Method and system for analyzing a test specimen using a vibration response signal - Patents.com

By accounting for background noise through calibration measurements without excitation, the method improves the signal-to-noise ratio in acoustic measurements at elevated temperatures, ensuring accurate characterization of material properties.

JP7569811B2Active Publication Date: 2024-10-18GRINDOSONIC BV
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2021575422
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-06-20
Filing Date
2020-06-22
Publication Date
2024-10-18
Estimated Expiration
2040-06-22

AI Technical Summary

Technical Problem

Existing methods face challenges in maintaining a high signal-to-noise ratio during acoustic measurements of material properties at elevated temperatures, particularly due to background vibrations from heating equipment, which deteriorate the accuracy of material property determination.

Method used

A method and system that accounts for background noise by performing calibration measurements without vibrational excitation, followed by acoustic measurements with controlled vibrational excitation, allowing for improved analysis of vibration response signals at elevated temperatures.

Benefits of technology

Enhances the accuracy of material property determination by mitigating the impact of background noise, particularly at high temperatures, thereby improving the signal-to-noise ratio and enabling precise characterization of material properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007569811000014
    Figure 0007569811000014
  • Figure 0007569811000015
    Figure 0007569811000015
  • Figure 0007569811000016
    Figure 0007569811000016
Patent Text Reader

Abstract

The present invention relates to a method for acoustically measuring material properties of a test specimen at elevated temperatures, the method comprising: a. heating the test specimen within a test temperature range; b. performing background measurements within the test temperature range by capturing vibration signals from the test specimen during a calibration period, thereby obtaining a noise signal; c. performing acoustic measurements on the test specimen within the test temperature range and during a test period, the steps being: c1. applying a vibration excitation to the test specimen; and c2. capturing vibration signals of the test specimen during the test period, thereby obtaining a vibration response signal to the vibration excitation; and d. obtaining material properties of the test specimen by analyzing the vibration response signal, thereby taking into account the noise signal. The present invention also relates to a system for acoustically measuring material properties of a test specimen at elevated temperatures.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] Technical Field The present invention relates to a method and system for analyzing specimens using sonic or ultrasonic waves, which is particularly useful for detecting defects and anomalies in solids and for characterizing the E modulus, G modulus and Poisson's constant.

[0002] The present invention also relates to a method and system for obtaining thermal expansion parameters of a test specimen. [Background technology]

[0003] Background technology Testing of solids can be done in several ways. The first test usually consists of a visual inspection to see if the solid has the correct size and shape and to check for surface defects. However, in many cases the properties of a solid depend heavily on its internal structure which may not be visible to the eye. For example, the strength of metals and alloys depends heavily on the specific type and amount of bulk defects. These defects may be small or large and may occur due to natural factors, manufacturing methods, wear, accidents, etc.

[0004] Regardless of how the defect occurs, in some cases it is important to know the condition of the solid relative to the defect. In order to analyze a solid for defects, invasive or non-invasive methods can be used on a specimen of the solid. This allows the analysis without destroying or modifying the specimen, with non-invasive methods. Thus, non-invasive methods are typically used on specimens that still need to be used at a later time or that need to undergo further testing (which may themselves be invasive or non-invasive).

[0005] One type of non-invasive testing method for solids uses vibrations to analyze the test specimen. Hereby, the test specimen is subjected to controlled vibrations that can propagate through the solid and thereby be transmitted, reflected or absorbed. The controlled vibrations can be induced with impulse excitation techniques (IET), whereby the test specimen is positioned so that it can vibrate substantially unhindered when subjected to an impact. In impulse excitation techniques, the material properties of the test specimen are then determined by impacting the sample with a dedicated tool or projectile and analyzing the vibrations obtained when captured with a vibration signal measuring sensor, such as a piezoelectric sensor, microphone, laser vibrometer or accelerometer. The vibrations through the solid are also called sounds or sound waves, and the measurements are also called acoustic measurements. Thus, the vibration signal measuring sensor is also called "acoustic sensor" in the context of this application.

[0006] An apparatus for testing solids using sound is described in WO 2019 / 020825. This document discloses an apparatus for analyzing the mechanical vibration response of a solid material sample, comprising an array of impactors configured to impact respective distinct points on the surface of said solid material sample, a sensor configured to capture said mechanical vibration response as a time-varying signal following the impact of said at least one impactor, and processing means configured to analyze said time-varying signal to determine the frequencies and damping constants of the sinusoids constituting said time-varying signal. The invention also relates to a corresponding method for characterizing a solid material sample.

[0007] Analysis of the response of a solid specimen to vibrational excitation typically involves the extraction of one or more, preferably all, of the following parameters: -Young's modulus (E), which indicates the tensile elasticity of the test specimen; - Shear modulus (G), which indicates the response of the specimen to shear stress; -Poisson's ratio (ν), which describes the deformation of the specimen in the direction perpendicular to the applied uniaxial stress, These properties typically depend on the frequency or frequency range of the vibration excitation. This allows a specimen to have several resonant frequencies that depend on the different vibration modes of the specimen. The important modes here are bending and torsion modes. The parameter values ​​at these resonant frequencies are important quantities for describing the condition of the specimen.

[0008] In many applications, solid parts, for example in machines, are used at different temperatures. This can cause the operating temperature to vary rapidly and / or over a wide temperature range. For example, a vehicle brake disc can heat up fairly quickly during operation (essentially from ambient temperature to over 500°C in just a few seconds). Another example is a kerosene injection nozzle for an aircraft jet, which can heat up to over 1500°C during operation. The high temperature range can greatly affect the material properties of the components, especially the elastic properties such as Young's modulus, shear modulus, and Poisson's ratio mentioned above. For example, in general, solids can be expected to become more flexible at higher temperatures, generally due to weakening of internal bonds, which basically means that E and G are expected to decrease gradually with increasing temperature.

[0009] At different temperatures, solid components may have different material properties. This may affect the function of the component. It is important to find the temperature or temperature range at which the component's normal or intended function is disturbed. This may be due to the bulk properties of the material, defects that may be induced by temperature changes, defects that may become more significant at higher temperatures, variability in the expansion of different parts of the component, etc. Specific examples of temperature dependence of material properties of components are as follows: A general change in elastic properties, which reduces the stiffness of the component and thus prevents its proper functioning, e.g. a brake disc may become too elastic at high temperatures for proper braking - Phase transitions at certain temperatures or within certain temperature ranges can significantly change the material properties of the components - Chemical reactions can equally change the material properties of the components - Precipitations of stoichiometrically different phases in alloys can be present in materials, for example due to incorrect manufacturing methods, leading to internal material boundaries between materials with different temperature-dependent expansion. Obviously, this can lead to serious problems. - Laminates or other layered components whereby adhesion of one layer to the next can decrease with increasing temperature.

[0010] To test the proper function of a solid component at different temperatures and / or over the entire temperature range of its intended operation, the material properties of a test specimen need to be measured at different temperatures. Hereby, the test specimen can be, for example, the complete component, a part of the component, or a piece of the same material as the component. The test is preferably performed in a controlled environment that allows at least control of the temperature. The material properties are then measured at the different temperatures.

[0011] The inventors have found that it can be very difficult in practice to measure material properties of a test specimen over a wide temperature range, which can extend from less than -50°C to more than 2000°C. Creating a temperature-controlled environment for such a temperature range usually requires several ovens with vibration-generating components. Obviously, background vibrations generated by the oven can interfere with the measurement process. These background vibrations are usually worse at higher temperatures. Furthermore, since some material properties (e.g., E and G) can be expected to decrease with increasing temperature, the signal also decreases. Both effects result in a lower signal-to-noise (STN) ratio at higher temperatures.

[0012] The present invention aims to solve the problem of deterioration of the STN ratio in acoustic measurements of test pieces at high temperatures.

[0013] Additionally, the present invention also provides a relatively inexpensive and accurate method for determining one or more thermal expansion parameters of a material by acoustic measurement techniques. Summary of the Invention [Means for solving the problem]

[0014] Summary of the Invention In a first aspect, the present invention relates to a method for acoustically measuring material properties of a test specimen at elevated temperatures, the method comprising: a. heating the test specimen within a test temperature range; b. performing background measurements within said test temperature range by capturing vibration signals from a test specimen during a calibration period, thereby obtaining a noise signal; c. performing acoustic measurements on the test specimen within the test temperature range and for a test period; c1. applying a vibration excitation to a test specimen; and c2. Capturing a vibration signal of the test specimen during a test period, thereby obtaining a vibration response signal to said vibration excitation; d. Obtaining material properties of the test specimen by analyzing the vibration response signal, thereby taking into account noise signals.

[0015] Firstly, taking into account the background noise of the environment when performing the analysis of the vibration response leads to a better determination of the material properties. Secondly, by taking into account the background noise in the same test temperature range as the acoustic measurements, the inventors have found that a much better analysis of the vibration response can be performed. This is because the noise can be highly dependent on the temperature range, for example due to heating elements, ventilation devices, or any other equipment or equipment components used to perform the measurements, each of which can behave differently in different temperature ranges.

[0016] The inventors have further found that the best results are achieved when the background measurement is performed by performing all steps of the acoustic measurement, except for the application of a vibrational excitation to the test specimen. Thus, in a preferred embodiment, the step b of performing the background measurement comprises performing all steps of the step c of performing the acoustic measurement, except for the step c1 of applying a vibrational excitation to the test specimen. This applies to all embodiments of the method described above, as well as the methods described hereinafter in the present specification and claims.

[0017] In addition to a method, the present invention also relates to a system for acoustically measuring material properties of a test specimen at elevated temperatures, the system comprising: a heating chamber provided with a heating element for bringing the test specimen into a test temperature range; a sensor for capturing a vibration signal from the test specimen during a period of time; an impact system comprising an impactor and an impactor actuator for applying a vibration excitation to a test specimen disposed within the heating chamber; A control system associated with the heating chamber, the sensor, and the impactor, Direct the heating chamber to bring the test specimen into the test temperature range; commanding an impact system to actuate the impactor using an impactor actuator such that a vibration excitation is mechanically applied by the impactor to a test specimen disposed within the heating chamber during a test period, and to obtain a vibration response signal from a sensor to the vibration excitation; commanding the impact system to actuate the impactor using the impactor actuator such that the impactor does not mechanically impart vibration excitation to the test specimen disposed within the heating chamber during a calibration period and to acquire a noise signal from the sensor; A control system configured to obtain material properties of the test specimen by analyzing the vibration response signal, thereby taking noise signals into account.

[0018] In a second aspect, the present invention relates to a method for thermal expansion measurement for obtaining thermal expansion parameters of a test specimen, the method comprising the steps of: - extracting at least two resonant frequencies from experimental data at a first temperature; - obtaining a first value of a first dimensional parameter from the at least two resonant frequencies at the first temperature; - comparing the first value of the first dimensional parameter at the first measurement temperature with a second value of the first dimensional parameter at a second temperature; - calculating thermal expansion parameters from said comparison.

[0019] Thereby, the at least two resonant frequencies at the first temperature are material properties of the test specimen, which can preferably be obtained by the acoustic measurement method described above and further herein. The system for acoustically measuring material properties of the test specimen at elevated temperatures described above and further herein can preferably be used to obtain the at least two resonant frequencies.

[0020] BRIEF DESCRIPTION OF THE DRAWINGS These and other features and advantages of embodiments of the present invention will be described in more detail with reference to the accompanying drawings. [Brief description of the drawings]

[0021] [Figure 1] 1 shows a schematic of the vibration induced in a beam specimen upon excitation in bending mode. [Diagram 2] 1 shows a schematic of the vibration induced in a beam specimen upon excitation in torsional mode. [Diagram 3] 1 illustrates a schematic diagram of an embodiment of a measurement system according to the invention; [Figure 4] 1 illustrates a schematic diagram of an embodiment of a measurement method according to the present invention; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0022] In the known Impact Excitation Technique (IET) procedure, the test specimen is positioned so that it can vibrate substantially unhindered when impacted. This can be achieved by placing the specimen on a piece of lightweight foam or on a linear support (e.g., a wire or narrow bar) carefully positioned below the zero (node) of the vibration mode to be excited. Excitation is performed by impacting the sample at the antinode, i.e., the point where the local amplitude of the induced motion is maximum for the mode of interest.

[0023] FIG. 1 shows a schematic representation of the vibration induced in a beam specimen when excited in bending (specifically, out-of-plane) mode. The natural frequency f f denotes the dynamic Young's modulus E of the sample. For the illustrated beam with mass m, length L, width b, and thickness t, the following relationship can be used:

[0024]

number

[0025] The correction factor T is defined as follows when L / t≧20:

[0026]

number

[0027] Figure 2 shows a schematic of the vibration induced in a beam-like sample under test upon excitation of a torsional mode. The natural frequency of this vibration mode, f t denotes the shear modulus of the sample. For the illustrated beam with mass m, length L, width b, and thickness t, the following relationship can be used:

[0028]

number

[0029] The correction factor R is defined as follows:

[0030]

number

[0031] These known methods of determining E and G rely solely on the peak frequencies in the spectrum of the sample's response. The inventors have found that while a shift in E and / or G relative to expected values ​​may by itself indicate a defect in the sample, an abnormally fast decay of a particular frequency component is a more reliable predictor of such a defect.

[0032] The inventors have found that the response of a solid specimen to an impact excitation is physically close to a sum of exponentially decaying sine waves. By assuming this particular mathematical form of the excitation response, better accuracy can be obtained than simply extracting peaks in the (fast) Fourier transform, based on the underlying physics of the phenomenon. The damping constant gives better insight into the presence of defects than the mere identification of the resonant frequencies of the specimen. Identification of the damping constant thereby constitutes a harmonic inversion problem that can be solved by known mathematical methods.

[0033] Furthermore, the inventors have found that the material properties E and G can change depending on the temperature of the test specimen. This can be observed in acoustic measurements, where the material structure of the test specimen can change with temperature, such that a shift in resonant frequency occurs with temperature changes. For example, a slow variation in resonant frequency with temperature can be expected due to a slow weakening of internal boundaries or a slow increase in bulk and surface defects, which tend to result in a decrease in E and G. However, a sudden or unexpected change in material properties within a particular temperature range tends to indicate a new type of defect occurring in that temperature range. Also, even if the material properties change slowly, the present method and system make it possible to determine at what point the material properties have changed to such an extent that the test specimen or any component made from the same material or with the same manufacturing process as the test specimen will not meet the desired specifications.

[0034] In a preferred embodiment, the vibration excitation in step c1 is mechanically induced in the test specimen, preferably by using an impactor configured to contact the test specimen in step c1 and not contact the test specimen in step b.

[0035] In one embodiment of the invention, the impact system comprises a ballistic impactor, and the impact actuator is configured to apply an impulse to said ballistic impactor. Preferably, the method of the invention is carried out using said impact system, and in the acoustic measurement step, a measurement impulse is provided to the ballistic impactor, which imparts a vibrational excitation to the test specimen, and in the background measurement step, a background impulse is provided to the ballistic impactor, which imparts no vibrational excitation to the test specimen. In this embodiment, the background impulse is preferably as close as possible to the measurement impulse. In one embodiment, the measurement impulse and the background impulse differ in magnitude by at most 2 times, more preferably at most 1.8 times, even more preferably at most 1.6 times, even more preferably at most 1.4 times, even more preferably at most 1.2 times, and most preferably at most 1.1 times. Alternatively or additionally, the measurement impulse and the background impulse differ in terms of direction, preferably by an angle of at most 60°, more preferably at most 45°, even more preferably at most 35°, even more preferably at most 25°, even more preferably at most 15°, and most preferably at most 5°.

[0036] In a more preferred embodiment, the ballistic impactor is configured to approach the test specimen from below along the vertical direction, whereby preferably the measurement impulse provided to the ballistic impactor is configured to mechanically contact the test specimen, and the background impulse provided to the ballistic impactor is configured not to reach the test specimen, whereby in a preferred embodiment the background impulse is at least 50%, more preferably at least 60%, even more preferably at least 70%, even more preferably at least 80%, even more preferably at least 90% of the measurement impulse. It should be noted that the closer the background impulse is to the measurement impulse, the better the noise signal obtained and the more accurate the material properties obtained.

[0037] An embodiment including a ballistic impactor configured to approach the test specimen from below along a vertical direction is shown in FIG.

[0038] FIG. 3 shows a heating chamber (301) comprising a set of heating elements (302, 303, 304, 305, 306) capable of bringing the heating chamber and / or the test specimen to a desired temperature or range of temperatures. The heating elements (302, 303) are attached to the heating chamber walls and can supply heat to the heating chamber walls, for example, by heat exchange with a hot, high-pressure fluid, electrical resistance heating, magnetic induction, etc. The heat of these wall heating elements can be distributed within the heating chamber, for example, by ventilation devices (304, 305). The ventilation devices (304, 305) may also be configured to supply a warm fluid, such as heated air or steam, to the heating chamber. The heating elements may also comprise radiant heating elements, such as microwave elements (306). The heating chamber preferably also comprises one or more thermometers for measuring the actual temperature within the heating chamber and / or of the test specimen, and preferably also comprises a control circuit configured to control the temperature of the test specimen and / or the heating chamber.

[0039] The test specimen (307) is suspended by a support structure (308, 309) that allows the specimen to vibrate as freely as possible, for example by supporting it at the locations of the vibration nodes of the specimen. An acoustic sensor (310) or multiple acoustic sensors, which may comprise a microphone or a laser interferometer, may be brought into contact with the specimen (311), preferably at a well-defined location, or a waveguide may be used to guide the acoustic response to the acoustic sensor, preferably with one end of the waveguide being brought close to or directly in contact with the specimen in the heating chamber, and the other end preferably located outside the heating chamber. The latter embodiment allows the sensor to be located outside the heating chamber.

[0040] In a preferred embodiment, the acoustic sensor comprises a laser interferometer, which is particularly useful for measurements in a vacuum and allows for non-contact measurements. Alternatively or additionally, the acoustic sensor may comprise an ultrasonic measurement sensor and / or a time-of-flight sensor and / or a Doppler type sensor, for example as described below. -SR. Huang, RM. Lerner, K. J. Parker, "Time-Domain Doppler Estimator of the Amplitude of Vibrating Targets," Journal of the Acoustical Society of America, 91(2), 965-974 (1992), - J. Tapson, "High-precision short-range ultrasonic detection by resonant mode-locking," Ultrasonics, 33, 6, 441-444 (1995)), and - R. Kazys, R. Sliteris, L. Mazeika, "Ultrasonic Techniques for Vibration Measurement", Proceedings of the 15th World Congress on Non-Destructive Testing, 15-21 October 2000, Rome, https: / / www.ndt.net / article / wcndt00 / papers / idn246 / idn246.htm. These types of sensors may also be used for non-contact measurements.

[0041] In one embodiment, the method of the present invention is carried out in which the heating chamber comprises a pressure below atmospheric pressure, preferably 0.5 bar or less, more preferably 0.2 bar or less, and most preferably essentially a vacuum pressure. This allows non-contact vibration measurements at low to zero pressure, preferably using a laser interferometer. Measurements at reduced pressures down to zero attenuate ambient noise, thereby increasing the signal-to-noise ratio.

[0042] The impact system comprises a ballistic impactor (312) to which an impulse can be applied by an impactor actuator (313). The ballistic impactor (312) is a ceramic rod capable of withstanding high temperatures and whose properties do not change significantly with temperature. It can be fired upwards (314) towards the test specimen using the impactor actuator (313), which: a guide tube (315) through the bottom of the heating chamber for guiding the ballistic impactor preferably along the vertical direction; - an electromechanically actuated hammer (316) configured to impart a preferably vertical impulse (317) to the impactor (312). The hammer (316) may comprise an electric coil (318) and a movable rod or projectile (319) that can move in response to an electric current flowing through the coil (318). An example of such a system is presented in US Pat. No. 6,782,970, whereby in the present invention the projectile of the impactor actuator impacts the ceramic impactor (312) rather than directly on the specimen. Alternatively, a pressure-driven impactor or pressure-driven impact actuator (380) for imparting the impulse to the impactor may be used.

[0043] When performing step b, the impactor actuator is configured to provide an impulse to the ballistic impactor that brings the ballistic impactor to within 2 cm below the test specimen without contacting the test specimen. When performing step c, particularly step c1, the impactor actuator is configured to provide an impulse to the ballistic impactor that brings the ballistic impactor into contact with the test specimen, thereby mechanically inducing a vibration excitation in the test specimen. During step b, background noise can be measured. This noise can come from, for example, the heating element, but also, and perhaps primarily, from the impactor actuator and the impactor, which also make noise that can be picked up by the sensor.

[0044] In one embodiment of the invention, steps a-d are performed repeatedly multiple times, preferably at the same temperature, at different temperatures or within different temperature ranges. In a preferred embodiment, the test specimen is heated sequentially, whereby steps a-d are performed within successive temperature ranges.

[0045] For example, the test specimen can be heated continuously from room temperature (20° C.) at a rate of 1° C. / s. Steps a-d can then be performed periodically every 20 seconds, meaning that a first set of steps a-d is performed in a temperature range of 20 to 40° C., a second set of steps a-d is performed in a temperature range of 40 to 60° C., and so on up to a maximum temperature range of, for example, 1780 to 1800° C. It should be noted, however, that the temperature ranges do not have to be equally large, and can, for example, be smaller relative to the temperature range of interest. For example, if it is known that the test specimen or a component made from the same material as the test specimen will be used mainly at temperatures of 700 to 800° C., it can be decided to measure the material properties between these temperatures more accurately by taking a smaller temperature range, for example extending to 5° C.

[0046] It is further noted that the measurements performed in steps b and / or c can be combined with measurements performed in steps b and / or c at other temperatures in order to obtain more accurate noise signals and / or vibration response signals. For example, assume that steps a-d are performed in a temperature range of 80°C-100°C and in a temperature range of 100°C-120°C. Thereby, step b could be performed a first time in a partial temperature range of 82-87°C and a second time in a partial temperature range of 102-107°C, while step c could be performed a first time in a partial range of 92-97°C. In such a case, the analysis of step d can be performed taking into account the two noise signals obtained in two steps b. Thus, in a preferred embodiment, steps a, b, c and / or d are performed more than once in a temperature range. Alternatively or additionally, steps a, b, c and / or d may be performed multiple times in different temperature ranges that may overlap.

[0047] In one embodiment, the control system comprises processing means configured to analyze the vibration response signal taking into account the noise signal to determine material properties of the test specimen.

[0048] Thereby, the processing means may be preferably configured to subtract the noise signal from the vibration response signal in the time domain, or more preferably in the frequency domain, by using a Fourier transform or a fast Fourier transform or a harmonic decomposition on the captured signal. The subtraction may also be performed in a combination of the time domain and the frequency domain. The processing means is preferably configured to analyze the time-varying signal to determine the frequencies and damping constants of the sinusoids constituting the time-varying signal, i.e. to solve the harmonic inversion problem. The harmonic inversion problem, which more generally consists of determining the frequencies, damping constants, amplitudes and phases of the sinusoids constituting a discrete-time finite-length signal consisting of the sum of a finite number of such sinusoids in a given bandwidth, is well known in the literature but has not been associated to IET to date. Vladimir A. Mandelshtam and Howard S. Taylor, in their seminal paper "Harmonic inversion of time signals and its applications", The Journal of Chemical Physics 107, 6756 (1997), describe the use of the general filter diagonalization method of Wall and Neuhauser to solve the harmonic inversion problem by reassessing it as one of small matrix diagonalization. Computer-based implementations of this technique are known in the art, including the "Harminv" program by Steven G. Johnson of the Massachusetts Institute of Technology. The results of the analysis can be output to a screen 140 or to any other suitable interface for storage or further processing by other equipment.

[0049] The processing means may consist of one or more dedicated hardware components (e.g. ASICs), suitably configured configurable hardware components (e.g. FPGAs), a microprocessor with suitable software, or a combination of the above. The same components may also perform other functions.

[0050] In a preferred embodiment of the invention, the test specimen is a workpiece, a device or a component of a device. In another preferred embodiment of the invention, the test specimen has a well-defined shape, preferably a beam shape, and is made from the same material or using the same manufacturing technique as the workpiece, device or component of a device.

[0051] FIG. 4 shows an embodiment of the method according to the invention. In a first step a, the temperature is brought within a first temperature range (1021). Then, step b is performed (1002), whereby care is taken not to impact the specimen (1001), whereby the impact system is preferably activated, but such that impact is avoided. Then, step c is performed, whereby the specimen is impacted (step c1, 1010) and a vibration response signal is captured (step c2, 1020). The signal is then analyzed (step d, 1030), whereby E, G, ν and / or other properties (particularly also the damping constant) are obtained within the temperature range of step a. The impact avoidance activation step (1001), noise capture step (1002), impact step (1010), and response capture step (1020) may be performed repeatedly (as shown, for example if the device has multiple impactors operating in series) before the signal is analyzed (1030), or each captured signal may be analyzed separately. This allows the noise signals and / or vibration response signals at different temperatures or temperature ranges to be combined in the analysis of step d to obtain more accurate values ​​of the material properties and / or to determine the temperature dependence of these material properties.

[0052] Depending on the selected excitation mode, the analysis step 1030 may further include determining the dynamic Young's modulus (E) or shear modulus (G) from the frequencies of the spectrum of responses, in particular by identifying the peak frequencies and applying the formulas as above.

[0053] Preferably, the analyzing step further comprises a step 1040 of comparing the decay constant with a reference value. This step allows the method according to the invention to be used for quality control purposes. Indeed, a method of controlling the quality of a manufactured product comprises the steps of characterizing at least a part of the manufactured product as said solid material sample using the above-mentioned method, and signaling a "pass" condition 1040 / yes if the decay constant is within a predefined margin of said reference value and declaring a "fail" condition 1040 / no if the decay constant is outside said predefined margin of said reference value. Thus, according to one aspect of the invention, a method of controlling the quality of a manufactured product is provided, comprising the steps of characterizing at least a part of the manufactured product as said test piece using the above-mentioned method, and signaling a "pass" condition if the decay constant is within a predefined margin of said reference value and declaring a "fail" condition if the decay constant is outside said predefined margin of said reference value.

[0054] The invention also relates to a computer program product comprising coding means adapted to cause a processor to carry out the computational steps of the method described above.

[0055] As mentioned above, in a second aspect, the present invention relates to a method for thermal expansion measurement for obtaining thermal expansion parameters of a test specimen, the method comprising the steps of: - extracting at least two resonant frequencies from experimental data at a first temperature; - obtaining a first value of a first dimensional parameter from the at least two resonant frequencies at the first temperature; - comparing the first value of the first dimensional parameter at the first measurement temperature with a second value of the first dimensional parameter at a second temperature; - calculating thermal expansion parameters from said comparison.

[0056] Thereby, the at least two resonant frequencies at the first temperature are material properties of the test specimen, which can preferably be obtained by the acoustic measurement method described above and further herein. The system for acoustically measuring material properties of the test specimen at elevated temperatures described above and further herein can preferably be used to obtain the at least two resonant frequencies.

[0057] In the thermal expansion measurement method, the second value of the first dimensional parameter at the second temperature may be a known reference value, e.g., a known dimension of the test specimen at room temperature or 0°C or another predetermined temperature, or may be obtained by extraction of two resonant frequencies from experimental data at the second temperature, preferably, said two resonant frequencies at the second temperature are obtained as material properties of the test specimen using the method and / or system for acoustically measuring material properties of a test specimen described herein.

[0058] The thermal expansion parameters may preferably be: a size dimension, such as length, width, thickness, surface, volume, in such a case the thermal expansion parameter is preferably the difference in value between the size dimension at a first temperature and the size dimension at a second temperature - an absolute expansion ratio, such as a linear expansion ratio, preferably obtained by taking the ratio of the size at a first temperature to the size at a second temperature a relative expansion ratio, preferably obtained by taking the ratio between the difference in value between the size dimension at the first and second temperatures and a reference value of the size dimension, which may be any well-defined reference value, preferably the value of the size dimension at the first temperature or at the second temperature or at a given reference temperature a thermal expansion coefficient or an average thermal expansion coefficient, preferably obtained by taking the ratio of the relative expansion ratio and the temperature difference between the first temperature and the second temperature - preferably an anisotropic ratio obtained by taking the ratio between a first dimension and a second dimension different from the first dimension at a first temperature and comparing this value with the same ratio at a second temperature. This can result for example in the anisotropic ratio of the thermal expansion coefficients, i.e. the ratio of the thermal expansion coefficient along a first direction to the thermal expansion coefficient along a second direction, or their average in the interval between the first and second temperatures.

[0059] The thermal expansion parameter may also be any combination and / or derived quantity of the above parameters.

[0060] The thermal expansion parameters can be calculated analytically in a preferred embodiment. A preferred method of analytical calculation is as follows and is illustrated by using standard ASTM C 215-02 for calculating the E modulus based on impulse excitation of concrete specimens. -The bending mode resonance frequency at the first temperature is obtained. A longitudinal compression mode resonant frequency is obtained at a first temperature. - bending mode resonance frequency f f1 is, for example, for a beam-shaped specimen with mass m, length L, thickness t and width b,

[0061]

number

[0062] Regarding L / t≧20, the correction coefficient T is

[0063]

number

[0064] is defined as - Resonance frequency of the longitudinal compression mode f f2 is, for example, for a beam-shaped specimen with mass m, length L, thickness t and width b,

[0065]

number

[0066] About -E is the value of the elastic modulus equal to the first temperature T 1 The size dimension at can be obtained as follows:

[0067]

number

[0068] - second temperature T 2 For example, the anisotropic ratio of the thermal expansion coefficient averaged between the first temperature and the second temperature can be obtained by comparing the size dimension value at

[0069]

number

[0070] It is possible to calculate

[0071]

number

[0072] where

[0073]

number

[0074] Where:

[0075]

number

[0076] is the temperature interval [T 1 ,T 2 ] is the longitudinal thermal expansion coefficient averaged over

[0077]

number

[0078] is the same temperature interval [T 1 ,T 2 ] is the thermal expansion coefficient through the thickness averaged over the thickness of the specimen. This ratio can be important in itself to know about certain types of materials, especially to determine and quantify the anisotropy of the material, and changes in this ratio over a particular temperature interval can indicate phase transformation or fracture of the specimen.

[0079] This allows the test specimen to have, for example, dimensions of (10 cm x 2 cm x 5 mm) at room temperature (20°C), which may then serve as the size dimension value at the second temperature.

[0080] Here, the value of the resonant frequency at the first temperature may preferably be obtained in a single acoustic measurement at the first temperature, and optionally, the value of the resonant frequency at the second temperature may also preferably be obtained in a single acoustic measurement at the second temperature. Preferably, these are obtained using the acoustic measurement method and / or system of the present invention. This allows the resonant frequencies of the different modes to be easily measured by identifying the peaks of the acoustic response in the frequency domain. In some cases, uncertainty may arise in identifying which resonant frequency belongs to which mode. In such cases, the identification of the resonant frequency for the mode may be obtained via modeling and / or simulation calculations, or via a set of additional acoustic measurements, preferably whereby the test specimen is shocked to excite the particular mode.

[0081] As mentioned above, the comparison can be made using analytical methods, e.g., equation-based methods, whereby values ​​of the dimensional parameters are analytically extracted. Alternatively or additionally, the comparison can be made using simulation methods, e.g., the simulation method comprises a step of modeling the test piece using a set of model parameters related to the dimensional parameters, the simulation method comprises a resonance calculation algorithm for obtaining at least two resonant frequencies, the model parameters are varied to optimally reproduce the at least two resonant frequencies, thereby obtaining an optimal set of model parameters, and values ​​of the dimensional parameters are calculated from the optimal set of model parameters. The simulation method preferably includes a finite element method.

[0082] From the two measured resonant frequencies, values ​​for, for example, the E modulus and size dimensions can be derived using equations.

[0083] More resonant frequencies can be used, for example: - Torsional resonance frequency - First harmonic of bending mode - Second harmonic of bending mode - First harmonic of longitudinal compression mode -Second harmonic of longitudinal compression mode or any combination or derived quantity thereof.

[0084] Note that the harmonics may depend on the proportions of the specimen, so that in the case of anisotropic expansion, the harmonic resonant frequencies are not necessarily multiples of the ground mode resonant frequencies. This allows for values ​​of more than one size dimension parameter, which is useful in the case of anisotropic expansion. Furthermore, by using more than two resonant frequencies, the resulting system may be overdetermined, in which case a best fit solution for the desired size dimension can be obtained, for example, by analytical and / or simulation methods.

[0085] The invention also relates to a computer program product comprising coding means adapted to cause a processor to carry out the calculation steps of the thermal expansion measurement method described above.

Claims

1. 1. A method for acoustically measuring material properties of a test specimen at elevated temperatures, comprising: a. heating the test specimen within a test temperature range; b. performing background measurements within the test temperature range by capturing vibration signals from the test specimen during a calibration period, thereby obtaining a noise signal; c. performing acoustic measurements on the test specimen during the test temperature range and duration; c1. applying a vibrational excitation to the test specimen; capturing a vibration signal of the test specimen during the test period, thereby obtaining a vibration response signal to the vibration excitation; d. obtaining the material properties of the test specimen by analyzing the vibration response signal taking into account the noise signal; The vibration excitation of step c1 is mechanically induced in the test specimen; An impact system is used that includes a ballistic impactor and an impactor actuator configured to provide an impulse to the ballistic impactor, using the ballistic impactor to provide a vibration excitation to the test specimen; In the acoustic measurement step c, a measurement impulse that imparts vibration excitation to the test piece is provided to the ballistic impactor in step c1; In the background measurement step b, a background impulse that does not impart vibration excitation to the test specimen is provided to the ballistic impactor; The method, wherein the noise signal includes noise arising from the impactor actuator and the ballistic impactor.

2. The method of claim 1 , wherein the ballistic impactor is configured to approach the test specimen from below along a vertical direction.

3. 3. The method of claim 2, wherein the measurement impulse provided to the ballistic impactor is configured to mechanically contact the test specimen and the background impulse provided to the ballistic impactor is configured not to reach the test specimen.

4. The method of any one of claims 1 to 3, wherein steps a to d are carried out multiple times at the same temperature, at different temperatures or within different temperature ranges.

5. The method of any one of claims 1 to 3, wherein the test specimen is heated successively, whereby steps a to d are performed within successive temperature ranges.

6. 6. The method according to claim 1, wherein in step d) the temperature dependence of the material properties is determined.

7. 7. The method according to claim 1, wherein in step d) Young's modulus (E), shear modulus (G) and / or Poisson's modulus (v) are determined.

8. 8. A method according to claim 1, wherein in step d) a damping constant of the material properties is determined, said damping constant being the damping constant of a sine wave constituting the time-varying vibration response signal.

9. 1. A system for acoustically measuring material properties of a test specimen at elevated temperatures, comprising: a heating chamber equipped with a heating element for bringing the test specimen into a test temperature range; a sensor configured to capture a vibration signal from said test specimen during a period of time; an impact system comprising an impactor and an impactor actuator for applying a vibrational excitation to a test specimen placed in said heating chamber; a control system associated with said heating chamber, said sensor and said impactor, directing the heating chamber to bring the test specimen into a test temperature range; commanding the impact system to actuate the impactor using the impactor actuator such that a vibration excitation is mechanically applied by the impactor to a test specimen disposed within the heating chamber during a test period, and to obtain a vibration response signal from the sensor to the vibration excitation; commanding the impact system to actuate the impactor using the impactor actuator such that the impactor does not mechanically impart vibrational excitation to the test specimen disposed within the heating chamber during a calibration period and to acquire a noise signal from the sensor; a control system configured to obtain the material properties of the test specimen by analyzing the vibration response signal taking into account the noise signal; the noise signal includes noise arising from the impactor actuator and the impactor; the impact system comprises a ballistic impactor, the impactor actuator configured to impart an impulse to the ballistic impactor; the impactor actuator is configured to provide a measurement impulse to the ballistic impactor to impart vibrational excitation to the test specimen during an acoustic measurement step; whereby the impactor actuator is configured to apply a background impulse to the ballistic impactor to avoid impacting the test specimen in a background measurement step, a background impulse that does not impart vibration excitation to the test specimen is provided to the ballistic impactor in the background measurement step, and the noise signal includes noise arising from the impactor actuator and the ballistic impactor in the background measurement step. system.

10. 10. The system of claim 9, wherein the control system comprises processing means configured to analyze the vibration response signal by subtracting the noise signal from the vibration response signal in the time domain or the frequency domain, or a combination of the time domain and the frequency domain.

Citation Information

Patent Citations

  • Tester of super fine material

    JP1993332908A

  • Apparatus and method for performing an impact excitation technique

    WO2019020825A1