Composite Film
A composite film with a polymer matrix of two polyolefin components addresses the challenge of recyclability and sealing strength in aluminum-based cover sheets by achieving thin layer thicknesses and high production speeds, ensuring effective sealing and recyclability.
Patent Information
- Application Number
- JP2022522828
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-10-17
- Filing Date
- 2020-10-16
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2040-10-16
AI Technical Summary
Existing cover sheets for packaging containers, particularly those made from aluminum foil, face challenges in achieving reduced plastic content for recyclability while maintaining strong sealing adhesion and peelability, often leading to processing difficulties due to the addition of mineral fillers which deteriorate the extrusion process.
A composite film with a thin extruded layer comprising a polymer matrix of two polymeric components, including a first polyolefin and a second polyolefin plastomer or elastomer, allows for reduced plastic content and improved recyclability, achieving high linear speeds during production without defects, and provides strong sealing seam strength.
The composite film achieves thin layer thicknesses of 10-18 g/m² for the extruded layer, ensuring good sealing seam strength and recyclability, while avoiding processing issues and maintaining peelability, with the ability to produce cover sheets at high linear speeds.
Smart Images

Figure 0007578685000001
Abstract
Description
[Technical field]
[0001] The present disclosure relates to composite films, cover sheets, and methods for making the composite films. [Background technology]
[0002] Particularly in the food and pet food sectors, so-called cover sheets are used to seal packaging containers, which are sealed to the edges of the containers to seal the packaging containers. Examples of such packaging containers include, for example, yogurt cups, trays or similar containers.
[0003] In particular, for good processability, advantageous barrier properties and recyclability, these cover sheets are often made of aluminum foil, which is optionally printed, painted and / or embossed and coated with sealing material on the sealing side. Depending on the embodiment, the sealing material is, for example, a laminated sealing film, a sealing varnish, an extrusion coating or a combination of these techniques. In this case, the layer applied on the aluminum foil often not only serves to ensure sealing, but also, in some cases, serves to impart structural properties to the cover sheet, such as, for example, improved puncture resistance, more advantageous tear behavior, high burst pressure, etc.
[0004] DE 10253110 B4 for example discloses a cover sheet which comprises an aluminium layer which is coated with at least three coextrusion coatings.
[0005] Since only the aluminum portion of this cover sheet can be recycled without problems, there is an interest in reducing the portion of the material applied as the sealing layer. However, this is in conflict with technical requirements: on the one hand, the sealing layer must be strong enough to produce a sufficiently good sealing adhesion, and on the other hand, it should have good peel behavior, i.e. this must be possible without the consumer using excessive force to peel the cover sheet from the packaging container (and without the cover sheet being torn). In addition, it must also be taken into consideration that the sealing layer is suitable for the packaged goods, e.g. food. To improve the peel behavior, peel additives, in particular mineral fillers, such as talc, can be added to the material of the sealing layer. However, this mineral filler deteriorates the processability of the polymer material and leads to problems during extrusion. It is therefore necessary to extrude the appropriate sealing layer with a relatively large layer thickness.
[0006] WO 2012 / 113530 A1 describes a composite film consisting of an aluminum foil in combination with a coextruded layer consisting of an intermediate layer consisting of polypropylene mixed with a filler and connected to it on both sides with adhesion promoter layers consisting of polypropylene modified with maleic anhydride.
[0007] US 5,626,929 A describes a composite film comprising an aluminum layer laminated with a sealing layer using a urethane adhesive. The sealing layer is composed of a mixture of butene-1 / ethylene copolymer and ethylene homopolymer, and an inorganic filler. The sealing layer has a thickness of 24 g / m 2 ~48g / m 2 0.5 mm thick, so that the proportion of plastic in the composite film is high. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] DE10253110B4 [Patent Document 2] WO2012 / 113530A1 [Patent Document 3] US5,626,929A [Patent Document 4] WO2007 / 115816A1 [Patent Document 5] US2004 / 0236042A1 [Patent Document 6] US7557172B2 Summary of the Invention [Problem to be solved by the invention]
[0009] The present disclosure aims, inter alia, to provide an aluminum cover sheet that has improved recyclability, thereby allowing the proportion of plastic to be reduced, and that can be extruded onto an aluminum layer. [Means for solving the problem]
[0010] In a first aspect, the disclosure relates to a composite film (particularly for producing a cover sheet) according to claim 1. Furthermore, the disclosure also relates to a method for producing such a composite film (particularly for producing a cover sheet). The extruded layer can therefore be produced particularly thin, and in addition, high line speeds can be achieved during production. Line speeds of about 400 m / min or more can be achieved without defects or holes in the molten film of the extruded layer. This is an unexpected effect, since the addition of a release force additive usually reduces the melt strength to such an extent that the corresponding extruded layer must be designed thicker or the line speed must be reduced. Surprisingly, by adding a second polymer component, the thickness of the extruded layer can be significantly reduced at a constant high line speed. At the same time, good and solid sealing seam strength can be achieved.
[0011] In the present invention, the extrusion layer is 10 to 18 g / m 2 , especially 10 g / m 2 and 15g / m 2 and the total thickness is between 100 and 200 g / m 2 and 5g / m 2 and the thickness of the sealing layer is in particular between 6 g / m 2 and 10g / m 2 This very thin coating allows the ratio of polymer to aluminum in the composite film to be adjusted to very low values, so that the composite film can be used below the limit values that determine the recyclability of the composite film.
[0012] Advantageously, the proportion of the first polymer component in the polymer matrix can be between about 30% and about 70% by weight, which in particular allows the melt viscosity to be adjusted to an advantageous value.
[0013] In one advantageous embodiment, the proportion of the second polymer component in the polymer matrix can be between 30% and 70% by weight. By selecting the proportion of the second polymer component, in particular the sealing seam strength and burst pressure of the cover sheet produced from the composite film can be influenced in a targeted and advantageous manner.
[0014] In yet another advantageous embodiment, the aluminum layer, preferably consisting of a soft or semi-rigid aluminum foil, can be applied with a thickness of 10 μm to 70 μm, in particular 20 to 38 μm, which provides very good barrier properties and allows the production of cover sheets with customary customer desired properties such as feel, appearance, peel behavior, etc.
[0015] Optionally, the extruded layer may have an outer cover layer adjacent to the sealing layer, the cover layer having a thickness of 1 g / m 2 and 3g / m 2Preferably, the cover layer has a thickness between 0.01 mm and 0.1 mm. The cover layer is thin enough so as not to adversely impair, at least essentially, the function of the sealing layer. In some cases, the cover layer may also impart advantageous properties to the surface, for example by improving the thermal adhesion properties. The cover layer offers process-technical advantages, especially during the production of the composite film, since deposition of the release force additive on the extrusion die is avoided.
[0016] The second polymer component may preferably comprise a polymer component selected from ethylene / propylene copolymers, in particular semi-crystalline ethylene-propylene copolymers (which are especially substantially free of dienes), alpha-olefin copolymers, in particular ethylene / alpha-olefin copolymers and / or propylene / alpha-olefin copolymers, ethylene-propylene-diene elastomers, and combinations of these materials.
[0017] The disclosure further relates to a cover sheet for sealing packaging containers, which is produced from the composite film described above, in particular by punching or cutting.
[0018] The present disclosure further relates to a method for producing a cover sheet for sealing a packaging container, the cover sheet being produced, in particular by punching or cutting, from a composite film produced by the method described herein.
[0019] The invention will now be explained in more detail below with reference to FIG. 1, which shows an exemplary, schematic and non-limiting advantageous embodiment of the invention. [Brief description of the drawings]
[0020] [Figure 1] FIG. 1 shows the layer structure of the cover sheet. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0021] The composite film 1, shown diagrammatically in cross section in FIG. 1 for producing a cover sheet, essentially has an aluminum layer 2, which is coated on its product-facing side with a multilayer extrusion layer 3. Optionally, the side of the aluminum layer 2 facing away from the product can be provided with a primer layer 4 for printing. The representation in FIG. 1 is purely schematic and not to scale. In particular, it therefore does not represent real thickness ratios.
[0022] The extruded layer 3 is applied onto the aluminum layer 2 as a coextrusion during the working process and comprises an adhesion promoter layer 5 and a peelable sealing layer 6. Optionally, a thin cover layer 7 can additionally be applied onto the sealing layer. The extruded layer 3 is preferably applied to a thickness of 10 g / m 2 and 18g / m 2 Between 10g / m 2 and 15g / m 2 The total thickness is between .
[0023] The aluminum layer 2 preferably consists of a soft or semi-rigid aluminum foil and has a preferred thickness of about 20 μm to about 38 μm. In some cases, the thickness may be thicker or thinner if desired or necessary for a particular application. Usually, aluminum layers having a thickness of, for example, between 10 μm and 70 μm are used for cover sheets. The aluminum layer 2 serves as a substrate onto which the stack of extruded layers 3 is applied in a coextrusion process.
[0024] The adhesion promoter layer 5 improves the adhesion between the sealing layer 6 and the aluminum layer 2, and a large number of materials are known in the prior art that can be used to manufacture the adhesion promoter layer 5. Exemplarily, said materials for the adhesion promoter layer 5 include ethylene-acrylic acid copolymers (EAA), ethylene-methacrylic acid (EMAA), maleic anhydride modified LDPE (PE-g-MAOH), terpolymers (e.g. Lotader from Arkema), and the like. TM), ionomers, and similar materials considered in the art to be suitable for this purpose, or combinations of these materials.
[0025] The adhesion promoter layer 5 should in particular enable good adhesion between the sealing layer 6 and the aluminum layer 2, even without subsequent necessary heat treatment, for example for full activation of the adhesion promoter layer 5. Such heat treatment, which is typically carried out after coextrusion at temperatures between 200° C. and 300° C., can negatively affect the flatness of the composite film 1. For example, this can lead to curling of the cover sheet produced with the composite film 1, which impairs the processability of the cover sheet, in particular the sealing on the container for sealing the container. Such problems can occur when using maleic anhydride grafted adhesion promoters (for example PP-MAOHs or PP-MAOH). The previously described adhesion promoters, which can also be used in particular with a polyethylene-based sealing layer 6, are directly deposited on the aluminum layer 2 and do not require a heat treatment after coextrusion.
[0026] The adhesion promoter layer 5 is preferably 3 g / m 2 and 5g / m 2 The layer thickness can be extruded with a layer thickness between 0.01 and 0.05 mm. The layer thickness actually required is usually selected according to the manufacturer's instructions. The layer thickness of the adhesion promoter layer can be selected, for example, according to the following criteria: This layer thickness is selected as thin as possible, since a sufficiently thick sealing layer is required for sealing with an overall thin coating (a total thickness of up to 18 g is preferred), and from a cost point of view, the above-mentioned materials are generally more expensive than those used for the sealing layer. However, the adhesion promoter layer must be thick enough so that a consistently uniform layer remains to ensure sufficiently good adhesion of the extrusion coating on the aluminum foil.
[0027] The sealing layer 6 has a polymer matrix to which a release force additive is added in a proportion of between 10% and 35% by weight. The sealing layer 6 is particularly preferably 6 g / m 2 and 12g / m 2In order to achieve better recyclability of the composite film, it is sensible to minimize the thickness of the extruded layer and in this case especially the thickness of the sealing layer 6. In this case, the sealing layer 6 should be as thin as possible, while still ensuring the necessary sealing seam strength and peel properties. Another technical limitation is the manufacturability of the extruded layer 3, since if the layer thickness is too thin, holes and other defects can form in the extruded layer 3. Minimizing the thickness of the extruded layer is within the capabilities of an average person skilled in the art with knowledge of the teachings disclosed herein.
[0028] The release force additive can be, in particular, a mineral filler, which is especially food-compatible.In particular, the release force additive can be selected from talc, CaCO3, chalk, silicate (e.g. mica, kaolin), other mineral fillers or a combination of these materials.The release force additive can have a particle size that does not impair or only negligibly impairs the thin sealing layer, especially in a given sealing layer.In particular, the particle size D98 ("top cut") can be, for example, less than 20 μm.
[0029] The polymer matrix of the encapsulation layer 6 includes at least two different polymer components, which are referred to herein as a "first polymer component" and a "second polymer component." Optionally, additional polymer components may be present. The designations selected are merely for identification purposes and should not be construed as limiting.
[0030] The first polymer component is a polyolefin, in particular a polyethylene, especially a low density polyethylene (LDPE). However, other polyethylene types, such as linear low density polyethylene (LLDPE), medium density polyethylene (MDPE) or high density polyethylene (HDPE), can also be considered. However, due to the molecular structure, LDPE is particularly well suited. The proportion of the first polymer component in the polymer matrix is between about 30% and about 70% by weight.
[0031] The first polymer component serves as the "base material" of the sealing layer 6 and influences not only the cost of the material but also the basic parameters that need to be considered with regard to processability, such as melt viscosity, stretchability or melt strength and melt film stability of the polymer matrix or sealing layer 6 during extrusion. By varying the proportion of the first polymer component, in particular the melt viscosity of the polymer matrix can be varied. Advantageous melt viscosities of the polymer matrix are in the range of between about 2 g / 10 min and about 15 g / 10 min in terms of melt flow index (MFI value).
[0032] The second polymer component is 900 kg / m 3 The proportion of the second polymer component in the polymer matrix is between about 10% and about 40% by weight.
[0033] "Polyolefin plastomers and polyolefin elastomers" in the context of this disclosure refer to copolymers based on polyolefins, which have a lower density (900 kg / m) than the corresponding homopolymers. 3 less than 1000 .mu.m) and greater elasticity. Examples of polyolefin plastomers and / or elastomers include, but are not limited to, ethylene / propylene copolymers, especially those containing propylene and small proportions of ethylene, ethylene / alpha-olefin copolymers, propylene / alpha-olefin copolymers, ethylene-propylene-diene elastomers, and combinations of these materials. Polyolefin plastomers and elastomers combine the properties of elastomers (i.e., materials that are form-stable but elastically deformable) with the advantages of other plastics, such as their processability.
[0034] In the technical literature, a distinction is sometimes made between polyolefin plastomers and polyolefin elastomers, where the maximum elastic modulus is generally 885 kg / m 3~900kg / m 3 Materials having a density of 885 kg / cm3 are called polyolefin plastomers, especially at low densities, i.e. for example 885 kg / cm3. 3 At densities below 1000 MPa, the term polyolefin elastomer is preferably used. However, the above distinction is not always used consistently. Therefore, for the sake of clarity, in the context of this disclosure, the term "polyolefin plastomer and / or polyolefin elastomer" is used consistently for all these polymers. Thus, the above terms, as used herein, include both materials referred to in the art as polyolefin plastomers and materials referred to as polyolefin elastomers.
[0035] Polyolefin plastomers and polyolefin elastomers are generally characterized by high toughness and high puncture resistance, good compatibility with fillers and oils, and excellent mixability with polyolefins.
[0036] In practical applications, it is important to ensure the mixability of the first, second and possibly further polymer components. This can be achieved, inter alia, by the selection and adaptation of material parameters, where the most important parameters of the second polymer component are taken as an example below.
[0037] An important parameter for the evaluation of the processability of polymeric materials is the melt index, in particular the melt mass flow rate (MFR) and the associated melt volume flow rate (MVR). In the context of the present disclosure, the terms "melt mass flow rate" (MFR) and "melt volume flow rate" (MVR) refer to values determined according to the standard DIN EN ISO 1133 in the version in force on the priority date of this application. MFR is also referred to in the literature and practice as "melt index", "melt flow rate", "melt mass flow rate" or "melt flow index" (MFI). Similarly, MVR is also referred to in the literature and practice as "melt volume rate" or "melt volume index" (MVI).
[0038] Preferred values for the melt mass flow rate of the second polymer component at 2.16 kg and 190° C. range between 2 g / 10 min and 15 g / min.
[0039] A further important parameter for the selection of the second polymer component is the breaking elongation, the values of which can be determined according to the standard DIN EN ISO 527 in the version in force on the priority date of this application.
[0040] Preferred values for the elongation at break of the second polymer component are at least several times the elongation at break of the first polymer component, in particular more than 200%, especially more than 1000%.
[0041] The melting temperature of the second polymer component is in particular lower than the melting temperature of the first polymer component. In this case, the melting temperature can be measured according to any method, provided that the same method is used for the first and second polymer components (i.e., the values are measured in a similar manner and therefore comparable). For example, the melting temperature can be measured according to the standard DIN EN ISO3146, the version of which is valid at the priority date of this application.
[0042] Preferably, the melting temperature value of the second polymer component is less than 90%, in particular less than 80%, than the corresponding melting temperature of the first polymer component.
[0043] For example, polyolefin plastomers or polyolefin elastomers that can be used as the second polymer component or as part of the second polymer component include, for example, "Vistamaxx" from Exxon Mobil Chemical. TM " from The Dow Chemical Company under the name "Versify TM " and "Aplyfy TM " from Borealis AG under the name "Queo TM" from Sumitomo Chemical under the name "ESPRENE SPO TM " or Mitsui Elastomers Singapore PTE LTD. under the name "Tafmer TM ". In some cases, combinations or mixtures of these materials, optionally including additional polyolefin plastomers and / or polyolefin elastomers of other types, can also be used as the second polymer component. The polyolefin plastomers and polyolefin elastomers that can be used according to the present disclosure are not limited to currently commercially available products, but include all polyolefin plastomers and polyolefin elastomers that are known in the art or that can be produced from materials known in the art by the average person skilled in the art with possible parameter changes.
[0044] Polyolefin plastomers or polyolefin elastomers which can be used, for example, as the second polymer component or as part of the second polymer component are also disclosed, for example, in the following patent documents: WO2007 / 115816A1 (Patent Document 4) discloses a propylene-based polyolefin elastomer, which is referred to in this document as a "propylene based elastomer". It comprises a first semi-crystalline polymer component in the form of a copolymer consisting of up to 95% by weight of propylene and a limited proportion of ethylene.
[0045] US 2004 / 0236042 A1 (Patent Document 5) discloses a method for producing a polyolefin elastomer, in particular a thermoplastic polymer composition using a major proportion of propylene and a relatively small proportion of ethylene.
[0046] US7557172B2 (Patent Document 6) discloses ethylene-based polyolefin plastomers, which are ethylene / alpha-olefin copolymers.
[0047] The contents of US2004 / 0236042A1, US7557172B2 and WO2007 / 115816A1 are hereby incorporated by reference into the description or application of this invention wherever this is possible.
[0048] Although it is true that a higher proportion of the second polymer component may result in more difficult or laborious processing during extrusion, the seal seam strength of the sealing layer 6 is improved, especially when the sealing layer 6 is formed thin. In addition to the seal seam strength, the burst pressure can also be favorably influenced by varying the proportion of the second polymer component.
[0049] When selecting materials for the second polymer component, it should be taken into account that the lower the density of the second polymer component, the more elastomeric (i.e. rubber-like) it will behave. However, the melting point will also be lowered and the adhesion will be increased (due to the softening of the material at elevated temperatures). This may lead to processing problems during extrusion (e.g. adhesion to chill rolls) or to processing problems of the finished material (e.g. blocking on rolls, runnability of the material web). The average person skilled in the art, with knowledge of the teachings disclosed herein, can meaningfully select the appropriate combination of materials by routine work and testing, taking into account the attendant conditions described in this regard.
[0050] The polymer matrix of the sealing layer 6 may optionally contain additional polymeric components in amounts up to 25% by weight.
[0051] This further polymer component may in particular be selected from LLDPE (C4, C6, C8), mLLDPE (C4, C6, C8), polypropylene homopolymer, polypropylene copolymer, or a combination of such materials.
[0052] Said further polymer components can be useful, for example, to influence the sealing properties. For example, they can be adapted to a particular cup material, for example a cup comprising polypropylene and / or polyethylene in various proportions. Furthermore, for hot-filling (where better thermal adhesion properties are required), it can be advantageous to increase the melting point of the sealing material, for example by using C6 polymer as the further polymer component, since this has a higher melting point than the first polymer component, for example LDPE.
[0053] The cover layer 7, if provided, has a density in particular of 1 to 3 g / cm 2 The material of the cover layer 7 is in particular selected from LDPE, LLDPE, MDPE or a combination of these materials.
[0054] The cover layer 7 is very thin and therefore only influences the sealing properties of the sealing layer 6 to an insubstantial extent, at least in a negative way. The application of the cover layer 7 is particularly advantageous in terms of process technology, for example, the cover layer isolates the walls of the extrusion die from the material of the sealing layer 6. This avoids the deposition of mineral fillers, in particular talc, on the extrusion die.
[0055] In the detailed description and claims, the terms "essentially" or "about" mean, unless otherwise stated where appropriate, a deviation of up to 10% of the stated value, both downward and upward where physically possible, or only in the direction that is otherwise meaningful, and thus, in the case of degrees (angles and temperature), ±10°.
[0056] All quantity descriptions and percentage descriptions, especially those for the purpose of limiting the present invention, should be understood with a tolerance of ±10%, except in relation to the examples. Thus, a description of "11%" means, for example, "9.9% to 12.1%". In descriptions such as "solvent", the word "ein" should not be regarded as a numeral, but as an indefinite article or pronoun, unless the context indicates otherwise.
[0057] The term "combination" or "combinations" refers to all types of combinations, from two of the associated components to many or all of such components, unless otherwise stated, and the term "comprising" also refers to "consisting of."
[0058] Individual features and variations described in individual configurations and examples may be freely combined with individual features and variations of other examples and configurations (unless otherwise stated where appropriate) and may be used without necessarily combining other details of each configuration or each example in order to characterize the invention, particularly in the claims. While this application is directed to the invention set forth in the claims, the disclosure of this application also includes: 1. A composite film (1) having an aluminum layer (2) and a sealing layer (6), in particular a composite film (1) for producing a cover sheet, wherein the sealing layer (6) comprises a polymer matrix having at least a first polymer component and a second polymer component, the polymer matrix of the sealing layer (6) being doped with a release force additive, in particular a mineral filler, for example talc, the first polymer component being selected from polyolefins, and the second polymer component each having a release force of 900 kg / m or more. 3 A composite film (1), comprising a polyolefin plastomer and / or a polyolefin elastomer having a density of less than 1000 nm, and combinations of such materials, The composite film (1) includes an extruded layer (3) extruded in multiple layers by coextrusion onto the aluminum layer (2), the extruded layer (3) includes a sealing layer (6) and an adhesion promoter layer (5) disposed between the sealing layer (6) and the aluminum layer (2), and the extruded layer (3) has a coating weight of 10 to 18 g / m 2 , especially 10g / m 2 and 15g / m 2 and the thickness of the adhesion promoter layer (5) is in particular 3 g / m 2 and 5g / m 2 and the thickness of the sealing layer (6) is in particular between 6 g / m 2 and 10g / m 2 The composite film (1) is characterized in that 2. The composite film (1) according to claim 1, characterized in that the proportion of the first polymer component in the polymer matrix is in particular between about 30% and about 70% by weight. 3. The composite film (1) according to 1 or 2 above, characterized in that the first polymer component is polyethylene, in particular low-density polyethylene. 4. The composite film (1) described in any one of 1. to 3. above, characterized in that the proportion of the second polymer component in the polymer matrix is between 30% and 70% by weight. 5. The composite film (1) according to any one of 1. to 4. above, characterized in that the aluminum layer (2), preferably made of soft or semi-rigid aluminum foil, is formed to a thickness of 10 μm to 70 μm, particularly 20 to 38 μm. 6. The extrusion layer (3) has an outer cover layer (7) adjacent to the sealing layer (6), and the cover layer (7) is preferably 1 g / m 2 and 3g / m 2 The composite film (1) described in any one of 1. to 5. above, characterized in that it has a thickness between. 7. The composite film (1) according to any one of 1. to 6. above, characterized in that the second polymer component comprises a polymer component selected from ethylene / propylene copolymers, in particular semicrystalline ethylene-propylene copolymers (which are particularly substantially free of dienes), alpha-olefin copolymers, in particular ethylene / alpha-olefin copolymers and / or propylene / alpha-olefin copolymers, ethylene-propylene-diene elastomers, and combinations of such substances. 8. A cover sheet for sealing a packaging container, which is produced from a composite film (1) according to any one of 1. to 7. above, in particular by punching or cutting. 9. A method for producing a composite film (1), in particular a composite film (1) for producing a cover sheet, comprising the steps of: - providing an aluminum layer (2), and - extruding a multi-layer extruded layer (3) onto the aluminum layer (2), the multi-layer extruded layer (3) including an adhesion promoter layer adjacent to the aluminum layer (2) and a sealing layer (6) adjacent to the adhesion promoter layer (5), the extruded layer (3) being at a coating weight of 10 to 18 g / m 2 , especially 10g / m 2 and 15g / m 2 and the thickness of the adhesion promoter layer (5) is in particular between 3 g / m 2 and 5g / m 2 and the thickness of the sealing layer (6) is in particular between 6 g / m 2 and 10g / m 2 The step between Including, The sealing layer (6) comprises a polymer matrix having at least a first polymer component and a second polymer component, wherein the polymer matrix of the sealing layer (6) is doped with a release force additive, in particular a mineral filler such as talc, and the first polymer component is selected from polyolefins, and the second polymer component has a density of 900 kg / m or less, respectively. 3 selected from polyolefin plastomers and / or polyolefin elastomers, and combinations of such materials; The method. 10. The method according to claim 9, characterized in that the proportion of the first polymer component in the polymer matrix is in particular between about 30% and about 70% by weight. 11. The method according to claim 9 or 10, wherein the first polymer component is polyethylene, in particular low density polyethylene. 12. The method according to any one of 9. to 11. above, characterized in that the proportion of the second polymer component in the polymer matrix is between 30% and 70% by weight. 13. The method according to any one of the above items 9 to 11, characterized in that the aluminum layer (2), preferably made of a soft or semi-rigid aluminum foil, is formed to a thickness of 10 μm to 70 μm, particularly 20 to 38 μm. 14. The extrusion layer (3) has an outer cover layer (7) adjacent to the sealing layer (6), and the cover layer (7) is preferably 1 g / m 2 and 3g / m 2 The method according to any one of the above items 9 to 13, characterized in that the thickness is between . 15. A method for producing a cover sheet for sealing a packaging container, the cover sheet being produced, in particular by punching or cutting, from a composite film (1) produced by a method according to any one of claims 9 to 14 above.
Claims
1. A composite film (1) having an aluminum layer (2) and a sealing layer (6), the sealing layer (6) comprises a polymer matrix having at least a first polymer component and a second polymer component, the polymer matrix of the sealing layer (6) is added with a release force additive in a proportion between 10% and 35% by weight, the first polymer component is selected from polyolefins, and the second polymer component has a release force of 900 kg / m or more, respectively. 3 A composite film (1) comprising a polyolefin plastomer and / or a polyolefin elastomer having a density of less than 1000 nm, and a combination of such materials, The composite film (1) comprises an extruded layer (3) extruded in multiple layers by coextrusion onto the aluminum layer (2), the extruded layer (3) comprises a sealing layer (6) and an adhesion promoter layer (5) disposed between the sealing layer (6) and the aluminum layer (2), and the extruded layer (3) has a total thickness of 10 to 18 g / m2.
2. A composite film (1) as described in claim 1, characterized in that the thickness of the adhesion promoter layer (5) is between 3 g / m 2 and 5 g / m 2 .
3. A composite film (1) according to claim 1 or 2, characterized in that the thickness of the sealing layer (6) is between 6 g / m 2 and 10 g / m 2 .
4. A composite film (1) according to any one of claims 1 to 3, characterized in that the proportion of the first polymer component in the polymer matrix is between about 30% and about 70% by weight.
5. A composite film (1) according to any one of claims 1 to 4, characterized in that the first polymer component is polyethylene.
6. A composite film (1) according to any one of claims 1 to 5, characterized in that the proportion of the second polymer component in the polymer matrix is between 30 and 70% by weight.
7. A composite film (1) described in any one of claims 1 to 6, characterized in that the aluminum layer (2) made of aluminum foil is formed with a thickness of 10 μm to 70 μm.
8. The extruded layer (3) has an outer cover layer (7) adjacent to the sealing layer (6), the cover layer (7) having a thickness of 1 g / m 2 and 3 g / m 2 A composite film (1) according to any one of claims 1 to 7, characterized in that it has a thickness between
9. 9. The composite film (1) according to any one of claims 1 to 8, characterized in that the second polymer component comprises a polymer component selected from ethylene / propylene copolymers, alpha-olefin copolymers, ethylene-propylene-diene elastomers, and combinations of such materials.
10. A composite film (1) according to any one of claims 1 to 9, characterized in that the release force additive is a mineral filler.
11. A composite film (1) according to any one of claims 1 to 9, characterized in that the release force additive is talc.
12. A cover sheet for sealing packaging containers, which is produced by punching or cutting from a composite film (1) according to any one of claims 1 to 11.
13. A method for producing a composite film (1) comprising the steps of: - providing an aluminium layer (2), and - extruding a multi-layer extruded layer (3) onto the aluminium layer (2), the multi-layer extruded layer (3) comprising an adhesion promoter layer adjacent to the aluminium layer (2) and a sealing layer (6) adjacent to the adhesion promoter layer (5), the extruded layer (3) having a total thickness of 10-18 g / m2; Including, The sealing layer (6) comprises a polymer matrix having at least a first polymer component and a second polymer component, wherein the polymer matrix of the sealing layer (6) is added with a release force additive in a proportion between 10% and 35% by weight, and the first polymer component is selected from polyolefins, and the second polymer component has a density of 900 kg / m 3 selected from polyolefin plastomers and / or polyolefin elastomers, and combinations of such materials; The method.
14. The method according to claim 13, characterized in that the thickness of the adhesion promoter layer (5) is between 3 g / m 2 and 5 g / m 2 .
15. The method according to claim 13 or 14, characterized in that the thickness of the sealing layer (6) is between 6 g / m 2 and 10 g / m 2 .
16. The method according to any one of claims 13 to 15, characterized in that the proportion of the first polymer component in the polymer matrix is between about 30% and about 70% by weight.
17. The method according to any one of claims 13 to 16, characterized in that the first polymer component is polyethylene.
18. 18. The method according to claim 13, wherein the proportion of the second polymer component in the polymer matrix is between 30% and 70% by weight.
19. The method according to any one of claims 13 to 17, characterized in that the aluminum layer (2) made of aluminum foil is formed with a thickness of 10 μm to 70 μm.
20. The extruded layer (3) has an outer cover layer (7) adjacent to the sealing layer (6), the cover layer (7) having a thickness of 1 g / m 2 and 3 g / m 2 20. The method according to claim 13, characterized in that the layer has a thickness between 0.01 and 0.
1.
21. The method according to claim 13, wherein the release force additive is a mineral filler.
22. The method according to any one of claims 13 to 20, characterized in that the release force additive is talc.
23. A method for producing a cover sheet for sealing a packaging container, the cover sheet being produced by punching or cutting from a composite film (1) produced by the method according to any one of claims 13 to 22.
Citation Information
Patent Citations
lid composite material with coextrusion coating
DE10253110B4
Sealant material for polypropylene and readily openable hermetically sealed container
JP2002179852A
Sealant film, packaging material, lid material, and container
JP2006305886A
Lid material
JP2013202980A
Lid material and method for manufacturing the same
JP2015033824A