Method for fabricating a three-dimensional memory structure of a NOR memory string
By forming trenches and depositing materials with lower aspect ratios, the method addresses the challenge of achieving fine pitch word lines in 3D NOR memory arrays, enhancing manufacturing efficiency and reducing complexity.
Patent Information
- Application Number
- JP2023504166
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-07-21
- Filing Date
- 2021-07-21
- Publication Date
- 2024-10-25
- Estimated Expiration
- 2041-07-21
AI Technical Summary
Etching conductive materials to achieve a very fine pitch between word lines in 3D NOR memory arrays is challenging due to high aspect ratios, which complicates the manufacturing process.
A method involving the formation of trenches between active multilayer strips with insulating material, followed by filling and etching to create semiconductor structures with a lower aspect ratio, allowing for the deposition of charge trapping layers and conductive materials to form word lines without direct etching of conductive materials.
This approach enables the formation of word lines with a fine pitch without the need for high-aspect-ratio etching, improving manufacturing efficiency and reducing complexity in 3D NOR memory array production.
Smart Images

Figure 0007573722000001 
Figure 0007573722000002 
Figure 0007573722000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a manufacturing process for memory integrated circuits, and more particularly to a process for fabricating thin film storage transistors in three-dimensional memory structures formed on a planar surface of a semiconductor substrate. [Background technology]
[0002] (CROSS-REFERENCE TO RELATED ART) High density memory arrays, e.g., three-dimensional arrays of NOR memory strings ("3D NOR memory arrays"), are disclosed, for example, in U.S. Patent Application Publication No. 2017 / 0092371A1, entitled "Capacitive-Coupled Non-Volatile Thin-film Transistor Strings in Three-Dimensional Arrays" ("Structure Document I"), and U.S. Patent Application Publication No. 2018 / 0366489A1, entitled "3-Dimensional NOR Memory Array Architecture and Methods for Fabrication Thereof" ("Structure Document II"). The disclosures of Structure Documents I and II (collectively hereinafter referred to as "Structure Documents") are incorporated herein by reference in their entirety. These 3D NOR memory arrays can operate to provide highly desirable speed memory circuits that are comparable to conventional memory circuits, such as, for example, dynamic random access memories ("DRAMs"), which have much lower circuit density and significantly higher power dissipation.
[0003] In some structural literature embodiments, a 3D NOR memory array includes multiple stacks of NOR memory strings, each stack having multiple NOR memory strings stacked one on top of the other. In the disclosure, the NOR memory string includes multiple storage cells sharing a common drain region ("common bit line") and a common source region ("common source line"), the storage cells being located on one or both sides along the length of the NOR memory string. Each storage cell is controlled by a conductor ("word line" or "local word line") that is substantially perpendicular to the memory string. Each word line may be shared along its length by multiple storage cells of other NOR memory strings located on the opposite side of the word line. However, to achieve high density in a 3D NOR memory array, a fine pitch between adjacent word lines is required. Etching conductors (e.g., tungsten) with high aspect ratios (e.g., 50 or more) is a challenging task. Summary of the Invention
[0004] In accordance with one embodiment of the present invention, a process for making a NOR memory array having word lines spaced at a very fine pitch includes the steps of: (i) providing on a planar surface of a semiconductor substrate first and second semiconductor structures spaced from one another by trenches having a predetermined width in a first direction substantially parallel to the planar surface, the first and second semiconductor structures each including active multilayer strips extending longitudinally along a second direction substantially orthogonal to the first direction and stacked together along a third direction substantially perpendicular to the planar surface, adjacent ones of the active multilayer strips being electrically insulated from one another by a layer of insulating material, each active multilayer strip including first and second semiconductor layers of a first conductivity type separated from one another by a dielectric material; and (ii) recessing sidewalls of the trenches in the multilayer strips along the first direction to form a first insulating layer between adjacent ones of the active multilayer strips. (iii) forming a trench between the layers; (iv) filling the trench with a first fill material; (v) forming first and second shafts spaced apart along a second direction by removing a portion of each multilayer strip from each of the first and second semiconductor structures and removing a portion of the second insulating material from the trench in each shaft; (vi) filling the first and second shafts with the second fill material; (vii) removing the first fill material from the trench between the first and second shafts; and (viii) conformally providing a charge trapping layer on sidewalls of the trench and filling a remaining portion of the trench with a conductive material.
[0005] The first and second semiconductor layers, charge trapping layers, and conductive materials of each active multi-layer strip may provide a common bit line, a common source line, a charge storage layer, and a gate electrode, respectively, of the thin-film storage transistors of the NOR memory string. In one embodiment, the predetermined material may be a channel polysilicon material that serves as a channel region of the thin-film storage transistors. In another embodiment, the predetermined material may be replaced after the word lines are formed with a final channel material and sealed with a dielectric liner (e.g., an atomic layer deposition (ALD) silicon oxide liner).
[0006] The present invention avoids the problem of etching conductive material to provide local word lines arranged at a very fine pitch: the etching of the shafts that provide isolation between thin film storage transistors can be performed at a lower aspect ratio than that required to etch the conductive material.
[0007] In one embodiment of the present invention, the first and second semiconductor layers are N + The third semiconductor layer may comprise doped amorphous silicon or polysilicon, and the third semiconductor layer may comprise doped amorphous silicon or polysilicon. - The charge trapping layer may comprise doped amorphous or polysilicon, the insulating material may comprise silicon oxycarbide (SiOC) or silicon oxide, and the charge trapping layer may comprise (i) a tunneling layer (e.g., any silicon oxide (SiO x ), silicon nitride (SiN), silicon oxynitride (SiON), any aluminum oxide (AlO x ), any hafnium oxide (HfO x ), zirconium oxide (ZrO x ), any hafnium silicon oxide (HfSi x O y), optional hafnium zirconium oxide (HfZrO), or any combination thereof), (ii) a charge storage layer (e.g., silicon nitride (SiN), hafnium oxide (HfO2), or hafnium silicon oxynitride (HfSiON)) and a blocking layer (e.g., optional silicon oxide, aluminum oxide, or both). The conductive material may include a metal liner (e.g., titanium (Ti), titanium nitride (TiN), tantalum (Ta), or tantalum nitride (TaN)) and a refractory metal (e.g., tungsten (W), tungsten nitride (WN), or molybdenum (Mo)). The first fill material may include silicon oxide.
[0008] According to one embodiment of the present invention, a cap (e.g., tungsten) may be provided to protect against subsequent process steps after the charge trapping layer and local word lines are formed. The shaft may be lined with a dielectric liner (e.g., silicon nitride) prior to filling with a second fill material (e.g., silicon oxide).
[0009] The present invention can be better understood from the following detailed description considered in conjunction with the accompanying drawings. [Brief description of the drawings]
[0010] [Figure 1] 1 is a schematic top view of a modular unit ("tile") 100 in a memory structure including a three-dimensional NOR memory array, according to one embodiment of the present invention. [Figure 2A-1] 2 shows a cross-section in the ZX plane of memory structure 200 after deposition of multiple layers of material (described below), according to one embodiment of the present invention. [Figure 2A-2] 2A-2C illustrate continuous recessing and etching steps to create the stepped portion 102a or 102b of FIG. 1, according to one embodiment of the present invention. [Figure 2B]2 illustrates a cross-section in the XZ plane of the resulting memory structure 200 after isolation etching of the P-doped amorphous silicon layer 250 has been performed, according to one embodiment of the present invention. [Figure 2C] The resulting memory structure 200 is shown in cross section in the XZ plane after deposition of silicon oxide 223 to fill trenches 216 and planarization. [Figure 2D] FIG. 2 shows a cross-section in the XZ plane of the resulting memory structure 200 after a second group of trenches 218 have been formed, according to one embodiment of the present invention. [Figure 2E] FIG. 2 illustrates a cross-section in the XZ plane of the resulting memory structure 200 after removing the SiN layers 204a and 204e from each active multi-layer 204, according to one embodiment of the present invention. [Figure 2F] 2 illustrates a cross-section in the XZ plane of the resulting memory structure 200 after replacing SiN layers 204a and 204e from each active multilayer 204 with conductive material 229, in accordance with one embodiment of the present invention. [Figure 2G] FIG. 2 illustrates an XZ cross-section of the resulting memory structure 200 after forming grooves in the conductive material 229, the N+ amorphous semiconductor layers 204b and 204d, and the oxide layer 203 of each active multilayer 204, according to one embodiment of the present invention. [Figure 2H] 2 shows an XZ cross-section of the resulting memory structure 200 after depositing channel polysilicon 250 in trench 218, according to one embodiment of the present invention. [Figure 2I] 2 shows an XZ cross-section of the resulting memory structure 200 after depositing silicon oxide 223 in trench 218, according to one embodiment of the present invention. [Figure 2J-1] FIG. 2 is a top view of the resulting memory structure 200 after forming the shaft 263, according to one embodiment of the present invention. [Figure 2J-2] FIG. 2J-1 is a cross-sectional view (in the XZ plane along line AA' in FIG. 2J-1) of the memory structure 200 obtained after forming the shaft 263, according to one embodiment of the present invention. [Figure 2K-1] FIG. 2 shows a top view of the resulting memory structure 200 after filling the shaft 263 with sacrificial silicon 265, according to one embodiment of the present invention. [Figure 2K-2] FIG. 2K-1 is a cross-sectional view (in the XZ plane along line AA′ of FIG. 2K-1) of the memory structure 200 obtained after filling the shaft 263 with sacrificial silicon 265, according to one embodiment of the present invention. [Figure 2L-1] FIG. 2 shows a top view of memory structure 200 obtained after removing silicon oxide 223 from trench 218, according to one embodiment of the present invention. [Figure 2L-2] 2L-1 shows a cross-sectional view (in the XZ plane along line AA' in FIG. 2L-1) of the resulting memory structure 200 after silicon oxide 223 has been removed from trenches 218, according to one embodiment of the present invention. [Figure 2M-1] FIG. 2 shows a top view of memory structure 200 obtained after depositing conductive material 272 in trench 218, according to one embodiment of the present invention. [Figure 2M-2] 2M-1 shows a cross-sectional view (in the XZ plane along line AA' in FIG. 2M-1) of the resulting memory structure 200 after depositing conductive material 272 in trench 218, according to one embodiment of the present invention. [Figure 2N-1] FIG. 2 shows a top view of the memory structure 200 obtained after forming a cap 272t to protect the charge trapping layer 268, according to one embodiment of the present invention. [Figure 2N-2] FIG. 2N-1 is a cross-sectional view (in the XZ plane along line A-A' in FIG. 2N-1) of the memory structure 200 obtained after forming a cap 272t to protect the charge trapping layer 268 according to one embodiment of the present invention. [Figure 2O-1] FIG. 2 is a top view of the resulting memory structure 200 after removing the sacrificial amorphous silicon 265, according to one embodiment of the present invention. [Figure 2O-1] FIG. 2O-1 shows a cross-sectional view (in the XZ plane along line A-A' of FIG. 2O-1) of the memory structure 200 obtained after removing the sacrificial amorphous silicon 265, according to one embodiment of the present invention. [Figure 2P-1] FIG. 2 is a top view of the memory structure 200 obtained after removing the silicon nitride liner 264 according to another embodiment of the present invention. [Figure 2P-2] FIG. 2P-1 is a cross-sectional view (in the XZ plane along line AA′ of FIG. 2P-1) of the memory structure 200 obtained after removing the silicon nitride liner 264 according to another embodiment of the present invention. [Figure 2Q-1] FIG. 2 is a top view of the memory structure 200 obtained after removing the channel polysilicon 250 according to another embodiment of the present invention. [Figure 2Q-2] FIG. 2Q-1 is a cross-sectional view (in the XZ plane along line AA' of FIG. 2Q-1) of the memory structure 200 obtained after removing the channel polysilicon 250 according to another embodiment of the present invention. [Figure 2R-1] FIG. 2 is a top view of the memory structure 200 obtained after depositing channel polysilicon 280 according to another embodiment of the present invention. [Figure 2R-2] FIG. 2R-1 is a cross-sectional view (in the XZ plane along line AA′ of FIG. 2R-1) of the memory structure 200 obtained after depositing channel polysilicon 280 according to another embodiment of the present invention. [Figure 2S-1] FIG. 2 is a top view of the memory structure 200 obtained after forming trenches in the channel polysilicon 280 according to another embodiment of the present invention. [Figure 2S-2] FIG. 2S-1 is a cross-sectional view (in the XZ plane along line AA' of FIG. 2S-1) of the memory structure 200 obtained after forming grooves in the channel polysilicon 280 according to another embodiment of the present invention. [Figure 2T-1] FIG. 2 is a top view of the resulting memory structure 200 after depositing an ALD oxide liner 285, according to another embodiment of the present invention. [Figure 2T-2] FIG. 2T-1 is a cross-sectional view (in the XZ plane along line A-A' of FIG. 2T-1) of the resulting memory structure 200 after depositing an ALD oxide liner 285, according to an alternative embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] 1 is a schematic top view of a modular unit ("tile") 100 in a memory structure including a three-dimensional NOR memory array, according to one embodiment of the present invention. The tile 100 is typically formed on a flat surface of a semiconductor substrate, such as a single crystal epitaxial layer of a silicon wafer. In order to facilitate visualization of the three-dimensional structure, a Cartesian coordinate system has been used herein, assuming a plane on the XY plane and a normal to the plane in the Z direction orthogonal to the XY plane.
[0012] In some examples, the semiconductor substrate may include support circuits for the 3D NOR memory array formed in, below, or on the 3D NOR memory array. Such support circuits may include both analog and digital circuits. Examples of such support circuits include shift registers, latches, sense amplifiers, reference cells, power lines, bias and reference voltage generators, inverters, NAND, NOR, Exclusive-Or and other logic gates, input / output drivers, address decoders (e.g., bit line and word line decoders), and other memory elements, such as data encoding and decoding circuits including error detection and correction circuits, sequencers, and state machines. This specification begins with a description of the semiconductor substrate in which such support circuits, if any, have already been formed in a conventional manner. This specification and the skill of those skilled in the art will familiarize themselves with the constraints or associated design options imposed or made available by the processes or steps performed in forming the support circuits of the semiconductor substrate in various embodiments of the present invention.
[0013] As shown in FIG. 1, tile 100 includes an "array" portion 101 disposed between "staircase portions" 102a and 102b. The thin-film storage transistors of the NOR memory strings of tile 100 are formed in array portion 101, and staircase portions 102a and 102b allow connection to the common bit lines, and optionally also to a common source line, of the NOR memory strings through conductive vias. (The structure literature discloses a manner in which the common source line is precharged to act as a virtual voltage reference during programming, reading, and erasing operations, thereby eliminating the need for continuous electrical connection to support circuitry during such operations.) In FIG. 1, array portion 101 and staircase portions 102a and 102b are not drawn to scale. For example, array portion 101 may have an area much larger than either of staircase portions 102a and 102b.
[0014] FIG. 2A-1 shows a cross-section in the ZX plane of a memory structure 200 after deposition of multiple material layers (described below) according to an embodiment of the present invention. First, a pad oxide 201 (e.g., silicon oxide) is provided on a planar surface of a semiconductor substrate. Then, an etch stop layer 202 (e.g., tungsten (W), tungsten nitride (WN), aluminum oxide (AlO) or aluminum nitride (AlN)) is provided. Then, a silicon oxycarbide (SiOC) layer 203 is provided to insulate the etch stop layer 202 from the subsequently deposited layers. Then, the active multilayers 204 (8 in total as shown in FIG. 2A-1) are successively deposited. Each active multilayer 204 is composed of, in order of deposition, (i) a silicon nitride (SiN) layer 204a, (ii) a silicon nitride (SiN) layer 204b, (iii) a silicon nitride (SiN) layer 204c, (iv) a silicon nitride (SiN) layer 204d, (v) a silicon nitride (N) layer 204e, (vi) a silicon nitride (N) layer 204f, (vii) a silicon nitride (N) layer 204g, (v) a silicon nitride (N) layer 204h, (vii) a silicon nitride (N) layer 204h, (v) a silicon nitride (N) layer 204h, (v) a silicon nitride (N) layer 204h, (v) a silicon nitride (N) layer 204i ... + (iii) a sacrificial oxide layer 204c; and (iv) a N + 2A-1 as SiOC layer 203. An insulating SiOC layer 205 is then deposited on top of the active multi-layer 204. The result is the memory structure 200 of FIG. 2A-1.
[0015] FIG. 2A-2 shows successive trenching and etching steps for creating the staircase portion 102a or 102b of FIG. 1 according to an embodiment of the present invention. As shown in FIG. 2A-2(1), the surface of the memory structure 200 is patterned to form a mask layer 210 to expose a first portion of the memory structure 211. The exposed portion of the insulating SiOC layer 205 is then removed to expose a portion of the active multilayer 204 underneath. The exposed portion of the active multilayer 204 is then removed to expose a portion of the SiOC layer 203 underneath. The resulting structure is shown in FIG. 2A-2(2). A trench is then formed in the mask layer 210 to expose a new portion of the insulating SiOC layer 205. The removal of the exposed SiOC layers 205 and 203, the removal of the active multilayer 204, and the trenching of the mask layer 210 are then repeated seven more times, thereby forming the staircase structure 102a or 102b. An oxide is then deposited to fill the removed portion of the active layer 240. Mask layer 210 is removed and a chemical mechanical polishing (CMP) step is performed to planarize the top surface of memory structure 200. Conductor-filled vias may be created at a suitable subsequent time to provide connections to conductor layers in active multilayer 204.
[0016] The formation of the staircase structures 102a and 102b is described herein before the detailed description below of the processing of the array portion 101. However, processing of the array portion 101 may occur before the formation of the staircase structures 102a and 102b.
[0017] At the beginning of processing of the array portion 101, a hard mask layer (e.g., a carbon hard mask) is deposited and photolithographically patterned on the memory structure 200. The hard mask transfers its pattern to allow etching of a first group of trenches 216 in the memory structure 200. Each of the trenches 216 extends through the insulating layers 205 and 203, the active multilayer 204, and the etch stop layer 202. In one embodiment, the trenches 216 are each 70 nm wide, with corresponding ends of adjacent trenches spaced 190 nm apart from each other. In this embodiment, the trenches 216 are etched with an aspect ratio of less than 50 (or even less than 30). A series of etching steps etch the SiN layers 204a and 204e, N + A groove of, for example, 10 nm is formed in the doped amorphous silicon layers 204b and 204d and the oxide layer 204c. - A doped amorphous silicon (or polysilicon) layer 250 is conformally deposited and etched back (i.e., isolated etched). + Amorphous silicon layers 204b and 204d provide common bit and source lines for the thin film transistors of the NOR memory strings that are to be formed. - The doped amorphous silicon layer 250 provides the channel region for the storage transistor of the NOR memory string. A hard mask and extra P - The doped amorphous polysilicon layer 250 is removed (e.g., by CMP). - A cross-sectional view in the XZ plane of the resulting memory structure 200 after isolation etching of the doped amorphous silicon layer 250 has been performed is shown in FIG. 2B, in accordance with one embodiment of the present invention.
[0018] The trenches 216 are then filled by depositing silicon oxide 223, which is then planarized by removing (e.g., by CMP) the silicon oxide 223 on the surface of the semiconductor structure 200, as shown in the cross-sectional view in the XZ plane of FIG. 2C.
[0019] A second group of trenches 218 is then etched using substantially the same method as trenches 216, as described above with reference to FIG. 2B. A second group of trenches 218 is created between adjacent trenches 216. Because trenches 216 are filled with oxide, the material stack between adjacent trenches has substantially the same pitch as the etching of the first group of trenches 216, thus providing mechanical support during the etching of trenches 218. The trenches 218 are performed with substantially the same aspect ratio as the etching of trenches 216. In this manner, multiple groups of trenches are formed, allowing the etching of each trench formation to be performed within a desired aspect ratio (e.g., less than 50). A cross-section in the XZ plane of the resulting memory structure 200 after the second group of trenches 218 is formed is shown in FIG. 2D, according to one embodiment of the present invention.
[0020] Through trenches 218, the SiN layers 204a and 204e of each active multi-layer 204 may be removed using, for example, a silicon nitride wet etch. A cross-section in the XZ plane of the resulting memory structure 200 after removing the SiN layers 204a and 204e of each active multi-layer 204 is shown in Figure 2E, in accordance with one embodiment of the present invention.
[0021] In an atomic layer deposition (ALD) step, a conductive material 229 (e.g., a liner of one or more of the following materials - titanium, titanium nitride (TiN), tantalum (Ta), or tantalum nitride (TaN)) is deposited. A refractory metal (e.g., tungsten (W), tungsten nitride, or molybdenum (Mo)) is then implanted into the cavities created by removing the SiN layers 204a and 204e from each of the active multilayers 204. An etch-back step or an anisotropic etch then removes the conductive material 229 from the bottom of the trenches 218, leaving a substantially conformal layer on their sidewalls. The memory structure 200 obtained after replacement of the SiN layers 204a and 204e from each of the active multilayers 204 with the conductive material 229 is shown in FIG. 2F in cross section in the XZ plane, according to one embodiment of the present invention.
[0022] The conductive material 229 is N + An optional conductive layer is formed in contact with the amorphous silicon layers 204b and 204d. + Since amorphous silicon layers 204b and 204d will be the common bit line and common source line, respectively, of the NOR memory strings being formed, conductive material 229 reduces the resistivity of the common bit line and common source line.
[0023] The conductive material 229 may be removed from the sidewalls of the trench 218 and further etched to form additional grooves. A series of etching steps then removes the first and second N + The doped amorphous silicon layers 204b and 204d and the oxide layer 204c are grooved, for example, by 10 nm. + An XZ cross section of the resulting memory structure 200 after forming grooves in amorphous semiconductor layers 204b and 204d and oxide layer 203 of each active multilayer 204 is shown in FIG. 2G, in accordance with one embodiment of the present invention.
[0024] Next, P - A doped amorphous silicon layer ("channel polysilicon") 250 may be conformally deposited on the sidewalls of trench 218 using substantially the same methods as described above with reference to Figure 2B. The resulting XZ cross section of memory structure 200 after deposition of channel polysilicon 250 into trench 218 is shown in Figure 2H, in accordance with one embodiment of the present invention.
[0025] Trenches 218 may then be filled with silicon oxide 223 and planarized using methods similar to those described above in connection with the steps for providing silicon oxide 223 in Figure 2C. An XZ cross-section of memory structure 200 obtained after deposition of silicon oxide 223 in trenches 218 is shown in Figure 2I, in accordance with one embodiment of the present invention.
[0026] After depositing silicon oxide 223 in trench 218 and planarizing it, no further distinction between trenches 216 and 218 is necessary in the detailed description that follows. Thus, in the following, trenches 216 and 218 will both be referred to as trench 218. The next step is to provide a storage layer and gate electrode ("word line" or "local word line") for each thin-film storage transistor of the NOR memory string.
[0027] After planarization of silicon oxide 223, a hard mask 260 is provided over memory structure 200, photolithographically patterned, and developed. Hard mask 260 includes a column of elliptical openings 261. (Herein, a "column" of objects refers to objects aligned along the Y direction, and a "row" of objects refers to objects aligned along the X direction.) In FIG. 2J-1, adjacent columns of openings 261 are offset relative to one another along the X direction such that nearest openings in adjacent columns have a greater spacing between them than if such openings were side-by-side in the X direction. In one embodiment, adjacent openings within each column are arranged with a pitch of 110 nm along the Y direction, and adjacent columns are also arranged with a pitch of 110 nm along the X direction. In this embodiment, the major and minor axes of each opening may be, for example, 100 nm and 60 nm along the X and Y directions, respectively. A series of etches through opening 261 excavates a corresponding shaft 263, removes oxide layer 203 and active multilayer 204, and reaches etch stop layer 202. A top view and a cross-sectional view in the XZ plane along line A-A' in FIG. 2J-1 of the resulting memory structure 200 after forming shaft 263 are shown in FIG. 2J-1 and FIG. 2J-2, respectively, according to one embodiment of the present invention. The aspect ratio of the etching step that creates shaft 263 still has an aspect ratio that is substantially within a desired range (e.g., less than 50).
[0028] A silicon nitride liner 264 (e.g., 5 nm thick) is then conformally deposited on shaft 263 and then filled with sacrificial amorphous silicon 265. Hard mask 260 is then removed and the surface of memory structure 200 is planarized (e.g., by CMP). A top view and a cross-sectional view (in the XZ plane along line A-A' in FIG. 2K-1) of the resulting memory structure 200 after filling shaft 263 with sacrificial amorphous silicon 265 are shown in FIG. 2K-1 and FIG. 2K-2, respectively, in accordance with one embodiment of the present invention.
[0029] A wet etch then removes the silicon oxide 223 from the trenches 218. A top view and a cross-sectional view (in the XZ plane along line A-A' in FIG. 2L-1) of the resulting memory structure 200 after the silicon oxide 223 is removed from the trenches 218 are shown in FIG. 2L-1 and FIG. 2L-2, respectively, in accordance with one embodiment of the present invention.
[0030] A conformal charge trapping layer 268 is then conformally deposited on the sidewalls of the trench 218. The charge trapping layer 268 may be multi-layered, including: (i) a tunneling layer (e.g., any silicon oxide (SiO x ), silicon nitride (SiN), silicon oxynitride (SiON), any aluminum oxide (AlO x ), any hafnium oxide (HfO x ), zirconium oxide (ZrO x ), any hafnium silicon oxide (HfSi x O y ), hafnium zirconium oxide (HfZrO), or any combination thereof), (ii) a charge storage layer (e.g., silicon nitride (SiN), hafnium oxide (HfCk), or hafnium silicon oxynitride (HfSiON)), and (iii) a blocking layer (e.g., any silicon oxide (SiO x ), any aluminum oxide (AlO x), or both). The conductive material may include a metal liner (e.g., titanium (Ti), titanium nitride (TiN), tantalum (Ta) or tantalum nitride (TaN)) and a refractory metal (e.g., tungsten (W), tungsten nitride (WN), or molybdenum (Mo)).
[0031] A tunnel dielectric layer (e.g., silicon oxide), a storage layer (e.g., silicon nitride), and a blocking dielectric layer (e.g., silicon oxide, aluminum oxide, or both). The trenches 218 may then be filled with a conductive material 272 (e.g., tungsten with a TiN adhesion layer), which forms a gate electrode (i.e., a "word line" or "local word line") for the storage cells of each active multilayer 240 along the length of the gate electrode. The gate electrode thus formed may be 60 nm by 60 nm or smaller. A planarization step (e.g., CMP) may be used to remove excess conductive material 272 from the top surface of the memory structure 200. A top view and a cross-sectional view (in the XZ plane along line A-A' in FIG. 2M-1) of the resulting memory structure 200 after depositing the conductive material 272 in the trenches 218 and planarizing are shown in FIG. 2M-1 and FIG. 2M-2, respectively, in accordance with one embodiment of the present invention.
[0032] Cap 272t may be provided to facilitate contact to the underlying wordline and to protect charge trapping layer 268 in subsequent processing steps. The cap may be formed using additional masking, patterning, deposition (including conductive material 272), and planarization steps. A top view and a cross-sectional view (in the XZ plane along line A-A' in FIG. 2N-1) of the resulting memory structure 200 after forming cap 272t are shown in FIGs. 2N-1 and 2N-2, according to one embodiment of the present invention.
[0033] The sacrificial amorphous silicon 265 may then be removed from the shaft 263 and replaced with silicon oxide to act as isolation between the thin-film storage transistors. Excess silicon oxide on the top surface of the memory structure 200 may be removed by a planarization step (e.g., CMP). Alternatively, the shaft 263 may be left unfilled, with the voids acting as isolation between the thin-film storage transistors. A top view and a cross-sectional view (in the XZ plane along line A-A' in FIG. 2O-1) of the resulting memory structure 200 after the sacrificial amorphous silicon 265 has been removed are shown in FIG. 2O-1 and FIG. 2O-2, respectively, in accordance with one embodiment of the present invention. At this point, the process for the formation of the 3D NOR memory string array is substantially complete without the need for etching the conductive material 272 to form the word lines. Conventional interconnect layers, programmable switch circuits, and other useful circuits may be formed on top of the memory structure 200 using conventional methods.
[0034] In the process described in detail above, the channel polysilicon 250 is formed early in the manufacturing process (e.g., before the formation of the shaft 263 described above with reference to Figures 2J-1 and 2J-2). In order to have a higher quality channel region in each thin-film storage transistor, in another embodiment, the channel polysilicon 250 is replaced after removing the sacrificial amorphous silicon 265. According to this other embodiment of the invention, after removing the amorphous silicon 265, the silicon nitride liner 264 is also removed. A top view and a cross-sectional view (in the XZ plane along the line A-A' in Figure 2P-1) of the resulting memory structure 200 after the silicon nitride liner 264 is removed are shown in Figures 2P-1 and 2P-2, according to another embodiment of the invention.
[0035] The channel polysilicon 250 is then removed, for example, by wet etching. A top view and a cross-sectional view (in the XZ plane along line A-A' in FIG. 2Q-1) of the resulting memory structure 200 after removal of the channel polysilicon 250 are shown in FIG. 2Q-1 and FIG. 2Q-2, respectively, according to another embodiment of the present invention.
[0036] Next, P - Doped channel polysilicon 280 is deposited, for example, up to 10 nm on the sidewalls of shaft 263 in the cavity obtained by removing channel polysilicon 250 from under charge trapping layer 268. A top view and a cross-sectional view (in the XZ plane along line A-A' in FIG. 2R-1) of memory structure 200 obtained after deposition of channel polysilicon 280 are shown in FIG. 2R-1 and FIG. 2R-2, respectively, according to another embodiment of the present invention.
[0037] Greater isolation may be provided by forming trenches in the channel polysilicon 280. A top view and a cross-sectional view (in the XZ plane along line A-A' in FIG. 2S-1) of the resulting memory structure 200 after forming trenches in the channel polysilicon 280 are shown in FIG. 2S-1 and FIG. 2S-2, respectively.
[0038] An ALD silicon oxide liner 285 (e.g., 10 nm) is then deposited on the sidewalls of the channel polysilicon 280 trench and shaft 263 to provide isolation. Top and cross-sectional views (in the XZ plane along line A-A' in FIG. 2T-1) of the resulting memory structure 200 after deposition of the ALD oxide liner 285 are shown in FIG. 2T-1 and FIG. 2T-2, respectively, in accordance with another embodiment of the present invention.
[0039] Silicon oxide may be deposited on shaft 263 to act as isolation between the thin-film storage transistors. Excess silicon oxide on the top surface of memory structure 200 may be removed by a planarization step (e.g., CMP). Shaft 263 may also be left unfilled, with voids acting as isolation between the thin-film storage transistors.
[0040] The above detailed description is provided to illustrate specific embodiments of the present invention and is not intended to be limiting. Numerous variations and modifications are possible within the scope of the present invention, which is set forth in the appended claims.
Claims
1. providing first and second multi-layer structures on a planar surface of a semiconductor substrate spaced apart from one another by trenches having a width in a first direction substantially parallel to said planar surface; the first and second multi-layer structures each include active multi-layer strips extending longitudinally along a second direction substantially perpendicular to the first direction and stacked together along a third direction substantially perpendicular to the surfaces, adjacent ones of the active multi-layer strips being electrically insulated from one another by layers of insulating material, each active multi-layer strip including first and second conductor layers spaced apart from one another by a dielectric material; forming a groove between adjacent layers of insulating material by recessing sidewalls of the trench in the active multi-layer strip along the first direction; placing a material in the groove; filling the trench with a first fill material; forming first and second shafts spaced apart along the second direction by removing a portion of each multi-layer strip from each of the first and second multi-layer structures and removing a portion of insulating material from the trenches in each shaft; filling the first and second shafts with a second filler material; removing the first fill material from the trench between the first shaft and the second shaft; and conformally depositing a data storage layer on the sidewalls of the trench and filling a remainder of the trench with a conductive material.
2. The method of claim 1 , wherein the insulating material comprises silicon oxycarbide (SiOC).
3. The method of claim 1 , wherein the data storage layer includes a tunneling layer, a charge storage layer, and a blocking layer.
4. The tunneling layer may be any silicon oxide (SiO x ), silicon nitride (SiN), silicon oxynitride (SiON), any aluminum oxide (AlO x ), any hafnium oxide (HfO x ), zirconium oxide (ZrO x) , any hafnium silicon oxide (HfSi x O y 4. The method of claim 3, further comprising one or more of: hafnium zirconium oxide (HfZrO);
5. The blocking layer may be any silicon oxide (SiO x ) and optional aluminum oxide (AlO x 4. The method of claim 3, comprising one or more of the following:
6. The charge storage layer is made of silicon nitride (SiN), hafnium oxide (HfO 2 4. The method of claim 3, wherein the insulating layer comprises one or more of:
7. The method of claim 1 , wherein the conductive material comprises a metal liner and a refractory metal.
8. The method of claim 7 , wherein the metal liner comprises one or more of titanium (Ti), titanium nitride (TiN), tantalum (Ta), and tantalum nitride (TaN).
9. The method of claim 7 , wherein the refractory metal comprises one or more of tungsten (W), tungsten nitride (WN), and molybdenum (Mo).
10. The method of claim 1 , wherein the first fill material comprises silicon oxide.
11. The method of claim 1 , further comprising forming a cap over both the data storage layer and the conductive material in the trench.
12. The method of claim 1 , wherein the predetermined material comprises a semiconductor layer.
13. The method of claim 12 including providing a dielectric liner on the sidewalls of the first and second shafts prior to filling the shafts with the second fill material.
14. The method of claim 13 , wherein the dielectric liner comprises silicon nitride.
15. The method of claim 13 , wherein the second fill material comprises silicon oxide.
16. 14. The method of claim 13, further comprising the step of removing the second fill material and replacing it with the insulating material after filling the trench with the conductive material.
17. The method of claim 11 , further comprising the step of removing the second fill material from the shaft and the predetermined material after forming the cap, and replacing the predetermined material with a semiconductor layer.
18. 20. The method of claim 17, further comprising sealing the semiconductor layer in the shaft with an atomic layer deposition (ALD) silicon oxide liner after replacing the selected material.
19. 20. The method of claim 18, further comprising filling the shaft with the insulating material after providing an ALD silicon oxide liner.
20. 2. The method of claim 1 , wherein the first and second conductor layers, the data storage layer, and the conductive material of each active multi-layer strip provide a common bit line, a common source line, a charge storage layer, and a gate electrode of thin-film storage transistors of a NOR memory string, respectively.
21. 10. The method of claim 1, wherein the trench is one of a plurality of trenches formed in a multi-layer structure, the trench being formed by multiple high aspect ratio etches.
22. 22. The method of claim 21 , wherein each said high aspect ratio etch has an aspect ratio of less than 50.
23. The method of claim 1 , wherein each of the active multi-layer strips further comprises a metal layer adjacent to and in contact with one or more of the first and second conductor layers.
24. 24. The method of claim 23, comprising the step of the metal layer of the active multi-layer strip replacing a sacrificial material that was disposed prior to forming the trench.
25. The method of claim 1 , further comprising providing an etch stop layer between the first and second multi-layer structures and the planar surface of the semiconductor substrate.
26. 26. The method of claim 25, wherein the etch stop layer comprises one or more of tungsten (W), tungsten nitride (WN), aluminum oxide (AlO), or aluminum nitride (AlN).
27. 26. The method of claim 25, further comprising a pad oxide layer between the etch stop layer and the planar surface of the semiconductor substrate.
Citation Information
Patent Citations
Porous silicon oxycarbide integrated circuit insulator
JP2003510795A
Storage device with multi-level structure
JP2008160121A
Nonvolatile semiconductor storage device
JP2010251572A
Capacitively Coupled Nonvolatile Thin-Film Transistor Strings in a Three-Dimensional Array
JP2019526934A
Process For Forming Resistive Switching Memory Cells Using Nano-Particles
US20140213032A1