Phosphine detector

A phosphine detector using basic copper carbonate and cellulose fibers with specified sizes for continuous detection addresses the limitations of existing electrically dependent detectors, offering power-free, responsive phosphine exposure monitoring.

JP7578653B2Active Publication Date: 2024-11-06YAZAKI CORP
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
JP2022126235
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-08-08
Publication Date
2024-11-06
Estimated Expiration
2042-08-08

AI Technical Summary

Technical Problem

Existing phosphine detectors require electricity and intermittently sample gas, making it difficult to constantly detect high phosphine exposure concentrations in small articles and are costly.

Method used

A phosphine detector comprising basic copper carbonate particles, cellulose fibers, and a binder, with specific size ranges, that changes color in response to phosphine exposure without electricity, allowing continuous detection.

Benefits of technology

The detector provides continuous, highly responsive phosphine detection without power consumption, enabling visual or machine-readable color change for high concentration detection.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007578653000001
    Figure 0007578653000001
  • Figure 0007578653000002
    Figure 0007578653000002
  • Figure 0007578653000003
    Figure 0007578653000003
Patent Text Reader

Abstract

To provide a highly responsive phosphine detector capable of constantly detecting phosphine with no electricity.SOLUTION: A phosphine detector 1 is provided, comprising a support 10, a plurality of basic copper carbonate particles supported on a surface of the support 10, and a phosphine detection unit 20 containing a plurality of cellulose fibers and a binder for biding the plurality of basic copper carbonate particles to the plurality of cellulose fibers. The plurality of basic copper carbonate particles has an average particle diameter of 0.01 to 1 μm, inclusive, the plurality of cellulose fibers has an average length of 5 to 30 μm, inclusive, and the binder has an average particle diameter of 80 nm to 1 μm, inclusive. An average fiber diameter of the plurality of cellulose fibers is greater than the average particle diameter of the binder.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a phosphine detector. [Background technology]

[0002] Fumigation with phosphine PH3 is widely used in warehouses, on ships, and inside equipment to eliminate pests. For example, fumigation on a cargo ship usually involves exposing the cargo to a prescribed amount of phosphine for several days or more with the cargo holds closed.

[0003] However, since phosphine is harmful to humans, it is necessary to detect phosphine in the environment. Conventionally, detection of phosphine in the environment has been performed using gas measurement devices equipped with a gas detection mechanism such as an electrically powered sensor, and gas detector tubes, etc. When using gas detector tubes, detection is performed using gas samples that are intermittently drawn in from the environment by hand or electrically.

[0004] Patent Document 1 discloses a gas measurement device that uses a detection paper carrying a reagent that reacts with multiple types of measurement gases such as phosphine to produce a reaction mark that changes in optical density. This gas measurement device can measure the types and concentrations of multiple types of measurement gases. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2015-232532 A Summary of the Invention [Problem to be solved by the invention]

[0006] In recent years, it has become desirable to know the level of past phosphine exposure concentration for each item that has been subjected to fumigation. In order to detect the level of past phosphine exposure concentration, it is preferable to be able to constantly detect the phosphine exposure concentration for each item. Furthermore, in order to constantly detect the phosphine exposure concentration for many items loaded onto a cargo ship or the like, a detector that does not require human intervention is required.

[0007] However, the gas measuring device of Patent Document 1 requires electricity. Therefore, it is difficult for the gas measuring device of Patent Document 1 to constantly detect the phosphine exposure concentration of small individual items, and there is a problem that the cost of constant detection is high. In addition, the gas detection tube intermittently sucks in and detects the gas sample, so there is a problem that the phosphine exposure concentration cannot be constantly detected.

[0008] The present invention has been made in consideration of the problems inherent in the conventional techniques. An object of the present invention is to provide a phosphine detector that is capable of constantly detecting phosphine without power consumption and has high responsiveness. [Means for solving the problem]

[0009] A phosphine detector according to an embodiment of the present invention includes a support and a phosphine detector supported on the surface of the support and including a plurality of basic copper carbonate particles, a plurality of cellulose fibers, and a binder that binds the plurality of basic copper carbonate particles and the plurality of cellulose fibers. The average particle diameter of the basic copper carbonate particles is 0.01 μm or more and 1 μm or less. The average length of the cellulose fibers is 5 μm or more and 30 μm or less. The average particle diameter of the binder is 80 nm or more and 1 μm or less. The average fiber diameter of the cellulose fibers is larger than the average particle diameter of the binder. Effect of the Invention

[0010] According to the present invention, it is possible to provide a phosphine detector that is capable of constantly detecting phosphine without power consumption and has high responsiveness. [Brief description of the drawings]

[0011] [Figure 1] FIG. 1 is a schematic plan view showing an example of a phosphine detection element according to an embodiment of the present invention. [Diagram 2] 2 is a schematic cross-sectional view of the phosphine detecting element according to the present embodiment taken along line II-II in FIG. 1. [Diagram 3] This shows the results of evaluating the response to phosphine exposure due to differences in binder types. [Figure 4] This shows the results of evaluating the responsiveness to phosphine exposure depending on the film thickness of the phosphine detection part. [Diagram 5] This shows the results of evaluating the response to phosphine exposure due to differences in the composition of the phosphine detection part. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] The phosphine detection element according to the present embodiment will be described in detail below with reference to the drawings. Note that the dimensional ratios in the drawings are exaggerated for the convenience of explanation and may differ from the actual ratios.

[0013] [Phosphine detector] Fig. 1 is a plan view of a phosphine detection element 1 according to this embodiment. Fig. 2 is a cross-sectional view of the phosphine detection element 1 according to this embodiment taken along line II-II in Fig. 1. As shown in Figs. 1 and 2, the phosphine detection element 1 includes a support 10 and a phosphine detection unit 20 supported on the surface of the support 10.

[0014] (Support) The support 10 supports the phosphine detection unit 20. The material of the support 10 is not particularly limited, and may include, for example, at least one selected from the group consisting of paper, plastic, metal, ceramics, and wood. The support 10 may be capable of supporting the phosphine detection unit 20 at least on the surface of the support 10. For this reason, the phosphine detection unit 20 may be formed inside the support 10 in addition to on the surface of the support 10 by impregnating the inside of the support 10 with a detection ink described below.

[0015] The support 10 may be, for example, paper. Paper can reduce the emission of carbon dioxide into the atmosphere from the viewpoint of carbon neutrality. In addition, paper is inexpensive and combustible, so it can be easily disposed of together with other constituent materials.

[0016] The support 10 may be, for example, a label sticker. By simply printing the phosphine detection unit 20 on the label sticker, it can be easily used as an indicator that can be attached to an object.

[0017] The shape of the support 10 is not particularly limited as long as it can support the phosphine detection unit 20. Examples of the shape of the support 10 include a flat plate, a curved plate, and a polygonal prism such as a cube or a rectangular parallelepiped.

[0018] When the support 10 is a flat plate, the thickness of the support 10 may be 0.1 mm or more and 5 mm or less. When the thickness of the support 10 is within the above range, it is easy to handle as the phosphine detection element 1. The thickness of the support 10 may be 0.2 mm or more. In addition, the thickness of the support 10 may be 2 mm or less, 1 mm or less, or 0.5 mm or less.

[0019] (Phosphine detection unit) The phosphine detection unit 20 includes a plurality of basic copper carbonate particles, a plurality of cellulose fibers, and a binder. In the phosphine detection unit 20, each of the plurality of cellulose fibers may form a gap between the cellulose fibers. Also, each of the plurality of basic copper carbonate particles may be disposed between each of the plurality of cellulose fibers.

[0020] <Basic copper carbonate particles> Basic copper carbonate is reactive to phosphine and is chemically stable when exposed to substances other than phosphine. Specifically, basic copper carbonate is less likely to discolor due to temperature and humidity compared to copper acetate. Also, basic copper carbonate is not excessively reactive compared to silver acetate. More specifically, silver acetate can detect phosphine at a low concentration such as 1 ppm, but is prone to discoloration due to temperature, humidity and light, making it difficult to determine whether it is exposed to a concentration such as 100 ppm. On the other hand, basic copper carbonate has different reactivity depending on the exposure concentration and exposure time of phosphine. Therefore, by using basic copper carbonate, a phosphine detection unit 20 can be formed in which the reactivity to the exposure concentration and exposure time of phosphine is controlled.

[0021] Basic copper carbonate may contain Cu(OH)2·CuCO3, also known as malachite. Cu(OH)2·CuCO3 is green before exposure to phosphine, and has the property of turning black when reduced by exposure to phosphine. The color of Cu(OH)2·CuCO3 changes to black, which is presumably due to Cu, the reaction product of Cu(OH)2·CuCO3 and phosphine, as shown in the following reaction formula (1). Note that the by-products in the following reaction formula (1) include, for example, solids derived from phosphoric acid.

[0022] 2Cu(OH)2·CuCO3+PH3→Cu+byproducts (1)

[0023] In addition, copper phosphate and copper oxide (Cu2O), which are produced due to the reaction of 2Cu(OH)2·CuCO3 with phosphine, also react with phosphine to produce black reaction products.

[0024] There may be voids between the multiple basic copper carbonate particles contained in the phosphine detection unit 20. The average particle size of the basic copper carbonate particles is not particularly limited, but may be smaller than the average fiber size of the cellulose fibers. In such a case, since an appropriate amount of voids can be formed by the cellulose fibers, the reactivity of the phosphine detection unit 20 can be maintained at a good level.

[0025] Specifically, the average particle diameter of the plurality of basic copper carbonate particles is 0.01 μm or more and 1 μm or less. When the average particle diameter is 0.01 μm or more, the basic copper carbonate particles fill the gaps between the fibers, and the internal basic copper carbonate particles can be prevented from being less exposed to phosphine. When the average particle diameter is 1 μm or less, the specific surface area of ​​the basic copper carbonate particles increases, and the reactivity increases. In addition, since the cellulose fibers can form appropriate gaps, the reactivity of the phosphine detection unit 20 can be maintained at a good level. The average particle diameter of the basic copper carbonate particles may be 0.05 μm or more, or may be 0.1 μm or more. The average particle diameter of the basic copper carbonate particles may be 0.5 μm or less, or may be 0.2 μm or less. In this specification, the value of the "average particle diameter" is, unless otherwise specified, a value calculated as the average particle diameter of particles observed in several to several tens of fields of view using an observation means such as a scanning electron microscope (SEM) or a transmission electron microscope (TEM).

[0026] The content of the multiple basic copper carbonate particles is preferably 30% by mass or more and 50% by mass or less with respect to the phosphine detection unit 20. By setting the content of the basic copper carbonate particles to 30% by mass or more, the responsiveness of the phosphine detection unit 20 becomes higher. Furthermore, by setting the content of the basic copper carbonate particles to 50% by mass or less, it is possible to suppress the occurrence of cracks in the phosphine detection unit 20. The content of the basic copper carbonate particles may be 35% by mass or more. Furthermore, the content of the basic copper carbonate particles may be 45% by mass or less, or may be 40% by mass or less.

[0027] The shape of the basic copper carbonate particles is not particularly limited, and may be at least one shape selected from the group consisting of needle-like, angular, dendritic, fibrous, flaky, irregular, teardrop-like, and spherical.

[0028] The specific surface area of ​​the basic copper carbonate particles is not particularly limited. The larger the specific surface area, the higher the reaction responsiveness tends to be.

[0029] <Cellulose fiber> The cellulose fibers are entangled to form gaps between the cellulose fibers. The gaps improve the air permeability, so that when the phosphine detection unit 20 is exposed to phosphine, the phosphine can easily come into contact with the basic copper carbonate particles. The cellulose fibers can also support the basic copper carbonate particles.

[0030] From the viewpoint of carbon neutrality, cellulose fibers can reduce carbon dioxide emissions into the atmosphere. In addition, cellulose fibers are industrially produced in various sizes, so they can be obtained at low cost, and can be selected according to the purpose, such as controlling the reactivity due to voids, making them easy to form into films and mold. In addition, cellulose fibers are safer than carbon nanofibers and ceramic fibers, and there is no need to worry about their effects on the respiratory system, so they can be handled safely during production and use. In addition, cellulose fibers are flammable and easy to dispose of, and basic copper carbonate is also easily disposed of together with copper oxide (II), carbon dioxide, and water at 220°C. In addition, cellulose fibers are less likely to have a negative effect on reactivity.

[0031] The average length of the plurality of cellulose fibers is 5 μm or more and 30 μm or less. When the average length of the cellulose fibers is 5 μm or more, appropriate voids are formed, and the reactivity of the phosphine detection unit 20 is increased. Furthermore, when the average length of the cellulose fibers is 30 μm or less, defects are less likely to occur when the detection ink is printed by screen printing. The average length of the cellulose fibers may be 6 μm or more. Furthermore, the average length of the cellulose fibers may be 20 μm or less, or 10 μm or less.

[0032] The average fiber diameter of the cellulose fibers is larger than the average particle diameter of the binder. With this configuration, appropriate voids are formed in the phosphine detection unit 20, and when the phosphine detection element 1 is exposed to phosphine, the basic copper carbonate particles are more likely to react with phosphine.

[0033] The average fiber diameter of the plurality of cellulose fibers may be 5 μm or more and 30 μm or less. When the average fiber diameter of the cellulose fibers is 5 μm or more, appropriate voids are formed, and the reactivity of the phosphine detection unit 20 is increased. Furthermore, when the average fiber diameter of the cellulose fibers is 30 μm or less, problems are less likely to occur when the detection ink is printed by screen printing. The average fiber diameter of the cellulose fibers may be 6 μm or more. Furthermore, the average fiber diameter of the cellulose fibers may be 20 μm or less, or 10 μm or less.

[0034] The aspect ratio of the average length to the average fiber diameter of the cellulose fibers may be 1 or more and 1.5 or less. When the aspect ratio is 1 or more, appropriate voids are formed, and the reactivity of the phosphine detection unit 20 is increased. Furthermore, when the aspect ratio is 1.5 or less, problems are less likely to occur when the detection ink is printed by screen printing. The aspect ratio may be 1.3 or less, or may be 1.1 or less.

[0035] Unless otherwise specified, the average length and average fiber diameter of multiple cellulose fibers are calculated as the average length or diameter of cellulose fibers observed in several to several tens of fields of view using an observation means such as a scanning electron microscope (SEM) or a transmission electron microscope (TEM).

[0036] The content of cellulose fiber may be 20% by mass or more and 40% by mass or less with respect to the phosphine detection unit 20. By making the content of cellulose fiber 20% by mass or more, it is possible to suppress the occurrence of cracks in the phosphine detection unit 20. Furthermore, by making the content of cellulose fiber 40% by mass or less, the responsiveness of the phosphine detection unit 20 is further improved. The content of cellulose fiber may be 30% by mass or more. Furthermore, the content of cellulose fiber may be 35% by mass or less.

[0037] <Binder> The binder binds a plurality of basic copper carbonate particles and a plurality of cellulose fibers. The binder is a plurality of particles. The material of the binder is not particularly limited, but an organic binder may be used. The binder may contain, for example, at least one of a resin and a cellulose nanofiber. The resin used in the binder may contain at least one selected from the group consisting of an acrylic resin, an epoxy resin, a vinyl resin, and a cellulose resin. Examples of the cellulose resin include hydroxyethyl cellulose.

[0038] The average particle diameter of the binder is 80 nm or more. By having the average particle diameter of the binder be 80 nm or more, the gaps formed by the cellulose fibers are prevented from being filled, the breathability of the phosphine detection unit 20 is maintained, and good reactivity can be obtained when the phosphine detection body 1 is exposed to phosphine. The average particle diameter of the binder may be smaller than the average particle diameter of the basic copper carbonate particles. The average particle diameter of the binder is 1 μm or less. When the average particle diameter is 1 μm or less, the cellulose fibers can form appropriate gaps, so that the reactivity of the phosphine detection unit 20 can be kept good. The average particle diameter of the binder may be 90 nm or more. In addition, the average particle diameter of the binder may be 500 nm or less, 200 nm or less, 150 nm or less, or 120 nm or less. In this specification, the value of the "average particle diameter" is, unless otherwise specified, a value calculated as the average value of particle diameters of particles observed in several to several tens of fields of view using an observation means such as a scanning electron microscope (SEM) or a transmission electron microscope (TEM).

[0039] The shape of the binder is not particularly limited, and may be at least one shape selected from the group consisting of needle-like, angular, dendritic, fibrous, flaky, irregular, teardrop-like, and spherical.

[0040] The binder content may be 25 mass% or more and 40 mass% or less with respect to the phosphine detection unit 20. By setting the binder content within the above range, the responsiveness of the phosphine detection unit 20 can be improved. The binder content may be 27 mass% or more. In addition, the binder content may be 38 mass% or less, 33 mass% or less, or 30 mass% or less.

[0041] 1 and 2, the phosphine detection unit 20 of the phosphine detection element 1 has a trapezoidal cross-sectional shape. However, the phosphine detection unit 20 of this embodiment may have a cross-sectional shape other than a trapezoid, for example, a rectangular shape. The phosphine detection unit 20 may also have a barcode or QR code (registered trademark) shape.

[0042] The thickness of the phosphine detection unit 20 may be 20 μm or more and 200 μm or less. When the thickness of the phosphine detection unit 20 is 20 μm or more, the coloring of the phosphine detection unit can be clearly confirmed. Furthermore, when the thickness of the phosphine detection unit 20 is 200 μm or less, cracks are less likely to occur on the surface of the phosphine detection unit 20, and unevenness in the reaction of the phosphine detection unit 20 can be suppressed. The thickness of the phosphine detection unit 20 may be 50 μm or more. Furthermore, the thickness of the phosphine detection unit 20 may be 120 μm or less, or 80 μm or less.

[0043] The phosphine detection element 1 is placed on the surface of or in a measurement target article to which exposure to phosphine is to be measured. When the phosphine detection element 1 is placed on the surface of or in a measurement target article, it may simply be placed on the surface of or in the measurement target article, or it may be attached using an adhesive, adhesive tape, or the like.

[0044] Next, the function of the phosphine detector 1 will be described. The phosphine detector 20 of the phosphine detector 1 changes color before and after exposure to a predetermined amount of phosphine. For example, the basic copper carbonate Cu(OH)2·CuCO3 contained in the phosphine detector 20 has the property of being green before exposure to phosphine, and changing color to black when reduced by exposure to phosphine.

[0045] The discoloration of the phosphine detection unit 20 maintains the color after discoloration once. Therefore, the phosphine detection element 1 can detect the level of the phosphine exposure concentration in the past. The discoloration of the phosphine detection element 20 can be detected visually or by machine to detect the degree of discoloration. Furthermore, since the discoloration is based on the reduction of basic copper carbonate by phosphine, it occurs without electricity. Furthermore, since the above action occurs without electricity, it is possible to constantly detect exposure to phosphine. Furthermore, since the above discoloration occurs only in the phosphine detection element 1, it is possible to miniaturize the phosphine detection element 1 within a range where the discoloration can be detected.

[0046] The phosphine detector 1 of this embodiment includes a support 10 and a phosphine detector 20 supported on the surface of the support 10 and including a plurality of basic copper carbonate particles, a plurality of cellulose fibers, and a binder that binds the plurality of basic copper carbonate particles and the plurality of cellulose fibers together. The average particle diameter of the basic copper carbonate particles is 0.01 μm or more and 1 μm or less. The average length of the cellulose fibers is 5 μm or more and 30 μm or less. The average particle diameter of the binder is 80 nm or more and 1 μm or less. The average fiber diameter of the cellulose fibers is larger than the average particle diameter of the binder.

[0047] According to the phosphine detector 1, the color of the phosphine detection section 20 changes before and after exposure to a predetermined amount of phosphine. Therefore, the phosphine detector 1 is small and can constantly detect phosphine without requiring electricity.

[0048] Furthermore, the basic copper carbonate particles, cellulose fibers, and binder in the phosphine detection unit 20 have a predetermined size. Therefore, appropriate gaps are formed between the cellulose fibers, the breathability of the phosphine detection unit 20 is maintained, and good reactivity can be obtained when the phosphine detection element 1 is exposed to phosphine.

[0049] In addition, basic copper carbonate is an insulator, and when it reacts with phosphine, copper, which is a conductor, is produced from basic copper carbonate. Therefore, it may be possible to detect copper electrically. For example, it may be possible to detect copper remotely by incorporating the phosphine detector 1 into an RFID (radio frequency identifier).

[0050] [Manufacturing method of phosphine detector] Next, a method for producing the phosphine detection element 1 according to this embodiment will be described. The phosphine detection element 1 can be obtained by forming a phosphine detection unit 20 on the surface of a support 10. Specifically, the phosphine detection element 1 according to this embodiment may include a step of preparing a detection ink, a step of applying the detection ink to the support 10, and a step of removing the dispersion liquid.

[0051] In the step of preparing the detection ink, a detection ink containing basic copper carbonate particles, cellulose fibers, and a binder is prepared. The detection ink can be obtained by mixing the basic copper carbonate particles, cellulose fibers, and the binder by stirring or the like. The basic copper carbonate particles, cellulose fibers, and binder may be those described above.

[0052] The detection ink may be prepared using a binder liquid dispersed in a dispersion liquid. The binder liquid has fluidity in the detection ink, and when the phosphine detection unit 20 is formed, the binder contained in the phosphine detection unit 20 binds the basic copper carbonate particles and the cellulose fibers. The binder liquid containing the binder may be a slurry or an emulsion. The dispersion liquid contained in the binder liquid may be, for example, an inorganic solvent such as water, or an organic solvent such as alcohol.

[0053] The detection ink may contain a dispersion liquid for adjusting the fluidity of the detection ink, if necessary. However, if the detection ink has the desired fluidity with the dispersion liquid contained in the binder liquid, additional dispersion liquid does not need to be added to the detection ink. For example, an inorganic solvent such as water or an organic solvent such as alcohol is used as the dispersion liquid. The dispersion liquid contained in the binder liquid and the dispersion liquid additionally added to the detection ink may be the same type or different types. Among these, it is preferable to use water as the dispersion liquid from the viewpoint of environmental consideration.

[0054] In the step of applying the detection ink to the support 10, the ink prepared in the step of preparing the detection ink is applied to the support 10. The method of applying the detection ink to the support 10 is not particularly limited, and the detection ink can be applied, for example, by dripping, coating, spraying, printing, and combinations thereof. Examples of dripping include dripping onto the support 10 using a dropper or pipette. Examples of coating include coating using a bar coater. Examples of printing include screen printing, toner printing, inkjet printing, letterpress printing, intaglio printing, and combinations thereof. Among these, it is preferable to apply the detection ink to the support 10 by screen printing from the viewpoint of making the film thickness uniform.

[0055] In the step of removing the dispersion liquid, the dispersion liquid is removed from the detection ink applied to the support 10. By removing the dispersion liquid from the detection ink, a phosphine detection unit 20 is formed, which includes a plurality of basic copper carbonate particles, a plurality of cellulose fibers, and a binder that binds the plurality of basic copper carbonate particles and the plurality of cellulose fibers together. Methods for removing the dispersion liquid include filtration such as suction filtration, natural drying at room temperature, drying by heating, and combinations of these.

[0056] According to the method described above, the phosphine detector 1 including the support 10 and the phosphine detection unit 20 described above can be manufactured. EXAMPLES

[0057] The present embodiment will be described in more detail below with reference to examples and comparative examples, but the present embodiment is not limited to these examples.

[0058] The following materials were prepared as raw materials for the detection inks of the Examples and Comparative Examples. (1) Basic copper carbonate particles Cu(OH)2·CuCO3 (Kanto Chemical Co., Ltd., copper(II) carbonate (basic), 2N5), average particle size 1μm (2) Cellulose fibers NP Fiber W-06MG (Nippon Paper Industries Co., Ltd.), fiber diameter 6 μm, fiber length 6 μm (3) Binder (3-1) Binder A Saibinol (registered trademark) EC-2020 (Saiden Chemical Co., Ltd.) Acrylic resin emulsion, concentration 42 wt%, viscosity 1,040 mPa·s, particle size 100 nm, Tg 11°C (3-2) Binder S BiNFi-s WFo-10002 (Sugino Machine Co., Ltd.), aqueous slurry containing cellulose nanofibers, concentration 2% by mass, viscosity 6,000 mPa·s, fiber diameter 10 nm to 50 nm, fiber length several to several tens of μm, (3-3) Binder N Cellenpia (registered trademark) TEMPO oxidized CNF (1% standard product) (Nippon Paper Industries Co., Ltd.), aqueous slurry containing cellulose nanofibers, concentration 1% by mass, viscosity 4,500 mPa s, fiber diameter 4 nm, fiber length up to approximately 1 μm (3-4) Binder C Hydroxyethyl cellulose (reagent: H0392) (Tokyo Chemical Industry Co., Ltd.), water-soluble cellulose powder, viscosity 5,500 mPa·s (when dissolved in 2% water), fiber diameter 0.4 nm, fiber length up to 3 μm (4)Water Ion-exchanged water (electrical conductivity 0.1μS / cm)

[0059] [Example 1] First, basic copper carbonate particles were crushed to an average particle size of approximately 0.1 μm. Next, 0.2 g (8.6 mass%) of the crushed basic copper carbonate particles, 0.2 g (8.6 mass%) of cellulose fiber, 0.408 g (7.4 mass%) of binder, and 1,520 μL (75.5 mass%) of water were mixed and stirred for 3 hours to prepare the detection ink. Binder A was used as the binder.

[0060] Next, the quantitatively collected detection ink was applied to a support (label sticker, A-one (registered trademark) 72244, 3M) with a bar coater to a coating thickness of 100 μm, and then dried and cured for about 1 hour at 25° C. Then, a phosphine detection element was produced, which contained 35% by mass of basic copper carbonate particles, 35% by mass of cellulose fiber, and 30% by mass of binder, and had a phosphine detection portion with a film thickness of about 30 μm formed on the support.

[0061] [Comparative Example 1] First, basic copper carbonate particles were crushed to an average particle diameter of about 0.1 μm. Next, 0.2 g (2.7% by mass) of the crushed basic copper carbonate particles, 0.2 g (2.7% by mass) of cellulose fiber, 3.529 g of binder (0.9% by mass of binder component), and 3530 μL (93.7% by mass) of water were mixed and stirred for 3 hours to prepare the detection ink. Binder S was used as the binder.

[0062] Next, the quantitatively collected detection ink was applied to a support (label sticker, A-one (registered trademark) 72244, 3M) with a bar coater to a coating thickness of 100 μm, and then dried and cured for about 1 hour at 25° C. Then, a phosphine detection element was produced, which contained 42.5 mass% basic copper carbonate particles, 42.5 mass% cellulose fiber, and 15 mass% binder, and had a phosphine detection portion with a film thickness of about 30 μm formed on the support.

[0063] [Comparative Example 2] First, basic copper carbonate particles were crushed to an average particle diameter of about 0.1 μm. Next, 0.2 g (2.7% by mass) of the crushed basic copper carbonate particles, 0.2 g (2.7% by mass) of cellulose fiber, 7.058 g of binder (0.9% by mass of binder component), and 0 μL (93.7% by mass) of water were mixed and stirred for 3 hours to prepare the detection ink. Binder N was used as the binder.

[0064] Next, the quantitatively collected detection ink was applied to a support (label sticker, A-one (registered trademark) 72244, 3M) with a bar coater to a coating thickness of 100 μm, and then dried and cured for about 1 hour at 25° C. Then, a phosphine detection element was produced, which contained 42.5 mass% basic copper carbonate particles, 42.5 mass% cellulose fiber, and 15 mass% binder, and had a phosphine detection portion with a film thickness of about 30 μm formed on the support.

[0065] [Comparative Example 3] First, basic copper carbonate particles were crushed to an average particle diameter of about 0.1 μm. Next, 0.2 g (2.7% by mass) of the crushed basic copper carbonate particles, 0.2 g (2.7% by mass) of cellulose fiber, 3.529 g of binder (0.9% by mass of binder component), and 3530 μL (93.7% by mass) of water were mixed and stirred for 3 hours to prepare the detection ink. Binder C was used as the binder.

[0066] Next, the quantitatively collected detection ink was applied to a support (label sticker, A-one (registered trademark) 72244, 3M) with a bar coater to a coating thickness of 100 μm, and then dried and cured for about 1 hour at 25° C. Then, a phosphine detection element was produced, which contained 42.5 mass% basic copper carbonate particles, 42.5 mass% cellulose fiber, and 15 mass% binder, and had a phosphine detection portion with a film thickness of about 30 μm formed on the support.

[0067] [Comparative Example 4] First, basic copper carbonate particles were crushed to an average particle size of about 0.1 μm. Next, 0.5 g (10.5% by mass) of the crushed basic copper carbonate particles, 0.5 g (10.5% by mass) of cellulose fiber, 0 g of binder (0% by mass of binder component), and 3750 μL (78.9% by mass) of water were mixed and stirred for 3 hours to prepare the detection ink.

[0068] Next, the quantitatively collected detection ink was applied to a support (label sticker, A-one (registered trademark) 72244, 3M) with a bar coater to a coating thickness of 100 μm, and then dried and cured for about 1 hour at 25° C. Then, a phosphine detection element was produced, which contained 50 mass % basic copper carbonate particles and 50 mass % cellulose fibers and had a phosphine detection portion with a film thickness of about 30 μm formed on the support.

[0069] [evaluation] (Fumigation test) First, a 100 L acrylic chamber was prepared in a laboratory set at approximately 25°C. Next, the phosphine detector obtained as described above was placed in the 100 L acrylic chamber. Next, while checking the concentration with a gas detector tube, phosphine standard gas was continuously injected into the acrylic chamber so that the phosphine concentration in the acrylic chamber was 100 ppm. Then, photographs of the phosphine detector were taken at predetermined intervals. The results are shown in Figure 3.

[0070] As shown in Fig. 3, the phosphine detection element of Example 1 changed color from green to black after 22 hours of exposure to phosphine, and was able to detect phosphine. On the other hand, the phosphine detection elements of Comparative Examples 1 to 4 did not achieve the same sensitivity as Example 1, even after 22 hours of exposure to phosphine. It was also confirmed that the color change of the phosphine detection part increased as the binder diameter increased.

[0071] Next, we confirmed the effect of differences in film thickness on the response to phosphine exposure.

[0072] [Example 2] First, basic copper carbonate particles were crushed to an average particle size of about 0.1 μm. Next, 4 g (14 mass%) of the crushed basic copper carbonate particles, 4 g (14 mass%) of cellulose fiber, 8.1633 g of binder (12 mass% binder component), and 12,480 μL (60 mass%) of water were mixed and stirred for 3 hours to prepare the detection ink. Binder A was used as the binder.

[0073] Next, the quantitatively collected detection ink was applied to a support (label sticker, A-one (registered trademark) 64201, 3M) using a screen printer to a coating thickness of 100 μm, and then dried and cured for about 1 hour at 25° C. Then, a phosphine detection element was produced, which contained 35 mass% basic copper carbonate particles, 35 mass% cellulose fibers, and 30 mass% binder, and had a phosphine detection portion with a film thickness of 30 μm formed on the support.

[0074] [Example 3] A phosphine detector was prepared in the same manner as in Example 2, except that the film thickness of the phosphine detector was 70 μm.

[0075] [Example 4] A phosphine detector was prepared in the same manner as in Example 2, except that the film thickness of the phosphine detector was 100 μm.

[0076] [evaluation] (Fumigation test) A fumigation test was carried out in the same manner as described above, and the results are shown in Figure 4.

[0077] As shown in Figure 4, in all Examples, a change in color of the phosphine detection part from green to black due to exposure to phosphine was confirmed. In particular, a clear color change due to exposure to phosphine was confirmed in Example 3, in which the film thickness was 70 µm, and Example 4, in which the film thickness was 100 µm.

[0078] Next, we confirmed the effect of differences in the detection ink formulation on the response to phosphine exposure.

[0079] [Examples 5 to 10] A phosphine detector was produced in the same manner as in Example 4, except that the detection ink was prepared so that the phosphine detection part had the composition shown in FIG.

[0080] [evaluation] (Fumigation test) A fumigation test was carried out in the same manner as described above, and the results are shown in Figure 5.

[0081] As shown in FIG. 5, in all the examples, the color of the phosphine detection part was changed from green to black due to exposure to phosphine. In particular, when the binder amount was set to 30 mass%, it was confirmed that the responsiveness of the phosphine detection body was superior to that when the binder amount was set to 35 mass%. It was also confirmed that the responsiveness of the phosphine detection body was superior as the content of basic copper carbonate particles was increased. However, although not shown in the figure, if the amount of basic copper carbonate particles was increased too much, there is a risk of increasing cracks.

[0082] From the above results, it was confirmed that phosphine can be detected continuously without electricity and that a highly responsive phosphine detector can be provided.

[0083] Although the present embodiment has been described above, the present embodiment is not limited to this, and various modifications are possible within the scope of the gist of the present embodiment. [Explanation of symbols]

[0084] 1 Phosphine detector 10 Support 20 Phosphine detector

Claims

1. A support; a phosphine detection unit supported on a surface of the support and including a plurality of basic copper carbonate particles, a plurality of cellulose fibers, and a binder that binds the plurality of basic copper carbonate particles and the plurality of cellulose fibers, respectively; Equipped with The binder includes a resin, The average particle size of the plurality of basic copper carbonate particles is 0.01 μm or more and 1 μm or less, The average length of the plurality of cellulose fibers is 5 μm or more and 30 μm or less, The average particle size of the binder is 80 nm or more and 120 nm or less, A phosphine detection element, wherein an average fiber diameter of the plurality of cellulose fibers is larger than an average particle diameter of the binder.

2. The phosphine detection element according to claim 1 , wherein a content of the binder is 25% by mass or more and 33% by mass or less with respect to the phosphine detection part.

3. 3. The phosphine detection element according to claim 1, wherein a content of the plurality of basic copper carbonate particles is 30% by mass or more and 50% by mass or less with respect to the phosphine detection portion.

4. 3. The phosphine detector according to claim 1, wherein the thickness of the phosphine detection part is 50 μm or more and 200 μm or less.

5. 3. The phosphine detector according to claim 1, wherein the average fiber diameter of the plurality of cellulose fibers is 5 μm or more and 30 μm or less.

6. A phosphine detector as described in claim 1 or 2, wherein the binder resin includes an acrylic resin.

7. A phosphine detection body as described in claim 1 or 2, wherein the average particle diameter of the binder is 80 nm or more and 100 nm or less.

Citation Information

Patent Citations

  • Test paper for detecting arsine

    JP1982010451A

  • Detection agent

    JP1986296268A

  • Multi-layered analyzing element

    JP1987047552A

  • Test paper

    JP2002277453A

  • Sensing element and method

    JP2007278926A