Methods of selective deposition

Silylamine-based SAMs with nitrogen-containing plasma treatment enhance selective deposition on conductive surfaces, addressing inefficiencies in existing methods by improving selectivity and deposition rates while protecting dielectric materials.

JP7569861B2Active Publication Date: 2024-10-18APPLIED MATERIALS INC
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2022542960
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-09-03
Filing Date
2021-07-21
Publication Date
2024-10-18
Estimated Expiration
2041-07-21

AI Technical Summary

Technical Problem

The semiconductor industry faces challenges in achieving selective deposition on conductive and dielectric surfaces without damaging dielectric materials, as existing methods like hydrogen plasma treatment can harm dielectric surfaces and traditional SAM precursors have low vapor pressures and high hydrophobicity, making deposition inefficient.

Method used

A method using silylamine-based self-assembled monolayers (SAMs) with nitrogen-containing plasma treatment to prepare substrates, forming -NH terminations on dielectric surfaces, enhancing selectivity and allowing precise deposition on conductive materials while preserving dielectric integrity.

Benefits of technology

Improves selectivity and deposition rates on conductive surfaces by up to 50% compared to hydrogen plasma treatment, ensuring minimal damage to dielectric materials and maintaining high vapor pressure for efficient SAM precursor delivery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007569861000002
    Figure 0007569861000002
  • Figure 0007569861000003
    Figure 0007569861000003
  • Figure 0007569861000004
    Figure 0007569861000004
Patent Text Reader

Abstract

Methods for selective deposition are described herein. Additionally, methods for improving selectivity are described, including an ammonia plasma pre-cleaning process. In some embodiments, a surfactant layer is selectively formed on a dielectric surface using a silylamine. A ruthenium film can then be selectively deposited on a conductive surface. In some embodiments, the ammonia plasma removes oxide contamination from the conductive surface without adversely affecting the dielectric surface.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] FIELD OF THE DISCLOSURE Embodiments of the present disclosure generally relate to a method for selective deposition of a film onto a conductive or metallic surface. Some embodiments of the present disclosure are directed to a method for selective deposition utilizing silylamines to form a self-assembled monolayer (SAM). Some embodiments of the present disclosure are directed to a method for selective deposition including an ammonia plasma pre-cleaning process. [Background technology]

[0002] The semiconductor industry faces many challenges in the pursuit of device miniaturization, including the rapid scaling of nanoscale features. Such challenges include the fabrication of complex devices that often use multiple lithography steps and etching processes. Moreover, the semiconductor industry needs a low-cost alternative to the high-cost EUV to pattern complex architectures. To keep the trend of device miniaturization going and keep chip production costs low, selective deposition has shown promise. It has the potential to remove expensive lithography steps by simplifying integration schemes.

[0003] Selective deposition of materials can be accomplished in a variety of ways. For example, some processes can have inherent selectivity to surfaces based on the surface chemistry. These processes are rare and generally specific to the reactants used, the material being formed, and the substrate surface.

[0004] Self-assembled monolayers (SAMs) are a technique that allows for selective deposition onto many material surfaces. Ideally, during the SAM stabilization process, the SAM forms completely over all dielectric surfaces, blocking 100% of film buildup from subsequent deposition steps so that films grow only on conductor / metal surfaces.

[0005] However, the SAM grows with an asymptotic thickness as a function of deposition time and cycle number, and as a result, an ideal SAM that blocks 100% of the film is extremely difficult to achieve.

[0006] Additionally, most SAM precursors contain long hydrophobic carbon chains to hinder deposition: the hydrophobic carbon chains increase the hydrophobicity of the surface on which the SAM is deposited, but can also reduce the vapor pressure, making it more difficult to deliver the precursor into the processing chamber.

[0007] Therefore, new SAM precursors that offer good selectivity and have relatively high vapor pressure are needed.

[0008] The selectivity of a SAM-based selective deposition process also generally depends on the condition of the substrate surface prior to SAM deposition. For example, for substrates containing metal surfaces to be deposited, it may be necessary to remove native metal oxides prior to SAM formation and / or film deposition. Traditionally, oxides are removed from metal surfaces by hydrogen plasma treatment. However, treating substrates containing dielectric surfaces with hydrogen plasma can damage the dielectric material. Summary of the Invention [Problem to be solved by the invention]

[0009] Therefore, new substrate treatment processes are needed that improve selectivity without damaging the dielectric material. [Means for solving the problem]

[0010] One or more embodiments of the present disclosure are directed to a method of selective deposition comprising: depositing a substrate containing a conductive material and a dielectric material with a compound having the general formula ((CH3)2N): x Si(CH3) y ((CH2) zCH3) to selectively form a surfactant layer on the dielectric material, where x is 1 to 3, y is 0 to 2, x+y is equal to 3, and z is 0 to 17. A film is selectively deposited on the conductive material.

[0011] An additional embodiment of the present disclosure is directed to a method of improving selectivity, comprising exposing a substrate including a conductive material having oxide contaminants and a dielectric material having an -OH surface termination to a plasma formed from a nitrogen-containing gas to remove the oxide contaminants and form an -NH surface termination on the dielectric material.

[0012] A further embodiment of the present disclosure is directed to a method of selective deposition comprising exposing a substrate including a conductive material having oxide contaminants and a dielectric material having an -OH surface termination to a plasma formed from a nitrogen-containing gas to remove the oxide contaminants and form an -NH surface termination on the dielectric material. x Si(CH3) y ((CH2) z A surfactant layer is selectively formed on the dielectric material by exposure to a silylamine of 0.25% by weight of 1000 ppm ...

[0013] So that the above-recited features of the present disclosure can be understood in detail, a more particular description of the present disclosure briefly summarized above can be had by reference to embodiments, some of which are illustrated in the accompanying drawings. It should be noted, however, that the accompanying drawings illustrate only typical embodiments of the present disclosure and should not be considered as limiting the scope of the present disclosure, since the present disclosure may admit of other equally effective embodiments. [Brief description of the drawings]

[0014] [Figure 1] 1 illustrates an exemplary substrate during processing in accordance with one or more embodiments of the present disclosure. [Diagram 2] FIG. 1 illustrates an exemplary processing method according to one or more embodiments of the present disclosure. [Figure 3A] FIG. 1 illustrates a patterned substrate after treatment with a process including a hydrogen plasma pre-clean. [Figure 3B] FIG. 2 illustrates a patterned substrate after processing according to one or more embodiments of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] Before describing certain example embodiments of the present disclosure, it is to be understood that the present disclosure is not limited to the details of structure or process steps set forth in the following description as the present disclosure is capable of other embodiments and of being practiced or carried out in various ways.

[0016] As used herein and in the appended claims, the terms "substrate" and "wafer" are used interchangeably and both refer to a surface or a portion of a surface on which a process acts. Furthermore, it will be understood by those skilled in the art that a reference to a substrate may also refer to only a portion of the substrate, unless the context indicates otherwise. Additionally, a reference to depositing on a substrate can refer to both a bare substrate and a substrate on which one or more films or features have been deposited or formed.

[0017] Furthermore, as used herein, "substrate" refers to any substrate or material surface formed on a substrate on which a film treatment is performed during a manufacturing process. For example, substrate surfaces on which treatment can be performed include materials such as silicon, silicon oxide, strained silicon, silicon-on-insulator (SOI), carbon-doped silicon oxide, silicon nitride, doped silicon, germanium, gallium arsenide, glass, sapphire, and any other materials such as metals, metal nitrides, alloys, and other conductive materials, depending on the application. Substrates include, but are not limited to, semiconductor wafers.

[0018] Substrates can be exposed to pretreatment processes to polish, etch, reduce, oxidize, hydroxylate (or otherwise generate or graft targeted chemical moieties to impart chemical functionality), anneal, and / or bake the substrate surface. In addition to direct film treatment on the surface of the substrate itself, in this disclosure, any of the disclosed film treatment steps can also be performed on underlying layers formed on the substrate, as disclosed in more detail below, and the term "substrate surface" is intended to include such underlying layers as the context indicates. Thus, for example, when a film / layer or partial film / layer is deposited on a substrate surface, the exposed surface of the newly deposited film / layer becomes the substrate surface. What a given substrate surface comprises will depend on what film is to be deposited, as well as the particular chemistry used.

[0019] As used herein, a "patterned substrate" refers to a substrate having a plurality of distinct material surfaces. In some embodiments, the patterned substrate comprises a first surface and a second surface. In some embodiments, the first surface comprises a dielectric material and the second surface comprises a conductive material. In some embodiments, the first surface comprises a conductive material and the second surface comprises a dielectric material.

[0020] As used herein and in the appended claims, the terms "reactive gas," "process gas," "precursor," "reactant," and the like are used interchangeably to mean gases that contain species that react with the substrate surface. For example, a first "reactive gas" may simply adsorb to the surface of the substrate and be available for further chemical reaction with a second reactive gas.

[0021] Some embodiments of the present disclosure provide methods of selective deposition utilizing silylamine-based SAMs. Some embodiments of the present disclosure provide methods and apparatus for increasing the effective selectivity of SAM-based selective deposition.

[0022] As used herein and in the appended claims, terms such as "selectively depositing on a first surface over a second surface" mean that a first amount of film or layer is deposited on a first surface and a second amount of film or layer is deposited on a second surface, where the second amount of film is less than the first amount of film or no film is deposited on the second surface. The term "over" as used in this context does not refer to the physical orientation of one surface over the other, but rather the relationship of one surface to another surface in terms of thermodynamic or kinetic properties of a chemical reaction. For example, selectively depositing a cobalt film on a copper surface over a dielectric surface means that a cobalt film deposits on the copper surface and little or no cobalt film deposits on the dielectric surface, or that the formation of a cobalt film on the copper surface is thermodynamically or kinetically favored compared to the formation of a cobalt film on the dielectric surface.

[0023] In some embodiments, "selectively" means that the target material forms on the target surface at a rate that is about 10, 15, 20, 25, 30, 35, 40, 45, or 50 times faster than it forms on the non-selected surfaces. Stated another way, the selectivity of the target material surface over the non-selected surfaces is about 10:1, 15:1, 20:1, 25:1, 30:1, 35:1, 40:1, 45:1, or 50:1 or more.

[0024] One strategy for achieving selective deposition employs the use of a blocking layer, which is formed on the substrate material on which deposition is to be avoided, with negligible effect on the target substrate material. The film can be deposited on the target substrate material, while deposition on other substrate materials is "blocked" by the blocking layer. The blocking layer can optionally be removed without any eventual adverse effect on the deposited film.

[0025] Some embodiments of the present disclosure incorporate a blocking layer, commonly referred to as a self-assembled monolayer (SAM) or SAM layer. A self-assembled monolayer (SAM) consists of a regular array of spontaneously assembled organic molecules (SAM molecules) adsorbed to a surface. These molecules generally consist of one or more moieties (head groups) that have an affinity for the substrate and a relatively long, inert, linear hydrocarbon portion (tail group). SAM molecules are essentially surfactants that have a hydrophilic functional head with a hydrophobic carbon chain tail.

[0026] SAM formation occurs by fast adsorption of molecular head groups at the surface and slow association of molecular tail groups with each other through van der Waals interactions. SAM precursors are chosen such that the head groups selectively react with the substrate material to be blocked during deposition. Deposition is then performed, and in some embodiments the SAM can be removed, for example, by pyrolysis (with desorption of by-products) or an integration-compatible ashing process.

[0027] A typical process flow for selective deposition can include a) providing a patterned substrate, b) growing a SAM (either by CVD, ALD, or immersion), and c) selectively depositing a film (e.g., by CVD or ALD). In a typical process flow, a SAM is used as a sacrificial layer to enable selective deposition.

[0028] Essentially, the growth of a SAM on a surface is a chemisorption process. The coverage of the SAM layer, determined by the chemisorption kinetics, follows the Elovich equation:

number

[0029] 1 , one or more embodiments of the present disclosure are directed to a processing method 100. A substrate 105 is provided with a first material 110 and a second material 120. The first material 110 has a first surface 112, and the second material 120 has a second surface 122. The first surface 112 is on the first material 110, and the second surface 122 is on the second material 120, which is different from the first material 110.

[0030] In some embodiments, the first material 110 comprises a dielectric material and the second material 120 comprises a conductive material. In some embodiments, the dielectric material comprises one or more of silicon oxide, silicon nitride, silicon carbide, low-k dielectrics, and combinations thereof. In some embodiments, the conductive material comprises one or more of copper, manganese, cobalt, tungsten, ruthenium, or molybdenum. In some embodiments, the first surface comprises a dielectric material consisting essentially of silicon oxide and the second surface comprises a conductive material consisting essentially of copper. As used herein and in the appended claims, the term "consisting essentially of" means that about 95%, 98%, or 99% or more of the specified material is the described material.

[0031] The substrate 105 (including the first surface 112 and the second surface 122) is exposed to a SAM precursor to selectively form a SAM layer 130 on the first material 110 (or the first surface 112) over the second material (or the second surface 122).

[0032] The substrate may be exposed to the SAM precursor by any suitable process. In some embodiments, the substrate is exposed to the SAM precursor by a chemical vapor deposition (CVD) process. In some embodiments, the substrate is exposed to the SAM precursor by an ALD process. In some embodiments, the substrate is exposed to the SAM precursor by a dipping or "wet" process.

[0033] The SAM precursor can be any compound that can selectively form a SAM layer on the first surface 112 over the second surface 122. Generally, the SAM precursor includes at least one blocking molecule. Throughout this disclosure and the appended claims, the terms blocking molecule and surfactant are used interchangeably. Similarly, the terms "SAM layer" and "surfactant layer" are used interchangeably.

[0034] Blocking molecules have the general formula AL, where A is a reactive head group and L is a tail group. In some embodiments, the reactive group may be included at the end of the tail group opposite the head group.

[0035] As used in this manner, a “head group” is any chemical moiety that associates with the first surface 112 and a “tail group” is any chemical moiety that extends away from the first surface 112 .

[0036] In some embodiments, A is (RN) x R' y Si-, where each R and R' is independently selected from C1-C6 alkyl, C1-C6 cycloalkyl, and C1-C6 aryl, x is 1 to 3, and y is 0 to 2. In some embodiments, x+y is equal to 3.

[0037] Some of the reactive head groups include two or more reactive moieties in a single reactive head group attached to a tail group, L. (For example, ((RN)Si- can bind up to three times to a surface). In some embodiments, A includes reactive groups attached to two or more tail groups, L. In these embodiments, each of the tail groups may be the same or different.

[0038] In some embodiments, L is -(CH) n CH3 and n is 0 to 17. In some embodiments, L is -(CH2) n -, n is an integer from 0 to 18, and the reactive group is at the end of the tail group opposite the head group. In some embodiments, the tail group may be branched. In some embodiments, the tail group may be substituted. In some embodiments, the tail group may be unsaturated. In some embodiments, the tail group may comprise a cycloalkyl group or an aryl group.

[0039] In some embodiments, the tail groups associate with each other via relatively slow van der Waals interactions. In some embodiments, the tail groups can be the same or different, allowing for the formation of homogeneous or heterogeneous SAMs. In some embodiments, the SAM precursor includes at least two different blocking molecules, allowing for the formation of heterogeneous SAMs.

[0040] In some embodiments, the blocking compound is a silylamine. In some embodiments, the blocking compound has the general formula ((CH3)2N) x Si(CH3) y ((CH2) z CH3), where x is 1 to 3, y is 0 to 2, x+y is equal to 3, and z is 0 to 17. In some embodiments, z is 5 or less. In some embodiments, z is 0.

[0041] The SAM precursor can be delivered to the substrate as a single compound or as a sequential exposure of multiple compounds to form the SAM layer 130. In some embodiments, the first surface 112 is exposed to a single compound that organizes in an ordered or semi-ordered manner at the surface.

[0042] After formation of the SAM layer 130, the film 115 is deposited on the second surface 122. The amount of film 115 formed on the first surface 112 is less than the amount of film formed on the second surface 122. A measure of the amount of film 115 formed on a surface can be the average thickness of the film formed on each surface. In some embodiments, the film 115 has a first average thickness on the first surface 112 and a second average thickness on the second surface 122. Alternatively, the deposition of the film 115 can be described as selectively depositing the film 115 on the second surface 122 over the first surface 112. Although the film 115 shown in FIG. 1 is not shown on the first surface 112, one skilled in the art will understand that a small amount of deposition may occur.

[0043] In some embodiments, film 115 comprises a metal film. In some embodiments, the film comprises or consists essentially of ruthenium. In some embodiments, after depositing film 115 consisting essentially of ruthenium, a cobalt film is deposited on film 115 to form a Ru-Co capping layer on second material 120.

[0044] The film 115 may be deposited by any suitable process. In some embodiments, the film 115 is deposited by CVD. In some embodiments, the film 115 is deposited by ALD. In some embodiments, the film 115 is deposited by exposing the substrate to multiple reactants. In some embodiments, the multiple reactants are separately exposed to the substrate. In some embodiments, the multiple reactants are separated in time. In some embodiments, the multiple reactants are separated in space.

[0045] Some embodiments of the present disclosure provide a method for improving the selectivity of a selective deposition process. Some embodiments of the present disclosure advantageously provide a method for removing oxide contaminants from a conductive material. Without being bound by theory, it is believed that the selective deposition of a blocking compound relies on the different surface terminations between the first material 110 and the second material 120. Furthermore, the removal of oxide contaminants from the conductive surface increases the -H termination on the conductive material.

[0046] A further typical cleaning method for removing oxide contaminants (H2 plasma) may also damage the -OH termination of the dielectric material. Some embodiments of the present disclosure advantageously remove oxide contaminants without reducing the -OH termination of the dielectric material.

[0047] 2, a cleaning method 200 for improving selectivity is described. The method 200 begins in operation 210 by providing a patterned substrate. In some embodiments, the patterned substrate can be the substrate 105 described above. The patterned substrate includes a conductive material and a dielectric material. The conductive material has oxide contaminants thereon. The dielectric material has an -OH surface termination.

[0048] In some embodiments, the conductive material comprises copper and the oxide contaminants comprise CuO. In some embodiments, the dielectric material comprises SiO2 with -OH surface termination.

[0049] In operation 220, the patterned substrate is exposed to a plasma formed from a nitrogen-containing gas to remove oxide contaminants and form -NH surface terminations on the dielectric material. In some embodiments, all or nearly all of the surface terminations on the dielectric material are converted from -OH terminations to -NH terminations. In some embodiments, more than 10%, more than 25%, more than 50%, more than 80%, or more than 90% of the -OH surface terminations are converted to -NH terminations.

[0050] Without being bound by theory, it is believed that the conversion of -OH terminations to -NH terminations has little or no effect on the selectivity of the blocking compound on the first surface over the second surface. In contrast, conventional oxide removal processes that rely on hydrogen-based plasmas convert at least a portion of the -OH terminations to -H terminations, thereby adversely affecting the selectivity of the blocking compound and subsequently deposited films.

[0051] The nitrogen-containing gas may be any suitable gas that removes oxide contaminants from the conductive material surface. In some embodiments, the nitrogen-containing gas includes one or more of ammonia, diimide, or nitrogen gas (N2). In some embodiments, the nitrogen-containing gas consists essentially of ammonia (NH3). As used in this context, a process gas consisting essentially of a listed gas includes, on a molar basis, 95% or more, 98% or more, 99% or more, or 99.5% or more of the listed gas, excluding inert diluent or carrier gases.

[0052] The plasma may be generated by any suitable means, including, but not limited to, remote plasma and direct plasma. The plasma may be an inductively coupled plasma (ICP) or a conductively coupled plasma (CCP). The plasma may have a power in the range of 200W to 1000W, in the range of 300W to 800W, in the range of 400W to 600W, or in the range of 450W to 550W.

[0053] The substrate may be exposed to the plasma for a period of time sufficient to remove oxide contaminants from the conductive surface, hi some embodiments, the substrate is cleaned by the plasma for a period of time ranging from 0.5 seconds to 30 seconds, from 1 second to 10 seconds, or from 2 seconds to 5 seconds.

[0054] In some embodiments, the method 200 continues in operation 230 by exposing the substrate to a blocking compound. The blocking compound can be any suitable compound for selectively forming a SAM layer on one of the materials of the substrate. In some embodiments, the blocking compound selectively forms a SAM layer on a dielectric material over a conductive material. In some embodiments, the blocking compound is a silylamine as described above. In some embodiments, the blocking compound selectively forms a SAM layer on a conductive material over a dielectric material.

[0055] After formation of the SAM layer, a film may be selectively deposited on the unblocked material surface in operation 240. The film may be deposited by any suitable means, including but not limited to CVD or ALD. In some embodiments, the film comprises ruthenium.

[0056] As discussed above, the plasma formed from the nitrogen-containing gas improves the selectivity of the deposited film. In some embodiments, the selectivity improvement is evident compared to a non-cleaned substrate. In some embodiments, the selectivity of the film is improved by 5% or more, 10% or more, 20% or more, or 25% or more compared to a similar process that does not clean the substrate.

[0057] In some embodiments, the improved selectivity is evident compared to processes utilizing a hydrogen plasma to clean the substrate, in some embodiments, the deposition rate of a film on a substrate cleaned with a nitrogen-containing plasma is at least 5% greater, at least 10% greater, at least 20% greater, at least 30% greater, at least 40% greater, or at least 50% greater than the deposition rate on a substrate cleaned with a hydrogen plasma.

[0058] In optional operation 250, the surfactant layer may be removed. In some embodiments, the surfactant layer is removed by exposure to a plasma or an ashing process. Some embodiments of the present disclosure advantageously provide a surfactant layer that does not adversely affect the conductivity or resistance of the resulting device. Thus, in some embodiments, the surfactant layer is not removed. EXAMPLES

[0059] Two patterned substrates with alternating lines of copper and silicon oxide were prepared for processing. The first substrate was cleaned with a hydrogen plasma. The second substrate was cleaned with an ammonia plasma. Both substrates were exposed to a 400 W plasma at 3 Torr for 10 seconds. Both substrates were exposed to dodecyldimethyl(dimethylamino)silane. Both substrates were exposed to triruthenium dodecacarbonyl and hydrogen gas at 175°C and 5 Torr to selectively deposit ruthenium on the copper lines.

[0060] SEM images of the resulting substrates are shown in Figure 3A (hydrogen plasma) and Figure 3B (ammonia plasma). The hydrogen plasma cleaned substrate shows ruthenium deposits on the darker dielectric lines, demonstrating relatively poor selectivity. In contrast, the ammonia plasma cleaned substrate shows no ruthenium deposits on the dielectric lines, thereby demonstrating excellent selectivity.

[0061] Additionally, the ammonia plasma cleaned substrates demonstrated superior deposition rates for the deposited ruthenium films: for the ammonia plasma cleaned substrates, the deposition rate was 0.028 Å / s compared to only 0.018 Å / s for the hydrogen plasma cleaned substrates.

[0062] Throughout this specification, references to "one embodiment," "some embodiments," "one or more embodiments," or "an embodiment" mean that a particular feature, structure, material, or characteristic described in connection with an embodiment is included in at least one embodiment of the present disclosure. Thus, the appearance of phrases such as "in one or more embodiments," "some embodiments," "in one embodiment," or "in one embodiment" in various places throughout this specification do not necessarily refer to the same embodiment of the present disclosure. Moreover, particular features, structures, materials, or characteristics may be combined in any suitable manner in one or more embodiments.

[0063] Although the disclosure herein has been described with reference to specific embodiments, those skilled in the art will understand that the described embodiments are merely illustrative of the principles and applications of the disclosure. It will be apparent to those skilled in the art that various modifications and variations can be made to the disclosed method and apparatus without departing from the spirit and scope of the disclosure. Thus, the disclosure can include modifications and variations that come within the scope of the appended claims and their equivalents.

Claims

1. 1. A method of selective deposition comprising the steps of: The substrate containing the conductive material and the dielectric material is treated with a compound having the general formula ((CH 3 ) 2 N) x Si(CH 3 ) y ((CH 2 ) z CH 3 ), where x is 1 to 3, y is 0 to 2, x+y is equal to 3, and z is 0 to 17; selectively depositing a film on the conductive material; Including, the film comprises a metal film; the metal film consists essentially of ruthenium; after depositing the metal film consisting essentially of ruthenium, a cobalt cap is deposited on the metal film to form a Ru-Co capping layer; the surfactant layer does not adversely affect the conductivity or resistance of the resulting device; The method, wherein the surfactant layer is not removed after the film is selectively deposited.

2. The method of claim 1 , wherein the conductive material comprises one or more of copper, manganese, cobalt, tungsten, ruthenium, or molybdenum.

3. The method of claim 1 , wherein the dielectric material comprises one or more of silicon oxide or a low-k dielectric.

4. The silylamine is (N(CH 3 ) 2 )Si(CH 3 ) 3 2. The method of claim 1 , consisting essentially of:

5. The method of claim 1 , wherein z is 5 or less.

6. The method of claim 1 , wherein selectively depositing the film comprises a chemical vapor deposition process.

7. A method for improving selectivity includes exposing a substrate including a conductive material having oxide contaminants and a dielectric material having an —OH surface termination to a plasma formed from a nitrogen-containing gas to remove the oxide contaminants and form an —NH surface termination on the dielectric material; exposing the substrate to a surfactant to selectively form a surfactant layer on the dielectric material over the conductive material, or vice versa; selectively depositing a film on the conductive material or the dielectric material, respectively; Including, the film comprises a metal film; the metal film consists essentially of ruthenium; after depositing the metal film consisting essentially of ruthenium, a cobalt cap is deposited on the metal film to form a Ru-Co capping layer; the surfactant layer does not adversely affect the conductivity or resistance of the resulting device; The method, wherein the surfactant layer is not removed after the film is selectively deposited.

8. The method of claim 7 , wherein the conductive material comprises copper and the oxide contaminants comprise CuO.

9. The nitrogen-containing gas is NH 3 , N 2 H 2 , or N 2 The method of claim 7, comprising one or more of:

10. The nitrogen-containing gas is ammonia (NH 3 10. The method of claim 9, consisting essentially of

11. The method of claim 7, wherein the plasma has a power in the range of 300W to 800W.

12. The method of claim 7, wherein the substrate is cleaned by the plasma for a period of between 1 second and 10 seconds.

13. 1. A method of selective deposition comprising the steps of: exposing a substrate including a conductive material having oxide contaminants and a dielectric material having an -OH surface termination to a plasma formed from a nitrogen-containing gas to remove said oxide contaminants and form an -NH surface termination on said dielectric material; The substrate is formed by the general formula (N(CH 3 ) 2 ) x Si(CH 3 ) y ((CH 2 ) z CH 3 ), where x is 1 to 3, y is 0 to 2, x+y is equal to 3, and z is 0 to 5; selectively depositing a film on the conductive material; Including, the film comprises a metal film; the metal film consists essentially of ruthenium; after depositing the metal film consisting essentially of ruthenium, a cobalt cap is deposited on the metal film to form a Ru-Co capping layer; the surfactant layer does not adversely affect the conductivity or resistance of the resulting device; The method, wherein the surfactant layer is not removed after the film is selectively deposited.

14. The method of claim 13 , wherein the conductive material comprises copper and the film comprises ruthenium.

Citation Information

Patent Citations

  • Thickness detection system for patterned wafers

    JP2008532258A

  • Semiconductor device and method of manufacturing the same

    JP2014187307A

  • Selective accumulation by surface treatment

    JP2017222928A

  • Methods for thermally forming a selective cobalt layer

    US20160133563A1