Automatic kerf offset mapping and correction system for laser dicing.

The hybrid laser scribing and plasma etching process with offset correction addresses misalignment issues in semiconductor dicing, improving die yield and wafer efficiency by minimizing damage and optimizing die density.

JP7576108B2Active Publication Date: 2024-10-30APPLIED MATERIALS INC
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
JP2022578617
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-06-22
Filing Date
2021-05-20
Publication Date
2024-10-30
Estimated Expiration
2041-05-20

AI Technical Summary

Technical Problem

Current methods for dicing semiconductor wafers, such as scribing and sawing, result in chipping and cracking of integrated circuits due to misaligned scribe lines, leading to reduced die yield and wasted wafer area, while plasma dicing is limited by high costs and manufacturing issues.

Method used

A hybrid laser scribing and plasma etching process with automatic offset mapping and correction, using a sacrificial wafer to determine precise scribe line alignment, followed by laser scribing and plasma etching to singulate dies with improved accuracy.

Benefits of technology

Enhances die density and yield by minimizing chipping and cracking, optimizing wafer utilization, and reducing manufacturing costs through precise alignment and efficient dicing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007576108000001
    Figure 0007576108000001
  • Figure 0007576108000002
    Figure 0007576108000002
  • Figure 0007576108000003
    Figure 0007576108000003
Patent Text Reader

Abstract

Embodiments of the present disclosure include a method for determining scribing offset in a hybrid laser scribing and plasma dicing process. In one embodiment, the method includes forming a mask over a semiconductor wafer. In one embodiment, the semiconductor wafer includes multiple dies separated from one another by streets. In one embodiment, the method further includes patterning the mask and the semiconductor wafer with a laser scribing process. In one embodiment, the patterning provides openings in the streets. In one embodiment, the method further includes removing the mask and measuring the scribing offset of the openings relative to the streets.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims priority to U.S. Patent Application No. 16 / 908,537, filed June 22, 2020, the entire contents of which are incorporated herein by reference.

[0002] FIELD OF THE DISCLOSURE Embodiments of the present disclosure relate to the field of semiconductor processing, and more particularly to a method for dicing semiconductor wafers, each wafer having multiple integrated circuits thereon. [Background technology]

[0003] In semiconductor wafer processing, integrated circuits are formed on wafers (also called substrates) composed of silicon or other semiconductor materials. Typically, layers of various materials that are either semiconductive, conductive, or insulating are utilized to form the integrated circuits. These materials are doped, deposited, and etched using various well-known processes to form the integrated circuits. Each wafer is processed to form a number of individual areas that contain the integrated circuits, known as dies.

[0004] Following the integrated circuit formation process, the wafer is "diced" to separate the dies into separate dies for packaging or for use in unpackaged form in a larger circuit. The two main techniques used to dice wafers are scribing and sawing. In scribing, a diamond-tipped scriber is moved across the wafer surface along pre-formed scribe lines. These scribe lines extend along the spaces between the dies. These spaces are commonly referred to as "streets." The diamond scriber creates shallow scratches in the wafer surface along the streets. When pressure is applied, such as with a roller, the wafer separates along the scribe lines. The cracks in the wafer are aligned with the crystal lattice structure of the wafer substrate. Scribing can be used for wafers up to about 10 mils (thousandths of an inch) thick. For dicing thicker wafers, sawing is currently the preferred method.

[0005] In sawing, a diamond tipped saw rotating at high revolutions per minute contacts the wafer surface and cuts the wafer along the streets. The wafer is mounted on a support, such as an adhesive film stretched across a film frame, and the saw repeatedly strikes both the vertical and horizontal streets. A problem with both scribing and sawing is that chips and grooves can form along the cut edge of the die. In addition, cracks can form and propagate from the edge of the die into the substrate, rendering the integrated circuit inoperable. The crystal structure of the wafer is affected by the lattice constants, which can cause chips and grooves to form along the cut edge of the die. <110> In the 100 mm orientation, chipping and crack formation are particularly problematic with scribing because only one side of a square or rectangular die can be scribed. As a result, cleaving the other side of the die results in a jagged separation line. Chipping and crack formation require greater die spacing on the wafer (e.g., chips and cracks are kept a certain distance from the actual integrated circuit) to prevent damage to the integrated circuits. This spacing requirement results in fewer die being formed on a standard size wafer, wasting wafer real estate that could be used for circuits. The waste of semiconductor wafer real estate is exacerbated by the use of saws. The blade of a saw is approximately 15 microns thick. Thus, the circuits on each die must often be spaced 300 to 500 microns apart to prevent the integrated circuits from being adversely affected by cracks or other damage around the cuts made by the saw. Additionally, after sawing, each die must be thoroughly cleaned to remove particles and other contaminants from the sawing process.

[0006] Plasma dicing has also been used, but it can have limitations. For example, one limitation that can prevent the implementation of plasma dicing can be cost. Standard lithography steps for patterning resist can make the implementation cost prohibitive. Another limitation that can prevent the implementation of plasma dicing is that plasma processing of common metals (such as copper) for dicing along the streets can cause manufacturing issues or throughput limitations. Summary of the Invention

[0007] Embodiments of the present disclosure include a method for determining scribing offset in a hybrid laser scribing and plasma dicing process. In one embodiment, the method includes forming a mask over a semiconductor wafer. In one embodiment, the semiconductor wafer includes a plurality of dies separated from one another by streets. In one embodiment, the method further includes patterning the mask and the semiconductor wafer with a laser scribing process. In one embodiment, the patterning provides openings in the streets. In one embodiment, the method further includes removing the mask and measuring the scribing offset of the openings relative to the streets.

[0008] Embodiments disclosed herein may also include a method of singulating a semiconductor wafer. In one embodiment, the method may include forming a mask over the semiconductor wafer, where the semiconductor wafer includes a plurality of dies separated from one another by streets. In one embodiment, the method may further include patterning the mask and the semiconductor wafer with a laser scribing process that utilizes a wafer map integrated with offset correction. In one embodiment, the patterning forms openings through the mask and in the streets of the semiconductor wafer.

[0009] The embodiments disclosed herein may also include a semiconductor substrate. In one embodiment, the semiconductor substrate may include a device layer over the semiconductor substrate. In one embodiment, multiple dies are in the device layer, and the dies are separated from each other by streets. In one embodiment, the semiconductor substrate may further include trenches in the streets, where one or more of the trenches are misaligned with (offset from) the streets. [Brief description of the drawings]

[0010] [Figure 1] 1 is a flowchart depicting operations for determining an offset correction for a laser scribing process according to one embodiment. [Figure 2A] 2A-2C are cross-sectional views depicting a process for determining an offset correction for a laser scribing process, according to one embodiment. [Figure 2B] 2A-2C are cross-sectional views depicting a process for determining an offset correction for a laser scribing process, according to one embodiment. [Figure 2C] 2A-2C are cross-sectional views depicting a process for determining an offset correction for a laser scribing process, according to one embodiment. [Figure 3A] FIG. 2 is a plan view of a wafer having multiple dies separated by streets with scribe lines along the streets, according to one embodiment. [Figure 3B] FIG. 13 is a plan view of a scribe line having a translation offset from the centerline of the street, according to one embodiment. [Figure 3C] FIG. 13 is a plan view of a scribe line having an angular offset from the centerline of the street, according to one embodiment. [Figure 3D] FIG. 13 is a plan view of a non-linear scribe line in a street, according to one embodiment. [Figure 4] 1 is a flowchart depicting operations for singulating a semiconductor wafer, according to one embodiment. [Figure 5A] 5A-5C are cross-sectional views depicting a process for singulating a semiconductor wafer using a wafer map with offset correction, according to one embodiment. [Figure 5B] 5A-5C are cross-sectional views depicting a process for singulating a semiconductor wafer using a wafer map with offset correction, according to one embodiment. [Figure 5C] 5A-5C are cross-sectional views depicting a process for singulating a semiconductor wafer using a wafer map with offset correction, according to one embodiment. [Figure 6] 1 is a flowchart depicting operations for singulating a semiconductor wafer, according to one embodiment. [Figure 7A] 7A and 7B are cross-sectional views depicting a process for singulating a semiconductor wafer using a wafer map with offset correction, according to one embodiment. [Figure 7B] 7A and 7B are cross-sectional views depicting a process for singulating a semiconductor wafer using a wafer map with offset correction, according to one embodiment. [Figure 8] FIG. 1 illustrates a block diagram of a tool layout for laser and plasma dicing of a wafer or substrate according to one embodiment of the present disclosure. [Figure 9] 1 illustrates a block diagram of an exemplary computer system in accordance with one embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] A method for dicing semiconductor wafers, each having multiple integrated circuits (ICs) thereon, is described. In the following description, numerous specific details are described, such as an offset mapping approach for a hybrid laser and plasma dicing process, to provide a thorough understanding of embodiments of the present disclosure. It will be apparent to one of ordinary skill in the art that embodiments of the present disclosure may be practiced without these specific details. In other instances, well-known aspects, such as the fabrication of integrated circuits, have not been described in detail in order to not unnecessarily obscure embodiments of the present disclosure. Furthermore, it should be understood that the various embodiments shown in the figures are illustrative representations and are not necessarily drawn to scale.

[0012] A hybrid wafer or substrate dicing process may be performed that includes first laser scribing followed by plasma etching to singulate the dies. The laser scribing process may be used to cleanly remove the mask layers, organic and inorganic dielectric layers, and device layers. The laser scribing process may then be terminated once the wafer or substrate is exposed or partially scribed. The plasma etching portion of the dicing process may then be used to etch through the bulk of the wafer or substrate, such as bulk single crystal silicon, to effect singulation or dicing of the dies or chips. More specifically, one or more embodiments are directed to performing offset correction of laser-generated scribe lines, for example for dicing applications.

[0013] Automated offset mapping and correction for laser dicing operations is described herein. In one embodiment, a sacrificial wafer is used to identify the offset of the laser scribe lines relative to the centerlines of the streets between the dies. Because the laser dicing operation is highly repeatable, the offsets identified on the sacrificial wafer may be used during subsequent laser dicing operations of production wafers. In one embodiment, the sacrificial wafer is substantially similar to the production wafers that are subsequently singulated. In other embodiments, the sacrificial wafer is a short-loop wafer.

[0014] To provide context, in a hybrid wafer or substrate dicing process, a wafer map is used to generate a layout for laser scribe lines. After the wafer map is generated, the laser scribing process is performed. Currently, the scribe lines are measured in-situ using machine vision on the coated wafer during the laser scribing process. The determined offset is then applied on the fly to subsequent scribe lines to offset the measured offset. In such a situation, the presence of the coating may cause errors in the measured offset. In particular, the offset error may be due to the refractive effect of the coating. In addition, the offset is typically not uniform across the wafer. Therefore, using the offset measurement of a single scribe line is not an accurate way to account for the offset in subsequent scribe lines.

[0015] Misaligned (misregistered) scribe lines can result in the scribe lines being too close to the edge of the die. If the scribe lines are too close to the edge of the die, chipping and / or other damage resulting from the singulation process can damage the integrated circuits of the die. Thus, improperly aligned (misregistered) scribe lines lead to a reduced yield of dies from the wafer. To account for the misaligned (misregistered) scribe lines, the width of the streets between the dies may be increased. However, this reduces the usable area of ​​the wafer and reduces the number of dies per wafer. Thus, advantages of implementing one or more embodiments described herein may include one or more of: (1) more accurately aligned scribe lines, (2) increased die density on the wafer, and / or (3) higher wafer yield.

[0016] Embodiments of the present disclosure may include a process for identifying the offset of scribe lines across a wafer. In particular, the offset may be identified on a sacrificial wafer and then the measured offset may be applied to a production wafer that is subsequently singulated. The offset measured according to embodiments disclosed herein is more accurate than the in-situ measurement described above because the coating (i.e., mask layer) is removed before the measurement is made. Thus, the measurement is free of refraction errors. Furthermore, in some embodiments, the offset error of each scribe line on the wafer may be measured. This allows each scribe line to be adjusted independently, providing more accurate alignment across the wafer.

[0017] In accordance with one or more embodiments of the present disclosure, a method is provided for determining offset corrections for scribe lines on a semiconductor wafer including integrated circuits. Figure 1 is a flowchart 120 illustrating operations in a method for determining scribe line offsets for a semiconductor wafer including multiple integrated circuits according to one embodiment of the present disclosure. Figures 2A-2C show cross-sectional views of a semiconductor wafer including multiple integrated circuits during a method for determining offset corrections for scribe lines on a semiconductor wafer, corresponding to operations of flowchart 120, according to one embodiment of the present disclosure.

[0018] 2A, a mask 234 is formed over a semiconductor wafer or substrate 231. The mask 234 is comprised of a layer that covers and protects the integrated circuits 232 formed on the surface of the semiconductor wafer 231. The mask 234 also covers the intervening streets 233 formed between each integrated circuit 232.

[0019] According to one embodiment of the present disclosure, forming the mask 234 includes forming a layer, such as, but not limited to, a photoresist layer or an I-line patterning layer. For example, a polymer layer, such as a photoresist layer, may be composed of a material that would otherwise be suitable for use in a lithography process. In one embodiment, the photoresist layer is composed of a positive photoresist material, such as, but not limited to, a 248 nanometer (nm) resist, a 193 nm resist, a 157 nm resist, an extreme ultraviolet (EUV) resist, or a phenolic resin matrix with a diazonaphthoquinone sensitizer. In another embodiment, the photoresist layer is composed of a negative photoresist material, such as, but not limited to, polycis-isoprene or polyvinyl cinnamate.

[0020] In another embodiment, forming the mask 234 includes forming a layer that is deposited in a plasma deposition process. For example, in one such embodiment, the mask 234 is comprised of a plasma deposited Teflon or Teflon-like (polymeric CF2) layer. In one particular embodiment, the polymeric CF2 layer is deposited in a plasma deposition process that includes the gas C4F8.

[0021] In another embodiment, forming the mask 234 includes forming a water-soluble mask layer. In one embodiment, the water-soluble mask layer is readily dissolvable in an aqueous medium. For example, in one embodiment, the water-soluble mask layer is comprised of a material that is soluble in one or more of an alkaline solution, an acidic solution, or deionized water. In one embodiment, the water-soluble mask layer maintains its water solubility even when exposed to a heating process (e.g., heated in the range of about 50-160 degrees Celsius). For example, in one embodiment, the water-soluble mask layer is soluble in an aqueous solution after exposure to chamber conditions used in a laser and plasma etch singulation process. In one embodiment, the water-soluble mask layer is comprised of a material such as, but not limited to, polyvinyl alcohol, polyacrylic acid, dextran, polymethacrylic acid, polyethyleneimine, or polyethylene oxide. In a particular embodiment, the water-soluble mask layer has an etch rate in an aqueous solution in the range of about 1-15 microns per minute, and in particular, about 1.3 microns per minute.

[0022] In another embodiment, forming the mask 232 includes forming a UV curable mask layer. In one embodiment, the mask layer has a sensitivity to UV light that reduces the adhesive properties of the UV curable layer by at least about 80%. In one such embodiment, the UV layer is comprised of a polyvinyl chloride or acrylic material. In one embodiment, the UV curable layer is comprised of a material or stack of such materials whose adhesive properties weaken when exposed to UV light. In one embodiment, the UV curable adhesive film is sensitive to UV light at about 365 nm. In one such embodiment, this photosensitivity allows for the use of LED light to perform the cure.

[0023] In one embodiment, the semiconductor wafer or substrate 231 is made of a material suitable for withstanding the manufacturing process, upon which the semiconductor processing layers may be appropriately disposed. For example, in one embodiment, the semiconductor wafer or substrate 231 is made of a Group IV material, such as, but not limited to, crystalline silicon, germanium, or silicon / germanium. In a particular embodiment, providing the semiconductor wafer 231 includes providing a single crystal silicon substrate. In a particular embodiment, the single crystal silicon substrate is doped with impurity atoms. In another embodiment, the semiconductor wafer or substrate 204 is made of a III-V material, such as, for example, a III-V material substrate used in the fabrication of light emitting diodes (LEDs).

[0024] In one embodiment, a semiconductor wafer or substrate 231 has an array of semiconductor devices disposed thereon or within it as part of an integrated circuit 232. Examples of such semiconductor devices include, but are not limited to, memory devices or complementary metal oxide semiconductor (CMOS) transistors fabricated in a silicon substrate and encapsulated in a dielectric layer. Metal interconnects may be formed in the dielectric layer over and around the devices or transistors and may be used to electrically couple the devices or transistors to form the integrated circuit 232. The materials making up the streets 233 may be similar or identical to the materials used to form the integrated circuit 232. For example, the streets 233 may be composed of layers of dielectric materials, semiconductor materials, and metallization. In one embodiment, one or more of the streets 233 include test devices similar to the actual devices of the integrated circuit 232.

[0025] 2B, the mask 234 is patterned with a laser scribing process to provide a patterned mask 234 having gaps 235, exposing areas of the semiconductor wafer or substrate 231 between the integrated circuits 232. Thus, the laser scribing process is used to remove material of the streets 233 originally formed between the integrated circuits 232. According to one embodiment of the present disclosure, patterning the mask 234 with a laser scribing process includes forming trenches 235 partially in the areas of the semiconductor wafer 231 between the integrated circuits 232, as depicted by the dashed lines in FIG.

[0026] In one embodiment, the laser scribing process includes using a Gaussian source laser beam. In one such embodiment, the laser scribing process includes using a femtosecond source laser beam. For example, in one embodiment, a laser having a wavelength in the visible spectrum plus ultraviolet (UV) and infrared (IR) ranges (together a broadband optical spectrum) is used to provide the femtosecond-based laser pulses, and the femtosecond-based laser pulses are scribed over a period of about 10 femtoseconds (10 -15 In one embodiment, the ablation is not, or is substantially not, wavelength dependent, and is therefore suitable for composite films, such as films on mask 234, street 233, and possibly portions of semiconductor wafer or substrate 231.

[0027] To achieve a clean laser scribe cut, the selection of laser parameters such as beam profile will be important to develop a good laser scribing and dicing process that minimizes chipping, microcracks, and delamination. The cleaner the laser scribe cut, the smoother the etching process that may be performed for final die singulation. A semiconductor device wafer typically has multiple functional layers disposed thereon of different material types (e.g., conductors, insulators, semiconductors) and different thicknesses. Such materials may include, but are not limited to, organic materials such as polymers, metals, or inorganic dielectrics such as silicon dioxide and silicon nitride.

[0028] In one such embodiment, the femtosecond laser source has a pulse width in the range of about 10 femtoseconds to 500 femtoseconds, but preferably in the range of about 100 femtoseconds to 400 femtoseconds. In one embodiment, the femtosecond laser source has a wavelength in the range of about 1570 nanometers to 200 nanometers, but preferably in the range of about 540 nanometers to 250 nanometers. In one embodiment, the laser and corresponding optical system provide a focal spot at the work surface in the range of about 3 microns to 15 microns, but preferably in the range of about 5 microns to 10 microns, or between 10-15 microns.

[0029] In one embodiment, the laser source has a pulse repetition rate in the range of 200 kHz to 10 MHz, but preferably in the range of about 500 kHz to 5 MHz. In one embodiment, the laser source delivers pulse energy to the work surface in the range of about 0.5 μJ to 100 μJ, but preferably in the range of about 1 μJ to 5 μJ. In one embodiment, the laser scribing process travels along the workpiece surface at a speed in the range of about 500 mm / sec to 5 m / sec, but preferably in the range of about 600 mm / sec to 2 m / sec.

[0030] The scribing process may be performed in only one pass or multiple passes, but in one embodiment is preferably performed in 1-2 passes. In one embodiment, the scribe depth in the workpiece is in the range of about 5 microns to 50 microns, preferably in the range of about 10 microns to 20 microns deep. In one embodiment, the kerf width of the generated laser beam is in the range of about 2 microns to 15 microns, but preferably in the range of about 6 microns to 10 microns (as measured at the device / silicon interface) for scribing / dicing silicon wafers.

[0031] The laser parameters may be selected for benefits and advantages such as providing a sufficiently high laser intensity to achieve ionization of the inorganic dielectric (e.g., silicon dioxide) and minimizing damage to underlying layers resulting in delamination and chipping prior to direct ablation of the inorganic dielectric, etc. The parameters may also be selected to precisely control the ablation width (e.g., kerf width) and depth to provide a process throughput that is meaningful for industrial applications.

[0032] Referring to operation 123 of flowchart 120 and corresponding FIG. 2C, mask 234 is removed. Mask 234 may be removed by any suitable process depending on the material used for mask 234. In one particular embodiment, mask 234 may be removed by an ashing process or by exposure to a suitable solution to dissolve mask 234. In the case of a UV curable mask, mask 234 may be exposed to UV light prior to removal. After mask 234 is removed, an offset O of opening 235 relative to street 233 is measured. For example, offset O may be a measurement of the offset of the centerline of opening 235 relative to the centerline of street 233. Such an offset may be referred to as a translation offset. However, it should be understood that other offset types may also be measured. For example, offset may be an angular offset in some embodiments. Angular offset is described in more detail below. In one embodiment, the measurement may be performed using machine vision capabilities integrated with the laser scribing tool. In an alternative embodiment, the machine vision used to measure the offset may be located in a tool other than the laser scribing tool.

[0033] Referring to operation 125 of Flowchart 120, an offset correction is calculated. The offset correction is a correction parameter that may be added to the wafer map to account for the measured offset. In one embodiment, operation 126 of Flowchart 120 may include storing the offset correction. The offset correction may be stored in memory and may be used in subsequent laser scribing of production wafers.

[0034] 3A, a plan view of a wafer 330 is shown according to one embodiment. The wafer 330 may include a plurality of dies 336 distributed across a surface of the wafer 330. The dies 336 may be separated from one another by streets 337. The wafer 330 is a sacrificial wafer. That is, the wafer 330 may be used to provide offset correction values ​​for the scribe lines 335. The wafer 330 may not be further processed (e.g., the wafer 330 may not be singulated after the scribe lines 335 are formed).

[0035] In some embodiments, wafer 330 is substantially similar to a production wafer that will be subsequently singulated. In other embodiments, wafer 330 is a short-loop wafer. A short-loop wafer is a wafer that is manufactured with a subset of the processing operations used to provide a production wafer. For example, a short-loop wafer may include structures having dimensions equal to the dimensions of a die in a production wafer. A short-loop wafer may also include bumps on die 336. Using a short-loop wafer allows for reduced manufacturing costs since production wafers do not need to be sacrificed to provide offset measurements.

[0036] In one embodiment, laser scribe lines 335 are located in streets 337 of wafer 330. The laser scribe lines 335 can be measured to determine any offset from the streets 337 using a process similar to that described in flowchart 120 above. In one embodiment, all of the scribe lines 335 on the wafer are measured to provide offset correction for the entire wafer 330. In other embodiments, a subset of the scribe lines 335 are measured to provide offset correction.

[0037] 3B-3D, a series of plan views illustrating different categories of offsets are shown, in accordance with various embodiments.

[0038] 3B, a translation offset is illustrated according to one embodiment. As shown, a centerline 339 of the scribe line 335 is offset laterally from a centerline 338 of the street 337. In one such embodiment, the offset correction may include moving the scribe line 335 to align the centerline 339 of the scribe line 335 with the centerline 338 of the street 337.

[0039] 3C, an angular offset is illustrated according to one embodiment. As shown, a centerline 339 of the scribe line 335 is rotationally offset from a centerline 338 of the street 337 by an angle θ. In one such embodiment, the offset correction may include rotating the scribe line 335 by the angle θ to align the centerline 339 of the scribe line 335 with the centerline 338 of the street 337.

[0040] In Figures 3B and 3C, a single type of offset is provided (i.e., a translation offset in Figure 3B and an angular offset in Figure 3C), however, it should be understood that in some embodiments, the offset may also include both a translation offset and an angular offset.

[0041] 3D, a plan view of a scribe line 335 within a street 337 is shown according to a further embodiment. As shown, the scribe line 335 may have a non-linear shape. For example, the scribe line 335 of FIG. 3D has an S-shaped pattern. In such embodiments, the offset may be determined by measuring the offset at multiple locations and determining an average offset. For example, the offset at points A-E along the length of the scribe line 335 may be measured, and the average offset of points A-E can be used to provide the average offset of the scribe line 335. The average offset may include one or both of a translational offset and an angular offset.

[0042] In accordance with one or more embodiments of the present disclosure, a method is provided for dicing a semiconductor wafer including integrated circuits using offset correction. Figure 4 is a flowchart 440 illustrating operations of a method for dicing a semiconductor wafer including multiple integrated circuits according to one embodiment of the present disclosure. Figures 5A-5C show cross-sectional views of a semiconductor wafer including multiple integrated circuits during a method for dicing a semiconductor wafer corresponding to operations of flowchart 440 according to one embodiment of the present disclosure.

[0043] Referring to operation 441 of Flowchart 440 and corresponding FIG. 5A, a mask layer 534 is formed on a semiconductor wafer to provide a material stack 530 for hybrid laser ablation and plasma etch dicing. In one embodiment, the material stack 530 includes a mask layer 534, a device layer 532, and a substrate 531. The mask layer, device layer, and substrate are disposed on a die attach film 508 that is attached to a support tape 510. In one embodiment, the mask layer 534 is a water-soluble layer, such as the water-soluble layer described above in connection with mask 234. The device layer 532 includes an inorganic dielectric layer (such as a silicon dioxide layer) disposed on one or more metal layers (such as a copper layer) and one or more low-k dielectric layers (such as a carbon-doped oxide layer). The device layer 532 also includes streets 533 disposed between the integrated circuits, the streets including layers the same as or similar to the integrated circuits. The substrate 531 is a bulk single crystal silicon substrate.

[0044] In one embodiment, the bulk single crystal silicon substrate 531 is thinned from the backside prior to being attached to the die attach film 508. The thinning may be performed by a backside grinding process. In one embodiment, the bulk single crystal silicon substrate 531 is thinned to a thickness in the range of about 50-100 microns. It is important to note that in one embodiment, the thinning is performed prior to the dicing process of laser ablation and plasma etching. In one embodiment, the photoresist layer 534 has a thickness of about 5 microns and the device layer 532 has a thickness in the range of about 2-3 microns. In one embodiment, the die attach film 508 (or any suitable alternative capable of bonding a thinned or thinned wafer or substrate to the support tape 510) has a thickness of about 20 microns.

[0045] 5B, the mask layer 534 and the semiconductor wafer are patterned with a laser scribing process having an offset correction. In one embodiment, the offset correction may be specified using a sacrificial wafer (e.g., using a process such as the process described in Flowchart 120) prior to dicing of the material stack 530. Thus, the patterned trenches 535 may be substantially aligned with the streets 533. In one embodiment, operation 442 may include patterning the mask 534, the device layer 532, and a portion of the substrate 531 with a laser scribing process to form the trenches 535 in the substrate 531.

[0046] Referring to operation 443 and corresponding FIG. 5C , a deep through-silicon plasma etch process is used to extend trenches 535 down to die attach film 508, exposing a top portion of die attach film 508 and singulating silicon substrate 531. During the deep through-silicon plasma etch process, device layer 532 is protected by mask layer 534. In an embodiment, the singulation process may further include patterning die attach film 508, exposing a top portion of support tape 510, and singulating die attach film 508. In an embodiment, the die attach film is singulated by a laser process or by an etching process. Further embodiments may include subsequently removing the singulated portion of substrate 531 from support tape 510 (e.g., as individual integrated circuits). In an embodiment, the singulated die attach film 508 is retained on the backside of the singulated portion of substrate 531. Other embodiments may include removing mask layer 534 from device layer 532.

[0047] In one embodiment, etching the substrate 531 includes using a plasma etching process. In one embodiment, a through silicon via etching process is used. For example, in one particular embodiment, the etch rate of the material of the substrate 531 exceeds 25 microns per minute. For the plasma etching portion of the die singulation process, an ultra-high density plasma source may be used. One example of a suitable processing chamber for performing such a plasma etching process is the Applied Centura® Silvia™ Etch system available from Applied Materials, Sunnyvale, Calif., USA. The Applied Centura® Silvia™ Etch system combines capacitive and inductive RF coupling. This allows for more independent control of ion density and ion energy than is possible with capacitive coupling alone, with even improvements from magnetic enhancement. This combination effectively decouples ion density from ion energy, allowing for relatively high density plasma to be achieved even at very low pressures, without the use of potentially damaging high DC bias levels. This results in an exceptionally wide processing window. However, any plasma etch chamber capable of etching silicon may be used. In an exemplary embodiment, a deep silicon etch is used to etch a single crystal silicon substrate or wafer 531 at an etch rate that is greater than about 40% of a conventional silicon etch rate while maintaining essentially precise profile control and essentially scallop-free sidewalls. In a particular embodiment, a through-silicon via etch process is used. The etch process is based on a plasma generated from a reactive gas, typically a fluorine-based gas such as SF6, C4F8, CHF3, XeF2, or some other reactive gas capable of etching silicon at a relatively high etch rate. In another embodiment, the plasma etch operation described in connection with FIG. 5C employs a conventional Bosch dep / etch / dep process to etch through the substrate 531.Typically, the Bosch process consists of three sub-operations: deposition, directional bombardment etching, and isotropic chemical etching, which are performed multiple times (cycles) until the silicon is etched through.

[0048] 5A-5C, wafer dicing may be performed by initial ablation using a laser scribing process to ablate through the mask layer, through the wafer streets (including metallization), and partially into the silicon substrate. Die singulation may then be completed by a subsequent deep through-silicon plasma etch.

[0049] In accordance with one or more embodiments of the present disclosure, a method is provided for dicing a semiconductor wafer including integrated circuits using offset correction. Figure 6 is a flowchart 650 illustrating operations of a method for dicing a semiconductor wafer including multiple integrated circuits according to one embodiment of the present disclosure. Figures 7A-7B show cross-sectional views of a semiconductor wafer including multiple integrated circuits during a method for dicing a semiconductor wafer corresponding to operations of flowchart 650 according to one embodiment of the present disclosure.

[0050] Referring to operation 651 of Flowchart 650 and corresponding FIG. 7A, a mask layer 734 is formed on a semiconductor wafer to provide a material stack 730 for hybrid laser ablation and plasma etch dicing. In one embodiment, the material stack 730 includes a mask layer 734, a device layer 732, and a substrate 731. The mask layer, device layer, and substrate are disposed on a die attach film 708 that is attached to a support tape 710. In one embodiment, the mask layer 734 is a water-soluble layer, such as the water-soluble layer described above in connection with mask 234. The device layer 732 includes an inorganic dielectric layer (such as a silicon dioxide layer) disposed on one or more metal layers (such as a copper layer) and one or more low-k dielectric layers (such as a carbon-doped oxide layer). The device layer 732 also includes streets 733 disposed between the integrated circuits, the streets including layers the same as or similar to the integrated circuits. The substrate 731 is a bulk single crystal silicon substrate.

[0051] In one embodiment, the bulk single crystal silicon substrate 731 is thinned from the backside prior to being attached to the die attach film 708. The thinning may be performed by a backside grinding process. In one embodiment, the bulk single crystal silicon substrate 731 is thinned to a thickness of less than about 50 microns. It is important to note that in one embodiment, the thinning is performed prior to the dicing process of laser ablation and plasma etching. In one embodiment, the photoresist layer 734 has a thickness of about 5 microns and the device layer 732 has a thickness in the range of about 2-3 microns. In one embodiment, the die attach film 708 (or any suitable alternative capable of bonding a thinned or thinned wafer or substrate to the support tape 710) has a thickness of about 20 microns.

[0052] With reference to operation 652 of Flowchart 650 and corresponding FIG. 7B, the mask layer 734 and the semiconductor wafer are patterned with a laser scribing process having an offset correction. In one embodiment, the offset correction may be specified using a sacrificial wafer (e.g., using a process such as the process described in Flowchart 120) prior to dicing of the material stack 730. Thus, the patterned trenches 735 may be substantially aligned with the streets 733. In one embodiment, operation 652 may include patterning the mask 734, the device layer 732, and a portion of the substrate 731 with a laser scribing process to form the trenches 735 in the substrate 731.

[0053] It should be understood that in cases where laser scribing is used to pattern the mask as well as scribe completely through the wafer or substrate to singulate the die, the dicing or singulation process may be stopped after the laser scribing described above, and thus, in such cases, further singulation processing may not be required.

[0054] A single process tool may be configured to perform many or all of the operations in a laser ablation and plasma etch singulation process. For example, Figure 8 shows a block diagram of a tool layout for laser and plasma dicing of a wafer or substrate according to one embodiment of the present disclosure.

[0055] 8, processing tool 800 includes a factory interface 802 (FI) to which are coupled a number of load locks 804. A cluster tool 806 is coupled to the factory interface 802. The cluster tool 806 includes one or more plasma etch chambers, such as a plasma etch chamber 808. A laser scribing apparatus 810 is also coupled to the factory interface 802. The overall footprint of the process tool 800, in one embodiment, may be about 3500 millimeters (3.5 meters) by about 3800 millimeters (3.8 meters), as shown in FIG.

[0056] In one embodiment, the laser scribing apparatus 810 contains a laser assembly configured to provide a laser beam. In one such embodiment, the laser assembly is configured to provide machine vision capabilities suitable for measuring the offset of the scribe lines relative to the streets between the dies. In one embodiment, the laser scribing apparatus 810 is configured to provide offset measurements for all of the laser scribe lines on the wafer. In one embodiment, the laser assembly includes a Gaussian source laser beam. In one embodiment, the laser assembly includes a femtosecond source laser beam.

[0057] In one embodiment, the laser is suitable for performing the laser ablation portion of a hybrid laser and etch singulation process (such as the laser ablation process described above). In one embodiment, the laser scribe apparatus 810 also includes a moveable stage configured to move the wafer or substrate (or its carrier) relative to the laser. In one particular embodiment, the laser is also moveable. The overall footprint of the laser scribe apparatus 810 may be, in one embodiment, about 2240 millimeters by about 1270 millimeters, as depicted in FIG. 8.

[0058] In one embodiment, the one or more plasma etch chambers 808 are configured to etch the wafer / substrate through the gaps in the patterned mask to singulate the multiple integrated circuits. In one such embodiment, the one or more plasma etch chambers 808 are configured to perform a deep silicon etch process. In one particular embodiment, the one or more plasma etch chambers 808 are Applied Centura® Silvia™ Etch systems available from Applied Materials, Sunnyvale, Calif., USA. The etch chambers may be specifically designed for deep silicon etching used to create singulated integrated circuits contained on or in single crystal silicon substrates or wafers. In one embodiment, a high density plasma source is included in the plasma etch chamber 808 to increase the silicon etch rate. In one embodiment, two or more etch chambers are included in the cluster tool 806 portion of the process tool 800 to enable high manufacturing throughput of the singulation or dicing process.

[0059] Factory interface 802 may be an atmospheric port suitable for interfacing between an external manufacturing facility having a laser scribing apparatus 810 and cluster tool 806. Factory interface 802 may include a robot having an arm or blade for moving wafers (or their carriers) from a storage unit (e.g., a front-opening unified pod) to either or both of the cluster tool 806 or the laser scribing apparatus 810.

[0060] The cluster tool 806 may include other chambers suitable for performing functions in the singulation method. For example, in one embodiment, instead of the additional etch chamber, a deposition chamber 812 is included. The deposition chamber 812 may be configured to deposit a mask on or above the device layer of the wafer / substrate prior to laser scribing of the wafer / substrate. In one such embodiment, the deposition chamber 812 is suitable for depositing a photoresist layer. In another embodiment, instead of the additional etch chamber, a wet / dry station 814 is included. The wet / dry station may be suitable for cleaning residues and fragments or removing a mask after the substrate or wafer laser scribing and plasma etching singulation process. In yet another embodiment, instead of the additional deep silicon etch chamber, a plasma etch chamber is included, which is configured to perform a plasma-based cleaning process. In one embodiment, a metrology station is also included as a component of the processing tool 800.

[0061] Embodiments of the present disclosure may be provided as a computer program product or software that may include a machine-readable medium having instructions stored thereon, which may be used to program a computer system (or other electronic device) to perform a process according to an embodiment of the present disclosure. In one embodiment, the computer system is coupled to a process tool 800, as described in connection with FIG. 8. A machine-readable medium includes any mechanism for storing or transmitting information in a form readable by a machine (e.g., a computer). For example, a machine-readable (e.g., computer-readable) medium includes a machine (e.g., computer) readable storage medium (e.g., read-only memory (ROM), random access memory (RAM), magnetic disk storage media, optical storage media, flash memory devices, etc.), a machine (e.g., computer) readable transmission medium (in electrical, optical, acoustic, or other form of propagated signal (e.g., infrared signal, digital signal, etc.)), etc.

[0062] 9 shows a schematic diagram of a machine in the exemplary form of a computer system 900 within which a set of instructions may be executed to cause the machine to perform any one or more of the methods described herein. In alternative embodiments, the machine may be connected (e.g., networked) to other machines in a local area network (LAN), an intranet, an extranet, or the Internet. The machine may function as a server or a client machine in a client-server network environment, or as a peer machine in a peer-to-peer (or distributed) network environment. The machine may be a personal computer (PC), a tablet PC, a set-top box (STB), a personal digital assistant (PDA), a mobile phone, a web appliance, a server, a network router, switch, or bridge, or any machine capable of executing a set of instructions (sequential or otherwise) that define operations to be performed by the machine. Additionally, although a single machine is illustrated, the term "machine" should also be interpreted to include any collection of machines (e.g., computers) that individually or jointly execute a set (or sets) of instructions to perform any one or more of the methodologies described herein.

[0063] The exemplary computer system 900 includes a processor 902, a main memory 904 (e.g., read only memory (ROM), flash memory, dynamic random access memory (DRAM) such as synchronous DRAM (SDRAM) or Rambus DRAM (RDRAM), etc.), a static memory 906 (e.g., flash memory, static random access memory (SRAM), MRAM, etc.), and a secondary memory 918 (e.g., a data storage device), all of which communicate with each other via a bus 930.

[0064] Processor 902 represents one or more general-purpose processing devices, such as a microprocessor, a central processing unit, etc. More specifically, processor 902 may be a complex instruction set computing (CISC) microprocessor, a reduced instruction set computing (RISC) microprocessor, a very long instruction word (VLIW) microprocessor, a processor implementing other instruction sets, or a processor implementing a combination of instruction sets. Processor 902 may also be one or more special-purpose processing devices, such as an application specific integrated circuit (ASIC), a field programmable gate array (FPGA), a digital signal processor (DSP), a network processor, etc. Processor 902 is configured to execute processing logic 926 for performing the operations described herein.

[0065] The computer system 900 may further include a network interface device 908. The computer system 900 may also include a video display device 910 (e.g., a liquid crystal display (LCD), a light emitting diode display (LED), or a cathode ray tube (CRT)), an alphanumeric input device 912 (e.g., a keyboard), a cursor control device 914 (e.g., a mouse), and a signal generating device 916 (e.g., a speaker).

[0066] The secondary memory 918 may include a machine-accessible storage medium (or more specifically, a computer-readable storage medium) 932 having stored thereon one or more sets of instructions (e.g., software 922) that embody any one or more of the methods or functions described herein. The software 922 may also reside, completely or at least partially, within the main memory 904 and / or within the processor 902 during execution by the computer system 900. The main memory 904 and the processor 902 also constitute machine-readable storage media. The software 922 may also be transmitted or received over a network 920 via the network interface device 908.

[0067] While the exemplary embodiment illustrates the machine-accessible storage medium 932 as a single medium, the term "machine-readable storage medium" should be understood to include a single medium or multiple media (e.g., a centralized or distributed database, and / or associated caches and servers) that store one or more sets of instructions. The term "machine-readable storage medium" should also be interpreted to include any medium capable of storing or encoding a set of instructions that are executed by a machine and that cause the machine to perform any one or more of the methods of the present disclosure. Thus, the term "machine-readable storage medium" should be interpreted to include, but is not limited to, solid-state memories, optical media, and magnetic media.

[0068] In accordance with one embodiment of the present invention, a machine accessible storage medium has stored thereon instructions for causing a data processing system to perform a method for dicing a semiconductor wafer having a plurality of integrated circuits. The method includes forming a mask on the semiconductor wafer, the mask being comprised of a layer that covers and protects the integrated circuits. The mask is then patterned in a laser scribing process to provide openings in the streets. In one embodiment, the mask is removed and the scribing offset of the openings relative to the streets is measured. The measured offset may then be used in subsequent dicing of the wafer.

[0069] Thus, a hybrid wafer dicing approach using offset mapping of laser scribe lines in a laser beam and plasma etching process has been disclosed.

Claims

1. 1. A method for determining a scribing offset, comprising: forming a mask over a semiconductor wafer, the semiconductor wafer including a plurality of dies separated from one another by streets; patterning the mask and the semiconductor wafer with a laser scribing process to provide openings in the streets; removing the mask; and measuring a scribing offset of the opening relative to the street; the scribe lines in the street have a non-linear S-shaped pattern; Measuring the scribing offset comprises: measuring the offset at multiple points along the length of the non-linear S-shaped pattern of the scribe lines; and calculating an average offset of the offsets of the plurality of locations.

2. The method of claim 1 , wherein the scribing offset comprises a translation offset.

3. The method of claim 1 , wherein the scribing offset comprises an angular offset.

4. The method of claim 1 , wherein measuring the scribing offsets comprises measuring the offsets of all of the openings on the semiconductor wafer.

5. Calculating an offset correction; and The method of claim 1 , further comprising storing the offset correction.

6. 6. The method of claim 5, further comprising using the offset correction to update a wafer map used in a subsequent semiconductor wafer scribing process.

7. The method of claim 1 , wherein the semiconductor wafer is a production wafer.

8. The method of claim 1 , wherein the semiconductor wafer is a short loop wafer.

9. The method of claim 8 , wherein the short loop wafer includes the same bumping and die dimensions as a production wafer.

10. 1. A method for singulating a semiconductor wafer, comprising: forming a mask over a semiconductor wafer, the semiconductor wafer including a plurality of dies separated from one another by streets; patterning the mask and the semiconductor wafer with a laser scribing process utilizing a wafer map with integrated offset correction, the patterning including providing openings through the mask into the streets of the semiconductor wafer; the scribe lines in the street have a non-linear S-shaped pattern; The offset correction is measuring the offset at multiple points along the length of the non-linear S-shaped pattern of the scribe lines; and The offset is determined based on calculating an average offset of the offsets of the plurality of locations; The average offset is added to the wafer map.

11. The method of claim 10 , wherein the laser scribing process singulates the multiple dies of the semiconductor wafer.

12. The method of claim 10 , further comprising plasma etching the semiconductor wafer through the openings, the plasma etching singulating the plurality of dies of the semiconductor wafer.

13. The method of claim 10 , wherein the offset correction comprises a translation offset.

14. The method of claim 10 , wherein the offset correction comprises an angular offset.

Citation Information

Patent Citations

  • Processing device by energy beam

    JP1986206584A

  • Laser beam machine

    JP1998058173A

  • Alignment device and alignment method

    JP2004288792A

  • Laser beam machining device

    JP2005046891A

  • Alignment method of machining device

    JP2009021317A