BLOW MOLDING APPARATUS AND BLOW MOLDING METHOD

The blow molding apparatus optimizes preform cooling and mold stability through a temperature adjustment section with locking mechanisms, addressing cycle time and mold opening issues to enhance efficiency and reduce operating time.

JP7570961B2Active Publication Date: 2024-10-22NISSEI ASB MASCH CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2021062629
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-09-25
Filing Date
2021-04-01
Publication Date
2024-10-22
Estimated Expiration
2040-09-18

AI Technical Summary

Technical Problem

Existing blow molding technologies face challenges in shortening the preform cooling time within the injection mold to reduce the container molding cycle, while maintaining efficient operation and preventing mold opening due to compressed air, which can lead to increased operating time and decreased speed.

Method used

A blow molding apparatus with a temperature adjustment section that includes a first drive section for inserting a core mold into the preform and a second drive section for accommodating the preform in a cavity mold, equipped with locking mechanisms to restrict movement and optimize stroke ranges, ensuring efficient cooling and mold stability during the temperature adjustment process.

Benefits of technology

The apparatus achieves a significant reduction in operating time before and after preform cooling, enhances cooling efficiency, and prevents mold opening, thereby shortening the molding cycle time without compromising device speed or increasing actuator size.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007570961000001
    Figure 0007570961000001
  • Figure 0007570961000002
    Figure 0007570961000002
  • Figure 0007570961000003
    Figure 0007570961000003
Patent Text Reader

Abstract

To provide a blow molding device capable of shortening an operating time of a machine before and after cooling a preform.SOLUTION: A temperature adjustment unit of a blow molding device comprises: a first drive unit that drives in a first direction a core mold which supplies cooling air; a second drive unit that drives in a second direction a cavity mold which houses a preform; a first lock unit that, in a first position where the core mold is inserted into the preform, restricts movement of the first drive unit in the second direction; and a second lock unit that, in a second position where the preform is housed in the cavity mold, restricts movement of the second drive unit in the first direction.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a blow molding apparatus and a blow molding method. [Background technology]

[0002] A hot parison type blow molding machine has been known as one of the conventional manufacturing devices for resin containers. The hot parison type blow molding machine is configured to blow mold a resin container by utilizing the heat retained during injection molding of a preform, and is advantageous in that it can manufacture a variety of resin containers with excellent aesthetic appearance compared to the cold parison type.

[0003] For example, various proposals have been made for the purpose of shortening the molding cycle for the hot parison blow molding cycle. In order to shorten these molding cycles, it has been proposed to shorten the injection molding time of the preform (the cooling time of the preform in the injection mold), which is the rate-determining step, and to perform additional cooling of the hot preform in the downstream process (temperature adjustment process) after injection molding (see, for example, Patent Document 1). When additional cooling of the hot preform is performed in the temperature adjustment process after injection molding, a method is also known in which the outer peripheral surface of the preform is brought into contact with a cooling mold to exchange heat, and compressed air is blown into the preform to cool it.

[0004] Furthermore, in this type of blow molding apparatus, it has also been proposed to provide a locking mechanism in the drive device of the blow molding mold in order to prevent the mold from opening or the conveying plate (also called the rotating plate) from floating up due to the blow air that shapes the container (see, for example, Patent Documents 2 and 3). [Prior art documents] [Patent documents]

[0005] [Patent Document 1] Patent No. 6505344 [Patent Document 2] Patent No. 3370124 [Patent Document 3] Patent No. 3467341 Summary of the Invention [Problem to be solved by the invention]

[0006] When shortening the container molding cycle by shortening the cooling time of the preform in the injection mold, it is important to shorten the operating time (dry cycle) of the machines (especially the machines related to the temperature adjustment device) as much as possible before and after cooling the preform, and to ensure sufficient time for cooling the preform with the temperature adjustment device.

[0007] In addition, when cooling the preform by blowing compressed air into it in the temperature adjustment process after injection molding, the temperature adjustment mold may open up and down due to the compressed air introduced into the preform. If the actuator of the temperature adjustment device is enlarged to prevent such mold opening, the driving speed of the temperature adjustment device will decrease and the operation time of the device will become longer, and the time that the temperature adjustment device can cool the preform will be shortened accordingly.

[0008] The present invention has been made in view of the above problems, and has an object to provide a blow molding apparatus that can shorten the operating time of the machine before and after cooling of the preform. [Means for solving the problem]

[0009] A blow molding apparatus according to one aspect of the present invention includes an injection molding section that injection molds a resin preform having a bottom, a temperature adjustment section that supplies cooling air to the preform released from the injection molding section to adjust the temperature of the preform, and a blow molding section that blow molds the preform after temperature adjustment to manufacture a resin container. The temperature adjustment section includes a first drive section that drives a core mold that supplies cooling air in a first direction to insert the core mold into the preform, a second drive section that drives a cavity mold that accommodates the preform in a second direction opposite to the first direction to accommodate the preform in the cavity mold, At least one of the first drive unit and the second drive unit is provided with a lock unit that restricts at least one of the movement of the core mold in the second direction and the movement of the cavity mold in the first direction with respect to a position where the core mold abuts against the preform and the preform is housed in the cavity mold.

[0010] A blow molding apparatus according to another aspect of the present invention includes an injection molding section for injection molding a resin preform having a bottom, a temperature adjustment section for supplying cooling air to the preform released from the injection molding section to adjust the temperature of the preform, and a blow molding section for blow molding the preform after temperature adjustment to manufacture a resin container. The temperature adjustment section includes a first drive section for driving a core mold supplying the cooling air in a first direction to insert the core mold into the preform. , P a second driving unit that drives the cavity mold that accommodates the preform in a second direction opposite to the first direction to accommodate the preform in the cavity mold; A stroke changer that changes the range of movement of the core mold in the first direction or the range of movement of the cavity mold in the second direction is provided in at least one of the first drive unit or the second drive unit. Effect of the Invention

[0011] According to the present invention, the operating time of the machine before and after cooling of the preform can be reduced. [Brief description of the drawings]

[0012] [Figure 1] 1 is a diagram showing a schematic configuration of a blow molding device according to an embodiment of the present invention; [Diagram 2] FIG. 4 is a diagram illustrating an example of the configuration of a temperature adjustment unit. [Diagram 3] FIG. 4 is a diagram showing a configuration of a first driving unit of a temperature adjustment unit. [Figure 4] FIG. 13 is a diagram showing a first lock portion of the first drive portion. [Diagram 5] FIG. 13 is a diagram showing a configuration of a second driving unit of the temperature adjustment unit. [Figure 6] FIG. 13 is a view showing a second lock portion of the second drive portion. [Figure 7] 1 is a flow chart showing steps of a blow molding method. [Figure 8] 4 is a graph showing an example of temperature changes of preforms in the blow molding methods of this embodiment and a comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the embodiments, in order to make the description easier to understand, structures and elements other than the main parts of the present invention will be described in a simplified or omitted manner. In addition, in the drawings, the same elements are given the same reference numerals. Note that the shapes, dimensions, etc. of each element shown in the drawings are shown only for illustrative purposes, and do not represent the actual shapes, dimensions, etc.

[0014] 1 is a diagram showing a schematic configuration of a blow molding apparatus 20 according to the present embodiment. The blow molding apparatus 20 according to the present embodiment is an apparatus of the hot parison type (also called one-stage type) that blow molds a container by utilizing the heat (internal heat) retained during injection molding without cooling a preform 11 (not shown in FIG. 1) to room temperature.

[0015] The blow molding apparatus 20 includes an injection molding section 21, a temperature adjustment section 22, a blow molding section 23, a removal section 24, and a conveying mechanism 26. The injection molding section 21, the temperature adjustment section 22, the blow molding section 23, and the removal section 24 are disposed at positions rotated a predetermined angle (e.g., 90 degrees) around the conveying mechanism 26.

[0016] (Transport mechanism 26) The transport mechanism 26 includes a rotating plate 26a (not shown in FIG. 1) that rotates around an axis in the direction perpendicular to the paper surface of FIG. 1 (Z direction). The rotating plate is composed of a single disk-shaped flat plate member or a plurality of roughly fan-shaped flat plate members divided for each molding station. On the rotating plate 26a, one or more neck molds 27 (not shown in FIG. 1) that hold the neck portion of the preform 11 or a resin container (hereinafter simply referred to as a container) are arranged at each predetermined angle. The transport mechanism 26 includes a rotation mechanism (not shown), and by rotating the rotating plate 26a, the preform 11 (or the container) whose neck portion is held by the neck mold 27 is transported in this order to the injection molding section 21, the temperature adjustment section 22, the blow molding section 23, and the removal section 24. In addition, the conveying mechanism 26 further includes a lifting mechanism (vertical mold opening and closing mechanism) and a neck mold opening mechanism, and performs operations related to raising and lowering the rotating plate 26a, as well as operations related to closing and opening (mold release) the preform 11 in the injection molding section 21.

[0017] (Injection molding section 21) The injection molding section 21 includes an injection cavity mold and an injection core mold (not shown), and manufactures the preform 11. To the injection molding section 21, an injection device 25 that supplies a resin material that is a raw material of the preform 11 is connected.

[0018] In the injection molding section 21, the injection cavity mold, the injection core mold, and the neck mold 27 of the transport mechanism 26 are closed to form a mold space having a preform shape. Then, a resin material is poured from an injection device 25 into the mold space having the preform shape, whereby the preform 11 is manufactured in the injection molding section 21. Here, the overall shape of the preform 11 is a cylindrical shape with one end open and the other end closed at a bottom. A neck is formed at the end of the open side of the preform 11.

[0019] The material of the container and the preform 11 is a thermoplastic synthetic resin, and can be appropriately selected depending on the application of the container. Specific types of materials include, for example, PET (polyethylene terephthalate), PEN (polyethylene naphthalate), PCTA (polycyclohexane dimethylene terephthalate), Tritan (Tritan: copolyester), PP (polypropylene), PE (polyethylene), PC (polycarbonate), PES (polyethersulfone), PPUS (polyphenylsulfone), PS (polystyrene), COP / COC (cyclic olefin polymer), PMMA (polymethyl methacrylate: acrylic), PLA (polylactic acid), etc.

[0020] Incidentally, even when the injection molding section 21 is opened, the neck mold 27 of the transport mechanism 26 is not opened, but continues to hold and transport the preforms 11. The number of preforms 11 simultaneously molded in the injection molding section 21 (i.e., the number of containers that can be simultaneously molded by the blow molding device 20) can be set appropriately. As an example, in this embodiment, four preforms 11 are transported in one molding cycle.

[0021] (Temperature adjustment section 22) Temperature adjustment section 22 adjusts the temperature of preform 11 manufactured in injection molding section 21 to a temperature suitable for the final blow (for example, about 90°C to 105°C) by uniformly heating, removing temperature deviation, and adjusting the temperature distribution. Temperature adjustment section 22 also has the function of cooling preform 11 in a high temperature state after injection molding.

[0022] FIG. 2 is a diagram showing an example of the configuration of the temperature adjustment unit 22. As shown in FIG. The temperature adjustment unit 22 includes a core mold 31 (air inlet / outlet core or temperature control core) that is inserted into (or in contact with) the preform 11, and a cavity mold 32 (temperature control pot) having a temperature control space 33 capable of accommodating the preform 11. The temperature adjustment unit 22 also includes a first drive unit 34 that drives the core mold 31 in the vertical direction (Z direction) in Fig. 2, and a second drive unit 35 that drives the cavity mold 32 in the vertical direction (Z direction) in Fig. 2.

[0023] 2, four preforms 11 are held on the rotating plate 26a by four neck dies 27 provided on a neck die fixing plate 27a attached to the lower surface of the rotating plate 26a. Four core dies 31 and four temperature adjustment spaces 33 of cavity dies 32 are provided in the temperature adjustment section 22, and the positions of the core dies 31 and the temperature adjustment spaces 33 correspond to the positions of the preforms 11 on the XY plane. In addition, the core mold 31 and the first driving unit 34 are arranged on the upper side of the rotating plate 26a (e.g., on the upper base), and the cavity mold 32 and the second driving unit 35 are arranged on the lower side of the rotating plate 26a (e.g., on the machine base (lower base)).

[0024] 2 (Z direction), and has an air supply path (not shown) for introducing compressed air for cooling blow (cooling air) into the preform 11, and an exhaust path (not shown) for exhausting the cooling air from the preform 11. The cooling blow is a process in which compressed air at room temperature (20°C) or below is continuously flowed into the inside (hollow body) of the preform 11, and the preform 11 is cooled from the inside (inner surface) by convection of the compressed air.

[0025] Each core mold 31 is attached to the lower surface of a first driving unit 34 (specifically, a first movable plate 41 described later), and can be moved in the vertical direction (Z direction) in Fig. 2 by the operation of the first driving unit 34. In addition, the core mold 31 is configured to come into close contact with the inner circumference of the neck when inserted into the preform 11, maintaining airtightness between the core mold 31 and the preform 11.

[0026] The cavity mold 32 is attached to the upper surface side of the second drive unit 35, and can be moved in the vertical direction (Z direction) in Fig. 2 by the operation of the second drive unit 35. In addition, an opening of the temperature adjustment space 33 faces the upper surface of the cavity mold 32.

[0027] The temperature adjustment space 33 of the cavity mold 32 has approximately the same shape as the outer shape of the preform 11 manufactured in the injection molding section 21. A flow path (not shown) through which a temperature adjustment medium flows is formed inside the cavity mold 32. Therefore, the temperature of the cavity mold 32 is maintained at a predetermined temperature by the temperature adjustment medium. The cavity mold 32 may be composed of a pair of split molds that are separated along the longitudinal direction of the preform and open and close in the Y direction in the figure.

[0028] Next, a description will be given of the configuration of the first driving unit 34 of the temperature adjustment unit 22. Fig. 3 is a diagram showing the first driving unit 34. In Fig. 3, the core mold 31 is omitted for simplicity. The first driving portion 34 includes a first movable plate 41, a first fixed plate 42, a shaft 43, a first rod 44, a first driving cylinder 45, a first lock portion 46, and a first stroke change portion 47.

[0029] At least two (preferably four) shafts 43 are attached to the underside of the first fixed plate 42 in the first driving section 34. Only a pair of left and right shafts 43 are shown in Fig. 3. The shafts 43 extend in the vertical direction from the upper base 29 fixed at a predetermined height relative to the machine base 28, and the first fixed plate 42 is supported by the shafts 43 in a state where it is fixed at a predetermined height from the upper base 29. In addition, a first driving cylinder 45 is attached to the first fixed plate 42 facing downward, and a pair of first rods 44 extending in the vertical direction are inserted therethrough.

[0030] A first movable plate 41 is disposed below the first fixed plate 42. Each shaft 43 is inserted through the first movable plate 41, and the first movable plate 41 is movable in the up and down direction along the shaft 43. In addition, a core mold 31 is attached to the lower surface of the first movable plate 41 as shown in FIG.

[0031] A piston rod 45a and a first rod 44, which are driven to extend by a first drive cylinder 45, are fixed to the upper surface of the first movable plate 41. When the piston rod 45a extends relative to the first drive cylinder 45, the first movable plate 41 moves downward together with the first rod 44, and when the piston rod 45a contracts relative to the first drive cylinder 45, the first movable plate 41 moves upward together with the first rod 44.

[0032] Two first locking portions 46 are attached to the upper surface side of the first fixed plate 42. Each first locking portion 46 is provided at a position corresponding to the first rod 44, and has a locking piece 46a that advances and retreats in the left-right direction (X direction) in the figure, and a drive mechanism 46b that drives the locking piece 46a. Note that since the two first locking portions 46 have the same configuration, the following description will only describe the configuration of one, and a duplicate description of the other will be omitted.

[0033] FIG. 4(A) is a diagram showing the first locking portion 46 in an unlocked state, and FIG. 4(B) is a diagram showing the first locking portion 46 in a locked state. 4(A), the lock piece 46a of the first locking portion 46 is in a position retracted from the position of the first rod 44. In this unlocked state, the first rod 44 does not interfere with the lock piece 46a, and the first movable plate 41 is movable in the vertical direction.

[0034] 3(B), when the first movable plate 41 moves downward (in the first direction) and reaches the lower end of the stroke, the upper end of the first rod 44 is located below the position of the lock piece 46a. Although not shown in the figure, in this state, the core die 31 is inserted into the preform 11 and is in a position where it comes into contact with the neck portion of the preform 11 and stops. At this time, the lock piece 46a of the first lock part 46 can be moved to the position of the first rod 44 to enter the locked state shown in Fig. 4(B). In this locked state, when the first movable plate 41 is moved upward (in the second direction), the upper end of the first rod 44 abuts against and interferes with the lock piece 46a. Therefore, in the locked state of the first lock part 46, the upward movement of the first movable plate 41, which is located at the lower end side of the stroke, is restricted by the lock piece 46a.

[0035] As described above, in the locked state, the upper end of the first rod 44 abuts against the lock piece 46a, and the core mold 31 supported by the first movable plate 41 cannot move. This creates a state in which the core mold 31 is in reliable abutment (close contact) with the preform 11 supported by the neck mold 27, improving airtightness. In this state, cooling air is introduced from the core mold 31 into the preform 11, and cooling blow is performed. When cooling blow is performed, an upward force is generated in the core mold 31, which makes it easy for the core mold 31 to rise from the molding position, but since the upper end of the first rod 44 is firmly supported by the lock piece 46a, the upward movement of the core mold 31 is suppressed. Therefore, separation of the preform 11 and the core mold 31 is less likely to occur, and the possibility of leakage of cooling air is significantly reduced.

[0036] Returning to FIG. 3, the first stroke changer 47 is provided between the first fixed plate 42 and the first movable plate 41. The first stroke changer 47 has a stopper 48 attached to the lower surface of the first fixed plate 42 and a spacer member 49 attached to the upper surface of the first movable plate 41. The stopper 48 and the spacer member 49 are arranged at opposing (corresponding) positions on the XY plane, and are configured so that the stopper 48 and the spacer member 49 come into contact with each other when the first movable plate 41 is brought closer to the first fixed plate 42. In the example of FIGS. 2 and 3, two first stroke changers 47 are provided between the first fixed plate 42 and the first movable plate 41.

[0037] The stopper 48 is formed of, for example, a shock absorber. The stopper 48 has an upper surface fixed to the first fixed plate 42 and a bottom surface receiving the upper surface of the spacer member 49.

[0038] The spacer member 49 is attached replaceably to determine the upper limit position (the stopping position when the core die 31 is retracted) in the movement range of the first movable plate 41. The spacer member 49 is, for example, a block having a rectangular overall shape, and is fixed to the first movable plate 41 with bolts or the like.

[0039] The spacer member 49 can be selected from a number of types of members having different heights in the vertical direction so that the movement range of the first movable plate 41 is an appropriate dimension for advancing and retracting the core mold 31. For example, the dimension of the spacer member 49 is selected so that the core mold 31 completely comes out of the preform 11 when retracting, does not interfere with the rotating plate 26a, and the movement amount of the core mold 31 is minimized. As an example, FIG. 3(C) shows a state in which a spacer member 49a with a different height from that in FIG. 3(A) is attached. The height ha2 of the spacer member 49a in FIG. 3(C) is greater than the height ha1 of the spacer member 49 in FIG. 3(A) (ha2>ha1). Therefore, in the case of FIG. 3(C), the stopper 48 and the spacer member 49a come into contact when the first movable plate 41 is in a lower position compared to FIG. 3(A), so that the movement range of the first movable plate 41 is smaller. In other words, when the preform 11 is short, a long spacer member 49a is used to reduce the movement amount of the core mold 31, and when the preform 11 is long, a short spacer member 49a is used to increase the movement amount of the core mold 31. With this configuration, the movement amount (stroke amount) of the core mold 31 can be optimally adjusted according to the length of the preform 11.

[0040] Next, a description will be given of the configuration of the second driving unit 35 of the temperature adjustment unit 22. Fig. 5 is a diagram showing the second driving unit 35. In Fig. 5, the cavity mold 32 is omitted for simplicity. The second driving portion 35 includes a second movable plate 51, a second fixed plate 52, a second rod 54, a second driving cylinder 55, a second lock portion 56, and a second stroke change portion 57.

[0041] The second fixed plate 52 in the second drive unit 35 is fixed onto the machine base (lower base) 28. A second drive cylinder 55 is attached facing upward to the second fixed plate 52, and at least two (preferably two pairs (four)) second rods 54 extending in the vertical direction are inserted therethrough. FIG. 5 shows the second drive unit 35 provided with two pairs (four) of second rods 54. FIG. 5 shows only the front pair of the two pairs of second rods 54 arranged in parallel in the depth direction (Y direction) in the second drive unit 35.

[0042] A second movable plate 51 is disposed above the second fixed plate 52. The second movable plate 51 is supported from below by two or more (e.g., four) shafts (not shown) extending in the vertical direction, and is movable in the vertical direction along the shafts. In addition, a cavity mold 32 is attached to the upper surface of the second movable plate 51 as shown in FIG. 2.

[0043] A piston rod 55a, which is driven to extend by a second drive cylinder 55, and a second rod 54 are fixed to the lower surface of the second movable plate 51. When the piston rod 55a extends relative to the second drive cylinder 55, the second movable plate 51 moves upward together with the second rod 54, and when the piston rod 55a contracts relative to the second drive cylinder 55, the second movable plate 51 moves downward together with the second rod 54.

[0044] Two second locking parts 56 are attached to the upper surface side of the second fixed plate 52. Each second locking part 56 is provided at a position where the second rod 54 is disposed in the left-right direction (X direction) in the figure, and has a locking piece 56a that advances and retreats in the X direction, and a driving mechanism 56b that drives the locking piece 56a. The driving mechanism 56b has a driving rod 56e, and the driving rod 56e and its locking piece 56a are connected via a free joint 56d. Note that since the two second locking parts 56 have the same configuration, the following description will describe the configuration of one, and a duplicate description of the other will be omitted.

[0045] FIG. 6(A) is a diagram showing the second locking portion 56 in an unlocked state, and FIG. 6(B) is a diagram showing the second locking portion 56 in a locked state. 6(A), the lock piece 56a of the second locking portion 56 is in a position retracted from the position of the second rod 54. In this unlocked state, the second rod 54 does not interfere with the lock piece 56a, and the second movable plate 51 is movable in the vertical direction.

[0046] 5(B), when the second movable plate 51 moves upward (in the second direction) and reaches the upper end of the stroke, the lower end of the second rod 54 is located above the position of the lock piece 56a. Although not shown in the figure, in this state, the preform 11 is housed in the cavity mold 32, and the cavity mold 32 is in a position where it abuts against the neck mold 27 and stops. At this time, the lock piece 56a of the second lock section 56 can be moved to the position of the second rod 54 to enter the locked state shown in Fig. 6(B). In this locked state, when the second movable plate 51 is moved downward (in the first direction), the lower end of the second rod 54 abuts against and interferes with the lock piece 56a. Therefore, in the locked state of the second lock section 56, the downward movement of the second movable plate 51, which is located at the upper end side of the stroke, is restricted by the lock piece 56a.

[0047] Here, the basic configuration of the second locking portion 56 is similar to that of the first locking portion 46, but differs in that an inclined surface is formed on the upper surface side of the receiving portion 56c that receives the locking piece 56a and on the lower surface side of the locking piece 56a.

[0048] Specifically, the surface 56c1 of the receiving portion 56c that receives the lock piece 56a and the lower surface 56a1 of the lock piece 56a each form a wedge-shaped inclined surface that is inclined upward toward the direction in which the lock piece 56a extends. Therefore, as shown in FIG. 6B, when the lock piece 56a of the second locking portion 56 is extended, the surface 56c1 of the receiving portion 56c is pressed against the lower surface 56a1 of the lock piece 56a, generating a reaction force toward the upper side, and the movement of the lock piece 56a in the extension direction is converted into a force in the upward direction. In addition, a free joint 56d is provided between the lock piece 56a and the driving mechanism 56b (driving rod 56e). Therefore, it is possible to prevent the driving mechanism 56b (driving rod 56e) that advances and retreats in the X direction from becoming eccentric or tilting in the Z direction, and it is possible to move only the lock piece 56a smoothly upward by a predetermined amount while preventing damage to the driving mechanism 56b.

[0049] As described above, when the lower end of the second rod 54 is pushed up by the lock piece 56a in the locked state, the cavity mold 32 supported by the second movable plate 51 is also pushed up. This creates a state in which the cavity mold 32 is firmly abutted (closely attached) to the neck mold 27 of the rotating plate 26a. In this state, the preform 11 held by the neck mold 27 is accommodated in the cavity mold 32. Next, the temperature adjustment unit 22 introduces cooling air into the preform 11 (performs cooling blow). When the cooling blow is performed, a downward force is generated in the cavity mold 32, which tends to cause the cavity mold 32 to drop from the molding position, but since the lower end of the second rod 54 is firmly supported by the lock piece 56a, the downward movement (mold opening) of the cavity mold 32 is suppressed. Therefore, misalignment (such as misalignment) between the preform 11 and the cavity mold 32 is unlikely to occur, and the possibility that the preform 11 will come into contact with the cavity mold 32 in a misaligned state during cooling blowing is significantly reduced, making it impossible to perform appropriate temperature control. The downward force of the cooling air that the cavity mold 32 receives is transmitted from the lower end of the second rod 54 to the lock piece 56a, and the lock piece 56a is pressed against the surface 56c of the receiving portion 56c. 1 Therefore, the force of the drive mechanism 56 b The horizontal force must be set to be greater than the horizontal force generated in the receiving portion 56c by the cooling air.

[0050] Returning to FIG. 5, the second stroke changer 57 is provided between the machine base 28 and the second movable plate 51. The second stroke changer 57 has a stopper 58 attached to the machine base 28 and a spacer member 59 attached to the lower surface of the second movable plate 51. The stopper 58 and the spacer member 59 are arranged at positions facing each other (corresponding) on ​​the XY plane, and are configured so that the stopper 58 and the spacer member 59 come into contact with each other when the second movable plate 51 is brought closer to the machine base 28. In the example of FIG. 2 and FIG. 5, two stroke changers 57 are provided between the machine base 28 and the second movable plate 51. The stopper 58 may be provided on the second fixed plate 52 that is connected to the machine base 28 and movably supports the second movable plate 51.

[0051] The stopper 58 is formed of, for example, a shock absorber. The lower surface of the stopper 58 is fixed to the machine base 28, and the upper surface of the stopper 58 receives the bottom surface of the spacer member 59.

[0052] The spacer member 59 is attached replaceably to define a lower limit position (a stopping position when the cavity mold 32 is retracted) in the movement range of the second movable plate 51. The spacer member 59 is, for example, a block having a rectangular overall shape, and is fixed to the second movable plate 51 with bolts or the like.

[0053] The spacer member 59 can be selected from a number of types of members having different heights in the vertical direction so that the movement range of the second movable plate 51 is an appropriate dimension for advancing and retracting the cavity mold 32. For example, the dimension of the spacer member 59 is selected so that the preform 11 completely comes out of the cavity mold 32 during retraction without interfering with it, and the amount of movement of the cavity mold 32 is minimized. As an example, FIG. 5(C) shows a state in which a spacer member 59a with a different height from that in FIG. 5(A) is attached. The height hb2 of the spacer member 59a in FIG. 5(C) is greater than the height hb1 of the spacer member 59 in FIG. 5(A) (hb2>hb1). Therefore, in the case of FIG. 5(C), the stopper 58 and the spacer member 59a come into contact when the second movable plate 51 is in a higher position than in FIG. 5(A), so that the movement range of the second movable plate 51 is smaller. In other words, when the preform 11 is short, a long spacer member 59a is used to reduce the movement amount of the cavity mold 32, and when the preform 11 is long, a short spacer member 59a is used to increase the movement amount of the cavity mold 32. With this configuration, the movement amount (stroke amount) of the cavity mold 32 can be optimally adjusted according to the length of the preform 11.

[0054] (Blow molding section 23) Returning to FIG. 1, the blow molding section 23 performs blow molding on the preform 11 whose temperature has been adjusted in the temperature adjustment section 22, to manufacture a container. The blow molding section 23 includes a blow cavity mold, which is a pair of split molds corresponding to the shape of the container, an air introduction member (neither of which is shown) that also serves as a stretching rod, and an exhaust path (not shown in FIG. 1) for exhausting blow air from inside the container. The blow molding section 23 blow molds the preform 11 while stretching it. This allows the preform 11 to be shaped into the shape of the blow cavity mold to manufacture a container.

[0055] (Removal part 24) The removal section 24 is configured to release the neck of the container manufactured in the blow molding section 23 from the neck mold and remove the container to the outside of the blow molding apparatus 20.

[0056] (Explanation of the blow molding method) 7 is a flowchart showing steps of the blow molding method by the blow molding apparatus 20 of this embodiment. In this embodiment, before each step (S101 to S104) of the blow molding method described below is performed, a stroke changing step (S1 to S2) is performed to change the movement ranges of the first drive unit 34 and the second drive unit 35 in the temperature adjustment unit.

[0057] (Steps S1 to S2: Stroke change process) In the stroke changing step, when the movement range of the first drive part 34 is changed, the following operations are performed. First, a value is obtained by subtracting the stroke required to insert and remove the core mold 31 from the value of the maximum movement range of the first drive unit 34. Then, a member having a height equivalent to the value obtained above is prepared as the spacer member 49 to be used by the first drive unit 34 (S1: spacer member preparation step). Then, the prepared spacer member 49 is attached to the upper surface of the first movable plate 41 (S2: spacer member attachment step). This makes the movement range of the first drive unit 34 coincide with the stroke required to insert and remove the core mold 31.

[0058] Similarly, in the stroke changing step, when the movement range of the second drive part 35 is changed, the following operations are performed. First, a value is obtained by subtracting the stroke required to insert and remove the preform 11 from the cavity mold 32 from the value of the maximum movement range of the second driving unit 35. Then, a member having a height equivalent to the above-mentioned obtained value is prepared as a spacer member 59 to be used by the second driving unit 35 (S1: spacer member preparation step). Then, the prepared spacer member 59 is attached to the lower surface of the second movable plate 51 (S2: spacer member attachment step). This makes the movement range of the second driving unit 35 coincide with the stroke required to insert and remove the preform 11 from the cavity mold 32. When the stroke change process is completed, the following steps (blow molding cycle) of the blow molding method are performed. Note that the stroke change process is desirably performed simultaneously with the mold installation process for installing the mold for the injection molding part, the mold for the temperature adjustment part, the mold for the blow molding part, and the mold for the removal part to the blow molding device 20.

[0059] (Step S101: Injection molding process) First, in the injection molding section 21, resin is injected from the injection device 25 into a preform-shaped mold space formed by the injection cavity mold, the injection core mold, and the neck mold 27 of the transport mechanism 26, to produce the preform 11.

[0060] In step S101, the injection molding section 21 is opened immediately after the end of resin filling or after a minimum cooling time provided after the resin filling. That is, the preform 11 is released from the injection cavity mold and the injection core mold at a high temperature enough to maintain the outer shape of the preform 11. Then, the rotating plate 26a of the transport mechanism 26 rotates by a predetermined angle, and the preform 11 held by the neck mold 27 is transported to the temperature adjustment section 22.

[0061] Here, referring to Fig. 8, the temperature change of the preform 11 in the blow molding method of this embodiment will be described. The vertical axis of Fig. 8 indicates the temperature of the preform, and the horizontal axis of Fig. 8 indicates time. In Fig. 8, an example of the temperature change of the preform of this embodiment is shown in Fig. 8(A). Also, an example of the temperature change of the preform of a comparative example (conventional method) described later is shown in Fig. 8(B). Note that the gap between each process is the time required to transport the preform or container, and is the same.

[0062] In this embodiment, when the resin material is injection molded at a temperature equal to or higher than the melting point of the resin material, the injection molding section 21 performs only the minimum cooling of the preform 11 after injection molding, and the temperature adjustment section 22 performs cooling and temperature adjustment of the preform 11. In this embodiment, the time to cool the resin material after the injection of the resin material is completed in the injection molding section 21 (cooling time) is preferably 1 / 2 or less of the time to inject the resin material (injection time). In addition, the time to cool the resin material can be shorter than the time to inject the resin material depending on the weight of the resin material. The time to cool the resin material is more preferably 2 / 5 or less of the time to inject the resin material, even more preferably 1 / 4 or less, and particularly preferably 1 / 5 or less. Since the cooling time is significantly shorter than that of the comparative example, the skin layer (surface layer in a solidified state) of the preform is thinner than before, and the core layer (inner layer in a softened or molten state) is formed thicker than before. That is, compared to the comparative example, the thermal gradient between the skin layer and the core layer is large, and a preform having high retained heat is molded at a high temperature.

[0063] In this embodiment, the injection molded preform is demolded from the injection molding section 21 at a demolding temperature higher than that of the comparative example, and is transported to the temperature adjustment section 22. As the preform moves to the temperature adjustment section 22, the temperature of the preform is homogenized by heat exchange (thermal conduction) between the skin layer and the core layer. In addition, the preform is slightly cooled from the outer surface due to contact with the outside air. However, the temperature of the preform is maintained at approximately the high demolding temperature until it is transported to the temperature adjustment section 22. In the temperature adjustment section 22, the temperature of the preform is reduced from the high demolding temperature to the blow temperature, and the temperature of the preform is then maintained at the blow temperature until blow molding is performed. The blow temperature is a temperature suitable for blow molding, and is set to, for example, 90°C to 105°C for PET resin. However, a lower blow temperature improves the stretch orientation of the preform and can increase the strength (physical properties) of the container. Therefore, it is preferable to set the blow temperature to, for example, 90°C to 95°C for PET resin.

[0064] Here, the times for the injection molding process, temperature adjustment process, blow molding process, and container removal process are all the same due to the structure of the blow molding apparatus 20. Similarly, the transport times between each process are also the same.

[0065] On the other hand, as a comparative example, an example of temperature change of a preform when the preform is cooled in the injection molding process (FIG. 8(B)) will be described. In the comparative example, the preform is cooled in the mold of the injection molding section 21 to a temperature lower than or approximately equal to the blow temperature. As a result, the injection molding process time in the comparative example is longer than in the present embodiment. Then, the time of each process is set according to the time of the longest injection molding process, and as a result, the molding cycle time of the container is also longer.

[0066] (Step S102: Temperature adjustment process) Next, in the temperature adjusting section 22, temperature adjustment is performed to bring the temperature of the preform 11 close to a temperature suitable for the final blow.

[0067] In the temperature adjustment step, first, the preform 11 is accommodated in the temperature adjustment space 33 of the cavity mold 32 by driving the second driving part 35. At this time, the second locking part 56 is in a locked state, and the cavity mold 32 supported by the second movable plate 51 is restricted from moving downward. Next, the core mold 31 is inserted into the preform 11 by driving the first driving part 34. At this time, the first locking part 46 is in a locked state, and the core mold 31 supported by the first movable plate 41 is restricted from moving upward.

[0068] Thereafter, cooling air is introduced into the preform 11 from the air supply passage of the core mold 31, and the cooling air is exhausted from the exhaust passage of the core mold 31 (cooling blow is performed). The preform 11 is cooled from the inside by such convection of the cooling air. At this time, the preform 11 continues to be in contact with the cavity mold 32, so the temperature of the preform 11 is adjusted and cooled so that it does not become lower than a temperature suitable for blow molding from the outside, and further, the temperature deviation caused during injection molding is also reduced. Note that the temperature adjustment space 33 of the cavity mold 32 has approximately the same shape as the preform 11, so the shape of the preform 11 does not change significantly in the temperature adjustment section 22. Note that the cavity mold 32 may be composed of a pair of split molds, and a preliminary blow (a process in which the preform is temporarily inflated with compressed air to a size smaller than the container before the final blow) may be performed before the cooling blow.

[0069] When the cooling and temperature adjustment of the preform 11 is completed, the first locking portion 46 and the second locking portion 56 are both released from their locked states, and the cavity mold 32 and the core mold 31 are respectively retracted. Then, the rotating plate 26a of the transport mechanism 26 rotates a predetermined angle, and the temperature-adjusted preform 11 held in the neck mold 27 is transported to the blow molding section 23.

[0070] (Step S103: Blow molding process) Next, in the blow molding section 23, blow molding (final blow) of the container is carried out. First, the blow molding die is closed to accommodate the preform 11 in the die space, and a blow core die and a stretch rod are inserted into the neck of the preform 11. Then, while lowering the stretch rod, blow air is introduced from the blow core die into the preform 11. As a result, the preform 11 is bulged and shaped so as to fit closely into the die space of the blow molding die, and is blow molded into a container.

[0071] (Step S104: container removal process) When the blow molding is completed, the blow molding die is opened, which allows the container to be removed from the blow molding section 23. Next, the rotating plate 26a of the transport mechanism 26 rotates a predetermined angle, and the container is transported to the removal section 24. In the removal section 24, the neck of the container is released from the neck mold 27, and the container is removed to the outside of the blow molding apparatus 20.

[0072] This completes the series of steps in the blow molding method. Thereafter, the rotating plate 26a of the conveying mechanism 26 is rotated by a predetermined angle, and the above steps S101 to S104 are repeated.

[0073] The effects of the blow molding apparatus and the blow molding method of the present embodiment will be described below. When a hot parison type preform is molded using a crystalline thermoplastic resin (a resin that can be in a transparent amorphous state or a cloudy crystalline state), depending on the material, it may turn white (cloudy) due to insufficient cooling. For example, when PET resin is used as the material, if the preform is slowly cooled (for example, cooled at room temperature for several tens of seconds) in a temperature range where crystallization is promoted (120℃ to 200℃), crystallization due to the generation of spherulites occurs, and it tends to turn white. Therefore, in the past, the injection molding die for the preform was rapidly cooled (for example, at 10°C for 5 seconds) to shorten the time it took to pass through the above-mentioned crystallization temperature range, thereby allowing the preform to be cooled sufficiently during the injection molding process and preventing whitening of the preform.

[0074] In contrast, according to the blow molding method of this embodiment, the cooling step of the preform 11 is almost eliminated in the injection molding step (S101), and the preform is cooled in the temperature adjustment step (S102). In the temperature adjustment step (S102), cooling air is introduced into the preform 11 and the preform 11 is brought into close contact with the cavity mold 32 to adjust the temperature of the preform 11 and cool it. In this embodiment, since the temperature adjustment and cooling of the preform 11 can be performed in the temperature adjustment step (S102), the preform 11 can be released even in a high temperature state in the injection molding step (S101), and molding of the next preform 11 can be started quickly. That is, according to this embodiment, a container can be molded well while shortening the molding cycle time compared to the molding cycle time of the comparative example.

[0075] Furthermore, according to the blow molding method of this embodiment, in the stroke change process (S1 to S2), the movement range of the first drive unit 34 is adjusted to the stroke required to insert and remove the core mold 31, and the movement range of the second drive unit 35 is adjusted to the stroke required to insert and remove the preform 11 from the cavity mold 32. This allows the strokes of the first drive unit 34 and the second drive unit 35 of the temperature adjustment unit 22 to be optimized in accordance with the dimensions of the preform, and eliminates the need to move the first drive unit 34 and the second drive unit 35 excessively in the temperature adjustment step (S102) compared to when such adjustment is not performed. Therefore, in this embodiment, the operating time of the machine before and after the temperature adjustment and cooling of the preform 11 is shortened.

[0076] In other words, by shortening the operating time of the machine in the temperature adjustment step, the time for temperature adjustment and cooling of the preform 11 within a certain molding cycle time can be extended accordingly. Therefore, according to this embodiment, the cooling effect of the preform 11 in the temperature adjustment step is improved, and the molding cycle time can be easily shortened.

[0077] Furthermore, according to this embodiment, when cooling air is introduced into the preform 11 to cool it during the temperature adjustment process, the upward movement of the core mold 31 and the first movable plate 41 is restricted by the operation of the first locking portion 46, and the downward movement of the cavity mold 32 and the second movable plate 51 is restricted by the operation of the second locking portion 56. This makes it possible to suppress the core mold 31 and the cavity mold 32 from opening when cooling air is introduced into the preform 11 in the temperature adjustment process. In addition, it is not necessary to increase the size of the actuator as a measure against the above-mentioned mold opening. The first locking portion 46 and the second locking portion 56 can increase the mold holding force of the temperature adjustment portion 22 compared to a standard case that does not have these configurations. That is, according to this embodiment, it is possible to prevent the core mold 31 and the cavity mold 32 from being opened while avoiding a decrease in the operating speed of the device due to an increase in the size of the actuator. Moreover, according to this embodiment, it is possible to prevent a decrease in the operating speed and an increase in the occupied space due to an increase in the size of the actuator.

[0078] The present invention is not limited to the above-described embodiment, and various improvements and design changes may be made without departing from the spirit of the present invention.

[0079] In addition, the embodiments disclosed herein should be considered to be illustrative and not restrictive in all respects. The scope of the present invention is defined by the claims, not the above description, and is intended to include all modifications within the meaning and scope of the claims. [Explanation of symbols]

[0080] Reference Signs List 11...preform, 20...blow molding device, 21...injection molding section, 22...temperature adjustment section, 23...blow molding section, 31...core mold, 32...cavity mold, 34...first drive section, 35...second drive section, 41...first movable plate, 44...first rod, 46...first lock section, 47...first stroke change section, 49...spacer member, 51...second movable plate, 54...second rod, 56...second lock section, 57...second stroke change section

Claims

1. an injection molding unit that injection molds a resin preform having a bottom; a temperature adjustment unit that supplies cooling air to the preform released from the injection molding unit to adjust the temperature of the preform; a blow molding section for blow molding the preform after temperature adjustment to manufacture a resin container, The temperature adjustment unit is a first driving unit that drives the core mold that supplies the cooling air in a first direction to bring the core mold into contact with the preform; a second driving unit that drives a cavity mold that accommodates the preform in a second direction opposite to the first direction to accommodate the preform in the cavity mold, a locking portion that restricts at least one of a movement of the core mold in the second direction and a movement of the cavity mold in the first direction with respect to a position where the core mold abuts against the preform and the preform is accommodated in the cavity mold is provided on at least one of the first driving portion and the second driving portion. Blow molding equipment.

2. The lock portion is provided on the first drive portion. The blow molding apparatus of claim 1 .

3. The lock portion is provided on the second drive portion. The blow molding apparatus of claim 1 .

4. The first drive unit includes: A first movable plate supporting the core mold; a first rod extending from the first movable plate in the second direction and moving together with the first movable plate; The locking portion has a locking piece that advances and retreats in a direction intersecting the second direction, The lock piece interferes with the first rod that moves in the first direction when extended, thereby restricting the movement of the first movable plate in the second direction. The blow molding apparatus of claim 2.

5. The second drive unit includes: a second movable plate supporting the cavity mold; a second rod extending from the second movable plate in the first direction and moving together with the second movable plate; The locking portion has a locking piece that advances and retreats in a direction intersecting the first direction, The lock piece interferes with the second rod that moves in the second direction when extended, thereby restricting the movement of the second movable plate in the first direction.

4. The blow molding apparatus of claim 3.

6. an injection molding unit that injection molds a resin preform having a bottom; a temperature adjustment unit that supplies cooling air to the preform released from the injection molding unit to adjust the temperature of the preform; a blow molding section for blow molding the preform after temperature adjustment to manufacture a resin container, The temperature adjustment unit is a first driving unit that drives the core mold that supplies the cooling air in a first direction to bring the core mold into contact with the preform; a second driving unit that drives a cavity mold that accommodates the preform in a second direction opposite to the first direction to accommodate the preform in the cavity mold, a stroke change unit that changes a movement range of the core mold in the first direction or a movement range of the cavity mold in the second direction is provided in at least one of the first drive unit or the second drive unit; Blow molding equipment.

7. The stroke change unit is provided in the first drive unit.

7. The blow molding apparatus of claim 6.

8. The stroke change unit is provided in the second drive unit.

7. The blow molding apparatus of claim 6.

9. a first spacer member that determines a stop position of the first driving unit when the core die is retracted is replaceably attached to the stroke change unit; 8. The blow molding apparatus of claim 7.

10. a second spacer member that determines a stop position of the second drive unit when the cavity mold is retracted is replaceably attached to the stroke change unit; 9. The blow molding apparatus of claim 8.

11. An injection molding process of injection molding a resin preform having a bottom; a temperature adjustment step of supplying cooling air to the preform released after injection molding to adjust the temperature of the preform; a blow molding process section for producing a resin container by blow molding the preform after temperature adjustment, In the temperature adjustment step, a first driving unit drives the core mold that supplies the cooling air in a first direction to bring the core mold into contact with the preform; A cavity mold for accommodating the preform is driven in a second direction opposite to the first direction by a second driving unit to accommodate the preform in the cavity mold; a locking portion provided on at least one of the first driving portion and the second driving portion restricts at least one of the movement of the core mold in the second direction and the movement of the cavity mold in the first direction with respect to a position where the core mold abuts against the preform and the preform is accommodated in the cavity mold; Blow molding method.

12. A blow molding method using the blow molding apparatus according to claim 6, a stroke changing step of changing at least one of a movement range of the first drive unit in the first direction and a movement range of the second drive unit in the second direction by the stroke changing unit; After the stroke changing step, An injection molding process of injection molding a resin preform having a bottom; a temperature adjustment step of supplying cooling air to the preform released after injection molding to adjust the temperature of the preform; and a blow molding step of blow molding the preform after temperature adjustment to produce a resin container.

Citation Information

Patent Citations

  • Method and device for manufacturing biaxially oriented blow molded vessel

    JP1991234520A

  • Preform, die, production device and production method

    JP2017087651A

  • Control method of blow molding method for containers made of plastic material

    JP2017524572A

  • Blow molding apparatus and blow molding method

    JP3370124B2

  • blow molding machine

    JP3467341B2