Reconstituted tobacco sheet manufacturing apparatus and method
The described apparatus and method for manufacturing reconstituted tobacco sheets ensure uniform thickness and efficient cutting by using a die and slitting drum, addressing the challenge of varying water content in the raw material.
Patent Information
- Application Number
- JP2022538647
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-07-20
- Filing Date
- 2021-06-22
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2041-06-22
AI Technical Summary
Existing methods for manufacturing reconstituted tobacco sheets struggle to produce uniform thickness regardless of the water content in the raw material, requiring different apparatuses for varying water contents and complicating the manufacturing process.
A reconstituted tobacco sheet manufacturing apparatus and method that includes a die for forming and discharging the raw material into a sheet shape, a slitting drum for cutting, and a packaging device for efficient delivery, allowing for uniform thickness and cutting regardless of water content.
Enables the production of uniformly thick reconstituted tobacco sheets through a simple process, with efficient cutting and packaging, suitable for various water contents in the raw material.
Smart Images

Figure 0007577746000007 
Figure 0007577746000008 
Figure 0007577746000009
Abstract
Description
[Technical field]
[0001] The present invention relates to an apparatus and method for producing a reconstituted tobacco sheet. [Background technology]
[0002] Conventionally, the rolling method, the casting (slurry) method, and the paper-making method are known as methods for manufacturing reconstituted tobacco sheets. These manufacturing methods are selected according to the moisture content of the reconstituted tobacco raw material. Furthermore, each of these manufacturing methods is realized by a different reconstituted tobacco sheet manufacturing device.
[0003] The rolling method is known to be particularly suitable for reconstituted tobacco raw materials that contain less than 50% moisture by volume. In the rolling method, the kneaded material of the reconstituted tobacco raw materials is rolled and molded with rotating rollers to adjust the thickness, and then dried in a separately installed dryer.
[0004] The cast (slurry) method is known to be particularly suitable for reconstituted tobacco raw materials that contain 50% or more moisture by volume. In the cast (slurry) method, a fluid of the reconstituted tobacco raw material is continuously spread on a rotating drum or belt conveyor, and is smoothed to a desired thickness with a member called a blade, after which it is peeled off from the rotating drum or belt conveyor and dried in a separately provided dryer (see, for example, Patent Document 1).
[0005] The papermaking method is known to be particularly suitable for reconstituted tobacco raw materials containing 80% or more moisture by volume. In the papermaking method, a fluid of the reconstituted tobacco raw material is continuously spread on a liquid-permeable belt conveyor, and after the moisture is removed and the reconstituted tobacco raw material is made into a desired thickness by a compression roller, it is dried in a separately provided dryer. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Special Publication No. 2019-520036 Summary of the Invention [Problem to be solved by the invention]
[0007] An object of the present invention is to provide an apparatus and method for producing a reconstituted tobacco sheet that can obtain cut reconstituted tobacco sheets having a uniform thickness through a simple production process, regardless of the moisture content contained in the reconstituted tobacco raw material. [Means for solving the problem]
[0008] According to a first aspect of the present invention, there is provided a reconstituted tobacco sheet manufacturing apparatus. This reconstituted tobacco sheet manufacturing apparatus includes a die that forms and discharges reconstituted tobacco raw material into a sheet shape, and a slitting drum that cuts the sheet-like reconstituted tobacco raw material discharged from the die, and the die has a housing, a supply port formed in the housing through which the reconstituted tobacco raw material is supplied, and a discharge port formed on one side of the housing through which the reconstituted tobacco raw material is discharged. This makes it possible to obtain a cut reconstituted tobacco sheet of uniform thickness through a simple manufacturing process, regardless of the moisture content of the reconstituted tobacco raw material.
[0009] According to a second aspect of the present invention, the first aspect further includes a main drum that is disposed before the slitting drum and dries and conveys the reconstituted tobacco raw material discharged from the die. This allows the reconstituted tobacco sheet to be cut immediately after drying. In addition, by disposing the slitting drum after the main drum that dries the raw material, it is possible to prevent tar from adhering to the slitting drum.
[0010] According to a third aspect of the present invention, in the first or second aspect, a packing device is further provided downstream of the slitting drum, and the packing device has a weighing mechanism that measures the weight of a container in which the reconstituted tobacco raw material cut by the slitting drum is packed, and a conveying mechanism that carries the container into the weighing mechanism and carries the container out of the weighing mechanism. This allows the reconstituted tobacco raw material cut by the slitting drum to be efficiently packed and delivered to a downstream process.
[0011] According to a fourth aspect of the present invention, there is provided a method for producing a reconstituted tobacco sheet. This method for producing a reconstituted tobacco sheet comprises the steps of: supplying reconstituted tobacco raw material to a supply port of a die; forming and discharging the reconstituted tobacco raw material into a sheet shape from the discharge port of the die; and cutting the sheet-shaped reconstituted tobacco raw material discharged from the die. This makes it possible to obtain a cut reconstituted tobacco sheet of uniform thickness through a simple production process, regardless of the moisture content of the reconstituted tobacco raw material. [Brief description of the drawings]
[0012] [Figure 1] FIG. 1 is a side view showing a manufacturing apparatus for reconstituted tobacco sheets according to a first embodiment of the present invention. [Diagram 2] FIG. 1 is a cross-sectional view showing an extruder of a reconstituted tobacco sheet manufacturing apparatus according to a first embodiment of the present invention. [Diagram 3] 3 is a cross-sectional view taken along line III-III in FIG. 2. [Figure 4] FIG. 2 is a cross-sectional view showing a die of the reconstituted tobacco sheet manufacturing apparatus according to the first embodiment of the present invention. [Diagram 5] 5 is a cross-sectional view taken along the line VV in FIG. 4. [Figure 6] FIG. 5 is a side view of the die shown in FIG. 4, seen from the discharge port side. [Figure 7] FIG. 4 is a plan view showing a manufacturing apparatus for a reconstituted tobacco sheet according to a second embodiment of the present invention. [Figure 8] FIG. 4 is a plan view showing a manufacturing apparatus for reconstituted tobacco sheets according to a third embodiment of the present invention. [Figure 9] FIG. 11 is a side view showing a manufacturing apparatus for a reconstituted tobacco sheet according to a fifth embodiment of the present invention. [Figure 10] FIG. 13 is a side view of a die of a reconstituted tobacco sheet manufacturing device according to a sixth embodiment of the present invention, viewed from the discharge port side. [Figure 11] FIG. 13 is a side view of a die of a reconstituted tobacco sheet manufacturing device according to a seventh embodiment of the present invention, viewed from the discharge port side. [Figure 12] FIG. 13 is a side view of another die of the reconstituted tobacco sheet production device according to the seventh embodiment of the present invention, viewed from the discharge port side. [Figure 13] FIG. 13 is a side view showing a manufacturing apparatus for a reconstituted tobacco sheet according to an eighth embodiment of the present invention. [Figure 14] FIG. 13 is a side view showing a manufacturing apparatus for a reconstituted tobacco sheet according to a ninth embodiment of the present invention. [Figure 15] FIG. 23 is a side view showing a manufacturing apparatus for a reconstituted tobacco sheet according to a tenth embodiment of the present invention. [Figure 16] FIG. 23 is a side view showing a manufacturing apparatus for a reconstituted tobacco sheet according to a twelfth embodiment of the present invention. [Figure 17] FIG. 23 is a side view showing a manufacturing apparatus for a reconstituted tobacco sheet according to a thirteenth embodiment of the present invention. [Figure 18] FIG. 23 is a block diagram showing opening width control in a reconstituted tobacco sheet manufacturing apparatus according to a thirteenth embodiment of the present invention. [Figure 19] FIG. 23 is a side view showing a manufacturing apparatus for a reconstituted tobacco sheet according to a fourteenth embodiment of the present invention. [Figure 20] FIG. 23 is a block diagram showing the discharge speed control in the reconstituted tobacco sheet manufacturing apparatus according to the fourteenth embodiment of the present invention. [Figure 21] FIG. 23 is a side view showing a manufacturing apparatus for a reconstituted tobacco sheet according to a fifteenth embodiment of the present invention. [Figure 22] FIG. 23 is a block diagram showing hot air temperature control in a reconstituted tobacco sheet manufacturing apparatus according to a fifteenth embodiment of the present invention. [Figure 23]FIG. 23 is a side view showing a manufacturing apparatus for a reconstituted tobacco sheet according to a sixteenth embodiment of the present invention. [Figure 24] FIG. 23 is a side view showing a manufacturing apparatus for a reconstituted tobacco sheet according to a seventeenth embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] The reconstituted tobacco sheet manufacturing apparatus and method according to the present invention will be described below with reference to the drawings, in which the same or corresponding parts in each drawing are denoted by the same reference numerals.
[0014] First embodiment: Fig. 1 is a side view showing a reconstituted tobacco sheet manufacturing apparatus according to a first embodiment of the present invention. In Fig. 1, the reconstituted tobacco sheet manufacturing apparatus 100 includes an extruder 10, a die 20, a drum dryer (main drum) 30, a scraper 40, and rollers 51, 52. The drum dryer 30 has a shaft 31 and a drum body 32.
[0015] The extruder 10 pressure-feeds the reconstituted tobacco raw material supplied from a tank or the like (not shown) to the die 20. The die 20 discharges the reconstituted tobacco raw material supplied from the extruder 10, whereby the reconstituted tobacco raw material is formed as a reconstituted tobacco sheet 1 on the drum body 32 of the drum dryer 30. The drum dryer 30 dries and transports the reconstituted tobacco sheet 1 formed on the drum body 32. The scraper 40 peels the reconstituted tobacco sheet 1 dried by the drum dryer 30 from the drum body 32. Rollers 51, 52 guide the transport of the reconstituted tobacco sheet 1 peeled off by the scraper 40.
[0016] Here, the reconstituted tobacco raw material is a kneaded product containing at least one substance selected from polysaccharides (starch, dextrin, etc.), water or alcohol (ethanol, propylene glycol, etc.) as an arbitrary liquid medium, or at least one substance selected by the user, and tobacco plant flakes or granules. Note that the reconstituted tobacco raw material is not limited to the above and may contain other substances.
[0017] Fig. 2 is a configuration diagram showing an extruder of a reconstituted tobacco sheet manufacturing apparatus according to a first embodiment of the present invention. Fig. 3 is a cross-sectional view taken along the line III-III shown in Fig. 2. In Figs. 2 and 3, an extruder 10 has a housing 11, a supply port 12 formed at one end of the housing 11, an extrusion port 13 formed at the other end of the housing 11, and a screw 14 rotatably disposed within the housing 11.
[0018] The reconstituted tobacco raw material supplied to the extruder 10 through the supply port 12 from a tank or the like is sent to the extrusion port 13 while being kneaded by the rotation of the screw 14, and is then pumped from the extrusion port 13 to the die 20. Here, the discharge speed of the reconstituted tobacco sheet 1 discharged from the die 20 is determined according to the rotation speed of the screw 14.
[0019] Fig. 4 is a cross-sectional view showing a die of a manufacturing apparatus for a reconstituted tobacco sheet according to a first embodiment of the present invention. Fig. 5 is a cross-sectional view taken along the arrow VV shown in Fig. 4. Fig. 6 is a side view of the die shown in Fig. 4, seen from the discharge port side. In Figs. 4 to 6, the die 20 has a housing 23 consisting of a first block 21 and a second block 22, a supply port 24 formed in the first block 21 and communicating with the extrusion port 13 of the extruder 10, a manifold 25 formed between the first block 21 and the second block 22, in which the reconstituted tobacco raw material is stored, and a discharge port 26 communicating with the manifold 25.
[0020] The discharge port 26 is formed in a slit shape on one side surface of the housing 23. The direction perpendicular to the longitudinal direction of the discharge port 26 is defined as the width direction of the discharge port 26. The longitudinal length of the discharge port 26 is referred to as the opening length, and the width direction length of the discharge port 26 is referred to as the opening width. The discharge port 26 may be hole-shaped or groove-shaped. Due to the slit-shaped discharge port 26, the reconstituted tobacco raw material is adjusted to a uniform thickness according to the opening width of the discharge port 26 when discharged from the die 20, regardless of the moisture content contained in the reconstituted tobacco raw material, and is formed into a sheet shape and extruded.
[0021] The reconstituted tobacco raw material supplied from the extruder 10 to the die 20 via the supply port 24 is sent through the manifold 25 to the discharge port 26, and is discharged from the discharge port 26 onto the drum body 32 as a reconstituted tobacco sheet 1.
[0022] Returning to Fig. 1, the drum dryer 30 has a shaft 31 and a drum body 32 that rotates around the shaft 31. The drum body 32 dries the reconstituted tobacco sheet 1, for example, by steam that is fed into the drum body 32. The drum body 32 may be heated by a heater or the like.
[0023] The scraper 40 is disposed opposite the drum body 32 over the entire width of the drum body 32 perpendicular to the rotation direction of the drum body 32, and is adjusted so that its tip abuts or is close to the drum body 32. The scraper 40 is disposed near the end on the downstream side in the rotation direction of the drum body 32 so that the reconstituted tobacco sheet 1 discharged on the upstream side in the rotation direction of the drum body 32 is sufficiently dried.
[0024] The reconstituted tobacco sheet 1 discharged from the discharge port 26 of the die 20 onto the drum body 32 is dried by the drum body 32 into which steam is pumped, and the dried reconstituted tobacco sheet 1 is peeled off by a scraper 40 and delivered to a subsequent process. The subsequent process is, for example, a process in which the reconstituted tobacco sheet 1 is cut to a desired width, or a process in which the cut reconstituted tobacco sheet is wound onto a bobbin.
[0025] That is, the reconstituted tobacco sheet 1 is manufactured by a manufacturing method including the steps of supplying the reconstituted tobacco raw material to the supply port 24 of the die 20, forming the reconstituted tobacco raw material into a sheet-like form and discharging it from the discharge port 26 of the die 20, and cutting the sheet-like reconstituted tobacco raw material discharged from the die 20.
[0026] As described above, according to the first embodiment, the reconstituted tobacco sheet manufacturing device includes a die that discharges reconstituted tobacco raw material, and a main drum that dries and conveys the reconstituted tobacco raw material discharged from the die, and the die has a housing, a supply port formed in the housing through which the reconstituted tobacco raw material is supplied, and a discharge port formed on one side of the housing through which the reconstituted tobacco raw material is discharged. Therefore, a reconstituted tobacco sheet of uniform thickness can be obtained through a simple manufacturing process, regardless of the moisture content of the reconstituted tobacco raw material.
[0027] Second embodiment: Fig. 7 is a side view showing a reconstituted tobacco sheet manufacturing apparatus according to a second embodiment of the present invention. In Fig. 7, the reconstituted tobacco sheet manufacturing apparatus 100L includes a slitting drum 53 instead of the roller 52 shown in Fig. 1. The other configurations are the same as those of the first embodiment described above, and therefore will not be described.
[0028] The slitting drum 53 has at least two blades that rotate opposite to each other. The length of the blades in the direction of the rotation axis is configured to be longer than the length in the width direction of the reconstituted tobacco sheet 1. The slitting drum 53 cuts the reconstituted tobacco sheet 1 when the reconstituted tobacco sheet 1, which has been dried by the drum dryer 30 and peeled off by the scraper 40, passes between the blades.
[0029] Here, the slitting drum 53 can adopt various cutting methods such as straight cut, cross cut, and spiral cut by selecting the shape of the blade. That is, the reconstituted tobacco sheet 1 cut by the slitting drum 53 can be collected as it is as a strand or tobacco shreds. In conventional cigarettes, tobacco shreds having a width of about 1 mm and a length of about 5 mm to 20 mm are often randomly oriented and filled into a cylindrical paper tube. By selecting the shape of the blade of the slitting drum 53 in the second embodiment, it is also possible to produce tobacco shreds of a similar size to those often used in conventional cigarettes. Examples of such tobacco shred shapes include those disclosed in, for example, Figures 1, 3, 6 to 8 of JP2018-516075. In addition, if it is necessary to prepare strands of various sizes and shapes for the purpose of changing the filling rate or other quality changes, this can be done by appropriately selecting the blade of the slitting drum 53.
[0030] As described above, according to the second embodiment, a slitting drum is provided to cut the sheet-shaped reconstituted tobacco raw material discharged from the die, and therefore, a cut reconstituted tobacco sheet having a uniform thickness can be obtained through a simple manufacturing process, regardless of the moisture content of the reconstituted tobacco raw material.
[0031] Moreover, according to the second embodiment, a main drum is further provided, which is disposed before the slitting drum and dries and conveys the reconstituted tobacco raw material discharged from the die. Therefore, the reconstituted tobacco sheet can be cut immediately after drying. In addition, by disposing the slitting drum after the main drum that dries the raw material, it is possible to prevent tar from adhering to the slitting drum. Note that the slitting drum 53 may be used after the drum dryer 30 in each of the following embodiments.
[0032] Also, a packaging device may be provided downstream of the slitting drum 53. The packaging device has a weighing mechanism that measures the weight of the container in which the reconstituted tobacco sheet 1 cut by the slitting drum 53 is packed, and a conveying mechanism that carries the container into the weighing mechanism and carries the container out of the weighing mechanism. Here, the container may be a cardboard case of a predetermined size (for example, a C-48 case that is often used in the tobacco industry for packaging tobacco plants) or a plastic bag. When the weight of the container measured by the weighing mechanism reaches a predetermined weight, the conveying mechanism carries the container out of the weighing mechanism and carries the empty container into the weighing mechanism. This allows the reconstituted tobacco sheet 1 cut by the slitting drum 53 to be efficiently packed and handed over to a downstream process. Note that the reconstituted tobacco sheet 1 cut by the slitting drum 53 may be randomly packed in the container, or may be aligned and packed in the container.
[0033] Third embodiment: Fig. 8 is a plan view showing a reconstituted tobacco sheet manufacturing apparatus according to a third embodiment of the present invention. In Fig. 8, the reconstituted tobacco sheet manufacturing apparatus 100A includes X extruders 10A-10X and X dies 20A-20X, instead of the extruder 10 and die 20 shown in Fig. 1. X may be 2 or more. Furthermore, X dies 20A-20X may be connected to one extruder 10. The rest of the configuration is the same as in the first embodiment described above, and therefore description thereof will be omitted.
[0034] The extruders 10A-10X are connected to the dies 20A-20X, respectively. The dies 20A-20X are arranged along the longitudinal direction of the discharge port 26. The extruders 10A-10X pump the reconstituted tobacco raw material supplied from a tank or the like (not shown) to the dies 20A-20X, respectively. The dies 20A-20X discharge the reconstituted tobacco raw material supplied from the extruders 10A-10X onto the drum main body 32, respectively.
[0035] Here, by adjusting the opening length of the discharge openings 26 of the dies 20A-20X to the width of the bobbin on which the reconstituted tobacco sheet 1 is wound in the latter process described above, the process of cutting the reconstituted tobacco sheet 1 to a desired width in the latter process described above becomes unnecessary. In addition, by making the opening widths of the dies 20A-20X different from one another, it is possible to produce reconstituted tobacco sheets 1 of a plurality of thicknesses with a single drum dryer 30.
[0036] Moreover, by making the compositions of the reconstituted tobacco raw materials supplied to each of the extruders 10A-10X different from one another, it is possible to produce a plurality of types of reconstituted tobacco sheets 1 with a single drum dryer 30. Furthermore, by selectively driving sets of the extruders 10A-10X and dies 20A-20X, the production capacity of the reconstituted tobacco sheet production apparatus 100A can be easily adjusted.
[0037] As described above, according to the third embodiment, a plurality of dies are arranged along the longitudinal direction of the discharge port, which makes it possible to omit the step of cutting the obtained reconstituted tobacco sheet to a desired width.
[0038] Fourth embodiment: In the above-mentioned first embodiment, the opening width of the discharge port 26 of the die 20 was fixed, but in the manufacturing apparatus for a reconstituted tobacco sheet according to the fourth embodiment of the present invention, the die 20 has a variable width mechanism (not shown) that can change the opening width of the discharge port 26. The other configurations are the same as those of the above-mentioned first embodiment, so the explanation will be omitted.
[0039] The variable width mechanism is, for example, a screw. The variable width mechanism changes the opening width of the discharge port 26 by adjusting the gap between the first block 21 and the second block 22 shown in FIG. 6 according to the amount of tightening of the screw. Note that a plurality of screws may be provided, and the opening width of the discharge port 26 may be different between the end and center of the longitudinal direction of the discharge port 26. If the opening length of the discharge port 26 is large compared to the opening width of the discharge port 26, the discharge state will differ in the longitudinal direction of the discharge port 26. As described above, it is preferable to have a plurality of variable width mechanisms in the longitudinal direction of the discharge port 26 in order to adjust the state of the reconstituted tobacco sheet 1 in the width direction. The variable width mechanism may also have an actuator such as a motor that drives the screw. By using the variable width mechanism, the thickness of the reconstituted tobacco sheet 1 can be easily changed.
[0040] As described above, according to the fourth embodiment, the die has a variable width mechanism that can change the width direction length of the discharge port. Therefore, reconstituted tobacco sheets of a variety of thicknesses can be obtained without replacing the die. In addition, by changing the opening width of the discharge port so that the flow rate of the reconstituted tobacco raw material at the discharge port of the die is uniform in the longitudinal direction of the discharge port, the occurrence of wrinkles can be suppressed and the reconstituted tobacco sheet can be formed flat.
[0041] Fifth embodiment: Fig. 9 is a side view showing a reconstituted tobacco sheet manufacturing apparatus according to a fifth embodiment of the present invention. In Fig. 9, a reconstituted tobacco sheet manufacturing apparatus 100B includes three extruders 61-63 and a die 70, instead of the extruder 10 and die 20 shown in Fig. 1. The number of extruders is not limited to three, and may be two or more. Other configurations are the same as those of the first embodiment described above, and therefore description thereof will be omitted.
[0042] The extruders 61-63 are connected to the die 70. Raw materials are supplied to the extruders 61-63 from a tank or the like (not shown). At least one of the raw materials supplied to the extruders 61-63 contains reconstituted tobacco raw materials. The raw materials supplied to the extruders 61-63 may contain different raw materials or the same raw material. The extruders 61-63 pressure-feed the supplied raw materials to the die 70 using a screw or the like (not shown).
[0043] The die 70 has a plurality of supply ports 71-73 through which a plurality of raw materials are respectively supplied from the extruders 61-63, and a discharge port 74 formed in a slit shape on one side of the die 70. The die 70 spreads the raw materials supplied from the extruders 61-63 via the supply ports 71-73 in a manifold (not shown), and then causes the raw materials to join in the vicinity of the discharge port 74, and discharges the layered reconstituted tobacco sheet 1 onto the drum body 32. Note that the die 70 may cause a plurality of raw materials to join in a manifold.
[0044] Here, multiple raw materials are stacked and discharged from the discharge port 74 of the die 70, so that sheets with different properties can be multi-layered without being bonded together. Therefore, the sheet bonding process can be omitted, and a multi-layered reconstituted tobacco sheet 1 can be obtained with a simple configuration. Also, by multi-layering the sheets before drying the reconstituted tobacco sheet 1 with the drum dryer 30, the adhesion of each layer can be strengthened. Furthermore, by inserting a sheet with reduced stickiness into the multi-layered sheet, the reconstituted tobacco sheet 1 can be easily wound onto and unwound from a bobbin without the need for measures such as dusting powder or release paper.
[0045] As described above, according to the fifth embodiment, the die has a plurality of supply ports through which a plurality of raw materials are respectively supplied, and the raw materials are discharged in a stacked manner from the discharge port, so that the process of bonding a plurality of sheets can be omitted.
[0046] Sixth embodiment: Fig. 10 is a side view of the die of the reconstituted tobacco sheet manufacturing apparatus according to the sixth embodiment of the present invention, as viewed from the discharge port side. In Fig. 10, the die 20 further has a partition portion 27 that divides the discharge port 26 into a plurality of regions along the longitudinal direction of the discharge port 26. That is, in Fig. 10, the slit-shaped discharge port 26 shown in Fig. 6 opens intermittently. Other configurations are the same as those of the first embodiment described above, and therefore description thereof will be omitted.
[0047] The reconstituted tobacco raw material supplied from the extruder 10 to the die 20 via the supply port 24 is sent through the manifold 25 to the discharge port 26, and is discharged from the discharge port 26 onto the drum body 32 as a reconstituted tobacco sheet 1. At this time, because the discharge port 26 is open intermittently, the discharged reconstituted tobacco sheet 1 has already been formed into a strip. Therefore, the reconstituted tobacco sheet 1 dried in the drum dryer 30 can be collected as a strand as is after drying is completed.
[0048] As described above, according to the sixth embodiment, the die has a partition portion that divides the outlet into a plurality of regions along the longitudinal direction of the outlet. Therefore, the process of strand processing the sheet can be omitted. In addition, in the present invention, since the shape of the extruded reconstituted tobacco sheet is stable even before drying, it is effective to use a die 20 having a partition portion 27.
[0049] Seventh embodiment: Fig. 11 is a side view of the die of the reconstituted tobacco sheet manufacturing apparatus according to the seventh embodiment of the present invention, as viewed from the discharge port side. In Fig. 11, the die 20 further has at least one raised portion 28 that faces the width direction of the discharge port 26 along the longitudinal direction of the discharge port 26. Here, the cross-sectional shape of the raised portion 28 may be a triangle, a rectangle, a sine wave, a T-shape, or the like. That is, in Fig. 11, the slit-shaped discharge port 26 shown in Fig. 6 becomes an opening having two widths, the apex or a side including the apex of the raised portion 28 and the base side of the raised portion 28. The other configurations are the same as those of the first embodiment described above, and therefore description thereof will be omitted.
[0050] The reconstituted tobacco raw material supplied from the extruder 10 to the die 20 via the supply port 24 is sent through the manifold 25 to the discharge port 26, and is discharged from the discharge port 26 onto the drum body 32 as a reconstituted tobacco sheet 1. At this time, because the discharge port 26 is provided with the raised portions 28, the discharged reconstituted tobacco sheet 1 already has stripes formed with a cross-sectional shape corresponding to the raised portions 28. Therefore, the reconstituted tobacco sheet 1 dried in the drum dryer 30 can be collected as the reconstituted tobacco sheet 1 with stripes formed thereon after drying is completed.
[0051] As described above, according to the seventh embodiment, the die has at least one raised portion that faces the width direction of the discharge port along the longitudinal direction of the discharge port. Therefore, it is possible to perform surface processing (e.g., embossing) to increase the surface area per weight of the reconstituted tobacco sheet, while omitting the process of passing the reconstituted tobacco sheet between a pair of rollers and pressing it into a zigzag or wavy shape, as was done with conventional reconstituted tobacco sheets. Furthermore, in the present invention, since the shape of the discharged reconstituted tobacco sheet is stable even before drying, it is effective to use a die 20 having a raised portion 28.
[0052] 12, when the raised portion 28 is T-shaped, the ridges formed on the reconstituted tobacco sheet 1 will spread within the reconstituted tobacco sheet 1. This type of surface shape is not obtained by pressing the reconstituted tobacco sheet 1 with a roller, but can only be obtained by using the die 20 shown in the seventh embodiment.
[0053] Eighth embodiment: Fig. 13 is a side view showing a reconstituted tobacco sheet manufacturing apparatus according to an eighth embodiment of the present invention. In Fig. 13, the reconstituted tobacco sheet manufacturing apparatus 100C includes a drum dryer (sub-drum) 35 and a scraper 45 in addition to the reconstituted tobacco sheet manufacturing apparatus 100 shown in Fig. 1. The other configurations are the same as those of the first embodiment described above, and therefore will not be described.
[0054] Drum dryer 35 is disposed after drum dryer 30 and is used in combination with drum dryer 30. Drum dryer 35 has a shaft 36 and a drum body 37 that rotates about shaft 36. Drum body 37 is heated, for example, by steam fed into the inside of drum body 37. Drum body 37 may also be heated by a heater or the like. Drum dryer 30 and drum dryer 35 are configured so that their temperatures can be adjusted independently of each other.
[0055] The drum dryer 35 receives the reconstituted tobacco sheet 1 that has been dried by the drum dryer 30 and peeled off by the scraper 40, and further dries and transports the reconstituted tobacco sheet 1. The scraper 45 peels off the reconstituted tobacco sheet 1 that has been dried by the drum dryer 35 from the drum body 37.
[0056] Here, by using the drum dryer 30 and the drum dryer 35, the drying distance of the reconstituted tobacco sheet 1 can be extended, improving the drying capacity of the reconstituted tobacco sheet manufacturing apparatus 100C. As a result, it can also handle reconstituted tobacco raw material with a high moisture content.
[0057] In addition, when comparing the use of two drum dryers with the same drum diameter with the use of one drum dryer for the same drying distance, the use of two drum dryers allows each drum diameter to be half that of one drum dryer. In other words, the total volume of the two drum dryers can be half that of one drum dryer. Therefore, when two drum dryers are used, the required heat energy can be half that of the use of one drum dryer.
[0058] As described above, according to the eighth embodiment, the sub-drum used in combination with the main drum is further provided, and is disposed after the main drum, and receives the reconstituted tobacco raw material transported by the main drum and transports it further. Therefore, the reconstituted tobacco raw material dried and transported by the main drum can be further processed while extending the transport distance of the reconstituted tobacco raw material. Note that, although the sub-drum is a drum dryer in the eighth embodiment, this is not limiting, and the sub-drum may be a cooling drum that cools the reconstituted tobacco sheet 1 dried by the drum dryer 30.
[0059] Ninth embodiment: Fig. 14 is a side view showing a reconstituted tobacco sheet manufacturing apparatus according to a ninth embodiment of the present invention. In Fig. 14, the reconstituted tobacco sheet manufacturing apparatus 100D includes a drum dryer (sub-drum) 35 in addition to the reconstituted tobacco sheet manufacturing apparatus 100 shown in Fig. 1. The other configurations are the same as those of the first embodiment described above, and therefore will not be described.
[0060] Drum dryer 35 is disposed opposite drum dryer 30 and is used in combination with drum dryer 30. Drum dryer 35 has a shaft 36 and a drum body 37 that rotates about shaft 36. Shaft 36 is configured so that the gap between drum dryer 30 and drum dryer 35 can be arbitrarily adjusted by a drive mechanism (not shown).
[0061] Drum body 37 is heated, for example, by steam fed into drum body 37. Drum body 37 may also be heated by a heater or the like. Drum dryer 30 and drum dryer 35 are configured so that their temperatures can be adjusted independently of each other.
[0062] The drum dryer 35 dries and transports the reconstituted tobacco sheet 1 formed on the drum body 32 in cooperation with the drum dryer 30. The reconstituted tobacco sheet 1 transported by the drum dryer 30 and the drum dryer 35 is compressed when passing through the gap between the drum dryer 30 and the drum dryer 35.
[0063] Here, by compressing the reconstituted tobacco sheet 1 with the drum dryers 30 and 35, the consolidation effect of the drum dryers 30 and 35 can increase the density of the reconstituted tobacco sheet 1 compared to when it was extruded from the die 20. In addition, by adjusting the gap between the drum dryers 30 and 35, the thickness of the reconstituted tobacco sheet 1 that has passed through the gap between the drum dryers 30 and 35 can be controlled.
[0064] Furthermore, by passing the reconstituted tobacco sheet 1 through the gap between the drum dryers 30 and 35, the compaction effect of the drum dryers 30 and 35 can eliminate wrinkles and the like that occur in the reconstituted tobacco sheet 1 due to the distribution of the extrusion speed when it is extruded from the die 20. Furthermore, by embossing the surface of the drum body 37, the surface of the reconstituted tobacco sheet 1 can be embossed when it passes through the gap between the drum dryers 30 and 35, and the specific surface area can be increased. Note that the processing performed on the surface of the drum body 37 is not limited to embossing, and may be slit processing for cutting the reconstituted tobacco sheet 1, or the like.
[0065] As described above, according to the ninth embodiment, the secondary drum is further provided in combination with the primary drum, and is disposed opposite the primary drum to transport the reconstituted tobacco material discharged from the die in cooperation with the primary drum. Therefore, in cooperation with the primary drum, the secondary drum can perform further processing on the reconstituted tobacco material dried and transported by the primary drum.
[0066] Tenth embodiment: Fig. 15 is a side view showing a reconstituted tobacco sheet manufacturing apparatus according to a tenth embodiment of the present invention. In Fig. 15, the reconstituted tobacco sheet manufacturing apparatus 100E includes an extruder 10 and a die 20 provided in a drum dryer 35, in addition to the reconstituted tobacco sheet manufacturing apparatus 100D shown in Fig. 14. The other configurations are the same as those of the above-mentioned ninth embodiment, and therefore will not be described.
[0067] The extruder 10 provided in the drum dryer 35 is supplied with raw material supplied from a tank or the like (not shown). The raw material supplied to the extruder 10 may or may not contain reconstituted tobacco raw material. The extruder 10 pressure-feeds the supplied raw material to the die 20 using a screw or the like (not shown). The die 20 provided in the drum dryer 35 forms the raw material supplied from the extruder 10 into a sheet and discharges it onto the drum body 37. The sheets discharged from the die 20 provided in the drum dryer 30 and the die 20 provided in the drum dryer 35 are multi-layered when passing through the gap between the drum dryer 30 and the drum dryer 35.
[0068] Here, by passing the sheets discharged from the dies 20 provided on the drum dryers 30 and 35, respectively, through the gap between the drum dryers 30 and 35, it is possible to form a multi-layered sheet without laminating sheets having different properties. Therefore, it is possible to obtain a multi-layered reconstituted tobacco sheet 1 with a simple configuration by omitting the lamination process of the sheets. In addition, by forming the sheets into a multi-layered sheet before drying the reconstituted tobacco sheet 1 with the drum dryers 30 and 35, it is possible to strengthen the adhesion of each layer. Furthermore, by adjusting the gap between the drum dryers 30 and 35, it is possible to control the thickness of the reconstituted tobacco sheet 1 that has passed through the gap between the drum dryers 30 and 35.
[0069] As described above, according to the tenth embodiment, the sub-drum used in combination with the main drum and the die having the same configuration as the die provided on the main drum and discharging the discharge material onto the sub-drum are further provided, so that the process of laminating multiple sheets can be omitted.
[0070] Eleventh embodiment: In the reconstituted tobacco sheet manufacturing apparatus according to the eleventh embodiment of the present invention, the surfaces of the drum body 32 of the drum dryer 30 and the drum body 37 of the drum dryer 35 shown in the first embodiment and the like are subjected to a surface modification treatment in order to improve their characteristics.
[0071] Here, the improvement of characteristics refers to the improvement of abrasion resistance, corrosion resistance, peeling / releasability, and thermal conductivity, and the surface modification treatment includes chemical treatment such as plating and physical treatment such as blasting. Specific examples of characteristics and surface modification treatments are shown in Tables 1 to 6. As a result, the surface characteristics of drum body 32 of drum dryer 30 and drum body 37 of drum dryer 35 are improved, and the usability and durability of the device can be improved.
[0072] [Table 1]
[0073] [Table 2]
[0074] [Table 3]
[0075] [Table 4]
[0076] [Table 5]
[0077] [Table 6]
[0078] Those skilled in the art can select and apply a surface treatment appropriate for the purpose from the surface modification treatments listed in Tables 1 to 6. In Tables 1 to 6, ◎ indicates that the surface treatment can be applied regardless of the conditions of the extrusion material or the device. In Tables 1 to 6, ○ indicates that the surface treatment can be applied if either the conditions of the extrusion material or the device are met. In Tables 1 to 6, △ indicates that the surface treatment can be applied if both the conditions of the extrusion material and the device are met. In Tables 1 to 6, * indicates that the surface treatment can be applied if the conditions of the extrusion material (temperature and viscosity) and the conditions of the device (temperature of the drum surface and the movement speed of the drum surface) are met. In Table 3, insulation indicates that electrolytic corrosion is unlikely to occur on the surface due to insulation.
[0079] As described above, according to the eleventh embodiment, the main drum is subjected to a surface modification treatment. Therefore, the surface characteristics of the main drum can be improved. Note that the surface modification treatment is not limited to the main drum, and the sub-drum may also be subjected to the surface modification treatment.
[0080] Twelfth embodiment: Fig. 16 is a side view showing a reconstituted tobacco sheet manufacturing apparatus according to a twelfth embodiment of the present invention. In Fig. 16, the reconstituted tobacco sheet manufacturing apparatus 100F includes a hot air blower (auxiliary drying device) 80 in addition to the reconstituted tobacco sheet manufacturing apparatus 100 shown in Fig. 1. The other configurations are the same as those of the first embodiment described above, and therefore will not be described.
[0081] The hot air blower 80 is disposed on the drying path of the drum dryer 30, facing the drum body 32 of the drum dryer 30. The hot air blower 80 blows hot air to dry the reconstituted tobacco sheet 1 discharged onto the drum body 32 from the discharge port 26 of the die 20, from the front side of the reconstituted tobacco sheet 1. Here, the front side of the reconstituted tobacco sheet 1 refers to the side of the reconstituted tobacco sheet 1 that is not in contact with the drum body 32. The hot air blower 80 is configured to be able to adjust the drying capacity by its own parameters, such as the air volume, output, and hot air temperature. The hot air temperature can be set to a temperature equal to or higher than room temperature.
[0082] Here, by using the hot air blower 80, the drying capacity of the reconstituted tobacco sheet manufacturing apparatus 100F can be improved. Therefore, with a simple configuration, it is possible to handle reconstituted tobacco raw materials with a high moisture content. In addition, by using the hot air blower 80, both sides of the reconstituted tobacco sheet 1 can be dried simultaneously.
[0083] As described above, according to the twelfth embodiment, an auxiliary drying device is further provided that is disposed opposite the main drum and dries the reconstituted tobacco raw material discharged from the die. This improves the drying capacity of the reconstituted tobacco sheet manufacturing apparatus. In the twelfth embodiment, the auxiliary drying device is a hot air blower, but is not limited thereto, and the auxiliary drying device may be an IR heater. Moreover, instead of the auxiliary drying device, a cooling device that blows cold air to the reconstituted tobacco sheet 1 may be provided.
[0084] Thirteenth embodiment: Fig. 17 is a side view showing a reconstituted tobacco sheet manufacturing apparatus according to a thirteenth embodiment of the present invention. Fig. 18 is a block diagram showing opening width control in the reconstituted tobacco sheet manufacturing apparatus according to the thirteenth embodiment of the present invention. In Figs. 17 and 18, the reconstituted tobacco sheet manufacturing apparatus 100G includes a thickness detection sensor (state detection unit) 91 and a PLC (control unit) 200 in addition to the reconstituted tobacco sheet manufacturing apparatus 100 shown in Fig. 1. Furthermore, the die 20 of the reconstituted tobacco sheet manufacturing apparatus 100G has a variable width mechanism 92 that can change the opening width of the discharge port 26 using a motor as an actuator, as shown in the fourth embodiment above. Other configurations are similar to those of the first embodiment above, and therefore will not be described.
[0085] The thickness detection sensor 91 is provided near the discharge port 26. The thickness detection sensor 91 detects the thickness of the reconstituted tobacco sheet 1 discharged from the die 20 in a non-contact manner using X-rays, laser, ultrasonic waves, or the like, and outputs the thickness measurement value to a PLC (programmable logic controller) 200.
[0086] The PLC 200 may be built into the reconstituted tobacco sheet manufacturing apparatus 100G, or may be provided separately. The PLC 200 outputs a control command to the variable width mechanism 92 and controls the motor based on a thickness set value, which is the desired thickness of the reconstituted tobacco sheet 1, and a thickness measurement value from the thickness detection sensor 91, so that the difference between the thickness set value and the thickness measurement value becomes zero. This changes the opening width of the discharge port 26, and the thickness of the reconstituted tobacco sheet 1 discharged from the die 20 changes.
[0087] When the reconstituted tobacco sheet 1 is discharged from the die 20, the sheet expands due to pressure release, and the thickness of the reconstituted tobacco sheet 1 may not match the opening width of the discharge orifice 26. Thus, by feedback-controlling the opening width of the discharge orifice 26 in response to the uncontrollable factor of pressure release, the thickness of the reconstituted tobacco sheet 1 can be adjusted to the desired thickness.
[0088] As described above, according to the thirteenth embodiment, the die has a variable width mechanism as an actuator capable of changing the width direction length of the discharge port, the state detection unit detects the thickness of the reconstituted tobacco raw material discharged from the die, and the control unit controls the variable width mechanism based on the detection result by the state detection unit to change the width direction length of the discharge port, thereby making it possible to adjust the thickness of the reconstituted tobacco sheet to a desired thickness.
[0089] Fourteenth embodiment: Fig. 19 is a side view showing a reconstituted tobacco sheet manufacturing apparatus according to a fourteenth embodiment of the present invention. Fig. 20 is a block diagram showing discharge speed control in the reconstituted tobacco sheet manufacturing apparatus according to the fourteenth embodiment of the present invention. In Figs. 19 and 20, the reconstituted tobacco sheet manufacturing apparatus 100H includes a flow sensor (state detection unit) 93 and a PLC (control unit) 200 in addition to the reconstituted tobacco sheet manufacturing apparatus 100 shown in Fig. 1. In the reconstituted tobacco sheet manufacturing apparatus 100H, the screw 14 rotatably disposed in the housing 11 of the extruder 10 also functions as an actuator. The other configurations are the same as those of the first embodiment described above, and therefore will not be described.
[0090] The flow rate sensor 93 is provided near the discharge port 26. The flow rate sensor 93 detects the flow rate of the reconstituted tobacco sheet 1 discharged from the die 20 in a non-contact manner using a laser or the like, and outputs the flow rate measurement value to the PLC 200. Here, the flow rate measurement value is used as a value for estimating the discharge speed of the reconstituted tobacco sheet 1 discharged from the die 20.
[0091] The PLC 200 may be built into the reconstituted tobacco sheet manufacturing apparatus 100H, or may be provided separately. Based on a flow rate set value, which is a desired flow rate of the reconstituted tobacco sheet 1, and a flow rate measured value from the flow rate sensor 93, the PLC 200 outputs a control command to the screw 14 and controls the rotation of the screw 14 so that the difference between the flow rate set value and the flow rate measured value becomes zero. This changes the discharge speed of the reconstituted tobacco sheet 1 discharged from the die 20.
[0092] The discharge speed of the reconstituted tobacco sheet 1 discharged from the die 20 varies to a certain extent due to undulation of the screw 14. Therefore, by feedback controlling the discharge speed of the reconstituted tobacco sheet 1, the discharge speed of the reconstituted tobacco sheet 1 discharged from the die 20 can be maintained within a constant range. Furthermore, by keeping the discharge speed of the reconstituted tobacco sheet 1 constant, it is possible to prevent the reconstituted tobacco sheet 1 from dangling on the drum dryer 30 or from being torn off due to increased tension. Furthermore, by keeping the discharge speed of the reconstituted tobacco sheet 1 constant, it is possible to prevent variation in sheet thickness caused by pressure release, and stabilize the quality of the reconstituted tobacco sheet 1.
[0093] As described above, according to the fourteenth embodiment, the apparatus further includes an extruder that pressure-feeds the reconstituted tobacco raw material to the die, the extruder has a screw rotatably arranged in the housing as an actuator, the state detection unit detects at least one of the flow rate and discharge pressure of the reconstituted tobacco raw material discharged from the die, and the control unit controls the rotation of the screw based on the detection result by the state detection unit to change the discharge speed of the reconstituted tobacco raw material discharged from the die. Therefore, the discharge speed of the reconstituted tobacco sheet discharged from the die can be kept constant.
[0094] In the fourteenth embodiment, instead of or in addition to the flow rate sensor 93, a discharge pressure sensor that detects the discharge pressure of the reconstituted tobacco sheet 1 discharged from the die 20 may be provided near the discharge port 26 or inside the die 20. In this case, the discharge pressure detected by the discharge pressure sensor can be used as a value for estimating the discharge speed of the reconstituted tobacco sheet 1 discharged from the die 20.
[0095] Fifteenth embodiment: Fig. 21 is a side view showing a reconstituted tobacco sheet manufacturing apparatus according to a fifteenth embodiment of the present invention. Fig. 22 is a block diagram showing hot air temperature control in the reconstituted tobacco sheet manufacturing apparatus according to the fifteenth embodiment of the present invention. In Figs. 21 and 22, the reconstituted tobacco sheet manufacturing apparatus 100I includes a moisture sensor (state detection unit) 94 and a PLC (control unit) 200 in addition to the reconstituted tobacco sheet manufacturing apparatus 100 shown in Fig. 1. The reconstituted tobacco sheet manufacturing apparatus 100I also includes the hot air blower (auxiliary drying device) 80 shown in the twelfth embodiment described above as an actuator. Other configurations are similar to those of the first embodiment described above, and therefore description thereof will be omitted.
[0096] The moisture sensor 94 is provided after the scraper 40. The moisture sensor 94 detects the moisture content of the reconstituted tobacco sheet 1 peeled off by the scraper 40 in a non-contact manner using infrared rays, microwaves, or the like, and outputs the moisture content as a moisture content measurement value to the PLC 200. The hot air blower 80 is disposed on the drying path of the drum dryer 30, facing the drum body 32 of the drum dryer 30.
[0097] The PLC 200 may be built into the reconstituted tobacco sheet manufacturing apparatus 100I, or may be provided separately. Based on a moisture content set value, which is the desired moisture content of the reconstituted tobacco sheet 1, and a moisture content measured value from the moisture content sensor 94, the PLC 200 outputs a control command to the hot air blower 80 and controls the temperature of the hot air sent from the hot air blower 80 so that the difference between the moisture content set value and the moisture content measured value becomes zero. This changes the moisture content of the reconstituted tobacco sheet 1 dried by the drum dryer 30 and the hot air blower 80.
[0098] The moisture content of the reconstituted tobacco sheet 1 dried by the drum dryer 30 and the hot air blower 80 varies depending on the environment, season, and the like. Therefore, by feedback-controlling the moisture content of the reconstituted tobacco sheet 1, the moisture content of the reconstituted tobacco sheet 1 dried by the drum dryer 30 and the hot air blower 80 can be kept within a constant range. As a result, the quality of the reconstituted tobacco sheet 1 can be stabilized. Furthermore, since the hot air blower 80 is more responsive and easier to control than the drum dryer 30, the moisture content of the reconstituted tobacco sheet 1 can be controlled in detail. Furthermore, since the moisture content of the reconstituted tobacco sheet 1 can be automatically controlled, constant monitoring by an operator is not required.
[0099] As described above, according to the fifteenth embodiment, the apparatus further includes a drum that dries and transports the reconstituted tobacco raw material discharged from the die, and an auxiliary drying device that is disposed opposite the drum and dries the reconstituted tobacco raw material discharged from the die, the state detection unit detects the moisture content of the reconstituted tobacco raw material dried by the drum and the auxiliary drying device, and the control unit controls the auxiliary drying device based on the detection result by the state detection unit to change the moisture content of the reconstituted tobacco raw material dried by the drum and the auxiliary drying device. Therefore, the moisture content of the reconstituted tobacco sheet dried by the drum and the auxiliary drying device can be maintained within a certain range.
[0100] The reconstituted tobacco sheet manufacturing apparatus 100G according to the 13th embodiment, the reconstituted tobacco sheet manufacturing apparatus 100H according to the 14th embodiment, and the reconstituted tobacco sheet manufacturing apparatus 100I according to the 15th embodiment may be combined in any combination.
[0101] Sixteenth embodiment: Fig. 23 is a side view showing a reconstituted tobacco sheet manufacturing apparatus according to a sixteenth embodiment of the present invention. In Fig. 23, the reconstituted tobacco sheet manufacturing apparatus 100J includes an addition mechanism 95 in addition to the reconstituted tobacco sheet manufacturing apparatus 100 shown in Fig. 1. The other configurations are the same as those of the first embodiment described above, and therefore will not be described.
[0102] The adding mechanism 95 is provided near the discharge port 26, and adds, by spraying, a powdered or liquid flavor to the reconstituted tobacco sheet 1 discharged from the die 20. The installation position of the adding mechanism is not limited to the vicinity of the discharge port 26, and the adding mechanism may be provided on the drying path of the drum dryer 30.
[0103] The reconstituted tobacco sheet 1 produced according to the present invention has a smooth surface due to the pressure load in the die 20 and shrinkage during drying in the drum dryer 30, and therefore has low liquid permeability. Therefore, the fixation of the additives can be improved by adding a flavoring before or during drying of the reconstituted tobacco sheet 1. Furthermore, by providing an adding mechanism 95 in the reconstituted tobacco sheet manufacturing apparatus 100J, a step of adding a flavoring in a later process is not required.
[0104] As described above, according to the sixteenth embodiment, by further providing an addition mechanism for adding a powdered or liquid flavoring downstream of the die 20, the fixation of the additive can be improved.
[0105] Seventeenth embodiment: Fig. 24 is a side view showing a reconstituted tobacco sheet manufacturing apparatus according to a seventeenth embodiment of the present invention. In Fig. 24, a reconstituted tobacco sheet manufacturing apparatus 100K includes a buffer mechanism 55 in addition to the reconstituted tobacco sheet manufacturing apparatus 100 shown in Fig. 1. The other configurations are the same as those of the first embodiment described above, and therefore will not be described.
[0106] The buffer mechanism 55 is provided between the discharge port 26 and the drum dryer 30, and winds up and temporarily holds the reconstituted tobacco sheet 1 discharged from the die 20. Here, the buffer mechanism 55 is suitable for reconstituted tobacco raw material containing a low amount of moisture. Because the reconstituted tobacco sheet 1 before being dried by the drum dryer 30 has low strength, a suitable structure for the buffer mechanism 55 is one having, for example, a fixed roller 56 and a movable roller 57 that can move according to the tension of the reconstituted tobacco sheet 1. The buffer mechanism 55 moves the movable roller 57 so that the tension of the reconstituted tobacco sheet 1 is constant.
[0107] By providing the buffer mechanism 55, it is possible to cope with a case where the discharge speed of the reconstituted tobacco sheet 1 discharged from the die 20 and the rotation speed of the drum main body 32 cannot be synchronized due to a fluctuation in the discharge amount from the die 20, etc. Specifically, the discharge speed of the reconstituted tobacco sheet 1 and the rotation speed of the drum main body 32 can be relatively synchronized by unwinding the reconstituted tobacco sheet 1 held in the buffer mechanism 55 or temporarily holding the reconstituted tobacco sheet 1 in the buffer mechanism 55. Furthermore, even if a device upstream or downstream of the buffer mechanism 55 stops momentarily, the use of the buffer mechanism 55 can prevent the entire reconstituted tobacco sheet manufacturing apparatus 100K from stopping.
[0108] As described above, according to the seventeenth embodiment, by further providing a buffer mechanism 55 downstream of the die 20 for temporarily holding the reconstituted tobacco sheet 1 extruded from the die 20, it is possible to deal with cases where the extrusion speed of the reconstituted tobacco sheet 1 and the rotation speed of the drum main body 32 cannot be synchronized.
[0109] Although several embodiments of the present invention have been described above, the above-mentioned embodiments of the present invention are intended to facilitate understanding of the present invention and do not limit the present invention. The present invention may be modified or improved without departing from the spirit thereof, and the present invention includes equivalents thereof. Furthermore, the components described in the claims and the specification may be combined or omitted within the scope of solving at least part of the above-mentioned problems or achieving at least part of the effects. [Explanation of symbols]
[0110] 1. Reconstituted tobacco sheet 10, 10A~10X...Extruder 11. Housing 12…Supply inlet 13...Extrusion port 14…Screw 20, 20A~20X…Die 21…1st Block 22...Second Block 23. Housing 24…Supply inlet 25…Manifold 26…Discharge port 27…Partition 28...Protuberance 30...Drum dryer 31...Axis 32…Drum body 35...Drum dryer 36…Axis 37…Drum body 40…Scraper 45…Scraper 51...Laura 52...Laura 53…Slitting drum 55...Buffer mechanism 56…Fixed roller 57...Movable roller 61~63…Extruder 70…Die 71~73…Supply port 74…Discharge port 80…Hot air blower 91...Detection sensor 92…Variable width mechanism 93...Flow sensor 94...Moisture sensor 95...addition mechanism 100, 100A~100L…Reconstituted tobacco sheet manufacturing equipment
Claims
1. An apparatus for producing a reconstituted tobacco sheet, comprising: a die for forming the reconstituted tobacco material into a sheet and discharging it; a main drum that dries and conveys the sheet-shaped reconstituted tobacco material discharged from the die; a slitting drum that cuts the sheet-like reconstituted tobacco material that has been dried and transported by the main drum, The die includes: Housing and a supply port formed in the housing through which the reconstituted tobacco material is supplied; an outlet formed on one side of the housing for outletting the reconstituted tobacco material; The slitting drum has at least two blades that rotate opposite to each other. Reconstituted tobacco sheet manufacturing equipment.
2. 2. The reconstituted tobacco sheet manufacturing apparatus according to claim 1, The packaging device is further provided after the slitting drum, The packaging device includes: a weighing mechanism that measures the weight of a container in which the reconstituted tobacco material cut by the slitting drum is packed; a conveying mechanism that conveys the container to the weighing mechanism and conveys the container out of the weighing mechanism; Reconstituted tobacco sheet manufacturing equipment.
Citation Information
Patent Citations
Reconstituted tobacco shredding device through ultrasonic waves
CN104489896A
Production method of substitutive tobacco sheet
CN108477663A
Cutting device for strip
JP1999226895A
Casting apparatus and method for checking cast sheet thickness
JP2019520036A
Restructured tobacco dryer
US5203354A