Laminate
The laminate with a rosin layer between the diamond-like carbon and polyolefin base layer addresses the challenge of poor adhesion, resulting in improved barrier properties.
Patent Information
- Application Number
- JP2021126063
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-07-30
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2041-07-30
AI Technical Summary
Diamond-like carbon layers struggle to exhibit good barrier properties when laminated on base layers made of synthetic resin materials with polyolefin as the main component due to the rough surface of polyolefin, unlike polyester.
A laminate structure is developed with a diamond-like carbon layer laminated via a rosin layer on a base layer composed of polyolefin, where the rosin layer improves the adhesion and barrier properties.
The laminate achieves excellent barrier properties by using a rosin layer to facilitate the lamination of the diamond-like carbon layer on polyolefin-based base layers, enhancing the laminate's performance.
Smart Images

Figure 0007577421000002 
Figure 0007577421000003 
Figure 0007577421000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a laminate. [Background technology]
[0002] 2. Description of the Related Art A laminate having a diamond-like carbon layer laminated on a base layer formed of a synthetic resin material containing polyester as a main component is known (see, for example, Patent Document 1). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2009-241985 A Summary of the Invention [Problem to be solved by the invention]
[0004] It is known that a diamond-like carbon layer capable of exhibiting good barrier properties is laminated on a base layer formed of a synthetic resin material mainly composed of polyester. However, when the base layer is formed of a synthetic resin material mainly composed of polyolefin, not polyester, the surface of the base layer is relatively rough compared to that of polyester, and it has been considered difficult to laminate the diamond-like carbon layer so as to exhibit good barrier properties.
[0005] SUMMARY OF THE PRESENT EMBODIMENTS An object of the present invention is to provide a laminate having a diamond-like carbon layer capable of exhibiting good barrier properties on a substrate layer formed of a synthetic resin material containing polyolefin as a main component. [Means for solving the problem]
[0006] The laminate of the present invention is a laminate having a diamond-like carbon layer laminated via a rosin layer on a substrate layer formed of a synthetic resin material containing polyolefin as a main component.
[0007] In addition, the laminate of the present invention having the above-mentioned configuration is preferably a laminate in which 75% by weight or more of the base layer is the polyolefin.
[0008] In the laminate of the present invention having the above-mentioned configuration, the base material layer preferably contains a fibrous material.
[0009] In the laminate of the present invention having the above-mentioned configuration, the fiber material preferably contains vegetable fiber.
[0010] In addition, in the above-mentioned configuration, the laminate of the present invention is preferably a laminate forming at least a part of a container.
[0011] In addition, the method for manufacturing a laminate of the present invention is preferably a method for manufacturing a laminate having a preparation step of preparing the base layer, a coating step of forming the rosin layer by coating rosin on the base layer, and a deposition step of forming the diamond-like carbon layer by depositing diamond-like carbon on the rosin layer. Effect of the Invention
[0012] According to the present invention, it is possible to provide a laminate having a diamond-like carbon layer capable of exhibiting good barrier properties on a substrate layer formed of a synthetic resin material containing polyolefin as a main component. [Brief description of the drawings]
[0013] [Figure 1] 1 is a partially cross-sectional side view showing a laminate according to one embodiment of the present invention. [Diagram 2] 1 is a graph showing the measurement results of oxygen transmission rates in Examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.
[0015] As shown in FIG. 1, in one embodiment of the present invention, a laminate 1 has a base layer 2, a rosin layer 3, and a diamond-like carbon layer 4 (hereinafter, diamond-like carbon: also referred to as DLC) and forms at least a part of a container.
[0016] In this embodiment, the container has a cup-shaped container body 5 and a sealing material (not shown). The container body 5 has a peripheral wall 5a, a bottom wall 5b connected to the lower end of the peripheral wall 5a, and a flange wall 5c connected to the upper end of the peripheral wall 5a. The sealing material is releasably attached to the upper surface of the flange wall 5c when the container body 5 is filled with contents, and the laminate 1 forms the peripheral wall 5a and the bottom wall 5b.
[0017] The container is not limited to one having a cup-shaped container body 5, but may be, for example, one having a bottle-shaped container body 5 and a cap, a compact container for cosmetics, etc. Furthermore, the laminate 1 is not limited to one that forms at least a part of the container body 5, but may be one that forms at least a part of a lid member such as a cap. Furthermore, the laminate 1 is not limited to one that forms at least a part of the container.
[0018] The DLC layer 4 is laminated on the base layer 2 via the rosin layer 3. In this embodiment, the laminate 1 has the DLC layer 4 only on one side of the base layer 2, but this is not limited thereto, and the DLC layer 4 may be provided on both sides of the base layer 2. In this embodiment, the laminate 1 has the DLC layer 4 only on the container inner surface side of the base layer 2, but this is not limited thereto, and the DLC layer 4 may be provided only on the container outer surface side of the base layer 2. In addition, an additional layer having protection, decoration, or other desired functions may be provided on one or both sides of the laminate 1.
[0019] The base layer 2 is formed of a synthetic resin material mainly composed of polyolefin. That is, more than 50% by weight of the synthetic resin material forming the base layer 2 is polyolefin. When the base layer 2 is formed of such a synthetic resin material, it is difficult to laminate the DLC layer 4 directly onto the base layer 2 so as to exhibit good barrier properties, but good barrier properties can be exhibited by laminating the DLC layer 4 onto the base layer 2 via a rosin layer 3.
[0020] The base layer 2 may contain a component other than the above synthetic resin material. Even in this case, good barrier properties can be exhibited by laminating the DLC layer 4 on the base layer 2 via the rosin layer 3.
[0021] When the base layer 2 contains a component other than the above synthetic resin material, it is preferable that the ratio of polyolefin in the base layer 2 is high, and it is particularly preferable that 75% by weight or more of the components of the base layer 2 are polyolefin. When 75% by weight or more of the components of the base layer 2 are polyolefin, particularly good barrier properties can be exhibited by laminating the DLC layer 4 on the base layer 2 via the rosin layer 3.
[0022] The base layer 2 may contain a fiber material, and even in this case, good barrier properties can be exhibited by laminating the DLC layer 4 on the base layer 2 via the rosin layer 3. The fiber material is not particularly limited, but is, for example, vegetable fiber (such as cellulose). By using vegetable fiber as the fiber material, environmental compatibility can be improved.
[0023] The polyolefin is not particularly limited, and examples thereof include polypropylene, polyethylene, and blends thereof.
[0024] The rosin that forms the rosin layer 3 is the residue remaining after collecting balsams such as pine resin and distilling turpentine essential oil, and is a natural resin whose main components are rosin acids (abietic acid, palustric acid, isopimaric acid, etc.).
[0025] The method for laminating the rosin layer 3 on the base layer 2 is not particularly limited, and may be, for example, coating. The coating method is not particularly limited, and various methods may be used, such as dip coating, spray coating, spin coating, brush coating, etc. When wet coating is performed, for example, a rosin solution obtained by dissolving rosin in a solvent such as alcohol may be coated on the base layer 2.
[0026] The DLC layer 4 is an amorphous hard film made of a hydrocarbon or a carbon allotrope, and can be formed by, for example, a vapor deposition method. Vapor deposition methods that can be used include, for example, chemical vapor deposition (CVD) and physical vapor deposition (PVD). Examples of chemical vapor deposition include plasma CVD and thermal CVD. Examples of power sources used in plasma CVD include high frequency and microwaves.
[0027] The DLC layer 4 can be formed by plasma CVD using, for example, acetylene (C2H2) as a source gas. In this case, it is preferable to use a high frequency power source.
[0028] The laminate 1 can be manufactured, for example, through a preparation step, a coating step, and a vapor deposition step. The preparation step is a step of preparing a base layer 2. The coating step is a step of forming a rosin layer 3 by coating rosin on the base layer 2. The vapor deposition step is a step of forming a DLC layer 4 by vapor depositing DLC on the rosin layer 3.
[0029] The present invention is not limited to the above-described embodiment, and various modifications can be made without departing from the spirit and scope of the present invention.
[0030] Therefore, the laminate 1 of the above-mentioned embodiment can be modified in various ways as long as it is a laminate 1 having a diamond-like carbon layer 4 laminated on a base layer 2 formed of a synthetic resin material mainly composed of polyolefin via a rosin layer 3.
[0031] In addition, the laminate 1 of the above-described embodiment is preferably a laminate 1 in which 75% by weight or more of the base layer 2 is polyolefin in the above configuration.
[0032] In addition, in the laminate 1 of the above-described embodiment, it is preferable that the base material layer 2 of the laminate 1 contains a fiber material in the above configuration.
[0033] Moreover, in the laminate 1 of the above-described embodiment, in the above configuration, the fiber material preferably contains vegetable fiber.
[0034] Moreover, the laminate 1 of the above-described embodiment is preferably a laminate 1 that forms at least a part of a container in the above configuration.
[0035] In addition, the manufacturing method of the laminate 1 in the above-mentioned embodiment is preferably a manufacturing method of the laminate 1 having a preparation step of preparing a base layer 2, a coating step of forming a rosin layer 3 by coating rosin on the base layer 2, and a deposition step of forming a diamond-like carbon layer 4 by depositing diamond-like carbon on the rosin layer 3. EXAMPLES
[0036] Four samples with different materials for the base layer were prepared, and samples with neither rosin nor DLC layers, samples with only rosin layers, samples with only DLC layers, and samples with both rosin and DLC layers were produced to evaluate the oxygen barrier properties. The rosin layer was prepared by applying a rosin solution obtained by dissolving rosin in alcohol and drying it. For the samples with DLC layers, multiple types of rosin solutions with different rosin concentrations ranging from 3% to 50% by weight were prepared, and the rosin layers were prepared by applying each rosin solution, and the DLC layers were laminated, and the oxygen permeability was measured. The oxygen permeability was measured by the MOCON method under conditions of 23°C-55% RH on the outside and 23°C-90% RH on the inside. For samples 1 to 4, the oxygen permeability of the untreated sample without rosin coating or DLC deposition divided by the oxygen permeability of the sample with DLC deposition that showed the best barrier properties (i.e., the smallest oxygen permeability) was calculated as the barrier improvement factor BIF (barrier improvement factor). The results are shown in Table 1 below. [Table 1]
[0037] In sample 1, the base layer was formed using only polypropylene, in sample 2, the base layer was formed using polypropylene and cellulose (polypropylene content: 80% by weight), in sample 3, the base layer was formed using only a paper-blended resin (MAPKA (registered trademark) manufactured by Environmental Management Research Institute Co., Ltd., polypropylene content: 49% by weight), and in sample 4, the base layer was formed using a material obtained by blending the above-mentioned paper-blended resin and polypropylene in a 5:5 ratio.
[0038] Samples 1 to 4 were cup-shaped containers with an opening diameter of 76 mm and a total height of 75 mm, and the rosin layer and DLC layer were provided only on the inner surface of the container. The higher the rosin concentration, the easier it is to apply a larger amount of rosin by coating, but when the rosin concentration exceeds 50 wt%, coating of the rosin tends to become difficult. When the rosin concentration is 20 wt% or more, there was no significant change in the amount of rosin coating formed by coating and drying. The amount of rosin coating measured on the inner surface of the cup after drying was 0.10 to 0.16 g for a 20 wt% solution, 0.16 to 0.18 g for a 30 wt% solution, 0.18 to 0.19 g for a 40 wt% solution, and 0.17 to 0.22 g for a 50 wt% solution. The DLC layer in Samples 1 to 4 was formed by plasma CVD using acetylene as a raw material gas. At that time, a high frequency power source was used, the output setting was 800 W, and the film formation time was 1.6 seconds. In sample 1, the thickness of the formed DLC layer was 29 nm at the 75 mm and 45 mm height parts of the peripheral wall of the container body, 27 nm at the bottom wall part, and 28 nm on average.
[0039] As shown in Table 1, when no DLC layer was provided in Samples 1 to 4, the presence or absence of a rosin layer did not affect the oxygen barrier properties. Furthermore, among Samples 1 to 4 that had a rosin layer and a DLC layer, good oxygen barrier properties were observed, with a BIF of 3.6 even in Sample 3, which had the lowest polypropylene blend ratio (49 wt%), and a BIF of 76 in Sample 1, which had the highest polypropylene blend ratio (100 wt%).
[0040] The relationship between the rosin concentration and the oxygen transmission rate for the samples 1 to 4 with the DLC layer is shown in FIG. 2. As shown in FIG. 2, the oxygen transmission rate was suppressed by providing a rosin layer in all of the samples 1 to 4 with different fiber material blending rates. It is considered that the polar group of the rosin contributes to good film formation of the DLC layer by providing the DLC layer via the rosin layer. In addition, in all of the samples 1 to 4, the oxygen transmission rate was suppressed as the rosin concentration increased until the rosin concentration (i.e., the weight of the rosin that was applied) reached a certain value. In particular, in samples 1, 2, and 4 with polypropylene blending rates of 75% by weight or more, the oxygen transmission rate at a rosin concentration of 10% by weight was significantly suppressed compared to sample 3. [Explanation of symbols]
[0041] 1. Laminate 2 Base material layer 3 Rosin layer 4 DLC layer (Diamond-Like Carbon layer) 5 Container body 5a Peripheral wall 5b Bottom wall 5c flange wall
Claims
1. A laminate having a diamond-like carbon layer laminated on a base layer formed of a synthetic resin material containing polyolefin as a main component, with a rosin layer interposed therebetween.
2. The laminate according to claim 1 , wherein 75% by weight or more of the component of said base layer is said polyolefin.
3. The laminate according to claim 1 or 2, wherein the substrate layer comprises a fibrous material.
4. The laminate of claim 3 , wherein the fibrous material comprises vegetable fibers.
5. The laminate according to any one of claims 1 to 4, which forms at least a part of a container.
6. The method for manufacturing the laminate according to any one of claims 1 to 5, comprising: a preparation step of preparing the base layer; a coating step of forming the rosin layer by coating rosin on the base layer; and a deposition step of forming the diamond-like carbon layer by depositing diamond-like carbon on the rosin layer.
Citation Information
Patent Citations
primer
JP1984202230A
Biodegradable paper sheet and paper container
JP2003013391A
Cup-formed plastic container
JP2003072763A
Laminate and multi-layer plastic container using laminate
JP2004174782A
Container made of polyester resin excellent in gas barrier and heat-resistant properties
JP2009241985A