant energy produces a faster temperature rise than prior to the second and subsequent coating operations, resulting in a more pronounced expected misalignment of the substrate wafer, particularly for the first substrate wafer after the chamber etch, compared to the subsequently coated substrate wafers.
[0008] It is therefore proposed that the corrective measures for the first substrate wafer to be coated after chamber etching are calculated taking into account only the position deviations of the substrate wafer from the preceding coating operation, each measured on the substrate wafer itself, the first substrate wafer after chamber etching. Such substrate wafers are referred to below as substrate wafers of the first category. The corrective measures are calculated by averaging the position deviations. The term "position deviation" denotes the deviation of the position of the center of the placed substrate wafer relative to the center of the susceptor.
[0009] For the calculation of the average (arithmetic mean) preferably position deviations of at least three first category substrate wafers are used, more preferably position deviations of 5-10 such substrate wafers are used. The chamber etches respectively preceding the first category substrate wafers are preferably themselves preceded immediately by a chamber etch before coating of the first substrate wafer to be coated takes place.
[0010] It is possible in principle for each substrate wafer category to calculate independent corrective measures for the patterns of substrate wafers of the first category, however, generally speaking, it is sufficient for substrate wafers that are not the first wafer after chamber etching to calculate corrective measures based on the position deviation of the substrate wafer from a previous different coating operation that was not the first coating operation after chamber etching.
[0011] The substrate wafer on which the epitaxial layer is deposited in accordance with the present invention is a semiconductor wafer containing a dopant, and is preferably a substrate wafer made of single crystal silicon.
[0012] The invention will now be explained in more detail with reference to the drawings. [Brief description of the drawings]
[0013] [Figure 1] FIG. 1 shows, in a cross-sectional representation, an apparatus for depositing epitaxial layers from the gas phase onto a substrate wafer, with a typical configuration. [Diagram 2] FIG. 13 shows the positions of first and second average values of the position deviations of a first category of substrate wafers and a different category of substrate wafers relative to the center of a susceptor. [Diagram 3] FIG. 13 shows the distribution of centers of a first category of substrate wafers after placement on a susceptor relative to the center of the susceptor in a polar coordinate grid. [Figure 4]FIG. 13 shows the distribution of the centers of different categories of substrate wafers after placement on a susceptor relative to the center of the susceptor in a polar coordinate grid. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] DETAILED DESCRIPTION OF EXEMPLARY EMBODIMENTS OF THEINVENTION The apparatus for depositing epitaxial layers on substrate wafers shown in Figure 1 comprises a deposition chamber 3 having an upper cover 1, a lower cover 2, an upper lining 7 and a lower lining 8 enclosing a reaction space. Not depicted are the upper and lower lamp arrays present outside the deposition chamber 3. The radiant energy of the lamps brings the deposition chamber to the required temperature for gas-phase (vapor) deposition.
[0015] For the coating operation, the substrate wafer 4 is placed on the susceptor 5, which is rotatably held from below by a carrier arm. Previously, the substrate wafer is placed on the end effector of the robot and moved by the robot to a placement position. Arranged around the susceptor is a preheat ring 6. The substrate wafer 4 is placed on the susceptor 5 and after coating can be lifted from the susceptor 5 by lifting pins that pass through the susceptor 5.
[0016] For coating of the substrate wafer 4, deposition gas enters the deposition chamber 3 through an upper gas inlet opening 9 provided in the upper lining 7 and is passed along a flow direction past the substrate wafer to an upper gas outlet 11. Optionally, further lower gas inlet opening 12 and lower gas outlet 13 may be provided for passing a purge gas under the susceptor 5 to a lower gas outlet 13.
[0017] If the placement position for the robot is established such that the center of the substrate wafer is located vertically above the center of the susceptor, there is a relatively high probability that after the substrate wafer is placed, its center will not be located at the center of the susceptor. The particular reason for this are thermal stresses, which are relieved and displace the center of the substrate wafer from its intended position.
[0018] It has now been discovered that the fewer the number of coating operations completed since the last chamber etch, the greater the amount of displacement from the center of the susceptor. According to the invention, this discovery is taken into account when calculating corrective actions that jointly determine the placement position to which the robots move the substrate wafer before it is placed on the susceptor. The corrective actions are calculated for each first substrate wafer to be coated after the chamber etch by averaging from the position deviations of previously coated substrate wafers, and the position deviations used in the calculation are only the position deviations of the first category of substrate wafers, i.e. of the substrate wafer itself that is each first to be coated after the chamber etch.
[0019] Without the proposed averaging based on the components of the first category, the vague averaging of the position deviations would result in a less accurate corrective action, since the special effects of the position deviations immediately after the chamber etching are averaged out. However, the corrective action should be very accurate, since the centering of the substrate wafer on the susceptor has advantageous consequences for the resulting edge shape of the semiconductor wafer with the epitaxial layer, and also reduces the risk of particle generation during the deposition of the epitaxial layer.
[0020] FIG. 2 shows the substrate wafer 4 placed on the susceptor 5 so that the center 10 of the susceptor 5 coincides with the center of the substrate wafer 4. In this target position, the substrate wafer 4 is concentric with respect to the susceptor 5 and with respect to the preheat ring 6. Without corrective measures, the center of the substrate wafer will be located, depending on its components of the first category or of a different category, in the vicinity of the average position calculated for this category, for example in the vicinity of the first average position 15 in the case of components of the first category or in the vicinity of the second average position 14 in the case of components of a different category. In the drawings, in order to be able to illustrate the invention, the positions 14 and 15 are located at unrealistic distances from the susceptor center 10. In actual fact, typical position deviations are less than 1000 μm away from the susceptor center 10.
[0021] The distance between the first average position 15 and the center 10 of the susceptor 5 corresponds to the length of vector 17. The distance between the second average position 14 and the center 10 of the susceptor 5 corresponds to the length of vector 16. If vector 16 or vector 17 is displaced so that its beginning coincides with the center 10 of the susceptor, the vector's point points to the placement position where the robot is requested to move the substrate wafer at its center to compensate for the expected position deviation. Thus, vector 17 represents a corrective action for the robot in relation to the first substrate wafer to be coated after chamber etching, and vector 16 represents a corrective action for the robot in relation to a different category of substrate wafer.
[0022] 3 and 4 show the measured position deviations of a boron-doped substrate wafer made of monocrystalline silicon with a diameter of 300 mm in a polar coordinate grid for a substrate wafer of the first category (with zero coating operations performed since the last chamber etch) and for a substrate wafer of a different category (with seven coating operations performed since the last chamber etch), respectively. A comparison of the depicted distributions of position deviations makes it clear that the amount of position deviation is significantly more pronounced when the substrate wafer under consideration is a wafer of the first category coated immediately after the chamber etch. [Explanation of symbols]
[0023] List of reference numbers used 1 Top cover 2 Bottom cover 3. Deposition chamber 4. Substrate Wafer 5 Susceptor 6 Preheat Ring 7 Upper Lining 8 Lower Lining 9 Upper gas inlet opening 10 Center of susceptor 11 Upper gas outlet 12 Lower gas inlet opening 13 Lower gas outlet 14. Second average position of the centers of the arranged substrate wafers 15 First average position of the center of the arranged substrate wafer 16 Vector 17 Vector
Claims
1. 1. A process for manufacturing a semiconductor wafer having an epitaxial layer vapor-deposited in a deposition chamber, comprising: removing from the deposition chamber material deposited therein during a previous coating operation by etching the deposition chamber; and coating operations carried out successively in the etched deposition chamber, the coating operations in each case comprising: the substrate wafer being placed on a susceptor having a circular periphery by a robot, the robot moving the substrate wafer to a placement position and placing the substrate wafer on the susceptor with a corrective action such that a center of the substrate wafer is not located above a center of the susceptor at the placement position, the coating operation further comprising: depositing an epitaxial layer on the substrate wafer to form a semiconductor wafer having an epitaxial layer; The process, wherein for each first substrate wafer moved by the robot to the placement position after the etch of the deposition chamber, the amount of the corrective action corresponds to an average of position deviations of a plurality of previously coated substrate wafers themselves, each of which is to be coated first after a preceding chamber etch.
2. The process of claim 1 , wherein the number of previously coated substrate wafers is at least three.
Citation Information
Patent Citations
Manufacturing method for epitaxial wafer and vapor growth device
JP2016213218A
Wafer transfer and placing device, vapor phase growth device, wafer transfer and placing method, and method of manufacturing epitaxial silicon wafer
JP2020102589A
Method and system for positioning wafer in semiconductor manufacturing fabrication
US20160293471A1