Method for fabricating a three-dimensional memory structure of a NOR memory string

The manufacturing process for three-dimensional NOR memory arrays addresses density and power dissipation challenges by forming thin film storage transistors in shafts and trenches, enhancing the efficiency and speed of memory operations.

JP7573721B2Active Publication Date: 2024-10-25SUNRISE MEMORY CORP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023504165
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-07-21
Filing Date
2021-07-21
Publication Date
2024-10-25
Estimated Expiration
2041-07-21

AI Technical Summary

Technical Problem

Existing three-dimensional NOR memory arrays face challenges in achieving high density and low power dissipation while maintaining desirable operational speeds, particularly in the formation of thin film storage transistors within semiconductor substrates.

Method used

A manufacturing process that forms thin film storage transistors in three-dimensional memory structures by creating shafts and trenches in a semiconductor substrate, using a sequence of deposition and etching steps to form conductive and insulating layers, including charge trapping layers and conductive materials like titanium nitride and tungsten, to create efficient storage cells.

Benefits of technology

The process enhances the density and reduces power dissipation of three-dimensional NOR memory arrays, enabling faster and more efficient memory operations by optimizing the structure and conductivity of the memory cells.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007573721000001
    Figure 0007573721000001
  • Figure 0007573721000002
    Figure 0007573721000002
  • Figure 0007573721000003
    Figure 0007573721000003
Patent Text Reader

Abstract

A method for fabricating a three-dimensional NOR memory array provides the thin-film storage transistors of each NOR memory string in a shaft or in a portion of a trench between adjacent shafts.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a process for fabricating memory integrated circuits, and more particularly to a process for fabricating thin film storage transistors in a three-dimensional memory structure formed on the surface of a semiconductor substrate. [Background technology]

[0002] (CROSS-REFERENCE TO RELATED ART) High density memory arrays, e.g., three-dimensional arrays of NOR memory strings ("3D NOR memory arrays"), are disclosed, for example, in U.S. Patent Application Publication No. 2017 / 0092371A1, entitled "Capacitive-Coupled Non-Volatile Thin-film Transistor Strings in Three-Dimensional Arrays" ("Structure Document I"), and U.S. Patent Application Publication No. 2018 / 0366489A1, entitled "3-Dimensional NOR Memory Array Architecture and Methods for Fabrication There of" ("Structure Document II"). The disclosures of Structure Documents I and II (collectively hereinafter referred to as "Structure Documents") are incorporated herein by reference in their entirety. These 3D NOR memory arrays can operate to provide memory circuits with high density and capacity as well as memory circuits with highly desirable speeds that rival conventional memory circuits, such as, for example, dynamic random access memories ("DRAMs"), which have much lower circuit density and significantly higher power dissipation.

[0003] In some structural literature embodiments, a 3D NOR memory array includes multiple stacks of NOR memory strings, each stack having multiple NOR memory strings stacked one on top of the other. In the disclosure, a NOR memory string includes multiple storage cells sharing a common drain region (a "common bit line") and a common source region (a "common source line"), the storage cells being provided on one or both sides along the length of the NOR memory string. Each storage cell is controlled by a conductor (a "word line" or "local word line") that is substantially perpendicular to the memory string. Each word line may be shared by multiple storage cells in different NOR memory strings along its length. Summary of the Invention

[0004] According to one embodiment of the present invention, a method for fabricating a three-dimensional NOR memory array provides each thin-film storage transistor of a NOR memory string in a portion of a shaft or a trench between adjacent shafts.

[0005] According to the embodiment, the method may include: (i) providing a semiconductor structure on a planar surface of a semiconductor substrate, the semiconductor structure including a plurality of active multilayers stacked on top of one another along a first direction substantially perpendicular to the planar surface, adjacent active multilayers being electrically insulated from one another by layers of dielectric material, and each active multilayer including first and second semiconductor layers of a first conductivity type separated from one another by the dielectric material, (ii) providing a plurality of shafts arranged in a regular pattern substantially orthogonal to one another and along both a second direction and a third direction, each of which is orthogonal to the first direction, extending depthwise through the semiconductor structure along the first direction and having a predetermined magnitude along the second direction, and (iii) providing a plurality of shafts each of which is arranged in a regular pattern substantially orthogonal to one another and along both a second direction and a third direction, each of which is orthogonal to the first direction, the shafts extending depthwise through the semiconductor structure along the first direction and having a predetermined magnitude along the second direction, the ... the first direction and arranged in a regular pattern along the second direction and having a predetermined magnitude along the second direction, the shafts each of which is arranged in a regular pattern substantially orthogonal to the first direction and arranged in a regular pattern along the second direction and having a predetermined magnitude along the second direction, the shafts each of which is arranged in a regular pattern substantially orthogonal to the first direction and arranged in a regular pattern along the second direction and having a predetermined magnitude along the second A method comprising: providing a plurality of trenches in a semiconductor structure, the trenches extending depthwise along a first direction and longitudinally along a third direction, the trenches (a) intersecting a plurality of the shafts in the second direction, and (b) having a width along the second direction less than a size of the shafts; and (iv) forming, either in (a) each shaft or in (b) a portion between adjacent ones of the shafts of each trench, (1) a third semiconductor layer of a second conductivity type different from the first conductivity type formed adjacent to and in contact with the first and second semiconductor layers of each active multilayer, (2) a charge trapping layer adjacent to the third semiconductor layer, and (3) a conductor layer (in contact with the charge trapping layer), the conductor layer may include, for example, a metal liner (e.g., titanium nitride) and a filler conductive material (tungsten (W)).

[0006] In this embodiment, the first and second semiconductor layers, the third semiconductor layer, the charge trapping layer, and the conductor of each active multilayer respectively provide a common bit line, a common source line, a channel region, a charge storage layer, and gate electrodes of the thin film storage transistors in the NOR memory string.

[0007] A portion of each trench between adjacent shafts is filled with an insulating material when the third semiconductor layer is formed in each shaft, and similarly, each shaft is filled with an insulating material when the third semiconductor layer is formed in said portion of each trench between adjacent shafts.

[0008] In one embodiment, each of the active multilayers may further include a conductive layer adjacent and in contact with at least one of the first and second semiconductor layers. The conductive layer in each active multilayer may be formed by replacing a sacrificial layer in each active multilayer. The conductive layer may be formed using an atomic layer deposition (ALD) conductive material, such as tungsten.

[0009] In one embodiment, the charge trapping layer includes a tunneling layer (eg, silicon oxide), a charge storage layer, and a blocking layer (eg, silicon oxide, aluminum oxide, or both).

[0010] In one embodiment, prior to providing the trench in the semiconductor structure, the shaft is lined with a dielectric liner (eg, an oxide liner) and filled with a sacrificial material (eg, carbon or tungsten).

[0011] The present invention can be better understood from the following detailed description considered in conjunction with the accompanying drawings. [Brief description of the drawings]

[0012] [Figure 1] 1 is a schematic top view of a modular unit ("tile") 100 in a memory structure including a three-dimensional NOR memory array, according to one embodiment of the present invention. [Figure 2A-1] 2 shows a cross-section in the ZX plane of memory structure 200 after deposition of multiple layers of material (described below), according to one embodiment of the present invention. [Figure 2A-2] 2A-2C illustrate continuous recessing and etching steps to create the stepped portion 102a or 102b of FIG. 1, according to one embodiment of the present invention. [Figure 2B-1] 1 is a top view of the array portion 101 of the memory structure 200. FIG. [Figure 2B-2]FIG. 2B-1 illustrates a cross-section in the XZ plane of memory structure 200 along line A-A' of FIG. 2B-1 after an etching step creates shaft 218 down to etch stop layer 202 in one embodiment of the present invention. [Figure 2C-1] 2 shows a top view of the resulting memory structure 200 after the hard mask 225 is patterned, according to one embodiment of the present invention. [Figure 2C-2] 2C-1 shows a cross-sectional view (in the XZ plane along line AA' in FIG. 2C-1) of the resulting memory structure 200 after the hard mask 225 is patterned, according to one embodiment of the present invention. [Figure 2D-1] FIG. 2 is a top view of the resulting memory structure 200 after the hard mask 225 is removed, according to one embodiment of the present invention. [Figure 2D-2] FIG. 2D-1 is a cross-sectional view (in the XZ plane along line AA' of FIG. 2D-1) of the memory structure 200 obtained after the hard mask 225 is removed, according to one embodiment of the present invention. [Figure 2E-1] FIG. 2 is a top view of memory structure 200 obtained after pillars 231 have been removed, according to one embodiment of the present invention. [Figure 2E-2] FIG. 2E-1 is a cross-sectional view (in the XZ plane along line AA' of FIG. 2E-1) of the resulting memory structure 200 after pillars 231 have been removed, according to one embodiment of the present invention. [Figure 2F-1] FIG. 2 is a top view of memory structure 200 resulting after removing SiN layers 204a and 204e from each active multi-layer exposed along the sidewalls of shaft 218, according to one embodiment of the present invention. [Figure 2F-2] This is a cross-sectional view (in the XZ plane along line A-A' in Figure 2F-1) of memory structure 200 obtained after removing SiN layers 204a and 204e from each active multilayer exposed along the sidewall of shaft 218, according to one embodiment of the present invention. [Figure 2G-1] FIG. 2 shows a top view of memory structure 200 obtained after replacing SiN layers 204a and 204e of each active multilayer with conductor layers 204f and 204g, according to one embodiment of the present invention. [Figure 2G-2]2G-1) are cross-sectional views (in the XZ plane along line A-A' in FIG. 2G-1) of the memory structure 200 obtained after replacing the SiN layers 204a and 204e of each active multilayer with conductor layers 204f and 204g, respectively, according to one embodiment of the present invention. [Figure 2H-1] FIG. 2 shows a top view of the memory structure 200 obtained after forming trenches in the channel polysilicon layer 250, according to one embodiment of the present invention. [Figure 2H-2] 2G-1 )。 FIG. 2G-1 shows a cross-sectional view of the memory structure 200 after forming the grooves in the channel polysilicon layer 250. [Figure 2I] 2 is a cross-sectional view in the XZ plane of the memory structure 200 obtained after deposition of a conductive material 252, according to one embodiment of the present invention. [Figure 3A-1] 2 shows a top view of the memory structure 200 obtained after forming grooves in the conductor layers 204f and 204g according to another embodiment of the present invention. [Figure 3A-2] 3A-1 shows a cross-sectional view (in the XZ plane along line AA' in FIG. 3A-1) of the memory structure 200 obtained after forming grooves in the conductor layers 204f and 204g according to another embodiment of the present invention. [Figure 3B-1] FIG. 2 is a top view of a memory structure 200 obtained after a channel polysilicon layer 250 is deposited, according to another embodiment of the present invention. [Figure 3B-2] FIG. 3B-1 is a cross-sectional view (on the XZ plane along line AA' in FIG. 3B-1) of the memory structure 200 obtained after a channel polysilicon layer 250 is deposited according to another embodiment of the present invention. [Figure 3C-1] FIG. 2 is a top view of the resulting memory structure 200 after conductive material 252 is deposited and planarized, according to another embodiment of the present invention. [Figure 3C-2] FIG. 3C-1 is a cross-sectional view (in the XZ plane along line AA' of FIG. 3C-1) of the resulting memory structure 200 after conductive material 252 is deposited and planarized, according to another embodiment of the present invention. [Figure 3D-1]FIG. 2 shows a top view of the resulting memory structure 200 after insulating material 255 is deposited and planarized, according to another embodiment of the present invention. [Figure 3D-2] FIG. 3D-1 is a cross-sectional view (in the XZ plane along line AA' of FIG. 3D-1) of the resulting memory structure 200 after an insulating material 255 is deposited and planarized, according to another embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] 1 is a schematic top view of a modular unit ("tile") 100 in a memory structure including a three-dimensional NOR memory array, according to one embodiment of the present invention. The tile 100 is typically formed on a flat surface of a semiconductor substrate, such as a single crystal epitaxial layer of a silicon wafer. In order to facilitate visualization of the three-dimensional structure, a Cartesian coordinate system has been used herein, assuming a plane on the XY plane and a normal to the plane in the Z direction orthogonal to the XY plane.

[0014] In some examples, the semiconductor substrate may include support circuits for the 3D NOR memory array formed in, below, or on the 3D NOR memory array. Such support circuits may include both analog and digital circuits. Examples of such support circuits include shift registers, latches, sense amplifiers, reference cells, power lines, bias and reference voltage generators, inverters, NAND, NOR, Exclusive-Or and other logic gates, input / output drivers, address decoders (e.g., bit line and word line decoders), and other memory elements, such as data encoding and decoding circuits including error detection and correction circuits, sequencers, and state machines. This specification begins with a description of the semiconductor substrate in which such support circuits, if any, have already been formed in a conventional manner. This specification and the skill of those skilled in the art will familiarize themselves with the constraints or associated design options imposed or made available by the processes or steps performed in forming the support circuits of the semiconductor substrate in various embodiments of the present invention.

[0015] As shown in FIG. 1, tile 100 includes an "array" portion 101 disposed between "staircase portions" 102a and 102b. The thin-film storage transistors of the NOR memory strings of tile 100 are formed in array portion 101, and staircase portions 102a and 102b allow connection to the common bit lines, and optionally also to a common source line, of the NOR memory strings through conductive vias. (The structure literature discloses a manner in which the common source line is precharged to act as a virtual voltage reference during programming, reading, and erasing operations, thereby eliminating the need for continuous electrical connection to support circuitry during such operations.) In FIG. 1, array portion 101 and staircase portions 102a and 102b are not drawn to scale. For example, array portion 101 may have an area much larger than either of staircase portions 102a and 102b.

[0016] FIG. 2A-1 shows a cross-section in the ZX plane of a memory structure 200 after deposition of multiple material layers (described below) according to an embodiment of the present invention. First, a pad oxide 201 (e.g., silicon oxide) is provided on a planar surface of a semiconductor substrate. Then, an etch stop layer 202 (e.g., tungsten (W), tungsten nitride (WN), aluminum oxide (AlO) or aluminum nitride (AlN)) is provided. Then, a silicon oxycarbide (SiOC) layer 203 is provided to insulate the etch stop layer 202 from the subsequently deposited layers. Then, the active multilayers 204 (8 in total as shown in FIG. 2A-1) are successively deposited. Each active multilayer 204 is composed of, in order of deposition, (i) a silicon nitride (SiN) layer 204a, (ii) a silicon nitride (SiN) layer 204b, (iii) a silicon nitride (SiN) layer 204c, (iv) a silicon nitride (SiN) layer 204d, (v) a silicon nitride (N) layer 204e, (vi) a silicon nitride (N) layer 204f, (vii) a silicon nitride (N) layer 204g, (v) a silicon nitride (N) layer 204h, (vii) a silicon nitride (N) layer 204h, (v) a silicon nitride (N) layer 204h, (v) a silicon nitride (N) layer 204h, (v) a silicon nitride (N) layer 204i ... + (iii) a sacrificial oxide layer 204c; (iv) a doped amorphous silicon (or polysilicon) layer 204b; +2A-1 as SiOC layer 203. An insulating SiOC layer 205 is then deposited on top of the active multi-layer 204. The result is the memory structure 200 of FIG. 2.

[0017] FIG. 2A-2 shows successive trench forming and etching steps to create the staircase portion 102a or 102b of FIG. 1 according to an embodiment of the present invention. As shown in FIG. 2A-2(1), the surface of the memory structure 200 is patterned to form a mask layer 210 to expose a first portion of the memory structure 211. The exposed portion of the insulating SiOC layer 205 is then removed to expose a portion of the active multilayer 204 underneath. The exposed portion of the active multilayer 204 is then removed to expose a portion of the SiOC layer 203 underneath. The resulting structure is shown in FIG. 2A-2(2). A trench is then formed in the mask layer 210 to expose a new portion of the insulating SiOC layer 205. The removal of the exposed SiOC layers 205 and 203, the removal of the active multilayer 204, and the formation of the trench in the mask layer 210 are then repeated seven more times, thereby forming the staircase structure 102a or 102b. An oxide is then deposited to fill the removed portion of the active layer 240. Mask layer 210 is removed and a chemical mechanical polishing (CMP) step is performed to planarize the top surface of memory structure 200 .

[0018] The formation of the staircase structures 102a and 102b is described herein before a detailed description of the processing of the array portion 101. However, processing of the array portion 101 may occur before the formation of the staircase structures 102a and 102b.

[0019] A hard mask layer 215 (e.g., a carbon hard mask) is then deposited on the memory structure 200 and patterned by photolithography. FIG. 2B-1 is a top view of the array portion 101 of the memory structure 200, showing the hard mask layer 215 patterned with a number of openings 217 exposing corresponding portions of the memory structure 200. In FIG. 2B-1, the openings 217 are shown as circular, but any suitable shape (e.g., elliptical) may be adopted. A series of etching steps removes the insulating layers 205 and 203 and the exposed portions of the active multilayer 204 until the etch stop layer 202 is reached, thereby forming the shaft 218. FIG. 2B-2 is a diagram showing a cross section of the memory structure 200 in the XZ plane along the line A-A' in FIG. 2B-1 after the etching step, according to one embodiment of the present invention. (Herein, a "column" of objects refers to objects aligned along the Y direction, and a "row" of objects refers to objects aligned along the X direction.) In FIG. 2B-1, adjacent columns of openings 217 are staggered with respect to one another such that nearest openings in adjacent columns have a greater spacing than if such openings were aligned in the X direction. In one embodiment, adjacent columns of openings 217 are 160 nm apart along the X direction, and each opening 217 may have a diameter of 100 nm. Shaft 218 may be up to 2 microns deep, such that the etch step has an aspect ratio that is less than 20.

[0020] The shaft 218 may be lined with an oxide liner 220 and filled with a sacrificial material 221 (e.g., carbon or tungsten (W) with an adhesion layer of titanium nitride (TiN)). The surface of the memory structure 200 may then be planarized using CMP or etched back if carbon is used as the sacrificial material. After filling the shaft 218 with the sacrificial material 221, a hard mask 225 is deposited and patterned to form rectangular openings 240 exposing portions (e.g., each 60 nm wide in one embodiment) of the memory structure 200 that overlap the columns of the filled shafts 218 (i.e., along the Y direction). After patterning the hard mask 225, a top view and a cross-sectional view (in the XZ plane along line A-A' in FIG. 2C-1) of the resulting memory structure 200 are shown in FIG. 2C-1 and FIG. 2C-2, respectively, according to one embodiment of the present invention.

[0021] A series of successive etches remove the portions of the SiOC layer 205, the active multilayer 204, and the etch stop layer 202 successively exposed under the rectangular portion (opening) 240 of the hard mask 225, and the memory structure 200 becomes a number of stacks separated by trenches 245. The etches are designed to be selective to the oxide liner 220 and the sacrificial material 221 of the filled shaft 218, so that the filled shaft 218 becomes a pillar 231 of the sacrificial material 221 surrounded on its cylindrical surface by the oxide liner 220. Additional wet etches may be performed to remove stringers of various materials. The hard mask 225 may then be removed (e.g., by CMP or by ashing as required). After the removal of the hard mask 225, a top view and a cross-sectional view (in the XZ plane along line A-A' in FIG. 2D-1) of the resulting memory structure 200 are shown in FIG. 2D-1 and FIG. 2D-2, respectively, according to one embodiment of the present invention.

[0022] The trenches 245 may then be filled with silicon oxide, for example using atomic layer deposition (ALD) or spin-on techniques. Excess oxide on the top surface of the memory structure 200 may then be removed, for example using CMP. The pillars 231 are then removed, for example using a suitable wet etch. A top view and a cross-sectional view (in the XZ plane along line A-A' in FIG. 2E-1) of the resulting memory structure 200 after removing the pillars 231 are shown in FIG. 2E-1 and FIG. 2E-2, respectively, in accordance with one embodiment of the present invention.

[0023] Removal of pillar 231 restores shaft 218 in the silicon oxide filler of trench 245, exposing active multilayer 204. Through shaft 218, SiN layers 204a and 204e of each of active multilayers 204 may be removed using, for example, a silicon nitride wet etch. A top view in the XZ plane and a cross-sectional view (along line A-A' in FIG. 2F-1) of the resulting memory structure 200 after removal of SiN layers 204a and 204e from each of active multilayers 204 are shown in FIG. 2F-1 and FIG. 2F-2, respectively, in accordance with one embodiment of the present invention.

[0024] The ALD step deposits a conductive material in the cavity created by the removal of the SiN layers 204a and 204e in each of the active multilayers 204. The conductive material may include, for example, a metal liner (e.g., titanium (Ti), titanium nitride (TiN), tantalum (Ta) or tantalum nitride (TaN)), followed by a refractory metal (e.g., tungsten (W), tungsten nitride (WN) or molybdenum (Mo)). An anisotropic isolation etch then removes the conductive material from the shaft 218. The conductor layers 204f and 204g replacing the SiN layers 204a, 204e of each active multilayer, respectively, may have grooves, for example, on the order of 10 nm. A top view and a cross-sectional view in the XZ plane (along line A-A' in FIG. 2G-1) of the memory structure 200 obtained after replacing the SiN layers 204a and 204e from each of the active multilayers 204 with conductor layers 204f and 204g are shown in FIG. 2G-1 and FIG. 2G-2, respectively, in accordance with one embodiment of the present invention. The conductor layers 204f and 204g are N + The N of each active multilayer 204 is an optional conductive layer formed adjacent to and in contact with the amorphous silicon layers 204b and 204d. + Amorphous silicon layers 204b and 204d will become the common bit and source lines of the NOR memory strings being formed. Conductive layers 204f and 204g reduce the resistivity in the common bit and source lines.

[0025] Then, the sacrificial oxide layer 204c of each active multilayer 204, + The amorphous silicon layer 204b and the N + A groove may be formed in the amorphous silicon layer 204d to form a cavity for depositing the channel material of the thin-film storage transistor. A polysilicon layer 250 for forming the channel region of the thin-film storage transistor is then deposited, etched back for isolation, and grooved to remove the stringers. A top view and a cross-sectional view (in the XZ plane along line A-A' in FIG. 2H-1) of the memory structure 200 obtained after groove formation in the channel polysilicon layer 250 are shown in FIG. 2H-1 and FIG. 2H-2, respectively, in accordance with one embodiment of the present invention.

[0026] A charge trapping layer 251 is then conformally deposited on the sidewalls of the shaft 218. The charge trapping layer 251 may be a multilayer including a tunnel dielectric layer (e.g., silicon oxide), a storage layer (e.g., silicon nitride), and a blocking dielectric layer (e.g., silicon oxide, aluminum oxide, or both). The shaft 218 can then be filled with a conductive material 252 (e.g., tungsten, with a TiN adhesion layer) to form gate electrodes ("word lines") for the storage cells of each active multilayer 240 along the length of the gate electrodes. A cross-sectional view in the XZ plane of the memory structure 200 obtained after the conductive material 252 has been deposited is shown in FIG. 2I, according to one embodiment of the present invention.

[0027] In the process illustrated in Figures 2A-2I, each thin film storage transistor is formed in one of the shafts 218 that contains a curved channel region, a charge storage layer 251, and a gate electrode formed from conductive material 252. In such an embodiment, the straight portions of the trenches 245 provide isolation between the thin film storage transistors. Alternatively, the thin film storage transistors may be formed in the straight portions of the trenches 245, and the shafts 218 may be filled with an insulating material to provide isolation between the thin film storage transistors. The process of such an alternative embodiment is now described.

[0028] According to another embodiment of the present invention, as shown in Figures 2E-1 and 2E-2, following removal of the hard mask 225, replacement of the SiN layers 204a and 204e by the conductor layers 204f and 204g, respectively, is performed substantially in the manner described above with reference to Figures 2E-2G, except that the oxide liner 220 and the sacrificial material 221 are not removed, and therefore the removal of the SiN layers 204a and 204 starts from the straight portion of the trench 245, rather than through the shaft 218. The conductor layers 204f, 204g, respectively replacing the SiN layers 204a, 204e of each active multilayer, may have grooves, for example of the order of 10 nm. A top view in the XZ plane and a cross-sectional view (along the line A-A' in Figure 3A-1) of the memory structure 200 obtained after forming the grooves in the conductor layers 204f and 204g, according to another embodiment of the present invention, are shown in Figures 3A-1 and 3A-2, respectively.

[0029] Thereafter, the sacrificial oxide layer 204c of each active multilayer 204, + The amorphous silicon layer 204b and the N + A cavity for depositing the channel material of the thin-film storage transistor may be formed by forming a groove in the amorphous silicon layer 204d. A polysilicon layer 250 for forming the channel region of the thin-film storage transistor is then deposited, etched back to set the spacing, and grooved to remove the stringers. A top view in the XZ plane and a cross-sectional view (along line A-A' in FIG. 3B-1) of the memory structure 200 obtained after forming the groove in the channel polysilicon layer 250 are shown in FIG. 3B-1 and 3B-2, respectively, according to another embodiment of the present invention.

[0030] A charge trapping layer 251 is then conformally deposited on the sidewalls of the trench 245. The charge trapping layer 251 may be a multi-layer including: (i) a tunneling layer (e.g., any silicon oxide (SiO x ), silicon nitride (SiN), silicon oxynitride (SiON), any aluminum oxide (AlO x ), any hafnium oxide (HfO x ), zirconium oxide (ZrOx ), any hafnium silicon oxide (HfSi x O y ), hafnium zirconium oxide (HfZrO), or any combination thereof), (ii) a charge storage layer (e.g., silicon nitride (SiN), hafnium oxide (HfCk), or hafnium silicon oxynitride (HfSiON)), and (iii) a blocking layer (e.g., any silicon oxide (SiO x ), any aluminum oxide (AlO x ), or both).

[0031] The trenches 245 may then be filled with a conductive material 252 (e.g., tungsten, with a TiN adhesion layer), which forms the gate electrodes ("word lines") for the storage cells of each active multilayer 240 along the length of the gate electrodes. Excess conductive material on the surface of the memory structure 200 may be removed by CMP. A top view in the XZ plane and a cross-sectional view (along line A-A' in FIG. 3C-1) of the memory structure 200 obtained after the conductive material 252 is deposited and planarized are shown in FIG. 3C-1 and FIG. 3C-2, respectively, in accordance with one embodiment of the present invention.

[0032] The pillars 231 in the shaft 218 are then removed, for example using a suitable wet etch. Removal of the pillars 231 restores the shaft 218 in the conductive material 252 of the trench 245. The shaft 218 may then be filled with a suitable insulating material 255 (e.g., silicon oxide). The excess insulating material on the memory structure 200 may then be removed by CMP. A top view in the XZ plane and a cross-sectional view (along line A-A' in FIG. 3D-1) of the memory structure 200 obtained after deposition of the insulating material 255 are shown in FIG. 3D-1 and FIG. 3D-2, respectively, in accordance with one embodiment of the present invention.

[0033] The above detailed description is provided to illustrate specific embodiments of the present invention and is not intended to be limiting. Numerous variations and modifications are possible within the scope of the present invention, which is set forth in the appended claims.

Claims

1. providing a semiconductor structure on a planar surface of a semiconductor substrate, the semiconductor structure including a plurality of active multi-layers stacked on top of one another along a first direction substantially perpendicular to the planar surface, adjacent active multi-layers being electrically insulated from one another by layers of dielectric material, each active multi-layer including first and second semiconductor layers of a first conductivity type separated from one another by the dielectric material; providing a plurality of shafts arranged in a regular pattern substantially orthogonal to one another and along both a second direction and a third direction each orthogonal to the first direction, the shafts extending depthwise along the first direction through the semiconductor structure, and the shafts having a predetermined dimension along the second direction; providing a plurality of trenches in the semiconductor structure, each of which extends depthwise along the first direction and longitudinally along the third direction, (a) intersecting a plurality of the shafts in the second direction, and (b) having a width along the second direction that is less than a dimension of the shaft; forming, either in (i) each shaft, or (ii) a portion of each trench between adjacent ones of the shafts, (a) a third semiconductor layer of a second conductivity type different from the first conductivity type formed adjacent to and in contact with the first and second semiconductor layers of each active multilayer, (b) a charge trapping layer adjacent to the third semiconductor layer, and (c) a conductor layer in contact with the charge trapping layer.

2. 2. The method of claim 1, wherein the first and second semiconductor layers, the third semiconductor layer, the charge trapping layer, and the conductor of each active multilayer respectively provide a common bit line, a common source line, a channel region, a charge storage layer, and a gate electrode of a thin-film storage transistor in a NOR memory string.

3. The method of claim 1 , wherein the portion of each of the trenches between adjacent shafts is filled with an insulating material when the third semiconductor layer is formed in each of the shafts.

4. The method of claim 1 , wherein each of the shafts is filled with an insulating material when the third semiconductor layer is formed in the portion of each of the trenches between adjacent shafts.

5. The method of claim 1 , wherein each of the active multi-layers further comprises the conductor layer adjacent and in contact with at least one of the first and second semiconductor layers.

6. 2. The method of claim 1 , wherein the conductor layer is formed by removing a sacrificial layer in each of the active multilayers through the shaft (or through the portion of each of the trenches between adjacent shafts) and replacing it by depositing a conductive material using atomic layer deposition (ALD).

7. The method of claim 6 , wherein the conductive material comprises tungsten.

8. The method of claim 1 , wherein the dielectric material comprises silicon oxycarbide (SiOC).

9. The method of claim 1 , wherein the charge trapping layer includes a tunneling layer, a charge storage layer, and a blocking layer.

10. The tunnel layer may be any silicon oxide (SiO x ), silicon nitride (SiN), silicon oxynitride (SiON), any aluminum oxide (AlO x ), any hafnium oxide (HfO x ), zirconium oxide (ZrO x ), any hafnium silicon oxide (HfSi x O y 10. The method of claim 9, further comprising one or more of: hafnium zirconium oxide (HfZrO);

11. The charge storage layer is made of silicon nitride (SiN), hafnium oxide (HfC 2 10. The method of claim 9, further comprising one or more of: a) a silicon oxynitride (SiON); and b) a silicon nitride (HfSiON).

12. The blocking layer may be any silicon oxide (SiO x ) and aluminum oxide (AlO x 11. The method of claim 10, comprising one or more of the following:

13. The method of claim 1 , wherein the conductor layer comprises a metal liner and a refractory metal.

14. 14. The method of claim 13, wherein the metal liner comprises one or more of titanium (Ti), titanium nitride (TiN), tantalum (Ta), and tantalum nitride (TaN).

15. 14. The method of claim 13, wherein the refractory metal comprises one or more of tungsten (W), tungsten nitride (WN), and molybdenum (Mo).

16. The method of claim 1 , further comprising lining the shaft with a dielectric liner prior to providing the trench in the semiconductor structure.

17. The method of claim 16 , wherein the dielectric liner comprises an oxide liner.

18. The method of claim 16 , further comprising filling the shaft with a sacrificial material.

19. The method of claim 18 , wherein the sacrificial material comprises carbon or tungsten (W).

20. 20. The method of claim 19, further comprising providing an adhesion layer of titanium nitride surrounding the sacrificial material.

21. When the third semiconductor layer is formed in the shaft, the step of forming the third semiconductor layer comprises: removing a sacrificial material from the shaft; forming a trench in the first and second semiconductor layers and in the dielectric layer in each of said active multilayers to create a cavity; and a step of depositing the third semiconductor layer.

22. The method of claim 21 , wherein the charge trapping layer is conformally deposited on a sidewall of the shaft.

23. 23. The method of claim 22, further comprising forming the conductor layer by depositing a conductive material to fill each of the shafts after forming the charge trapping layer.

24. forming the third semiconductor layer using the portion of each of the trenches between adjacent shafts, forming a cavity by forming a trench in the first and second semiconductor layers and a dielectric layer of each of the active multilayers through an exposed portion of each of the trenches between adjacent shafts; and depositing the third semiconductor layer.

25. 25. The method of claim 24, wherein the charge trapping layer is conformally deposited on sidewalls of the portion of each of the trenches between adjacent shafts.

26. 26. The method of claim 25, wherein the conductor layer is formed by depositing a conductive material to fill the portion of each of the trenches between adjacent shafts after forming the charge trapping layer.

27. 27. The method of claim 26, further comprising filling the shaft with an insulating material.

28. The method of claim 1 , further comprising providing an etch stop layer between the first and second semiconductor layers and the planar surface of the semiconductor substrate.

29. 30. The method of claim 28, wherein the etch stop layer comprises one or more of tungsten (W), tungsten nitride (WN), aluminum oxide (AlO), or aluminum nitride (AlN).

30. 30. The method of claim 28, further comprising a pad oxide layer between the etch stop layer and the planar surface of the semiconductor substrate.

Citation Information

Patent Citations

  • Porous silicon oxycarbide integrated circuit insulator

    JP2003510795A

  • Storage device with multi-level structure

    JP2008160121A

  • Capacitively Coupled Nonvolatile Thin-Film Transistor Strings in a Three-Dimensional Array

    JP2019526934A

  • Non-volatile memory device, method of operating the same, and method of fabricating the same

    KR1020120085603A

  • Method for forming pattern in semiconductor device

    US20080160765A1